A method for preparing a double-layer antibacterial polyvinyl chloride composite pipe

By using a double-layer structure and co-extrusion molding technology, an antibacterial agent is added to the inner layer, and a high-strength PVC-U substrate is used for the outer layer. An interlocking structure is formed through mold design, which solves the problems of high cost, low utilization rate of antibacterial agent and poor interlayer bonding of traditional antibacterial PVC pipes, and achieves efficient inhibition of bacterial growth and improved mechanical properties.

CN121821749BActive Publication Date: 2026-11-17浙江中财管道科技股份有限公司
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202511936620.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-12-22
Publication Date
2026-11-17
Estimated Expiration
2045-12-22

AI Technical Summary

Technical Problem

Traditional antibacterial PVC pipes suffer from high costs, low utilization of antibacterial agents, and poor interlayer bonding.

Method used

It adopts a double-layer structure, with an antibacterial agent added to the inner layer and a high-strength PVC-U substrate used on the outer layer. Through co-extrusion molding equipment and mold design, an interlocking structure is formed between the inner and outer layers to ensure the effective combination of the antibacterial agent in the inner and outer layers.

Benefits of technology

It achieves efficient inhibition of bacterial growth, reduces the amount of antibacterial agent used, lowers costs, improves interlayer bonding strength, and meets the requirements for compressive and impact resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121821749B_ABST
    Figure CN121821749B_ABST
Patent Text Reader

Abstract

This invention discloses a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe, comprising the following steps: S1: Inner layer antibacterial material mixing: ① Add 55% PVC-type resin, 27.5% calcium carbonate, 4.4% stabilizer, 3% CPE, and 1.2% composite lubricant to a hot mixer and heat mix to 80°C; ② Add 8.3% plasticizer and 0.6% antibacterial agent, and continue heat mixing to 120°C; ③ Transfer the material to a cold mixer and cold mix to 60°C to obtain an inner layer antibacterial material mixture; S2: Inner layer antibacterial granule preparation: Feed the inner layer antibacterial material mixture obtained in S1 into a granulator for granulation to obtain inner layer antibacterial granules; S3: Double-layer co-extrusion molding: Add the inner layer antibacterial granules obtained in S2 and the outer layer PVC-U substrate to the corresponding barrels of a co-extruder for extrusion molding to obtain a composite pipe. This invention provides a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of plastic pipe manufacturing equipment technology, and more specifically, to a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe. Background Technology

[0002] Polyvinyl chloride (PVC) pipes are widely used in building water supply and drainage, industrial fluid transportation, and other fields due to their low cost, corrosion resistance, and excellent processing performance. However, the inner wall of traditional PVC pipes is prone to the growth of bacteria and mold over long-term use, forming a biofilm. This not only affects the hygiene and safety of the transported medium but may also shorten the service life of the pipes due to biological corrosion.

[0003] Existing antibacterial PVC pipes are mostly manufactured by adding antibacterial agents integrally. While this achieves an antibacterial effect, the large amount of antibacterial agent required significantly increases pipe costs. Furthermore, since the outer layer does not need to directly contact the transported medium, excessive addition of antibacterial agents is a waste of resources. In the production of composite pipes (especially multi-layer co-extruded composite pipes), the introduction of antibacterial agents often leads to problems such as decreased interlayer peel strength. The essence of this is the "incompatibility" between the properties of the antibacterial agent itself and the interlayer bonding mechanism of the composite pipe. Summary of the Invention

[0004] The purpose of this invention is to overcome the shortcomings of the prior art and provide a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe, which solves the problems of high cost, low utilization rate of antibacterial agent and poor interlayer bonding of traditional antibacterial PVC pipes.

[0005] To achieve the above objectives, the present invention adopts the following technical solution: a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe, comprising the following steps: S1: mixing the inner layer antibacterial material: ① adding 55% PVC-type resin, 27.5% calcium carbonate, 4.4% stabilizer, 3% CPE, and 1.2% composite lubricant by mass percentage into a hot mixer and hot mixing to 80°C; ② adding 8.3% plasticizer and 0.6% antibacterial agent, and continuing hot mixing to 120°C; ③ transferring the material to a cold mixer and cold mixing to 60°C to obtain an inner layer antibacterial material mixture; S2: preparing inner layer antibacterial granules: feeding the inner layer antibacterial material mixture obtained in S1 into a granulator for granulation to obtain inner layer antibacterial granules; S3: double-layer co-extrusion molding: adding the inner layer antibacterial granules obtained in S2 and the outer layer PVC-U substrate into the corresponding barrels of a co-extruder for extrusion molding to obtain a composite pipe.

