Semiconductor device and method of manufacturing the same
By designing multi-layer epitaxial layers and rectifier structures, combined with a polyimide protective layer, the problems of poor electrical isolation and environmental regulations in the process of shrinking semiconductor devices have been solved, achieving thinning of high-voltage components and improved heat dissipation capabilities.
Patent Information
- Application Number
- CN202510587149.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-08
- Publication Date
- 2026-11-10
AI Technical Summary
Existing semiconductor devices suffer from poor electrical isolation during the miniaturization process, leading to decreased product reliability. Meanwhile, EU environmental regulations restrict the use of lead-containing solders, necessitating the search for lead-free solder alternatives.
It adopts a multi-layer epitaxial structure, including a first epitaxial layer and a second epitaxial layer, combined with a rectifier structure and an electrode structure, using polyimide as a protective layer, and the electrode structure penetrates the substrate and protrudes from its bottom surface, avoiding the use of lead-containing materials.
It achieves the thinning of high-voltage components, improves electrical isolation and heat dissipation, complies with EU environmental regulations, and reduces ohmic contact resistance.
Smart Images

Figure CN123076004A_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to a semiconductor device having a double epitaxial layer and a method for manufacturing the same. Background Technology
[0002] The semiconductor integrated circuit industry has experienced rapid growth over the past few decades. Technological advancements in semiconductor materials and design have resulted in increasingly compact and complex circuits. Advances in related processing and manufacturing technologies have also enabled new materials and designs.
[0003] In the development of semiconductors, as the smallest manufacturable component size decreases, the number of interconnect devices per unit area also increases. This limits the permissible separation distance between conductive elements in the current conduction path, leading to poor electrical isolation and decreased product reliability. Furthermore, the use of lead-containing solder in semiconductor device packaging is currently the mainstream approach. However, with the enactment and restrictions of EU environmental regulations, researchers are constantly searching for other suitable materials to replace lead solder. Currently, lead-free solder remains an unresolved issue, failing to meet environmental requirements. Summary of the Invention
[0004] Embodiments of this disclosure relate to a semiconductor device, comprising: a first epitaxial layer having a first surface and a second surface opposite to each other; a second epitaxial layer disposed on the first surface of the first epitaxial layer and having a third surface remote from the first epitaxial layer; a first rectifier structure disposed on the third surface of the second epitaxial layer; and a first electrode structure disposed on the third surface of the second epitaxial layer, the first electrode structure comprising: a first electrode sheet located on and electrically connected to the first rectifier structure; and a second electrode sheet having a first portion located on the third surface of the second epitaxial layer and a second portion extending from the third surface toward the second surface of the first epitaxial layer, wherein the second portion penetrates the first epitaxial layer and the second epitaxial layer and protrudes from the second surface of the first epitaxial layer; and a second electrode structure disposed on the second surface of the first epitaxial layer, wherein the second electrode structure contacts the bottom and a portion of the sidewall of the second portion of the second electrode sheet protruding from the second surface.
[0005] Embodiments of this disclosure relate to a method of manufacturing a semiconductor device. The method includes: forming a rectifying structure on a first surface of a substrate, wherein the substrate includes a first epitaxial layer and a second epitaxial layer stacked in a vertical direction, the second epitaxial layer being adjacent to the first surface and the first epitaxial layer being remote from the first surface; forming a first dielectric layer covering the substrate and the rectifying structure, wherein the first dielectric layer has a plurality of openings exposing portions of the rectifying structure and portions of the substrate; removing the portions of the substrate exposed by the first dielectric layer to form a first opening, wherein the depth of the first opening is greater than the thickness of the first epitaxial layer and the second epitaxial layer; forming a first electrode structure on the first surface of the substrate and in the first opening; reducing the thickness of the substrate such that the bottom of the first electrode structure protrudes from the substrate; forming a second electrode structure on a second surface of the substrate opposite to the first surface, wherein the second electrode structure covers the bottom of the first electrode structure; and forming a molding material layer surrounding the second electrode structure and the substrate.
[0006] To make the above features and advantages of this disclosure more apparent and easier to understand, the embodiments are described in detail below with reference to the accompanying drawings. Attached Figure Description
[0007] The various embodiments of this disclosure can be best understood when read in conjunction with the accompanying drawings and the following detailed description. It should be noted that the structures are not drawn to scale. In fact, for clarity of explanation, the dimensions of the various structures may be arbitrarily enlarged or reduced.
[0008] Figure 1 The diagram shown is a cross-sectional view of a semiconductor device according to certain embodiments of this invention;
[0009] Figure 2 The diagram shown is a cross-sectional view of a semiconductor device according to certain embodiments of this invention;
[0010] Figure 3 The image shown is a top view of a semiconductor device according to certain embodiments of this invention;
[0011] Figure 4 The diagram shown is a circuit layout diagram of a semiconductor device according to certain embodiments of this invention;
[0012] Figure 5-21 The diagram shown is a cross-sectional view of one or more stages in a method for manufacturing a semiconductor device according to certain embodiments of this invention.
[0013] Identical or similar components are designated using the same reference numerals in the drawings and detailed description. Several embodiments of this disclosure will be readily understood from the following detailed description in conjunction with the accompanying drawings. Detailed Implementation
[0014] The following disclosure provides numerous different embodiments or examples for implementing various features of the provided subject matter. Specific examples of components and configurations are described below. Of course, these are merely examples and are not intended to be limiting. In this disclosure, references to forming a first feature above or on a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which an additional feature may be formed between the first and second features such that the first and second features are not in direct contact. Furthermore, reference numerals and / or letters may be repeated in various instances of this disclosure. Such repetition is for simplicity and clarity and does not in itself indicate a relationship between the various embodiments and / or configurations discussed.
[0015] Embodiments of this disclosure are discussed in detail below. However, it should be understood that this disclosure provides many applicable concepts that can be embodied in a wide variety of specific environments. The specific embodiments discussed are merely illustrative and do not limit the scope of this disclosure.
[0016] The embodiments are described in detail below with reference to the accompanying drawings, but these embodiments are not intended to limit the scope of this disclosure. Furthermore, the drawings are for illustrative purposes only and are not based on original dimensions; therefore, their size and scale may differ from actual dimensions.
[0017] The terms “top,” “bottom,” and “side” are used with reference to the accompanying drawings and should not be construed as indications of directional limitations when describing the physical apparatus.
[0018] The term "photolithography" refers to a microfabrication process used to pattern parts on a bulk of thin film or wafer, in which a series of processes including applying photoresist, exposure, development and curing are performed in sequence.
[0019] The term "front-end process" refers to the processing steps of a semiconductor die, which typically begins with the fabrication of circuitry embedded in and on the die and ends with the formation of a passivation layer. The term "front-end etching process" refers to the etching process performed during the "front-end process," which is typically used to create patterns on the surface of the die. A typical "front-end etching process" may include, for example, wet chemical etching.
[0020] The term "back-end process" refers to the processing steps of a semiconductor die, which typically begin after the front-end process is completed and generally includes steps such as back-side grinding, die bonding, wire bonding, molding, sawing, and testing. The term "back-end etching process" refers to the etching process performed during the "back-end process," which can be used to form patterns on the bottom of the die. Typical "back-end etching processes" include, for example, plasma etching or sawing.
[0021] The semiconductor device disclosed herein does not contain lead-containing electrical contact pads, complying with EU environmental regulations. Compared to existing processes, the semiconductor device disclosed herein also has the following differences and advantages. First, the semiconductor device disclosed herein has a multilayer epitaxial layer 1 with varying concentrations. Unlike existing processes that achieve concentration gradients through diffusion or ion implantation in a single epitaxial layer, the use of multilayer epitaxial layers allows for a larger concentration difference within a relatively small thickness. Furthermore, the semiconductor device disclosed herein uses polyimide as a protective layer on the front side of the semiconductor device, thus eliminating the need for encapsulation materials (or molding materials). This not only facilitates heat dissipation but also improves forward instantaneous current. Additionally, the semiconductor device disclosed herein has a cathode structure protruding from the bottom surface of the substrate 10, which not only reduces ohmic contact resistance but also further enhances the heat dissipation capacity of the semiconductor device. Combining these structural features, the semiconductor device disclosed herein can thus realize high-voltage devices (e.g., voltages higher than 650 ft, or between 650 and 1500 ft) with a thin substrate 10 (thickness less than or equal to 100 micrometers).
