Anti-crusting vertical continuous graphitization furnace and anti-crusting method
By installing a disturbance device in a vertical continuous graphitization furnace, ash vapor and powdered raw materials are prevented from being tied in the sub-high temperature zone, the problem of hindering gas discharge of the hard shell is solved, and the pressure in the furnace is stable and safe operation is achieved.
Patent Information
- Application Number
- CN202411289858.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
When the existing vertical continuous graphitization furnace produces high-purity graphite, the ash vapor cools down and condenses in the sub-high temperature zone and forms a hard shell layer, which hinders the smooth discharge of impurity evaporating gas, resulting in the increase in the pressure inside the furnace and Risk of safety accidents.
Install a disturbance device, including a mechanical agitation device and an airflow disturbance device, through external forces or airflow disturbance materials in the preheating zone and the sub-high temperature heating zone, to prevent the formation or breakage of the hard shell layer and ensure the smooth discharge of impurities evaporated gas.
It effectively prevents the formation of a hard shell layer, maintains the pressure in the furnace smoothly, avoids material spraying accidents, and ensures the safe operation of the graphitization furnace.
Smart Images

Figure CN119085304A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of graphitization furnaces, and in particular to an anti-crusting vertical continuous graphitization furnace and an anti-crusting method. Background Art
[0002] Carbonaceous raw materials (petroleum coke, needle coke, asphalt, etc.) can be subjected to high temperature (2000-3000°C) heat treatment to perfect their atomic structure and transform them into graphite carbon with a three-dimensional regular and ordered structure of graphite, thereby achieving the purpose of graphitization.
[0003] Graphite has very high melting and boiling points, and its melting point is much higher than the boiling point of the impurities it contains. In the process of high-temperature graphitization, in addition to the lattice transformation of carbon atoms, various impurities also evaporate into gas at high temperatures. With the reduction of impurities and the increase of fixed carbon content, the purity of graphite increases, and its application value also increases.
[0004] The vertical continuous graphitization furnace transmits electricity to the graphitization furnace through graphite electrodes, and uses the resistance of the carbon raw material itself to convert the electrical energy entering the furnace into thermal energy. Its characteristics are continuous production, improved product quality, improved working conditions, controllable waste emissions, energy consumption is reduced by at least 50% compared with the Acheson graphitization furnace, and the temperature in the furnace can exceed 2500℃.
[0005] The common vertical continuous graphitization furnace is divided into four areas from top to bottom: preheating area, sub-high temperature heating area, high temperature heating area and cooling area. The carbon raw material is added from the top feed pipe and is continuously heated to 2500-3000℃ during the entire falling process to achieve high temperature graphitization of the carbon raw material. After the graphitization in the high temperature heating area is completed, the material enters the cooling area at the bottom of the furnace for cooling and discharge. The ash of the carbon raw material is evaporated into gas at a high temperature of more than 2500℃ in the high temperature heating area. Due to the buoyancy, the ash gas will naturally rise, penetrate the sub-high temperature heating area and the preheating area in turn, and then gather at the top of the furnace, and be sucked out of the furnace by the exhaust hole at the top.
[0006] At present, the problem of producing high-purity graphite in vertical continuous graphitization furnace is that the production of high-purity graphite has very high requirements for raw materials, including the impurity content and particle size of the raw materials. In particular, the particle size requirement is very fine (<1mm), which makes the permeability of the material layer in the furnace very poor, and the pressure of the gas evaporated from the high temperature in the furnace continues to rise until it is discharged smoothly.
[0007] The ash vapor evaporated from the high temperature heating zone rises naturally and needs to pass through the secondary high temperature heating zone before it can be discharged. During the penetration process, the high temperature ash vapor will cool down when it encounters the secondary high temperature carbon raw material, condense from gaseous state to solid state, and form a hard shell layer occupying the entire cross section of the furnace in the secondary high temperature area.
