Stress relief process for metal wire
By maintaining a constant temperature and implementing closed-loop control during the slow cooling process after spheroidizing annealing of metal wire, the problem of residual stress in metal wire was solved, achieving efficient and stable stress elimination and microstructure softening, thus improving processing stability and product quality.
Patent Information
- Application Number
- CN202512038394.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-31
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2045-12-31
AI Technical Summary
In the existing technology, residual stress in metal wires is not effectively eliminated before cold working, which leads to easy deformation, cracking and dimensional instability during processing, affecting product qualification rate and processing stability.
During the slow cooling process after spheroidizing annealing of metal wire, a constant temperature range of 550℃ to 600℃ is maintained. Stress relief is achieved by combining this with a continuous production line, and process parameters are adjusted in real time through a closed-loop control system to ensure stress relaxation effect.
It enables continuous integrated processing of metal wires, effectively eliminates residual stress, improves production efficiency and product qualification rate, avoids deformation and cracking problems in subsequent processing, and enhances process stability and adaptability.
Smart Images

Figure CN121737396B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of heat treatment technology for metallic materials, and in particular to stress relief processes for metal wires. Background Technology
[0002] Currently, high-carbon steel and alloy steel wire rods usually need to undergo spheroidizing annealing before cold working such as drawing and cold heading, in order to transform lamellar pearlite into spheroidal pearlite, reduce material hardness, and improve plasticity.
[0003] Current mainstream spheroidizing annealing processes, such as the well-known batch annealing, typically involve the following steps: furnace loading, heating to above Ac1 temperature, prolonged holding at that temperature, followed by slow cooling in the furnace. This process has two significant drawbacks: First, due to its batch processing nature, it suffers from low production efficiency, high energy consumption, and long production cycles, failing to meet the demands of modern industry for efficient continuous production. Second, and more critically, the core objective of this process is solely spheroidization, lacking an effective mechanism to eliminate the microscopic residual stresses generated during the initial rolling, drawing, and heat treatment of the wire rod. These residual stresses can become potential hazards in subsequent processing (especially multi-pass, high-reduction-area drawing), easily leading to uneven deformation, dimensional deviations, and even drawing breakage (commonly known as "wire breakage"), severely impacting product yield, processing stability, and the final product's performance.
[0004] The above content is only used to help understand the technical solution of this application and does not represent an admission that all of the above content is prior art. Summary of the Invention
[0005] The main objective of this invention is to provide a stress relief process for metal wires, which aims to solve the technical problems in the prior art, especially the failure to effectively eliminate residual stress inside the metal wires after annealing, which leads to deformation, cracking and dimensional instability in subsequent processing.
[0006] To achieve the above objectives, the present invention proposes a stress relief process for metal wires, the stress relief process for metal wires comprising the following steps: Heating the metal wire; The heated metal wire is subjected to spheroidizing annealing treatment; The metal wire that has undergone spheroidizing annealing is then slowly cooled. During the slow cooling process, the metal wire is kept at a constant temperature within a first preset temperature range to eliminate residual stress inside it.
[0007] Furthermore, the slow cooling step is carried out at a cooling rate of 0.8℃ / min to 1.5℃ / min; the constant temperature holding step is carried out in a temperature range of 550℃ to 600℃ for a holding time of 30 to 60 minutes; and the constant temperature holding is completed during the continuous travel of the metal wire.
[0008] Optionally, the heating step involves heating the metal wire to 720°C to 760°C.
[0009] Optionally, the spheroidizing annealing process includes: maintaining the metal wire at a constant temperature of 720°C to 760°C for 4 to 8 hours.
[0010] Optionally, the slow cooling step specifically includes: cooling the metal wire from the spheroidizing annealing temperature to 600°C at a cooling rate of 0.8°C / min to 1.5°C / min, and then entering the isothermal holding stage of 550°C to 600°C.