[0022] Figure 1 This is a schematic diagram of a semiconductor device 1 according to certain embodiments of the present disclosure. The drawings have been simplified for illustrative purposes to facilitate a better understanding of the features of the present disclosure. The semiconductor device 1 may be a high-voltage rectifier device (e.g., a high-voltage fast recovery epitaxial diode (FRED)).
[0023] Reference Figure 1 The semiconductor device 1 includes a semiconductor layer 11, a first epitaxial layer 12 and a second epitaxial layer 13 disposed on the top surface 11A of the semiconductor layer 11, a rectifier structure 15 disposed on the top surface 13A of the epitaxial layer 13, a first electrode 16a disposed on the rectifier structure 15, and a second electrode 16b extending from above the top surface 13A of the epitaxial layer 13 to the bottom surface 11B of the semiconductor layer 11.
[0024] Semiconductor layer 11 has opposing surfaces 11A and 11B, first epitaxial layer 12 has opposing surfaces 12A and 12B, and second epitaxial layer 13 has opposing surfaces 13A and 13B. Semiconductor layer 11, first epitaxial layer 12, and second epitaxial layer 13 are stacked vertically. In some embodiments, surface 11A of semiconductor layer 11 contacts surface 12B of first epitaxial layer 12, and surface 12A of first epitaxial layer 12 contacts surface 13A of second epitaxial layer 13. For ease of explanation, the stacked structure of semiconductor layer 11, first epitaxial layer 12, and second epitaxial layer 13 is defined as substrate 10, where surface 13A of second epitaxial layer 13 defines the top surface of substrate 10, and surface 11B of semiconductor layer 11 defines the bottom surface of substrate 10. For ease of explanation, directions orthogonal to the top and bottom surfaces of substrate 10 are defined as vertical directions, and directions orthogonal to the vertical direction are defined as horizontal directions. In some embodiments, surfaces 11A, 11B, 12A, 12B, 13A, and 13B are parallel to each other and may be horizontal surfaces extending in a horizontal direction.
[0025] The semiconductor layer 11 can be made of polycrystalline silicon or monocrystalline silicon. The semiconductor layer 11 can include n-type or p-type doping. For example, the semiconductor layer 11 includes p-type doped regions and n-type doped regions (configurable as p-type transistors) that can be configured for n-type transistors. The n-type doped regions are doped with n-type dopants, such as phosphorus, arsenic, other n-type dopants, or combinations thereof. The p-type doped regions are doped with p-type dopants, such as boron, indium, other p-type dopants, or combinations thereof. The n-type or p-type doped regions can be formed by performing ion implantation, diffusion, and / or other suitable doping processes. The semiconductor layer 11 has a first-type doped region extending from surface 11A to surface 11B and covering the entire surface 11A. For ease of explanation, the first type is described below using the n-type as an example, but this disclosure is not limited thereto; the n-type (first type) or p-type (second type) semiconductor layer 11 can be adjusted according to the conductivity type of the semiconductor rectifier device 1.
[0026] The first epitaxial layer 12 and the second epitaxial layer 13 are silicon-containing polycrystalline structure layers formed by epitaxial growth. In some embodiments, the first epitaxial layer 12 or the second epitaxial layer 13 comprises polycrystalline silicon. The first epitaxial layer 12 and the second epitaxial layer 13 have the same conductivity type as the semiconductor layer 11, i.e., type I doping. In some embodiments, N-type charged ions are introduced during epitaxial growth to form the N-type first epitaxial layer 12 without additional ion implantation. In some embodiments, N-type charged ions are uniformly distributed throughout the first epitaxial layer 12. The semiconductor layer 11, as the drain contact well region of the semiconductor structure 1, requires a high type I doping concentration. In some embodiments, the type I doping concentration of the first epitaxial layer 12 is lower than the type I doping concentration of the semiconductor layer 11. The method for forming the second epitaxial layer 13 can refer to the method for forming the first silicon carbide layer 12, and will not be repeated here. In some embodiments, there is an observable interface between the first epitaxial layer 12 and the second epitaxial layer 13. In some embodiments, the second epitaxial layer 13 has a resistivity between 15 and 50 ohms per centimeter (ohm-cm). In some embodiments, the first epitaxial layer 12 has a resistivity between 1 and 20 ohms per centimeter (ohm-cm). In some embodiments, the semiconductor layer 11 has a resistivity between 0.01 and 0.06 ohms per centimeter (ohm-cm). A higher doping concentration in the first silicon carbide layer 12 helps reduce the recovery time of the reverse current, and a lower doping concentration in the second silicon carbide layer 13 helps increase the breakdown voltage (BV). A greater difference in doping concentration between the first epitaxial layer 12 and the second silicon carbide layer 13 (i.e., a greater difference in resistivity, since doping concentration is inversely proportional to resistivity) is beneficial for reducing noise. Since the first and second epitaxial layers 12 and 13 are formed via different epitaxial growth steps, they can be designed with significantly different doping concentrations as needed, which is beneficial for thinning the total thickness of the substrate 10 without causing noise problems. In some embodiments, the thickness of the semiconductor layer 11 ranges from 5 to 30 micrometers (μm). In some embodiments, the thickness of the first silicon carbide layer 12 and the thickness of the second silicon carbide layer 13 are approximately the same, for example, between 10 and 45 micrometers (μm). In some embodiments, the thickness of the first silicon carbide layer 12 is less than the thickness of the second silicon carbide layer 13. In some embodiments, the thickness of the first silicon carbide layer 12 ranges from 5 to 35 micrometers (μm). In some embodiments, the thickness of the second silicon carbide layer 13 ranges from 5 to 15 micrometers (μm). In some embodiments, the thickness of the substrate 10 ranges from 30 to 100 micrometers (μm).
[0027] Semiconductor device 1 may include a cell region located in a central region and a termination region located in a peripheral region surrounding the cell region. For the purpose of simplifying the drawings, the cell region and the termination region are not indicated by symbols in the drawings. The second epitaxial layer 13 includes a plurality of doped regions 122 located in the cell region and the termination region, and a plurality of doped regions 123 located in portions of the doped regions 122. The doped regions 122 extend from the top surface 13A to the bottom surface 13B of the second epitaxial layer 13, and the doped regions 122 have a depth less than the thickness of the second epitaxial layer 13. In some embodiments, adjacent doped regions 122 are separated from each other. In some embodiments, the doped regions 122 have a second conductivity type different from the first conductivity type. The doped regions 123 have the same second conductivity type as the doped regions 122, and their second type ion doping concentration is higher than that of the doped regions 122. The doped regions 123 serve as contact doped regions for electrodes and are therefore disposed in the doped regions 122 that are in contact with or adjacent to the electrodes.
[0028] A rectifying structure 15 is disposed on the top surface 13A of the second epitaxial layer 13. In some embodiments, the rectifying structure 15 is located at least in a cell region of the semiconductor device 1 (the cell region is not shown in the figures, but it is understood that the semiconductor device 1 has a cell region located in the central region and a termination region surrounding the cell region). The rectifying structure 15 can be a single-layer structure or a multi-layer structure. In some embodiments, the rectifying structure 15 includes multiple metal layers of different materials. In some embodiments, a portion of the rectifying structure 15 contacts a portion of the top surface 13A of the second epitaxial layer 13. In some embodiments, the material of the rectifying structure 15 includes copper, aluminum, titanium, indium, aluminum, gallium, silicon, alloys thereof, or combinations thereof. In some embodiments, the semiconductor device 1 further includes a dielectric layer 132 disposed on the top surface 13A of the second epitaxial layer 13. In some embodiments, the edge portion of the rectifying structure 15 is separated from the top surface 13A of the second epitaxial layer 13 by the dielectric layer 132.
