Battery cells and electronic devices
By introducing support components and heat-absorbing or flame-retardant components in the cell, the deformation problem caused by electrode expansion during the cycling process of wound cells is solved, thereby improving the safety performance and thermal management capability of the cell.
Patent Information
- Application Number
- CN202411976914.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-30
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2044-12-30
AI Technical Summary
During cycling, the expansion of the electrode sheets in wound cells causes deformation of the core, leading to poor battery interface and reduced cell safety performance.
The support structure includes an outer shell and multiple reinforcing members. The outer shell is fitted to the wall of the winding center hole. The multiple reinforcing members are spaced apart to form sub-cavities. The sub-cavities are equipped with heat-absorbing or flame-retardant members. The heat-absorbing members are used for cooling and heat dissipation, and the flame-retardant members are used to suppress cell combustion.
Improve the structural strength and safety performance of the battery cell, reduce the risk of electrode deformation, and enhance the thermal management and fire resistance of the battery cell.
Smart Images

Figure CN119650884B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of energy storage technology, and in particular to a battery cell and electronic device. Background Technology
[0002] During cycling, wound battery cells can deform due to electrode expansion. This deformation can lead to poor battery interface performance and reduce the cell's safety. Summary of the Invention
[0003] In view of the above situation, this application provides a battery cell that is beneficial to improving the safety performance of the battery cell.
[0004] Embodiments of this application provide a battery cell, which includes an electrode assembly and a support member. The electrode assembly includes a first electrode, a second electrode, and a separator, with the separator disposed between the first and second electrodes. The electrode assembly has a winding central hole. The first electrode, the separator, and the second electrode are wound around the winding central hole. The support member is disposed in the winding central hole. The support member includes a housing and a plurality of reinforcing members. The housing has a receiving cavity, and at least a portion of the outer surface of the housing is fitted against the wall of the winding central hole. The plurality of reinforcing members are connected to the inner surface of the housing, and the plurality of reinforcing members are spaced apart and divide the receiving cavity into a plurality of sub-cavities. At least one sub-cavity contains a heat-absorbing element or a flame-retardant element.
[0005] In the aforementioned battery cell, the spaced reinforcements enhance the structural strength of the outer casing. The casing fits snugly against the wall of the central winding hole to support the electrode assembly, reducing the risk of electrode assembly deformation and thus improving the cell's safety performance. At least one sub-cavity contains a heat-absorbing or flame-retardant component. The heat-absorbing component is configured to cool or dissipate heat inside the electrode assembly, while the flame-retardant component is configured to suppress cell combustion in the event of thermal runaway, thereby improving the cell's safety performance.
[0006] In some embodiments of this application, along the winding direction of the electrode assembly, the separator includes a first starting segment extending beyond the starting ends of the first and second electrodes. The first starting segment is wound around the support at least one turn to improve the tightness of the fit between the housing and the wall of the winding center hole.
[0007] In some embodiments of this application, the outer shell includes two planar regions and two arcuate regions. The two planar regions are spaced apart along a first direction, and the two arcuate regions are spaced apart along a second direction and respectively connected to the two ends of the two planar regions. The two planar regions and the two arcuate regions enclose a receiving cavity. The first direction is perpendicular to the second direction. Reinforcing members connect the two planar regions, and multiple reinforcing members are arranged along the second direction. Sub-cavities are formed between two adjacent reinforcing members or between an arcuate region and a reinforcing member adjacent to the arcuate region.
[0008] In some embodiments of this application, the radius of the arc corresponding to the arc surface area is R1, 1mm≤R1≤3mm, so that the arc surface area matches the bending curvature at the corner of the electrode assembly, thereby improving the stability of the arc surface area supporting the corner of the electrode assembly, reducing the risk of electrode assembly deformation, and thus improving the safety performance of the battery cell.
[0009] In some embodiments of this application, along the second direction, the distance between two adjacent reinforcing members is W1, 10mm≤W1≤20mm, so that the space of the sub-cavity can accommodate the heat-absorbing member or the flame-retardant member, and can improve the support stability of the shell on the electrode assembly.
[0010] In some embodiments of this application, the thickness of the planar region is T1, where 0.3mm≤T1≤2mm, to improve the support stability of the planar region for the electrode assembly and to increase the energy density of the battery cell.
[0011] In some embodiments of this application, the thickness of the arc-shaped region is T2, where 0.3mm≤T2≤2mm, in order to improve the support stability of the arc-shaped region for the electrode assembly and to increase the energy density of the battery cell.
[0012] In some embodiments of this application, sub-cavities with heat-absorbing elements and sub-cavities with flame-retardant elements are arranged alternately to improve the balance between heat absorption capacity and flame-retardant capacity.
