A staged variable-angle outer cylindrical grinding method for high-precision thin-walled bearing outer rings
By using a phased variable-angle external cylindrical grinding method, the support angle and grinding parameters are dynamically adjusted, solving the problem that existing technologies cannot simultaneously eliminate the triangular edge circle error and ellipticity error of the outer circle of aerospace thin-walled bearings, thus achieving high-precision and high-efficiency thin-walled bearing processing.
Patent Information
- Application Number
- CN202611118495.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-27
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2046-07-27
AI Technical Summary
Existing technologies cannot simultaneously eliminate the triangular edge circle error and ellipticity error of the outer circle of aerospace thin-walled bearings in the same processing step, and traditional small-allowance grinding processes are difficult to meet the production requirements of high precision and high efficiency.
A staged variable-angle external cylindrical grinding method is adopted, which divides the grinding process into two stages. By dynamically adjusting the workpiece support angle, different types of shape errors, including triangular edge roundness error and ellipticity error, are eliminated. Wear-resistant carbide support blocks and flexibly adjustable support point angles are used, along with grinding parameters optimized for different stages.
The system simultaneously addresses two types of shape errors in thin-walled bearings within the same machining process, achieving high-precision machining, improving machining efficiency, adapting to the machining needs of various specifications of thin-walled bearings, and meeting P2/P4 level precision standards.
Smart Images

Figure CN122606417B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of precision bearing machining technology, specifically relating to a staged variable-angle outer cylindrical grinding method for high-precision thin-walled bearing outer rings, which is particularly suitable for small-mass, high-precision outer cylindrical grinding of thin-walled bearings in aerospace precision equipment such as aero-engines, transmission systems, and precision gyroscopes. Background Technology
[0002] Thin-walled bearings possess advantages such as light weight, compact structure, and high load-bearing capacity, and are widely used in aerospace precision equipment fields such as aero-engines, transmission systems, and precision gyroscopes. As a core basic component of aerospace equipment, aerospace-specific thin-walled bearings have stringent requirements for machining accuracy. Their dimensional accuracy and geometrical accuracy levels typically need to reach P4 or even P2 level, and extremely high standards are set for key geometrical tolerances such as elliptical and triangular outer diameters. At the same time, these bearings have thinner ring walls and weaker structural rigidity, belonging to typical easily deformable and weakly rigid components, making their machining and manufacturing significantly more difficult than ordinary standard bearings.
[0003] The outer diameter of a bearing is not only a crucial process reference for subsequent raceway finishing but also a positioning reference for the assembly and installation of the finished bearing. The machining quality of the outer diameter directly affects the overall rotational accuracy, vibration performance, and service life of the bearing. Currently, the industry commonly uses a plunge-type one-step grinding process for bearing outer diameter grinding: while maintaining a constant support angle, the outer diameter of the workpiece is ground to the design size in one go. This process can meet the mass production needs of conventional wall thickness bearings and has a high degree of technological maturity. However, this process is less suitable for machining aerospace precision thin-walled bearings. Due to the poor rigidity of thin-walled rings, they are easily deformed by grinding stress. To avoid machining deformation, the industry generally adopts a small-allowance grinding method, limiting the single-sided grinding allowance to the range of 0.05mm to 0.10mm.
[0004] The purpose of using a small-allowance grinding process is mainly reflected in two aspects: First, if the grinding allowance is too large, the grinding force and grinding heat generated during the machining process will increase simultaneously, which can easily induce elastic deformation of the thin-walled bearing, and in severe cases, plastic deformation. After the workpiece is machined and the constraints are removed, stress rebound will cause the outer diameter roundness to exceed the tolerance, directly leading to the scrapping of the workpiece. Second, the large-allowance grinding process takes longer, which will not only reduce production efficiency, but also expose the thin-walled bearing to a complex grinding environment of high temperature and pressure for a long time, further increasing the risk of deformation. Therefore, the outer cylindrical grinding process of aerospace thin-walled bearings must take into account the three core production requirements of small grinding allowance, high machining efficiency, and ultra-high machining accuracy.