[0029] Semiconductor device 1 may be a single die having a first electrode 16a and a second electrode 16b, which are disposed separately from each other. The first electrode 16a is located on and electrically connected to the rectifier structure 15. In some embodiments, the first electrode 16a contacts the rectifier structure 15. The second electrode 16b extends from above the top surface (i.e., surface 13A) of the substrate 10 to the bottom surface (i.e., surface 11B). The second electrode 16b penetrates the substrate 10 and protrudes from the bottom surface of the substrate 10. Specifically, the second electrode 16b has a vertical portion 164 penetrating the semiconductor layer 11, the first epitaxial layer 12, and the second epitaxial layer 13 to electrically connect to the electrode structure 17 located on the bottom surface 11B of the semiconductor layer 11. In some embodiments, the electrode structure 16 is also referred to as the front electrode structure 16, and the electrode structure 17 is also referred to as the back electrode structure 17. In some embodiments, the electrode structure 17 may be a single metal layer or a multi-layer metal layer structure. For illustrative purposes, the electrode structure 17 with a single metal layer is used as an example in the following description and accompanying drawings, but this disclosure is not limited thereto. In some embodiments, the bottom 164B of the second electrode 16b contacts the electrode structure 17. In some embodiments, the electrode structure 17 contacts the bottom surface and bottom sidewall of the second electrode 16b. The first electrode 16a and the second electrode 16b serve as the anode and cathode, respectively, during operation of the semiconductor device 1. For ease of explanation, the first electrode 16a is referred to as the anode and the second electrode 16b as the cathode in the following description.
[0030] The first electrode 16a and the second electrode 16b can each be a single-layer conductive structure or a multilayer conductive structure containing different metal materials. In some embodiments, the first electrode 16a includes a first conductive material layer 161 and a second conductive material layer 162 located on the first conductive material layer 161. In some embodiments, the first conductive material layer 161 contains copper and the second conductive material layer 162 contains tin, but this disclosure is not limited thereto, and the first conductive material layer 161 and the second conductive material layer 162 can have other suitable metal materials, such as tungsten, titanium, platinum, tantalum, etc. In the embodiments of this disclosure, the semiconductor device 1 does not contain lead. In some embodiments, for ease of manufacturing, the second electrode 16b can have a single or multilayer structure similar to the first electrode 16a. For example, the second electrode 16b can include the first conductive material layer 161 and the second conductive material layer 162 located on the first conductive material layer 161. In other words, the first conductive material layer 161 and the second conductive material layer 162 together define the electrode structure 16, and the electrode structure 16 includes the first electrode 16a as the anode and the second electrode 16b as the cathode. In some embodiments, the first conductive material layer 161 of the second electrode 16b extends on the top surface of the substrate 10 and extends from surface 13A to surface 11B, penetrating the substrate 10. In some embodiments, the bottom of the second electrode 16b protrudes from the bottom surface of the substrate 10. In some embodiments, the second conductive material layer 162 of the second electrode 16b is located on the first conductive material layer 161 on the top surface of the substrate 10 and is separated from the top surface of the substrate 10.
[0031] To reduce leakage current, the portion of the first electrode 16a not in contact with the rectifier structure 15 is separated from the top surface of the substrate 10 by a dielectric structure 14, and the second electrode 16b, partially located above the top surface of the substrate 10, is also separated from the top surface of the substrate 10 by the dielectric structure 14. To adapt to the market trend of miniaturized products, the dielectric structure 14 can be made of a dielectric material with good dielectric properties; furthermore, to achieve good adhesion and reduce the problem of easy detachment between dissimilar dielectrics, the dielectric structure 14 can have multiple layers. For example, the dielectric structure 14 may include a first passivation layer 141 conformally disposed on the substrate 10, the dielectric layer 132, and the rectifier structure 15, and a second passivation layer 142 covering the first passivation layer 141. The first passivation layer 141 and the second passivation layer 142 may have the same or different dielectric materials (depending on the embodiment, the first passivation layer 141 and the second passivation layer 142 may also be referred to as dielectric layer 141 and dielectric layer 142; hereinafter, to distinguish them from dielectric layer 132, they are referred to as first passivation layer 141 and second passivation layer 142). In some embodiments, the first passivation layer 141 conformally covers the substrate 10, the dielectric layer 132, and the rectifying structure 15. In some embodiments, the second passivation layer 142 covers the entire first passivation layer 141. In some embodiments, the second passivation layer 142 covers all the upper surfaces and sidewalls of the first passivation layer 141. In some embodiments, to maintain good leakage protection even in small-sized products, the material of the second passivation layer 142 includes polyimide, and the material of the first passivation layer 141 includes silicon nitride, silicon oxide, or a combination thereof to provide better adhesion.
[0032] The semiconductor device 1 further includes an electrode structure 17 disposed on the bottom surface of the substrate 10. The electrode structure 17 is electrically connected to the second electrode 16b. In some embodiments, the electrode structure 17 conformally covers the portion of the second electrode 16b that protrudes from the bottom surface of the substrate 10. The semiconductor device 1 further includes a molding material layer 19 disposed on the bottom surface of the substrate 10 and covering the electrode structure 17. The molding material layer 19 protects the electrode structure 17 and fills the dicing channels to protect the sidewalls of the substrate 10. In some embodiments, the molding material layer 19 has a flat surface away from the electrode structure 17.
[0033] Figure 2 , Figure 3 , Figure 4 This is a schematic diagram of a semiconductor device 2 according to certain embodiments of the present disclosure, wherein Figure 2 The image shows along Figure 3 A cross-sectional view of semiconductor device 2 along the A-A' tangent line. Figure 3 This is a top view of semiconductor device 2. Figure 4This is a circuit layout diagram of semiconductor device 2. At least some of these figures have been simplified to better understand the nature of this disclosure. Semiconductor device 2 may be a bridge rectifier device.
[0034] Reference Figure 2 , Figure 3 Semiconductor device 2 includes multiple semiconductor dies, such as Figure 2 The diagram shows a first die C1, a second die C2 adjacent to the first die C1 along a first horizontal direction (e.g., the X direction), a third die C3 adjacent to the first die C1 along a second horizontal direction (e.g., the Y direction), and a fourth die C4 adjacent to the third die C3 along the second horizontal direction and to the second die C2 along the first horizontal direction. Each semiconductor die C1, C2, C3, and C4 includes a portion of the substrate 10; in other words, the substrate 10 is divided into multiple blocks during the manufacturing process, for example... Figure 2 The first block R1 and the second block R2 and Figure 3 The third block R3 and the fourth block R4. Multiple blocks R1, R2, R3, and R4 correspond to multiple semiconductor dies C1, C2, C3, and C4, respectively, and the multiple blocks R1, R2, R3, and R4 are separated by a molding material layer 19. Each semiconductor die C1, C2, C3, and C4 has a structure similar to that of semiconductor device 1. For demonstration purposes, the following description mainly focuses on the parts that are different from semiconductor device 1, and the parts that are similar to or the same as those of semiconductor device 1 will not be repeated.
[0035] Reference Figure 2 , Figure 3 Each die has a plurality of electrodes. For example, the first die C1 has a first electrode 16a as an anode and a second electrode 16b as a cathode, with the anode and cathode being separately disposed from each other. As described above, multiple semiconductor dies C1, C2, C3, and C4 have similar structures, and the substrates 10 of adjacent semiconductor dies C1, C2, C3, and C4 are separated by a molding material layer 19. For example... Figure 1 As shown, a portion of the molding material layer 19 is located between the first block R1 and the second block R2; for example... Figure 2 As shown, the molding material layer 19 surrounds each semiconductor die C1, C2, C3, and C4. The molding material layer 19 extends from the top surface of the substrate 10 to the bottom surface and further covers the electrode structure 17 located on the bottom surface.