[0013] In some embodiments of this application, the heat-absorbing element is made of paraffin wax. Paraffin wax has a wide phase change temperature range, and the phase change temperature of the heat-absorbing element can be adjusted by regulating the content and type of paraffin wax in the heat-absorbing element. Paraffin wax has a high latent heat of phase change, enabling it to store a large amount of heat. Paraffin wax has good chemical stability, allowing it to repeatedly undergo endothermic and exothermic phase changes, resulting in low leakage risk and high safety. Furthermore, paraffin wax has viscosity, facilitating contact with the inner wall of the cavity.
[0014] In some embodiments of this application, the flame-retardant component includes a housing and a flame retardant. The housing has a receiving cavity, and the flame retardant is disposed within the receiving cavity. The melting point of the housing is 100°C to 130°C. When the temperature inside the battery cell reaches the melting point of the housing, the housing melts, and the flame retardant is released, dissolved, and dispersed inside the battery cell to suppress battery cell combustion in the event of thermal runaway. The housing seals the flame retardant inside the battery cell before the melting point of the housing is reached, reducing the risk that the flame retardant will affect the normal use of the battery cell.
[0015] In some embodiments of this application, the shell material includes polymethyl methacrylate, and the shell accounts for 3% to 10% of the weight of the flame retardant component, so as to facilitate the encapsulation of the flame retardant by the shell and to improve the flame retardant effect.
[0016] In some embodiments of this application, the flame retardant material includes at least one of alkyl phosphate esters, fluoroalkyl phosphate esters, aromatic phosphate esters, fluorinated flame retardants, and carbonates to enhance the flame retardant effect.
[0017] In some embodiments of this application, the material of the support includes at least one of aluminum, nickel, copper, and ceramic, in order to improve the structural strength of the support and facilitate the outer shell to act as a heat conductor between the heat absorber and the electrode assembly for heat conduction.
[0018] Embodiments of this application also provide an electronic device, which includes any of the battery cells described in the above embodiments.
[0019] In the aforementioned battery cell and electronic device, the spaced arrangement of multiple reinforcing members enhances the structural strength of the casing. The casing fits snugly against the wall of the central winding hole to support the electrode assembly, reducing the risk of electrode assembly deformation and thus improving the safety performance of the battery cell. At least one sub-cavity contains a heat-absorbing element or a flame-retardant element. The heat-absorbing element is configured to cool or dissipate heat inside the electrode assembly, while the flame-retardant element is configured to suppress battery cell combustion in the event of thermal runaway, thereby improving the battery cell's safety performance. Attached Figure Description
[0020] Figure 1 This is a schematic diagram of the battery cell structure in one embodiment of this application.
[0021] Figure 2 This is a schematic diagram of the assembly of the electrode components and support components of the battery cell in one embodiment of this application.
[0022] Figure 3 This is a schematic diagram of the structure of the support member of the battery cell in one embodiment of this application, with heat-absorbing and flame-retardant members filling the corresponding sub-cavities.
[0023] Figure 4 This is a schematic diagram of the structure of the support member of the battery cell in another embodiment of this application, wherein heat-absorbing and flame-retardant elements are coated on the cavity walls of the corresponding sub-cavities.
[0024] Figure 5 This is a schematic diagram of the structure of an electronic device in one embodiment of this application.
[0025] Explanation of main component symbols 100 cells Electronic devices 200 Electrode assembly 10 10A winding center hole First Polar Film 11 First son, Ji'er 111 Second electrode 12 Second son, Ji'er 121 Separator 13 First starting section 131 Support component 20 Casing 21 Receiving cavity 21A Subcavity 21A1 Opening 21B Sub-opening 21B1 First gap 21C Second gap 21D Planar area 211 Curved area 212 Heat absorption element 30 Flame retardant parts 40 Packaging bag 50 Main body 51 Top Wall 511 Bottom wall 512 Top sealing section 52 First Pole Ear 60 Second pole ear 70 First direction X Second direction Y Axial Z The following detailed description, in conjunction with the accompanying drawings, will further illustrate this application. Detailed Implementation
[0026] The technical solutions of the embodiments of this application will be described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, and not all embodiments.
[0027] It should be noted that when a component is considered to be "connected" to another component, it can be directly connected to the other component or may also have a component that is centrally located. When a component is considered to be "set" on another component, it can be directly set on the other component or may also have a component that is centrally located.
[0028] When a value is considered "equal" to another value, it means that the two values are equal within a set deviation range, which is within 5%. In other words, if at least one of the two values fluctuates within the set deviation range, they are considered approximately equal even if their values are not equal. Similarly, when a value is considered to have a "1:1" ratio with another value, it means that the two values are equal within a set deviation range, which is within 5%. Again, if at least one of the two values fluctuates within the set deviation range, they are considered equal in ratio even if their values are not equal.
[0029] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein in the specification of this application is for the purpose of describing particular embodiments only and is not intended to be limiting of the application. The term "and / or" as used herein includes any and all combinations of one or more of the associated listed items. The term "overlap" as used herein refers to the overlapping of the projected portions of two components or the coincidence of the projected portions of two components.
