A bifunctional polyetheramine additive for efficient purification and separation of crude coal gas and its application

The bifunctional polyetheramine additive prepared by the microchannel reactor solves the problems of cleaning, dispersion and demulsification separation in the crude coal gas ammonia water system, achieving efficient purification and separation, simplifying the process and reducing costs.

CN122465133BActive Publication Date: 2026-11-17SOUTH CHINA UNIV OF TECH +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202610344930.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-03-20
Publication Date
2026-11-17
Estimated Expiration
2046-03-20

AI Technical Summary

Technical Problem

The existing technology lacks a dual-function additive that can efficiently clean and disperse and rapidly demulsify and separate crude coal gas ammonia water systems. This leads to increased turbidity and viscosity of the circulating ammonia water caused by the emulsion, increasing equipment load and environmental pollution. Furthermore, traditional agents may introduce new pollutants or have poor biodegradability.

Method used

A bifunctional polyetheramine additive was prepared using a microchannel reactor. Through block polymerization and precise ring-opening addition reaction, a linear polyetheramine compound was formed, which has cleaning and demulsification functions. Oil-water separation was achieved by utilizing the synergistic effect of hydrophobic and hydrophilic blocks and polyamine groups.

Benefits of technology

It achieves efficient purification and separation of crude coal gas, simplifies the process flow, reduces costs, avoids equipment blockage and corrosion, and improves the recovery rate of valuable substances and wastewater treatment efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
  • Figure SMS_5
    Figure SMS_5
Patent Text Reader

Abstract

This invention discloses a bifunctional polyetheramine additive for efficient purification and separation of crude coal gas and its applications. The additive uses lauryl alcohol as an initiator, undergoing block polymerization with propylene oxide and ethylene oxide sequentially. Following epichlorohydrin bridging and alkali-based ring closure to generate terminally epoxy-containing polyethers, the additive is finally amination-terminated in a microchannel reactor with polyethylene polyamine at a 1:1 molar ratio of epoxy groups to primary amine groups, forming a linear polyetheramine compound. This additive possesses a linear "hydrophobic-hydrophilic-polyamine" structure, enabling simultaneous efficient cleaning and rapid demulsification in a weakly alkaline ammonia system. This dual-effect additive significantly improves oil-water separation efficiency and oil recovery rate, simplifies the dosing process, and reduces operating costs. The preparation process utilizes a microchannel reactor for continuous synthesis, allowing for precise control of reaction conditions. The resulting product has a well-defined structure and narrow molecular weight distribution, making it suitable for crude coal gas purification and emulsion treatment in industries such as coal chemical and coking.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of industrial gas purification technology, specifically relating to a bifunctional polyetheramine additive for achieving efficient purification and separation of crude gas and its application, particularly a polyetheramine compound that combines efficient cleaning and rapid demulsification functions. Background Technology

[0002] In industries such as coal chemical and coking, the produced crude coal gas contains a large number of impurities, such as dust, tar, naphthalene, hydrogen sulfide, and ammonia. Currently, ammonia water scrubbing is widely used for preliminary purification of crude coal gas. In ammonia water, the tar in the crude coal gas (especially light tar and phenolic substances) readily forms an extremely stable oil / water / dust emulsion system under the action of flow shear force and surfactants. This emulsion is highly stable, and gravity settling alone is insufficient for effective separation in a short time, leading to increased load on subsequent processes. The emulsion causes increased turbidity and viscosity of the circulating ammonia water, not only reducing its scrubbing effect but also forming viscous deposits in equipment and pipelines, causing blockages, corrosion, and reduced heat transfer efficiency. If the emulsified ammonia water, rich in toxic substances such as phenols and cyanides, cannot be effectively demulsified, valuable substances are difficult to recover, and subsequent wastewater treatment becomes more difficult and costly, resulting in environmental pollution and resource waste.

[0003] Traditional cleaning agents focus on dispersion and wetting, but may exacerbate emulsification; while traditional demulsifiers have a single function and lack front-end cleaning and dispersion capabilities; they are inefficient, requiring the addition of two or more agents, increasing system complexity and cost; some traditional agents may have poor biodegradability or introduce new contaminants. Current technology lacks a highly efficient additive that can efficiently clean and disperse crude coal gas in an ammonia-water system first, and then rapidly demulsify and separate it, combining these two functions into one. Summary of the Invention

[0004] To address the shortcomings and deficiencies of existing technologies, the primary objective of this invention is to provide a bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas. This additive comprises hydrophobic polyoxypropylene (PO) blocks, hydrophilic polyoxyethylene (EO) blocks, and terminal polyamine groups. The entire molecule exhibits a linear or slightly branched linear structure, enabling simultaneous cleaning and demulsification of the crude coal gas ammonia-water system, simplifying the process, improving efficiency, and reducing costs.