[0011] Optionally, the isothermal holding step further includes a closed-loop control process: real-time monitoring of the hardness or residual stress of the metal wire; when the monitored value deviates from the preset target range, dynamic compensation adjustment is made to the isothermal holding temperature and / or time according to a preset offset-adjustment mapping relationship. For example, the mapping relationship may be: when the real-time hardness value is more than 10 HV higher than the target value, the isothermal temperature is increased by 10-15℃, and the isothermal holding time is extended by 10-25 minutes simultaneously.
[0012] Optionally, the process is performed in a continuous heat treatment furnace, and the isothermal holding step is carried out in a specially designed, temperature-controllable isothermal zone in the slow cooling section of the furnace body.
[0013] Optionally, the metal wire is a high-carbon steel or alloy steel wire that still needs to be drawn into shape in multiple passes after continuous spheroidizing annealing.
[0014] Optionally, taking SWRH82B high-carbon steel wire as an example, the heating step is to heat to 750℃; the spheroidizing annealing treatment step is to maintain a constant temperature of 750℃ for 6 hours; the slow cooling step is to cool to 580℃ at a rate of 1.2℃ / min; and the constant temperature holding step is to maintain a constant temperature of 580℃ for 45 minutes.
[0015] This invention proposes a stress relief process for metal wires. Compared to the existing batch-type spheroidizing annealing process, which suffers from low production efficiency and residual stress buildup leading to deformation and cracking during subsequent processing, this application integrates spheroidizing annealing and stress relief into a continuous process. During the slow cooling process after spheroidizing annealing, a constant temperature holding platform is set within the temperature range of 550°C to 600°C for 30 to 60 minutes. That is, by holding the wire at this specific temperature range, the creep effect of the material at this temperature promotes dislocation rearrangement and stress relaxation. There is no need for separate stress relief treatment after spheroidizing annealing. By starting a continuous production line, spheroidizing and stress relief can be achieved simultaneously on a single production line, completing the continuous integrated processing of the wire. This allows the processed wire to simultaneously meet the requirements of softened structure and low residual stress, avoiding problems such as subsequent drawing cracking and dimensional instability caused by residual stress without secondary heat treatment, thus improving heat treatment efficiency and wire processing qualification rate.
[0016] Furthermore, by introducing a closed-loop control mechanism based on real-time hardness or stress monitoring, and dynamically compensating process parameters according to a preset offset-adjustment mapping relationship, the process stability and adaptability to different materials and working conditions are further improved. It is compatible with the modification of existing continuous annealing furnaces, has low implementation costs, and has good prospects for industrial application. Attached Figure Description
[0017] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with this application and, together with the description, serve to explain the principles of this application.
[0018] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0019] Figure 1 A schematic flowchart of the stress relief process for metal wires provided in Embodiment 1 of this application; Figure 2 This is a schematic flowchart of Embodiment 2 of the stress relief process for metal wires in this application; The purpose, features, and advantages of this application will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0020] It should be understood that the specific embodiments described herein are merely illustrative of the technical solutions of this application and are not intended to limit this application.
[0021] This application provides a stress relief process for metal wires, referring to... Figure 1 , Figure 1 This is a schematic flowchart of the first embodiment of the stress relief process for metal wires in this application.
[0022] In the first embodiment, the stress relief process for the metal wire includes steps S10 to S40: Step S10: Heat the metal wire; After the coiled metal wire is unwound, it is continuously fed into the heating section of the heat treatment furnace at a constant speed.
[0023] Specifically, the wire is heated uniformly and controllably to above the Ac1 phase transition point by resistance heating elements distributed at the top and bottom of the furnace.
[0024] In this embodiment, the wire is heated to a temperature range of 720°C to 760°C.
[0025] The purpose of this step is to austenitize the wire structure, creating the necessary conditions for the subsequent dissolution and spheroidization of cementite. If the heating temperature is too low, spheroidization will be insufficient; if it is too high, it may lead to coarse grains or complete dissolution of cementite, which is not conducive to obtaining a uniform spheroidized structure.
[0026] Step S20: Perform spheroidizing annealing treatment on the heated metal wire; After leaving the heating section, the wire enters the spheroidizing and heat preservation section, where temperature uniformity control is more precise. In this section, the wire is kept at a constant temperature of 720℃ to 760℃ for an extended period.
