A method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation

By combining gradient pyrolysis and melt oxidation, the problems of incomplete removal of organic matter and volatilization of inorganic salts in chemical waste salts have been solved, achieving complete harmless treatment and resource utilization of chemical waste salts.

CN120920480BActive Publication Date: 2026-11-17CHANGZHENG ENG
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202511216498.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-08-28
Publication Date
2026-11-17
Estimated Expiration
2045-08-28

AI Technical Summary

Technical Problem

Existing chemical waste salt treatment technologies cannot completely remove toxic and harmful organic substances. Inorganic salts are easily volatilized when heated at high temperatures, and the treatment methods are complex and prone to causing secondary pollution.

Method used

The gradient pyrolysis coupled with melt oxidation method is adopted. First, a temperature gradient is formed by heating from the bottom of the primary reactor to the top. The top layer of chemical waste salt is solid and the bottom layer is molten liquid. Then, oxidizing gas is introduced into the secondary reactor to carry out a deep oxidation reaction, so as to achieve complete removal of organic matter.

Benefits of technology

It effectively reduces the organic content in chemical waste salt, reduces the volatilization of inorganic salts, simplifies the treatment process, avoids secondary pollution, and promotes the resource utilization of recycled salt.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120920480B_ABST
    Figure CN120920480B_ABST
Patent Text Reader

Abstract

This invention discloses a method for treating chemical waste salt using gradient pyrolysis coupled with molten oxidation, belonging to the field of harmless treatment technology for chemical waste salt. The method provided by this invention includes: (1) gradient pyrolysis: placing the chemical waste salt in a primary reactor, and performing gradient pyrolysis from bottom to top using a bottom heat source inside the primary reactor, so that the top layer of the chemical waste salt remains solid while the bottom layer yields molten liquid waste salt; (2) molten oxidation: placing the molten liquid waste salt in a secondary reactor, controlling the reaction temperature by heating the secondary reactor, introducing oxidizing gas to carry out the reaction, and outputting molten regenerated salt. This invention solves the problems existing in the prior art, such as incomplete removal of organic matter from chemical waste salt, large volatilization of inorganic salts due to high-temperature heating, complex disposal methods, and easy secondary pollution. It can achieve thorough harmless treatment of chemical waste salt, promote the secondary utilization of regenerated salt, and help promote its industrialization and marketization.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of harmless treatment technology for chemical waste salt, and in particular to a method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation. Background Technology

[0002] In the chemical industry, including pesticides, pharmaceuticals, fine chemicals, and coal chemicals, large quantities of industrial waste salt are generated due to processes and raw materials used in production. This waste salt is rich in various toxic and harmful organic compounds and impurities. Most enterprises dispose of it through landfill, resulting in land occupation and pollution of the surrounding environment, posing a significant threat to the ecological environment. With increasing public awareness of the hazards of industrial waste and the strengthening of national management of hazardous industrial waste, the harmless treatment of industrial waste salt has become an urgent need for chemical enterprises. Currently, the main technologies for the harmless treatment of chemical waste salt include the following four:

[0003] (1) Pyrolysis treatment: This method utilizes a high-temperature environment (typically 400–800℃) to thermochemically decompose organic pollutants in waste salt while maintaining the stability of inorganic salt components, thus separating organic pollutants from inorganic salts. This technology solves the problem of organic pollution while preserving the resource value of inorganic salts. However, the heating temperature is relatively low, resulting in poor treatment of non-volatile and non-pyrolytic organic matter. Different heating methods may lead to uneven heat distribution and localized overheating and agglomeration of chemical waste salts.

[0004] (2) High-temperature incineration method, which uses high-temperature incineration (usually above 800℃) to decompose the organic matter in chemical waste salt, and promote the separation of organic pollutants from inorganic products. This method has high treatment efficiency and good product purity, but the high temperature can easily cause serious volatilization of waste salt, making it difficult to recover. Molten waste salt is easy to stick to the surface of equipment, causing corrosion and affecting normal operation. Indirect heat exchange heating method often results in complex system and high investment and operating costs.

[0005] (3) Membrane separation method: This method uses a filter membrane to filter organic matter and impurities from industrial wastewater. After concentration or evaporation and crystallization, waste salt is obtained, which reduces the content of toxic and harmful substances in the waste salt. However, due to the limited filtration efficiency, the waste salt produced may not meet national environmental protection requirements or resource reuse requirements. Continuing to carry out secondary harmless treatment leads to complex processes and increased investment and operating costs.

[0006] (4) Washing method, which uses water or chemical detergents to dissolve chemical waste salt, neutralize and wash away organic matter and impurities in the waste salt. It is suitable for chemical waste salt with simple organic composition and low content. In addition, the liquid after washing may contain toxic and harmful organic matter or secondary pollutants, which still need to be further treated to render it harmless, making the disposal process complicated and limiting its industrial application.