[0005] Another objective of this invention is to provide a method for preparing the aforementioned bifunctional polyetheramine additive for efficient purification and separation of crude coal gas. This invention uses lauryl alcohol as a starting agent, and in the presence of a catalyst, it undergoes block polymerization with propylene oxide (PO) and ethylene oxide (EO) to form a polyether alcohol intermediate. Then, the polyether alcohol intermediate reacts with epichlorohydrin to generate a chlorinated polyether intermediate. Subsequently, the chlorinated polyether intermediate undergoes an intramolecular ring-closure reaction under alkaline conditions to generate a highly active terminal epoxy polyether. Finally, through a microchannel reactor, the epoxy groups of the terminal epoxy polyether undergo a ring-opening addition reaction with a polyethylenepolyamine (such as triethylenetetramine) in a precise 1:1 molar ratio to form a linear polyetheramine compound.

[0006] This invention employs a continuous preparation method using a microchannel reactor, which has the advantages of high reaction efficiency, stable product quality, and ease of scale-up production.

[0007] Another object of the present invention is to provide the application of the above-mentioned bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas in crude coal gas absorption and oil-water separation.

[0008] To achieve this objective, the present invention adopts the following technical solution:

[0009] In a first aspect, the present invention provides a bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas, the structural formula of which is:

[0010] C 12 H 25 O-(PO) m -(EO) n -CH2-CH(OH)-CH2-NH-(CH2CH2NH) p -CH2CH2NH2, where m is 5-10, n is 8-12, and p is 1-2.

[0011] Preferably, m is 8, n is 10, and p is 2.

[0012] Secondly, the present invention provides a method for preparing the above-mentioned bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas, comprising the following steps:

[0013] (1) Synthesis of block polyether intermediate: Initiator lauryl alcohol and catalyst were added to the reactor and heated to the polymerization reaction temperature under an inert gas atmosphere. Propylene oxide (PO) was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of propylene oxide. After the introduction of propylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. Ethylene oxide (EO) was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of ethylene oxide. After the introduction of ethylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. After cooling, lauryl alcohol-PO-EO block polyether intermediate was obtained.

[0014] The reaction formula for step (1) is as follows:

[0015]

[0016] (2) Preparation of chlorinated polyether intermediate: The lauryl alcohol-PO-EO block polyether intermediate obtained in step (1) is mixed with epichlorohydrin and reacted under acid catalyst and heating conditions to obtain chlorinated polyether intermediate;

[0017] The reaction formula for step (2) is as follows:

[0018]

[0019] (3) Synthesis of terminal epoxy polyether: The chlorinated polyether intermediate obtained in step (2) is mixed with an alkaline solution to carry out an intramolecular ring-closing reaction. After separation and purification, terminal epoxy polyether is obtained.

[0020] The reaction formula for step (3) is as follows:

[0021]

[0022] (4) Linear amination end-capping reaction: The epoxy polyether obtained in step (3) and polyethylene polyamine are continuously pumped into a microchannel reactor in a 1:1 molar ratio and reacted at 120-160℃ and 0.5-2.0 MPa pressure. The material residence time is 5-30 minutes to obtain a polyetheramine additive with both cleaning and demulsification functions.

[0023] The reaction formula for step (4) is as follows:

[0024] .

[0025] Under the conditions of step (4) of this invention, the epoxy group at the end of the epoxy-terminated polyether undergoes a ring-opening addition reaction with the primary amino group of the polyethylene polyamine molecule, forming a linear polyetheramine through single bridging of the polyethylene polyamine molecule; the reaction effluent is collected and post-processed to obtain the linear polyetheramine additive. In the amination-capping reaction, the high nucleophilicity of the primary amino group (-NH2) of the polyethylene polyamine (such as TETA) molecule is utilized to enable it to undergo an efficient and quantitative ring-opening addition reaction with the epoxy group of the epoxy-terminated polyether. The feed molar ratio of the epoxy group of the epoxy-terminated polyether to the polyethylene polyamine (such as triethylenetetramine) is precisely controlled at 1:1 by a microchannel reactor to ensure that each TETA molecule reacts with one epoxy-terminated polyether molecule, thereby forming a linear polyetheramine with an increased molecular weight and terminal polyamine. Under these conditions, by precisely controlling the amount of polyethylene polyamine and epoxy-terminated polyether molecule added and by conducting a continuous reaction in a microchannel reactor, the generation of branching or cross-linking byproducts is avoided.

