Activity-controllable light calcined magnesia calcining system and process

Through the furnace secondary activity regulation and heat recovery process, the problem of uncontrollable activity in light flask magnesium oxide production is solved, and the product quality is stable and energy consumption is reduced, which is suitable for large-scale industrial production.

CN120444917APending Publication Date: 2025-08-08TIANJIN CEMENT IND DESIGN & RES INST CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202510446897.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-04-10
Publication Date
2025-08-08

AI Technical Summary

Technical Problem

In the existing light flask magnesium oxide production process, the product activity is uncontrollable, the quality is unstable, the energy consumption is high, the pollution is serious, the degree of automation is low, and the utilization of low-grade ores is insufficient.

Method used

A system that combines the secondary activity regulation, cooling and heat recovery process of furnace kilns is adopted. Through the coordination of preheating, activation furnace, regulation kiln and cooling system, the active magnesium oxide content of the product is accurately controlled, so as to achieve efficient utilization of hot air and reduce energy consumption.

Benefits of technology

It achieves stable and adjustable content of active magnesium oxide, improves the stability of product quality, reduces system energy consumption, is suitable for large-scale industrial production, and has high cost performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120444917A_ABST
    Figure CN120444917A_ABST
Patent Text Reader

Abstract

The calcination system comprises a preheating system, an activation furnace, a regulation and control kiln, a hot blast stove and a cooling system, the preheating system, the activation furnace, the regulation and control kiln and the cooling system are sequentially connected, an activation furnace burner is arranged on the activation furnace, a high-temperature recovery air outlet of the cooling system is connected with the activation furnace, and a high-temperature recovery air outlet of the hot blast stove is connected with the hot blast stove. A low-temperature recovery air outlet of the cooling system is connected with the hot blast stove, a hot blast stove burner is arranged on the hot blast stove, an air outlet of the hot blast stove is connected with the regulation and control kiln, hot air generated by fuel combustion in the hot blast stove enters the regulation and control kiln, the temperature in the regulation and control kiln is controlled to be kept at a certain constant temperature, and the content of active magnesium oxide is stabilized at a certain constant value. According to the invention, through mutual cooperation of secondary activity regulation and control, cooling and heat recovery processes of the kiln, hot air in the system is efficiently utilized and the energy consumption of the system is reduced while the content of active magnesium oxide in the product is precisely regulated and controlled, so that the system is suitable for large-scale industrial production, the cost is reduced and the cost performance is high.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of magnesium oxide preparation, and in particular to a light-burned magnesium oxide calcining system and process with controllable activity. Background Art

[0002] Magnesite is a key raw material for magnesium oxide production. my country possesses abundant magnesite resources, with proven reserves of 3.642 billion tons, accounting for 28.85% of the global total, and characterized by concentrated resource distribution. Although my country is a major magnesite resource country, years of reckless mining and extensive production methods have led to a growing shortage of high-grade ore, resulting in unstable product quality, low production efficiency, and low added value. Low-temperature calcination of magnesite produces light-burned magnesium oxide, an important strategic material widely used in metallurgy, building materials, construction (decoration), environmental protection, electrical and electronics, and aerospace.

[0003] Building-grade magnesium oxide is one of the main raw materials for making magnesium cementitious materials. The most important indicator of building-grade magnesium oxide is its activity. Different building materials have different requirements for the activity of magnesium oxide powder. The activity of building-grade magnesium oxide is required to be between 50% and 70%. The higher the active magnesium oxide content, the shorter the citric acid neutralization test time and the stronger the chemical activity of the light-burned magnesium oxide.

