A ceramic brick and its preparation method

By preparing ceramic bricks with inclined grooves on the surface and coated with silicon carbide and carbon black, the problem of moss growth in areas with poor light conditions was solved, achieving the effect of inhibiting moss growth and maintaining water permeability.

CN123062284APending Publication Date: 2026-11-10KUNMING UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611052663.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-15
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Existing permeable ceramic bricks are prone to moss growth on their surface in areas with poor lighting conditions, which affects their permeability and aesthetics.

Method used

Ceramic bricks are prepared using waste residue raw materials, binders, foaming agents, powders and carbon black blocks, etc. The surface is provided with inclined grooves and coated with silicon carbide and carbon black coatings. Silicon carbide is used as a heat-conducting substrate and carbon black is used as a heat-absorbing coating to increase the surface temperature and inhibit the growth of moss.

Benefits of technology

It effectively inhibits moss growth, maintains water permeability, improves the surface performance of bricks, saves costs, and is easy to operate.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a ceramic brick and its preparation method in the field of building ceramic materials technology. The brick is made from the following raw materials in parts by weight: 60-75 parts waste residue, 1-2 parts binder, 5-10 parts foaming agent, 25-35 parts powder, 1-3 parts carbon black blocks, and 2-5 parts silicon carbide. This invention utilizes readily available coal gangue, desulfurized gypsum, and powder as the main raw materials, saving costs. The preparation method is simple and easy to operate. The ceramic brick has inclined grooves on its surface for convenient and timely drainage, reducing the accumulation of pollutants on the surface and reducing slippage when stepped on. Simultaneously, the use of silicon carbide as a thermally conductive substrate and carbon black as a heat-absorbing coating accelerates heat absorption and conduction, thereby increasing the surface temperature and inhibiting moss growth.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of building ceramic materials technology, specifically to a ceramic brick and its preparation method. Background Technology

[0002] Ceramic bricks are plate-shaped ceramic products made from inorganic non-metallic raw materials such as clay through molding and sintering. They are mainly used for the decoration and protection of building walls and floors. Their molding processes include dry pressing and extrusion. After high-temperature firing, they are classified according to their water absorption rate into earthenware bricks (>10%), porcelain bricks (<0.5%), and intermediate categories, corresponding to different application scenarios. With the advancement of urbanization, the area of ​​hard paving such as urban roads, squares, and parking lots is gradually expanding. Large amounts of impermeable materials such as concrete cover the surface, severely blocking rainwater infiltration and easily causing road surface water accumulation, which can lead to urban flooding in severe cases. Therefore, permeable ceramic bricks are currently used for road or ground paving in some situations. However, when permeable ceramic bricks are laid in areas with poor lighting conditions, moss easily grows on their surface, which not only harms the permeability but also affects the aesthetics. Therefore, there is an urgent need to design a permeable ceramic brick that can inhibit moss growth on the surface. Based on this, this invention designs a ceramic brick and its preparation method to solve the above problems. Summary of the Invention

[0003] The purpose of this invention is to provide a ceramic brick and its preparation method to solve the problems mentioned in the background art.

[0004] To achieve the above objectives, the present invention provides the following technical solution: a ceramic brick, made from the following raw materials in parts by weight: the raw materials include 60-75 parts of waste residue, 1-2 parts of binder, 5-10 parts of foaming agent, 25-35 parts of powder, 1-3 parts of carbon black blocks and 2-5 parts of silicon carbide; The waste residue raw material consists of 10-15 mesh coal gangue and 20-30 mesh coal gangue, with each mesh size accounting for a ratio of 1:3. The adhesive has the following chemical composition by mass percentage: 0.5-0.9% polyvinyl alcohol, 0.8-0.95% hydroxypropyl methylcellulose, and 0.7-1% starch ether. The foaming agent is composed of 100-150 mesh desulfurized gypsum and 200-300 mesh calcium carbonate, with the ratio of each mesh size being 1.5:1. The powder comprises 55-75 parts kaolin, 15-25 parts quartz, and 10-18 parts feldspar.

[0005] The preparation method of ceramic tiles includes the following steps: S1: Clean the waste residue raw material, dry it and set it aside for later use; S2: The waste residue raw material in S1 is mixed with foaming agent and powder according to the pre-designed ratio to make a batch material. Then, 0.8-1% of the total mass of the batch material is added as binder, water is added and mixed evenly, and then the mixture is put into a mold and pressed to form a green body. S3: The ceramic blank obtained in S2 is grooved so that its surface is evenly spaced with embedded oblique grooves along the length direction. S4: Silicon carbide is used as a raw material to coat the surface of the blank on the inner wall of the inclined groove, and then a second coating is performed using a green blank made of carbon black blocks as a connecting slurry. S5: The entire body of the ceramic tile is first dried in air or a drying oven, then sintered and kept warm in a muffle furnace or resistance furnace, and cooled with the furnace to obtain ceramic tiles.