[0026] Preferably, the catalyst in step (1) is an alkaline catalyst, including at least one of alkali metal hydroxide and alkali metal alkoxide, more preferably at least one of potassium hydroxide and sodium methoxide.

[0027] Preferably, the catalyst in step (1) accounts for 0.5 to 2.0% of the mass of lauryl alcohol, and more preferably 1.0 to 1.5%.

[0028] Preferably, the polymerization reaction temperature in step (1) is 110-130 °C, and more preferably 115-125 °C.

[0029] Preferably, the molar ratio of lauryl alcohol and propylene oxide in step (1) is 1:(5-10).

[0030] Preferably, in the block polyether intermediate of step (1), the molar ratio of PO / EO is (5-10):(8-12), more preferably 8:10.

[0031] Preferably, the inert gas atmosphere in step (1) includes at least one of nitrogen, argon and helium.

[0032] Preferably, the cooling in step (1) refers to cooling the material to 60-80 °C.

[0033] Preferably, the acid catalyst in step (2) is at least one of boron trifluoride diethyl ether complex, tin tetrachloride and p-toluenesulfonic acid.

[0034] Preferably, the acid catalyst in step (2) accounts for 0.2 to 0.5% of the mass of the lauryl alcohol-PO-EO block polyether intermediate.

[0035] Preferably, the molar ratio of lauryl alcohol-PO-EO block polyether intermediate to epichlorohydrin in step (2) is 1:(0.8-1.2), more preferably 1:(0.9-1.1), and most preferably 1:1.

[0036] Preferably, the heating temperature in step (2) is 60-90°C.

[0037] Preferably, the reaction time under the acid catalyst and heating conditions in step (2) is 2 to 4 hours.

[0038] Preferably, the alkali in the alkaline solution in step (3) is at least one of sodium hydroxide and potassium hydroxide, and its amount is 1.0 to 1.2 times the molar amount of chlorine atoms in the chlorinated polyether intermediate.

[0039] Preferably, the temperature of the intramolecular ring-closing reaction in step (3) is 40-80°C and the time is 1-3 hours.

[0040] Preferably, the concentration of the alkaline solution in step (3) is 1 to 10 mmol / mL; more preferably, it is 5 mmol / mL.

[0041] Preferably, the polyethylene polyamine in step (4) is at least one of triethylenetetramine (TETA) and diethylenetriamine (DETA), more preferably triethylenetetramine.

[0042] Preferably, the reaction temperature of the microchannel reactor in step (4) is 140-155℃, the pressure is 1.0-1.5MPa, and the material residence time is 10-20 minutes.

[0043] Thirdly, the present invention provides the application of the above-mentioned bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas in crude coal gas absorption and oil-water separation.

[0044] Preferably, the above-mentioned bifunctional polyetheramine additive for efficient purification and separation of crude coal gas is applied to the removal of complex scale formed by tar, asphaltene, polycyclic aromatic hydrocarbons, monocyclic aromatic hydrocarbons and dust, etc., generated in the absorption of crude coal gas by ammonia water and oil-water separation, and to the demulsification of emulsions.

[0045] Preferably, the polyetheramine additive that combines cleaning and demulsification functions has an application temperature ≥50 ℃ and the application system is weakly alkaline, specifically with a pH of 8.9 to 9.5.

[0046] Compared with the prior art, the present invention has the following advantages and beneficial effects:

[0047] (1) Molecular structure innovation (block design and TETA end capping)

[0048] The overall structure is a "comb-like" amphiphilic structure: hydrophobic chains (lauryl group + PO block) and hydrophilic chains (EO block + polyamine head group) are connected by rigid linkers. The PO / EO block provides moderate interfacial activity and penetration, assisting the polyamine group to reach and act on the oil-water interface, while the EO block ensures the overall water solubility of the molecule. The multiple terminal amine groups are highly polar and can strongly bind with acidic components in tar (such as asphaltenes and naphthenic acids) through acid-base interactions or hydrogen bonding, thus more effectively replacing natural emulsifiers and achieving rapid demulsification. The linear molecule achieves a sequential function of "first wetting and cleaning, then adsorption and demulsification".