[0004] Currently, the main furnace types for light-burned magnesium oxide are reverberatory kilns, suspension furnaces, rotary kilns, and vertical furnaces. Reverberatory kilns typically handle raw material particle sizes between 100 and 200 mm, making them incapable of roasting powders and crushed materials. This can easily lead to surface overburning and internal underburning, resulting in unstable product quality, low output, high energy consumption (standard coal consumption ≥ 300 kg per ton of product), severe pollution, high labor intensity, and a low degree of automation. Suspension furnaces can directly roast flotation ore powder with a moisture content of 1% to 2% and a particle size ≤ 200 μm. In a suspended state, the gas-solid contact area is large, heat exchange is rapid, and heat consumption is low. The system is completely enclosed, allowing for centralized collection and treatment of flue gases. This system has a high degree of automation, small footprint, and quick construction. However, its disadvantage is that the product is too active, with an active magnesium oxide content of ≥ 90%, resulting in rapid reaction rates for subsequent products and a short coagulation time, making construction difficult. The biggest problem with using vertical furnaces and rotary kilns is that there are too many explosions during the decomposition process of the ore, which produces a lot of dust, affecting the air permeability of the vertical kiln and the overall kiln condition of the rotary kiln, resulting in unstable product quality and uncontrollable activity.

[0005] In summary, the problems existing in the prior art are:

[0006] (1) The product activity of the existing reverberatory kiln and rotary kiln production processes is uncontrollable and the product quality is unstable.

[0007] (2) The activity of the magnesium oxide product calcined in the suspension furnace is too high, which causes the subsequent products to react quickly and the coagulation time is too short to be used for construction.

[0008] (3) The existing reverberatory kiln production process has low output, high energy consumption, serious pollution, high labor intensity and low degree of automation.

[0009] (4) A large amount of low-grade ore and magnesite crushed ore cannot be fully utilized. Summary of the Invention

[0010] In order to solve the problem of uncontrollable activity of light-burned magnesium oxide products, the present invention provides a light-burned magnesium oxide calcining system and process with controllable activity. Through the cooperation of the secondary activity control, cooling and heat recovery processes of the furnace, while accurately controlling the active magnesium oxide content of the product, the hot air in the system is efficiently utilized, thereby reducing the energy consumption of the system. The entire production system can achieve precise control of the active magnesium oxide content, stable product quality, energy-saving and low-carbon production line, simple process and equipment, suitable for large-scale industrial production, reducing costs, and high cost performance.

[0011] The present invention is achieved as follows: a light-burned magnesium oxide calcining system with controllable activity includes a preheating system, an activation furnace, a control kiln, a hot blast furnace and a cooling system. The preheating system, activation furnace, control kiln and cooling system are connected in sequence. An activation furnace burner is provided on the activation furnace. The high-temperature recovery air outlet of the cooling system is connected to the activation furnace. The low-temperature recovery air outlet of the cooling system is connected to the hot blast furnace. A hot blast furnace burner is provided on the hot blast furnace. The air outlet of the hot blast furnace is connected to the control kiln. The hot air generated by the combustion of fuel in the hot blast furnace enters the control kiln. The temperature in the control kiln is controlled to be maintained at a certain constant temperature, so that the active magnesium oxide content is stabilized at a certain constant value.

[0012] In the above technical solution, preferably, multiple distribution valves are provided on the discharge pipe of the penultimate cyclone separator of the preheating system, so that the material enters the activation furnace at multiple points. The multiple distribution points control the temperature distribution in the activation furnace, so that the outlet temperature of the activation furnace is 600-900°C, and the content of active magnesium oxide out of the activation furnace is ≥85%.

[0013] In the above technical solution, preferably, the temperature in the kiln is regulated in the range of 800-1100°C, the speed of the kiln is regulated in the range of 0-2.5r / min, the residence time of the material in the kiln is regulated in the range of 10-90min, and the active magnesium oxide content is regulated in the range of 50%-70%.

[0014] In the above technical solution, preferably, a lining structure with protrusions is provided in the regulating kiln to prevent the material from passing through too fast and to increase the heat transfer efficiency.

[0015] In the above technical solution, preferably, a heat-insulating material with low thermal conductivity and a high-temperature resistant working layer material are provided in the regulating kiln, so that the surface temperature of the regulating kiln is ≤150°C.