[0006] Preferably, the cross-section of the inclined groove in S3 is V-shaped, and the depth is between 0.1-0.5cm.

[0007] Preferably, in step S4, silicon carbide is first processed into 100-200 mesh particles using a ball mill, and then made into a high solids content slurry, which is then applied to the surface of the inclined trough by spraying.

[0008] Preferably, the green body bonding slurry in S4 further includes a ceramic matrix, an organic binder, and a solvent, and the carbon black block is made of nano-sized powder.

[0009] Preferably, the method for preparing the carbon black block into nano-sized powder is as follows: carbon black is mixed with organic liquid and dispersant to form a slurry, and the agglomeration is broken up by high-speed collision and shearing of the grinding media using a vertical sand mill, colloid mill or high-energy ball mill, so that the particle size can be reduced to below 100nm.

[0010] Preferably, the sintering temperature in the muffle furnace or resistance furnace is 1500-1800℃, the heating rate is 5℃ / min, and the holding time is 1-1.5h.

[0011] Preferably, the overall moisture content of the mixture after adding water in step S2 and mixing evenly is controlled at 4.5%-6.5%.

[0012] Preferably, the grinding media are zirconium oxide beads, silicon nitride beads, or zirconium silicate beads.

[0013] Preferably, the solvent includes ethanol and polyethylene glycol 200.

[0014] Compared with the prior art, the beneficial effects of the present invention are: 1. This invention utilizes readily available coal gangue, desulfurized gypsum, and powder as the main raw materials, saving costs, and the preparation method is simple and easy to operate; 2: The ceramic tiles have sloping grooves on their surface to facilitate timely drainage, reduce the accumulation of pollutants on the surface, and reduce slipping when stepped on. At the same time, the use of silicon carbide as a heat-conducting substrate and carbon black as a heat-absorbing coating can accelerate heat absorption and conduction, thereby increasing the surface temperature and inhibiting the growth of moss. Detailed Implementation

[0015] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0016] In the description of this invention, it should be understood that the terms "upper", "lower", "front", "rear", "left", "right", "top", "bottom", "inner", "outer", etc., indicating the orientation or positional relationship are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of this invention.

[0017] The present invention provides a technical solution: a ceramic brick, which is made from the following raw materials in parts by weight: the raw materials include 60-75 parts of waste residue, 1-2 parts of binder, 5-10 parts of foaming agent, 25-35 parts of powder, 1-3 parts of carbon black blocks and 2-5 parts of silicon carbide. The waste residue raw material consists of 10-15 mesh coal gangue and 20-30 mesh coal gangue, with each mesh size accounting for a ratio of 1:3. The chemical composition of the binder is 0.5-0.9% polyvinyl alcohol, 0.8-0.95% hydroxypropyl methylcellulose and 0.7-1% starch ether by mass percentage. The amount of binder added during use is extremely low (usually <1%), which plays a role in the strength of the green brick and is not present in the finished brick.

[0018] The foaming agent is composed of 100-150 mesh desulfurized gypsum and 200-300 mesh calcium carbonate, with the ratio of each mesh size being 1.5:1. The powder consists of 55-75 parts kaolin, 15-25 parts quartz, and 10-18 parts feldspar. Kaolin provides plasticity and binding force, ensuring the integrity of the powder granulation and pressing. Quartz serves as a skeleton material, inhibiting drying and firing shrinkage, and improving the hardness and dimensional stability of the finished product. Feldspar melts at high temperatures to form a liquid phase, promoting densification sintering and reducing the firing temperature.

[0019] The preparation method of ceramic tiles includes the following steps: S1: Clean the waste residue raw material, dry it and set it aside for later use; S2: The waste residue raw material in S1 is mixed with foaming agent and powder according to the pre-designed ratio to make a batch material. Then, 0.8-1% of the total mass of the batch material is added as binder, water is added and mixed evenly, and then the mixture is put into a mold and pressed to form a green body. S3: The ceramic blank obtained in S2 is grooved so that the surface of the blank is evenly spaced along the length direction with embedded oblique grooves. Specifically, the oblique grooves are formed by pressing with a mold or manually removing them. Finally, the blank is fired in a kiln and the oblique grooves become the inherent structure of the brick. S4: Silicon carbide is used as a raw material to coat the surface of the blank on the inner wall of the inclined groove, and then a second coating is performed using a green blank made of carbon black blocks as a connecting slurry. S5: The entire body of the ceramic tile is first dried in air or a drying oven, then sintered and kept warm in a muffle furnace or resistance furnace, and cooled with the furnace to obtain ceramic tiles.