[0027] Specifically, the isothermal holding time is 4 to 8 hours. During this process, the lamellar cementite gradually dissolves into the austenite, and under long-term heat treatment, through the diffusion of carbon atoms, it re-nucleates and grows at the austenite grain boundaries and defects, eventually forming uniform, fine spherical cementite particles.
[0028] This step is crucial for reducing wire stiffness. Insufficient heat treatment time will result in low spheroidization and residual lamellar structures; excessive heat treatment may cause excessive growth of spherical carbides, which is also detrimental to plasticity.
[0029] Step S30: Slowly cool the metal wire that has undergone spheroidizing annealing treatment; The spheroidized and heat-insulated wire enters the slow cooling section. This section uses a precise programmed temperature control system to slowly and evenly reduce the furnace temperature.
[0030] Specifically, the cooling rate is controlled at 0.8℃ / min to 1.5℃ / min, slowly cooling the wire from the spheroidization temperature (approximately 720-760℃) to approximately 600℃. This slow cooling process aims to simulate equilibrium cooling, allowing sufficient time for the carbides precipitated along the grain boundaries during the cooling process to accumulate on the already formed spheroidized carbides, thereby stabilizing and optimizing the spheroidized structure and avoiding the formation of new lamellar pearlite or the introduction of large thermal stress due to excessively rapid cooling.
[0031] Step S40: During the slow cooling process, the metal wire is kept at a constant temperature within a first preset temperature range to eliminate residual stress inside it.
[0032] After the wire is cooled to approximately 600°C in the slow cooling section, it does not immediately enter a lower temperature zone. Instead, it enters a specially designed and constructed "stress relaxation platform" section (i.e., a constant temperature zone). In this section, the wire stops cooling within a specific medium temperature range of 550°C to 600°C and is held at a constant temperature for 30 to 60 minutes.
[0033] Specifically, the 550-600℃ range was chosen because: for high-carbon steel, this temperature is much higher than its recrystallization temperature, and the material still exhibits good high-temperature creep properties, with sufficient atomic mobility; at the same time, it is much lower than the Ac1 point, preventing the initiation of new phase transformations and avoiding interference with the already formed spheroidized structure. Maintaining a constant temperature at this level provides the kinetic conditions for releasing the microscopic residual stresses (such as dislocation entanglements and lattice distortions) accumulated within the wire during all previous processing stages. Through the slip, climb, and reorganization of dislocations, the elastic strain energy is consumed, thereby achieving active stress relaxation.
[0034] Crucially, this isothermal holding process is completed synchronously during the continuous movement of the wire. The wire passes through the isothermal zone at the same uniform speed as when it enters the furnace, achieving "online" stress relief. This is fundamentally different from batch processing methods that require stopping the machine and performing stress-relief annealing separately, and is the key to achieving high efficiency.
[0035] Through the aforementioned steps S10 to S40, this embodiment of the application successfully integrates spheroidizing annealing and stress relief treatment into a continuous, uninterrupted process. Taking SWRH82B wire as an example, after this process, its hardness can be stably controlled below 220HV, the spheroidization rate exceeds 90%, and the residual stress level can be reduced by approximately 40% compared to the traditional single spheroidizing annealing process, laying an excellent foundation for the microstructure and stress state of subsequent stringent drawing processes.
[0036] Based on the first embodiment described above, the second embodiment further refines the stress relaxation platform control strategy in step S40 by introducing an intelligent closed-loop control system based on real-time feedback to address material property fluctuations and minor changes in furnace conditions, ensuring the ultimate stability of the process effect. (Refer to...) Figure 2 The closed-loop control system includes an online monitoring unit, a control logic unit, and an execution unit.
[0037] In this embodiment, step S40 further includes the following closed-loop control process: Non-contact online monitoring devices are integrated at the entrance and / or exit of the "stress relaxation platform" section. For example, an ultrasonic hardness tester can be used to measure the surface hardness of the wire online, or an X-ray stress analyzer can be used to analyze the residual stress on the surface online. The monitoring data is transmitted to the control system in real time.