[0007] Patent application CN117299755A discloses an energy-saving method for the melt oxidation and detoxification of waste salt. Specifically, it involves mixing pharmaceutical waste salt with fuel gas and introducing it into a melt oxidation and detoxification device. A combined fuel gas and electrically assisted heating method is used, employing multi-stage combustion and melt oxidation to fully detoxify the waste salt. The molten product is then water-quenched and recrystallized to obtain high-purity salt. However, the buffer plate design in the melt oxidation and detoxification device increases the risk of waste salt adhesion and blockage, and the resistance wire of the electrically assisted heating structure is prone to corrosion and damage due to prolonged exposure to the molten salt environment. Patent CN109882854B discloses a method for the harmless treatment of industrial waste salt slag using high-temperature pyrolysis with suspension incineration technology. The carbonization temperature and method are selected based on the critical softening point and critical carbonization point of different salt slags to avoid softening of the waste salt and equipment adhesion caused by high temperatures. The treatment process includes at least four cycles of high-temperature suspension pyrolysis at temperatures ranging from 200 to 600°C, with the temperature increasing sequentially with the number of cycles. This treatment method sets the qualification standard as a COD value of less than 150 ppm after the obtained product is diluted into a 20% aqueous solution. The high COD residue does not meet the standards for recycled industrial salt. Patent application CN111790731A discloses an industrial waste salt conversion device and method. Waste salt raw material enters the feed desorption furnace via a desorption conveyor. In the multi-stage reaction chamber of the feed desorption furnace, organic matter and inorganic salts in the waste salt raw material are separated. The resulting purified waste salt is mixed with additives and enters the waste salt conversion furnace, where it interacts with self-circulating particles and hot fluid, undergoing a series of highly efficient thermal melting conversion reactions to generate a stable solid product. The operating pressure of the feed desorption furnace is 0–1000 kPa, and the operating temperature is 300–1000 °C. The operating pressure of the waste salt conversion furnace is 0–1000 kPa, and the operating temperature is 1000–1500 °C. This technology has a high degree of integration and a complex system, requiring auxiliary agents and other aids for the conversion of organic matter. Patent CN106914474B provides a process and equipment for the graded decomposition, carbonization, and harmless treatment of industrial waste salt. This process uses a multi-stage decomposition and carbonization furnace to grade and carbonize industrial waste salt, with a temperature setting range of 400–800℃. The critical carbonization temperature of each stage of the decomposition and carbonization furnace is determined based on the melting point of the industrial waste salt and the different carbonization points of the various organic compounds it contains. The decomposition and carbonization furnace uses a hot airflow heating method, achieving dynamic heat exchange within the furnace. However, the high-temperature residence time of industrial waste salt is relatively short, limiting its efficiency in treating non-volatile, high-boiling-point organic compounds.

[0008] In summary, current mature technologies for the detoxification and harmless treatment of chemical waste salts are still insufficient to meet the market demand for clean and efficient treatment of chemical waste salts. Summary of the Invention

[0009] The purpose of this invention is to provide a method for treating chemical waste salt by gradient pyrolysis coupled with molten oxidation, so as to at least solve the problems existing in the prior art, such as incomplete removal of toxic and harmful organic matter in chemical waste salt, large volatilization of inorganic salts when chemical waste salt is heated at high temperature, and complex disposal methods for chemical waste salt that are prone to secondary pollution.

[0010] To achieve the above objectives, the present invention provides a method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation, comprising the following steps:

[0011] (1) Gradient pyrolysis: Chemical waste salt is placed in a primary reactor and subjected to gradient pyrolysis from bottom to top through a heat source at the bottom of the primary reactor, so that the top layer of chemical waste salt remains in a solid state and the bottom layer is molten liquid waste salt.

[0012] (2) Molten oxidation: The molten liquid waste salt is placed in a secondary reactor. The reaction temperature is controlled by heating the secondary reactor. Oxidizing gas is introduced to carry out the reaction and molten regenerated salt is output.

[0013] In step (1) of this application, the working principle of gradient pyrolysis is to use the bottom of the primary reactor as the heat source, and heat the chemical waste salt from bottom to top through heat conduction and heat radiation. A cold top layer is formed on the top of the chemical waste salt, and the bottom layer is molten liquid waste salt. This can avoid the large-scale volatilization of inorganic salts, and at the same time, gradient pyrolysis reduces the content of organic matter in the chemical waste salt.

[0014] Optionally, in step (1), the chemical waste salt includes inorganic salts and organic pollutants;

[0015] The inorganic salts include sodium chloride and / or sodium sulfate;

[0016] The agglomerated particle size of the chemical waste salt is ≤100mm;

[0017] The moisture content of the chemical waste salt is ≤5%;

[0018] The organic pollutant content of the chemical waste salt is expressed as TOC, and the TOC content is 3000-200000 mg / kg.