[0016] In the above technical solution, preferably, the cooling system comprises a heat recovery unit and a cooling unit connected in sequence, and the hot material leaving the control kiln directly enters the heat recovery unit for cooling, wherein the air outlet of the heat recovery unit is connected to the activation furnace, and the air outlet of the cooling unit is connected to the hot air furnace.

[0017] In the above technical solution, it is further preferred that the air temperature at the air outlet of the heat recovery unit is 400-800°C, and the air temperature at the air outlet of the cooling unit is 100-300°C.

[0018] In the above technical solution, it is further preferred that the air outlet of the cooling unit is connected to a dust collector, and the air outlet of the dust collector is connected to a waste heat recovery air duct through a fan, and a primary air branch and a secondary air branch are provided on the waste heat recovery air duct, the primary air branch is connected to the hot blast furnace burner, and the secondary air branch is connected to the air inlet of the hot blast furnace, and the air after dust collection enters the hot blast furnace for use as primary air and secondary air.

[0019] In the above technical solution, it is further preferred that the primary air branch pipe and the secondary air branch pipe are both provided with fans and valves to adjust the air volume of the secondary air and control the temperature of the hot air out of the hot air furnace.

[0020] In the above technical solution, it is further preferred that a cold air duct is provided on the inlet air duct of the dust collector, and a valve is provided on the cold air duct, so that the finished products collected by the dust collector enter the finished product transportation system.

[0021] In the above technical solution, it is further preferred that the discharge port of the cooling unit is connected to the finished product transportation system.

[0022] A process for calcining light-burned magnesium oxide with controllable activity comprises the following steps:

[0023] S1: Magnesite ore is fed into the preheating system and undergoes multiple heat exchanges with the flue gas from the activation furnace to remove moisture. After undergoing multi-stage gas-solid heat exchange, the material enters the activation furnace, where magnesium carbonate is decomposed to produce light-burned magnesium oxide products, generating a large amount of flue gas. The activation furnace outlet temperature is controlled at 600-900°C, and the active magnesium oxide content is ≥85%.

[0024] S2: After the material is activated in the activation furnace, it is separated into gas and solid by the final cyclone separator of the preheating system and then enters the control kiln for calcination. The hot air generated by burning fuel in the hot blast furnace enters the control kiln. The material is calcined at a constant temperature between 800-1100℃. The speed of the control kiln is 0-2.5rpm. The material stays in the control kiln for 10-90min. Some active magnesium oxide is overburned and loses its activity, so that the active magnesium oxide content is stabilized at a value between 50-70%. The hot material leaving the control kiln enters the cooling system;

[0025] S3: Cooling air is introduced into the cooling system to exchange heat with the hot material. The high-temperature hot air after heat exchange is 400-800℃ and enters the activation furnace as tertiary air. The low-temperature hot air after heat exchange is 100-300℃ and enters the hot blast furnace. The hot air generated by the combustion of fuel in the hot blast furnace enters the regulating kiln.

[0026] In the above technical solution, preferably, the low-temperature hot air after heat exchange passes through the dust collector to collect dust, and then enters the hot air furnace burner as primary air in one path and enters the hot air furnace as secondary air in the other path, thereby realizing efficient heat recovery and utilization.

[0027] The advantages and positive effects of the present invention are:

[0028] 1. The present invention combines the functions of calcining, cooling and heat recovery of magnesium oxide, and obtains a light-burned magnesium oxide product with stable and adjustable activity, which greatly improves the stability of product quality. At the same time, it realizes full heat recovery and utilization, reduces system energy consumption, and can reduce the standard coal consumption per ton of product, thereby achieving energy saving and efficiency improvement.

[0029] 2. In order to obtain magnesium oxide products with adjustable and controllable activity, the present invention uses multi-point feeding in the activation furnace to adjust the temperature in the calcining furnace to adapt to the activation of magnesite raw materials of different grades, thereby ensuring the stability of the system and the activity of the product.