[0038] The control system has preset target parameter ranges for the steel grade of the wire rod being processed (for example, for SWRH82B, the target hardness value is ≤220HV). The system compares the real-time monitored values with the target range.
[0039] When the monitored value deviates from the preset target range, the control system does not perform a simple proportional adjustment. Instead, it uses the preset offset-adjustment mapping relationship stored in its internal memory, which is summarized from a large amount of process test data, to perform precise and linked dynamic compensation adjustment on the temperature set point of the "stress relaxation platform" and / or the speed of the wire passing through that section (i.e., the equivalent isothermal time).
[0040] As a specific and preferred example of the mapping relationship, when the system detects a real-time hardness value exceeding the target value by more than 10 HV (indicating that stress relaxation may be insufficient), the control system will automatically execute the following compensation strategy: The temperature of the "stress relaxation platform" will be increased by 10-15°C from the base setpoint (e.g., 580°C) to utilize the stronger atomic diffusion capability at higher temperatures to accelerate stress relaxation; simultaneously, the isothermal holding time (achieved through fine-tuning the wire speed) will be extended by 10-25 minutes to provide more time for stress release. This "temperature and time coordinated adjustment" mapping relationship is not easily obtained by those skilled in the art through conventional reasoning or simple experiments; it reflects a deep understanding and optimization of the process mechanism.
[0041] By introducing this closed-loop control process, this technology possesses adaptive adjustment capabilities. For example, when the original stress state or composition of the incoming wire fluctuates slightly, the system can automatically identify and adjust the process parameters to compensate, ensuring that the stress relief effect of each wire segment in the final output remains stable within the optimal range, greatly improving product consistency and process robustness.
[0042] Based on the first and second embodiments described above, this third embodiment provides a specific and complete implementation method.
[0043] In this embodiment, SWRH82B high carbon steel wire (Φ12.0mm wire rod) is used as an example to illustrate the specific application of this process.
[0044] Specifically, the process is performed in a modified continuous roller hearth heat treatment furnace production line. This production line sequentially includes a heating section, a spheroidizing and holding section, a slow cooling section, a stress relaxation plateau section (i.e., a constant temperature zone), and a final cooling section. The stress relaxation plateau section is an independent temperature zone specifically separated from the original slow cooling section. This zone has high-precision temperature control capabilities, with a temperature control accuracy of ±3℃. Its length is calculated and determined based on the processing line speed and the required constant temperature holding time. Furthermore, an online ultrasonic hardness tester is integrated at the entrance of this stress relaxation plateau section for real-time monitoring of the wire hardness.
[0045] The specific steps are as follows: Step SS10: After uncoiling the SWRH82B wire, it is continuously fed into the heating section of the heat treatment furnace at a preset constant speed. The wire is uniformly heated by the heating element until the wire temperature reaches the preset first target temperature. Step SS20: The wire is fed into the heat treatment furnace and kept at the first target temperature for a first preset time to allow the lamellar cementite structure inside the wire to be fully spheroidized into spheroidized cementite structure. Step SS30: The wire is fed into the slow cooling section of the heat treatment furnace, and the wire temperature is reduced from the first target temperature to the second target temperature at a preset first cooling rate to stabilize the spherical cementite structure. Step SS40: After the wire temperature reaches the second target temperature, the wire is placed in a specially designed stress relaxation platform section in the heat treatment furnace and kept at a constant temperature for a second preset time within the first preset temperature range. The creep effect of the wire in this temperature range is used to promote the rearrangement of internal dislocations and the relaxation of micro-stress, thereby eliminating residual stress.
[0046] Specifically, for SWRH82B high-carbon steel wire: the first target temperature in step SS10 is 750℃; the first preset duration in step SS20 is 6 hours; the first cooling rate in step SS30 is 1.2℃ / min, and the second target temperature is 580℃; the first preset temperature range in step SS40 is 580℃, and the second preset duration is 45 minutes.
[0047] Specifically, in this embodiment, step SS40 further includes a closed-loop control process: An online ultrasonic hardness tester monitors the surface hardness of the wire entering the constant temperature zone in real time, and the measured real-time hardness value is 225 HV.