[0006] The present invention is further configured such that the composite pipe includes an outer layer and an inner layer, the outer layer is formed by curing an outer PVC-U substrate, and its wall thickness accounts for 87.5% of the composite pipe wall thickness, and the inner layer is formed by curing inner antibacterial particles, and its wall thickness accounts for 12.5% ​​of the composite pipe wall thickness.

[0007] The present invention is further configured such that the composite lubricant is composed of a silane coupling agent and a polyethylene wax, wherein the mass ratio of the silane coupling agent to the polyethylene wax is 1:1 to 3:1.

[0008] The present invention is further configured such that, during the S3 co-extrusion molding process, the melting temperature of the inner antibacterial material is controlled at 160-180℃, and the melting temperature of the outer PVC-U substrate is controlled at 170-190℃.

[0009] The present invention is further configured such that the calcium carbonate is light calcium carbonate, the PVC-type resin is PVC-5 resin, the antibacterial agent is nano-silver antibacterial agent or quaternary ammonium salt antibacterial agent, the stabilizer is calcium-zinc composite stabilizer, and the plasticizer is dioctyl phthalate.

[0010] The present invention is further configured to use a co-extrusion molding equipment, the co-extrusion molding equipment including a co-extrusion die, the co-extrusion die including a first die sleeve, a second die sleeve, and a die rod, the die rod being inserted into the second die sleeve, the second die sleeve being inserted into the first die sleeve, a gap cavity being formed between the first die sleeve and the second die sleeve, the gap cavity through which the outer layer PVC-U substrate melt flows, a cavity being formed between the second die sleeve and the die rod, the cavity through which the inner layer antibacterial particle melt flows, the die rod including a sizing part, a shaping cavity being formed between the sizing part and the first die sleeve, the melt in the cavity and the gap cavity converging in the shaping cavity, the outer wall of the second die sleeve being provided with a first protrusion, and multiple first protrusions being evenly distributed along the circumference of the second die sleeve.

[0011] The invention is further configured such that the first protrusion includes a second inclined portion, the second inclined portion gradually tilts towards the side closer to the axis of the second mold sleeve along the direction of molten material flow in the gap cavity, the second mold sleeve is provided with a first groove, the first groove passes through the second inclined portion radially along the second mold sleeve, and the two ends of the first groove are respectively connected to the cavity and the gap cavity.

[0012] The invention is further configured such that the first protrusion also includes a third inclined portion, the third inclined portion being connected to the inclined end of the second inclined portion in the axial direction of the second mold sleeve, and the third inclined portion gradually inclined in the direction of molten material flow in the gap cavity toward the side away from the axial direction of the second mold sleeve.

[0013] The present invention is further configured such that the outer wall of the first protrusion is provided with a second protrusion, the second protrusion is located on both sides of the third inclined portion, and the length direction of the second protrusion is along the axial direction of the first protrusion.

[0014] The invention is further configured such that the first protrusion also includes a fourth inclined portion, the fourth inclined portion gradually tilts towards the side closer to the axis of the second mold sleeve along the flow direction of the molten material in the gap cavity, the fourth inclined portion is connected to the side of the third inclined portion away from the second inclined portion, the second mold sleeve is provided with a second groove, the second groove extends through the second inclined portion along the radial direction of the second mold sleeve, and the two ends of the second groove are respectively connected to the cavity and the gap cavity.

[0015] In summary, the present invention has the following beneficial effects:

[0016] 1. An antibacterial agent is added to the inner layer, directly contacting the transported medium. This results in a high antibacterial rate, effectively inhibiting the growth of common bacteria such as Escherichia coli and Staphylococcus aureus, ensuring the hygiene and safety of the transported medium. The antibacterial agent is added only to the inner layer, while the outer layer uses conventional PVC-U substrate. This reduces the amount of antibacterial agent used, lowering costs compared to integral antibacterial pipes, thus combining economy and practicality. The outer layer accounts for 87.5% of the total wall thickness and uses high-strength PVC-U substrate, ensuring the pipe has excellent pressure and impact resistance, meeting the requirements of GB / T 10002.1-2006 standard. The inner layer adds a CPE impact modifier, further enhancing the pipe's overall mechanical properties.