[0030] This application provides a battery cell, which includes an electrode assembly and a support member. The electrode assembly includes a first electrode, a second electrode, and a separator, with the separator disposed between the first and second electrodes. The electrode assembly has a winding central hole. The first electrode, the separator, and the second electrode are wound around the winding central hole. The support member is disposed in the winding central hole. The support member includes a housing and a plurality of reinforcing members. The housing has a receiving cavity, and at least a portion of the outer surface of the housing is fitted against the wall of the winding central hole. The plurality of reinforcing members are connected to the inner surface of the housing, and the plurality of reinforcing members are spaced apart and divide the receiving cavity into a plurality of sub-cavities. At least one sub-cavity contains a heat-absorbing element or a flame-retardant element.
[0031] In the aforementioned battery cell, the spaced reinforcements enhance the structural strength of the outer casing. The casing fits snugly against the wall of the central winding hole to support the electrode assembly, reducing the risk of electrode assembly deformation and thus improving the cell's safety performance. At least one sub-cavity contains a heat-absorbing or flame-retardant component. The heat-absorbing component is configured to cool or dissipate heat inside the electrode assembly, while the flame-retardant component is configured to suppress cell combustion in the event of thermal runaway, thereby improving the cell's safety performance.
[0032] The embodiments of this application will be further described below with reference to the accompanying drawings.
[0033] Please refer to the following: Figure 1 and Figure 2 One embodiment of this application provides a battery cell 100, which can be used again after being discharged by recharging to activate the active material.
[0034] The battery cell 100 includes an electrode assembly 10 and a support member 20. The electrode assembly 10 is used to convert chemical energy into electrical energy. The electrode assembly 10 includes a first electrode 11, a second electrode 12, and a separator 13 disposed between the first electrode 11 and the second electrode 12. The polarity of the first electrode 11 is opposite to that of the second electrode 12.
[0035] The electrode assembly 10 has a winding center hole 10A. A first electrode 11, a separator 13, and a second electrode 12 are wound around the winding center hole 10A. Specifically, the separator 13, the first electrode 11, the separator 13, and the second electrode 12 are wound around the winding center hole 10A, or the first electrode 11, the separator 13, the second electrode 12, and the separator 13 are wound around the winding center hole 10A. There are two possible winding directions: clockwise and counterclockwise. This application uses counterclockwise winding as an example for explanation.
[0036] A support member 20 is disposed in the winding center hole 10A. The support member 20 includes a housing 21 and a plurality of reinforcing members 22. The housing 21 has a receiving cavity 21A, and at least a portion of the outer surface of the housing 21 is in contact with the hole wall of the winding center hole 10A. The plurality of reinforcing members 22 are connected to the inner surface of the housing 21, and the plurality of reinforcing members 22 are spaced apart and divide the receiving cavity 21A into a plurality of sub-cavities 21A1. The spaced arrangement of the plurality of reinforcing members 22 can improve the structural strength of the housing 21. The contact between the housing 21 and the hole wall of the winding center hole 10A can provide support for the electrode assembly 10, reduce the risk of deformation of the electrode assembly 10, and thus improve the safety performance of the battery cell 100.
[0037] Please refer to the following: Figure 2 and Figure 3 At least one sub-cavity 21A1 is provided with a heat-absorbing element 30 or a flame-retardant element 40. The heat-absorbing element 30 is configured to cool or dissipate heat inside the electrode assembly 10, and the flame-retardant element 40 is configured to suppress the combustion of the battery cell 100 in the event of thermal runaway, so as to improve the safety performance of the battery cell 100.
[0038] Please see Figure 3 In some embodiments, the heat-absorbing element 30 fills the sub-cavity 21A1 to improve the cooling or heat dissipation effect. Specifically, when viewed along the Z-axis, there are no gaps in the sub-cavity 21A1 where the heat-absorbing element 30 is located.
[0039] Please see Figure 4 In some embodiments, the heat absorber 30 is coated on the inner wall of the sub-cavity 21A1 to improve the connection stability between the heat absorber 30 and the sub-cavity 21A1. Specifically, when viewed along the Z-axis, a gap is provided in the middle of the sub-cavity 21A1 where the heat absorber 30 is provided.
[0040] Please refer to it again. Figure 3 In some embodiments, the flame-retardant element 40 is filled within the sub-cavity 21A1 to enhance the flame-retardant effect. Specifically, when viewed along the Z-axis, the sub-cavity 21A1 with the flame-retardant element 40 has no gaps.
[0041] Please refer to it again. Figure 4In some embodiments, the flame retardant 40 is coated on the inner wall of the sub-cavity 21A1 to improve the connection stability between the flame retardant 40 and the sub-cavity 21A1. Specifically, when viewed along the Z-axis, a gap is provided in the middle of the sub-cavity 21A1 where the flame retardant 40 is provided.
[0042] Please continue reading. Figure 1 and Figure 2 In some embodiments, along the axial direction Z of the winding central hole 10A, the two ends of the outer shell 21 are respectively provided with openings 21B communicating with the receiving cavity 21A. Correspondingly, each opening 21B includes a plurality of sub-openings 21B1, and each sub-opening 21B1 communicates with a sub-cavity 21A1.
