In-situ variable-temperature tensile transmission X-ray scattering characterization device
By designing an in-situ variable temperature stretched transmission X-ray scattering characterization device, real-time monitoring and precise control of thin film structure under multi-field conditions are achieved, which solves the problem that multi-field coupling cannot be achieved in traditional technology, and improves the depth and accuracy of material structure response research.
Patent Information
- Application Number
- CN202510527892.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-04-25
- Publication Date
- 2025-07-25
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Traditional transmittance X-ray scattering technology cannot achieve coupling of multiple external field conditions, especially real-time monitoring and precise control under mechanical loading and temperature changes, which makes it difficult to in-depth research on the structural response of materials under dynamic external fields, and the existing temperature control modules have problems such as insufficient temperature field uniformity and poor thermal stability.
A in-situ variable temperature stretched transmission X-ray scattering characterization device is designed, including a base, a top support, a tension structure, a heating structure and a driving structure. The coupling of tension and temperature is achieved through sealing cooperation, and the in-situ information is collected using X-rays, so that the evolution information of the film structure can be obtained under different temperature fields under the set stress field.
Real-time monitoring and precise control of thin film structures under multi-field conditions are achieved, and the transmission X-ray in-situ testing capability is provided under high or low temperature conditions, which improves the depth and accuracy of material structure response research.
Smart Images

Figure CN120369439A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of thin film testing, and particularly relates to an in-situ variable temperature tensile transmission X-ray scattering characterization device. Background Art
[0002] Synchrotron radiation light source is a high-energy, high-brightness, and high-stability light source, providing advanced research means for various experimental methods. Among them, transmission X-ray scattering (TXS) is an important means for characterizing the structure of materials. By analyzing the scattering signals generated when X-rays penetrate the sample, the structural information at the nano- to atomic scale inside the materials can be resolved.
[0003] In recent years, with the surge in the application requirements of functional materials in the fields of flexible electronics, energy storage, biomedicine, etc., the research on the real-time structural response of materials under dynamic external fields (such as mechanical deformation, temperature change) has become a key scientific issue. The potential of transmission X-ray scattering technology in this field has gradually emerged. Compared with reflection X-ray technology, the transmission mode has the advantages of large penetration depth and the ability to obtain bulk structural characteristics, and is particularly suitable for studying the three-dimensional structure evolution behavior of thin films, polymer materials, composite materials and other thin-layer or soft matter systems.
[0004] Traditional transmission X-ray scattering technology is usually designed for static or single external field conditions, unable to achieve the coupling of multiple external field conditions. Conventional tensile equipment often cannot be compatible with the X-ray optical path, and cannot achieve precise control and real-time monitoring in the transmission mode within a wide strain range (such as >100%), resulting in difficulties in in-depth research on the mechanical-structure correlation. For temperature-sensitive material systems, the existing temperature control modules have problems such as insufficient temperature field uniformity and poor thermal stability, and it is difficult to be effectively integrated with the mechanical loading device, resulting in limited efficiency of in-situ transmission X-ray testing under high or low temperature conditions. Therefore, there is an urgent need for an in-situ variable temperature tensile transmission X-ray scattering characterization device to solve these problems. Summary of the Invention
[0005] The purpose of the present invention is to provide an in-situ variable temperature tensile transmission X-ray scattering characterization device to solve the above problems.
[0006] To achieve the above purpose, the present invention provides the following solutions:
[0007] An in-situ variable temperature tensile transmission X-ray scattering characterization device, comprising:
[0008] A base, provided with a light inlet hole at the bottom for X-ray incidence;
[0009] A top support, detachably arranged on the top of the base, the base and the top support are hermetically matched, and a light outlet hole for X-ray emission is provided in the middle of the top support;
[0010] A tension structure, disposed within the base, for clamping and stretching a specimen;
[0011] A heating structure, disposed within the tension structure, for adjusting the ambient temperature of the specimen;
[0012] A driving structure, in transmission connection with the tension structure, the driving structure being disposed on one side of the base;
[0013] A control board, electrically connected to the tension structure, the driving structure, and the heating structure, the control board being mounted on the base.
