A semiconductor device and its fabrication method

By combining thermal oxidation and etching processes, the reliability problem caused by silicon sharp corners in semiconductor devices was solved, the uniformity and integrity of the gate oxide layer were achieved, the reliability of the device was improved and the production cost was reduced.

CN123076183APending Publication Date: 2026-11-10SIEN (QINGDAO) INTEGRATED CIRCUITS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611594169.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-15
Publication Date
2026-11-10

AI Technical Summary

Technical Problem

Semiconductor devices are prone to forming silicon sharp corner structures at the edges of the active region and the corners of the trench, which can lead to problems such as local thinning of the gate oxide layer, local reduction of the breakdown electric field, and electric field concentration, thus affecting the reliability of the device.

Method used

By combining thermal oxidation and etching processes, a sacrificial layer is formed to cover the silicon surface and consume silicon material to form protruding sharp corners. These corners are then etched into rounded corners, increasing the radius of curvature at the edge of the silicon surface and avoiding stress concentration and local electric field distortion.

Benefits of technology

It improves the uniformity and integrity of the gate oxide layer thickness in semiconductor devices, enhances device reliability, and reduces production and modification costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123076183A_ABST
    Figure CN123076183A_ABST
Patent Text Reader

Abstract

This application discloses a semiconductor device and its fabrication method, applicable to the field of semiconductor devices. The method involves: first, providing an initial structure with an exposed silicon surface and initial sharp corners at the edges of the silicon surface; then, oxidizing the silicon surface using an oxidation process to form a sacrificial layer covering the silicon surface, and consuming silicon material to form raised sharp corners based on the initial sharp corners; the radius of curvature of the raised sharp corners is smaller than that of the initial sharp corners; finally, performing an etching process to etch the sacrificial layer down to the exposed raised sharp corners at the edges of the silicon surface, and then continuing etching to round the raised sharp corners. This process rounds the raised sharp corners at the edges of the silicon surface formed by the difference in oxidation consumption, increasing the radius of curvature at the edges of the silicon surface, delaying stress concentration at the sharp corners, and enabling the subsequently grown gate oxide layer to maintain excellent thickness uniformity and integrity, thereby effectively improving the reliability of the semiconductor device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of semiconductor device technology, and in particular to a semiconductor device and a method for fabricating the same. Background Technology

[0002] With the continuous development of semiconductor devices, the uniformity and integrity of the gate oxide layer directly determine the stability of the threshold voltage, the magnitude of the leakage current, and the reliability. However, after processes such as shallow trench isolation and active region definition, silicon sharp corner structures are easily formed at the edges of the active region and the corners of the trenches on the surface of the silicon substrate.

[0003] Currently, when growing a gate oxide layer on the surface of the active region, stress concentration and uneven oxidation rates at the sharp corners of the active region result in relatively slow silicon consumption at these locations, inducing the formation of silicon protrusions. Ultimately, this leads to problems such as localized thinning of the gate oxide layer, localized reduction in the breakdown electric field, and electric field concentration, affecting the reliability of semiconductor devices.

[0004] Therefore, improving the reliability of semiconductor devices has become an urgent problem to be solved. Summary of the Invention

[0005] To address the aforementioned issues, this application provides a semiconductor device and its fabrication method, which can improve the reliability of the semiconductor device.

[0006] The embodiments of this application disclose the following technical solutions: In a first aspect, embodiments of this application provide a method for fabricating a semiconductor device, the method comprising: An initial structure is provided; the initial structure has an exposed silicon surface with initial sharp corners at the edges; The silicon surface is oxidized using an oxidation process to form a sacrificial layer covering the silicon surface, and the silicon material is consumed to form a protruding sharp corner based on the initial sharp corner; the radius of curvature of the protruding sharp corner is smaller than the radius of curvature of the initial sharp corner; An etching process is performed to etch the sacrificial layer until the protruding sharp corners of the silicon surface edge are exposed, and then etching continues to etch the protruding sharp corners into rounded corners.

[0007] Optionally, the top of the rounded corner is lower than the top of the silicon surface.

[0008] Optionally, the radius of curvature of the fillet is selected from 30-50 nm.

[0009] Optionally, the etching process is a reactive ion etching process.

[0010] Optionally, the gas introduced into the reactive ion etching process includes: A mixture of sulfur hexafluoride and oxygen.

[0011] Optionally, the etching process, which involves etching the sacrificial layer to expose the protruding sharp corners at the edge of the silicon surface, and then continuing etching to round off the protruding sharp corners, includes: An etching process is performed to etch the sacrificial layer down to the protruding sharp corners of the exposed silicon surface edge, resulting in a residual sacrificial layer; The residual sacrificial layer is passivated by the etching process to form a passivation layer, and the protruding sharp corners are etched into rounded corners.