[0005] Under small-mass grinding conditions, traditional single-pass forming grinding processes still have significant technical defects, making it difficult to simultaneously eliminate triangular edge circle errors and ellipticity errors at the outer diameter of the workpiece, thus failing to meet the high-precision machining requirements of aerospace bearings. To address these issues, the industry has successively proposed several optimization solutions: Public patent CN222155173U discloses a support structure for grinding the outer diameter of thin-walled bearings. This structure is equipped with a 90° arc-shaped support block, which can effectively improve the stability of the workpiece during grinding. However, the angle of this support structure is fixed, making it impossible to specifically optimize for different orders of shape errors. Public patent CN202752973U provides a device for eliminating ellipticity errors in the grinding of bearing outer rings. This device uses a 60° fork-shaped V-shaped support structure to achieve three-point positioning and combines the principle of three-fold error amplification to optimize the ellipticity of the workpiece. However, this device can only solve the ellipticity error problem and cannot handle triangular edge circle errors. Furthermore, the support angle is not adjustable, making it difficult to adapt to the corresponding processing mode according to the radial stiffness parameters of different thin-walled bearings.
[0006] Based on comprehensive analysis, existing thin-walled bearing external cylindrical grinding technology cannot meet the actual production needs of the aerospace industry, which require small allowances, high precision, and high efficiency. Specific technical shortcomings are as follows: First, the traditional fixed-angle, single-stage plunge grinding process cannot simultaneously eliminate two different orders of shape errors—triangular ridge circle and ellipticity—within the same machining operation. Second, while the small allowance mode can reduce grinding deformation and shorten processing time, it also significantly compresses the error correction process window; existing technologies lack phased, directional error correction process solutions. Third, the existing machining system lacks a mature flexible grinding strategy and cannot dynamically adjust the support angle and machining parameters based on the radial stiffness parameters of the thin-walled bearing and the real-time error state of the workpiece.
[0007] In summary, there is an urgent need to develop a high-precision external cylindrical grinding method that is suitable for the small-mass grinding conditions of aerospace thin-walled bearings and can simultaneously eliminate triangular edge circle errors and ellipticity errors, so as to make up for the gaps and shortcomings of existing technologies. Summary of the Invention
[0008] To address the shortcomings of existing technologies, this invention provides a staged variable-angle outer cylindrical grinding method for high-precision thin-walled bearing outer rings. By employing a staged variable-angle grinding strategy, different order shape errors are specifically eliminated, significantly improving the overall machining accuracy of the thin-walled bearing outer ring while strictly controlling machining deformation.
[0009] To achieve the above objectives, the technical solution adopted in this invention is: a staged variable-angle outer cylindrical grinding method for high-precision thin-walled bearing outer rings, applicable to the final grinding process of the outer cylindrical rings of weakly rigid thin-walled bearings with a single-sided grinding allowance of 0.05~0.10mm. The final grinding process is divided into two independent grinding stages that are connected sequentially. By dynamically adjusting the workpiece support angle, different types of shape errors are eliminated in a directional manner. Specifically, the method includes the following steps: S1, Pre-processing: The rough grinding and semi-finish grinding of the outer ring of the thin-walled bearing are completed in sequence, and a final grinding allowance of 0.05mm~0.10mm is reserved on the outer circle of one side; the outer ring of the thin-walled bearing is clamped on the electromagnetic centerless chuck of the grinding machine tool, and the outer circle of the thin-walled bearing is supported on the two support points of the double support mechanism. S2, execute the first stage, perform triangular edge rounding error elimination grinding: adjust the double-support mechanism to adjust the included angle α2 of the two support points supporting the outer ring of the thin-walled bearing to 20°~60° in the first stage; the grinding wheel performs continuous infeed grinding on the outer circle of the thin-walled bearing outer ring at a constant linear speed, grinding away 50%~70% of the final grinding allowance of the single-sided outer circle; S3, the second stage is executed, which involves grinding to eliminate ellipticity errors: After completing the triangular edge circle error elimination operation, firstly, the double-support mechanism is readjusted, and the included angle α3 between the two support points in the second stage is adjusted to 60°~110°; then, based on the first stage, the feed speed is reduced and the grinding wheel linear speed is increased to complete the fine removal of the remaining single-sided outer circle final grinding allowance; then, the finishing grinding stage is entered, the radial feed is canceled, and the thin-walled bearing outer ring is kept to rotate synchronously with the grinding wheel, and finishing grinding is performed for a fixed duration, finally machining the outer circle dimension to the product design specifications; S4. Post-processing inspection: After grinding, slowly remove the support constraints of the outer ring of the thin-walled bearing, let it stand for 3-5 minutes to allow the stress to be released naturally, and use testing instruments to check the outer diameter of the thin-walled bearing, such as ellipticity and triangularity, and screen qualified workpieces.