[0030] 3. Based on the mechanism of partial overburning of magnesium oxide, the present invention designs a control kiln, rationally designs the temperature and time in the kiln, causes a portion of the active magnesium oxide to lose its activity, and further stabilizes the content of active magnesium oxide so that it does not fluctuate. The hot flue gas in the control kiln comes from the hot blast furnace, and the temperature of the flue gas leaving the hot blast furnace is controlled by regulating the secondary air volume, thereby ensuring the temperature stability in the control kiln.

[0031] 4. The present invention sets up a multi-stage cooling system including a heat recovery unit and a cooling unit, and rationally designs the cooling air volume so that the hot air leaving the heat recovery unit is used in the activation furnace, and the hot air leaving the cooling unit is used as primary air and secondary air after dust collection to enter the hot air furnace. This system can achieve full combustion of fuel, stable and adjustable content of activated magnesium oxide, full cooling of finished products, and full recovery of waste heat, which can effectively reduce the system's heat consumption and investment costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Figure 1 This is a schematic diagram of the activity-controllable light-burned magnesium oxide calcining system provided in Example 1 of the present invention.

[0033] In the picture:

[0034] 1- preheating system; 101- final cyclone separator; 102- material distribution valve;

[0035] 2-Activation furnace; 3-Hot blast furnace; 4-Hot blast furnace burner; 5-Activation furnace burner; 6-Control kiln; 7-Smoke chamber; 8-Kiln door cover; 9-Heat recovery unit; 10-Cooling unit; 11-Dust collector; 12-Blower; 13-Finished zipper machine; 14-Tertiary air duct; 15-Waste heat recovery duct; 16-Primary air branch pipe; 17-Secondary air branch pipe; 18-Kiln tail high-temperature fan; 19-Cold air duct;

[0036] a-magnesite; b-finished magnesium oxide; A-cooling air; B-flue gas from preheating system; C-excess air;

[0037] The dotted line with an arrow is the direction of airflow; the solid line with an arrow is the direction of material flow. DETAILED DESCRIPTION

[0038] The following will clearly and completely describe the technical solutions in the embodiments of the present invention in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative efforts are within the scope of protection of the present invention.

[0039] In the description of the present invention, it should be understood that the terms "up", "down", "front", "back", "left", "right", "inside", "outside", etc., indicating directions or positional relationships, are based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they should not be understood as limiting the present invention.

[0040] In the description of the present invention, it should be noted that, unless otherwise expressly specified or limited, the terms "mounted," "connected," and "connected" should be understood in a broad sense. For example, they may refer to fixed, detachable, or integral connections; mechanical or electrical connections; direct or indirect connections through an intermediate medium; and internal communication between two components. Those skilled in the art will understand the specific meanings of the above terms in the present invention based on the specific circumstances.

[0041] Example 1

[0042] See also Figure 1The embodiment of the present invention provides a calcining system for light-burned magnesium oxide with controllable activity, comprising a preheating system 1, an activation furnace 2, a hot blast furnace 3, a control kiln 6, a smoke chamber 7 connected to the control kiln, and a cooling system. The preheating system 1, the activation furnace 2, the control kiln 6, and the cooling system are connected in sequence. The control kiln 6 comprises a kiln tail smoke chamber 7 and a kiln door cover 8. The control kiln 6 is not provided with a burner (i.e., no fuel inlet is provided). The activation furnace 2 and the hot blast furnace 3 are respectively provided with burners. The activation furnace burner 5 is located at the lower part of the activation furnace 2, and the hot blast furnace burner 4 is located at the head of the hot blast furnace 3.

