A graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity
By designing a composite structure of outer circumferential heat exchange grooves and inner axial fins on the graphite furnace cylinder of the hydrogen chloride synthesis furnace combustion chamber, combined with a self-healing material layer, the problems of uneven strength and low heat exchange efficiency are solved, achieving high-efficiency heat exchange and self-repair, thus improving the safety and service life of the equipment.
Patent Information
- Application Number
- CN202610886513.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-18
- Publication Date
- 2026-11-10
AI Technical Summary
The existing graphite furnace cylinder of the combustion chamber of the hydrogen chloride synthesis furnace has uneven strength in the design of the jacket flow hole, which easily leads to stress concentration, resulting in safety hazards such as cracks and explosions, while the heat exchange efficiency is limited.
The structure adopts a composite structure of circumferential heat exchange grooves on the outer side of the cylinder and axial heat exchange fins on the inner side, combined with multiple layers of self-healing material, including a stress response layer, a temperature activation layer and a sealing layer. It utilizes the shear thinning characteristics of the stress response layer and the temperature-grade activated glass melt for automatic repair, thereby enhancing structural strength and heat exchange efficiency.
It significantly improves the heat exchange efficiency and structural strength of the combustion chamber, enables autonomous repair of microcracks, extends equipment life and improves safety, and adapts to high-temperature operating environments.
Smart Images

Figure CN123065239A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of hydrogen chloride synthesis furnace technology, and in particular to a graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity. Background Technology
[0002] The hydrogen chloride synthesis furnace is a key piece of equipment used to produce hydrogen chloride gas through the combustion reaction of chlorine and hydrogen. Its combustion chamber is usually made of graphite material because graphite has good corrosion resistance and thermal conductivity. In order to remove the large amount of heat generated by combustion in a timely manner, a jacket is usually installed on the outside of the furnace cylinder, and a cooling medium (deionized water) is circulated in the jacket for heat exchange.
[0003] In related technologies, it is common practice to create openings along the wall thickness of the outer side of the furnace cylinder to allow the liquid phase within the jacket to flow and achieve heat exchange. However, this method of creating openings for liquid phase flow can easily lead to uneven strength in the circumferential direction. Under thermal stress and pressure, stress concentration can easily occur at the edges of the openings, potentially causing cracks or even bursts, posing certain safety hazards. Therefore, this method needs to be improved. Summary of the Invention
[0004] To address the aforementioned issues, this application provides a graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity.
[0005] The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity provided in this application adopts the following technical solution: A graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity includes a cylinder body. A heat exchange groove is provided on the outer side of the cylinder body, and the heat exchange groove is arranged circumferentially along the cylinder body. Heat exchange fins are provided on the inner side of the cylinder body, and the heat exchange fins are arranged axially along the cylinder body.
[0006] By adopting the above technical solution, heat exchange grooves (which can be multiple annular grooves or a single spiral groove) are opened circumferentially on the outer side of the cylinder, avoiding the local stress concentration caused by the traditional through-hole structure, and making the strength distribution of the cylinder wall thickness more uniform. At the same time, the heat exchange grooves significantly increase the heat exchange area on the outer side, and the cooling medium can fully remove heat when flowing in the grooves. The heat exchange fins arranged axially on the inner side further increase the heat exchange area on the inner side, and the fins themselves have good thermal conductivity, which can quickly conduct heat from the inner wall to the entire cylinder. The synergistic effect of increasing the heat exchange area simultaneously inside and outside significantly improves the overall heat exchange efficiency of the combustion chamber wall, increasing the thermal conductivity by more than 30% compared to the traditional through-hole structure. More importantly, the circumferential heat exchange grooves slightly reduce the radial stiffness of the cylinder, while the axial heat exchange fins act as reinforcing ribs, improving the radial bending strength of the cylinder. Together, they form a "woven mesh" skeleton structure, ensuring both high heat exchange performance and structural strength, fundamentally solving the technical contradiction of balancing heat exchange and strength in traditional graphite furnace tubes.
[0007] Furthermore, the heat exchange groove is an annular groove, and several of the annular grooves are evenly distributed along the axial direction of the cylinder.
[0008] By adopting the above technical solution, the annular groove structure is easy to machine and can be completed using a conventional lathe, resulting in low manufacturing costs. Multiple annular grooves are evenly distributed along the axial direction, allowing the cooling medium to flow independently within each groove, ensuring uniform flow distribution and stable heat exchange. Simultaneously, the evenly distributed annular grooves make the stress distribution along the cylinder wall thickness direction more uniform, avoiding localized stress concentration.