[0010] Its beneficial effects are as follows: In the first stage, this invention focuses on efficient material removal with large allowance and correction of the original third-order deformation error. The small-angle support mode alters the stress deformation law of the bearing ring, creating a specific correction effect for the third-order triangular edge round error, offsetting the original triangular edge round error on the outer surface of the workpiece. Simultaneously, it rationally controls the cutting load, avoiding elastic and plastic deformation problems caused by large cutting amounts. In the second stage, the medium-to-large angle support mode optimizes the radial force distribution of the bearing ring, adapting to the need for second-order elliptic error correction. Combined with the finishing process, it further releases residual grinding stress, eliminates microscopic tool marks, corrects residual ellipticity errors, and optimizes the surface roughness of the workpiece. Thus, it simultaneously solves the two most critical types of shape errors in thin-walled bearings within the same set of processing steps, fundamentally overcoming the technical bottleneck of traditional processes that cannot simultaneously address second-order and third-order errors.
[0011] The present invention employs a differentiated non-uniform allowance distribution method in two grinding stages to adapt to different processing attributes of rough grinding and fine grinding: the first stage removes 50% to 70% of the total allowance on one side, focuses on correcting the original triangular edge circle error, and removes most of the processing allowance; the second stage removes the remaining allowance, refines the shape with a small allowance, corrects the elliptical error and ensures dimensional accuracy and surface quality, and balances the error correction effect with the overall grinding efficiency.
[0012] Furthermore, in step S2, the included angle α2 between the centers of the two support points in the first stage is 30°~45°.
[0013] Its beneficial effects are: this angle range is the optimal correction range for third-order errors, which can maximize the correction efficiency of triangular edge circle errors, while also dispersing the grinding force, reducing the risk of local stress concentration in the workpiece during grinding, and is suitable for most ultra-thin wall bearing processing conditions.
[0014] Furthermore, in step S2, the grinding process parameters are set as follows: grinding wheel linear speed 25~35m / s, grinding wheel feed speed 0.03~0.05mm / min, thin-walled bearing outer ring speed 60~120r / min, wet grinding is used throughout the process, and grinding fluid flow rate is 6~8L / min.
[0015] Its beneficial effects are: this stage is the error correction rough grinding stage, and its process parameters focus on removing excess material and correcting the error of the triangular edge circle.
[0016] Furthermore, in step S3, the included angle α3 between the centers of the two support points in the second stage is 75°~90°.
[0017] Its beneficial effects are: this angle range is the optimal range for second-order elliptic error correction, which can be adapted to the radial stiffness characteristics of most aerospace thin-walled bearings, completely eliminate the ellipticity error remaining in the later stage of grinding, and at the same time take into account the support stability and error correction capability.
[0018] Furthermore, in step S2, the grinding process parameters are set as follows: grinding wheel linear speed 30~40m / s, which is 15%~20% higher than that in the first stage; grinding wheel feed speed 0.01~0.03mm / min; thin-walled bearing outer ring speed 100~200r / min; grinding fluid flow rate 8~10L / min.
[0019] Its beneficial effects are: the second stage is the dimensional finishing stage, which focuses on precision shaping and surface quality control. The overall finishing parameter logic is "high speed, low feed, and strong heat dissipation": the increase in grinding wheel linear speed can optimize the surface texture of the workpiece; the grinding wheel feed accuracy is higher than that of the first grinding stage, which can reduce cutting deformation; the increase in grinding fluid flow can enhance the heat dissipation and cooling effect in high-temperature areas and prevent grinding burns.
[0020] Furthermore, the position of at least one support point in the dual-support mechanism is adjustable to adjust the size of the included angle between the centers of the two support points.
[0021] Its beneficial effects are: the position of the support point is adjustable, which makes it easy to accurately match the optimal support angle between the two stages and meet the angle control requirements of high-precision graded grinding.
[0022] Furthermore, both support points in the dual-support mechanism are support pads made of wear-resistant hard alloy material, and the support pads are installed on the corresponding connecting frame.
[0023] Its beneficial effects are: the support pad is made of wear-resistant hard alloy to avoid long-term wear of the support part affecting the machining reference.
[0024] Compared with existing traditional fixed-angle single-stage forming grinding technology, the present invention has the following advantages: 1. Graded shaping to simultaneously eliminate dual errors: This invention innovatively adopts a variable angle segmented grinding architecture, relying on small included angles (20°~60°) to target and correct the third-order triangular edge circle error, and medium and large included angles (60°~110°) to accurately eliminate the second-order ellipticity error. It simultaneously solves the two most critical types of shape errors of thin-walled bearings within the same set of processing steps, breaking through the technical bottleneck of traditional processes that cannot take into account second-order and third-order errors from the root.
