Continuous production line of polyether-ether-ketone composite board and production method thereof
The polyetheretherketone (PEEK) composite board production line, which integrates segmented conveyor belts and transfer components, combines gluing, alignment, and pressing within the bonding box. This solves the problems of complex production equipment and processes, enabling efficient and simplified production of PEEK composite boards and improving the bonding yield and production capacity.
Patent Information
- Application Number
- CN202511581706.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-31
- Publication Date
- 2026-01-02
AI Technical Summary
In the continuous production line of polyetheretherketone composite boards, the application of adhesive and bonding of the boards require multiple processes and fixtures, resulting in complex production equipment and processes.
The system employs a segmented conveyor belt and transfer components, integrating the three processes of gluing, alignment, and pressing within the bonding box. It utilizes vacuum adsorption and inclined telescopic blocks to achieve precise bonding in one go, while a deceleration assembly and gluing rollers ensure uniform glue layer coverage. Simultaneous melting and curing are achieved through a moving hot press channel.
It simplifies production equipment, reduces alignment errors and interface defects, improves bonding yield, increases single-line capacity and reduces energy consumption, and meets aerospace-grade flatness requirements.
Smart Images

Figure CN121246261A_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The present application relates to the technical field of polyether ether ketone composite board processing, in particular to a continuous production line for polyether ether ketone composite board and a production method thereof. BACKGROUND
[0002] The continuous production line for polyether ether ketone composite board adopts a fusion mode of hot press forming and automatic tape laying (AFP) technology, and realizes uniform interlayer bonding and interface bonding strength improvement by using precise temperature control and pressure to bond multiple layers of carbon fiber prepreg and molten PEEK matrix layer by layer, so as to efficiently and continuously produce high-performance composite boards with high bonding quality and low warping deformation. In the bonding section of the continuous production line for polyether ether ketone composite board, the alignment of the board for gluing and board bonding is generally realized by two processes, and the blank to be bonded needs to be realized by multiple clamps in the process of transfer and alignment, so the production equipment and process are relatively complex. SUMMARY
[0003] The present application aims to provide a continuous production line for polyether ether ketone composite board and a production method thereof to solve the problem that in the bonding section of the continuous production line for polyether ether ketone composite board, the alignment of the board for gluing and board bonding is generally realized by two processes, and the blank to be bonded needs to be realized by multiple clamps in the process of transfer and alignment, so the production equipment and process are relatively complex.
[0004] To achieve the above-mentioned purpose, the present application provides the following technical scheme: A continuous production line for polyether ether ketone composite board and a production method thereof, comprising a segmented conveyor belt for conveying polyether ether ketone composite board blanks, a first transfer member and a second transfer member are installed inside the segmented conveyor belt, a power assembly is installed at the lower end of the first transfer member and the second transfer member, an adhesive unit is installed at the upper end of the segmented conveyor belt, an opening is provided at the upper end of the adhesive unit, a speed reduction assembly is installed outside the opening, a gluing assembly is installed on one side of the speed reduction assembly, and inclined expansion blocks are installed on both sides of one end of the adhesive unit; the first transfer member comprises a horizontal plate, the horizontal plates are fixedly connected by a connecting plate, a connecting shaft is fixedly connected inside the connecting plate, a rubber air bag is fixedly connected to the inner side of one end of the horizontal plate, a buffer pad is installed on one side of the rubber air bag, a sliding cavity is formed in the horizontal plate, a sliding block is slidably connected inside the sliding cavity, an adsorption groove is formed in the sliding block, a piston plate is slidably connected inside the adsorption groove, and the rubber air bag is communicated with the sliding cavity through a gas pipe at one end.
[0005] As a further optimization of the present application, wherein: the power assembly comprises a fixed frame, one side of the fixed frame is fixedly connected with the driving motor shell through bolts, both ends of the inner side of the upper end of the fixed frame are welded with fixed sleeves, the fixed frame is provided in a U shape, the driving motor main shaft is fixedly connected with the connecting shaft through the fixed frame and the fixed sleeve, and the fixed sleeve and the connecting plate are rotationally connected.
[0006] As a further optimization of the present application, wherein: the bonding unit comprises a bonding box, the bonding box is internally provided with equidistantly arranged telescopic baffles on both sides, and the bonding box is provided with a feeding port at one end close to the first transfer member.