[0009] Furthermore, the heat exchange groove is a spiral groove.
[0010] By adopting the above technical solution, the spiral groove can guide the cooling medium to flow in a spiral pattern, increasing the degree of fluid turbulence and thus improving the convective heat transfer coefficient. Compared with annular grooves, spiral grooves have no discontinuities, resulting in lower fluid resistance. Furthermore, a single spiral groove can cover the entire length of the cylinder, simplifying manufacturing. The spiral groove can also create a continuous reinforcing rib effect on the cylinder surface, contributing more significantly to the overall strength of the cylinder.
[0011] Furthermore, the cylindrical body is covered with reinforcing members at the heat exchange groove.
[0012] By adopting the above technical solution, the opening of the heat exchange grooves weakens the wall thickness of the cylinder to a certain extent, and the covering reinforcement can compensate for the strength loss, which is especially suitable for high-pressure or large-diameter furnace cylinders. The reinforcement can be made of carbon cloth and / or carbon fiber tow. These materials have high specific strength, high modulus and excellent heat resistance, and their coefficient of thermal expansion is similar to that of graphite matrix. At the same time, the high thermal conductivity of carbon materials themselves will not significantly reduce the heat exchange efficiency.
[0013] Furthermore, the reinforcing member is carbon cloth and / or carbon fiber bundles.
[0014] By adopting the above technical solutions, carbon fiber reinforced composite materials possess extremely high tensile strength and modulus, and are resistant to high temperatures and corrosion. Wrapping or covering the outside of the heat exchange tank with it can significantly improve the circumferential tensile strength of the cylinder. Simultaneously, the porosity of carbon fiber allows the cooling medium to permeate without hindering heat exchange.
[0015] Furthermore, the inner side of the reinforcing member is also provided with a multi-layered composite self-healing material layer, which includes a stress response layer, a temperature activation layer, and a sealing layer from the inside out. The stress response layer fills the bottom of the heat exchange tank and is composed of a non-Newtonian fluid material with shear-thinning properties. It is solid or highly viscous in a stress-free state. When a crack occurs in the furnace cylinder body at the corresponding position at the bottom of the heat exchange tank and a local stress concentration is formed, the viscosity of this layer decreases and it penetrates along the crack. The temperature activation layer covers the stress response layer and contains at least two glassy powders with different melting points. It melts stepwise within the normal operating temperature range of the synthesis furnace, providing a continuous liquid repair medium replenishment for the stress response layer. The sealing layer is a porous ceramic cover plate, which is fixedly covered on the temperature activation layer.
[0016] By employing the above technical solution, when microcracks develop in the graphite furnace cylinder due to thermal stress during long-term operation, the stress field at the crack tip triggers the shear-thinning properties of the stress-responsive layer material, causing its viscosity to drop sharply and penetrate along the crack. This process requires no external energy input and is entirely activated automatically by the local stress generated by crack propagation. Subsequently, the low-melting-point glass powder in the temperature-activated layer melts at the furnace temperature, providing a continuous liquid repair medium for the penetrated material, filling the crack and solidifying it. The sealing layer prevents excessive loss of the repair medium when not activated, while allowing molten glass to seep out when needed. This self-healing system can automatically repair early microcracks without shutting down the furnace, preventing them from expanding into through-cracks, significantly improving the safety and service life of the furnace cylinder.
[0017] Furthermore, the stress-responsive layer material is composed of the following components in parts by mass: 40-60 parts of silicate glass powder, 5-15 parts of nano-silicon carbide whiskers, 10-20 parts of boric anhydride, and 1-5 parts of thixotropic modifier; the thixotropic modifier is fumed silica or attapulgite that has undergone surface hydrophobic treatment, so that the yield stress of the material is ≥500Pa when there is no shear, and the viscosity is reduced to less than 1 / 100 of the original value when the shear stress is ≥1000Pa.
[0018] By employing the above technical solution, silicate glass powder provides a repair matrix with moderate fluidity at high temperatures. Nano-silicon carbide whiskers enhance the mechanical properties of the repair layer and adjust its coefficient of thermal expansion to match the graphite matrix. Boric anhydride, exhibiting excellent fluidity at high temperatures (melting point approximately 577℃), can act as a flux to lower the softening temperature of the glass powder and improve wettability. A thixotropic modifier imparts shear-thinning properties to the material, characteristic of a non-Newtonian fluid: a yield stress ≥500 Pa at static conditions, ensuring the material does not flow under normal operating conditions; when shear stress ≥1000 Pa is generated at the crack tip, the viscosity decreases by more than two orders of magnitude, ensuring rapid filling of cracks once they form. The synergistic effect of this formulation gives the material both sufficient high-temperature stability and sensitive stress response.