[0012] Optionally, after passivating the residual sacrificial layer to form a passivation layer through the etching process and etching the protruding sharp corners into rounded corners, the method further includes: The passivation layer is removed by wet cleaning to obtain the target silicon surface.

[0013] Optionally, the silicon surface is an active region surface, and after removing the passivation layer using wet cleaning to obtain the target silicon surface, the process further includes: The target silicon surface is oxidized to form a gate oxide layer covering the active region surface.

[0014] Optionally, the oxidation process is selected from any one of wet oxidation, dry oxygen oxidation, chlorine-containing wet oxidation, or in-situ steam growth oxidation.

[0015] Secondly, embodiments of this application provide a semiconductor device, the device comprising: A silicon surface with rounded edges; the rounded edges are obtained by etching raised sharp corners at the edges of the silicon surface.

[0016] Compared with the prior art, this application has the following beneficial effects: This application provides a method for fabricating a semiconductor device. In this method, firstly, an initial structure is provided; the initial structure has an exposed silicon surface with initial sharp corners at the edges; then, an oxidation process is used to oxidize the silicon surface to form a covering. A sacrificial layer is formed on the silicon surface, and silicon material is consumed to form a raised tip based on the initial tip; the radius of curvature of the raised tip is smaller than the radius of curvature of the initial tip; finally, an etching process is performed to etch the sacrificial layer to expose the raised tip at the edge of the silicon surface, and then etching continues to etch the raised tip into a rounded corner.

[0017] Therefore, by combining thermal oxidation and etching processes, the sharp corners of silicon protrusions formed by differences in oxidation consumption at the silicon surface edge are etched into rounded corners, increasing the radius of curvature of the silicon surface edge and delaying stress concentration at the sharp corners. Furthermore, since the rounded corner structure no longer causes local electric field distortion, the subsequently grown gate oxide layer can maintain excellent thickness uniformity and integrity, thereby effectively improving the reliability of semiconductor devices.

[0018] Furthermore, this solution does not require complex modifications to existing semiconductor manufacturing equipment, and the process steps are simple and efficient, enabling the reliability of semiconductor devices to be improved at a lower production cost. Attached Figure Description

[0019] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0020] Figure 1 A flowchart illustrating a method for fabricating a semiconductor device, as provided in an embodiment of this application; Figure 2 This is a schematic diagram of the structure of a semiconductor device provided in an embodiment of this application; Figure 3 A schematic diagram of the fabrication process of a semiconductor device provided in an embodiment of this application; Figure 4 This is a partially enlarged schematic diagram of the silicon surface during a semiconductor device fabrication process provided in this application embodiment. Detailed Implementation

[0021] The semiconductor device and its fabrication method provided in this application can be used in the field of semiconductor devices. The above is only an example and does not limit the application field of the semiconductor device and its fabrication method provided in this application.

[0022] The terms "first," "second," "third," and "fourth," etc., used in this application specification, claims, and drawings are used to distinguish different objects, not to limit a specific order.

[0023] In the embodiments of this application, the terms "as an example" or "for example" are used to indicate that they are examples, illustrations, or explanations. Any embodiment or design that is described as "as an example" or "for example" in the embodiments of this application should not be construed as being more preferred or advantageous than other embodiments or design options. Specifically, the use of terms such as "as an example" or "for example" is intended to present the relevant concepts in a specific manner.

[0024] The terminology used in the implementation section of this application is for the purpose of explaining specific embodiments of this application only, and is not intended to limit this application.

[0025] As mentioned earlier, after shallow trench isolation and active region definition processes are performed on the surface of the silicon substrate, silicon sharp corner structures are easily formed at the edges of the active region and the corners of the trench.

[0026] However, further research by the inventors revealed that when a gate oxide layer is grown on the surface of the active region, stress concentration and uneven oxidation rates at the sharp corners of the active region result in relatively slow silicon consumption at these locations, inducing the formation of silicon protrusions. Ultimately, this leads to defects in the gate oxide layer such as localized thinning, reduced localized breakdown electric field, and electric field concentration, affecting the reliability of the semiconductor device.

[0027] Currently, the inventors know of several methods to improve silicon bumps, including directly depositing gate oxide layers using non-thermal oxidation methods such as chemical vapor deposition (CVD), passively reducing the overall thickness of the thermal oxide film to alleviate the local electric field intensity at the bumps, and modifying or customizing existing semiconductor manufacturing equipment to introduce dedicated rounded corner etching or special planarization modules. However, the inventors have found that these solutions generally have significant limitations and defects in practical applications.

