A processing technology for ultra-thin irregularly shaped tendons in all-steel tire molds
By combining electrical discharge molding with 3D additive manufacturing and embedding a rib base, the processing problem of ultra-thin irregular ribs in all-steel tire molds has been solved, achieving efficient and high-quality processing results and improving the service life and appearance quality of tire molds.
Patent Information
- Application Number
- CN202310906435.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-07-24
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-07-24
AI Technical Summary
Existing technologies struggle to efficiently process the complex ultra-thin irregularly shaped tendons of all-steel tire molds, resulting in problems such as high electrode wear, long processing cycles, rough surfaces, and low fatigue strength. Furthermore, the development cycle is tight.
The method employs electrical discharge molding combined with 3D additive manufacturing and embedding the rib base. The ultra-thin rib is protected by electrical drilling of reference grooves, 3D additive processing and auxiliary punch tools, and spot welding is used to enhance its firmness, thus achieving efficient processing.
It shortens the processing cycle, improves the rigidity and fatigue strength of ultra-thin irregular ribs, avoids the instability of electrical discharge machining, and enhances the service life and appearance quality of the mold.
Smart Images

Figure CN119347319B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of all-steel tire mold pattern processing technology, specifically a processing technology for ultra-thin irregular ribs in all-steel tire molds. Background Technology
[0002] Tire molds are used for vulcanizing and molding various types of tires. They are an important tool used in the tire vulcanization process. In current technology, the processing of tread patterns for all-steel tire molds generally adopts electrical discharge molding (EDM). This process can complete the processing of conventional tread patterns. In recent years, as the design of all-steel tire tread patterns has become more three-dimensional and complex, with the emergence of irregular ribs, some shortcomings of the EDM process have become increasingly apparent.
[0003] ① The spindles of existing three-axis electrode engraving and milling machines and EDM forming equipment can only move in a directional manner, which cannot meet the shape requirements of complex ribs with multiple undercuts;
[0004] ② The electrode wear is high and sintering is easy when the ultra-thin ribs are electro-machined, so a large current cannot be used, the electro-machine efficiency is low and the processing cycle is long.
[0005] ③ Electrical discharge molding can cause surface roughness, cracking, and reduced fatigue strength in extremely thin ribs, thus reducing the service life of tire molds;
[0006] ④ When customers put forward new mold product requirements, the development cycle is very tight. How to achieve the processing of extremely thin irregular shapes and other difficult patterns, and how to shorten the processing cycle of patterns are technical problems that urgently need to be solved by those skilled in the art.
[0007] Based on this, a processing technology for ultra-thin irregular ribs in all-steel tire molds is now provided, which can eliminate the drawbacks of existing equipment. Summary of the Invention
[0008] The purpose of this invention is to provide a processing technology for ultra-thin irregularly shaped ribs in all-steel tire molds, so as to solve the problems in the background art.
[0009] To achieve the above objectives, the present invention provides the following technical solution:
[0010] A processing technology for ultra-thin irregularly shaped ribs in an all-steel tire mold includes the following steps:
[0011] Step 1: Electro-etch the irregular patterned ribs of the patterned ring, and use a graphite electrode to etch the cavity material with the etched lines as the positioning reference to form an electro-etched reference groove using a single-section frequency etching process.
[0012] Step 2: The ultra-thin irregular ribs are processed using 3D additive manufacturing. A special embedded rib base is added to ensure that there is a grinding allowance at the joints of the ultra-thin irregular ribs. The width and depth are consistent with the dimensions of the single-section slotted electrode in Step 1. The chamfered bottom of the rib base is used to prevent interference from the rounded corners caused by electrode wear during the later embedding operation.
[0013] Step 3: During the embedding operation, the rib points are subjected to overload, and the extremely thin parts of the ribs are easily deformed and damaged. A special auxiliary punch tool is made, namely, an embedding punch, to protect the extremely thin parts of the ribs from stress and keep them intact.