[0043] The battery cell 100 includes a packaging bag 50, a first tab 60, and a second tab 70. The packaging bag 50 includes a main body 51 and a top sealing portion 52, and the electrode assembly 10 is housed in the main body 51. The main body 51 includes a top wall 511 and a bottom wall 512 disposed opposite each other along the Z-axis. The top sealing portion 52 is connected to the top wall 511. The first tab 60 is connected to the first electrode 11 and extends from the top sealing portion 52, and the second tab 70 is connected to the second electrode 12 and extends from the top sealing portion 52.
[0044] Along the axial direction Z, the top wall 511 and the bottom wall 512 are respectively disposed on one side of the two openings 21B of the sub-cavity 21A1 to restrict the position of the heat-absorbing element 30 or the flame-retardant element 40 in the corresponding sub-cavity 21A1.
[0045] Please continue reading. Figure 1 and Figure 2 In some embodiments, along the axial direction Z, the edge of the first electrode 11 near the top wall 511 is located outside the edge of the second electrode 12 near the top wall 511, and the end of the housing 21 with the opening 21B is located between the edges of the first electrode 11 and the second electrode 12 near the top wall 511. Firstly, this improves the stability of the housing 21 in supporting the first electrode 11 and the second electrode 12. Secondly, it allows a first gap 21C to be formed between the end of the housing 21 with the opening 21B and the top wall 511. The first gap 21C is used to release, dissolve, and disperse the flame retardant 40 into the interior of the battery cell 100 when the internal temperature of the battery cell 100 reaches a preset temperature.
[0046] In some embodiments, along the axial direction Z, the edge of the first electrode 11 near the bottom wall 512 is located outside the edge of the second electrode 12 near the bottom wall 512, and one end of the housing 21 with another opening 21B is located between the edges of the first electrode 11 and the second electrode 12 near the bottom wall 512. Firstly, this improves the stability of the housing 21 in supporting the first electrode 11 and the second electrode 12. Secondly, it allows a second gap 21D to be formed between the end of the housing 21 with the other opening 21B and the bottom wall 512. The second gap 21D is used to release and dissolve the flame retardant 40 into the interior of the battery cell 100 when the internal temperature of the battery cell 100 reaches a preset temperature.
[0047] Please continue reading. Figure 2 In some embodiments, along the winding direction of the electrode assembly 10, the separator 13 includes a first starting segment 131 extending beyond the starting end of the first electrode 11 and the starting end of the second electrode 12. The first starting segment 131 is wound around the support 20 at least one turn, forming the wall of the winding central hole 10A. The first starting segment 131 is wound around the support 20 at least one turn to improve the tightness of the fit between the housing 21 and the wall of the winding central hole 10A.
[0048] Optionally, the number of turns of the first starting segment 131 around the support member 20 is one of 1, 1.5, 2, 2.5, 3, or any other value greater than 1.
[0049] Please refer to 3. In some embodiments, the outer shell 21 includes two planar regions 211 and two arcuate regions 212. When viewed along the axial direction Z, the two planar regions 211 are spaced apart along the first direction X, and the two arcuate regions 212 are spaced apart along the second direction Y and are respectively connected to the two ends of the two planar regions 211. The two planar regions 211 and the two arcuate regions 212 enclose a receiving cavity 21A. The first direction X is perpendicular to the second direction Y.
[0050] The reinforcing member 22 connects two planar regions 211. Multiple reinforcing members 22 are arranged along the second direction Y. The sub-cavity 21A1 is formed between two adjacent reinforcing members 22 or between the arc surface region 212 and the reinforcing member 22 adjacent to the arc surface region 212.
[0051] Optionally, the multiple reinforcing members 22 are arranged at equal intervals along the second direction Y so that the pressure on the housing 21 is evenly distributed to the multiple reinforcing members 22 when it is subjected to the pressure of the electrode assembly 10, which is beneficial to improving the structural strength of the housing 21.
[0052] In some embodiments, the number of reinforcing members 22 is 5, and the 5 reinforcing members 22 divide the receiving cavity 21A into 6 sub-cavities 21A1, wherein 4 sub-cavities 21A1 are formed between two adjacent reinforcing members 22, and 2 sub-cavities 21A1 are formed between the arcuate region 212 and the reinforcing member 22 adjacent to the arcuate region 212.
[0053] Optionally, the number of reinforcing members 22 can also be any one of other positive integers such as 1, 2, 3, 4, 6, etc.