[0028] Specifically, compared to silicon dioxide thin films formed by high-temperature thermal growth, the gate oxide layer deposited directly by non-thermal oxidation methods such as chemical vapor deposition often has poor compactness and higher interface state density. It is difficult to form a high-quality interface with atomically flat surface and few defects on the active region surface, which leads to a decrease in carrier mobility, threshold voltage drift and degradation of the overall electrical performance of the device.

[0029] Passively reducing the overall thickness of the thermal oxide film to alleviate the local electric field intensity at the protruding sharp corners often comes at the cost of sacrificing the overall physical thickness of the gate oxide layer. This not only leads to an increase in gate leakage current (e.g., enhanced carriers directly induce tunneling effects), but also fails to fundamentally change the geometry of the sharp corners at the edge of the active region, and still cannot eliminate device reliability failures caused by stress concentration.

[0030] Introducing machine modification solutions such as dedicated rounded corner etching or special planarization processing modules usually involves extremely high equipment R&D and capital expenditures, as well as long production line downtime and debugging cycles, and lacks good compatibility with existing large-scale mature semiconductor device manufacturing production lines.

[0031] In view of the above, embodiments of this application provide a method for fabricating a semiconductor device. In this method, firstly, an initial structure is provided; the initial structure has an exposed silicon surface and an initial sharp corner at the edge of the silicon surface; then, an oxidation process is used to oxidize the silicon surface to form a sacrificial layer covering the silicon surface, and silicon material is consumed to form a raised sharp corner based on the initial sharp corner; the radius of curvature of the raised sharp corner is smaller than the radius of curvature of the initial sharp corner; finally, an etching process is performed to etch the sacrificial layer to expose the raised sharp corner at the edge of the silicon surface, and then etching continues to etch the raised sharp corner into a rounded corner.

[0032] Therefore, by combining thermal oxidation and etching processes, the sharp corners of silicon protrusions formed by differences in oxidation consumption at the silicon surface edge are etched into rounded corners, increasing the radius of curvature of the silicon surface edge and delaying stress concentration at the sharp corners. Furthermore, since the rounded corner structure no longer causes local electric field distortion, the subsequently grown gate oxide layer can maintain excellent thickness uniformity and integrity, thereby effectively improving the reliability of semiconductor devices.

[0033] Furthermore, this solution does not require complex modifications to existing semiconductor manufacturing equipment, and the process steps are simple and efficient, enabling the reliability of semiconductor devices to be improved at a lower production cost.

[0034] To enable those skilled in the art to better understand the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present application, and not all embodiments. Based on the embodiments in the present application, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present application.

[0035] See Figure 1 The figure is a flowchart of a semiconductor device fabrication method provided in an embodiment of this application. The method includes: S101: Provides the initial structure.

[0036] Specifically, the initial structure has an exposed silicon surface 300, and the edges of the silicon surface have initial sharp corners 201.

[0037] The initial sharp corner 201 of the silicon surface edge is typically formed at the edge of the active region or at the corner of a trench. This embodiment of the application takes the initial sharp corner 201 located at the edge of the active region as an example, and the active region surface described in this embodiment is the silicon surface. For example, see... Figure 2 The initial structure can be prepared using the following process: First, a pad oxide layer and a silicon nitride mask layer are sequentially formed on the surface of the silicon substrate 100. Then, shallow isolation trenches are etched in the silicon substrate using photolithography and anisotropic dry etching processes. Next, the shallow isolation trenches are filled with an insulating dielectric and the surface is planarized using a chemical mechanical planarization (CMP) process to form a shallow trench isolation structure (STI) 200. Finally, the mask layer is selectively removed to fully expose and define the active region 300 surrounded by the shallow trench isolation structure 200.

[0038] like Figure 3 (a) and Figure 4 As shown in (a), Figure 4 (a) is Figure 3 In the enlarged schematic diagram of the silicon surface in (a), it can be seen that after the silicon substrate 100 is manufactured by the shallow trench isolation structure 200 and the active region 300, microscopic initial sharp corner 201 structures are often formed in local areas such as the edge of the active region 300 and the corner of the shallow trench isolation structure 200. The local radius of curvature at the initial sharp corner 201 is usually less than 5nm, exhibiting a high degree of morphological sharpness.

[0039] S102: The silicon surface is oxidized using an oxidation process to form a sacrificial layer 400 covering the silicon surface, and silicon material is consumed to form a raised sharp corner 202 based on the initial sharp corner 201.