[0049] (2) Chemical pathway innovation (epoxychloropropane bridging)

[0050] A precise synthetic route was adopted: "polyether alcohol → chloropolyether → (base ring closure) → terminal epoxy polyether → 1:1 amination". The key steps, namely epichlorohydrin bridging and base-catalyzed ring closure to generate highly reactive terminal epoxy polyethers, ensured the quantitative and directional nature of the reaction with polyamines. Compared to directly using bis- or poly-epoxy reagents, this route resulted in fewer side reactions and more precise molecular weight control.

[0051] (3) Innovation in preparation process (continuous synthesis using microchannel reactor)

[0052] The target product of this invention is a linear polyether amine with terminal polyamines formed by reacting reactive polyethers and amines in a 1:1 ratio. Therefore, it abandons the traditional batch-type batch reaction and innovatively conducts the amination reaction of terminal epoxy-based polyethers and polyamines continuously in a microchannel reactor. The core of this process lies in the efficient mixing and precise temperature control of the microchannel reactor, which solves the problems of amine over-crosslinking (one polyamine molecule connecting multiple polyether chains) or amine molecule residue caused by the non-selectivity of the reaction in traditional batch reactions. By strictly controlling the molar ratio of reactive polyether to amine to amine at 1:1 and utilizing the characteristics of the microchannel reactor to complete the reaction rapidly and uniformly, the degree of reaction is precisely controlled, avoiding the formation of branched or crosslinked byproducts, and ensuring the formation of a linear product with a well-defined structure and narrow molecular weight distribution. This process not only significantly shortens the reaction time and improves the stability of product performance, but also makes the production process safer and more controllable, which is a key technological guarantee for realizing the high-performance additives of this invention.

[0053] (4) Functional innovation (one dose, two effects)

[0054] This adjuvant integrates cleaning and demulsification functions on a single molecule. At the front end of the system, it leverages the hydrophilicity and dispersing power of the EO segments to clean with ammonia and absorb crude coal gas. At the back end of the system, or as the concentration accumulates, its hydrophobic structure rapidly occupies the interface, achieving oil-water separation. This enables intelligent switching and synergy of functions, truly realizing "dual effects with one agent," simplifying the dosing system and reducing overall costs. Detailed Implementation

[0055] The present invention will be further described in detail below with reference to embodiments, but the implementation of the present invention is not limited thereto.

[0056] Unless otherwise specified in the embodiments of this invention, the conditions shall be performed according to conventional conditions or conditions recommended by the manufacturer. All raw materials and reagents used, unless otherwise specified, are commercially available conventional products.

[0057] Example 1

[0058] Step 1: Add 186.3 g (1.0 mol) lauryl alcohol and 2.24 g (1.2% of lauryl alcohol by mass) potassium hydroxide flake catalyst to a 2L high-pressure reactor. Under nitrogen protection, heat to 120°C and evacuate to a vacuum (-0.095 MPa) while stirring and dehydrating for 30 minutes. Remove the vacuum, and under a nitrogen atmosphere, maintain the temperature at 120°C. Slowly add 464.5 g (8.0 mol) propylene oxide (PO) dropwise at constant pressure, controlling the pressure inside the reactor to not exceed 0.4 MPa. After the PO is added, maintain the temperature at 120°C for aging until the pressure drops to atmospheric pressure and remains constant for 30 minutes. Raise the temperature to 125°C and slowly add 440.4 g (10.0 mol) ethylene oxide (EO) using the same method, controlling the pressure to not exceed 0.4 MPa. After the addition is complete, maintain the temperature at 125°C until the pressure no longer decreases. The material was cooled to 80°C to obtain lauryl alcohol-PO-EO block polyether intermediate M-8 / 10.

[0059] Step 2: Take 218.2 g (0.20 mol, based on hydroxyl groups) of the product from Step 1 and place it in a 500 mL three-necked flask. Add 18.5 g (0.20 mol) of epichlorohydrin and 0.5 g of boron trifluoride diethyl ether complex. Stir the reaction mixture at 75 °C for 3 hours. Wash the reaction solution twice with a 5% sodium bicarbonate aqueous solution, and then wash with water until neutral. Dry the solution with anhydrous sodium sulfate and filter to obtain the chlorinated polyether intermediate.