[0054] Please refer to the following: Figure 1 and Figure 2 In some embodiments, the first electrode 11 has multiple first sub-electrode tabs 111 on the side facing the top wall 511. The first sub-electrode tabs 111 are bundled together and connected to the first electrode tab 60. The second electrode 12 has multiple second sub-electrode tabs 121 on the side facing the top wall 511. The second sub-electrode tabs 121 are bundled together and connected to the second electrode tab 70. Viewed along the Z-axis, the portion of the first electrode 11 with the first sub-electrode tabs 111 overlaps with the planar region 211, and the portion of the second electrode 12 with the second sub-electrode tabs 121 overlaps with the planar region 211. This allows the planar region 211 to support the portions of the first electrode 11 with the first sub-electrode tabs 111 and the portions of the second electrode 12 with the second sub-electrode tabs 121, reducing the risk of deformation of the electrode assembly 10 when the first electrode tab 60 and the second electrode tab 70 are subjected to external force, thereby improving the safety performance of the battery cell 100.
[0055] Please continue reading. Figure 3 In some embodiments, the radius of the arc corresponding to the arc surface area 212 is R1, 1mm≤R1≤3mm, so that the arc surface area 212 is adapted to the bending arc at the corner of the electrode assembly 10, thereby improving the stability of the arc surface area 212 in supporting the corner of the electrode assembly 10, reducing the risk of deformation of the electrode assembly 10, and thus improving the safety performance of the battery cell 100.
[0056] Optionally, R1 can be any value within the range of 1mm, 1.5mm, 2mm, 2.5mm, 3mm, and any other value within the range of 1mm≤R1≤3mm.
[0057] Please continue reading. Figure 3In some embodiments, along the second direction Y, the distance between two adjacent reinforcing members 22 is W1, where 10mm ≤ W1 ≤ 20mm. When W1 is too small (less than 10mm), the space of the sub-cavity 21A1 is too small to accommodate the heat-absorbing member 30 or the flame-retardant member 40; when W1 is too large (greater than 20mm), the span of the planar area 211 is too long, which can easily form a weak area, resulting in a decrease in the support stability of the outer shell 21 for the electrode assembly 10. By limiting W1 to 20mm, the space of the sub-cavity 21A1 can accommodate the heat-absorbing member 30 or the flame-retardant member 40, and the support stability of the outer shell 21 for the electrode assembly 10 can be improved.
[0058] Optionally, W1 can be any value within the range of 10mm, 11mm, 12mm, 13mm, 14mm, 15mm, 16mm, 17mm, 18mm, 19mm, 20mm, and any other value within the range of 10mm≤W1≤20mm.
[0059] Please continue reading. Figure 3 In some embodiments, the thickness of the planar region 211 is T1, where 0.3mm ≤ T1 ≤ 2mm. When T1 is too small (less than 0.3mm), the structural strength of the planar region 211 is weak, resulting in reduced stability of the planar region 211 in supporting the electrode assembly 10. When T1 is too large (greater than 2mm), the space occupied by the outer casing 21 in the first direction X is large, resulting in wasted space and reduced energy density of the cell 100. By limiting the thickness to 0.3mm ≤ T1 ≤ 2mm, the stability of the planar region 211 in supporting the electrode assembly 10 is improved, and the energy density of the cell 100 is also increased.
[0060] Optionally, T1 can be any value within the range of 0.3mm, 0.4mm, 0.5mm, 0.6mm, 0.7mm, 0.8mm, 0.9mm, 1mm, 1.1mm, 1.2mm, 1.3mm, 1.4mm, 1.5mm, 1.6mm, 1.7mm, 1.8mm, 1.9mm, 2mm, or any other value within the range of 0.3mm≤T1≤2mm.
[0061] Please continue reading. Figure 3 In some embodiments, the thickness of the arc-shaped region 212 is T2, where 0.3mm ≤ T2 ≤ 2mm. When T2 is too small (less than 0.3mm), the structural strength of the arc-shaped region 212 is weak, resulting in reduced stability of the arc-shaped region 212 in supporting the electrode assembly 10. When T2 is too large (greater than 2mm), the space occupied by the outer casing 21 in the second direction Y is large, resulting in wasted space and reduced energy density of the battery cell 100. By limiting the thickness to 0.3mm ≤ T2 ≤ 2mm, the stability of the arc-shaped region 212 in supporting the electrode assembly 10 is improved, and the energy density of the battery cell 100 is also increased.
[0062] Optionally, T2 can be any value within the range of 0.3mm, 0.4mm, 0.5mm, 0.6mm, 0.7mm, 0.8mm, 0.9mm, 1mm, 1.1mm, 1.2mm, 1.3mm, 1.4mm, 1.5mm, 1.6mm, 1.7mm, 1.8mm, 1.9mm, 2mm, or any other value within the range of 0.3mm≤T2≤2mm.
[0063] In some embodiments, T1 = T2, so that the force on the periphery of the housing 21 is uniform.
[0064] In some embodiments, T1 > T2, in order to specifically improve the structural strength of the planar region 211, so as to be suitable for scenarios where the planar region 211 is more susceptible to external impact than the curved region 212.
[0065] In some embodiments, T1 < T2, in order to specifically improve the structural strength of the curved surface region 212, so as to be suitable for scenarios where the curved surface region 212 is more susceptible to external impact than the flat surface region 211.