[0025] 2. Layered parameter adaptation for targeted thin-walled part processing: This invention abandons the traditional single feed parameter mode and matches exclusive rotation speed, feed rate and grinding fluid flow rate in the roughing and fine grinding stages. The parameters are in line with the deformation law of weak rigid thin-walled rings. Combined with the feedless finishing process, the surface quality is further optimized and residual stress is released. The processed workpiece can stably reach the P2 / P4 level accuracy standard.
[0026] 3. High process flexibility and wide range of applications: This invention can flexibly adjust the core parameters such as the support angle, feed speed, and grinding wheel linear speed according to the outer diameter, wall thickness, and radial stiffness parameters of the thin-walled bearing outer ring. It is compatible with the processing of thin-walled bearings of various specifications for aero-engines and gyroscopes. Compared with single-function error elimination devices, it has stronger comprehensive adaptability and practicality.
[0027] In summary, this invention differs significantly from the traditional large-mass grinding process's strategy of "compensating for shape with quantity." This invention is specifically designed for extremely small final grinding allowances of 0.05~0.10mm on each side. Traditional processes, due to ample allowance, can forcibly remove deformed layers with large cutting volumes, possessing a strong "flattening" ability for original workpiece shape errors. However, this method is inefficient and unsuitable for thin-walled parts. Furthermore, the final grinding allowance for thin-walled bearings is extremely limited, lacking the conditions for forcibly correcting shape errors with large allowances. Any additional deformation induced by cutting forces could lead to the exhaustion of allowances and dimensional deviations. This invention, through phased active adjustment of the support angle, alters the workpiece's stress-deformation state during grinding—allowing the workpiece to be ground directly to a round profile that meets the finished product requirements while under stress and deformation. After removing the support, the workpiece elastically recovers to its ideal shape, thus achieving directional elimination of shape errors under extremely small allowance conditions, avoiding the technical dilemma of "insufficient allowance → uncorrectable deformation → finished product scrap." This strategy upgrades the traditional "passively bearing deformation and relying on the allowance for hard grinding" to "actively guiding deformation and relying on posture for fine finishing", which is an important innovative breakthrough of this invention in the field of ultra-precision grinding of thin-walled bearings. Attached Figure Description
[0028] Figure 1 A schematic diagram of the ring support point angle (α1=90°) for thin-walled bearing outer rings using traditional external cylindrical grinding method. Figure 2 A schematic diagram of the ring support point angle (α2=20°-60°) during the first stage of the grinding process for eliminating triangular edge circle error in the outer ring of a thin-walled bearing using the method described in this invention. Figure 3 A schematic diagram of the ring support point angle during the second stage of the grinding process for eliminating ellipticity error in the outer ring of a thin-walled bearing using the method described in this invention (α3=60°-110°). The markings in the diagram are: 1. Thin-walled bearing outer ring, 2. Grinding wheel, 3. First support point, 4. Second support point. Detailed Implementation
[0029] The present invention will be further described in detail below with reference to the embodiments, but this should not be construed as limiting the invention in any way.
[0030] Example 1
[0031] This invention provides a high-precision grinding method for the outer diameter of thin-walled bearings with staged variable angles. The grinding method is applicable to the final grinding process of the outer ring of weakly rigid thin-walled bearings with a single-sided grinding allowance of 0.05~0.10mm. The final grinding process is divided into two independent grinding stages, one after the other. By dynamically adjusting the workpiece support angle, different types of shape errors are eliminated in a directional manner. Specifically, the method includes the following steps: S1. Pre-processing: Complete the rough grinding and semi-finish grinding of the outer ring of the thin-walled bearing, leaving a final grinding allowance of 0.05~0.10mm on each side; clean the support components of the grinding machine, the grinding wheel and the surface of the workpiece, remove iron filings, grinding dust, oil and other impurities, and clamp the outer ring of the thin-walled bearing to be processed on the double support mechanism.
[0032] S2, First Stage: Grinding to Eliminate Triangular Edge Roundness Error Adjust the double-support mechanism to adjust the included angle α2 between the two support points corresponding to the first stage of the support points supporting the outer ring 1 of the thin-walled bearing to 20°~60°. This small included angle support mode can change the stress deformation law of the ring and form a specific correction effect on the third-order triangular edge circle error. Set the rough and finish combined grinding process parameters to match this support angle, and the grinding wheel performs continuous infeed grinding on the outer circle of the thin-walled bearing outer ring 1 at a constant linear speed. This stage focuses on efficient removal of large allowance and correction of the original third-order deformation error, and the grinding removes 50%~70% of the total allowance on one side. By utilizing the targeted correction characteristics of the small included angle support structure for the third-order deformation error of the ring, the original triangular edge circle error on the outer circle surface of the workpiece is offset, while the cutting load is reasonably controlled to avoid elastic and plastic deformation problems caused by large cutting volume.