[0014] Step 4: Combine Step 1 and Step 2 to form a complete cavity pattern. Spot weld at the joints to enhance the firmness between the ultra-thin irregular ribs and the pattern block body. Trim the pattern block to make the overall pattern appearance uniform.
[0015] Preferably, the processing in step 1 uses an electrical discharge machining (EDM) machine to electrically machine the embedded groove of the ultra-thin irregular-shaped rib with standard parameters, which requires roughing, semi-finishing and finishing.
[0016] Preferably, before the 3D additive manufacturing of the ultra-thin irregular-shaped rib in step 2, the pattern ring is processed into segments using a wire cutting device, and then a single piece is used for the rib embedding operation.
[0017] Preferably, in step 3, the auxiliary punch tool, i.e., the material and hardness of the embedded punch must be greater than that of the rib part.
[0018] Preferably, the embedded punch is made of 45# steel that has been quenched and has a hardness greater than HRC55.
[0019] Preferably, the depth and width error of the groove around the entire pattern in step 1 is ≤0.05mm.
[0020] Preferably, the length of the rib base in step 2 is 0.2 mm.
[0021] Compared with the prior art, the beneficial effects of the present invention are as follows:
[0022] This invention solves the technical problem of existing molding processes being unable to achieve multiple undercut surfaces for complex patterns by combining electrical discharge grooving, 3D additive manufacturing, and subsequent embedding processes. It breaks through the limitations of traditional electrical discharge, which is characterized by low efficiency and long cycle time, and greatly shortens the processing cycle of patterns. When the thickness of the pattern is less than 0.8mm, the processing quality is better than that of traditional electrical discharge machining. The pattern has high rigidity and fatigue resistance, and avoids the phenomenon of sintering caused by instability in the electrical discharge process, which greatly improves the appearance quality and service life of the pattern. Attached Figure Description
[0023] Figure 1 This is a schematic diagram of step A1 of the present invention.
[0024] Figure 2 This is a schematic diagram of step A2 of the present invention.
[0025] Figure 3 This is a cross-sectional schematic diagram of the structure in step A2 of the present invention.
[0026] Figure 4 This is a schematic diagram of step A3 of the present invention.
[0027] Figure 5 This is a diagram showing the complete cavity effect after step A4 of the present invention.
[0028] Figure 6 This is a flowchart of the process steps for the ultra-thin irregular rib of the all-steel tire mold of the present invention.
[0029] Figure label annotations: 1. Electro-drilled reference groove; 2. Ultra-thin irregular rib; 3. Rib base; 4. Embedded punch. Detailed Implementation
[0030] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments.
[0031] Please see Figures 1-6 A processing technology for ultra-thin irregularly shaped ribs in an all-steel tire mold includes the following steps:
[0032] Step 1: Electro-drill lines are drawn on the irregular patterned ribs of the patterned ring. Using graphite electrodes as the positioning reference, the cavity material is etched with a single-section frequency to form an electro-drilled reference groove 1.
[0033] Step 2: The ultra-thin irregular rib 2 is processed using 3D additive manufacturing. A special embedded rib base 3 is added so that there is a grinding allowance at the joint of the two ultra-thin irregular ribs 2. The width and depth are consistent with the dimensions of the single-section slotted electrode in Step 1. The bottom chamfer of the rib base 3 is used to prevent the rounded corner interference caused by electrode wear during the later embedding operation.
[0034] Step 3: During the embedding operation, the rib points are subjected to overload, and the extremely thin parts of the ribs are easily deformed and damaged. A special auxiliary punch tool is made, namely, the embedding punch 4, to protect the extremely thin parts of the ribs from stress and keep them intact.
[0035] Step 4: Combine Step 1 and Step 2 to form a complete cavity pattern. Spot weld at the joints to enhance the firmness between the ultra-thin irregular rib 2 and the pattern block body. Trim the pattern block to make the overall pattern appearance uniform.