[0014] Optionally, the tension structure includes:
[0015] Two parallel slide rails, the slide rails being fixed to the base;
[0016] A platform support one and a platform support two, both ends of the platform support one and both ends of the platform support two are respectively slidably disposed on the two slide rails, the platform support one and the platform support two respectively clamp both ends of the specimen;
[0017] Both the platform support one and the platform support two are in transmission connection with the driving structure;
[0018] The heating structure is mounted on the platform support one and the platform support two;
[0019] The platform support two / platform support one is equipped with a tension detection unit, the tension detection unit is used to detect the tension of the specimen.
[0020] Optionally, the heating structure includes two heating components, the two heating components are respectively fixed on the platform support one and the platform support two, and the heating components are electrically connected to the control board;
[0021] The heating component includes an electric heating element and a temperature controller, and the electric heating element is used to heat the specimen.
[0022] Optionally, the tension detection unit includes a tension sensor, the tension sensor is fixed on the platform support one / platform support two, the tension sensor is used to clamp one end of the specimen, and the tension sensor is electrically connected to the control board.
[0023] Optionally, the driving structure includes a lead screw, which is threadedly connected to the platform support two and the platform support one, the lead screw is a bidirectional screw, the platform support two and the platform support one are respectively disposed at both ends of the lead screw, one end of the lead screw is rotatably connected to the base, and the other end of the lead screw is in transmission connection with a driving component.
[0024] Optionally, the driving component includes a transmission part and an output part. The output part is in transmission connection with the transmission part, and the transmission part is in transmission connection with the lead screw.
[0025] Optionally, the transmission part includes a worm gear. The worm gear is axially connected to the other end of the lead screw. The worm gear meshes with a worm, and the worm is in transmission connection with the output part.
[0026] Optionally, the output part includes a motor. The fixed end of the motor is fixedly connected to the base, the output shaft of the motor is axially connected to the worm, and the motor is electrically connected to the control board.
[0027] Optionally, sliders are fixedly connected to both ends of the bottom of the second platform support and the first platform support. The sliders are slidably arranged in the corresponding slide rails.
[0028] Optionally, the lead screw is rotatably connected to an end support through a bearing, and the end support is fixed on the base.
[0029] Compared with the prior art, the present invention has the following advantages and technical effects:
[0030] During use, after removing the top support, both ends of the specimen are installed on the tensioning structure, and then the top support is hermetically installed back on the base, so that the specimen is in a relatively sealed environment. The temperature of the specimen accommodation cavity formed by enclosing between the base and the top support is adjusted through the heating structure to achieve the coupling of tension and temperature. X-rays are incident through the light inlet hole at the bottom of the base, penetrate the sample, and are emitted through the light outlet hole in the middle of the top support, and are received by the light collection device, so that the in-situ information of the film structure evolution under different temperature fields in the set stress field can be obtained. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the following will briefly introduce the drawings required for use in the embodiments. Obviously, the drawings in the following description are only some embodiments of the present invention. For those of ordinary skill in the art, other drawings can be obtained based on these drawings without creative efforts:
[0032] Figure 1 It is the internal structure diagram of the present invention;
[0033] Figure 2 It is the overall structure diagram of the present invention;
[0034] Figure 3 It is the structure diagram of the base of the present invention;
[0035] Figure 4 It is the schematic diagram of the experimental installation of the present invention
[0036] Figure 5 It is the two-dimensional image of the blend samples of N3 and N2200 with different ratios of the present invention varying with the tensile strain;
[0037] Figure 6 It is the orientation parameter curve of the blend samples of N3 and N2200 with different ratios of the present invention varying with the tensile strain;
[0038] Figures 7 - 8 It is the two-dimensional image of the P3HT sample of the present invention varying with the tensile strain;
[0039] Figure 9 It is the orientation parameter curve of the P3HT sample of the present invention varying with the tensile strain;
[0040] Figure 10 It is the two-dimensional image of the PDPTT sample of the present invention varying with the tensile strain;
[0041] Figure 11 It is the orientation parameter curve of the PDPTT sample of the present invention varying with the tensile strain;
[0042] Figure 12 It is the two-dimensional image of the blend samples of PM6 and PAEF of the present invention varying with the tensile strain;
[0043] Among them, 1. Base; 2. Worm; 3. Lead screw; 4. Worm gear; 5. Slide rail; 6. Slide block; 7. Bearing; 8. Platform support two; 9. Platform support one; 11. End support; 12. Tensile force sensor; 13. Heating component; 14. Control board; 15. Top support; 16. Motor. Detailed implementation manners
[0044] Next, the technical solutions in the embodiments of the present invention will be clearly and completely described in conjunction with the accompanying drawings in the embodiments of the present invention. Obviously, the described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. All other embodiments obtained by those of ordinary skill in the art based on the embodiments of the present invention without creative efforts shall fall within the protection scope of the present invention.