[0007] As a further optimization of the present application, wherein: the bonding box is provided in a "mouth" shape in transverse projection, the inclined telescopic blocks provided on one side of the bonding unit are arranged at the feeding port of the bonding box, both sides of the feeding port are provided in an arc shape, the top end of the telescopic baffle is provided in an arc shape, and the distance between adjacent telescopic baffles is equal to the thickness of the bonded polyether ether ketone composite plate.
[0008] As a further optimization of the present application, wherein: the glue applying assembly comprises a glue applying box, a plurality of glue applying rollers are mounted on one side of the glue applying box, and a glue inlet is mounted on the upper end of the glue applying box.
[0009] As a further optimization of the present application, wherein: the deceleration assembly comprises two fixed plates, a guide rod is fixedly connected inside any one of the fixed plates, telescopic springs are fixedly connected outside the guide rod, an internal shaft is mounted between the telescopic springs, a retardation roller is rotationally connected outside the internal shaft, and the internal shaft and the guide rod are slidingly connected.
[0010] As a further optimization of the present application, wherein: the retardation roller is provided with two, the two retardation rollers are parallel, the internal shaft and the guide rod are perpendicularly arranged at 90°, and the retardation roller is arranged on both sides of the opening on the upper end of the bonding unit.
[0011] As a further optimization of the present application, wherein: the horizontal plate provided inside the first transfer member is provided with two, the horizontal projection of the sliding block is T-shaped, the vertical section of the adsorption groove is T-shaped, the horizontal projection of the piston plate is T-shaped, the piston plate is slidingly connected with the adsorption groove through a sealing ring, and the lower end of the piston plate is fixedly connected with the bottom of the sliding cavity.
[0012] As a further optimization of the present application, wherein: the inclined telescopic block is provided with four, and one end of the inclined telescopic block close to the feeding port is provided in an inclined surface.
[0013] As a further optimization of the present application, wherein: the method comprises the following steps: Step 1: during the operation of the device, the external industrial power supply is powered on; After power-on is completed, the polyether ether ketone composite plate blank is conveyed by the sectional conveyor, when the polyether ether ketone composite plate blank is conveyed to the upper end of the first transfer element, the horizontal plate is driven by the power assembly to rotate by 90°, and the polyether ether ketone composite plate blank located at the upper end of the sectional conveyor is transferred to the inside of the bonding box; Step 2: during the process that the horizontal plate transfers the polyether ether ketone composite plate blank to the inside of the bonding box, the rubber air bag is extruded by the lower end of the bonding box, at this time, the gas enters the sliding cavity through the air pipe, the sliding block is ejected, the piston plate performs vacuumization on the upper end of the adsorption groove, the adsorption groove is used to prevent the polyether ether ketone composite plate blank from tilting during the vertical process, and the sliding block pushes the polyether ether ketone composite plate blank to the side, away from the feeding port, of the inclined telescopic block; Step 3: another part of the polyether ether ketone composite plate blank is discharged from the opening position at the upper end of the bonding box synchronously, during the discharging process, the gluing assembly glues the surface of the polyether ether ketone composite plate blank, after the gluing is completed, the polyether ether ketone composite plate blank is adapted and bonded with the polyether ether ketone composite plate blank transferred by the first transfer element in the bonding box; Step 4: the polyether ether ketone composite plate after bonding is moved in the bonding box under the pushing of the next group of feeding, in the process, the telescopic baffle continuously presses, the bonding box can heat the inside during the operation, when the polyether ether ketone composite plate after bonding moves away from the side, away from the feeding port, the second transfer element is controlled to transfer the polyether ether ketone composite plate after bonding to the sectional conveyor, and the discharging is completed.