[0036] In order to achieve Figure 4 The circuit layout shown allows the bare chips C1, C2, C3, and C4 to be electrically connected for use as a bridge rectifier. Figure 2 The cathode of the first bare die C1 and the anode of the second bare die C2 shown are electrically connected. For example... Figure 2As shown, the second die C2 has two electrodes 16c and 16d, which are the cathode and anode of the second die, respectively. For ease of explanation, the first electrode 16a of the first die C1 is referred to as anode 16a, the second electrode 16b is referred to as cathode 16b, and the electrode 16c of the second die C2 is referred to as anode 16c, and the electrode 16d is referred to as anode 16d.
[0037] Since the cathode 16b of the first bare die C1 and the anode 16c of the second bare die C2 are adjacent, they can be directly electrically connected using the first conductive material layer 161 and the second conductive material layer 162. Figure 2 Cross-sectional view and Figure 3 As can be seen from the top view, the cathode 16b of the first bare die C1 and the anode 16c of the second bare die C2 each include a portion of a first conductive material layer 161 and a portion of a second conductive material layer 162. The portion of the first conductive material layer 161 located on the first block R1 and the portion of the first conductive material layer 161 located on the second block R2 are in contact with each other, and the portion of the second conductive material layer 162 located on the first block R1 and the portion of the second conductive material layer 162 located on the second block R2 are in contact with each other.
[0038] refer to Figure 3 The cathode 16b of the first bare die C1 and the anode 16c of the second bare die C2 are connected along the first horizontal direction to form an electrode plate P2. Similarly, the anode 16a of the first bare die C1 and the anode 16e of the third bare die C3 are adjacent along the second horizontal direction, so they can be directly electrically connected using the first conductive material layer 161 and the second conductive material layer 162 to form an electrode plate P1; the cathode 16f of the third bare die C3 and the anode 16g of the fourth bare die C3 are adjacent along the first horizontal direction, so they can be directly electrically connected using the first conductive material layer 161 and the second conductive material layer 162 to form an electrode plate P4; the cathode 16h of the fourth bare die C4 and the cathode 16h of the second bare die C3 are adjacent along the second horizontal direction, so they can be directly electrically connected using the first conductive material layer 161 and the second conductive material layer 162 to form an electrode plate P3.
[0039] Electrode P2 includes the cathode 16b of the first bare die C1, and therefore electrode P2 has a portion 163 located on the top surface 12A of the silicon carbide substrate 10, and a portion 164 located below the top surface 12A of the silicon carbide substrate 10. Generally speaking, portion 163 extends in a horizontal direction and is therefore also called horizontal portion 163, and portion 164 extends in a vertical direction and is therefore also called vertical portion 164. Similarly, electrode P3 and P4 also have horizontal portions 163 and vertical portions 164. Electrode P1, because it only includes the anode 16a of the first bare die C1 and the anode 16e of the third bare die C3, does not have the vertical portion 164 located below the top surface 12A of the silicon carbide substrate 10, and only has the horizontal portion 163 located on the top surface 12A of the silicon carbide substrate 10.
[0040] Figures 5 to 19 The figures illustrate one or more stages in a method of manufacturing a semiconductor device 1 according to certain embodiments of this invention. At least some of these figures have been simplified to better understand the nature of this disclosure.
[0041] Reference Figure 5 The manufacturing method includes: sequentially forming epitaxial layers 11 and 12 on a semiconductor layer 11 to form a substrate 10. In some embodiments, the semiconductor layer 11 is the entirety or a portion near the top surface of a silicon wafer. In some embodiments, a first epitaxial layer 12 is epitaxially grown on surface 11A of the semiconductor layer 11. In some embodiments, a second epitaxial layer 13 is epitaxially grown on surface 12A of the first epitaxial layer 12. The semiconductor layer 11, epitaxial layer 11, and epitaxial layer 12 have the same conductivity type, such as N-type, and the doping concentration of the first silicon carbide layer 11 is greater than the doping concentration of the second silicon carbide layer 12. In some embodiments, the doping concentration of the first epitaxial layer 12 is less than the doping concentration of the semiconductor layer 11, and the doping concentration of the second epitaxial layer 13 is less than the doping concentration of the first epitaxial layer 12. It should be noted that since the first silicon carbide layer 11 is thinned in subsequent manufacturing steps, therefore... Figure 5 The first silicon carbide layer 11 in the steps shown has a surface 11B' that is different from the surface 11B' of the first silicon carbide layer 11. Figure 1 or Figure 2 Surface 11B is shown in the diagram.
[0042] In some embodiments, the semiconductor layer 11 may be made at least a portion of the wafer near surface 11A to have N-type conductivity via ion implantation. In some embodiments, N-type ions may be introduced during epitaxial growth to form an N-type first epitaxial layer 12 without additional ion implantation. Similarly, in some embodiments, N-type ions are introduced during epitaxial growth to form an N-type second epitaxial layer 13 without additional ion implantation. In some embodiments, N-type ions are uniformly introduced during epitaxial growth to form a first epitaxial layer 12 or a second epitaxial layer 13 with a uniform doping concentration, wherein the ion concentration introduced during epitaxial growth does not change over time. In some embodiments, the second epitaxial layer 13 may have a doping concentration gradient that increases from surface 13A to surface 13B. In some embodiments, the increasing doping concentration gradient may be adjusted according to the required breakdown voltage and resistance of the product. In some embodiments, N-type ions are introduced during epitaxial growth, wherein the concentration of introduced ions decreases with the duration of epitaxial growth to form a second epitaxial layer 13 having a doping concentration increasing from surface 13A to surface 13B. Similarly, the first epitaxial layer 12 may also have a doping concentration increasing from surface 12A to bottom surface 12B as needed. Additionally, the semiconductor layer 11 may be ion implanted to have a concentration gradient increasing from surface 11A to surface 11B'. Regardless of whether the semiconductor layer 11, the first epitaxial layer 12, or the second epitaxial layer 13 has a uniform or non-uniform doping concentration, to achieve the aforementioned effect of the concentration difference, the doping concentration of the semiconductor layer 11 will still be greater than the doping concentration of the first epitaxial layer 12, and the doping concentration of the first epitaxial layer 12 will still be greater than the doping concentration of the second epitaxial layer 13. In some embodiments, the substrate 10 has a doping concentration increasing from the top surface (e.g., surface 13A of the second epitaxial layer 13) to the bottom surface (e.g., surface 11B' of the semiconductor layer 11).
[0043] Furthermore, the substrate 10 can be divided into multiple blocks, such as a first block R1 and a second block R2, which represent the positions of different dies to be formed later. For example, the first block R1 and the second block R2 can each form a single similar die. Figure 1 The bare die of the semiconductor device 1 shown, or for example, the first block R1 and the second block R2, can be formed in a similar manner. Figure 2 The first bare die C1 and the second bare die C2 are shown.
[0044] Reference Figure 6 The manufacturing method includes: forming a patterned masking layer 131 on the surface 13A of the second epitaxial layer 13, and performing ion implantation on the second epitaxial layer 13 using the patterned masking layer 131 as a mask to form a plurality of doped regions 121 in the second epitaxial layer 13 adjacent to the surface 13A.
[0045] The patterned mask layer 131 may be a dielectric layer, the material of which is, for example, a nitride, an oxide, an oxynitride, or a combination thereof. In some embodiments, a dielectric layer is formed on the surface 13A of the second epitaxial layer 13, a patterned photoresist layer is then formed on the dielectric layer, and the dielectric layer is etched using the patterned photoresist layer as a mask to form the patterned mask layer 131. The patterned mask layer 131 has a plurality of openings located in the first block R1 and a plurality of openings located in the second block R2. The plurality of openings in the patterned mask layer 131 define the locations of the doped regions 121 formed in subsequent steps.
[0046] Subsequently, ion implantation is performed on the silicon carbide substrate 10 using the patterned mask layer 131 as a mask to form a plurality of doped regions 121 in the second epitaxial layer 13 adjacent to the top surface of the substrate 10. In some embodiments, the patterned photoresist layer is removed before the ion implantation step. The doped regions 121 have a different conductivity type than the second epitaxial layer 13, for example, P-type. In some embodiments, the P-type ion doping concentration of the doped regions 121 is greater than the N-type ion doping concentration in the second epitaxial layer 13.