[0008] This hard shell layer is very harmful. It prevents the smooth discharge of impurity evaporation gas, causing the gas pressure in the furnace to continue to rise, which can easily make the operating pressure in the furnace too high, resulting in increased equipment investment. Especially when discharging materials at the bottom of the graphitization furnace, the material layer drops as a whole, and the hard shell layer drops with it. Uneven sedimentation will always occur, and the hard shell layer will be damaged by force. High-pressure gas will be suddenly released from the damaged hard shell layer, causing "spraying" to cause material leakage, posing a threat to the safe operation of the graphitization furnace and causing safety accidents.
[0009] In summary, when producing high-purity graphite in the existing vertical continuous graphitization furnace, the ash vapor will be cooled in the sub-high temperature zone and will be agglomerated with the fine powdered raw material to form a hard shell layer occupying the entire furnace cross-section in the sub-high temperature zone, hindering the smooth discharge of impurity evaporation gas. Summary of the invention
[0010] The object of the present invention is to provide an anti-crusting vertical continuous graphitization furnace and an anti-crusting method, so as to solve the technical problem in the prior art that when producing high-purity graphite in the vertical continuous graphitization furnace, ash vapor will be cooled in the sub-high temperature zone and agglomerated with the fine powder raw material to form a hard shell layer occupying the entire cross-section of the furnace in the sub-high temperature zone, thereby hindering the smooth discharge of impurity evaporation gas.
[0011] In order to solve the above technical problems, the present invention specifically provides an anti-crusting vertical continuous graphitization furnace, wherein the inside of the graphitization furnace is composed of a preheating zone, a sub-high temperature heating zone, a high temperature heating zone and a cooling zone from top to bottom;
[0012] The top of the graphitization furnace is provided with an exhaust hole and a feed pipe, and the bottom of the graphitization furnace is provided with a discharge pipe;
[0013] A vertical graphite electrode is arranged in the graphitization furnace, and the bottom end of the graphite electrode is located at the lower edge of the high-temperature heating zone;
[0014] The graphitization furnace is equipped with a disturbance device, which can disturb the materials in the preheating zone and the secondary high temperature heating zone by external force to prevent the formation of a hard shell layer in the preheating zone and the secondary high temperature heating zone.
[0015] As a preferred embodiment of the present invention, the disturbance device is configured as a mechanical stirring device installed in the graphitization furnace, which is used to stir the materials in the preheating zone and the secondary high temperature heating zone to prevent the formation of a hard shell layer or break the formed hard shell layer.
[0016] As a preferred embodiment of the present invention, the mechanical stirring device comprises a stirring component installed in the graphitization furnace and a motor installed outside the graphitization furnace, and the motor is used to drive the stirring component to rotate;
[0017] The stirring components are arranged transversely, and a plurality of stirring components are evenly arranged around the graphite electrode.
[0018] As a preferred solution of the present invention, the motor is installed outside the side wall of the graphitization furnace and is fixedly connected to the stirring component penetrating the side wall of the graphitization furnace through a coupling, and can drive the stirring component to rotate vertically.
[0019] As a preferred solution of the present invention, the motor is installed outside the top plate of the graphitization furnace, and is transmission-connected to the stirring component via a transmission shaft penetrating the top plate of the graphitization furnace, so as to drive the stirring component to rotate laterally.
[0020] As a preferred embodiment of the present invention, the disturbance device includes an air pump and an air inlet pipe running through the graphitization furnace, which can blow inert gas into the graphitization furnace to make the materials in the preheating zone and the secondary high temperature heating zone in a bubbling fluidized state.
[0021] As a preferred solution of the present invention, a plurality of air inlet pipes are vertically and evenly installed at the bottom of the graphitization furnace, and the air outlets of the air inlet pipes are located in the cooling zone.
[0022] As a preferred solution of the present invention, the air inlet pipe is transversely arranged on the interface between the secondary high temperature heating zone and the high temperature heating zone;
[0023] In addition, a plurality of air inlet pipes are evenly arranged around the graphite electrode, and a plurality of air inlet holes are arranged on a side of each air inlet pipe facing the sub-high temperature zone heating zone to allow the inert gas to enter evenly.