[0045] To make the above objects, features, and advantages of the present invention more obvious and understandable, the present invention will be further described in detail below in conjunction with the accompanying drawings and specific implementation manners.
[0046] Refer to Figures 1 to 12 , the present invention discloses an in-situ variable-temperature tensile transmission X-ray scattering characterization device, including:
[0047] Base 1, with a light inlet hole for X-ray incidence opened at the bottom;
[0048] The top support 15 is detachably arranged on the top of the base 1. The base 1 is in sealed cooperation with the top support 15. A light-emitting hole for X-ray emission is provided in the middle of the top support 15.
[0049] The tension structure is arranged in the base 1 and is used for clamping and stretching the specimen.
[0050] The heating structure is arranged in the tension structure and is used for adjusting the environmental temperature of the specimen.
[0051] The driving structure is in transmission connection with the tension structure and is arranged on one side of the base 1.
[0052] The control board 14 is electrically connected to the tension structure, the driving structure and the heating structure, and the control board 14 is installed on the base 1.
[0053] During use, after removing the top support 15, both ends of the specimen are installed on the tension structure, and then the top support 15 is sealed and installed back on the base 1, so that the specimen is in a relatively sealed environment. The temperature of the specimen accommodation cavity formed by enclosing between the base 1 and the top support 15 is adjusted by the heating structure to realize the coupling of tension and temperature. The X-ray is incident from the bottom light-incident hole of the base 1, penetrates the sample, and then is emitted from the light-emitting hole in the middle of the top support 15 and received by the light collection device, and the in-situ information of the film structure evolution under different temperature fields under the set stress field can be obtained.
[0054] As an optional implementation manner, the tension structure includes:
[0055] Two parallel slide rails 5 are arranged, and the slide rails 5 are fixed to the base 1;
[0056] The platform support one 9 and the platform support two 8. Both ends of the platform support one 9 and both ends of the platform support two 8 are respectively slidably arranged on the two slide rails 5. The platform support one 9 and the platform support two 8 respectively clamp both ends of the specimen;
[0057] Both the platform support one 9 and the platform support two 8 are in transmission connection with the driving structure;
[0058] The heating structure is installed on the platform support one 9 and the platform support two 8;
[0059] The platform support two 8 / the platform support one 9 is equipped with a tension detection unit, and the tension detection unit is used for detecting the specimen tension.
[0060] As an optional implementation manner, the heating structure includes two heating components 13. The two heating components 13 are respectively fixed on the platform support one 9 and the platform support two 8, and the heating components 13 are electrically connected to the control board 14;
[0061] The heating component 13 includes an electric heating element and a temperature controller, and the electric heating element is used for heating the specimen.
[0062] As an alternative embodiment, the tensile force detection unit includes a tensile force sensor 12, which is fixed on the platform support one 9 / platform support two 8. The tensile force sensor 12 is used to clamp one end of the specimen, and the tensile force sensor 12 is electrically connected to the control board 14.
[0063] As an alternative embodiment, the driving structure includes a lead screw 3, which is threadedly connected to the platform support two 8 and the platform support one 9. The lead screw 3 is a bidirectional screw. The platform support two 8 and the platform support one 9 are respectively arranged at both ends of the lead screw 3. One end of the lead screw 3 is rotatably connected to the base 1, and the other end of the lead screw 3 is drivingly connected to a driving component.
[0064] As an alternative embodiment, the driving component includes a transmission part and an output part. The output part is drivingly connected to the transmission part, and the transmission part is drivingly connected to the lead screw 3.
[0065] As an alternative embodiment, the transmission part includes a worm gear 4, which is axially connected to the other end of the lead screw 3. The worm gear 4 meshes with a worm 2, and the worm 2 is drivingly connected to the output part.
[0066] As an alternative embodiment, the output part includes a motor 16. The fixed end of the motor 16 is fixedly connected to the base 1. The output shaft of the motor 16 is axially connected to the worm 2, and the motor 16 is electrically connected to the control board 14.
[0067] As an alternative embodiment, both ends of the bottom of the platform support two 8 and the platform support one 9 are fixedly connected with sliders 6, and the sliders 6 are slidably arranged in the corresponding slide rails 5.