[0019] Furthermore, the stress-responsive layer material also contains a microencapsulated reducing agent, which is boron carbide or silicon powder, encapsulated in graphene-coated silica microcapsules.
[0020] By employing the above technical solution, when crack propagation leads to microcapsule rupture, the reducing agent (boron carbide or silicon powder) is released. At high temperatures, boron carbide reacts with oxygen: B4C + O2 → B2O3 + CO2. The resulting B2O3 is also an excellent glassy filler, which can further fill the microcracks and consume surrounding oxygen. Silicon powder reacts to form SiO2. This localized protective atmosphere prevents graphite from being oxidized at high temperatures, extending the furnace barrel life. The graphene coating enhances the thermal conductivity and mechanical strength of the microcapsules, ensuring that they rupture in a timely manner under stress rather than leaking prematurely.
[0021] Furthermore, the temperature activation layer is composed of two types of glass powder with different softening temperature ranges: the first component has a softening temperature of 650℃~750℃, and the second component has a softening temperature of 850℃~950℃; when the furnace operating temperature is below 750℃, only the first component melts to provide the repair medium; when the temperature exceeds 850℃, the second component also melts, increasing the fluidity of the repair medium.
[0022] By adopting the above technical solution, a temperature-stage release mechanism is achieved. The normal wall temperature of the combustion chamber in a hydrogen chloride synthesis furnace is typically between 650 and 750°C. Within this temperature range, only the first component melts, providing basic repair capability and preventing excessive glass melt from flowing into the crack and causing waste. When abnormally high temperatures occur (such as localized overheating or abnormal combustion) exceeding 850°C, the second component also begins to melt. At this point, the crack may be more severe, requiring more repair medium and higher fluidity to address the issue. This staged design ensures both economic efficiency in daily operation and sufficient repair capability in emergency situations.
[0023] Furthermore, the temperature activation layer is composed of CaO-Al2O3-SiO2 glass powder and MgO-B2O3-SiO2 glass powder in a mass ratio of 1:1 to 3:1; wherein the softening temperature of the CaO-Al2O3-SiO2 glass powder is 650℃ to 750℃, and the softening temperature of the MgO-B2O3-SiO2 glass powder is 850℃ to 950℃.
[0024] By employing the above technical solutions, CaO-Al2O3-SiO2 based glasses (such as anorthite glass) exhibit good thermal stability and a coefficient of thermal expansion similar to graphite (approximately 4–5 × 10⁻⁶ / K). MgO-B₂O₃-SiO₂ based glasses (such as cordierite glass) have higher softening points and lower viscosity, exhibiting good fluidity at high temperatures. When the two are mixed in a specific ratio, continuously adjustable viscosity and filling properties can be provided across different temperature ranges.
[0025] Furthermore, the bottom of the heat exchange tank is provided with stress concentration micro-protrusions arranged circumferentially at intervals, the height of the micro-protrusions being 0.1 to 0.5 mm and the spacing being 1 to 5 mm.
[0026] By employing the above technical solution, the stress-concentration micro-protrusions can preferentially terminate crack tips at the root of the micro-protrusion when cracks occur in the furnace cylinder, generating a local stress peak higher than the average stress field at this location. This triggers the shear thinning response of the stress-response layer earlier and more sensitively. This is equivalent to actively guiding the location and direction of crack initiation, transforming random and uncontrollable crack behavior into a controllable and predictable repair trigger point. The height and spacing of the micro-protrusions are optimized to effectively amplify stress without becoming new crack sources due to processing defects.
[0027] Furthermore, the self-healing material has a multiple repair memory function: after the first repair is completed, the stress response layer material remaining at the bottom of the heat exchange tank still maintains sufficient volume and responsiveness. When the same area cracks again, the residual material is reactivated and penetrates into the repair. This memory function is provided by pre-strained NiTi alloy particles, pre-strained zirconia particles, or silicon carbide particles.
[0028] By employing the above technical solution, the pre-strained particles release their stored strain energy at high temperatures, generating restoring stress. This restoring stress continuously acts on the residual stress-response layer material, maintaining close contact with the crack tip. Even after multiple repairs, the residual material retains sufficient response volume and rheological properties. This overcomes the limitation of traditional self-healing materials failing after a single use, enabling the furnace shell to self-repair minor damage multiple times throughout its service life.
[0029] Furthermore, a gas pressure sensor is installed inside the heat exchange tank. The gas pressure sensor is electrically connected to a controller outside the furnace cylinder to monitor the gas pressure changes in the heat exchange tank in real time. When the self-healing material penetrates the crack and causes the gas pressure in the annular groove to drop, the controller sends a repair status indication signal.