[0024] In order to solve the above technical problems, the present invention further provides a method for preventing crusting of a vertical continuous graphitization furnace, using the vertical continuous graphitization furnace, comprising the following steps:
[0025] The disturbance device on the graphitization furnace is started to disturb the materials in the preheating zone and the sub-high temperature heating zone by external force to prevent the formation of a hard shell layer in the preheating zone and the sub-high temperature heating zone.
[0026] As a preferred embodiment of the present invention, the external force disturbance is a mechanical disturbance or an airflow disturbance;
[0027] The mechanical disturbance method is: a mechanical stirring device is installed in the preheating zone and the sub-high temperature heating zone in the graphitization furnace to stir the materials in the preheating zone and the sub-high temperature heating zone to prevent the formation of a hard shell layer or break the hard shell layer that has been formed;
[0028] The method of air flow disturbance is: blowing inert gas into the graphitization furnace through an air pump and an air inlet pipe running through the graphitization furnace, so that the materials in the preheating zone and the secondary high temperature heating zone are in a bubbling fluidized state to prevent the formation of a hard shell layer.
[0029] Compared with the prior art, the present invention has the following beneficial effects:
[0030] During the graphitization process, the disturbance device in the graphitization furnace can disturb the materials in the preheating zone and the secondary high temperature heating zone to prevent the powdered materials in the zone from forming a hard crust layer by agglomerating with the condensed ash. This allows the impurity evaporation gas to be discharged smoothly, stabilizes the operating pressure in the furnace, avoids the material spraying accident caused by the damage of the hard crust layer due to stress, and maintains the safe operation of the graphitization furnace. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. Obviously, the drawings in the following description are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.
[0032] Figure 1 It is a schematic diagram of the structure of the stirring component when it rotates vertically in an embodiment of the present invention;
[0033] Figure 2 It is a schematic diagram of the structure when the stirring component rotates horizontally in an embodiment of the present invention;
[0034] Figure 3 This is a schematic diagram of the structure when the air inlet pipe is located at the bottom of the furnace in an embodiment of the present invention;
[0035] Figure 4 It is a schematic diagram of the structure when the air inlet pipe is located at the furnace side in an embodiment of the present invention;
[0036] Figure 5 for Figure 4 Enlarged schematic diagram of the middle intake pipe.
[0037] The numbers in the figure represent the following:
[0038] 1-graphitizing furnace, 2-preheating zone, 3-secondary high temperature heating zone, 4-high temperature heating zone, 5-cooling zone, 6-exhaust hole, 7-feeding pipe, 8-discharge pipe, 9-graphite electrode, 10-stirring component, 11-drive shaft, 12-intake pipe. DETAILED DESCRIPTION
[0039] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0040] The present invention specifically provides an anti-crusting vertical continuous graphitization furnace, wherein the inside of the graphitization furnace 1 is composed of a preheating zone 2, a sub-high temperature heating zone 3, a high temperature heating zone 4 and a cooling zone 5 from top to bottom;
[0041] The top of the graphitization furnace 1 is provided with an exhaust hole 6 and a feed pipe 7, and the bottom of the graphitization furnace 1 is provided with a discharge pipe 8;
[0042] A vertical graphite electrode 9 is provided in the graphitization furnace 1 for supplying electricity to the graphitization furnace 1. The electrical resistance of the carbon raw material itself is used to convert the electrical energy entering the furnace into thermal energy. The bottom end of the graphite electrode 9 is located at the lower edge of the high-temperature heating zone 4.
[0043] The graphitization furnace 1 is equipped with a disturbance device, which can disturb the materials in the preheating zone 2 and the sub-high temperature heating zone 3 by external force to prevent the formation of a hard shell layer in the preheating zone 2 and the sub-high temperature heating zone 3.
[0044] The working principle of the vertical continuous graphitization furnace is as follows:
[0045] The carbonaceous raw material is added from the top discharge pipe 7, and the discharge rate is controlled by the discharge speed of the bottom discharge pipe 8, thereby controlling the graphitization time of the carbonaceous raw material.