[0040] Specifically, the silicon surface mentioned above is the silicon surface of the active region 300, and the radius of curvature of the protruding sharp corner 202 is smaller than the radius of curvature of the initial sharp corner 201.

[0041] As an example, see Figure 3 (b) and Figure 4 (b) Figure 4 (b) is Figure 3 (b) A magnified schematic diagram of a portion of the silicon surface. The active region 300 silicon surface is oxidized using an oxidation process. During this process, oxidizing agents such as oxygen or water vapor diffuse into the interior of the active region 300 silicon surface, further reacting chemically with the silicon to form an oxide film covering the active region 300 silicon surface, i.e., the sacrificial layer 400. Figure 4 As can be clearly seen in the schematic diagram in (b), the thickness of the sacrificial layer 400 film located at the protruding sharp corner is less than the thickness of the sacrificial layer 400 film located in the flat region of the active region 300.

[0042] Specifically, since there is a local curvature abrupt change in the geometry at the initial sharp corner 201, when the oxidation reaction proceeds, the sharp corner structure will generate severe stress concentration, thereby inhibiting the diffusion of the oxidant and the local oxidation rate, resulting in relatively slow silicon consumption at this location. Consequently, the original initial sharp corner 201 further evolves into a more prominent convex sharp corner 202. In addition, since the silicon consumption at the convex sharp corner 202 is relatively slow, the thickness of the sacrificial layer 400 film at the convex sharp corner 202 is less than the thickness of the sacrificial layer 400 film in the flat region of the active region 300.

[0043] Through microscopic morphology characterization, the inventors discovered that the sharpness of the raised corners 202 formed during the oxidation process of the sacrificial layer 400 was further intensified, resulting in a significantly smaller radius of curvature for the raised corners 202 compared to the initial corners 201. This indicates that the sacrificial layer 400 is not merely a transitional sacrificial oxide film; its growth process further intensifies potential corner defects, forming raised corners 202 with even more severe morphology, thus facilitating subsequent rounding treatment through selective etching.

[0044] Preferably, the oxidation process for growing the sacrificial layer 400 can be selected from any one of wet oxidation, dry oxidation, chlorine-containing wet oxidation, or in-situ steam generation (ISSG). Chlorine-containing wet oxidation typically involves introducing chlorine-containing compounds such as hydrogen chloride (HCl) or dichloroethylene (DCE) into an oxidizing atmosphere.

[0045] S103: Perform an etching process, etching the sacrificial layer 400 to the protruding sharp corner 202 at the edge of the exposed silicon surface, and then continue etching to etch the protruding sharp corner 202 into a rounded corner 203.

[0046] For example, the etching process can employ an etching process that is highly selective for silicon materials, wherein the etching rate of the active region 300 surface is significantly higher than the etching rate of the sacrificial layer 400 material.

[0047] As a specific embodiment, the sacrificial layer 400 is made of silicon dioxide, and the etching process can be reactive ion etching (RIE). Furthermore, during this RIE process, the introduced reactive etching gas includes a mixture of sulfur hexafluoride (SF6) and oxygen (O2). After etching, the desired result is obtained as shown below. Figure 3 The structure shown in (c) is as follows.

[0048] Specifically, see Figure 4 (c) and Figure 4 In (d), where, Figure 4 (c) and Figure 4 (d) indicates Figure 3 The morphological changes of the silicon surface during the etching process are shown in (c). Since the reactive gas contains a small amount of oxygen, the oxygen diffuses to the surface of the active region 300 during the etching process, slowly oxidizing the silicon material. The oxidation principle is the same as that in step S102 above. The silicon consumption rate at the protruding sharp corner 202 is less than that in the flat area. Furthermore, given that the reactive gas contains a large amount of corrosive sulfur hexafluoride, relying on its highly efficient chemical corrosiveness, the overall etching rate is greater than the oxidation rate during the etching process.

[0049] Meanwhile, the reactant gas contains a large amount of sulfur hexafluoride, which, due to its strong chemical corrosive properties, results in an overall etching rate significantly higher than the oxidation rate. Because the sacrificial layer 400 at the protruding corner 202 is thinner than that in the flat region, it will be etched away first during the etching process, exposing the protruding corner 202 at the edge of the active region 300 surface. Meanwhile, the sacrificial layer 400 in the flat region has not yet been completely etched away, retaining a residual oxide film, and its silicon surface structure is as follows: Figure 4 As shown in (c).