[0017] 2. During the co-extrusion process, a first protrusion is set through the second die sleeve, so that a groove is formed on the inner wall of the outer layer during the molding process. The subsequent inner layer molten material enters the gap cavity through the first groove, thereby entering the groove on the inner wall of the outer layer and forming an inner layer protrusion. The inner protrusion and the outer layer groove form an interlocking structure, which improves the bonding force and solves the problem of reduced interlayer peel strength caused by the introduction of antibacterial agent, thereby improving the bonding strength between the antibacterial layer and the PVC layer. Attached Figure Description

[0018] Figure 1 This is a cross-sectional view of an embodiment;

[0019] Figure 2 for Figure 1 Enlarged view of point A in the middle;

[0020] Figure 3 for Figure 1 A cross-sectional view along the MM direction;

[0021] Figure 4 for Figure 3 Enlarged view of point B in the middle;

[0022] Figure 5 for Figure 1 A cross-sectional view along the NN direction;

[0023] Figure 6 for Figure 5 Enlarged view of point C in the middle;

[0024] Figure 7 This is a cross-sectional view of the composite structure in the embodiment;

[0025] Figure 8 for Figure 7 Enlarged view of point D in the middle.

[0026] Reference numerals: First mold sleeve 1, Second mold sleeve 2, Feed cavity 21, Feed hole 22, Guide ring 23, Conical surface 231, First protrusion 24, First inclined part 241, First straight part 242, Second inclined part 243, Third inclined part 244, Second straight part 245, Fourth inclined part 246, First groove 247, Second groove 248, Arc surface 249, End 2491, Second protrusion 250, Mold rod 3, Fixing ring 31, Channel 311, Guide part 32, Sizing part 33, Cavity 4, Gap cavity 5, Shaping cavity 6, Composite tube 7, Outer layer 71, Groove 711, Inner layer 72, Protrusion 721. Detailed Implementation

[0027] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0028] This embodiment discloses a method for preparing a double-layer antibacterial polyvinyl chloride composite pipe, the specific method of which is as follows:

[0029] Step S1: Mix the inner antibacterial material.

[0030] This step utilizes a stepwise hot-mixing-cold-mixing process to achieve uniform dispersion of each component and prevent the antibacterial agent from agglomerating. The specific operation is as follows:

[0031] ① By weight percentage, add 55% PVC-type resin, 27.5% calcium carbonate, 4.4% stabilizer, 3% CPE (chlorinated polyethylene), and 1.2% composite lubricant to a hot mixer. Start the hot mixer and control the speed at 800-1000 r / min, mixing until the material temperature reaches 80℃. The PVC-type resin used is PVC-5 resin, which has good processing fluidity and mechanical strength; the calcium carbonate is light calcium carbonate, which can improve the rigidity and dimensional stability of the inner layer material; the stabilizer is a calcium-zinc composite stabilizer, environmentally friendly and free of heavy metals, which can effectively inhibit the degradation of PVC resin during high-temperature processing; CPE, as an impact modifier, can improve the toughness of the inner layer material and prevent low-temperature brittleness of the pipe; the composite lubricant is composed of silane coupling agent and polyethylene wax in a weight ratio of 1:1 to 3:1. The silane coupling agent can enhance the interfacial bonding force between inorganic fillers and organic resins, while the polyethylene wax can reduce friction between materials and equipment and improve processing fluidity.

[0032] ② Add 8.3% plasticizer and 0.6% antibacterial agent to the hot mixer and continue hot mixing until the material temperature reaches 120℃. At this point, the plasticizer fully penetrates into the PVC resin particles, and the antibacterial agent is evenly dispersed in the melt. The plasticizer selected is dioctyl phthalate (DOP), which has high plasticizing efficiency and good compatibility with PVC. The antibacterial agent selected is either nano-silver antibacterial agent or quaternary ammonium salt antibacterial agent. Nano-silver antibacterial agent inhibits bacteria by destroying the bacterial cell membrane with metal ions, while quaternary ammonium salt antibacterial agent inhibits bacterial reproduction through cation adsorption. Both have the characteristics of broad antibacterial spectrum and good durability.

[0033] ③ Quickly transfer the hot-mixed materials to a cold mixer, controlling the speed of the cold mixer at 600-800 r / min, and cold mix until the material temperature drops to 60℃ to obtain the inner layer antibacterial material mixture. The cold mixing process can avoid the deactivation of stabilizers caused by residual heat, and at the same time reduce the material temperature, preparing for the subsequent granulation process.

[0034] Step S2: Preparation of inner antibacterial particles.