[0030] By adopting the above technical solution, operators can use the monitoring system to know in real time whether microcracks have occurred in the furnace cylinder and whether self-repair has been initiated. This indication signal can be used to schedule preventative maintenance and avoid sudden failures. Simultaneously, data from the pressure sensor can also be used to analyze the frequency and location of crack occurrences, providing a basis for optimizing the furnace cylinder design.
[0031] In summary, this application includes at least one of the following beneficial effects: 1. The composite structure of circumferential heat exchange grooves on the outer side of the cylinder and axial heat exchange fins on the inner side not only significantly improves the heat exchange area and thermal conductivity of the combustion chamber, but also uses axial fins to reinforce radial strength, thus solving the problems of uneven strength and limited heat exchange in traditional open-type structures.
[0032] 2. By setting a multi-layer composite self-healing material layer in the heat exchange tank, the automatic detection and filling of microcracks is achieved by utilizing the shear thinning characteristics of stress response. Combined with the continuous replenishment of glass melt activated by temperature gradation, online self-healing of the graphite furnace cylinder is realized under high-temperature operation, which significantly improves the safety and service life of the equipment.
[0033] 3. A highly sensitive and selective stress triggering mechanism is achieved through a stress-responsive layer with a specific formulation (silicate glass, nano-silicon carbide whiskers, boric anhydride, and thixotropic modifier). It does not flow when static but flows immediately upon shearing, thus avoiding false triggering.
[0034] 4. Adding microencapsulated reducing agents to the stress-response layer releases a reducing atmosphere during crack propagation, effectively inhibiting the oxidation and corrosion of graphite, making it particularly suitable for high-temperature, oxygen-containing environments such as hydrogen chloride synthesis furnaces.
[0035] 5. Stress concentration micro-protrusions are set at the bottom of the heat exchange tank to actively guide the location of cracks and amplify local stress, thereby improving the response sensitivity of the self-healing system and enabling micro-cracks to be repaired before they expand into macroscopic cracks.
[0036] 6. The introduction of a multi-repair memory function (pre-strain particles) enables the self-healing material to be used repeatedly, significantly extending the overall service life of the furnace cylinder.
[0037] 7. By monitoring the repair status in real time through pressure sensors, intelligent maintenance early warning is achieved, which improves the maintainability and safety of the equipment. Attached Figure Description
[0038] Figure 1 This is a schematic diagram of the structure of an embodiment of this application.
[0039] Figure 2 This is an axial sectional view of an embodiment of this application.
[0040] Figure 3This is a radial sectional view of an embodiment of this application.
[0041] Figure 4 This is a schematic diagram of the structure in this application embodiment where only the reinforcing member strengthens the heat exchange tank; Figure 5 This is a schematic diagram of the connection relationship between the self-healing material layer and the reinforcing member in an embodiment of this application.
[0042] In the figure: 1. Cylinder; 11. Heat exchanger groove; 12. Heat exchanger fins; 13. Reinforcing member; 2. Self-healing material layer; 21. Stress response layer; 22. Temperature activation layer; 23. Sealing layer. Detailed Implementation
[0043] The present application will be further described in detail below with reference to the accompanying drawings. It should be noted that the embodiments and features in the embodiments of the present application can be combined with each other.
[0044] I. Structural Part Reference Figures 1 to 3 This application discloses a graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity, comprising a cylinder body 1. The cylinder body 1 is formed by isostatic pressing of high-purity fine-particle graphite and then machining. A heat exchange groove 11 is provided circumferentially on the outer wall of the cylinder body 1. The heat exchange groove 11 can be multiple annular grooves evenly distributed along the axial direction of the cylinder body, or it can be a continuous spiral groove. This embodiment uses an annular groove as an example. Heat exchange fins 12 are integrally formed on the inner wall of the cylinder body 1. The heat exchange fins 12 extend parallel to the axial direction of the cylinder body, and their cross-section is rectangular or trapezoidal. The heat exchange fins 12 can also be fixed to the inner wall of the cylinder body by embedding, bonding, or other methods.
[0045] Reference Figure 4 The heat exchange tank 11 is covered with a reinforcing member 13, which is formed by winding and curing carbon fiber bundles impregnated with phenolic resin, or it can be a carbon cloth laminate. The contact surface between the reinforcing member 13 and the cylinder 1 is coated with graphite thermally conductive adhesive to ensure heat transfer efficiency.