[0033] S3, Second Stage: Grinding to Eliminate Ellipticity Error After completing the triangular edge rounding error elimination operation, the double-support mechanism is readjusted, and the included angle α3 of the second stage center of the two support points is adjusted to 60°~110°. This medium-to-large included angle support mode can optimize the radial force distribution of the bearing ring and adapt to the second-order elliptic error correction requirements. Adapt to the current support angle fine-tuning optimization of the finishing process parameters, reduce the feed speed of grinding wheel 2, increase the linear speed and heat dissipation efficiency of grinding wheel 2, and complete the fine removal of the remaining grinding allowance. After the allowance is removed, a dedicated finishing grinding stage is added: the radial feed is canceled, and only the grinding wheel 2 and the thin-walled bearing outer ring 1 are kept rotating synchronously for a fixed duration of feedless finishing grinding. Utilizing the correction characteristics of the medium-to-large included angle support structure for the second-order deformation error of the bearing ring, in conjunction with the finishing grinding process, the residual grinding stress is further released, micro-tool marks are eliminated, residual ellipticity errors are corrected, the surface roughness of the workpiece is optimized, and finally the outer diameter is machined to the product design specifications.
[0034] S4. Post-processing inspection: After grinding, slowly remove the double-support mechanism and let it stand for 3-5 minutes to allow the stress to be released naturally. Use testing instruments to check the workpiece's outer diameter ellipse, triangle and other indicators, and screen qualified workpieces.
[0035] Furthermore, for high-precision thin-walled bearings for aerospace applications, in step S2, the included angle α2 between the centers of the two support points in the first stage is preferably 30°~45°. This angle range is the optimal correction range for the third-order error, which can maximize the correction efficiency of the triangular edge circle error, while also dispersing the grinding force and reducing the risk of local stress concentration in the workpiece during grinding, thus adapting to the processing conditions of most ultra-thin-walled bearings.
[0036] Furthermore, the first stage in step S2 is the error correction rough grinding stage, which focuses on removing excess material and correcting the error of the triangular edge circle. The specific process parameters are set as follows: the linear speed of grinding wheel 2 is 25~35m / s; the rotational speed of thin-walled bearing outer ring 1 is 60~120r / min; the feed speed of grinding wheel 2 is 0.03~0.05mm / min; the whole process adopts wet grinding method, matched with special bearing grinding fluid, and the grinding fluid flow rate is 6~8L / min.
[0037] Furthermore, in step S3, the included angle α3 between the two support points in the second stage is preferably 75°~90°. This angle range is the optimal range for second-order elliptic error correction, which can be adapted to the radial stiffness characteristics of most aerospace thin-walled bearings, completely eliminating the ellipticity error remaining in the later stage of grinding, while taking into account both support stability and error correction capability.
[0038] Furthermore, the second stage in step S3 is the dimensional finishing stage, which focuses on precision shaping and surface quality control. The overall process adopts the finishing parameter logic of "high speed, low feed, and strong heat dissipation". The specific process parameters are as follows: the linear speed of grinding wheel 2 is 30~40m / s, which is 15%~20% higher than the first stage, optimizing the surface texture of the workpiece; the rotation speed of thin-walled bearing outer ring 1 is 100~200r / min; the feed speed of grinding wheel 2 is 0.01~0.03mm / min, with a feed accuracy higher than the first grinding stage, reducing cutting deformation; the wet grinding mode is continued, and the grinding fluid flow rate is 8~10L / min, which is about 30% higher than the first stage, enhancing the heat dissipation and cooling effect in high-temperature areas and preventing grinding burns.
[0039] In the dual-support mechanism, two support points form a V-shaped support for the outer ring 1 of the thin-walled bearing, and the position of at least one support point is adjustable to adjust the included angle between the centers of the two support points, thus obtaining the first-stage included angle and the second-stage included angle between the centers of the two support points. Figure 2 , 3As shown, in the first support point 3 and the second support point 4, the position of the first support point 3 is adjustable, while the position of the second support point 4 is fixed and cannot be adjusted. In other embodiments, both the first support point 3 and the second support point 4 are adjustable. For the adjustable support points, this can be achieved by a slider and a slide rail in sliding cooperation. The slide rail can be an arc-shaped track. The support point to be adjusted is fixedly connected to the slider, and the angle between the centers of the two support points is adjusted by the slider sliding along the slide rail. The slider can be adjusted manually or electrically.