[0068] As an alternative embodiment, the lead screw 3 is rotatably connected to an end support 11 through a bearing 7, and the end support 11 is fixed on the base 1.
[0069] This device is composed of the following structures, including:
[0070] External frame: base 1, top support 15 and end support 11;
[0071] Transmission system: motor 16, worm 2, worm gear 4, lead screw 3, bearing 7;
[0072] Moving components: slider 6, slide rail 5, platform support two 8, platform support one 9;
[0073] Auxiliary components: control board 14, heating component 13 and tensile force sensor 12.
[0074] Among them, the base 1 constitutes a three-dimensional basic support platform, and the top support 15 forms a detachable closed connection with the upper surface of the base 1 through sealing. The motor 16 is fixed on the lateral mounting surface of the base 1. The motor 16 is a servo motor, and its output shaft is coaxially connected to the worm 2. The worm 2 meshes with the worm gear 4 to drive the screw rod 3 to rotate. The screw rod 3 is installed on the end support 11 through the bearing 7, and the end support 11 is fixed on the base 1.
[0075] The moving component includes a slide rail 5 arranged in parallel on the surface of the base 1 and a slider 6 that cooperates with the slide rail 5. The slider 6 is fixed and limited by the platform support two 8 and the platform support one 9.
[0076] The auxiliary components include a control board 14, a heating component 13, and a tension sensor 12. The control board 14 and the heating component 13 are arranged between the transmission structures. The tension sensor 12 is connected to the end of the conveyor chain and forms a closed-loop control with the control board 14 and the motor 16. Each auxiliary component is assembled based on the base 1, and the top support 15 forms a closed protection for the internal structure.
[0077] Among them, the specimen is a thin film sample. The thin film sample includes a pure elastomer film or a composite film, which is composed of a substrate and a functional film deposited on the substrate. The substrate is an elastomer film.
[0078] The elastomer film includes, but is not limited to, one of styrene-based thermoplastic elastomer SEBS, polysiloxane-based elastomer PDMS, thermoplastic polyurethane-based elastomer TPU, polyolefin-based thermoplastic elastomer POE, and polyamide-based thermoplastic elastomer TPA.
[0079] The functional film includes, but is not limited to, one of a conjugated polymer film and a ductile metal film.
[0080] The usage method of this device includes the following steps:
[0081] Fabricate the specimen;
[0082] Use the elastomer film as a flexible substrate, and use physical or chemical deposition processes to prepare a functional film on the surface of the substrate to construct a thin film sample;
[0083] Install the specimen and install both ends of the specimen in the tensioning structure;
[0084] Precisely fix the thin film sample in the clamping area of the tensioning structure to ensure that the long axis direction of the sample is consistent with the stretching direction;
[0085] Irradiate X-rays, and at the same time start the tensioning structure and the heating structure. Tension through the tensioning structure and heat the specimen through the heating structure.
[0086] Irradiate a thin film sample with X-rays, set the tensile strain and temperature, and obtain in-situ information on the structural evolution of the thin film under different stress fields and / or different temperature fields.
[0087] Furthermore, irradiate a thin film sample with X-rays, set the tensile strain and temperature, and obtain in-situ information on the structural evolution of the thin film under different stress fields and / or different temperature fields, including: applying a gradient tensile load to the thin film specimen, setting the strain gradient parameters to 0%, 5%, 10%, 20%, 30%, 40%, 50%, 80%, 100%, 200%, 300%, 400%, 500%, 600%, 700%, 800%, 900%, 1000%. Each time the tensile strain is adjusted, the base 1 rotates 90°. At each tensile strain, control the X-ray irradiation of the thin film sample according to predetermined parameters to obtain in-situ information on the structural evolution of the thin film under different stress fields; under the condition of maintaining a constant tensile strain, establish a stepped temperature field of -50 - 300 °C with a step size of 10 °C by program-controlled temperature. Each time the temperature is adjusted, the base 1 rotates 90°. At each temperature, control the X-ray irradiation of the thin film sample according to predetermined parameters to obtain in-situ information on the structural evolution of the thin film under different temperature fields in the set stress field.
[0088] Furthermore, set the parameters as: exposure time 1 - 600 seconds.