[0020] In S3, the cross-section of the inclined groove is V-shaped, and the depth is between 0.1-0.5cm to avoid being too deep and affecting the overall strength. In S4, silicon carbide is first processed into 100-200 mesh particles by ball milling, and then made into a high solid content slurry. It is then applied to the surface of the inclined groove by spraying. Silicon carbide ceramic itself has extremely high hardness and wear resistance, which can significantly improve the surface performance of the brick. It is a suspension system with low viscosity and high stability. The core lies in powder surface modification, multi-level gradation and efficient dispersion / bonding synergy, so that the inclined groove surface forms a thermally conductive substrate, thereby increasing the surface temperature of the brick. In addition, the green body connecting slurry in S4 also includes ceramic matrix, organic binder and solvent. The carbon black block uses nano-sized powder. After the coating is cured at low temperature, it achieves metallurgical / reaction bonding with the whole body at high temperature, forming a heat-absorbing coating, which can generate more heat even in places with weak light intensity.

[0021] Furthermore, the method for preparing carbon black blocks into nano-sized powder is as follows: Carbon black is mixed with organic liquid and dispersant to form a slurry. This slurry is then broken up using a vertical sand mill, colloid mill, or high-energy ball mill through high-speed collision and shearing of the grinding media, reducing the particle size to below 100 nm. The sintering temperature in a muffle furnace or resistance furnace is 1500-1800℃, the heating rate is 5℃ / min, and the holding time is 1-1.5h. After uniform mixing with water in S2, the overall moisture content is controlled at 4.5%-6.5%, as excessive moisture content leads to delamination and sticking. Too low a temperature affects particle flow and green strength; the grinding media uses zirconia beads, silicon nitride beads, or zirconium silicate beads, which have superior hardness and toughness, are resistant to high temperatures, and have no aging instability issues. The solvents include ethanol and polyethylene glycol 200. Ethanol, as the main solvent, completely dissolves the binder to form a continuous binder phase. Combined with polyethylene glycol 200, it prevents carbon black agglomeration and ensures that the carbon black is uniformly suspended in the slurry. During the initial stages of curing and sintering, ethanol and polyethylene glycol 200 completely evaporate, leaving no inorganic residues and avoiding affecting the subsequent reaction and sintering quality.

[0022] Example 1

[0023] In this embodiment, the raw materials include 67 parts of waste residue, 6 parts of foaming agent, 11 parts of powder, 1 part of carbon black block, and 2 parts of silicon carbide. The cleaned and dried waste residue is mixed with the foaming agent and powder to form a batch. Then, 0.85% of the total mass of the batch is added as a binder. After mixing thoroughly with water, the mixture is placed in a mold and pressed to form a green body. The green body is then grooved, creating evenly spaced, inclined grooves along its length. Next, 2 parts of silicon carbide are applied to the inner wall of the grooves onto the surface of the green body. A second coating is then applied using a green body connecting slurry made from 1 part of carbon black block. The entire green body is first dried in a drying oven, then placed in a resistance furnace and heated to 1600℃ at a uniform rate of 5℃ / min and held for 1 hour. It is then cooled in the furnace. The resulting ceramic tile has a permeability coefficient of 4.33 × 10⁻⁶. cm / s, flexural strength is 3.45MPa.

[0024] Example 2

[0025] In this embodiment, the raw materials include 70 parts of waste residue, 8 parts of foaming agent, 30 parts of powder, 2 parts of carbon black blocks, and 2 parts of silicon carbide. The cleaned and dried waste residue is mixed with the foaming agent and powder to form a batch. Then, 0.9% of the total mass of the batch is added as a binder. After mixing thoroughly with water, the mixture is placed in a mold and pressed to form a green body. The green body is then grooved, creating evenly spaced, inclined grooves along its length. Next, 2 parts of silicon carbide are applied to the inner wall of the grooves onto the surface of the green body. A second coating is then applied using a green body connecting slurry made from 2 parts of carbon black blocks. The entire green body is first dried in a drying oven, then placed in a resistance furnace and heated to 1800℃ at a uniform rate of 5℃ / min and held for 1 hour. It is then cooled in the furnace. The resulting ceramic tile has a permeability coefficient of 5.45 × 10⁻⁶. cm / s, flexural strength is 3.05MPa.

[0026] Example 3

[0027] In this embodiment, the raw materials include 75 parts of waste residue, 10 parts of foaming agent, 35 parts of powder, 1 part of carbon black block, and 4 parts of silicon carbide. The cleaned and dried waste residue is mixed with the foaming agent and powder to form a batch. Then, 1% of the total mass of binder is added to the batch, water is added, and the mixture is poured into a mold and pressed to form a green body. The green body is then grooved, creating evenly spaced, inclined grooves along its length. Next, 4 parts of silicon carbide are applied to the inner wall of the grooves onto the surface of the green body. A second coating is then applied using a green body connecting slurry made from 1 part of carbon black block. The entire green body is first dried in a drying oven, then placed in a resistance furnace and heated to 1800℃ at a uniform rate of 5℃ / min and held for 1 hour. It is then cooled in the furnace. The resulting ceramic tile has a permeability coefficient of 4.05 × 10⁻⁵. The permeability is cm / s and the flexural strength is 5.15MPa. Therefore, the higher the permeability, i.e. the larger the permeability coefficient, the lower the flexural strength.