[0035] The antibacterial inner layer material mixture obtained in S1 is fed into a twin-screw granulator. The temperature of each section of the granulator is controlled at 140-170℃, and the screw speed is 150-200 r / min. After melting, shearing, extrusion, and pelletizing, uniformly sized antibacterial inner layer granules are obtained. Granulation improves the processing stability of the material and avoids the problem of uneven feeding that occurs during direct extrusion.

[0036] Step S3: Double-layer co-extrusion molding

[0037] A double-layer co-extrusion molding machine is used. The inner layer antibacterial granules obtained from S2 are added to the inner barrel of the co-extruder, and the outer layer PVC-U substrate is added to the outer barrel. The heating of both barrels is controlled: the melting temperature of the inner antibacterial material is 160-180℃, and the melting temperature of the outer PVC-U substrate is 170-190℃. The two molten materials enter the co-extrusion die through their respective flow channels. After converging and compounding in the die's shaping cavity, they are cooled, sized, drawn, and cut to obtain a double-layer antibacterial PVC composite pipe that meets the specifications. Figure 1 Composite pipe 7 in the middle). Figure 7 As shown, the composite pipe 7 includes an outer layer 71 and an inner layer 72 radially inside the outer layer 71. The outer layer 71 is formed by curing an outer PVC-U substrate, and its wall thickness accounts for 87.5% of the wall thickness of the composite pipe 7. The inner layer 72 is formed by curing inner antibacterial particles, and its wall thickness accounts for 12.5% ​​of the wall thickness of the composite pipe 7.

[0038] The introduction of antibacterial agents often leads to problems such as decreased interlayer peel strength and interface cracking. This is mainly because if the particle size of the antibacterial agent is much larger than the molecular chain spacing (nanoscale) of the composite pipe substrate, a "rigid particle barrier layer" will form at the interlayer interface. The molecular chains of adjacent layers cannot penetrate the antibacterial agent particles to achieve entanglement, resulting in tiny gaps at the interface. The interlayer bonding force decreases from "molecular-level adhesion" to "mechanical interlocking," making peeling more likely. Therefore, if... Figures 1-8 As shown, the co-extrusion molding equipment used in the above process includes a co-extrusion die to solve the problem of interlayer bonding force.

[0039] like Figure 1 As shown, the co-extrusion die includes a first die sleeve 1, a second die sleeve 2, and a die rod 3. Both the first die sleeve 1 and the second die sleeve 2 are cylindrical structures. The die rod 3 is inserted into the second die sleeve 2, and the second die sleeve 2 is inserted into the first die sleeve 1. The outer wall of the left end of the second die sleeve 2 is fixedly connected to the inner wall of the first die sleeve 1. A gap cavity 5 is formed between the first die sleeve 1 and the second die sleeve 2, through which the outer PVC-U substrate melt flows. The left end of the second die sleeve 2 is provided with a feed hole 22, which communicates with the gap cavity 5. Figure 1 The medium-sized molten material flows from left to right.

[0040] like Figure 1 As shown, a cavity 4 is formed between the second mold sleeve 2 and the mold rod 3. The cavity 4 is through which the inner layer of antibacterial granules melt flows. The left end of the mold rod 3 is provided with a fixing ring 31. The outer wall of the fixing ring 31 is fixedly connected to the inner wall of the second mold sleeve 2. The second mold sleeve 2 is provided with a feeding cavity 21. The fixing ring 31 is provided with a channel 311. The feeding cavity 21 is used to pass the inner layer of antibacterial granules melt. The inner layer of antibacterial granules melt enters the cavity 4 through the channel 311.

[0041] like Figure 1 As shown, the die rod 3 has a rod-shaped structure, including a guide portion 32 and a sizing portion 33. The right end of the second die sleeve 2 has a guide opening, through which the guide portion 32 passes. The sizing portion 33 is located on the side of the die rod 3 away from the second die sleeve 2. A shaping cavity 6 is formed between the sizing portion 33 and the first die sleeve 1. The molten material in the cavity 4 and the gap cavity 5 converges in the shaping cavity 6 to form Figure 7 The composite tube 7 shown.

[0042] Combination Figures 1-4 The outer wall of the second mold sleeve 2 is provided with a first protrusion 24. The first protrusion 24 protrudes radially outward along the outer wall of the second mold sleeve 2 to form a strip structure. The length direction of the first protrusion 24 is parallel to the axial direction of the second mold sleeve 2. Four first protrusions 24 are evenly distributed along the circumference of the second mold sleeve 2.