[0089] In some embodiments, the heating component 13 can fix the thin film sample. After the thin film sample is fixed, irradiate it with X-rays. By controlling the drive system, the tensile state of the thin film sample can be adjusted. The tensile stress sensor 12 can detect the tensile stress of the thin film sample, and then determine its tensile strain, so that the thin film sample can be controlled in the set tensile strain state. Through the detector, the scattering data of the thin film sample can be obtained, and then the in-situ information on the structural evolution of the thin film under different stress fields can be obtained. At the same time, the heating component 13 can control the temperature environment of the thin film sample. Under the set stress field, change the temperature environment of the thin film sample through the heating component 13, irradiate the thin film sample with X-rays, and based on the scattering data of the thin film sample collected by the detector, obtain the in-situ information on the structural evolution of the thin film under different temperature fields. Among them, the heating component 13 includes an electric heating element and a temperature controller. Since the temperature field of the thin film sample is higher than the normal room temperature environment, only heating is required. The electric heating element is used for heating, and a temperature probe is configured in the temperature controller. Use the temperature probe to collect the current temperature value. If the current temperature value reaches the set temperature value, the temperature controller controls the electric heating element to stop heating. In this way, the temperature can be controlled within the set temperature range through the heating component 13.
[0090] In some embodiments, the motor 16 operates to rotate the worm 2, thereby causing the lead screw 3 connected to the worm 2 to rotate, and the platform support two 8 and the platform support one 9 move towards or away from each other. By controlling the operating parameters of the motor 16, such as rotational speed, torque, etc., the rate at which the platform support two 8 and the platform support one 9 move towards or away from each other can be controlled, thereby achieving the control of the stretching rate of the thin film sample. Among them, two lead screws 3 can be provided to ensure the stability of the drive.
[0091] As an additional implementation, the thin film sample includes a pure elastomer film or a composite film, which is composed of a substrate and a functional film deposited on the substrate, and the substrate is an elastomer film. The deposition methods of the functional film include, but are not limited to, spin coating, drop coating, blade coating, vacuum evaporation.
[0092] As an additional implementation, the thickness of the substrate is 1 μm to 5 mm, and the thickness of the functional film is 10 nm to 10 μm.
[0093] In some embodiments, the elastomer film includes one of styrenic thermoplastic elastomers, polysiloxane elastomers, thermoplastic polyurethane elastomers, polyolefin thermoplastic elastomers, polyamide thermoplastic elastomers.
[0094] In some embodiments, the functional film includes one of conjugated polymer films, ductile metal films.
[0095] Exemplarily, the sample materials include, but are not limited to, elastomers, thiophene-based conjugated polymers, pyrrolopyrrole dione (DPP)-based conjugated polymers, isoindigo (IID)-based conjugated polymers, benzodithiophene (BDT)-based conjugated polymers, naphthalene / perylene diimide (NDI / PDI)-based conjugated polymers, benzothiadiazole (BTz)-based conjugated polymers, quinoxaline-based conjugated polymers, styrylene-based conjugated polymers, etc.
[0096] Exemplarily, the sample material includes, but is not limited to, a blend solution of any one or more of SEBS, PDMS, TPU, POE, TPA, PAEF, P3HT, PTVT-T, PDCBT, PDCBT-Cl, P4T2F-HD, P4T2F-OD, PDTP-DPP, PDPP3T, PDPP5T, PDPP-TT, PDPPTPT, PDPPSDTPS, PD2FCT-29DPP, PIID-DT, PTB7, PM6, PM7, PTB7-Th, asy-ranPBTBDT, PBnDT-FTAZ, D18, D18-CI, PFBCPZ, PBDB-T, J71, PTzBi-Si, PBT(TH), PBD(EDOT), PBD(TH), PBDTTPD-HT, PNDI-5DD, PNDI-POD, N2200, PNDI-TF-4T, PCDTBT, PCPDTBT, Si-PCPDTBT, IDTBT, PDTPBT, PTQ1, PTQ-10, PBQx-TC1, PffBT4T-2OD, CC1C10-PPV, BBL, PTAA, TIPS-TPD.
[0097] The device provided in this embodiment can collect the microstructural changes that occur in the functional film under tensile conditions. Through the transmission system, the polymer film can be precisely uniaxially stretched, with a strain range from 0% to 1000% and a strain rate range from 0.01 mm / min to 1000 mm / min. To ensure controllable tensile conditions, a load cell and a strain gauge sensor can also be integrated into the device to collect the weight and strain data of the film sample. These sensors help to accurately measure and control the applied strain during the experiment. A heating component 13 is installed on the base 1, which can heat the film sample to 300 °C. Importantly, a rotating platform can also be provided below the base 1, which can be well compatible with the beamline 1W1A of the Beijing Synchrotron Radiation Facility (BSRF) and the beamline 02U2 of the Shanghai Synchrotron Radiation Facility (SSRF).