[0047] Reference Figure 7 The manufacturing method includes: performing a thermal annealing process on a substrate 10 to diffuse dopant ions in a doped region 121, forming a doped region 122, and forming a dielectric layer 132 on the exposed substrate 10. The doped region 122 is formed after diffusion through the doped region 121; therefore, the doped region 122 and the doped region 121 have the same conductivity but a lower doping concentration, and the depth of the doped region 122 is greater than the depth of the doped region 121. In some embodiments, the dielectric layer 132 is formed after the formation of the doped region 122. In some embodiments, an oxidation step is performed on the surface 13A of the second epitaxial layer 13 to form the dielectric layer 132 on the exposed surface 13A of the second epitaxial layer 13. In some embodiments, the sidewalls of the dielectric layer 132 are in contact with the sidewalls of the dielectric layer 131, and the dielectric layer 132 does not cover the top surface of the dielectric layer 131. In some embodiments, the dielectric layer 132 is deposited to cover the exposed surface 13A of the second epitaxial layer 13 and the dielectric layer 131. In some embodiments, the thickness of dielectric layer 132 is less than the thickness of dielectric layer 131, but this disclosure is not limited thereto. In other embodiments, the thickness of dielectric layer 132 is greater than or equal to the thickness of dielectric layer 131.
[0048] Reference Figure 8The manufacturing method includes: removing a portion of the dielectric layer 132 to expose a portion of the second epitaxial layer 13 that will subsequently form an anode contact; and then ion implanting the exposed second epitaxial layer 13 to form a doped region 123. To reduce resistance, the portion of the second epitaxial layer 13 that will form the anode contact requires a high doping concentration of type II ions. Therefore, a portion of the dielectric layer 132 is removed to expose a portion of the doped region 121 located in the second epitaxial layer 13, and a doped region 123 is formed in the portion of the doped region 121 adjacent to the surface 13A of the second epitaxial layer 13. The doped region 123 and the doped region 122 have the same conductivity type, the doping concentration of the doped region 123 is greater than that of the doped region 122, and the depth of the doped region 123 is less than that of the doped region 121. In some embodiments, the doped region 123, serving as the anode contact doped region, is formed in the doped region 122 located in the central region of each block R1 or R2. In some embodiments, the doped region 123 is further formed in the doped region 122 located in the peripheral region of each block R1 or R2. In some embodiments, prior to ion implantation to form the doped region 123, a platinum (Pt) layer is sputtered to form on the surface 13A of the second epitaxial layer 13, followed by a thermal annealing step to allow platinum ions to diffuse into the doped region 122. The doped regions 122 and / or 123 containing platinum ions help reduce the power consumption of the semiconductor device 1 or 2.
[0049] Reference Figure 9 The manufacturing method includes: forming a rectifying structure 15, and in a rectifier, wherein the rectifying structure 15 at least covers a doped region 123. In some embodiments, the rectifying structure 15 contacts a portion of the substrate 10 exposed by dielectric layers 131 and 132, and is adjacent to the doped region 123 located in the second epitaxial layer 13. In some embodiments, the rectifying structure 15 further covers a portion of the dielectric layer 131 and / or the dielectric layer 132.
[0050] The rectifying structure 15 may include a single metal layer or multiple metal layers. In some embodiments, the rectifying structure 15 includes a single metal layer, as shown in the figures. In other embodiments, the rectifying structure 15 includes at least two metal layers stacked vertically. For example, the rectifying structure 15 may include a first metal layer and a second metal layer covering the first metal layer. The first metal layer may be, for example, a Schottky metal layer, which contacts the surface 13A of the second epitaxial layer 13 to form a Schottky junction. The second metal layer may serve as a conductive structure to provide electrical connections between other conductive pads or conductive lines and the first metal layer.
[0051] Reference Figure 10The manufacturing method includes forming a first passivation layer 141 covering the rectifying structure 15 and dielectric layers 131 and 132. In some embodiments, the material of the first passivation layer 141 includes nitrides, oxides, oxynitrides, or combinations thereof, serving as an adhesion layer between the subsequently formed second passivation layer 142 and the underlying material. The method for forming the first passivation layer 141 includes chemical vapor deposition (CVD), physical vapor deposition (PVD), or a combination thereof. The first passivation layer 141 has a plurality of openings on each block of the substrate 10 to define subsequently formed anode contact sites and cathode contact sites. For example, the first passivation layer 141 has openings O411 and O412 on the first block R1. Opening O411 exposes at least a portion of the rectifying structure 15 on the doped region 123 located in the central region of the first block R1, and opening O412 exposes a portion of the substrate 10 located in the peripheral region of the first block R1. The vertical projection of opening O412 does not overlap with the vertical projection of doped regions 123 and / or 122 (they may be adjacent or separate). As another example, the first passivation layer 141 has openings O413 and O414 on the second block R2. Opening O413 exposes at least a portion of the rectifying structure 15 on the doped region 123 located in the central region of the second block R2, and opening O414 exposes a portion of the substrate 10 located in the peripheral region of the second block R2. The vertical projection of opening O414 does not overlap with the vertical projection of doped regions 123 and / or 122 (they may be adjacent or separate). In some embodiments, the method further includes removing portions of the dielectric layer 131 and / or 132 exposed to the first passivation layer 141 to expose portions of the substrate 10.
[0052] Reference Figure 11The manufacturing method includes forming a second passivation layer 142 covering a first passivation layer 141. The first passivation layer 141 and the second passivation layer 142 constitute a dielectric structure 14. The second passivation layer 142 is designed to electrically isolate the subsequently formed anode and cathode from the rectifier structure 15 and the substrate 10, respectively, and therefore also has multiple openings to define the subsequently formed anode contact positions and cathode contact positions. In some embodiments, the second passivation layer 142 covers the edge of the first passivation layer 141. In some embodiments, the second passivation layer 142 covers the entire top surface and sidewalls of the first passivation layer 141. In some embodiments, the second passivation layer 142 has multiple openings corresponding to multiple openings in the first passivation layer 141. For example, the second passivation layer 142 has openings O421 and O422 on the first block R1. O421 corresponds to opening O411 and opening O422 corresponds to opening O412. The width of opening O421 is smaller than the width of O411, and opening O421 exposes a portion of the rectifying structure 15 located in O411. The width of opening O422 is smaller than the width of O412, and opening O422 exposes a portion of the substrate 10 located in O412. As another example, the second passivation layer 142 has openings O423 and O424 on the second block R2. O423 corresponds to opening O413 and opening O424 corresponds to opening O414. The width of opening O423 is smaller than the width of O413, and opening O423 exposes a portion of the rectifying structure 15 located in O413. The width of opening O424 is smaller than the width of O414, and opening O424 exposes a portion of the substrate 10 located in O414. In some embodiments, the second passivation layer 142 further covers the sidewalls of the dielectric layers 131 and / or 132 adjacent to the opening 412. In some embodiments, the second passivation layer 142 further covers the sidewalls of the dielectric layers 131 and / or 132 adjacent to the opening 414.
[0053] In some embodiments, a sintering process is performed after the formation of the first passivation layer 141 and before the formation of the second passivation layer 142, and the... Figure 10 The intermediate structure is tested. The first passivation layer 141 and the components formed prior to it can be manufactured in a semiconductor front-end fabrication plant, and the second passivation layer 142 and the components formed thereafter can be manufactured in a packaging plant. Therefore, before the formation of the second passivation layer 142, that is... Figure 10Before the intermediate structure is sent to the packaging plant, it can be subjected to circuit testing. In some embodiments, the first passivation layer 141 and the second passivation layer 142 are manufactured in different factories and therefore patterned using different photomasks, but this disclosure is not limited thereto. Depending on the processes that the manufacturing plant can perform, the above steps may be adjusted accordingly. In other embodiments, the first passivation layer 141 and the second passivation layer 142 can be patterned using the same photomask. In addition, in some embodiments, the material of the second passivation layer 142 includes polyimide, which forms a shape after photolithography (including exposure, development, curing, etc.). Figure 11 The configuration shown has rounded corners.