[0066] Please continue reading. Figure 3 In some embodiments, the sub-cavities 21A1 with heat-absorbing elements 30 and the sub-cavities 21A1 with flame-retardant elements 40 are arranged alternately to improve the balance between heat absorption capacity and flame-retardant capacity.
[0067] Please continue reading. Figure 3 In some embodiments, the heat absorber 30 has a phase change temperature. The heat absorber 30 is configured to generate a phase change and absorb heat when the temperature rises to the phase change temperature, thereby reducing the internal temperature of the battery cell 100 and keeping the electrode assembly 10 within a suitable temperature range, which is beneficial to improving the safety of the battery cell 100. Furthermore, the heat absorber 30 is located in the sub-cavity 21A1 and does not occupy additional space within the battery cell 100, which is beneficial to improving the energy density of the battery cell 100.
[0068] When the temperature inside the cell 100 drops below the phase change temperature of the heat absorber 30, the heat absorber 30 stops absorbing heat and undergoes a reverse phase change, i.e., a phase change that releases heat. In this way, the heat absorber 30 can repeatedly undergo phase changes and reverse phase changes during the cycling process of the cell 100.
[0069] It is understandable that the outer casing 21 can act as a heat conductor to conduct heat between the heat absorber 30 and the electrode assembly 10.
[0070] Optionally, the heat absorber 30 may be made of paraffin wax. Paraffin wax has a wide phase change temperature range, and the phase change temperature of the heat absorber 30 can be adjusted by regulating the content and type of paraffin wax in the heat absorber 30. Paraffin wax has a high latent heat of phase change, enabling it to store a large amount of heat. Paraffin wax has good chemical stability, allowing it to repeatedly undergo endothermic and exothermic phase changes, resulting in low leakage risk and high safety. Furthermore, paraffin wax has viscosity, facilitating contact with the inner wall of the sub-cavity 21A1.
[0071] Please continue reading. Figure 3 In some embodiments, the flame retardant 40 includes a housing and a flame retardant. The housing has a receiving cavity in which the flame retardant is disposed. The melting point of the housing is 100°C to 130°C. When the temperature inside the battery cell 100 reaches the melting point of the housing, the housing melts, and the flame retardant is released, dissolved, and dispersed inside the battery cell 100 to suppress combustion of the battery cell 100 in the event of thermal runaway. The housing seals the flame retardant inside the battery cell 100 before the melting point of the housing is reached, reducing the risk that the flame retardant will affect the normal use of the battery cell 100.
[0072] Optionally, the melting point of the shell is one of 100°C, 105°C, 110°C, 115°C, 120°C, 125°C, 130°C, or any other value in the range of 100°C to 130°C.
[0073] In some embodiments, the material of the housing includes polymethyl methacrylate, and the weight percentage of the housing in the flame retardant 40 is 3% to 10%, so as to facilitate the encapsulation of the flame retardant and to improve the flame retardant effect.
[0074] Optionally, the shell is hollow granular, and the specific shape of the granules can be spherical or polyhedral.
[0075] Optionally, the flame retardant material includes at least one of alkyl phosphates, fluoroalkyl phosphates, aromatic phosphates, fluorinated flame retardants, and carbonates to enhance the flame retardant effect.
[0076] Specifically, alkyl phosphates include at least one of trimethyl phosphate (TMP) and triethyl phosphate (TEP). Fluorinated alkyl phosphates include at least one of tri-(2,2,2-trifluoroethyl) phosphate (TFP), di-(2,2,2-trifluoroethyl)-methyl phosphate (BMP), and (2,2,2-trifluoroethyl)-diethyl phosphate (TDP). Aromatic phosphates include at least one of diphenyltoluene phosphate (CDP) and diphenylisooctyl phosphate (DPOF). Fluorinated flame retardants include allyl tris(2,2,2-trifluoroethyl). Carbonates include allyl (trifluoroethyl) carbonate (ATFEC).
[0077] In some embodiments, the material of the support member 20 includes at least one of aluminum, nickel, copper, and ceramic to improve the structural strength of the support member 20 and to facilitate the housing 21 to act as a heat conductor between the heat absorber 30 and the electrode assembly 10.
[0078] Please see Figure 5 An embodiment of this application also provides an electronic device 200, which includes the battery cell 100 from any of the above embodiments. Optionally, the electronic device 200 may be a vehicle, mobile phone, portable device, laptop computer, ship, spacecraft, electric toy, or power tool, etc.
[0079] In the aforementioned battery cell 100 and electronic device 200, the spaced reinforcement members 22 enhance the structural strength of the outer casing 21. The outer casing 21 fits against the wall of the winding center hole 10A to support the electrode assembly 10, reducing the risk of deformation of the electrode assembly 10 and thus improving the safety performance of the battery cell 100. At least one sub-cavity 21A1 is provided with a heat-absorbing member 30 or a flame-retardant member 40. The heat-absorbing member 30 is configured to cool or dissipate heat inside the electrode assembly 10, while the flame-retardant member 40 is configured to suppress combustion of the battery cell 100 in the event of thermal runaway, thereby improving the safety performance of the battery cell 100.