[0014] Compared with the prior art, the polyether ether ketone composite plate material produced by the device has the advantages that: 1、The segmented conveyor and the first and second transfer elements are rotation-vacuum adsorption linkage in the present application, three actions of "gluing-alignment-pressing" are integrated in one station of the bonding box: the blank is erected, vacuumization is prevented from tilting, the inclined telescopic block is automatically centered, synchronous gluing of the upper piece and positioning of the lower piece are completed, then the equidistant telescopic baffle continuously heats and presses, one-time precise bonding is realized, a plurality of clamps and transfer sequences are omitted, the device is simplified, the beat is shortened, alignment errors and interface defects are significantly reduced, and high-bonding-strength polyether ether ketone composite plate materials are continuously produced; 2、The pair of speed reduction rollers of the speed reduction assembly elastically clamp and limit the speed of the edges of the blank before the blank enters the bonding box, synchronous rolling of the gluing roller is cooperated, the uniformity of the glue layer thickness is ensured, and glue is not splashed; meanwhile, the telescopic spring of the speed reduction roller (which can automatically adjust the distance according to the thickness of the plate, realize "one machine for all thicknesses" in the range of 0.2-3 mm, reduce changeover downtime, improve the glue joint good product rate by 8%, and control the glue layer fluctuation within ±3 g / m²; 3. In this invention, the "U"-shaped closed structure of the bonding box and the internal equidistant telescopic baffles form a movable hot pressing channel. The slab is continuously heated and subjected to a uniform pressure of 0.3–0.5 MPa as it moves forward, so that the PEEK melting and solidification are completed simultaneously. The outlet temperature has dropped to the demolding temperature, and the slab can be directly taken out by the second transfer piece, realizing "hot in, cold out" without cooling waiting. The single-line production capacity is increased by more than 30%, energy consumption is reduced by 15%, and the warpage of the slab is <0.5 mm / m, which meets the flatness requirements of aerospace grade. Attached Figure Description
[0015] Figure 1 This is a schematic diagram of the overall structure of the present invention; Figure 2 For the present invention Figure 1 Enlarged structural diagram at point A in the middle; Figure 3 This is a schematic diagram of the installation position structure of the second transfer component of the present invention; Figure 4 This is a schematic diagram of the adhesive coating assembly structure of the present invention; Figure 5 This is a schematic diagram of the deceleration component structure of the present invention; Figure 6 This is a schematic diagram of the structure of the first transfer component of the present invention; Figure 7 For the present invention Figure 6 Enlarged structural diagram at point B.
[0016] In the diagram: 1. Power assembly; 11. Mounting bracket; 12. Drive motor; 13. Mounting sleeve; 2. Segmented conveyor belt; 3. Bonding unit; 31. Bonding box; 32. Telescopic baffle; 33. Feed inlet; 4. Glue application assembly; 41. Glue application box; 42. Glue inlet; 43. Glue application roller; 5. Deceleration assembly; 51. Fixing plate; 52. Deceleration roller; 53. Internal shaft; 54. Telescopic spring; 55. Guide rod; 6. Inclined telescopic block; 7. First transfer component; 71. Horizontal plate; 72. Buffer pad; 73. Rubber airbag; 74. Connecting shaft; 75. Connecting plate; 76. Air pipe; 77. Sliding cavity; 78. Sliding block; 79. Adsorption tank; 710. Piston plate; 8. Second transfer component. Detailed Implementation
[0017] Please see Figures 1-7 The present invention provides a technical solution: A continuous production line for polyetheretherketone (PEEK) composite boards and its production method are disclosed. The production line includes a segmented conveyor belt 2 for conveying PEEK composite board blanks. A first transfer member 7 and a second transfer member 8 are installed inside the segmented conveyor belt 2. A power assembly 1 is installed at the lower end of the first transfer member 7 and the second transfer member 8. An adhesive bonding unit 3 is installed in the middle of the upper end of the segmented conveyor belt 2. The adhesive bonding unit 3 has an opening at its upper end, and a speed reduction assembly 5 is installed outside the opening. An adhesive application assembly 4 is installed on one side of the speed reduction assembly 5. Inclined telescopic joints are installed at both the upper and lower ends of one end of the adhesive bonding unit 3. Block 6; The first transfer component 7 includes a horizontal plate 71, which is fixedly connected to each other by a connecting plate 75. A connecting shaft 74 is fixedly connected through the inside of the connecting plate 75. A rubber airbag 73 is fixedly connected to the inner side of one end of the horizontal plate 71. A buffer pad 72 is installed on one side of the rubber airbag 73. A sliding cavity 77 is opened inside the horizontal plate 71. A sliding block 78 is slidably connected inside the sliding cavity 77. An adsorption groove 79 is opened inside the sliding block 78. A piston plate 710 is slidably connected inside the adsorption groove 79. One end of the rubber airbag 73 is connected to the sliding cavity 77 through an air pipe 76.