[0046] The carbonaceous raw material falls slowly in the furnace by its own gravity. During the whole falling process, it passes through the preheating zone 2, the sub-high temperature heating zone 3 and the high temperature heating zone 4 in sequence and is continuously heated to 2500-3000°C to realize high temperature graphitization of the carbonaceous raw material.
[0047] In the preheating zone 2 and the secondary high temperature heating zone 3, the carbon raw materials are dried and calcined, and the moisture and volatile gases generated by evaporation naturally rise due to buoyancy and gather at the top of the furnace, and are sucked out of the furnace by the exhaust holes 6 at the top.
[0048] The temperature in the high-temperature heating zone 4 exceeds 2500°C, and the ash of the carbonaceous raw material (containing silicate minerals of potassium, sodium, magnesium, calcium, aluminum, and iron) is evaporated into gas at high temperature. Due to the buoyancy, the ash gas will naturally rise, and penetrate the secondary high-temperature heating zone 3 and the preheating zone 2 in turn, and then gather at the top of the furnace, and be sucked out of the furnace by the exhaust hole 6 at the top.
[0049] After graphitization is completed in the high-temperature heating zone 4, the material enters the furnace bottom cooling zone 5 for cooling and then is discharged.
[0050] During the graphitization process, the disturbance device in the graphitization furnace 1 can disturb the materials in the preheating zone 2 and the secondary high temperature heating zone 3 to prevent the powdered materials in the area from forming a hard crust layer by agglomerating with the condensed ash. This allows the impurity evaporation gas to be discharged smoothly, stabilizes the operating pressure in the furnace, avoids the material spraying accident caused by the damage of the hard crust layer due to stress, and maintains the safe operation of the graphitization furnace 1.
[0051] The disturbance device can be configured as a mechanical disturbance, an air flow disturbance or other forms.
[0052] The method of directly disturbing the materials in the preheating zone 2 and the sub-high temperature heating zone 3 by mechanical means is as follows:
[0053] The mechanical stirring device is installed in the graphitization furnace 1 to stir the materials in the preheating zone 2 and the secondary high temperature heating zone 3 to prevent the formation of a hard shell layer or to break the hard shell layer that has been formed.
[0054] Furthermore, the mechanical stirring device includes a stirring component 10 installed in the graphitization furnace 1 and a motor installed outside the graphitization furnace 1, and the motor is used to drive the stirring component 10 to rotate;
[0055] In order to achieve a better anti-crusting effect, the stirring member 10 is arranged horizontally, and a plurality of stirring members 10 are evenly arranged around the graphite electrode 9 .
[0056] Furthermore, the transmission shaft 11 of the mechanical stirring device can pass through the side wall of the graphitization furnace 1 and go out of the furnace, as follows:
[0057] The motor is installed outside the side wall of the graphitization furnace 1 and is fixedly connected to the stirring component 10 penetrating the side wall of the graphitization furnace 1 through a coupling, and can drive the stirring component 10 to rotate vertically.
[0058] It is also possible to pass through the top of the graphitization furnace 1 and exit the furnace, as follows:
[0059] The motor is installed outside the top plate of the graphitization furnace 1 and is connected to the stirring component 10 through a transmission shaft 11 that penetrates the top plate of the graphitization furnace 1 , so as to drive the stirring component 10 to rotate horizontally.
[0060] The method of disturbing the materials in the preheating zone 2 and the sub-high temperature heating zone 3 by air flow is as follows:
[0061] The disturbance device includes an air pump and an air inlet pipe 12 that runs through the graphitization furnace 1, and can blow inert gas into the graphitization furnace 1 to make the materials in the preheating zone 2 and the secondary high temperature heating zone 3 in a bubbling fluidized state.
[0062] Air flow disturbance can be blown in from the bottom of the furnace as follows:
[0063] A plurality of air inlet pipes 12 are vertically and evenly installed at the bottom of the graphitization furnace 1 , and the air outlets of the air inlet pipes 12 are located in the cooling zone 5 .