[0080] The following describes the specific implementation methods of the battery cells in the embodiments and comparative examples.
[0081] 1. Expansion Rate Test The battery cell was charged at 25°C with a constant current of 0.5C to 4.3V, then charged at a constant voltage of 4.3V to 0.05C (cutoff), and allowed to stand for 10 minutes. It was then discharged at a constant current of 1.0C to 3.0V and allowed to stand for 15 minutes. This cycle was repeated 1000 times. The initial cell thickness and the cell thickness after 1000 cycles were measured using a PPG thickness meter, and the thickness expansion rate was calculated.
[0082] 2. Discharge temperature rise test The battery cell was left to stand at a test temperature of 25°C for 5 minutes, then charged at a constant current of 0.5C to a voltage of 4.3V, followed by constant voltage charging to 0.05C. After standing for 2 hours to allow the lithium-ion battery temperature to drop to 25°C, it was discharged at a constant current of 5C to a voltage of 3V. During the charging and discharging process, a temperature sensor was placed on the center surface of the lithium-ion battery, and the battery was wrapped with insulating cotton. The temperature rise during charging and discharging was recorded. For example, during the discharging process, the temperature at the moment of completion of discharge was recorded, and this temperature minus 25°C is the 25°C discharge temperature rise (°C) of the battery cell.
[0083] 3. Hot Box Test First, the battery cells to be tested undergo pretreatment. The pretreatment conditions are as follows: after standing at a test temperature of 25±2℃ for 60 minutes, discharge to 3.0V with a constant current of 0.7C and stand for 10 minutes; then charge to 4.3V with a constant current of 0.5C, and then charge to 0.05C with a constant voltage of 4.3V. After pretreatment, the battery cells are placed vertically in a hot chamber for hot chamber testing. The temperature in the hot chamber is increased to 150℃ at a rate of 5℃ / min and maintained for 60 minutes. During the test, if the battery cell does not burn or explode, the hot chamber test is considered passed; otherwise, the hot chamber test is considered failed. If 100 battery cells are tested and the number of cells that pass the test is X, then the pass rate is X / 100.
[0084] Example 1: A battery cell with an initial thickness of 12mm, a length of 200mm, and a width of 150mm is assembled as follows: (1) Preparation of negative electrode sheet: The negative electrode active materials artificial graphite, conductive carbon black (Super P), and styrene-butadiene rubber (SBR) are mixed in a weight ratio of 96:1.5:2.5. Deionized water is added as a solvent to prepare a slurry with a weight percentage of 50 wt%. The slurry is stirred evenly and uniformly coated on one surface of a copper foil with a thickness of 8 μm. Then, it is dried at 110 °C to obtain a negative electrode sheet with a single-sided coating of negative electrode active material layer. When preparing a double-sided coated negative electrode sheet, the above steps are repeated on the other surface of the negative electrode sheet to obtain a negative electrode sheet with a double-sided coating of negative electrode active material layer. Then, the coated electrode sheet is cold-pressed to a thickness of 105 μm. Negative electrode tabs are die-cut on the copper foil at the edge of the negative electrode sheet. The negative electrode tabs are then assembled into a tab bundle and connected to the first tab.
[0085] (2) Preparation of the positive electrode sheet: Lithium cobalt oxide (LiCoO2), conductive carbon black (Super P), and polyvinylidene fluoride (PVDF) were mixed in a weight ratio of 97.5:1.0:1.5. N-methylpyrrolidone (NMP) was added as a solvent to prepare a slurry with a solid content of 75 wt%, and the mixture was stirred evenly. The slurry was uniformly coated on one surface of an aluminum foil with a thickness of 10 μm, and then dried at 90 °C to obtain a positive electrode sheet with a single-sided coating of positive active material. When preparing a double-sided coated positive electrode sheet, the above coating steps were repeated on the other surface of the aluminum foil. The coated electrode sheet was then cold-pressed to a thickness of 95 μm, and positive electrode tabs were die-cut on the aluminum foil at the edge of the positive electrode sheet. The positive electrode tabs were then assembled into a tab bundle and connected to the second tab.
[0086] (3) Preparation of electrolyte: In a dry argon atmosphere, ethylene carbonate (EC), ethyl methyl carbonate (EMC) and diethyl carbonate (DEC) are first mixed in a mass ratio of EC:EMC:DEC=30:50:20 to form a basic organic solvent. Then, lithium salt lithium hexafluorophosphate (LiPF6) is added to the basic organic solvent to dissolve and mix evenly to obtain an electrolyte with a lithium salt concentration of 1.15 mol / L.
[0087] (4) Preparation of the isolation membrane: A 7-micron thick porous polyethylene polymer film was used as the isolation membrane.
[0088] (5) Electrode assembly fabrication: The negative electrode sheet, separator, and positive electrode sheet are wound around the support member. The outer shell and reinforcing members of the support member are made of... Figure 3 The structure has a width of 135mm along the first direction, a length of 173mm along the second direction, R1=2mm, and W1=15mm.