[0054] The positions and configurations of openings O411, O412, O413, O414 and openings O421, O422, O423, O424 can be referenced simultaneously. Figure 3 The top view shown. The configurations of openings O411, O412, O413, O414 and openings O421, O422, O423, O424 may correspond to each other or not. For example, openings O411 and O421 have corresponding shapes, while opening O422 is located within opening O412 and does not have a shape corresponding to opening O412. In some embodiments, such as Figure 3 As shown, the second passivation layer 142 has a plurality of openings O422 corresponding to the number of vertical portions 164 of the cathode. In some embodiments, the plurality of openings O422 are separated from each other, all openings O422 are located in openings O412, and the width of a single opening O422 is smaller than the width of opening O412.
[0055] Reference Figure 12 The manufacturing method includes etching the substrate 10 to form an opening O1. In some embodiments, in Figure 11 A patterned photoresist layer is formed on the intermediate structure shown, exposing the substrate 10 located in openings O422 and O424. The exposed substrate 10 is then etched to form opening O1. In some embodiments, in Figure 9 A protective layer (e.g., a dielectric layer) is formed on the structure shown, exposing the substrate 10 located in openings O422 and O424. The exposed substrate 10 is then etched to form opening O1. In some embodiments, the substrate 10 is etched for a predetermined time length to control the opening O1 to stop within the semiconductor layer 11. Opening O1 does not penetrate the substrate 10. In some embodiments, the width of opening O1 is less than the minimum width of openings O422 or O424. In some embodiments, the shape of opening O1 corresponds to the shape of openings O422 or O424, and the configuration of opening O1 defines the configuration of the vertical portion 164 of the subsequently formed cathode (the configuration of opening O1 can be referenced). Figure 1 ,2 3). In some embodiments, the patterned photoresist layer or protective layer is removed after the etching process.
[0056] Reference Figure 13 The manufacturing method includes: forming a first conductive material layer 161 and filling it into a plurality of openings (e.g., O421, O422, O423, O424) in the second passivation layer 142 and into the opening O1 in the substrate 10, and forming a second conductive material layer 162 to cover the first conductive material layer 161. The method for forming the first conductive material layer 161 and the second conductive material layer 162 may include: forming a seed layer in... Figure 12 On the top surface of the intermediate structure shown, a patterned photoresist layer (or patterned dielectric layer) is then formed on a portion of the seed layer to cover areas other than the cathode and anode; subsequently, an electroplating process is performed on the entire substrate 10. Because the areas other than the cathode and anode are covered by the patterned photoresist layer (or patterned dielectric layer), the first conductive material layer 161 and the second conductive material layer 162 are not formed in areas other than the cathode and anode during the electroplating process. The electroplating process may include sequential electroplating of a first conductive material and electroplating of a second conductive material to separately form a first conductive material layer 161 having the first conductive material and a second conductive material layer 162 having the second conductive material. In some embodiments, the first conductive material layer 161 comprises copper, and the second conductive material layer 162 comprises tin. In embodiments of this disclosure, the semiconductor device 2 does not contain lead. In some embodiments, after the electroplating process, the patterned photoresist layer (or patterned dielectric layer) is removed. In some embodiments, after removing the patterned photoresist layer (or patterned dielectric layer), the exposed seed layer is removed (e.g., using wet etching). In some embodiments, the second conductive material layer 162 is reflowed to form a configuration with rounded corners as shown in the figures. The first conductive material layer 161 is filled into the opening O1, and the portion of the first conductive material layer 161 filled into the opening O1 serves as the vertical portion 164 of the cathode for electrical connection to the electrode structure 17 formed later; while the portions of the first conductive material layer 161 and the second conductive material layer 162 located on the top surface of the substrate 10 (i.e., 13A of the second epitaxial layer 13) serve as the horizontal portions 163 of the anode and cathode for providing an electrical path (or electrical contact point) for connection to an external voltage.
[0057] As above Figure 1As explained, the first conductive material layer 161 and the second conductive material layer 162 together define the electrode structure 16, wherein the portion of electrode 16 located on the first block R1 and electrically connected to the rectifier structure 15 serves as the anode 16a; the portion of electrode 16 located on the first block R1 having a vertical portion 164 and being separately disposed from the anode 16a serves as the cathode 16b; the portion of electrode 16 located on the second block R2 and electrically connected to the rectifier structure 15 serves as the anode 16c; and the portion of electrode 16 located on the second block R2 having a vertical portion 164 and being separately disposed from the anode 16c serves as the cathode 16d.
[0058] Reference Figure 14 The manufacturing method includes: thinning the substrate 10 to expose and protrude the bottom 164B of the vertical portion 164 in the substrate 10. In some embodiments, in order to remove a portion of the semiconductor layer 11 from the surface 11B' of the semiconductor layer 11, the substrate 11 is... Figure 13 After the intermediate structure shown is flipped, it is attached to the carrier plate S1 via the bonding layer 41 (e.g., a molding material or an encapsulation material). In some embodiments, backside grinding and / or chemical mechanical polishing (CMP) are applied. Figure 13 The surface 11B' of the substrate 10 shown is exposed up to the bottom 164B of the vertical portion 164. In some embodiments, backside grinding and / or chemical mechanical polishing (CMP) are applied to... Figure 13 The surface 11B' of the semiconductor layer 11 shown is exposed up to the bottom 164B of the vertical portion 164. In some embodiments, after the bottom 164B of the vertical portion 164 is exposed, an etching process is performed on the semiconductor layer 11 to further remove a portion of the semiconductor layer 11, causing the bottom 164B of the vertical portion 164 to protrude from the semiconductor layer 11. The bottom 164B of the vertical portion 164 protruding from the semiconductor layer 11 helps to reduce ohmic contact resistance and improve heat dissipation. In some embodiments, the thinned substrate 10 has a thickness in the range of 30 to 100 micrometers (μm).
[0059] Reference Figure 15The manufacturing method includes: forming an electrode structure 17 on a surface 11B of a semiconductor layer 11, wherein the electrode structure 17 has an opening O2 to define the location of a subsequently formed isolation structure 18. In some embodiments, the step of forming the electrode structure 17 includes: sputtering to form a metal material layer on the surface 11B of the semiconductor layer 11; forming a patterned photoresist layer on the metal material layer; etching the metal material layer with the patterned photoresist layer as a mask to form the electrode structure 17 with the opening O2; and removing the patterned photoresist layer. In some embodiments, the electrode structure 17 is subjected to a thermal annealing process (e.g., laser annealing) after forming the electrode structure 17 to form an ohmic contact with low resistance at the interface between the electrode structure 17 and the semiconductor layer 11. Since the vertical portions 164 of the cathodes (e.g., 16b and 16d) are exposed and protrude from the surface 11B of the semiconductor layer 11, the electrode structure 17 contacts the bottom 164B of the vertical portions 164 and conformally covers the portion of the vertical portions 164 protruding from the semiconductor layer 11. In some embodiments, electrode structure 17 contacts vertical portions 164 that protrude from the bottom surface and sidewalls of semiconductor layer 11. Openings O2 in electrode structure 17 define the location of molding material layers 19 subsequently formed between the dies; therefore, it can be understood that, from a top view, openings O2 surround each block (e.g., R1 and R2) of substrate 10. In some embodiments, openings O2 have a width W2. In some embodiments, the vertical projection of openings O2 is separated from the doped regions 121 surrounding blocks R1 and R2.