[0043] A raw material inlet is provided at the top of the preheating system 1. The discharge pipe of the penultimate cyclone separator of the preheating system 1 is connected to the activation furnace 2. The outlet temperature of the activation furnace 2 is 600-900°C. The air inlet of the final cyclone separator 101 of the preheating system 1 is connected to the air outlet duct of the activation furnace 2. The discharge pipe of the final cyclone separator 101 of the preheating system 1 is connected to the tail smoke chamber 7 of the control kiln. The hot material exiting the control kiln 6 is directly cooled by the cooling system. The high-temperature recovery air outlet of the cooling system is connected to the activation furnace 2. The low-temperature recovery air outlet of the cooling system is connected to the hot blast furnace 3. The air outlet of the hot blast furnace 3 is connected to the kiln door cover 8 of the control kiln. The hot air generated by the combustion of fuel in the hot blast furnace 3 enters the control kiln 6. The fuel in the hot blast furnace 3 can be coal, oil, natural gas, coal-to-gas, etc. The temperature in the control kiln 6 is controlled to maintain a constant temperature to stabilize the active magnesium oxide content at a constant value.

[0044] The fuel is burned in the hot blast furnace 3, and a relatively constant hot blast temperature can be precisely controlled to enter the control kiln 6. The temperature range in the control kiln 6 is adjusted between 800-1100°C, the rotation speed range in the control kiln 6 is adjusted between 0-2.5r / min, the residence time of the material in the control kiln 6 is 10-90min, and the active magnesium oxide content range is adjusted between 50%-70%.

[0045] After being ground to the appropriate particle size, the raw material magnesite a is fed into preheating system 1. Within preheating system 1, the material undergoes multi-stage gas-solid heat exchange with the flue gas exiting activation furnace 2 before entering activation furnace 2. Flue gas B exiting the preheating system enters the grinding system or flue gas treatment system. After being activated in activation furnace 2, the magnesium oxide undergoes gas-solid separation in the final cyclone separator 101 before entering control kiln 6 for further calcination. This causes some of the active magnesium oxide to overburn and lose its activity, thereby precisely controlling the active magnesium oxide content to a fixed value that can be adjusted between 50% and 70%. The hot material exiting control kiln 6 enters the cooling system. The high-temperature hot air exiting the cooling system enters activation furnace 2 as tertiary air. The low-temperature hot air exiting the cooling system enters hot blast furnace 3. The hot air generated by the fuel combustion in hot blast furnace 3 enters control kiln 6.

[0046] As a preferred embodiment, multiple dispensing valves 102 are provided on the discharge pipe of the penultimate cyclone separator of the preheating system 1, allowing the material to enter the activation furnace 2 at multiple points. These dispensing points control the temperature distribution within the activation furnace 2. In this embodiment, two dispensing valves 102 are provided on the discharge pipe of the penultimate cyclone. These three dispensing points control the temperature within the activation furnace 2, ensuring that the outlet temperature of the activation furnace 2 is 600-900°C and the active magnesium oxide content of the material leaving the activation furnace 2 is ≥85%. The preheating system 1 is a two- to six-stage cyclone separation preheater, preferably a five-stage cyclone separation preheater in this embodiment. Air lock valves are provided on the discharge pipes of each cyclone separator.

[0047] As a preferred embodiment, the control kiln is provided with a raised lining structure to prevent the material from passing through too quickly and to increase heat transfer efficiency. The control kiln is provided with a low thermal conductivity insulation material and a high temperature resistant working layer material to keep the surface temperature of the control kiln ≤ 150°C.

[0048] As a preferred embodiment, the cooling system comprises a heat recovery unit 9 and a cooling unit 10 connected in sequence. Hot material exiting the control kiln 6 enters the heat recovery unit 9 directly for cooling. The air outlet of the heat recovery unit 9 is connected to the lower portion of the activation furnace 2 via a tertiary air duct 14. The discharge port of the heat recovery unit 9 is connected to the cooling unit 10, which is then connected to the finished product transportation system. The air outlet of the cooling unit 10 is also connected to the hot blast furnace 3. The hot material exiting the control kiln 6 is sequentially cooled by the heat recovery unit 9 and the cooling unit 10. Under the action of the high-temperature fan 18 at the kiln tail, the high-temperature hot air exiting the heat recovery unit 9 is drawn as tertiary air to the activation furnace 2 for fuel combustion, with a temperature of 400-800°C. The low-temperature hot air exiting the cooling unit enters the hot blast furnace 2, with a temperature of 100-300°C. All the hot air is recycled, achieving efficient heat recovery and reducing system energy consumption.