[0028] In the description of this specification, references to terms such as "an embodiment," "example," "specific example," etc., indicate that a specific feature, structure, material, or characteristic described in connection with that embodiment or example is included in at least one embodiment or example of the invention. In this specification, illustrative expressions of the above terms do not necessarily refer to the same embodiment or example. Furthermore, the specific features, structures, materials, or characteristics described may be combined in any suitable manner in one or more embodiments or examples.

[0029] The preferred embodiments of the present invention disclosed above are merely illustrative of the invention. These preferred embodiments do not exhaustively describe all details, nor do they limit the invention to the specific implementations described. Clearly, many modifications and variations can be made based on the content of this specification. This specification selects and specifically describes these embodiments to better explain the principles and practical applications of the invention, thereby enabling those skilled in the art to better understand and utilize the invention. The invention is limited only by the claims and their full scope and equivalents.

Claims

1. A ceramic tile, characterized in that, It is made from the following raw materials in parts by weight: 60-75 parts waste residue, 1-2 parts binder, 5-10 parts foaming agent, 25-35 parts powder, 1-3 parts carbon black blocks and 2-5 parts silicon carbide; The waste residue raw material consists of 10-15 mesh coal gangue and 20-30 mesh coal gangue, with each mesh size accounting for a ratio of 1:

3. The adhesive has the following chemical composition by mass percentage: 0.5-0.9% polyvinyl alcohol, 0.8-0.95% hydroxypropyl methylcellulose, and 0.7-1% starch ether. The foaming agent is composed of 100-150 mesh desulfurized gypsum and 200-300 mesh calcium carbonate, with the ratio of each mesh size being 1.5:

1. The powder comprises 55-75 parts kaolin, 15-25 parts quartz, and 10-18 parts feldspar.

2. The method for preparing ceramic bricks according to claim 1, characterized in that, Includes the following steps: S1: Clean the waste residue raw material, dry it and set it aside for later use; S2: The waste residue raw material in S1 is mixed with foaming agent and powder according to the pre-designed ratio to make a batch material. Then, 0.8-1% of the total mass of the batch material is added as binder, water is added and mixed evenly, and then the mixture is put into a mold and pressed to form a green body. S3: The ceramic blank obtained in S2 is grooved so that its surface is evenly spaced with embedded oblique grooves along the length direction. S4: Silicon carbide is used as a raw material to coat the surface of the blank on the inner wall of the inclined groove, and then a second coating is performed using a green blank made of carbon black blocks as a connecting slurry. S5: The entire body of the ceramic tile is first dried in air or a drying oven, then sintered and kept warm in a muffle furnace or resistance furnace, and cooled with the furnace to obtain ceramic tiles.

3. The method for preparing ceramic bricks according to claim 2, characterized in that: The inclined groove in S3 has a V-shaped cross-section and a depth between 0.1 and 0.5 cm.

4. The method for preparing ceramic bricks according to claim 2, characterized in that: In step S4, silicon carbide is first processed into 100-200 mesh particles using a ball mill, and then made into a high solids content slurry, which is then applied to the surface of the inclined trough by spraying.

5. The method for preparing ceramic bricks according to claim 2, characterized in that: The green body bonding slurry in S4 also includes a ceramic matrix, an organic binder, and a solvent, and the carbon black block is made of nano-sized powder.

6. The method for preparing ceramic tiles according to claim 5, characterized in that: The method for producing nanoscale powder from carbon black blocks is as follows: carbon black is mixed with organic liquid and dispersant to form a slurry, and the agglomeration is broken up by high-speed collision and shearing of the grinding media using a vertical sand mill, colloid mill or high-energy ball mill, so that the particle size can be reduced to below 100nm.

7. The method for preparing ceramic bricks according to claim 2, characterized in that: The sintering temperature in the muffle furnace or resistance furnace is 1500-1800℃, the heating rate is 5℃ / min, and the holding time is 1-1.5h.

8. The method for preparing ceramic bricks according to claim 2, characterized in that: After adding water and mixing evenly, the overall moisture content of S2 is controlled at 4.5%-6.5%.

9. The method for preparing ceramic bricks according to claim 6, characterized in that: The grinding media are zirconium oxide beads, silicon nitride beads, or zirconium silicate beads.