[0019] Optionally, in step (1), the TOC content of the chemical waste salt is independently selected from any value or a range between any two of the following: 3000 mg / kg, 5000 mg / kg, 10000 mg / kg, 20000 mg / kg, 30000 mg / kg, 40000 mg / kg, 50000 mg / kg, 60000 mg / kg, 70000 mg / kg, 80000 mg / kg, 90000 mg / kg, 100000 mg / kg, 150000 mg / kg, and 200000 mg / kg.

[0020] Optionally, in step (1), the chemical waste salt is placed in the primary reactor in a flat layer with a thickness of x centimeters to ensure that the bottom layer of chemical waste salt is molten liquid waste salt and the top layer is solid. T1 represents the temperature of the bottom heat source, and T0 represents the melting point of the chemical waste salt.

[0021] In step (1) of this application, in order to satisfy the formation of a temperature gradient layer by pyrolysis of chemical waste salt, the thickness of the chemical waste salt is determined by the temperature T1 of the bottom heat source and the melting point T0 of the chemical waste salt.

[0022] Optionally, in step (1), the density of the bottom heat source is greater than the density of the chemical waste salt. Due to the influence of density and viscosity, the chemical waste salt and the bottom heat source are in a natural stratified state of upper and lower layers.

[0023] The temperature of the bottom heat source is 950–1300°C;

[0024] The solubility of the molten liquid waste salt in 100g of bottom heat source is less than 0.1g;

[0025] The bottom heat source includes molten glass, and the viscosity-temperature curve of the molten glass satisfies a viscosity ≥ 1 Pa·s at 1300℃. The selected heat source satisfies the requirement of continuously providing sufficient heat, has low solubility for waste salt, and a density higher than that of waste salt to form a stratified state. The viscosity can limit the settling of salt particles; the higher the viscosity, the slower the particles settle.

[0026] Optionally, in step (1), the temperature of the bottom heat source is independently selected from any value of 950°C, 1000°C, 1100°C, 1200°C, 1300°C or any range between two of them.

[0027] In this application, when the main component of the inorganic salt in the waste salt is sodium sulfate, its theoretical melting point is 884℃. Considering the need for heat dissipation during the heating process, if the bottom heat source temperature is lower than 900℃, it may not meet the requirement of heating to melting, and the melting rate will be too slow, which is not conducive to the realization. When the bottom heat source temperature is too high (above 1300℃), the viscosity of the bottom glass further decreases, and the upper solid layer is prone to sedimentation, reducing the stratification effect. At the same time, due to the high heating temperature and fast heat exchange rate, in order to ensure the stable existence of the top solid layer, the layer thickness is relatively thick and the mass is large, which further promotes sedimentation. Some of the molten glass may be higher than the overflow port of the waste salt molten salt, resulting in accidental discharge.

[0028] Optionally, in step (1), the primary reactor is provided with an overflow port, which is flush with the bottom plane of the chemical waste salt in the primary reactor. The molten liquid waste salt leaves the primary reactor by overflow, ensuring that the average residence time of the molten liquid waste salt in the primary reactor is ≤1min.

[0029] In the primary reactor of step (1) of this application, by adjusting the thickness of the spread layer, the TOC removal rate can reach more than 80% of the TOC content of the pretreated waste salt. If the removal rate is less than 80%, this method can still be used, but the residence time and oxidizing gas flow rate need to be increased in the secondary reactor.

[0030] Optionally, in step (2), the heating method is top heating;

[0031] The top heating is performed using a thermocouple or resistance wire;

[0032] The heating temperature is 950–1100°C.

[0033] In step (2) of this application, top heating is used to maintain the reaction temperature through radiation heat exchange, ensuring that the molten waste salt is always in a molten state; at the same time, oxidizing gas is added to fully mix and contact with the molten salt, and the organic matter contained therein undergoes an oxidation-reduction reaction to achieve deep removal of organic matter.

[0034] Optionally, in step (2), the oxidizing gas includes a single gas and / or air;

[0035] The single gas includes carbon dioxide and / or oxygen;

[0036] The purity of both the carbon dioxide and oxygen is 99%.

[0037] The oxidizing gas is directly introduced into the molten liquid waste salt;

[0038] The temperature of the oxidizing gas is 900–1300°C;

[0039] When the TOC removal rate of the primary reactor is ≥80%, the flow rate of the oxidizing gas is 1 to 10 times the oxygen required for the complete removal of residual TOC from the molten liquid waste salt; when the TOC removal rate of the primary reactor is <80%, the flow rate of the oxidizing gas is 2 to 10 times the oxygen required for the complete removal of residual TOC from the molten liquid waste salt.

[0040] In step (2) of this application, the purpose of introducing oxidizing gas is to stir and provide oxidant.

[0041] Optionally, in step (2), the temperature of the oxidizing gas is independently selected from any value of 900℃, 950℃, 1000℃, 1100℃, 1200℃, 1300℃ or any range between two of them.