[0098] When using this device for tensile testing, based on the set sensors and the control of the transmission system, some important information can be recorded, such as the displacement-time graph, stress-time graph, and stress-displacement graph, which can be recorded during the measurement process.
[0099] Therefore, through the device provided in this embodiment, information on the microstructural changes occurring in the semiconductor polymer film under various tensile conditions can be obtained, and at the same time, the temperature dependence of the nanostructure of many functional films under uniaxial stretching can be characterized.
[0100] The X-ray scattering experiment was mainly carried out on the 1W1A beamline of BSRF. In the tensile experiment, a customized sample stage was used to fix the sample. An X-ray beam with a specific wavelength penetrated the sample, and the scattered data was collected simultaneously using a 1MEIGER2X detector. The sample-to-detector distance (SDD) was set to a specific value (86.6 mm), and LaB6 was used for SDD calibration. By collecting the scattered X-ray information with a two-dimensional detector, a detailed scattering pattern could be obtained. The height of the central heating copper block was adjusted to be slightly higher than the fixture. The speed was set to 10 mm / min. The distance and height between the sample stage and the detector were adjusted to appropriate values to ensure optimal measurement and data collection.
[0101] The tensile strains of the specimens were 0%, 5%, 10%, 20%, 30%, 40%, 50%, 80% and 100%, 200%, 300%, 400%, 500%, 600%, 700%, 800%, 900%, 1000% respectively. At each strain, the incident angle was 0.2° and the exposure time was 5 seconds. Each time the strain was adjusted, the device turntable rotated 90°, and measurements were carried out perpendicular and parallel to the tensile direction respectively. For temperature-related measurements, the tensile strain was fixed at 40%. The hot stage temperature varied between -50°C, -40°C, -30°C, -20°C, -10°C, 0°C, 10°C, 20°C, 30°C, 40°C, 50°C, 60°C, 70°C, 80°C and 90°C, 100°C, 110°C, 120°C, 130°C, 140°C, 150°C, 160°C, 170°C, 180°C, 190°C, 200°C, 210°C, 220°C, 230°C, 240°C, 250°C, 260°C, 270°C, 280°C, 290°C and 300°C. The incident angle was maintained at 0.2° and the exposure time was 5 seconds. Each time the temperature was measured, the workbench rotated 90°. According to these steps, in-situ GIXS measurements were carried out using a new tensile device and software to obtain the structural changes of polymer films at different strain levels and temperatures.
[0102] Compared with the prior art, the present invention uses an elastomer film as the substrate, deposits a functional film on the substrate, fixes it on the fixture of a uniaxial tensile device, and sets a certain tensile rate / strain and temperature, then in-situ information on the structural evolution of the film under stress and temperature fields can be obtained, thus providing valuable information for the in-situ structural evolution of various functional films under tensile conditions, and can characterize the temperature dependence of the molecular-scale structure of functional films under uniaxial tension.
[0103] Based on the above-described method steps, the following embodiments of the present application will further prove the feasibility and progressiveness of the present application in combination with specific experiments.
[0104] Application Example 1:
[0105] The prepared SEBS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of the corresponding size; a certain mass of N3 and N2200 were weighed, added to chloroform, and chloroform solutions with a concentration of 15 mg / mL were prepared for pure N3, N3:N2200 mass ratio of 1:4, N3:N2200 mass ratio of 4:1, and pure N2200. They were placed on a hot plate at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved solution was spin-coated on the surface, and after film formation, it was annealed on a hot plate at 100 °C for 10 min; the sample was clamped on a fixture, the stretching speed was set at 10 mm / min, and the stretching strains were set at 0%, 2%, 4%, 6%, 8%, 10%, 12%, 15%, and 20% respectively. At each strain, the incident angle was 0.2° and the exposure time was 5 s. Figure 6 It is a two-dimensional image of samples with different mass ratios of N3 and N2200 varying with the stretching strain.