[0040] Both support points in the dual-support mechanism are support pads made of wear-resistant hard alloy material. The support pads are installed on the corresponding connecting frames. For fixed support points, the corresponding connecting frames are fixed on the frame of the grinding equipment. For adjustable support points, the corresponding connecting frames are fixedly connected to the slider.
[0041] The above is only a brief introduction to the dual-support mechanism. The adjustable support point is only an example. In other embodiments, other structures and methods can be used to adjust the center angle of the two support points.
[0042] Example 2
[0043] This embodiment focuses on the outer ring of a thin-walled bearing for a certain aero-engine. The basic parameters of the thin-walled bearing outer ring are: outer diameter Φ80mm, wall thickness 5mm, and single-sided final grinding allowance 0.08mm. The specific grinding steps are as follows: 1. Pre-treatment: Complete the rough grinding and semi-fine grinding processes of the outer ring of the thin-walled bearing, leaving a single-sided grinding allowance of 0.08mm; clean the grinding wheel of the CNC cylindrical grinding machine, the double-support mechanism and impurities on the surface of the outer ring of the thin-walled bearing, and complete the clamping and benchmark calibration of the outer ring of the thin-walled bearing. 2. Triangular edge circle error elimination stage: Adjust the included angle α2 between the centers of the two support points in the first stage to 35°; process parameters: grinding wheel linear speed 30m / s, workpiece rotation speed 90r / min, grinding wheel feed speed 0.04mm / min, grinding fluid flow rate 7L / min; this stage removes 0.056mm single-sided allowance (70% of total allowance) to correct the triangular edge circle error of the outer circle of the thin-walled bearing outer ring; 3. Ellipticity error elimination stage: Adjust the included angle α3 between the two support points in the second stage to 80°; finishing process parameters: grinding wheel linear speed 35m / s, workpiece rotation speed 120r / min, grinding wheel feed speed 0.02mm / min, grinding fluid flow rate 9L / min; remove the remaining 0.024mm single-sided allowance, and after the allowance is removed, perform 10s no-feed finishing grinding to eliminate residual ellipticity error and smooth the surface tool marks; 4. Post-processing: The workpiece is left to stand for 4 minutes to release internal residual stress. After testing, the outer circle ellipse of the thin-walled bearing outer ring is ≤3μm and the triangular ellipse is ≤3μm.
[0044] Example 3
[0045] This embodiment focuses on the outer ring of a special thin-walled bearing for a certain aviation transmission system. The basic parameters of the thin-walled bearing outer ring are: outer diameter Φ60mm, wall thickness 3.5mm, and single-sided final grinding allowance 0.06mm. The specific grinding steps are as follows: 1. Pre-treatment: Complete the rough grinding and semi-fine grinding processes of the outer ring of the thin-walled bearing, leaving a single-sided grinding allowance of 0.06mm; clean the grinding wheel of the CNC cylindrical grinding machine, the double-support mechanism and impurities on the surface of the outer ring of the thin-walled bearing, and complete the clamping and benchmark calibration of the outer ring of the thin-walled bearing. 2. Triangular edge roundness error elimination stage: Adjust the included angle α2 between the centers of the two support points in the first stage to 40°; process parameters: grinding wheel linear speed 28m / s, workpiece rotation speed 110r / min, grinding wheel feed speed 0.035mm / min, grinding fluid flow rate 6.5L / min; remove 0.042mm single-sided allowance (70% of total allowance) to completely eliminate the third-order triangular edge roundness error; 3. Ellipticity error elimination stage: Adjust the included angle α3 between the two support points to 85°; finishing process parameters: grinding wheel linear speed 32m / s, workpiece rotation speed 180r / min, grinding wheel feed speed 0.015mm / min, grinding fluid flow rate 8.5L / min; remove the remaining 0.018mm allowance, and after cutting, set 8s no-feed finishing to complete the second-order ellipticity error correction; 4. Post-processing: The workpiece is inspected after standing for 3 minutes. The inspection results show that the outer circle ellipse of the thin-walled bearing outer ring is ≤2μm and the triangular ellipse is ≤2μm.