[0042] In this application, the oxidizing gas enters the secondary reactor and reacts simultaneously with the molten waste salt through heat exchange. The temperature range of the oxidizing gas is controlled between 900 and 1300°C. If the gas temperature is too low, the waste salt may solidify, reducing the reaction rate and affecting the stability of the experiment. If the gas temperature is too high, the heat exchange between the gas and the liquid can easily cause the overall temperature of the molten waste salt pool to rise, increasing the amount of molten salt volatilization. Since the gas is heated through heat exchange during the solidification of the waste salt, the higher the gas temperature, the higher the heat exchange requirements and the greater the difficulty in achieving this.

[0043] In step (2) of this application, the residence time of molten liquid waste salt in the secondary reactor is determined by the TOC removal rate of the molten liquid waste salt after treatment in the primary reactor, and the flow rate of oxidizing gas is determined by the TOC removal rate and the residual TOC value of the molten liquid waste salt after treatment in the primary reactor.

[0044] Optionally, in step (2), the secondary reactor is provided with three molten salt outlets, which are divided into the first outlet, the second outlet, and the third outlet according to their height in the secondary reactor from low to high.

[0045] The vertical distance between the first discharge outlet and the bottom of the secondary reactor is 100-600 mm, the vertical distance between the first discharge outlet and the second discharge outlet is 100-600 mm, and the vertical distance between the second discharge outlet and the third discharge outlet is 100-600 mm.

[0046] After the reaction, the residence time of the molten liquid waste salt in the secondary reactor is controlled by the three molten salt outlets. When the TOC removal rate of the primary reactor is >90%, the first outlet is selected; when 80% ≤ TOC removal rate of the primary reactor is ≤90%, the second outlet is selected; and when the TOC removal rate of the primary reactor is <80%, the third outlet is selected.

[0047] Optionally, the pressure of the primary reactor in step (1) and the secondary reactor in step (2) are the same, and the pressure is a slight negative pressure, the range of which is -1 to 0 kPa.

[0048] Optionally, the pressure of the primary reactor in step (1) and the secondary reactor in step (2) are the same, and the pressure is slightly negative. The range of the slightly negative pressure is independently selected from any value or any range between -1kPa, -0.8kPa, -0.6kPa, -0.5kPa, -0.4kPa, -0.2kPa, and 0kPa.

[0049] Optionally, it also includes (3) a post-processing step: the gas generated by the primary reactor and the secondary reactor is transported to the downstream flue gas treatment unit for treatment, and the molten regenerated salt is cooled, heat exchanged, crushed and ground to obtain the regenerated salt product;

[0050] The cooling and heat exchange involves passing the molten regenerated salt through a first heat exchanger to reduce its temperature to 150-250°C. The water in the first heat exchanger carries away the heat, and the water and the oxidizing gas are further heated through a second heat exchanger, with the water temperature dropping to 60°C.

[0051] The recycled salt product meets the requirements of TOC ≤ 10 mg / kg and average particle size ≤ 5 mm.

[0052] In this application, the oxidizing gas is heated indirectly by exchanging heat with the molten liquid waste salt flowing out of the secondary reactor, thereby improving the heat utilization rate.

[0053] Compared with the prior art, the present invention has at least the following advantages:

[0054] (1) This invention employs a gradient pyrolysis coupled with melt oxidation method for treating chemical waste salt, which can completely remove toxic and harmful organic matter from chemical waste salt. Gradient pyrolysis is the primary detoxification process, where the chemical waste salt is mainly solid; melt oxidation is the deep detoxification process, where the chemical waste salt is molten liquid. The connection between the pyrolysis and melt oxidation processes relies on the bottom-up heating of the chemical waste salt during pyrolysis to form a gradient pyrolysis. After the temperature rises to the melting point of the chemical waste salt, it overflows from the primary reactor and enters the melt oxidation process in the secondary reactor. This method has excellent organic matter removal effect and is suitable for various chemical waste salts, especially those with high organic matter content, high volatility, and difficulty in pyrolysis. It can achieve the complete harmless disposal of chemical waste salt and promote the secondary utilization of recycled salt.

[0055] (2) The present invention uses the bottom heat source of the furnace body of the primary reactor to heat the waste salt. The chemical waste salt is heated from bottom to top through heat conduction and heat radiation. Solid waste salt is always present at the top layer, which avoids the problem of large amount of waste salt volatilization and difficulty in waste gas treatment caused by flame heating. At the same time, it overcomes the difficulty of high corrosion resistance requirements of equipment materials for gas heat exchange heating.

[0056] (3) This invention has no special catalysts or additives, is low in cost, and has a simple, quick and easy technical method with strong operability. The disposal process does not cause secondary pollution, which helps to promote its industrialization and marketization. Attached Figure Description

[0057] Figure 1 This is a flowchart of the method for treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to the present invention.

[0058] Figure 2 This is a schematic diagram of the structure of the primary reactor and the secondary reactor of the present invention. Detailed Implementation

[0059] To enable those skilled in the art to better understand the present invention, the technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of the present invention.