[0046] Reference Figure 5 In other embodiments, a multi-layered composite self-healing material layer 2 is further provided inside the heat exchange tank 11 and on the inner side of the reinforcing member 13. The self-healing material layer 2, from the inside out (i.e., from the bottom of the heat exchange tank towards the opening), consists of a stress-responsive layer 21, a temperature-activating layer 22, and a sealing layer 23. The stress-responsive layer 21 fills the bottom of the heat exchange tank 11. The temperature-activating layer 22 covers the stress-responsive layer 21. The sealing layer 23 is a porous ceramic cover plate (such as silicon carbide porous ceramic), which is applied to the outside of the temperature-activating layer 22 using a high-temperature adhesive, and its porosity is controlled between 30% and 50%.
[0047] Stress concentration micro-protrusions are machined on the bottom surface of the heat exchange tank 11, arranged circumferentially. The height of the stress concentration micro-protrusions is 0.3 mm, the spacing is 3 mm, and they are hemispherical or conical. When microcracks are generated in the inner wall of the furnace and extend to the bottom of the heat exchange tank, the crack tip preferentially terminates at the root of the stress concentration micro-protrusion, resulting in higher stress concentration at this point, thereby more effectively triggering the shear thinning response of the stress response layer 21.
[0048] The self-healing process is as follows: When a crack occurs on or within the inner wall of furnace cylinder 1, the crack extends towards the bottom of heat exchange tank 11. The stress field at the crack tip causes local shear thinning of the stress-responsive layer 21 material, reducing its viscosity and allowing the material to penetrate the crack. Simultaneously, the furnace temperature melts the low-melting-point glass powder in the temperature-activated layer 22, and the liquid glass flows downward along the crack, filling the crack gap and solidifying to form a dense repair. If the microcapsules are punctured during crack propagation, the reducing agent is released and consumes surrounding oxygen, preventing oxidation of the graphite matrix. After repair, the remaining stress-responsive layer material retains sufficient volume and responsiveness, allowing the process to be repeated when the same area cracks again.
[0049] II. Self-healing materials The formulations of the stress-responsive layer and the temperature-activated layer are verified through specific embodiments and comparative examples.
[0050] (I) Raw materials and preparation methods Preparation of stress-responsive layer material: Weigh each component according to the specified mass fractions. Place silicate glass powder (average particle size 20 μm), nano-silicon carbide whiskers (diameter 100 nm, aspect ratio 20), boric anhydride (analytical grade), and thixotropic modifier (hydrophobic fumed silica) into a ball mill and mix at 200 rpm for 2 hours. Then heat to 120℃ to melt the boric anhydride, stir evenly, cool and crush into particles with a particle size of 0.5–2 mm for later use.
[0051] Preparation of microencapsulated reducing agent: Graphene-coated silica microcapsules were prepared using an emulsion template method. A graphene oxide dispersion was mixed with tetraethyl orthosilicate to form an oil phase. Boron carbide powder (average particle size 2 μm) was added as a core material. Emulsification was performed in the presence of an emulsifier, followed by hydrothermal reduction with a reducing agent to obtain graphene-coated silica microcapsules with an average particle size of 20 μm. The microcapsules were then dispersed in stress-responsive layer particles at a specified ratio.
[0052] Preparation of temperature-activated layer material: CaO-Al2O3-SiO2 glass powder (softening temperature 700℃) and MgO-B2O3-SiO2 glass powder (softening temperature 900℃) are mixed in a mass ratio, ball-milled for 30 minutes, and passed through a 200-mesh sieve.
[0053] Sample preparation: A simulated heat exchange groove (10 mm wide, 8 mm deep) was machined on a graphite block (50 × 50 × 20 mm). Stress-responsive layer material and temperature-activated layer material were then sequentially filled in, and the block was sealed with a porous ceramic plate. The block was then placed in a high-temperature furnace to simulate the conditions of a hydrogen chloride synthesis furnace (nitrogen atmosphere, 750℃ for 100 hours), and then cooled to room temperature. Microcracks were pre-introduced on the back of the block using external force (cracks were created using the Vickers hardness tester indentation method), and the temperature was raised again to 750℃ to observe the repair process.
[0054] (II) Examples and Comparative Formulations Formulations (parts by weight) for stress-responsive layer and temperature-activated layer
[0055] 2. Shear thinning ratio: When the shear rate increases from 0.1 s⁻¹ to 100 s⁻¹, the viscosity change is measured, and the ratio of the viscosity at 100 s⁻¹ to the viscosity at 0.1 s⁻¹ is calculated.
[0056] 3. Crack filling rate: The repaired specimen is cut along the crack direction, the crack cross-section is observed with a scanning electron microscope, and the percentage of the crack length that is filled is calculated to the total crack length.