[0018] As a further implementation of this solution, the power assembly 1 includes a fixed frame 11. One side of the fixed frame 11 is fixedly connected to the housing of the drive motor 12 by bolts. Fixed sleeves 13 are welded and fixed at both ends of the upper inner side of the fixed frame 11. The fixed frame 11 is U-shaped. The main shaft of the drive motor 12 passes through the fixed frame 11 and the fixed sleeves 13 and is fixedly connected to the connecting shaft 74. The fixed sleeves 13 are rotatably connected to the connecting plate 75. Through the above arrangement, a stable power source is provided to the first transfer member 7 and the second transfer member 8. As a further implementation of this solution, the bonding unit 3 includes a bonding box 31. Equally spaced telescopic baffles 32 are installed on both sides of the bonding box 31. A feed inlet 33 is opened at one end of the bonding box 31 near the first transfer member 7. The lateral projection of the bonding box 31 is "U"-shaped. An inclined telescopic block 6 is positioned on one side of the bonding unit 3 at the feed inlet 33 of the bonding box 31. The sides of the feed inlet 33 are arc-shaped. The top of the telescopic baffles 32 is arc-shaped. The spacing between adjacent telescopic baffles 32 is equal to the thickness of the polyetheretherketone composite board after bonding. Through the above arrangement, the polyetheretherketone composite board blank can be bonded and pressed inside the bonding box 31. Simultaneously, an external drying device can be used for drying, further improving the stability of the production process. As a further implementation of this solution, the glue application assembly 4 includes a glue application box 41, with multiple glue application rollers 43 installed on one side of the glue application box 41 and a glue inlet 42 installed at the upper end of the glue application box 41. With the above settings, glue can be applied to one side of the polyether ether ketone composite board blank. As a further implementation of this solution, the deceleration assembly 5 includes two fixed plates 51. A guide rod 55 is fixedly connected inside any fixed plate 51. A telescopic spring 54 is fixedly connected to the outside of the guide rod 55. An internal shaft 53 is installed between the telescopic springs 54. A slowing roller 52 is rotatably connected to the outside of the internal shaft 53. The internal shaft 53 is slidably connected to the guide rod 55. There are two slowing rollers 52, which are parallel to each other. The internal shaft 53 is perpendicular to the guide rod 55 at 90°. The slowing rollers 52 are set on both sides of the upper end of the opening provided at the upper end of the bonding unit 3. Through the above arrangement, the polyetheretherketone composite board blank entering the bonding box 31 can be clamped and buffered by the two slowing rollers 52 to prevent the polyetheretherketone composite board blank from falling quickly to the bottom of the bonding box 31 and causing a collision. At the same time, the glue on the surface of the glue roller 43 can be further smoothed. As a further implementation of this solution, the first transfer member 7 is provided with two horizontal plates 71, the horizontal projection of the sliding block 78 is T-shaped, the vertical section of the adsorption groove 79 is T-shaped, the horizontal projection of the piston plate 710 is T-shaped, the piston plate 710 is slidably connected to the adsorption groove 79 through a sealing ring, and the lower end of the piston plate 710 is fixedly connected to the bottom of the sliding cavity 77. With the above arrangement, the polyether ether ketone composite board blank can be positioned and transported into the bonding box 31 by the rotational force during the process of conveying the polyether ether ketone composite board blank through the first transfer member 7. As a further implementation of this solution, four inclined telescopic blocks 6 are provided. The end of the inclined telescopic block 6 near the feed inlet 33 is set with an inclined surface. Through this setting, the polyether ether ketone composite board blank that enters the bonding box 31 can be separated from the first transfer piece 7. As a further implementation of this solution, the technical solution includes the following steps: Step 1: During equipment operation, connect to an external industrial power supply. After power is applied, a portion of the polyether ether ketone composite board blank is conveyed by the segmented conveyor belt 1. When this portion of the polyether ether ketone composite board blank is conveyed to the upper end of the first transfer piece 7, the power assembly 1 drives the horizontal plate 71 to rotate 90°, transferring the polyether ether ketone composite board blank located at the upper end of the segmented conveyor belt 2 into the bonding box 31. Step 2: During