[0060] It should be noted that the terms "first," "second," etc., in the specification, claims, and accompanying drawings of this invention are used to distinguish similar objects and are not necessarily used to describe a specific order or sequence. It should be understood that such data can be used interchangeably where appropriate to understand the embodiments of the invention described herein. Furthermore, the terms "comprising" and "having," and any variations thereof, are intended to cover non-exclusive inclusion; for example, a product or device comprising a series of units is not necessarily limited to those explicitly listed, but may include other units not explicitly listed or inherent to such product or device.

[0061] In this invention, the terms "upper," "lower," "left," "right," "front," "rear," "top," "bottom," "inner," "outer," "middle," "vertical," "horizontal," "lateral," and "longitudinal" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. These terms are primarily for the purpose of better describing the invention and its embodiments, and are not intended to limit the indicated devices, elements, or components to having a specific orientation, or to be constructed and operated in a specific orientation.

[0062] Furthermore, some of the aforementioned terms, besides indicating direction or positional relationships, may also have other meanings. For example, the term "above" may, in certain circumstances, indicate a dependency or connection. Those skilled in the art can understand the specific meaning of these terms in this invention based on the specific circumstances.

[0063] Furthermore, the terms "installation," "setup," "equipped with," "connection," "linking," and "socketing" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral structure; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium, or an internal connection between two devices, components, or parts. Those skilled in the art can understand the specific meaning of these terms in this invention based on the specific circumstances.

[0064] It should be noted that, unless otherwise specified, the embodiments and features described in the present invention can be combined with each other. The present invention will now be described in detail with reference to the accompanying drawings and embodiments.

[0065] Example 1

[0066] A method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation ( Figure 1 The flowchart of the method of the present invention is as follows:

[0067] (1) Pretreatment: Chemical waste salt is crushed and dried to obtain chemical waste salt raw material with a moisture content of 5%, a maximum agglomeration particle size of 100 mm, a TOC content of 106000 mg / kg, and a melting point of 800℃.

[0068] (2) Gradient pyrolysis: Chemical waste salt that meets the pretreatment conditions is spread evenly in a primary reactor equipped with a heat source at the bottom of the furnace body (see the structural diagram of the primary reactor). Figure 2 In this process, the bottom heat source is electrically charged molten glass with a viscosity-temperature curve that satisfies a viscosity of 2 Pa·s at 1300℃. The temperature of the bottom heat source is controlled at 950℃ (viscosity of 7 Pa·s). The density of the bottom heat source is greater than that of the chemical waste salt. Due to the influence of density and viscosity, the two are naturally stratified. The bottom heat source heats the chemical waste salt from bottom to top through thermal radiation and heat conduction, forming a temperature gradient pyrolysis. The top layer consists of cold-topped solid particles, and the bottom layer consists of molten liquid waste salt, with an average thickness of 50 cm and a pressure of slightly negative pressure -1 kPa. After the molten liquid waste salt is formed, its average residence time in the primary reactor is 1 minute. It flows out of the primary reactor through the overflow port (which is flush with the bottom plane of the chemical waste salt in the primary reactor) and enters the secondary reactor (see the structural diagram of the secondary reactor). Figure 2 The TOC removal rate of molten waste salt was 75%.

[0069] (3) Molten Oxidation: After the molten liquid waste salt enters the secondary reactor, the reaction temperature is controlled at 950℃ by a heating device (resistance wire) at the top of the secondary reactor. A high-temperature oxidizing gas (99% pure oxygen) is directly introduced into the molten liquid waste salt. The temperature of the high-temperature oxidizing gas is 900℃, and the flow rate of the oxidizing gas is 0.04 Nm³. 3 / s, allowing the molten salt and oxidizing gas to mix and come into contact fully, causing the contained organic matter to undergo an oxidation-reduction reaction, with a slight negative pressure of -1kPa, using the third exhaust outlet;

[0070] (4) Post-treatment: The gas generated by the primary reactor and the secondary reactor is transported to the downstream flue gas treatment unit for treatment. The molten waste salt liquid is cooled and heat exchanged, crushed and ground to a regenerated salt product with an average particle size of 5mm. At the same time, the heat of the molten salt cooling is recovered to heat the oxidizing gas to 900℃.

[0071] Example 2

[0072] A method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation ( Figure 1The flowchart of the method of the present invention is as follows:

[0073] (1) Pretreatment: Chemical waste salt is crushed and dried to obtain chemical waste salt raw material with a moisture content of 3%, a maximum agglomeration particle size of 90 mm, a TOC content of 24600 mg / kg, and a melting point of 820℃.