[0060] Reference Figure 16 The manufacturing method includes etching a substrate 10 exposed to the electrode structure 17 to form an opening O3 through the substrate 10. In some embodiments, the step of forming the opening O3 includes: forming a patterned photoresist layer on the electrode structure 17, wherein the patterned photoresist layer has an opening corresponding to and overlapping the opening O3; performing an etching process (e.g., wet etching or dry etching) on the substrate 10 using the patterned photoresist layer as a mask; and removing the patterned photoresist layer. In some embodiments, Figure 15 The step defines the patterned photoresist layer of electrode structure 17 and Figure 14 The patterned photoresist layer defining the opening O3 of the substrate 10 in the steps can be formed using the same photomask, so the patterned photoresist layers in the two steps can have the same pattern. In some embodiments, a wet etching process is used to form the opening O2 of the electrode structure 17. The wet etching process causes the sidewalls of the electrode structure 17 to shrink, so even if the same photomask is used, in Figure 16 In this step, the width W2 of opening O2 increases, and the increased width W2 of opening O2 becomes substantially larger than the width W3 of opening O3. In other embodiments, Figure 15 Steps and Figure 16The patterned photoresist layers in the steps are formed using different photomasks, but Figure 16 The patterned photoresist layer in the step has and Figure 15 The patterned photoresist layer in the step corresponds to a pattern with a smaller opening width, therefore the width W2 of opening O2 is... Figure 15 Steps and Figure 16 The steps will remain consistent, and the width W2 of opening O2 will be greater than the width W3 of opening O3. In some embodiments, dielectric layer 132 serves as an etch stop layer, so the etch process that removes part of the substrate 10 will stop at dielectric layer 132, and opening O3 will expose part of dielectric layer 132.
[0061] Reference Figure 17 The manufacturing method includes forming a molding material layer 19, wherein the molding material layer 19 fills openings O2 and O3 and covers the electrode structure 17. Openings O2 and O3 may be located in dicing regions, thus the molding material layer 19 fills the dicing regions, serving as electrical isolation between different blocks of the substrate 10. The molding material layer 19 also protects the electrode structure 17 from moisture and oxidation. Furthermore, since the substrate 10 has a very small thickness, which could lead to structural instability in the semiconductor device, the molding material layer 19 provides sufficient support to improve the durability of the semiconductor device. In some embodiments, the molding material layer 19 is formed by a coating or deposition process over the surface 11B of the semiconductor layer 11. In some embodiments, the molding material layer 19 contacts the dielectric layer 132. In some embodiments, the width of the molding material layer 19 at opening O2 is greater than the width at opening O3. In some embodiments, the molding material layer 19 has a flat surface 19B, away from the dielectric layer 132 and approximately parallel to the surface 11B of the semiconductor layer 11.
[0062] Reference Figures 18 to 19 The manufacturing method includes: taking Figure 17 The intermediate structure is peeled off from the carrier plate S1 and cut from above the surface 13A of the second epitaxial layer 13 to form a structure as shown in the figure. Figure 1 The semiconductor device 1 is shown. In some embodiments, it is flipped before the stripping step. Figure 17 The intermediate structure.
[0063] Semiconductor device 2 has a structure similar to that of semiconductor device 1, and can be transmitted via a similar means. Figures 5 to 19 The semiconductor device 2 is manufactured using the method shown. For demonstration purposes, the following description focuses on the steps that differ between the manufacturing methods of semiconductor device 2 and semiconductor device 1. Other similar steps can be found in the description above. Figures 5 to 19 Explanation.
[0064] Reference Figure 20 The manufacturing method of semiconductor device 2 includes: performing... Figures 5 to 12 The steps, and in Figure 12 After the steps, it forms as follows Figure 20 The first conductive material layer 161 shown is filled into multiple openings (e.g., O421, O422, O423, O424) of the second passivation layer 142 and the opening O1 of the substrate 10, and a second conductive material layer 162 is formed covering the first conductive material layer 161. The methods for forming the first conductive material layer 161 and the second conductive material layer 162 can be referred to... Figure 13 The explanation will not be repeated here. Figure 20 and Figure 13 The difference between the first conductive material layer 161 and the second conductive material layer 162 is that the cathode 16b and R2 located on the first block R1 are connected to the anode 16c located on the second block R2.
[0065] In order to form such Figure 2 , Figure 3 The structure shown, and as Figure 4 The circuit layout shown further includes a first conductive material layer 161 and a second conductive material layer 162 covering a portion of the substrate 10 located between the first block R1 and the second block R2. The first conductive material layer 161 and the second conductive material layer 162 together define the electrode structure 16, and according to the patterns of the first conductive material layer 161 and the second conductive material layer 162, they can be distinguished as multiple electrode pieces P1, P2, and P3. A portion of electrode piece P1 located on the first block R1 serves as the anode 16a; electrode piece P2 covers a portion of the first block R1 and a portion of the second block R2, wherein a portion of electrode piece P2 located on the first block R1 serves as the cathode 16b, and a portion of electrode piece P2 located on the second block R2 serves as the anode 16c; and a portion of electrode piece P3 located on the second block R2 serves as the cathode 16d. Although Figure 20 Electrode P4 is not shown, but a top view of semiconductor device 2 has been provided. Figure 2 The details are shown below and will not be repeated here.
[0066] Reference Figure 21 The manufacturing method of semiconductor device 2 includes: in Figure 20 After the steps, execute Figures 14 to 18 The steps involve cutting from above the top surface 12A of the silicon carbide substrate 10 to form a shape as shown in the figure. Figure 2 Semiconductor device 2 is shown. Figure 21 and Figure 19 The difference lies in the fact that, since semiconductor device 2 has four interconnected dies C1, C2, C3, and C4, it will not be cut on all the dicing paths during dicing; instead, it will be cut on a unit of four dies. (Refer to...) Figure 2 , Figure 3 , Figure 19The kerf region between the first block R1 and the second block R2 will not be sawn, the kerf region between the first block R1 and the third block R3 will not be sawn, the kerf region between the third block R3 and the fourth block R4 will not be sawn, and the kerf region between the second block R2 and the fourth block R4 will not be sawn. In other words, the molding material layer 19 of the semiconductor device 2 will fill the aforementioned regions, and the molding material layer 19 in these regions will contact the dielectric layer 132. Furthermore, compared to the semiconductor device 1, the first conductive material layer 161 and the second conductive material layer 162 of the semiconductor device 2 will further cover at least a portion of the molding material layer 19 in the aforementioned kerf regions (e.g., ...). Figure 2 (As shown).
[0067] The semiconductor device disclosed herein does not contain lead-containing electrical contact pads, complying with EU environmental regulations. Compared to existing processes, the semiconductor device disclosed herein has the following differences and advantages: First, the semiconductor device disclosed herein has multiple epitaxial layers 12 and 13 with varying concentrations. Unlike existing processes that achieve concentration gradients through diffusion or ion implantation in a single epitaxial layer, the use of multiple epitaxial layers 12 and 13 allows for a larger concentration difference within a relatively small thickness. Furthermore, the semiconductor device disclosed herein uses polyimide as a protective layer on the front (or top) surface of the semiconductor device, thus eliminating the need for encapsulation materials (or molding materials). This not only facilitates heat dissipation but also improves forward instantaneous current. Additionally, the semiconductor device disclosed herein has a cathode structure protruding from the bottom surface of the substrate 10, which not only reduces ohmic contact resistance but also further enhances the heat dissipation capability of the semiconductor device. Based on the above structural features, the semiconductor device disclosed herein further achieves the purpose of a high-voltage device (e.g., a voltage higher than 650 ft, or between 650 and 1500 ft) with a thinned substrate 10 (thickness less than or equal to 100 micrometers).
[0068] In this document, spatial relative terms such as “below,” “under,” “lower,” “above,” “upper,” “left,” and “right” may be used for ease of description to describe the relationship between one component or feature as shown in the accompanying drawings and one or more other components or features. In addition to the orientation depicted in the accompanying drawings, the spatial relative terms are also intended to cover different orientations of the device during use or operation. The device may be oriented in other ways (rotated 90 degrees or in other orientations), and the spatial relative descriptive terms used herein may be interpreted accordingly. It should be understood that when a component is referred to as “connected to” or “coupled to” another component, it may be directly connected to or coupled to the other component, or there may be an intermediate component present.