[0057] 4. Strength recovery rate after repair: Perform a three-point bending test on the repaired specimen and compare it with the original undamaged specimen to calculate the bending strength recovery rate.
[0058] 5. Antioxidant properties: The repaired test block was placed in air at 850℃ for 24 hours and the mass loss rate was measured.
[0059] 6. Multiple repair capability: Repeat the crack-repair cycle 3 times on the same test block, and check the crack filling rate after each repair.
[0060] (iv) Test Results Performance test results
[0061] 2. Fluxing and flow-promoting effects of boric anhydride Comparative Example 2, without the addition of boric anhydride, showed a normal static yield stress (490 Pa), but a shear thinning ratio of 0.05, a crack filling rate of only 55%, and a strength recovery rate of 48%. Boric anhydride melts at high temperatures (approximately 577°C), significantly reducing the viscosity of the glass powder and improving its wettability on the graphite surface, thus promoting the capillary penetration of the repair medium along the microcracks. After adding 15 parts of boric anhydride (Example 1), the filling rate increased to 96%.
[0062] 3. Antioxidant effect of microencapsulated reducing agents Comparative Example 4, without microcapsule reducing agent, showed an oxidation mass loss rate as high as 4.8% at 850℃, while Example 1 showed 2.1%. In Example 5, increasing the microcapsule content to 10% reduced the oxidation loss rate to 1.5%. This indicates that the boron carbide microcapsules rupture and release during crack propagation, reacting with oxygen to generate B2O3, which consumes the oxygen surrounding the crack. Simultaneously, B2O3 itself is a glassy filler, further sealing the crack; this dual effect enhances the antioxidant performance.
[0063] 4. The graded melting effect of the temperature-activated layer Comparative Example 5 uses only single-component CAS glass (softening temperature 700℃). While it has repair capabilities at normal furnace temperatures, when abnormally high temperatures occur (above 850℃), the lack of a second component with a higher softening point results in excessively low viscosity of the repair medium, leading to easy loss. In actual testing, the repair effect of Comparative Example 5 decreased after thermal cycling at 850℃. Example 1, however, uses a CAS / MBS mixture of 2:1. At 700℃, CAS melts to provide basic repair, and above 850℃, MBS also melts, increasing the volume and fluidity of the repair medium and adapting to more demanding conditions.
[0064] 5. Multiple repairs and verifications of memory function Example 1 maintained a 91% fill rate after three cycles of repair, indicating that the residual material still possesses responsiveness. This memory function originates from the pre-strained particles (SiC whiskers, which inherently possess some residual stress, can also be supplemented with NiTi alloy particles). Comparative Example 1 (pure glass powder) showed a fill rate of only 15% after three cycles, indicating that the material without memory function was depleted after just one repair.
[0065] 6. Formula with optimal overall performance Both Examples 1 and 2 exhibited excellent overall performance, with Example 2 (high whisker, high boron) showing slightly better strength and oxidation resistance, but slightly higher thixotropy. Example 1 achieved the best balance among all indicators and is suitable as a standard formulation.
[0066] III. Summary of Implementation Principles The implementation principle of the graphite furnace cylinder of the high thermal conductivity hydrogen chloride synthesis furnace in this application embodiment is as follows: The heat exchange grooves 11 on the outer circumferential side of the cylinder 1 and the heat exchange fins 12 on the inner axial side constitute an internal and external composite heat exchange structure, which greatly improves the heat exchange area and thermal conductivity. At the same time, the axial fins reinforce the radial strength, solving the problem of reduced strength in traditional slotted structures. A multi-layer composite self-healing material layer 2 is set in the heat exchange grooves 11: the thixotropic material in the stress response layer 21 remains solid when static. When the crack extends to the bottom of the heat exchange groove, the shear stress at the crack tip causes the material viscosity to drop sharply and penetrate into the crack; the graded glass powder in the temperature activation layer 22 melts step by step at the furnace temperature, providing a continuous liquid repair medium; the sealing layer 23 prevents the medium from being lost prematurely. The glass filling the crack forms a strong bond with the graphite matrix, restoring structural integrity. The reducing agent in the microcapsules is released when the crack extends, preventing graphite oxidation. The stress concentration micro-protrusions actively guide the crack location and amplify the local stress, improving the response sensitivity. After multiple repairs, the restoring stress provided by the pre-strained particles keeps the residual material active, achieving a "repair memory." Pressure sensors monitor real-time pressure changes within the heat exchange tank, sending a signal when the repair material seeps in and causes a pressure drop, enabling intelligent maintenance and early warning.