[0074] (2) Gradient pyrolysis: Chemical waste salt that meets the pretreatment conditions is spread evenly in a primary reactor equipped with a heat source at the bottom of the furnace body (see structural diagram). Figure 2 In this process, the bottom heat source is electrically charged molten glass with a viscosity-temperature curve that satisfies a viscosity of 2 Pa·s at 1300℃. The temperature of the bottom heat source is controlled at 1050℃. The density of the bottom heat source is greater than that of the chemical waste salt. Due to the influence of density and viscosity, the two naturally stratify. The bottom heat source heats the chemical waste salt from bottom to top through thermal radiation and conduction, forming a temperature gradient pyrolysis. The top layer consists of cold-topped solid particles, and the bottom layer is molten liquid waste salt, with an average thickness of 35 cm and a pressure of -0.5 kPa (slight negative pressure). After the molten liquid waste salt is formed, its average residence time in the primary reactor is 1 minute. It flows out of the primary reactor through the overflow port (which is flush with the bottom plane of the chemical waste salt in the primary reactor) and enters the secondary reactor. The TOC removal rate of the molten waste salt is 82%.

[0075] (3) Molten Oxidation: After the molten liquid waste salt enters the secondary reactor, the reaction temperature is controlled at 1000℃ by a heating device (thermocouple) at the top of the secondary reactor. A high-temperature oxidizing gas (air) is directly introduced into the molten liquid waste salt. The temperature of the high-temperature oxidizing gas is 1000℃, and the flow rate of the oxidizing gas is 0.016 Nm³. 3 / s, allowing the molten salt and oxidizing gas to mix and come into contact fully, causing the contained organic matter to undergo an oxidation-reduction reaction. The pressure is a slight negative pressure of -0.5kPa, and the second exhaust port is used.

[0076] (4) Post-treatment: The gas generated by the primary reactor and the secondary reactor is transported to the downstream flue gas treatment unit for treatment. The molten waste salt liquid is cooled and heat exchanged, crushed and ground to a regenerated salt product with an average particle size of 5mm. At the same time, the heat of molten salt cooling is recovered to heat the oxidizing gas.

[0077] Example 3

[0078] A method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation ( Figure 1 The flowchart of the method of the present invention is as follows:

[0079] (1) Pretreatment: Chemical waste salt is crushed and dried to obtain chemical waste salt raw material with a moisture content of 2%, a maximum agglomeration particle size of 100mm, a TOC content of 9800mg / kg, and a melting point of 800℃.

[0080] (2) Gradient pyrolysis: Chemical waste salt that meets the pretreatment conditions is spread evenly in a primary reactor equipped with a heat source at the bottom of the furnace body (see structural diagram). Figure 2 In this process, the bottom heat source is molten glass, whose viscosity-temperature curve satisfies a viscosity of 2 Pa·s at 1300℃. The temperature of the bottom heat source is controlled at 1300℃. The density of the bottom heat source is greater than that of the chemical waste salt. Due to the influence of density and viscosity, the two are naturally stratified. The bottom heat source heats the chemical waste salt from bottom to top through thermal radiation and heat conduction, forming a temperature gradient pyrolysis. The top layer consists of cold-top solid particles, and the bottom layer consists of molten liquid waste salt, with an average thickness of 40 cm and a pressure of -0.2 kPa. After the molten liquid waste salt is formed, its average residence time in the primary reactor is 1 minute. It flows out of the primary reactor through the overflow port (which is flush with the bottom plane of the chemical waste salt in the primary reactor) and enters the secondary reactor. The TOC removal rate of the molten waste salt is 90%.

[0081] (3) Molten Oxidation: After the molten liquid waste salt enters the secondary reactor, the reaction temperature is controlled at 1100℃ by a heating device (thermocouple) at the top of the secondary reactor. A high-temperature oxidizing gas (air) is directly introduced into the molten liquid waste salt. The temperature of the high-temperature oxidizing gas is 1300℃, and the flow rate of the oxidizing gas is 0.0036 Nm³. 3 / s, allowing the molten salt and oxidizing gas to mix and come into contact fully, causing the contained organic matter to undergo an oxidation-reduction reaction, with a slight negative pressure of -0.2kPa, using the first discharge outlet;

[0082] (4) Post-treatment: The gas generated by the primary reactor and the secondary reactor is transported to the downstream flue gas treatment unit for treatment. The molten waste salt liquid is cooled and heat exchanged, crushed and ground to a regenerated salt product with an average particle size of 5mm. At the same time, the heat of molten salt cooling is recovered to heat the oxidizing gas.

[0083] Comparative Example 1

[0084] The specific steps for treating chemical waste salt using only gradient pyrolysis are as follows:

[0085] (1) Pretreatment: Take chemical waste salt and dry and crush it to obtain chemical waste salt raw material with a moisture content of 2%, a maximum agglomeration particle size of 100mm, a TOC content of 9800mg / kg, and a melting point of 800℃.