[0106] Application Example 2:
[0107] The prepared SEBS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of the corresponding size; a certain mass of N3 and N2200 were weighed, added to chloroform, and chloroform solutions with a concentration of 15 mg / mL were prepared for pure N3, N3:N2200 mass ratio of 1:4, N3:N2200 mass ratio of 4:1, and pure N2200. They were placed on a hot plate at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved solution was spin-coated on the surface, and after film formation, it was annealed on a hot plate at 100 °C for 10 min; the sample was clamped on a fixture, the stretching strain was set at 5%, and the hot plate temperatures were set at 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, and 90 °C respectively. At each temperature, the incident angle was 0.2° and the exposure time was 5 s.
[0108] Application Example 3:
[0109] The prepared SEBS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of the corresponding size; a certain mass of P3HT was weighed, added to chloroform, and a chloroform solution with a concentration of 15 mg / mL was prepared. It was placed on a hot plate at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved P3HT solution was spin-coated on the surface, and after film formation, it was annealed on a hot plate at 100 °C for 10 min; the sample was clamped on a fixture, the stretching speed was set at 10 mm / min, and the stretching strains were set at 0%, 5%, 10%, 20%, 30%, 40%, 50%, 80%, and 100% respectively. At each strain, the incident angle was 0.2° and the exposure time was 5 s.
[0110] Application Example 4:
[0111] The prepared SEPS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of corresponding size; a certain mass of P3HT was weighed, added to chloroform, and configured into a chloroform solution with a concentration of 15 mg / mL. It was placed on a hot plate at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved P3HT solution was spin-coated on the surface, and after film formation, it was placed on a hot plate at 100 °C for annealing for 10 min; the sample was clamped on a fixture, the tensile strain was set to 40%, and the hot plate temperatures were set to 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, and 90 °C respectively. At each temperature, the incident angle was 0.2°, and the exposure time was 5 s.
[0112] Application Example 5:
[0113] The prepared SEBS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of corresponding size; a certain mass of PDPPT was weighed, added to chlorobenzene, and configured into a chlorobenzene solution with a concentration of 15 mg / mL. It was placed on a hot plate at 80 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved PDPPT solution was spin-coated on the surface, and after film formation, it was placed on a hot plate at 200 °C for annealing for 60 min; the sample was clamped on a fixture, the tensile speed was set to 3 mm / min, and the tensile strains were set to 0%, 5%, 10%, 20%, 30%, 40%, 50%, and 60% respectively. At each strain, the incident angle was 0.2°, and the exposure time was 5 s.
[0114] Application Example 6:
[0115] The prepared SEPS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of corresponding size; a certain mass of PDPPT was weighed, added to chlorobenzene, and configured into a chlorobenzene solution with a concentration of 15 mg / mL. It was placed on a hot plate at 80 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved PDPPT solution was spin-coated on the surface, and after film formation, it was placed on a hot plate at 200 °C for annealing for 60 min; the sample was clamped on a fixture, the tensile strain was set to 10%, and the hot plate temperatures were set to 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, 90 °C, and 120 °C respectively. At each temperature, the incident angle was 0.2°, and the exposure time was 5 s.
[0116] Application Example 7:
[0117] The prepared SEBS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of corresponding size; a certain mass of PM6 and PAEF were weighed, chloroform was added, and a chloroform solution with a mass ratio of PM6:PAEF of 7:3 and a concentration of 14 mg / mL was prepared. It was placed on a hot stage at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved P3HT solution was spin-coated on the surface, and after film formation, it was placed on a hot stage at 100 °C and annealed for 10 min; the sample was clamped on a fixture, the stretching speed was set to 10 mm / min, and the stretching strains were set to 0%, 5%, 10%, 20%, 30%, 40%, 50%, 80%, and 100% respectively. At each strain, the incident angle was 0.2° and the exposure time was 5 seconds.
[0118] Application Example 8:
[0119] The prepared SEPS flexible substrate with a thickness of about 0.2 mm was cut into a size of 1 cm × 5 cm and pasted on a glass substrate of corresponding size; a certain mass of PM6 and PAEF were weighed, chloroform was added, and a chloroform solution with a mass ratio of PM6:PAEF of 7:3 and a concentration of 14 mg / mL was prepared. It was placed on a hot stage at 40 °C and stirred overnight to dissolve into a homogeneous solution. The dissolved P3HT solution was spin-coated on the surface, and after film formation, it was placed on a hot stage at 100 °C and annealed for 10 min; the sample was clamped on a fixture, the stretching strain was set to 40%, and the hot stage temperatures were set to 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, and 90 °C respectively. At each temperature, the incident angle was 0.2° and the exposure time was 5 seconds.