[0064] When blowing from the bottom, the blowing flow rate should be well controlled to make the materials in the upper medium and low temperature heating zones produce bubbling and fluidization to prevent crusting. Fluidization should not be caused in the high temperature area and cooling zone, otherwise it will affect the temperature field distribution in the furnace and the conductive properties of the materials.
[0065] The gas blown in from the bottom can also be used to cool the high-temperature graphite products in the cooling zone 5. After preheating, it passes through the high-temperature zone and enters the medium and low-temperature zones as fluidizing air. The preheating process of the cooling zone 5 avoids the inert gas from affecting the high-temperature environment of the high-temperature zone.
[0066] Air flow disturbance can also be blown in from the side of the furnace, as follows:
[0067] The air inlet pipe 12 is transversely arranged on the interface between the sub-high temperature heating zone 3 and the high temperature heating zone 4. At this time, the airflow does not pass through the high temperature heating zone 4 and the cooling zone 5, so it does not affect the high temperature zone and the cooling zone 5.
[0068] In addition, a plurality of air inlet pipes 12 are evenly arranged around the graphite electrode 9 , and a plurality of air inlet holes are arranged on a side of each air inlet pipe 12 facing the sub-high temperature zone heating zone to allow the inert gas to enter evenly.
[0069] In order to solve the above technical problems, the present invention further provides a method for preventing crusting of a vertical continuous graphitization furnace, using the vertical continuous graphitization furnace, comprising the following steps:
[0070] The disturbance device on the graphitization furnace 1 is started to disturb the materials in the preheating zone 2 and the sub-high temperature heating zone 3 by external force to prevent the formation of a hard shell layer in the preheating zone 2 and the sub-high temperature heating zone 3.
[0071] Furthermore, the external force disturbance is a mechanical disturbance or an air flow disturbance;
[0072] The mechanical disturbance method is: a mechanical stirring device is installed in the preheating zone 2 and the sub-high temperature heating zone 3 in the graphitization furnace 1 to stir the materials in the preheating zone 2 and the sub-high temperature heating zone 3 to prevent the formation of a hard shell layer or break the hard shell layer that has been formed;
[0073] The method of air flow disturbance is: blowing inert gas into the graphitization furnace 1 through an air pump and an air inlet pipe 12 that runs through the graphitization furnace 1, so that the materials in the preheating zone 2 and the secondary high temperature heating zone 3 are in a bubbling fluidized state to prevent the formation of a hard shell layer.
[0074] The above embodiments are only exemplary embodiments of the present application and are not intended to limit the present application. The protection scope of the present application is defined by the claims. Those skilled in the art may make various modifications or equivalent substitutions to the present application within the essence and protection scope of the present application, and such modifications or equivalent substitutions shall also be deemed to fall within the protection scope of the present application.
Claims
1. A vertical continuous graphitization furnace for preventing encrustation, characterized in that: The inside of the graphitization furnace (1) is composed of a preheating zone (2), a secondary high temperature heating zone (3), a high temperature heating zone (4) and a cooling zone (5) from top to bottom; The top of the graphitization furnace (1) is provided with an exhaust hole (6) and a feed pipe (7), and the bottom of the graphitization furnace (1) is provided with a discharge pipe (8); A vertical graphite electrode (9) is arranged in the graphitization furnace (1), and the bottom end of the graphite electrode (9) is located at the lower edge of the high-temperature heating zone (4); The graphitization furnace (1) is provided with a disturbance device, which can disturb the materials in the preheating zone (2) and the secondary high temperature heating zone (3) by external force, so as to prevent the formation of a hard shell layer in the preheating zone (2) and the secondary high temperature heating zone (3).
2. The anti-crusting vertical continuous graphitization furnace according to claim 1, characterized in that: The disturbance device is configured as a mechanical stirring device installed in the graphitization furnace (1), and is used to stir the materials in the preheating zone (2) and the secondary high temperature heating zone (3) to prevent the formation of a hard shell layer or to break an already formed hard shell layer.