[0043] like Figure 2As shown, the first protrusion 24 includes a second inclined portion 243. The second inclined portion 243 gradually inclines towards the axis of the second mold sleeve 2 along the direction of molten material flow within the gap cavity 5. The second mold sleeve 2 is provided with a first groove 247, which corresponds to the second inclined portion 243. The first groove 247 passes radially through the second inclined portion 243 of the second mold sleeve 2, and its two ends connect to the cavity 4 and the gap cavity 5, respectively. Figure 2 , Figure 8 By setting the first protrusion 24, a groove 711 is formed on the inner wall of the outer layer 71, allowing the molten material of the subsequent inner layer 72 to enter the gap cavity 5 through the first groove 247, thereby entering the groove 711 and forming a protrusion 721. The protrusion 721 and the groove 711 form an interlocking structure, improving the bonding force. Specifically, as... Figure 4 As shown, the wall surfaces at both ends of the second inclined portion 243 along the circumferential direction of the second mold sleeve 2 are arc surfaces 249. The arc surface 249 includes two ends 2491, one end 2491 is located on the side close to the axis of the second mold sleeve 2, and the other end 2491 is located on the side away from the axis of the second mold sleeve 2, so that the groove 711 formed by the outer layer 71 can interlock with the protrusion 721, thereby improving the bonding force.

[0044] like Figure 2 As shown, the second mold sleeve 2 includes a guide ring 23 located on the left side. The guide ring 23 has a conical surface 231 to guide the molten material into the gap cavity 5. The left end of the first protrusion 24 has a first inclined portion 241. The first protrusion 24 includes a first straight portion 242. The first inclined portion 241 connects the conical surface 231 and the first straight portion 242 to form a smooth transition. The arrangement of the first straight portion 242 causes the outer layer 71 molten material to form a groove 711 when it passes through. As the second inclined portion 243 gradually contracts, the inner layer 72 molten material enters the groove 711 through the first groove 247.

[0045] like Figure 2 As shown, as a further configuration, the first protrusion 24 also includes a third inclined portion 244, which is connected to the second inclined portion 243 at its inclined end in the axial direction of the second mold sleeve 2. The third inclined portion 244 gradually inclines away from the axial direction of the second mold sleeve 2 along the flow direction of the molten material in the gap cavity 5. The first protrusion 24 also includes a second straight portion 245 located to the right of the third inclined portion 244. As the molten material passes through the third inclined portion 244 and the second straight portion 245, it is subjected to radial outward compression along the second mold sleeve 2, causing the molten material of the inner layer 72 to be compacted in the groove 711, reducing the gap, so as to better form an interlocking structure. At the same time, as Figure 8 , Figure 6As shown, the outer wall of the first protrusion 24 is provided with a second protrusion 250, which protrudes radially outward along the outer wall of the first protrusion 24. The second protrusion 250 is located on both sides of the third inclined portion 244, and its length direction is along the axial direction of the first protrusion 24. During the compaction process of the molten material in the inner layer 72 within the groove 711, the second protrusion 250 simultaneously compresses the molten material, and the auxiliary protrusion 721 and the groove 711 form an interlocking structure.

[0046] like Figure 2 As shown, the first protrusion 24 also includes a fourth inclined portion 246. The fourth inclined portion 246 gradually tilts towards the side closer to the axis of the second mold sleeve 2 along the direction of molten material flow in the gap cavity 5. The fourth inclined portion 246 is connected to the side of the third inclined portion 244 away from the second inclined portion 243. The second mold sleeve 2 is provided with a second groove 248. The second groove 248 passes through the second inclined portion 243 radially along the second mold sleeve 2. The two ends of the second groove 248 are respectively connected to the cavity 4 and the gap cavity 5. The function of the fourth inclined portion 246 is the same as that of the second inclined portion 243, and will not be described again.

[0047] The above description is merely a preferred embodiment of the present invention. The scope of protection of the present invention is not limited to the above embodiments. All technical solutions falling within the scope of the present invention's concept are within the scope of protection of the present invention. It should be noted that for those skilled in the art, any improvements and modifications made without departing from the principles of the present invention should also be considered within the scope of protection of the present invention.