[0060] Step 3: Dissolve all the chlorinated polyether intermediates obtained in Step 2 in 200 mL of toluene. Prepare a 40 mL aqueous solution containing 8.0 g (0.20 mol) NaOH, and slowly add it dropwise to the above solution at 55 °C. After the addition is complete, continue stirring for 2 hours. Allow the mixture to stand and separate the layers. Wash the organic phase with water until neutral, dry it, and then remove the toluene by rotary evaporation to obtain the epoxy-terminated polyether intermediate EP-8 / 10.

[0061] Step 4: Preheat the epoxy-terminated polyether intermediate EP-8 / 10 (containing approximately 0.10 mol of epoxy groups) obtained in Step 3 to 70°C as Material A. Weigh 14.6 g (0.10 mol) of triethylenetetramine (TETA, by molecular weight) as Material B. Set the microchannel reactor temperature to 150°C and the system pressure to 1.2 MPa. Pump Materials A and B into the reactor using a precision metering pump, controlling the total flow rate to maintain a residence time of 15 minutes, and precisely adjust the flow rate to ensure a molar feed ratio of epoxy groups in the epoxy-terminated polyether to triethylenetetramine of 1:1. Collect the effluent and distill it under reduced pressure at 100°C and -0.098 MPa to obtain a brownish-yellow viscous liquid, which is the target product sample A (linear polyether amine).

[0062] The intermediate synthesis method is the same as in Example 1, except that the feed amounts in step one are changed: PO is 580.6 g (10.0 mol), and EO is 352.3 g (8.0 mol). The product obtained in step one is designated as block polyether intermediate M-10 / 8, and the product obtained in step three is designated as epoxy polyether intermediate EP-10 / 8. Block polyether intermediate M-5 / 12 and epoxy polyether intermediate EP-5 / 12 are prepared using the same method.

[0063] Example 2

[0064] The toluene, n-octane, and asphaltenes toluene solution (10 wt%) were mixed thoroughly at a mass ratio of 7:2:1. The asphaltenes toluene solution provided the resin and asphaltenes.

[0065] Prepare a simulated oil stock solution with a total oil concentration of 8 g / L using the above mixture. Prepare an 8 wt% ammonia solution, adjust the pH to 9.0 ± 0.2 using ammonium chloride buffer, and obtain simulated ammonia solution. Accurately measure 200 mL of simulated ammonia solution into an absorption bottle and add 20.0 mg of coal powder. Add the analyte to achieve a final concentration of 200 mg / L in the system. Heat the system and maintain it at 80 °C. Accurately transfer 5.00 mL of the simulated oil stock solution (containing 40.0 mg of total oil) into the vaporization chamber. Introduce high-purity nitrogen as the carrier gas at a flow rate of 1.0 L / min. Rapidly heat the vaporization chamber to 160 °C to fully vaporize the oil and carry it into the absorption bottle with the carrier gas. The oil is then thoroughly contacted, washed, and absorbed by the ammonia solution containing the reagent through bubbling of the sintered glass core. This process lasts for 8 minutes.

[0066] Transfer all absorbed liquid to a 100 mL stoppered graduated cylinder and place it in an 80°C constant temperature water bath. Record the volume of the precipitated lower clear layer at regular intervals until the oil-water interface is clear and the volume no longer changes. Record the time (T) required for 90% oil-water separation. 90After standing for 30 minutes to ensure complete stratification, carefully and completely extract the entire upper oil phase using a microsyringe or capillary tube, transferring it to a pre-weighed (W1) weighing bottle. Dry the weighing bottle in a 105°C oven to constant weight (ensuring complete volatilization of toluene and n-octane, leaving only non-volatile components such as asphaltene), and weigh after cooling (W2). The recovered oil mass M = W2 - W1, and the total oil yield = M / 40.0. A higher oil yield indicates a greater total amount of oil washed and absorbed from the gas phase and ultimately recovered, indicating a better front-end cleaning and absorption effect.

[0067] Example 3: High PO type linear polyetheramine additive B

[0068] The synthesis method was the same as in Example 1, except that the epoxy-terminated polyether intermediate EP-8 / 10 in step four was replaced with an equal molar amount of epoxy-terminated polyether intermediate EP-10 / 8, which was reacted with TETA in a microchannel at the same 1:1 molar ratio. The resulting product was sample B.