3. The anti-crusting vertical continuous graphitization furnace according to claim 2, characterized in that: The mechanical stirring device comprises a stirring component (10) installed in the graphitization furnace (1) and a motor installed outside the graphitization furnace (1), wherein the motor is used to drive the stirring component (10) to rotate; The stirring member (10) is arranged transversely, and a plurality of the stirring members (10) are evenly arranged around the graphite electrode (9).
4. The anti-crusting vertical continuous graphitization furnace according to claim 3, characterized in that: The motor is mounted outside the side wall of the graphitization furnace (1) and is fixedly connected to a stirring component (10) penetrating the side wall of the graphitization furnace (1) via a coupling, and is capable of driving the stirring component (10) to rotate vertically.
5. The anti-crusting vertical continuous graphitization furnace according to claim 3, characterized in that: The motor is mounted outside the top plate of the graphitization furnace (1) and is transmission-connected to the stirring component (10) via a transmission shaft (11) penetrating the top plate of the graphitization furnace (1), so as to be capable of driving the stirring component (10) to rotate horizontally.
6. The anti-crusting vertical continuous graphitization furnace according to claim 1, characterized in that: The disturbance device comprises an air pump and an air inlet pipe (12) passing through the graphitization furnace (1), and is capable of blowing inert gas into the graphitization furnace (1) so that the materials in the preheating zone (2) and the secondary high temperature heating zone (3) are in a bubbling fluidized state.
7. The anti-crusting vertical continuous graphitization furnace according to claim 6, characterized in that: A plurality of air inlet pipes (12) are evenly and vertically installed at the bottom of the graphitization furnace (1), and the air outlets of the air inlet pipes (12) are located in the cooling zone (5).
8. The anti-crusting vertical continuous graphitization furnace according to claim 6, characterized in that: The air inlet pipe (12) is transversely arranged on the interface between the secondary high temperature heating zone (3) and the high temperature heating zone (4); Furthermore, a plurality of air inlet pipes (12) are evenly arranged around the graphite electrode (9), and a plurality of air inlet holes are arranged on a side of each air inlet pipe (12) facing the secondary high temperature zone heating zone, so that the inert gas can enter evenly.
9. A method for preventing crusting in a vertical continuous graphitization furnace, characterized in that: Using the vertical continuous graphitization furnace according to any one of claims 1 to 8 comprises the following steps: The disturbance device on the graphitization furnace (1) is started to disturb the materials in the preheating zone (2) and the secondary high temperature heating zone (3) by external force, so as to prevent the formation of a hard shell layer in the preheating zone (2) and the secondary high temperature heating zone (3).
10. The method for preventing crusting of a vertical continuous graphitization furnace according to claim 9, characterized in that: External disturbance is mechanical disturbance or air flow disturbance; The mechanical disturbance method comprises: installing a mechanical stirring device in the preheating zone (2) and the sub-high temperature heating zone (3) in the graphitization furnace (1) to stir the materials in the preheating zone (2) and the sub-high temperature heating zone (3) to prevent the formation of a hard shell layer or to break the hard shell layer that has been formed; The method for disturbing the air flow is as follows: an inert gas is blown into the graphitization furnace (1) through an air pump and an air inlet pipe (12) penetrating the graphitization furnace (1), so that the materials in the preheating zone (2) and the secondary high temperature heating zone (3) are in a bubbling fluidized state, so as to prevent the formation of a hard shell layer.
Citation Information
Patent Citations
Graphitization furnace for negative electrode material production
CN112524956A
Electric furnace combining electromagnetic induction and electric arc heating and using method thereof
CN116839353A
Anti-crusting vertical continuous graphitization furnace and anti-crusting method
CN119394002A
Electric forge furnace
CN203083376U
Heating and blowing electric arc furnace
CN214371650U
Cited By
Waste lithium battery graphite negative electrode material recovery system
CN224650254U