[0049] As a preferred embodiment, the air outlet of the cooling unit 10 is connected to the dust collector 11, and the discharge port of the dust collector 11 is connected to the finished product transportation system. The air outlet of the dust collector 11 is connected to the waste heat recovery air duct 15 through the fan 12. The waste heat recovery air duct 15 is provided with a primary air branch pipe 16 and a secondary air branch pipe 17. The primary air branch pipe 16 is connected to the hot air furnace burner 4, and the secondary air branch pipe 17 is connected to the air inlet of the hot air furnace 3. The air after dust collection enters the hot air furnace 3 for use as primary air and secondary air.

[0050] The air exiting cooling unit 10 enters dust collector 11. The finished magnesium oxide b collected by cooling unit 10 and dust collector 11 enters a finished product transport system. In this embodiment, the finished product transport system comprises a finished product zipper machine 13. One stream of hot air exiting dust collector 11 enters hot blast furnace burner 4 as primary air, and the other stream enters hot blast furnace 2 as secondary air, thereby achieving efficient heat recovery and reducing system energy consumption.

[0051] As a preferred embodiment, the air outlet of the dust collector 11 is also connected to the waste heat utilization system or the exhaust gas treatment system through the fan 12, so that the residual air C leaving the dust collector 11 enters other waste heat utilization systems or exhaust gas treatment systems.

[0052] As a preferred embodiment, fans and valves are provided on the primary air branch pipe 16 and the secondary air branch pipe 17, and the temperature of the hot air out of the hot blast furnace 3 is controlled by adjusting the air volume of the secondary air. Since the temperature of the central flame generated by the combustion of the fuel is relatively high, if it directly contacts the magnesium oxide, it will lead to the inability to accurately control the overburning rate and greatly reduce the stability of the product. Therefore, in order to ensure the stability of the activity of the product, the fuel is fed into the hot blast furnace 3 through the hot blast furnace burner 4 along with the primary air. Under the combustion assistance and regulation of the secondary air, hot air with appropriate heat and air volume is generated to enter the control kiln 6 for the magnesium oxide to keep warm so that it loses some of its activity. The control kiln 6 rotates at a low speed of 0 to 2.5 r / min, so that the material moves slowly from the smoke chamber 7 to the discharge port of the kiln door cover 8. The temperature in the control kiln 6 is between 800-1100°C, and the residence time of the material in the control kiln 6 is 10 to 90 minutes.

[0053] As a preferred embodiment, the inlet air duct of the dust collector 11 is further provided with a cold air duct 19, which is equipped with a valve. When the air volume and temperature in the outlet air duct of the cooling unit 10 are high, especially higher than the temperature that the dust collector equipment can withstand, the valve can be used to adjust the volume of cooling air A entering the dust collector 11, further cooling the hot air and finished products exiting the cooling unit 10, thereby ensuring the safe and stable operation of the dust collector 11 and the finished product transportation system and other equipment.

[0054] Example 2

[0055] See also Figure 1 The present invention provides a calcination process for light-burned magnesium oxide with controllable activity, comprising the following steps:

[0056] S1: The magnesite a raw material ground to a suitable particle size is fed into the preheating system 1. The raw material undergoes multiple heat exchanges with the flue gas from the activation furnace 2 in the preheating system 1 to remove moisture. The material after multi-stage gas-solid heat exchange enters the activation furnace 2. An activation furnace burner 5 is provided at the lower part of the activation furnace 2. Fuel is sprayed into the activation furnace burner 5. The heat released by the combustion of the fuel is used to decompose and activate the material in the activation furnace 2. The outlet temperature of the activation furnace is 600-900°C, and a high-temperature light-burned magnesium oxide product is obtained with an active magnesium oxide content of ≥85%, and a large amount of flue gas is generated. The flue gas generated in the activation furnace 2 enters the preheating system 1 and exchanges heat with the raw material to become low-temperature flue gas, which is discharged through the air outlet of the preheating system 1.