[0069] Example 4: High EO type linear polyetheramine additive C

[0070] The synthesis method was the same as in Example 1, except that the terminal epoxy polyether intermediate EP-8 / 10 in step four was replaced with an equal molar amount of terminal epoxy polyether intermediate EP-5 / 12, which was reacted with TETA in a microchannel at the same 1:1 molar ratio. The resulting product was sample C.

[0071] The molecular weights of the prepared terminal epoxy polyether intermediates and samples A, B, and C were determined by gel permeation chromatography (GPC), and the results are shown in Table 1. The molecular weight of intermediate EP-8 / 10 was approximately 1220 Da. After reacting with triethylenetetramine (TETA, molecular weight 146) at a 1:1 molar ratio, the theoretical molecular weight should increase by approximately 144 Da (considering atomic rearrangement in ring-opening addition). The measured Mn of sample A was 1850 Da, consistent with the theoretical trend. Samples B and C showed slight differences in polyether repeating unit molecular weight due to different PO / EO ratios, resulting in Mn values ​​ranging from 1790 to 1910 Da. All samples had dispersion coefficients below 1.12, indicating a narrow molecular weight distribution, consistent with the characteristics of precise microchannel synthesis.

[0072] Table 1

[0073]

[0074] Fourier transform infrared spectroscopy (FTIR) was used to characterize the terminal epoxy group polyether intermediate and samples A, B, and C. Analysis of the results showed that the terminal epoxy group polyether intermediate was precipitated at 912 cm⁻¹. -1There is a distinct characteristic absorption peak of epoxy groups (epoxy ring antisymmetric stretching vibration), while this peak completely disappears in all linear polyetheramine products (A, B, C), and is also absent at 3350 cm⁻¹. -1 A strong, broad peak (superposition of NH and OH stretching vibrations) and a peak at 1640 cm⁻¹ were observed nearby. -1 The presence of an NH bending vibration peak directly proves that the epoxy group underwent a complete ring-opening addition reaction with triethylenetetramine (TETA), generating the target polyetheramine structure. The characteristic peak of the polyether chain is at 1105 cm⁻¹. -1 The presence of the substance before and after the reaction indicates that the polyether backbone remains intact during the amination process.

[0075] Comparative Example 1: Physical Mixture D

[0076] The epoxy-terminated polyether intermediate EP-8 / 10 (containing approximately 0.10 mol of epoxy groups) from step three of Example 1 was directly added to a beaker along with 14.6 g (0.10 mol) of triethylenetetramine (TETA, by molecular weight). The mixture was stirred and mixed at 25°C for 30 hours to obtain a homogeneous mixture, denoted as sample D. The molar ratio of polyether to TETA in this mixture was 1:1, which was exactly the same as the material ratio in the chemical reaction of step four of Example 1.

[0077] Comparative Example 2: Ethylamine-bridged linear polyetheramine E

[0078] The synthesis method was the same as in Example 1, except that in step four, triethylenetetramine (TETA) was replaced with 6.0 g (0.10 mol) ethylamine (MEA), which was reacted with the terminal epoxy polyether intermediate EP-8 / 10 in a microchannel at a molar ratio of n(polyether):n(ethylamine) = 1:1. The resulting product was sample E.

[0079] Comparative Example 3: Product F synthesized using conventional batch reactor

[0080] The epoxy-terminated polyether intermediate EP-8 / 10 (containing approximately 0.10 mol of epoxy groups) and 14.6 g (0.10 mol) of TETA were added to a 1L conventional stainless steel reactor. Under nitrogen protection, the mixture was stirred and heated to 150°C. Since the mass and heat transfer efficiency of a conventional batch reactor is much lower than that of a microchannel reactor, the reaction was refluxed at this temperature for 4 hours to ensure complete reaction. After the reaction was completed, vacuum distillation was performed using the same method to obtain sample F.

[0081] Comparative Example 4: Excess Polyether

[0082] The synthesis method was the same as in Example 1, but the amount of EP-8 / 10 was doubled (containing 0.20 mol of epoxy groups), while the amount of TETA remained at 0.10 mol, i.e., a molar ratio of 2:1. Sample G was obtained.