the process of transferring the polyetheretherketone composite board blank to the bonding box 31 by the horizontal plate 71, the rubber airbag 73 is squeezed by the lower end of the bonding box 31. At this time, the gas enters the sliding chamber 77 through the air pipe 76, the sliding block 78 is pushed out, and the piston plate 710 evacuates the upper end of the adsorption tank 79. The adsorption tank 79 is used to prevent the polyetheretherketone composite board blank from tipping over during the process of standing up. The sliding block 78 pushes the polyetheretherketone composite board blank to the side of the inclined telescopic block 6 away from the feed port 33. Step 3: Simultaneously, another part of the polyether ether ketone composite board blank is cut from the upper opening of the bonding box 31. During the cutting process, the glue application component 4 applies glue to the surface of this part of the polyether ether ketone composite board blank. After the glue application is completed, it enters the bonding box 31 and is adapted to be bonded to the polyether ether ketone composite board blank transferred by the first transfer component 7. Step 4: After the bonding is completed, the polyetheretherketone composite board moves inside the bonding box 31 pushed by the next set of feeders. During this process, it is continuously pressed by the telescopic baffle 32. The bonding box 31 can be heated internally during operation. When a bonded polyetheretherketone composite board moves out from the side away from the feed port 33, the second transfer member 8 is controlled to transfer the bonded polyetheretherketone composite board to the segmented conveyor belt 2 to complete the unloading.
[0019] This article uses specific examples to illustrate the principles and implementation methods of the present invention. The above examples are only for the purpose of helping to understand the method and core ideas of the present invention. The above descriptions are only preferred embodiments of the present invention. It should be noted that due to the limitations of textual expression, while there are objectively infinite specific structures, those skilled in the art can make several improvements, modifications, or changes without departing from the principles of the present invention, and can also combine the above technical features in an appropriate manner. These improvements, modifications, changes, or combinations, or the direct application of the inventive concept and technical solution to other situations without modification, should all be considered within the scope of protection of the present invention.
Claims
1. A continuous production line for polyetheretherketone (PEEK) composite boards, comprising a segmented conveyor belt (2) for conveying PEEK composite board blanks, characterized in that, The segmented conveyor belt (2) is equipped with a first transfer component (7) and a second transfer component (8) on its inner side. A power assembly (1) is installed at the lower end of the first transfer component (7) and the second transfer component (8). An adhesive unit (3) is installed in the middle of the upper end of the segmented conveyor belt (2). An opening is provided at the upper end of the adhesive unit (3). A deceleration assembly (5) is installed on the outside of the opening. An adhesive application assembly (4) is installed on one side of the deceleration assembly (5). Inclined telescopic blocks (6) are installed at the upper and lower ends of both sides of one end of the adhesive unit (3). The first transfer component (7) includes a horizontal plate (71), which is fixedly connected to each other by a connecting plate (75). A connecting shaft (74) is fixedly connected through the inside of the connecting plate (75). A rubber airbag (73) is fixedly connected to the inner side of one end of the horizontal plate (71). A buffer pad (72) is installed on one side of the rubber airbag (73). A sliding cavity (77) is opened inside the horizontal plate (71). A sliding block (78) is slidably connected inside the sliding cavity (77). An adsorption groove (79) is opened inside the sliding block (78). A piston plate (710) is slidably connected inside the adsorption groove (79). One end of the rubber airbag (73) is connected to the sliding cavity (77) through an air tube (76).
2. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: The power assembly (1) includes a fixed frame (11). One side of the fixed frame (11) is fixedly connected to the housing of the drive motor (12) by bolts. Fixed sleeves (13) are welded and fixed at both ends of the upper inner side of the fixed frame (11). The fixed frame (11) is U-shaped. The main shaft of the drive motor (12) passes through the fixed frame (11) and the fixed sleeves (13) and is fixedly connected to the connecting shaft (74). The fixed sleeves (13) are rotatably connected to the connecting plate (75).
3. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: The bonding unit (3) includes a bonding box (31), and telescopic baffles (32) are installed on both sides of the bonding box (31) at equal intervals. The bonding box (31) has a feed port (33) at one end near the first transfer member (7).
4. The continuous production line for polyetheretherketone composite panels according to claim 3, characterized in that: The horizontal projection of the bonding box (31) is "U" shaped. The inclined telescopic block (6) on one side of the bonding unit (3) is located at the feed inlet (33) of the bonding box (31). The two sides of the feed inlet (33) are arc-shaped. The top of the telescopic baffle (32) is arc-shaped. The distance between adjacent telescopic baffles (32) is equal to the thickness of the polyether ether ketone composite board after bonding.
5. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: The glue application assembly (4) includes a glue application box (41), a plurality of glue application rollers (43) are installed on one side of the glue application box (41), and a glue inlet (42) is installed on the upper end of the glue application box (41).
6. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: The deceleration assembly (5) includes two fixed plates (51). A guide rod (55) is fixedly connected inside each fixed plate (51). A telescopic spring (54) is fixedly connected outside the guide rod (55). An internal shaft (53) is installed between the telescopic springs (54). A slowing roller (52) is rotatably connected outside the internal shaft (53). The internal shaft (53) and the guide rod (55) are slidably connected.
7. A continuous production line for polyetheretherketone composite panels according to claim 6, characterized in that: Two slowing rollers (52) are provided, and the two slowing rollers (52) are parallel to each other. The internal shaft (53) and the guide rod (55) are arranged at a 90° angle. The slowing rollers (52) are arranged on both sides of the upper end of the opening provided at the upper end of the bonding unit (3).
8. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: The first transfer member (7) has two horizontal plates (71) inside. The horizontal projection of the sliding block (78) is T-shaped. The vertical section of the adsorption groove (79) is T-shaped. The horizontal projection of the piston plate (710) is T-shaped. The piston plate (710) is slidably connected to the adsorption groove (79) through a sealing ring. The lower end of the piston plate (710) is fixedly connected to the bottom of the sliding cavity (77).
9. The continuous production line for polyetheretherketone composite panels according to claim 1, characterized in that: There are four inclined telescopic blocks (6), and the end of the inclined telescopic block (6) near the feed inlet (33) is set with an inclined surface.
10. A method for producing a polyetheretherketone composite board using a continuous production line according to any one of claims 1-9, characterized in that: Includes the following steps: Step 1: During equipment operation, connect to an external industrial power supply. After power is applied, a portion of the polyether ether ketone composite board blank is conveyed by the segmented conveyor belt (1). When this portion of the polyether ether ketone composite board blank is conveyed to the upper end of the first transfer piece (7), the power assembly (1) drives the horizontal plate (71) to rotate 90°, transferring the polyether ether ketone composite board blank located at the upper end of the segmented conveyor belt (2) into the bonding box (31). Step 2: During the process of transferring the polyetheretherketone composite board blank to the bonding box (31) on the horizontal plate (71), the rubber airbag (73) is squeezed by the lower end of the bonding box (31). At this time, the gas enters the sliding cavity (77) through the air pipe (76), the sliding block (78) is pushed out, and the piston plate (710) evacuates the upper end of the adsorption tank (79). The adsorption tank (79) is used to prevent the polyetheretherketone composite board blank from tipping over during the process of standing up. The sliding block (78) pushes the polyetheretherketone composite board blank to the side of the inclined telescopic block (6) away from the feed port (33). Step 3: Simultaneously, another part of the polyether ether ketone composite board blank is cut from the upper opening of the bonding box (31). During the cutting process, the glue application component (4) applies glue to the surface of this part of the polyether ether ketone composite board blank. After the glue application is completed, it enters the interior of the bonding box (31) and is adapted to be bonded with the polyether ether ketone composite board blank transferred by the first transfer component (7). Step 4: After the bonding is completed, the polyetheretherketone composite board moves inside the bonding box (31) pushed by the next set of feeders. During this process, it is continuously pressed by the telescopic baffle (32). The bonding box (31) can be heated inside during operation. When the bonded polyetheretherketone composite board moves out from the side away from the feed port (33), the second transfer component (8) is controlled to transfer the bonded polyetheretherketone composite board to the segmented conveyor belt (2) to complete the unloading.