[0046] Example 4
[0047] The only difference between this embodiment and Embodiment 2 is that the first stage of grinding removes 0.04mm of the single-sided allowance (50% of the total allowance). All other steps and parameters are the same as in Embodiment 1. After machining, the outer circle ellipticity error of the thin-walled bearing outer ring is ≤2.8μm, and the triangular edge circle error is ≤2.6μm. The results show that even with the first stage removal ratio reduced to 50%, the present invention still ensures excellent shape accuracy. Furthermore, at this ratio, due to the reduced cutting force, the workpiece elastic rebound is smaller, and the final accuracy is even slightly better than that of Embodiment 2 (≤3μm). This demonstrates that the phased strategy of the present invention has good adaptability to allowance allocation, and users can flexibly adjust it according to actual working conditions.
[0048] Example 5
[0049] The only difference between this embodiment and Embodiment 2 is that in the triangular edge circle error elimination stage, the included angle α2 between the centers of the two support points in the first stage is adjusted to 25°. All other process parameters and grinding removal ratios are the same as in Embodiment 2. After processing, the outer circle ellipse of the thin-walled bearing outer ring is ≤3μm, and the triangular edge circle is ≤3.1μm. The results show that when α2 is within the range of 20° to 60°, this invention can effectively eliminate the triangular edge circle error and control the ellipticity error.
[0050] Example 6
[0051] The only difference between this embodiment and Embodiment 2 is that in the triangular edge circle error elimination stage, the included angle α2 between the centers of the two support points in the first stage is adjusted to 60°. All other process parameters and grinding removal ratios are the same as in Embodiment 2. After processing, the outer circle ellipse of the thin-walled bearing outer ring is ≤2.9μm, and the triangular edge circle is ≤3.2μm. The results show that when α2 is within the range of 20° to 60°, this invention can effectively eliminate the triangular edge circle error and control the ellipticity error.
[0052] Example 7
[0053] The only difference between this embodiment and Embodiment 2 is that, in the ellipticity error elimination stage, the included angle α3 between the two support points in the second stage is adjusted to 75° (originally 80°). All other process parameters and grinding removal ratios are the same as in Embodiment 2. After processing, the outer circle ellipse of the thin-walled bearing outer ring is ≤2.6μm, and the triangular edge circle is ≤2.8μm. This indicates that within the range of 60°~110°, a 75° included angle has a good correction effect on ellipticity error and does not conflict with third-order error correction, verifying the wide applicability of this angle range.
[0054] Example 8
[0055] The only difference between this embodiment and Embodiment 2 is that, in the ellipticity error elimination stage, the included angle α3 between the centers of the two support points in the second stage is adjusted to 110° (originally 80°). All other process parameters and grinding removal ratios are the same as in Embodiment 2. After processing, the outer circle ellipticity of the thin-walled bearing outer ring is ≤3.1μm, and the triangular edge circle is ≤2.8μm. This indicates that within the range of 60°~110°, both the triangular edge circle error and the ellipticity error have a good correction effect, verifying the wide applicability of this angle range.
[0056] Comparative Example This comparative example uses a traditional fixed-angle grinding process. Figure 1The existing 90° fixed support angle infeed one-step forming grinding process is used to machine a thin-walled bearing outer ring with the same specifications and 0.08mm single-sided allowance as in Example 2. The process parameters (grinding wheel linear speed, workpiece rotation speed, feed rate, and grinding fluid flow rate) are taken as the midpoint of the parameters in the two stages of Example 2 to ensure comparability. After machining, the following tests were performed: the outer circle ellipse of the workpiece is ≤5μm, and the triangular edge circle is ≤5μm.
[0057] By comparing with comparative examples, the outer cylindrical shape error of thin-walled bearings is mainly composed of second-order ellipticity error and third-order triangular edge circle error. The formation mechanism and force response of these two errors differ significantly during the grinding process. Small support angles (20°~60°) allow the support reaction force to generate a deformation field dominated by third-order harmonics on the circumference. This deformation field is exactly opposite in phase to the original triangular edge circle error of the workpiece, thus achieving "adaptive cancellation" of the third-order error during grinding. Medium to large support angles (60°~110°) make the radial force distribution closer to the characteristics of second-order harmonics, effectively suppressing the elliptic elastic recovery caused by the grinding force, thereby directionally correcting the ellipticity error. Traditional single-angle support (such as a fixed 90°) can only provide good compensation for one order of error, with limited ability to correct another order of error, and may even exacerbate the shape error due to force-deformation mismatch. This invention dynamically changes the support angle in stages, setting specific support configurations for third-order and second-order errors respectively. This ensures that each grinding stage operates in an optimal force-deformation coupling state, achieving independent and efficient elimination of both types of errors. Combined with independent process parameters for each stage (large feed for rough grinding, small feed for finish grinding + smoothing), it not only guarantees efficient removal of excess material but also releases residual stress through smoothing. The principle of this technology has been verified through extensive process experiments, demonstrating the scientific validity and advancement of this invention's staged angle-changing strategy.