[0083] Comparative Example 5: PEI as the initiator

[0084] (1) Synthesis of block polyether intermediate: 60.0 g (approximately 0.10 mol based on nitrogen atoms) of polyethyleneimine (PEI, number-average molecular weight Mn=600) and 2.24 g of potassium hydroxide catalyst were added to a dry 2L high-pressure reactor. Following the method in step one of Example 1, under nitrogen protection, the temperature was raised to 120°C, and 464.5 g (8.0 mol) of propylene oxide (PO) was first introduced for polymerization. After the reaction was completed, 440.4 g (10.0 mol) of ethylene oxide (EO) was introduced for polymerization. After the reaction was completed and cooled, a star-shaped block polyether intermediate with PEI as the core was obtained, denoted as intermediate H-PO / EO.

[0085] (2) Chlorination and terminal epoxy: Following the methods in steps two and three of Example 1, the above intermediate H-PO / EO was reacted with epichlorohydrin and then cyclically closed with alkali to obtain a star-shaped polyether intermediate with terminal epoxy, denoted as H-EP.

[0086] (3) Amination-capping reaction: Following the method in step four of Example 1, the H-EP obtained in step (2) and polyethyleneimine (PEI) were continuously pumped into a microchannel reactor at a molar ratio of 1:1 for epoxy groups to primary amino groups. The reaction was carried out at 150°C and 1.2 MPa for 15 minutes. After the reaction was completed, the product was obtained by vacuum distillation, which was denoted as sample H.

[0087] The above samples were all tested according to Example 2. At the same time, the absorption and oil-water separation tests without any additives were used as blank controls. The results are shown in Table 2.

[0088] Table 2

[0089]

[0090] The above embodiments are preferred embodiments of the present invention, but the embodiments of the present invention are not limited to the above embodiments. Any changes, modifications, substitutions, combinations, or simplifications made without departing from the spirit and principle of the present invention shall be considered equivalent substitutions and shall be included within the protection scope of the present invention.

Claims

1. A bifunctional polyetheramine adjuvant for efficient purification and separation of raw coal gas, characterized in that, The structural formula is: C 12 H 25 O-(PO) m -(EO) n -CH2-CH(OH)-CH2-NH-(CH2CH2NH) p -CH2CH2NH2, wherein m is 5 to 10, n is 8 to 12, and p is 1 to 2; The preparation method of the bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas includes the following steps: (1) Synthesis of block polyether intermediate: The initiator lauryl alcohol and the catalyst were added to the reactor and heated to the polymerization reaction temperature under an inert gas atmosphere. Propylene oxide was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of propylene oxide. After the introduction of propylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. Ethylene oxide was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of ethylene oxide. After the introduction of ethylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. After cooling, lauryl alcohol-PO-EO block polyether intermediate was obtained. (2) Preparation of chlorinated polyether intermediate: The lauryl alcohol-PO-EO block polyether intermediate obtained in step (1) is mixed with epichlorohydrin and reacted under acid catalyst and heating conditions to obtain chlorinated polyether intermediate; (3) Synthesis of terminal epoxy polyether: The chlorinated polyether intermediate obtained in step (2) is mixed with an alkaline solution to carry out an intramolecular ring-closing reaction. After separation and purification, terminal epoxy polyether is obtained. (4) Linear amination end-capping reaction: The epoxy polyether obtained in step (3) and polyethylene polyamine are continuously pumped into a microchannel reactor at a molar ratio of epoxy to polyethylene polyamine of 1:

1. The reaction is carried out at 120-160℃ and 0.5-2.0 MPa pressure. The material residence time is 5-30 minutes to obtain a polyetheramine additive with both cleaning and demulsification functions.

2. The method for preparing the bifunctional polyetheramine adjuvant for realizing efficient purification and separation of the crude coal gas according to claim 1, characterized in that, Includes the following steps: (1) Synthesis of block polyether intermediate: The initiator lauryl alcohol and the catalyst were added to the reactor and heated to the polymerization reaction temperature under an inert gas atmosphere. Propylene oxide was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of propylene oxide. After the introduction of propylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. Ethylene oxide was introduced and the pressure inside the reactor was maintained at 0.2-0.5 MPa during the introduction of ethylene oxide. After the introduction of ethylene oxide, the polymerization reaction continued until the pressure inside the reactor dropped significantly and then stabilized again. After cooling, lauryl alcohol-PO-EO block polyether intermediate was obtained. (2) Preparation of chlorinated polyether intermediate: The lauryl alcohol-PO-EO block polyether intermediate obtained in step (1) is mixed with epichlorohydrin and reacted under acid catalyst and heating conditions to obtain chlorinated polyether intermediate; (3) Synthesis of terminal epoxy polyether: The chlorinated polyether intermediate obtained in step (2) is mixed with an alkaline solution to carry out an intramolecular ring-closing reaction. After separation and purification, terminal epoxy polyether is obtained. (4) Linear amination end-capping reaction: The epoxy polyether obtained in step (3) and polyethylene polyamine are continuously pumped into a microchannel reactor at a molar ratio of epoxy to polyethylene polyamine of 1:

1. The reaction is carried out at 120-160℃ and 0.5-2.0 MPa pressure. The material residence time is 5-30 minutes to obtain a polyetheramine additive with both cleaning and demulsification functions.

3. The preparation method according to claim 2, characterized in that, The molar ratio of lauryl alcohol to propylene oxide in step (1) is 1:(5-10); And / or, in the block polyether intermediate of step (1), the molar ratio of PO / EO is (5-10):(8-12).

4. The preparation method according to claim 2, characterized in that, In step (1), the molar ratio of PO / EO in the block polyether intermediate is 8:

10.

5. The preparation method according to claim 2 or 3, characterized in that, The polyethylene polyamine mentioned in step (4) is at least one of triethylenetetramine and diethylenetriamine; And / or, the reaction temperature of the microchannel reactor in step (4) is 140-155℃, the pressure is 1.0-1.5 MPa, and the material residence time is 10-20 minutes.

6. The preparation method according to claim 2 or 3, characterized in that, The polyethylene polyamine mentioned in step (4) is triethylenetetramine.

7. The preparation method according to claim 2 or 3, characterized in that, In step (2), the molar ratio of lauryl alcohol-PO-EO block polyether intermediate to epichlorohydrin is 1:(0.8-1.2). And / or, the heating temperature in step (2) is 60–90°C; And / or, the reaction time under the acid catalyst and heating conditions described in step (2) is 2 to 4 hours.

8. The preparation method according to claim 2 or 3, characterized in that, The molar ratio of lauryl alcohol-PO-EO block polyether intermediate to epichlorohydrin in step (2) is 1:(0.9~1.1).

9. The preparation method according to claim 2 or 3, characterized in that, The catalyst in step (1) is an alkaline catalyst, including at least one of alkali metal hydroxide and alkali metal alkoxide; And / or, the catalyst described in step (1) accounts for 0.5% to 2.0% of the mass of lauryl alcohol; And / or, the polymerization reaction temperature in step (1) is 110 to 130 °C.

10. The preparation method according to claim 2 or 3, characterized in that, The catalyst in step (1) is at least one of potassium hydroxide and sodium methoxide; And / or, the catalyst described in step (1) accounts for 1.0 to 1.5% of the mass of lauryl alcohol; And / or, the polymerization reaction temperature in step (1) is 115 to 125 °C.

11. The preparation method according to claim 2 or 3, characterized in that, The acid catalyst in step (2) is at least one of boron trifluoride diethyl ether complex, tin tetrachloride, and p-toluenesulfonic acid; And / or, the acid catalyst in step (2) accounts for 0.2 to 0.5% of the mass of the lauryl alcohol-PO-EO block polyether intermediate.

12. The preparation method according to claim 2 or 3, characterized in that, The alkali in the alkaline solution in step (3) is at least one of sodium hydroxide and potassium hydroxide, and its amount is 1.0 to 1.2 times the molar amount of chlorine atoms in the chlorinated polyether intermediate; And / or, the temperature of the intramolecular ring-closing reaction in step (3) is 40-80°C and the time is 1-3 hours; And / or, the concentration of the alkaline solution in step (3) is 1 to 10 mmol / mL.

13. The preparation method according to claim 2 or 3, characterized in that, The concentration of the alkaline solution in step (3) is 5 mmol / mL.

14. The preparation method according to claim 2 or 3, characterized in that, The inert gas atmosphere in step (1) includes at least one of nitrogen, argon and helium; And / or, the cooling in step (1) refers to cooling the material to 60-80 °C.

15. The application of the bifunctional polyetheramine additive for achieving efficient purification and separation of crude coal gas as described in claim 1 in crude coal gas absorption and oil-water separation.

Citation Information

Patent Citations

  • Dewatering demulsifier for triple composite driven extract and its production