[0069] As used herein, the terms “approximately,” “substantially,” “essentially,” and “about” are used to describe and explain small variations. When used in conjunction with an event or situation, the terms may refer to instances where the event or situation occurs precisely or instances where the event or situation is close to occurring. As used herein with respect to a given value or range, the term “about” generally means within ±10%, ±5%, ±1%, or ±0.5% of the given value or range. A range may be expressed herein as from one endpoint to another or between two endpoints. All ranges disclosed herein include endpoints unless otherwise specified. The term “substantially coplanar” may mean that the positional difference between two surfaces located along the same plane is within a few micrometers (μm), such as within 10 μm, 5 μm, 1 μm, or 0.5 μm when located along the same plane. When a numerical value or characteristic is referred to as “substantially” the same, the term may refer to a value within ±10%, ±5%, ±1%, or ±0.5% of the average of said values.
[0070] The foregoing has summarized the features of several embodiments and detailed aspects of this disclosure. The embodiments described in this disclosure can readily serve as the basis for designing or modifying other processes and structures to achieve the same or similar purposes and / or realize the same or similar advantages of the embodiments described herein. Such equivalent constructions do not depart from the spirit and scope of this disclosure, and various changes, substitutions, and modifications can be made without departing from the spirit and scope of this disclosure.
Claims
1. A semiconductor device, characterized in that, include: A first epitaxial layer having a first surface and a second surface that are opposite to each other; The second epitaxial layer is disposed on the first surface of the first epitaxial layer and has a third surface away from the first epitaxial layer; A first rectifier structure is disposed on the third surface of the second epitaxial layer; A first electrode structure is disposed on the third surface of the second epitaxial layer, the first electrode structure comprising: A first electrode plate is located on and electrically connected to the first rectifier structure; and The second electrode sheet has a first portion located on the third surface of the second epitaxial layer, and a second portion extending from the third surface toward the second surface of the first epitaxial layer, wherein the second portion penetrates the first epitaxial layer and the second epitaxial layer and protrudes from the second surface of the first epitaxial layer; and A second electrode structure is disposed on the second surface of the first epitaxial layer, wherein the second electrode structure contacts the bottom and part of the sidewall of the second portion of the second electrode sheet protruding from the second surface.
2. The semiconductor device of claim 1, wherein the first epitaxial layer and the second epitaxial layer have approximately the same thickness.
3. The semiconductor device according to claim 1, wherein the thickness of the first epitaxial layer is less than the thickness of the second epitaxial layer.
4. The semiconductor device according to claim 1, wherein the first epitaxial layer and the second epitaxial layer have the same conductivity type, and the doping concentration of the second epitaxial layer is less than the doping concentration of the first epitaxial layer.
5. The semiconductor device according to claim 1, further comprising: A semiconductor layer is disposed on the second surface of the first epitaxial layer, wherein the second portion of the second electrode sheet penetrates the semiconductor layer and protrudes from the fourth surface of the semiconductor layer away from the first epitaxial layer.
6. The semiconductor device of claim 5, wherein the second electrode structure extends along the fourth surface of the semiconductor layer and covers the second portion of the second electrode sheet protruding from the fourth surface of the semiconductor layer.
7. The semiconductor device according to claim 1, further comprising: A first dielectric layer is disposed between the first rectifier structure and a portion of the first electrode structure, and the... The material of the first dielectric layer includes polyimide.
8. The semiconductor device of claim 7, wherein, viewed from a top perspective view, the first dielectric layer surrounds the second portion of the second electrode sheet.
9. The semiconductor device according to claim 7, further comprising: A second dielectric layer is disposed between the first rectifier structure and the first dielectric layer, and the material of the first dielectric layer includes silicon nitride, silicon oxide, or a combination thereof.
10. The semiconductor device of claim 9, further comprising: A third dielectric layer is disposed between the second dielectric layer and the third surface of the second epitaxial layer, and the third dielectric layer has a dielectric material different from that of the second dielectric layer.
11. The semiconductor device of claim 1, further comprising: A molding material layer covers the second electrode structure and surrounds the sidewalls of the first epitaxial layer and the second epitaxial layer.
12. The semiconductor device according to claim 1, further comprising: The substrate includes at least a first epitaxial layer and a second epitaxial layer stacked in a vertical direction, wherein the third surface of the second epitaxial layer is the top surface of the substrate, and the second electrode structure is disposed on the bottom surface of the substrate; A molding material layer covers the second electrode structure and extends from the bottom surface of the substrate to the top surface and penetrates the substrate, wherein the molding material layer divides the substrate into at least a first block and a second block that are adjacent to each other in a horizontal direction; as well as A second rectification structure is disposed on the top surface of the substrate, wherein the first rectification structure is located on the first block, the second rectification structure is located on the second block, and the first portion of the second electrode sheet of the first electrode structure is electrically connected to the second rectification structure.
13. The semiconductor device of claim 12, wherein the first portion of the second electrode sheet is located on the third surface of the second epitaxial layer and extends horizontally and covers the molding material layer located between the first block and the second block.
14. The semiconductor device of claim 12, further comprising: The third electrode has a third portion located on the top surface of the substrate and a fourth portion extending from the third surface toward the second surface of the first epitaxial layer and through the substrate, wherein the fourth portion protrudes from the bottom surface of the substrate.
15. A method for manufacturing a semiconductor power device, characterized in that, include: A rectifying structure is formed on a first surface of a substrate, wherein the substrate includes a first epitaxial layer and a second epitaxial layer stacked in a vertical direction, the second epitaxial layer being adjacent to the first surface and the first epitaxial layer being away from the first surface; A first dielectric layer is formed to cover the substrate and the rectifier structure, wherein the first dielectric layer has a plurality of openings that expose portions of the rectifier structure and portions of the substrate, respectively. Remove the portion of the substrate exposed by the first dielectric layer to form a first opening, wherein the depth of the first opening is greater than the thickness of the first epitaxial layer and the second epitaxial layer; A first electrode structure is formed on the first surface of the substrate and in the first opening; Reduce the thickness of the substrate so that the bottom of the first electrode structure protrudes from the substrate; A second electrode structure is formed on a second surface of the substrate relative to the first surface, wherein the second electrode structure covers the bottom of the first electrode structure; as well as A molding material layer is formed to surround the second electrode structure and the substrate.
16. The manufacturing method of claim 15, wherein the second electrode structure exposes a portion of the second surface of the substrate, and the manufacturing method further comprises: The portion of the substrate exposed to the second electrode structure is removed from the second surface of the substrate to form a second opening, wherein the second opening penetrates the substrate.
17. The manufacturing method of claim 16, wherein the second opening is located in the cutting channel, and the molding material layer is formed in the second opening.
18. The manufacturing method according to claim 16, further comprising: Before forming the rectifier structure, an etch stop layer is formed on the first surface of the substrate.
19. The manufacturing method of claim 18, wherein the second opening overlaps the etch stop layer in a vertical direction, and the second opening stops at the etch stop layer.
20. The manufacturing method of claim 15, wherein the substrate further comprises a semiconductor layer located on the first epitaxial layer relative to the second epitaxial layer, and after reducing the thickness of the substrate, the bottom of the first electrode structure protrudes from the semiconductor layer.
21. The manufacturing method of claim 15, wherein the material of the first dielectric layer comprises polyimide, and the manufacturing method further comprises: Before forming the first dielectric layer, a second dielectric layer is formed to cover the substrate and the rectifier structure, wherein the second dielectric layer has a plurality of openings that overlap with the plurality of openings of the first dielectric layer.
22. The manufacturing method according to claim 21, wherein the material of the second dielectric layer comprises a nitride, an oxide, or a combination thereof.
23. The manufacturing method according to claim 15, wherein the first epitaxial layer and the second epitaxial layer comprise polycrystalline silicon or monocrystalline silicon, the first epitaxial layer and the second epitaxial layer have the same conductivity, and the doping concentration of the first epitaxial layer is greater than the doping concentration of the second epitaxial layer.
24. The manufacturing method according to claim 15, wherein forming the first electrode structure comprises: Electroplating forms a copper-containing metal layer on the first surface of the substrate and in the first opening; as well as Electroplating forms a tin-containing metal layer on the copper-containing metal layer.