Claims

1. A method for preparing a double-layer antibacterial polyvinyl chloride composite pipe, characterized in that, Includes the following steps: S1: Inner layer antibacterial material mixture: ① Add 55% PVC resin, 27.5% calcium carbonate, 4.4% stabilizer, 3% CPE, and 1.2% composite lubricant to a hot mixer and heat mix to 80℃ by weight percentage. ② Add 8.3% plasticizer and 0.6% antibacterial agent, and continue hot mixing to 120℃; ③ Transfer the materials to a cold mixer and cold mix at 60°C to obtain an inner layer antibacterial material mixture; S2: Preparation of inner layer antibacterial particles: The mixture of inner antibacterial materials obtained in S1 is fed into a granulator for granulation to obtain inner antibacterial granules. S3: Double-layer co-extrusion molding: The inner antibacterial granules obtained from S2 and the outer PVC-U substrate were respectively added to the corresponding barrels of a co-extrusion machine for extrusion molding to obtain a composite pipe (7); The composite pipe (7) includes an outer layer (71) and an inner layer (72). The outer layer (71) is formed by curing the outer PVC-U substrate, and its wall thickness accounts for 87.5% of the wall thickness of the composite pipe (7). The inner layer (72) is formed by curing the inner antibacterial particles, and its wall thickness accounts for 12.5% ​​of the wall thickness of the composite pipe (7). The composite lubricant is composed of a silane coupling agent and a polyethylene wax, wherein the mass ratio of the silane coupling agent to the polyethylene wax is 1:1 to 3:1; The calcium carbonate is light calcium carbonate, the PVC-type resin is PVC-5 resin, the antibacterial agent is nano-silver antibacterial agent or quaternary ammonium salt antibacterial agent, the stabilizer is calcium-zinc composite stabilizer, and the plasticizer is dioctyl phthalate; The preparation method uses a co-extrusion molding equipment, which includes a co-extrusion die. The co-extrusion die includes a first die sleeve (1), a second die sleeve (2), and a die rod (3). The die rod (3) is inserted into the second die sleeve (2), and the second die sleeve (2) is inserted into the first die sleeve (1). A gap cavity (5) is formed between the first die sleeve (1) and the second die sleeve (2). The gap cavity (5) allows the outer PVC-U substrate melt to flow through it. The second die sleeve (2) and the die rod (3) are connected in a co-extrusion molding equipment. A cavity (4) is formed between the rods (3), and the cavity (4) is through which the inner layer of antibacterial granules melt flows. The mold rod (3) includes a sizing part (33), and a shaping cavity (6) is formed between the sizing part (33) and the first mold sleeve (1). The melt in the cavity (4) and the gap cavity (5) converge in the shaping cavity (6). The outer wall of the second mold sleeve (2) is provided with a first protrusion (24), and multiple first protrusions (24) are evenly distributed along the circumference of the second mold sleeve (2). The first protrusion (24) includes a second inclined portion (243), which gradually tilts towards the axis of the second mold sleeve (2) along the flow direction of the molten material in the gap cavity (5). The second mold sleeve (2) is provided with a first groove (247), which penetrates the second inclined portion (243) radially along the second mold sleeve (2). The two ends of the first groove (247) are respectively connected to the cavity (4) and the gap cavity (5). The first protrusion (24) further includes a third inclined portion (244), which is connected to the second inclined portion (243) at its inclined end in the axial direction of the second mold (2). The third inclined portion (244) gradually inclines away from the axial direction of the second mold (2) along the flow direction of the molten material in the gap cavity (5).

2. The method for preparing a double-layer antibacterial polyvinyl chloride composite pipe according to claim 1, characterized in that, During the S3 co-extrusion molding process, the melting temperature of the inner antibacterial material is controlled at 160-180℃, and the melting temperature of the outer PVC-U substrate is controlled at 170-190℃.

3. The method for preparing a double-layer antibacterial polyvinyl chloride composite pipe according to claim 1, characterized in that, The outer wall of the first protrusion (24) is provided with a second protrusion (250), the second protrusion (250) is located on both sides of the third inclined portion (244), and the length direction of the second protrusion (250) is along the axial direction of the first protrusion (24).

4. The method for preparing a double-layer antibacterial polyvinyl chloride composite pipe according to claim 1, characterized in that, The first protrusion (24) further includes a fourth inclined portion (246), which is inclined towards the side closer to the axis of the second mold sleeve (2) along the flow direction of the molten material in the gap cavity (5). The fourth inclined portion (246) is connected to the side of the third inclined portion (244) away from the second inclined portion (243). The second mold sleeve (2) is provided with a second groove (248), which passes through the second inclined portion (243) radially along the second mold sleeve (2). The two ends of the second groove (248) are respectively connected to the cavity (4) and the gap cavity (5).

Citation Information

Patent Citations

  • Master batch with carbon nano tube as black pigment

    CN106147011A

  • Composition, crosslinked body and application thereof

    JP2016030810A