[0057] S2: After the material activated in the activation furnace 2 is separated from the gas and solid by the final cyclone separator 101 of the preheating system 1, it enters the control kiln 6 for calcination. The hot air generated by the combustion of the fuel in the hot blast furnace 3 enters the control kiln 6 and provides a precise temperature to the control kiln, providing heat for calcination and insulation of the material. The material in the control kiln 6 is calcined at a constant temperature between 800-1100°C. The rotation speed of the control kiln 6 is 0-2.5 rpm, so that the material moves slowly from the smoke chamber 7 to the discharge port of the kiln door cover 8. The material stays in the control kiln 6 for 10-90 minutes, causing some of the active magnesium oxide to be over-burned and lose its activity, thereby accurately controlling the active magnesium oxide content and stabilizing it at a value between 50-70%. The hot material leaving the control kiln 6 enters the heat recovery unit 9 of the cooling system.

[0058] S3: Cooling air is introduced into the heat recovery unit 9 to exchange heat with the hot material. The air exiting the heat recovery unit 9 is used as tertiary air to enter the activation furnace 2 for fuel calcination, reducing system energy consumption. The tertiary air temperature is 400-800°C. The hot material exiting the heat recovery unit 9 enters the cooling unit 10 to exchange heat with the cooling air entering the cooling unit 10, and is further cooled to the required product temperature. The finished magnesium oxide b collected by the cooling unit 10 enters the finished zipper machine 13. The outlet air temperature of the cooling unit 10 is 100-300°C. The air exiting the cooling unit 10 enters the dust collector 11. The finished magnesium oxide b collected by the dust collector 11 enters the finished zipper machine 13.

[0059] S4: The hot air temperature at the outlet of dust collector 11 is less than 250°C. Part of the air exiting dust collector 11 is used as primary air to transport fuel to hot blast furnace burner 4, and part is used as secondary air to enter hot blast furnace 3. In addition to supporting combustion, the secondary air also regulates air temperature and protects the hot blast furnace walls, thereby achieving efficient heat recovery and utilization. The residual air C enters other waste heat utilization systems or exhaust gas treatment systems.

[0060] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some or all of the technical features therein, and these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A light-burned magnesium oxide calcining system with controllable activity, comprising a preheating system, an activation furnace, a control kiln, a hot blast furnace and a cooling system, wherein the preheating system, the activation furnace, the control kiln and the cooling system are connected in sequence, an activation furnace burner is provided on the activation furnace, a high-temperature recovery air outlet of the cooling system is connected to the activation furnace, a low-temperature recovery air outlet of the cooling system is connected to the hot blast furnace, a hot blast furnace burner is provided on the hot blast furnace, an air outlet of the hot blast furnace is connected to the control kiln, hot air generated by fuel combustion in the hot blast furnace enters the control kiln, the temperature in the control kiln is controlled to be maintained at a constant temperature, and the content of active magnesium oxide is stabilized at a constant value.

2. The activity-controlled light-burned magnesium oxide calcining system according to claim 1, characterized in that: A plurality of distribution valves are provided on the discharge pipe of the penultimate cyclone separator of the preheating system, so that the material enters the activation furnace at multiple points. The multiple distribution points control the temperature distribution in the activation furnace, so that the outlet temperature of the activation furnace is 600-900°C and the active magnesium oxide content out of the activation furnace is ≥85%.

3. The activity-controlled light-burned magnesium oxide calcining system according to claim 1, characterized in that: The temperature in the kiln is regulated to be within the range of 800-1100° C., the rotation speed of the kiln is regulated to be within the range of 0-2.5 r / min, the residence time of the materials in the kiln is regulated to be 10-90 min, and the active magnesium oxide content is regulated to be within the range of 50%-70%.