[0086] (2) Gradient pyrolysis: Chemical waste salt that meets the pretreatment conditions is spread evenly in a primary reactor equipped with a heat source at the bottom of the furnace body (see structural diagram). Figure 2In this process, the bottom heat source is molten glass, whose viscosity-temperature curve satisfies a viscosity of 2 Pa·s at 1300℃. The temperature of the bottom heat source is controlled at 1300℃. The density of the bottom heat source is greater than that of the chemical waste salt. Due to the influence of density and viscosity, the two are naturally stratified. The bottom heat source heats the chemical waste salt from bottom to top through thermal radiation and heat conduction, forming a temperature gradient pyrolysis. The top layer consists of cold-top solid particles, and the bottom layer consists of molten liquid waste salt, with a thickness of 40 cm and a pressure of -0.2 kPa. After the molten liquid waste salt is formed, its average residence time in the primary reactor is 1 minute. It then flows out of the primary reactor through the overflow port (which is flush with the bottom plane of the chemical waste salt in the primary reactor) and enters the post-treatment process.

[0087] (3) Post-processing: The gas generated by the primary reactor is transported to the downstream flue gas treatment unit for treatment. The molten waste salt liquid is cooled and heat exchanged, crushed and ground to a recycled salt product with an average particle size of 5mm.

[0088] Comparative Example 2

[0089] The specific steps for treating chemical waste salt using only the melt oxidation method are as follows:

[0090] (1) Pretreatment: Take chemical waste salt and dry and crush it to obtain chemical waste salt raw material with a moisture content of 2%, a maximum agglomeration particle size of 100mm, a TOC content of 9800mg / kg, and a melting point of 800℃.

[0091] (2) Molten Oxidation: Disconnect the overflow ports of the primary and secondary reactors, and directly feed the waste salt solids through the overflow ports. The reaction temperature is controlled at 1100℃ by the heating device (thermocouple) at the top of the secondary reactor. High-temperature oxidizing gas (air) is directly introduced into the molten liquid waste salt. The temperature of the high-temperature oxidizing gas is 1300℃, and the flow rate of the oxidizing gas is 0.036 Nm³. 3 / s (Since this comparative example does not have a gradient pyrolysis process, the TOC of the waste salt entering the furnace is 9800 mg / kg, while in Example 3, when it enters the molten oxidation process, the TOC of the waste salt is only 980 mg / kg. Therefore, the oxygen demand of this comparative example is 10 times that of Example 3), so that the molten salt and the oxidizing gas are fully mixed and contacted, and the contained organic matter undergoes an oxidation-reduction reaction. The pressure is a slight negative pressure of -0.2 kPa, and the third exhaust port is used.

[0092] (3) Post-processing: The gas generated by the secondary reactor is transported to the downstream flue gas treatment unit for treatment. The molten waste salt liquid is cooled and heat exchanged, crushed and ground to a recycled salt product with an average particle size of 5mm.

[0093] Comparative Example 3

[0094] The specific steps for treating chemical waste salt using flame heating are as follows:

[0095] (1) Pretreatment: Take chemical waste salt and dry and crush it to obtain chemical waste salt raw material with a moisture content of 2%, a maximum agglomeration particle size of 100mm, a TOC content of 9800mg / kg, and a melting point of 800℃.

[0096] (2) Flame heating treatment: Waste salt is added to a rotary kiln incinerator for treatment. The kiln head is equipped with a flame heating device with a temperature set at 1300℃. High-temperature oxidizing gas (air) is introduced into the kiln at a temperature of 1300℃ and a flow rate of 0.036 Nm³. 3 / s, the organic matter contained therein undergoes a redox reaction, and the pressure is atmospheric pressure;

[0097] (3) Post-processing: The gas generated by the rotary kiln is transported to the downstream flue gas treatment unit for treatment. After the molten waste salt liquid flows out, it is cooled and heat exchanged, crushed and ground to a recycled salt product with an average particle size of 5mm.

[0098] Experimental Example 1

[0099] The TOC content of the regenerated salt products obtained in Examples 1-3 and Comparative Examples 1-7 was tested, and their salt volatilization rate was determined. The results are shown in Table 1.

[0100] Table 1 Comparison of experimental results

[0101] Grouping TOC content (mg / kg) Salt evaporation rate (%) Example 1 10 30.4 Example 2 8 32.8 Example 3 5 36 Comparative Example 1 326 14.4 Comparative Example 2 45 56.3 Comparative Example 3 105 78.9

[0102] As shown in Table 1, compared with the comparative example, the regenerated salt product obtained by the method of the present invention has a lower TOC content and a lower salt volatilization rate. Although the salt volatilization rate of Comparative Example 1 is lower than that of the present invention, its TOC content is much higher than that of the embodiments of the present invention. In summary, the product of the present invention has significant advantages in removing organic matter, reducing salt volatilization rate, and requiring no special catalysts or additives. The present invention can be widely applied to the harmless treatment of by-product waste salts in chemical industries such as pesticides, pharmaceuticals, fine chemicals, and coal chemicals.