[0048] The preset target hardness range in the control system is ≤220HV. Because the real-time monitored value (225HV) is more than 5HV higher than the target value, the dynamic adjustment program is triggered.
[0049] The control system automatically performs compensation adjustment based on the preset offset-adjustment mapping relationship (in this example, the mapping relationship is: when the hardness is 5-10 HV higher than the target value, the constant temperature is increased by 10℃, and the constant temperature time is extended by 15 minutes). The temperature setting value of the stress relaxation platform section is increased from the base value of 580℃ to 590℃.
[0050] By fine-tuning the cable travel speed, the cable's holding time in this section can be extended from 45 minutes to approximately 52 minutes.
[0051] The wire was kept at a constant temperature for 52 minutes under the adjusted parameters, and the residual stress was fully relaxed by utilizing the creep effect in this temperature range.
[0052] This embodiment proposes a stress relief process for metal wires, which addresses the problems of lengthy and inefficient processes caused by separating spheroidizing annealing and stress relief treatment in existing technologies, as well as the high residual stress level of the wire after annealing and the easy generation of defects in subsequent processing.
[0053] It should be noted that the above examples are only for understanding this application and do not constitute a limitation on the stress relief process for metal wires in this application. Any simple modifications based on this technical concept are within the protection scope of this application.
[0054] The above description is only a part of the embodiments of this application and does not limit the scope of protection of this application. All equivalent structural transformations made under the technical concept of this application and using the content of this application specification and drawings, or direct / indirect applications in other related technical fields, are included in the scope of protection of this application.
Claims
1. A stress relief process for metal wires, characterized in that, The stress relief process for the metal wire includes the following steps: Heating the metal wire; The heated metal wire is subjected to spheroidizing annealing treatment; The metal wire that has undergone spheroidizing annealing is then slowly cooled. During the slow cooling process, the metal wire is kept at a constant temperature within a first preset temperature range to eliminate residual stress inside it; the constant temperature holding step is carried out in a temperature range of 550°C to 600°C for 30 to 60 minutes; and the constant temperature holding is completed during the continuous movement of the metal wire. The slow cooling step includes: cooling the metal wire from the spheroidizing annealing temperature to 600°C at a cooling rate of 0.8°C / min to 1.5°C / min, and then entering the isothermal holding stage of 550°C to 600°C. The process is performed in a continuous heat treatment furnace, and the isothermal holding step is carried out in a specially designed, temperature-controllable isothermal zone in the slow cooling section of the furnace body. The step of heating the metal wire includes heating the metal wire to 720°C to 760°C. The spheroidizing annealing process includes: maintaining the metal wire at a constant temperature of 720°C to 760°C for 4 to 8 hours. The metal wire is a high-carbon steel or alloy steel wire that still needs to be drawn into shape through multiple passes after continuous spheroidizing annealing.
2. The stress relief process for metal wires as described in claim 1, characterized in that, The temperature holding step also includes a closed-loop control process: Real-time monitoring of the hardness or residual stress of the metal wire; When the monitored value deviates from the preset target range, the temperature and / or time of the constant temperature maintenance are dynamically compensated and adjusted according to the preset offset-adjustment mapping relationship.
3. The stress relief process for metal wires as described in claim 2, characterized in that, The mapping relationship is as follows: When the real-time hardness value is more than 10 HV higher than the target value, the constant temperature is increased by 10-15℃, and the constant temperature time is extended by 10-25 minutes.
4. The stress relief process for metal wires as described in claim 1, characterized in that, The metal wire is SWRH82B high carbon steel wire; the heating step is heating to 750℃; the spheroidizing annealing treatment step is holding at 750℃ for 6 hours; the slow cooling step is cooling to 580℃ at a rate of 1.2℃ / min; the constant temperature holding step is holding at 580℃ for 45 minutes.
Citation Information
Patent Citations
Process for producing high-nodularity fastener wire rod
CN104313281A
Ultra-high-speed continuous isothermal spheroidizing annealing method and device for carbon steel
CN113481354A