[0089] (6) Electrode assembly assembly: The electrode assembly is encapsulated in the housing.
[0090] (7) Electrolyte injection and encapsulation: Electrolyte is injected into the assembled electrode assembly, and the battery cell is obtained through vacuum encapsulation, standing, hot pressing, shaping and other processes.
[0091] Examples 2 and 3: Except for the parameters mentioned in Table 1, all other parameters are the same as in Example 1.
[0092] Comparative Example 1: No heat-absorbing or flame-retardant components were provided in the support. It should be noted that all other parameters of Comparative Example 1 are the same as those of Example 1.
[0093] Comparative Example 2: The winding center hole of the electrode assembly is not provided with a support. It should be noted that the other parameters of Comparative Example 2 are the same as those of Example 1.
[0094] Note: In Table 1, " / " indicates that the parameter is not included.
[0095] As can be seen from Comparative Examples 1-2 and Examples 1-3, the support member includes a shell and multiple reinforcing members. The shell has a receiving cavity, and at least a portion of the outer surface of the shell is in contact with the wall of the winding center hole. The multiple reinforcing members connected to the inner surface of the shell can reduce the expansion rate of the battery cell. The heat-absorbing element inside the sub-cavity can reduce the temperature rise of the battery cell. The flame-retardant element inside the sub-cavity can improve the pass rate of the hot box test.
[0096] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any changes or substitutions within the technical scope disclosed in this application should be covered within the scope of this application.
Claims
1. A battery cell, characterized in that, The battery cell includes: An electrode assembly includes a first electrode, a second electrode, and a separator, wherein the separator is disposed between the first electrode and the second electrode, and the electrode assembly has a winding center hole, wherein the first electrode, the separator, and the second electrode are wound around the winding center hole. A support member is disposed in the winding center hole. The support member includes a shell and a plurality of reinforcing members. The shell has a receiving cavity. At least a portion of the outer side of the shell is in contact with the hole wall of the winding center hole. The plurality of reinforcing members are connected to the inner side of the shell. The plurality of reinforcing members are spaced apart and divide the receiving cavity into a plurality of sub-cavities. At least one of the sub-cavities is provided with a heat-absorbing member or a flame-retardant member. The outer shell includes two planar areas and two arcuate areas. The two planar areas are spaced apart along a first direction, and the two arcuate areas are spaced apart along a second direction and are respectively connected to the two ends of the two planar areas. The two planar areas and the two arcuate areas enclose the receiving cavity. The first direction is perpendicular to the second direction. The reinforcing member connects the two planar regions, the plurality of reinforcing members are arranged along the second direction, the sub-cavities are formed between two adjacent reinforcing members or between the arc-shaped region and the reinforcing member adjacent to the arc-shaped region, at least one sub-cavity is provided with the heat-absorbing member, and at least one sub-cavity is provided with the flame-retardant member, the sub-cavities provided with the heat-absorbing member and the sub-cavities provided with the flame-retardant member are arranged at intervals.
2. The battery cell as described in claim 1, characterized in that, Along the winding direction of the electrode assembly, the separator includes a first starting segment extending beyond the starting ends of the first electrode and the second electrode, the first starting segment being wound around the support member at least one turn.
3. The battery cell as described in claim 1, characterized in that, The radius of the arc corresponding to the arc surface area is R1, where 1mm ≤ R1 ≤ 3mm.
4. The battery cell as described in claim 1, characterized in that, Along the second direction, the distance between two adjacent reinforcing members is W1, where 10mm ≤ W1 ≤ 20mm.
5. The battery cell as described in claim 1, characterized in that, The thickness of the planar region is T1, 0.3mm≤T1≤2mm; and / or, the thickness of the arcuate region is T2, 0.3mm≤T2≤2mm.
6. The battery cell as described in claim 1, characterized in that, The heat-absorbing element is made of paraffin wax.
7. The battery cell as described in claim 1, characterized in that, The flame-retardant component includes a housing and a flame retardant. The housing has a receiving cavity, and the flame retardant is disposed in the receiving cavity. The melting point of the housing is 100°C to 130°C.
8. The battery cell as described in claim 7, characterized in that, The material of the housing includes polymethyl methacrylate, and the housing accounts for 3% to 10% of the weight of the flame retardant component.
9. The battery cell as described in claim 7, characterized in that, The flame retardant material includes at least one of alkyl phosphate esters, fluoroalkyl phosphate esters, aromatic phosphate esters, fluorinated flame retardants, and carbonates.
10. The battery cell as described in claim 1, characterized in that, The material of the support includes at least one of aluminum, nickel, copper, and ceramic.
11. An electronic device, characterized in that, The electronic device includes a battery cell as described in any one of claims 1 to 10.
Citation Information
Patent Citations
Lithium ion battery
CN113611918A
Winding battery cell, preparation method, battery comprising winding battery cell and assembly method
CN115133100A
Battery cell, battery, electric device and winding equipment
CN217768478U