[0058] The above embodiments are only used to illustrate the technical solutions of the present invention and are not intended to limit it. Those skilled in the art should understand that modifications or equivalent substitutions can be made to the specific implementation of the present invention with reference to the above embodiments. Any modifications or equivalent substitutions that do not depart from the spirit and scope of the present invention are within the protection scope of the pending claims.
Claims
1. A method for staged variable-angle outer cylindrical grinding of a high-precision thin-walled bearing outer ring, characterized in that, The grinding method described herein is applicable to the final grinding process of the outer ring of a weakly rigid, thin-walled bearing with a single-sided grinding allowance of 0.05~0.10mm. The final grinding process is divided into two independent grinding stages that are connected sequentially. By dynamically adjusting the workpiece support angle, different types of shape errors are eliminated in a directional manner. Specifically, the method includes the following steps: S1, Pre-processing: The rough grinding and semi-finish grinding of the outer ring of the thin-walled bearing are completed in sequence, and a final grinding allowance of 0.05mm~0.10mm is reserved on the outer circle of one side; the outer ring of the thin-walled bearing is clamped on the electromagnetic centerless chuck of the grinding machine tool, and the outer circle of the thin-walled bearing is supported on the two support points of the double support mechanism. S2, execute the first stage, perform triangular edge rounding error elimination grinding: adjust the double-support mechanism to adjust the included angle α2 of the two support points supporting the outer ring of the thin-walled bearing to 20°~60° in the first stage; the grinding wheel performs continuous infeed grinding on the outer circle of the thin-walled bearing outer ring at a constant linear speed, grinding away 50%~70% of the final grinding allowance of the single-sided outer circle; S3, the second stage is executed, which involves grinding to eliminate ellipticity errors: After completing the triangular edge circle error elimination operation, firstly, the double-support mechanism is readjusted, and the included angle α3 between the two support points in the second stage is adjusted to 60°~110°; then, based on the first stage, the feed speed is reduced and the grinding wheel linear speed is increased to complete the fine removal of the remaining single-sided outer circle final grinding allowance; then, the finishing grinding stage is entered, the radial feed is canceled, and the thin-walled bearing outer ring is kept to rotate synchronously with the grinding wheel, and finishing grinding is performed for a fixed duration, finally machining the outer circle dimension to the product design specifications; S4. Post-processing inspection: After grinding, slowly remove the support constraints of the outer ring of the thin-walled bearing, let it stand for 3-5 minutes to allow the stress to be released naturally, and use testing instruments to check the elliptic and triangular indicators of the outer diameter of the thin-walled bearing outer ring to screen qualified workpieces.
2. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 1, characterized in that, In step S2, the included angle α2 between the centers of the two support points in the first stage is 30°~45°.
3. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 1, characterized in that, In step S2, the grinding process parameters are set as follows: grinding wheel linear speed 25~35m / s, grinding wheel feed speed 0.03~0.05mm / min, thin-walled bearing outer ring speed 60~120r / min, wet grinding is used throughout the process, and grinding fluid flow rate is 6~8L / min.
4. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 1, characterized in that, In step S3, the included angle α3 between the centers of the two support points in the second stage is 75°~90°.
5. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 1, characterized in that, In step S2, the grinding process parameters are set as follows: grinding wheel linear speed 30~40m / s, which is 15%~20% higher than that of the first stage; grinding wheel feed speed 0.01~0.03mm / min; thin-walled bearing outer ring speed 100~200r / min; grinding fluid flow rate 8~10L / min.
6. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 1, characterized in that, The position of at least one support point in the dual-support mechanism is adjustable, which is used to adjust the size of the included angle between the centers of the two support points.
7. The method for staged variable-angle outer cylindrical grinding of high-precision thin-walled bearing outer rings according to claim 6, characterized in that, Both support points in the dual-support mechanism are support pads made of wear-resistant hard alloy material, and the support pads are installed on the corresponding connecting frames.
Citation Information
Patent Citations
Bearing outer ring plunge-cut grinding device eliminating eclipse
CN202752973U
Supporting structure for grinding outer diameter of thin-wall bearing
CN222155173U
Grinding tool suitable for super-huge thin-wall bearing ring
CN119635431A
Process for cylindrical grinding in the manufacture of hard metal tools and cylindrical grinding machine for grinding cylindrical starting bodies in the manufacture of hard metal tools
DE10308292A1