[0120] In the description of the present invention, it should be understood that the orientation or positional relationship indicated by the terms "longitudinal", "transverse", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", etc. is based on the orientation or positional relationship shown in the drawings. It is only for the convenience of describing the present invention, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation to the present invention.
[0121] The above-described embodiments are only descriptions of the preferred embodiments of the present invention, and do not limit the scope of the present invention. Without departing from the design spirit of the present invention, various deformations and improvements made by those of ordinary skill in the art to the technical solutions of the present invention should fall within the protection scope determined by the claims of the present invention.
Claims
1. An in-situ temperature-variable tensile transmission X-ray scattering characterization device, characterized in that Comprising: A base (1) with a light inlet hole for X-ray incidence provided at the bottom; A top support (15) detachably provided on the top of the base (1), the base (1) being in sealed cooperation with the top support (15), and a light outlet hole for X-ray emission being provided in the middle of the top support (15); A tension structure provided in the base (1) for clamping and stretching a specimen; A heating structure provided in the tension structure for adjusting the environmental temperature of the specimen; A driving structure drivingly connected to the tension structure, the driving structure being provided on one side of the base (1); A control board (14) electrically connected to the tension structure, the driving structure and the heating structure, the control board (14) being installed on the base (1).
2. The in-situ variable-temperature tensile transmission X-ray scattering characterization device according to claim 1, wherein The tension structure includes: Two parallel slide rails (5) fixedly connected to the base (1); A platform support one (9) and a platform support two (8), with both ends of the platform support one (9) and both ends of the platform support two (8) slidably provided on the two slide rails (5) respectively, and the platform support one (9) and the platform support two (8) clamping both ends of the specimen respectively; Both the platform support one (9) and the platform support two (8) are drivingly connected to the driving structure; The heating structure is installed on the platform support one (9) and the platform support two (8); A tension detection unit is installed on the platform support two (8) / platform support one (9) for detecting the tension of the specimen.
3. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 2, characterized in that: The heating structure includes two heating components (13) respectively fixed on the platform support one (9) and the platform support two (8), and the heating components (13) are electrically connected to the control board (14); Each heating component (13) includes an electric heating element and a temperature controller, and the electric heating element is used for heating the specimen.
4. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 2, characterized in that: The tension detection unit includes a tension sensor (12) fixed on the platform support one (9) / platform support two (8), the tension sensor (12) being used for clamping one end of the specimen, and the tension sensor (12) is electrically connected to the control board (14).
5. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 2, characterized in that, The driving structure includes a lead screw (3) threadedly connected to the platform support two (8) and the platform support one (9), the lead screw (3) being a bidirectional screw, with the platform support two (8) and the platform support one (9) respectively provided at both ends of the lead screw (3), one end of the lead screw (3) being rotatably connected to the base (1), and the other end of the lead screw (3) being drivingly connected to a driving component.
6. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 5, characterized in that: The driving component includes a transmission part and an output part, the output part being drivingly connected to the transmission part, and the transmission part being drivingly connected to the lead screw (3).
7. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 6, characterized in that: The transmission part includes a worm wheel (4) axially connected to the other end of the lead screw (3), the worm wheel (4) meshing with a worm (2), and the worm (2) being drivingly connected to the output part.
8. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 7, characterized in that: The output part includes a motor (16), a fixed end of the motor (16) is fixedly connected to the base (1), an output shaft of the motor (16) is shaft-connected to the worm (2), and the motor (16) is electrically connected to the control board (14).
9. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 2, characterized in that: Both ends of the bottom of the platform support two (8) and the platform support one (9) are fixedly connected with sliders (6), and the sliders (6) are slidably arranged in the corresponding slide rails (5).
10. An in-situ temperature-variable tensile transmission X-ray scattering characterization device according to claim 5, characterized in that: The lead screw (3) is rotatably connected with an end support (11) through a bearing (7), and the end support (11) is fixed on the base (1).
Citation Information
Patent Citations
Low-temperature stretching rheometer and method for testing low-temperature performance of high molecular film
CN108152167A
In-situ tensile test device for synchrotron radiation light source white light Laue diffraction
CN117330431A
In-situ variable-temperature stretching device for grazing incidence X-ray scattering characterization and testing method
CN119000747A