[0067] To verify the shear thinning characteristics and high-temperature stability of the stress-responsive layer, rheological tests were performed on the stress-responsive layer materials of Examples 1-7 and Comparative Examples 1-5. A high-temperature rotational rheometer (Anton Paar MCR 302, equipped with an electric heating furnace and a 25mm parallel plate rotor with a 1.0mm gap) was used to test the steady-state shear viscosity versus shear rate at 750℃ and 850℃, as well as the static yield stress (through stress scan mode, frequency 0.1Hz, strain 0.01%~100%). The results are shown below.
[0068] Rheological properties of stress-responsive layer material (750℃)
[0069] Supplementary analysis: In Example 1, the static yield stress at 750℃ was 520 Pa, indicating that the material could remain solid and not flow under no external force. When the shear rate increased from 0.1 s⁻¹ to 100 s⁻¹, the viscosity decreased from 12500 Pa·s to 100 Pa·s, a decrease of two orders of magnitude, proving that the material is extremely sensitive to the shear stress generated by crack propagation and can rapidly penetrate microcracks. In Comparative Example 3, without the addition of a thixotropic modifier, the shear-thinning ratio was only 0.2, indicating a sluggish response.
[0070] To verify the material's adaptability at different furnace temperatures, rheological data at 850°C were added. It was found that in Example 1, the static yield stress decreased to 380 Pa at 850°C, while the shear thinning ratio remained at 0.009, indicating good responsiveness. Rheological properties of stress-responsive layer material (850℃)
[0071] Preparation and characterization of microencapsulated reducing agents Taking the microcapsule reducing agent in Example 1 as an example, the detailed preparation steps are as follows: Preparation of graphene oxide dispersion: Graphene oxide (GO, monolayer ratio >95%) was ultrasonically dispersed in deionized water at a concentration of 2 mg / mL.
[0072] Oil phase preparation: Mix 3.5g of tetraethyl orthosilicate (TEOS) with 5g of anhydrous ethanol, add 5g of boron carbide micro powder (average particle size 2μm, purity 99.5%), and ultrasonically disperse for 15min.
[0073] Emulsification: Add 0.5g of polyvinyl alcohol (PVA) to 100mL of deionized water, dissolve it, add the oil phase, and emulsify by high-speed shearing (10000rpm, 5min) to obtain an O / W emulsion.
[0074] Microencapsulation: Ammonia was added dropwise to the emulsion to adjust the pH to 9-10, and the mixture was stirred at room temperature for 12 hours to allow TEOS to hydrolyze and condense to form a silica shell. Then, 0.2 g of hydrazine hydrate was added, and the mixture was reduced at 80 °C for 2 hours to reduce GO to graphene (rGO) and coat the surface of the silica shell.
[0075] Separation and drying: centrifugation, washing with deionized water three times, and vacuum drying at 60℃ to obtain graphene-coated silica microcapsules, with boron carbide encapsulated inside.
[0076] Characterization results: Particle size distribution: D measured by laser particle size analyzer 50 = 18.6μm, D 90 = 28.3μm.
[0077] Encapsulation rate: According to thermogravimetric analysis (TGA, nitrogen atmosphere, heated to 1000℃), the boron carbide content accounts for 32.5 wt% of the total mass of the microcapsules.
[0078] Release temperature: Heating to 750℃ in air causes the microcapsule shell to rupture, releasing boron carbide and causing an oxidation reaction (weight loss plateau). The release temperature range is 680~780℃, matching the normal operating temperature of the synthesis furnace.
[0079] SEM images (images omitted) show that the microcapsules are spherical and intact, with wrinkled graphene sheets on the surface.
[0080] Multiple repair cycles and memory repair function tests Using the specimen from Example 1, three crack initiation-repair cycles were performed at 750°C. After each cycle, the strength recovery rate was tested by a three-point bending test, and the crack filling rate was observed by SEM. Meanwhile, a control group was established using a formulation without pre-strained particles (the pre-strained characteristics of nano-SiC whiskers were removed and replaced with ordinary SiC particles, based on Example 1).
[0081] Table 6 Performance of multiple repair cycles (Example 1 vs. control group) Loop count Example 1 Crack filling rate Crack filling rate in control group Example 1 Strength Recovery Rate Control group strength recovery rate 1st time 96% 94% 92% 90% 2nd time 93% 68% 88% 55% 3rd 91% 41% 85% 32% The nano-SiC whiskers in Example 1, due to their lattice distortion and residual stress (pre-strain) at high temperatures, can still provide continuous recovery stress after each repair, prompting the residual stress-response layer material to maintain contact with the crack tip, thus achieving multiple repair memory. Ordinary SiC particles in the control group have no pre-strain effect, and the filling rate drops significantly during the second repair. This data demonstrates that pre-strained particles (including pre-strained NiTi alloys, pre-strained zirconia, etc.) are key to imparting multiple repair capabilities.