[0036] Please see Figure 1In step 1, the processing is carried out using an electrical discharge machining (EDM) machine. The embedded groove of the ultra-thin irregular rib 2 is electrically machined using standard parameters, which requires roughing, semi-finishing and finishing.
[0037] Please see Figures 2-3 Before the 23D additive manufacturing of the ultra-thin irregular rib in step 2, the pattern ring is processed into segments using wire cutting equipment and then made into individual pieces for rib embedding.
[0038] Please see Figure 4 In step 3, the auxiliary punch tool, namely the embedded punch 4, must be made of a material with a hardness greater than that of the rib part, so as to continuously withstand the impact force of the embedding operation, and prevent the embedded punch 4 from being worn, twisted, or losing its reference, which would result in poor rib embedding effect.
[0039] Please see Figures 2-3 The embedded punch 4 is made of 45# steel and quenched, with a hardness greater than HRC55.
[0040] Please see Figure 1 In step 1, the depth and width of the groove around the entire pattern have an error of ≤0.05mm.
[0041] Please see Figures 2-3 In step 2, the length of the rib base 3 is increased by 0.2mm.
[0042] The above description is merely a specific embodiment of this disclosure, but the scope of protection of this disclosure is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this disclosure should be included within the scope of protection of this disclosure. Therefore, the scope of protection of this disclosure should be determined by the scope of the claims.
Claims
1. A processing technology for ultra-thin irregularly shaped reinforcing bars in an all-steel tire mold, characterized in that, Includes the following steps: Step 1: Electro-drill lines are drawn on the irregular patterned ribs of the patterned ring. Using graphite electrodes, the lines are used as positioning references, and the cavity material is etched at a single frequency to form an electro-drilled reference groove (1). Step 2: The ultra-thin irregular rib (2) is processed by 3D additive manufacturing. A special embedded rib base (3) is added so that there is a grinding allowance at the joint of the two ultra-thin irregular ribs (2). The width and depth are consistent with the dimensions of the single-section slotted electrode in Step 1. The bottom chamfer of the rib base (3) is used to prevent the rounded corner interference caused by electrode wear during the later embedding operation. Step 3: During the embedding operation, the rib points are subjected to overload, and the extremely thin parts of the ribs are easily deformed and damaged. To make a special auxiliary punch tool, namely, setting an embedding punch (4), the extremely thin parts of the ribs are protected from stress and kept intact. Step 4: The above steps 1 and 2 are combined to form a complete cavity pattern. Spot welding is performed at the joints to enhance the firmness between the ultra-thin irregular rib (2) and the pattern block body. The pattern block is then trimmed to make the overall pattern appearance uniform. Before the 3D additive manufacturing of the ultra-thin irregular rib (2) in step 2, the pattern ring is processed by wire cutting equipment to be divided into petals and then into a single piece for rib embedding. In step 3, the auxiliary punch tool, namely the material and hardness of the embedded punch (4) must be greater than that of the rib part; The embedded punch (4) is made of 45# steel and quenched, with a hardness greater than HRC55.
2. The processing technology for ultra-thin irregular-shaped ribs in an all-steel tire mold according to claim 1, characterized in that, In step 1, the processing is carried out using an electrical discharge machining (EDM) machine. The embedded groove of the ultra-thin irregular rib (2) is electrically machined using standard parameters, which requires roughing, semi-finishing and finishing.
3. The processing technology for ultra-thin irregular-shaped reinforcing bars in an all-steel tire mold according to claim 1, characterized in that, In step 1, the depth and width of the groove around the entire pattern have an error of ≤0.05mm.
4. The processing technology for ultra-thin irregular-shaped ribs in an all-steel tire mold according to claim 1, characterized in that, In step 2, the length of the rib base (3) is increased by 0.2mm.
Citation Information
Patent Citations
Tire mold and manufacturing method thereof
CN105058637A
Machining method of tire mold pattern block
CN111604656A