[0103] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them. Those skilled in the art should understand that modifications can be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method of gradient pyrolysis coupled with molten oxidation treatment of chemical waste salts, characterized by, Includes the following steps: (1) Gradient pyrolysis: Chemical waste salt is placed in a primary reactor and subjected to gradient pyrolysis from bottom to top through the bottom heat source inside the primary reactor, so that the top layer of chemical waste salt remains in a solid state and the bottom layer is molten liquid waste salt. (2) Molten oxidation: The molten liquid waste salt is placed in a secondary reactor, the reaction temperature is controlled by heating the secondary reactor, an oxidizing gas is introduced to carry out the reaction, and molten regenerated salt is output; In step (2), the secondary reactor is provided with three molten salt outlets, which are divided into the first outlet, the second outlet, and the third outlet according to their height in the secondary reactor from low to high. The vertical distance between the first discharge outlet and the bottom of the secondary reactor is 100~600mm, the vertical distance between the first discharge outlet and the second discharge outlet is 100~600mm, and the vertical distance between the second discharge outlet and the third discharge outlet is 100~600mm. After the reaction, the residence time of the molten liquid waste salt in the secondary reactor is controlled by the three molten salt outlets. When the TOC removal rate of the primary reactor is >90%, the first outlet is selected; when 80% ≤ TOC removal rate of the primary reactor ≤ 90%, the second outlet is selected; and when the TOC removal rate of the primary reactor is <80%, the third outlet is selected.

2. The method for treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, In step (1), the chemical waste salt includes inorganic salts and organic pollutants; The inorganic salts include sodium chloride and / or sodium sulfate; The agglomerated particle size of the chemical waste salt is ≤100mm; The moisture content of the chemical waste salt is ≤5%; The organic pollutant content of the chemical waste salt is expressed as TOC, and the TOC content is 3000~200000 mg / kg.

3. The method for treating chemical waste salt by gradient pyrolysis coupled with melt oxidation according to claim 1, characterized in that, In step (1), the chemical waste salt is placed in the primary reactor in a flat manner, and the thickness of the flat placement is set as x cm to ensure that the bottom layer of the chemical waste salt is a molten liquid waste salt and the top layer is in a solid state, wherein 10 ≤ x ≤ 50 × T1, T0 represents the melting point of the chemical waste salt.

4. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, In step (1), the density of the bottom heat source is greater than the density of the chemical waste salt, and the chemical waste salt and the bottom heat source are in a natural stratified state of upper and lower layers; The temperature of the bottom heat source is 950~1300℃; The solubility of the molten liquid waste salt in 100g of bottom heat source is less than 0.1g; The bottom heat source includes molten glass, and the viscosity-temperature curve of the molten glass satisfies a viscosity ≥ 1 Pa·s at 1300℃.

5. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, In step (1), the primary reactor is provided with an overflow port, which is flush with the bottom plane of the chemical waste salt in the primary reactor. The molten liquid waste salt leaves the primary reactor by overflow, ensuring that the average residence time of the molten liquid waste salt in the primary reactor is ≤1min.

6. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, In step (2), the heating method is top heating; The top heating is performed using a thermocouple or resistance wire; The heating temperature is 950~1100℃.

7. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, In step (2), the oxidizing gas includes a single gas and / or air; The single gas includes carbon dioxide and / or oxygen; The purity of both the carbon dioxide and oxygen is 99%. The oxidizing gas is directly introduced into the molten liquid waste salt; The temperature of the oxidizing gas is 900~1300℃; When the TOC removal rate of the primary reactor is ≥80%, the flow rate of the oxidizing gas is 1 to 10 times the oxygen required for the complete removal of residual TOC from the molten liquid waste salt; when the TOC removal rate of the primary reactor is <80%, the flow rate of the oxidizing gas is 2 to 10 times the oxygen required for the complete removal of residual TOC from the molten liquid waste salt.

8. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, The pressure of the primary reactor in step (1) is the same as that of the secondary reactor in step (2), and the pressure is slightly negative, with the range of slightly negative pressure being -1 to 0 kPa.

9. The method of treating chemical waste salt by gradient pyrolysis coupled with molten oxidation according to claim 1, characterized in that, It also includes (3) post-processing steps: the gas generated by the primary reactor and the secondary reactor is transported to the downstream flue gas treatment unit for treatment, and the molten regenerated salt is cooled, heat exchanged, crushed and ground to obtain the regenerated salt product; The cooling and heat exchange involves passing the molten regenerated salt through a first heat exchanger to reduce its temperature to 150-250°C. The water in the first heat exchanger carries away the heat, and the water and the oxidizing gas further exchange heat through a second heat exchanger to heat the oxidizing gas, with the water temperature dropping to 60°C. The recycled salt product meets the requirements of TOC ≤ 10 mg / kg and average particle size ≤ 5 mm.

Citation Information

Patent Citations

  • A process and equipment for the graded decomposition, carbonization, and harmless treatment of industrial waste salt.

    CN106914474B

  • A method for harmlessly treating industrial waste salt residue using high-temperature pyrolysis via suspension incineration technology.

    CN109882854B

  • Industrial waste salt converting device and method

    CN111790731A

  • Energy-saving waste salt melting oxidation detoxification method

    CN117299755A

  • Process for melting and purifying waste salt through heating glass body

    CN117324353A