[0082] Thermal conductivity test The thermal conductivity of graphite furnace cylinder samples with different structures was measured using a laser scintillation method (Netzsch LFA 457) in the range of room temperature to 800°C. The samples included: a conventional through-hole structure, a structure with only heat exchange grooves, a structure with only heat exchange fins, and the composite structure of the present application (Example 1).
[0084] In summary, this application achieves the goals of high thermal conductivity, self-healing, and long lifespan for the graphite furnace shell of the hydrogen chloride synthesis furnace combustion chamber through the synergy of structural optimization (outer circumferential heat exchange grooves + inner axial heat exchange fins) and an intelligent self-healing material system (stress-responsive shear-thinning layer + temperature-graded activated glass layer + microcapsule reducing agent + multiple repair memory function). Supplementary experimental data (rheological, DSC, TGA, SEM, mechanical testing, and thermal conductivity testing) demonstrate the feasibility and superiority of this technical solution.
[0085] The above description is merely a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, or improvements made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. A graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity, comprising a cylinder body, characterized in that: A heat exchange groove is provided on the outer side of the cylinder, and the heat exchange groove is arranged along the circumference of the cylinder. A heat exchange fin is provided on the inner side of the cylinder, and the heat exchange fin is arranged along the axial direction of the cylinder.
2. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 1, characterized in that: The heat exchange groove is an annular groove, and several heat exchange grooves are evenly distributed along the axial direction of the cylinder.
3. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 1, characterized in that: The heat exchange groove is a spiral groove.
4. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 1, characterized in that: The cylindrical body is covered with reinforcing members at the heat exchange tank.
5. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 4, characterized in that: The reinforcing element is carbon cloth and / or carbon fiber bundles.
6. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 1, characterized in that: The inner side of the reinforcing member is also provided with a multi-layer composite self-healing material layer, which includes a stress response layer, a temperature activation layer and a sealing layer from the inside to the outside. The stress response layer is filled at the bottom of the heat exchange tank and is composed of a non-Newtonian fluid material with shear thinning characteristics. It is in a solid or high-viscosity state under stress-free conditions. When the furnace body at the corresponding position at the bottom of the heat exchange tank develops cracks and forms local stress concentration, the viscosity of the material in this layer decreases and it penetrates along the cracks. The temperature activation layer covers the stress response layer and contains at least two glassy powders with different melting points. These powders melt step by step within the normal operating temperature range of the synthesis furnace, providing a continuous supply of liquid repair medium to the stress response layer. The sealing layer is a porous ceramic cover plate, which is fixedly placed on top of the temperature activation layer.
7. The graphite furnace cylinder for the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 6, characterized in that: The stress-responsive layer material is composed of the following components in parts by mass: 40-60 parts of silicate glass powder, 5-15 parts of nano-silicon carbide whiskers, 10-20 parts of boric anhydride, and 1-5 parts of thixotropic modifier; the thixotropic modifier is fumed silica or attapulgite that has undergone surface hydrophobic treatment, so that the yield stress of the material is ≥500 Pa when there is no shear, and the viscosity is reduced to less than 1 / 100 of the original value when the shear stress is ≥1000 Pa.
8. The graphite furnace cylinder of the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 7, characterized in that: The stress-responsive layer material also contains microencapsulated reducing agents, which are boron carbide or silicon powder, encapsulated in graphene-coated silica microcapsules.
9. The graphite furnace cylinder of the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 6, characterized in that: The temperature-activated layer consists of two types of glass powder with different softening temperature ranges: the first component has a softening temperature of 650℃ to 750℃, and the second component has a softening temperature of 850℃ to 950℃. When the furnace operating temperature is below 750℃, only the first component melts to provide the repair medium; when the temperature exceeds 850℃, the second component also melts, increasing the fluidity of the repair medium.
10. The graphite furnace cylinder of the combustion chamber of a hydrogen chloride synthesis furnace with high thermal conductivity according to claim 9, characterized in that: The temperature-activated layer is composed of CaO-Al2O3-SiO2 glass powder and MgO-B2O3-SiO2 glass powder in a mass ratio of 1:1 to 3:1; wherein the softening temperature of the CaO-Al2O3-SiO2 glass powder is 650℃ to 750℃, and the softening temperature of the MgO-B2O3-SiO2 glass powder is 850℃ to 950℃.