4. The activity-controlled light-burned magnesium oxide calcining system according to claim 1, characterized in that: The regulating kiln is provided with a lining structure with protrusions; the regulating kiln is provided with a heat insulating material with a low thermal conductivity coefficient and a high-temperature resistant working layer material, so that the surface temperature of the regulating kiln is ≤150°C.

5. The activity-controlled light-burned magnesium oxide calcining system according to claim 1, characterized in that: The cooling system comprises a heat recovery unit and a cooling unit connected in sequence, and the hot material leaving the control kiln directly enters the heat recovery unit for cooling, wherein the air outlet of the heat recovery unit is connected to the activation furnace, and the air outlet of the cooling unit is connected to the hot air furnace.

6. The activity-controlled light-burned magnesium oxide calcining system according to claim 5, characterized in that: The air temperature at the air outlet of the heat recovery unit is 400-800°C, and the air temperature at the air outlet of the cooling unit is 100-300°C.

7. The activity-controlled light-burned magnesium oxide calcining system according to claim 5, characterized in that: The air outlet of the cooling unit is connected to the dust collector, and the air outlet of the dust collector is connected to the waste heat recovery air duct through a fan. The waste heat recovery air duct is provided with a primary air branch pipe and a secondary air branch pipe. The primary air branch pipe is connected to the hot blast furnace burner, and the secondary air branch pipe is connected to the air inlet of the hot blast furnace. The air after dust collection is used as primary air and secondary air to enter the hot blast furnace.

8. The activity-controlled light-burned magnesium oxide calcining system according to claim 7, characterized in that: The primary air branch pipe and the secondary air branch pipe are both provided with fans and valves to adjust the air volume of the secondary air and control the temperature of the hot air leaving the hot air furnace.

9. The activity-controlled light-burned magnesium oxide calcining system according to claim 7, characterized in that: A cold air duct is provided on the inlet air duct of the dust collector, and a valve is provided on the cold air duct. The finished products collected by the dust collector enter the finished product transportation system.

10. The activity-controlled light-burned magnesium oxide calcining system according to claim 5, characterized in that: The discharge port of the cooling unit is connected to the finished product transportation system.

11. A process for calcining light-burned magnesia with controllable activity, the process being implemented based on the system for calcining light-burned magnesia with controllable activity according to any one of claims 1 to 10, characterized in that: The following steps are involved: S1: Magnesite ore is fed into the preheating system and undergoes multiple heat exchanges with the flue gas from the activation furnace to remove moisture. After undergoing multi-stage gas-solid heat exchange, the material enters the activation furnace, where magnesium carbonate is decomposed to produce light-burned magnesium oxide products, generating a large amount of flue gas. The activation furnace outlet temperature is controlled at 600-900°C, and the active magnesium oxide content is ≥85%. S2: After the material is activated in the activation furnace, it is separated into gas and solid by the final cyclone separator of the preheating system and then enters the control kiln for calcination. The hot air generated by burning fuel in the hot blast furnace enters the control kiln. The material is calcined at a constant temperature between 800-1100℃. The speed of the control kiln is 0-2.5rpm. The material stays in the control kiln for 10-90min. Some active magnesium oxide is overburned and loses its activity, so that the active magnesium oxide content is stabilized at a value between 50-70%. The hot material leaving the control kiln enters the cooling system; S3: Cooling air is introduced into the cooling system to exchange heat with the hot material. The high-temperature hot air after heat exchange is 400-800℃ and enters the activation furnace as tertiary air. The low-temperature hot air after heat exchange is 100-300℃ and enters the hot blast furnace. The hot air generated by the combustion of fuel in the hot blast furnace enters the regulating kiln.

12. The process for calcining light-burned magnesium oxide with controllable activity according to claim 11, characterized in that: After heat exchange, the low-temperature hot air passes through the dust collector to collect dust, and then enters the hot air furnace burner as primary air, and the other path enters the hot air furnace as secondary air, realizing efficient heat recovery and utilization.