[0050] Then, the etching process continues. During the etching process, on the one hand, the residual sacrificial layer 400 and the oxide layer generated by oxidation together form a passivation layer 500 in the flat area of ​​the active region 300, which effectively prevents the etching gas from excessively eroding the silicon material in the main flat area of ​​the active region 300. On the other hand, since the protruding corner 202 has the characteristics of being exposed on multiple sides such as the top and sides in spatial geometry, compared with the flat surface that is only bombarded by ions from directly above, the protruding corner 202 has a larger effective reaction area, which allows sulfur hexafluoride, which has a strong silicon corrosion gas, to produce efficient and rapid rounding treatment on the exposed protruding corner 202, etching the protruding corner 202 into a rounded corner 203, resulting in... Figure 4 The silicon surface structure shown in (d) is shown in the middle.

[0051] Therefore, through the synergistic combination of thermal oxidation and etching processes, this application successfully etched the protruding sharp corner 202 of the active region 300 edge, which deteriorated due to differences in oxidation consumption rates, into a rounded corner 203 structure. The top of this rounded corner 203 is lower than the top of the main body of the active region 300 surface, resulting in a gently sloping, rounded transition at the edge of the active region 300 surface. This morphology design optimizes the radius of curvature of the silicon surface edge of the active region 300 to the ideal range of 30-50 nm, improving the geometric abrupt changes at the edge of the active region 300 silicon surface and delaying stress concentration at the protruding sharp corner 202. Furthermore, because the rounded corner 203 structure improves the local electric field distortion and enhancement effect caused by the sharp morphology, the subsequently grown high-quality gate oxide layer 600 can achieve excellent thickness uniformity and interface integrity, effectively eliminating fatal defects such as local thinning, electric field concentration, and early breakdown, thereby effectively improving the reliability of the semiconductor device.

[0052] Furthermore, this solution requires no complex hardware modifications or custom development to existing semiconductor manufacturing equipment. It can directly achieve the rounding of the protruding sharp corner 202 using mature production line equipment and standard process operations. The entire process flow is clear and the steps are simple. While improving the reliability of semiconductor devices, it reduces manufacturing and modification costs, and has promising prospects for commercial promotion and mass production applications.

[0053] As an example, see Figure 3 (d) and Figure 4 In (e), where, Figure 4 (e) is Figure 3 (d) A partially enlarged schematic diagram of the silicon surface. After completing the rounding 203 etching of the protruding sharp corner 202, the method further includes: using a wet cleaning process to thoroughly remove the passivation layer 500 on the silicon surface of the active region 300, thereby obtaining a clean target silicon surface, i.e., the target active region 301. Specifically, a cleaning solution containing dilute hydrofluoric acid (DHF) can be used to wet-strip the passivation layer to obtain the target active region 301.

[0054] On the one hand, hydrofluoric acid can undergo a highly selective chemical dissolution reaction with the silicon dioxide material of the passivation layer 500. Due to the relatively low acid concentration of dilute hydrofluoric acid, the passivation layer 500 can be gradually and effectively peeled off at a gentle and controllable rate, thereby exposing the clean target active region 301. At the same time, since single crystal silicon exhibits high chemical inertness to hydrofluoric acid, the cleaning process maintains excellent selectivity for the silicon body at the edge of the active region 300 surface that has undergone rounding treatment, effectively reducing the damage to the morphology of the rounded corner 203 at the edge of the active region 300 surface during wet cleaning.

[0055] On the other hand, the wet cleaning process can also relatively uniformly remove microparticles, fluorocarbon polymer byproducts, and various trace contaminants remaining on the device surface during the etching stage. This gentle surface pretreatment not only effectively restores the intrinsic state and chemical activity of the active region surface, but also provides a target active region 301 surface with high flatness, few contaminants, and low interface state density for the thermal growth of the high-quality gate oxide layer 600 in subsequent processes. This plays a positive role in improving the integrity of the gate oxide layer 600, reducing leakage risk, and improving the reliability of semiconductor devices.

[0056] For example, see Figure 3 (e) and Figure 4 In (f), where Figure 4 (f) is Figure 3(e) A partially enlarged schematic diagram of the silicon surface. A thermal oxidation process can be used to oxidize the surface of the target active region 301 to form a high-quality gate oxide layer 600 on the surface of the target active region 301. Specifically, the thermal oxidation process typically introduces an oxidant (such as oxygen molecules or water vapor) at a high temperature. These oxidants diffuse inward and penetrate the already formed oxide layer, transporting them to the surface of the active region silicon 301. Subsequently, at the interface between silicon and silicon dioxide, the oxidant reacts chemically with the single-crystal silicon of the target active region, such as Si + 2H₂O → SiO₂ + 2H₂, or Si + O₂ → SiO₂, thereby continuously consuming the silicon material of the target active region and pushing it into the interior of the active region 300 to continuously grow a silicon dioxide film, forming the gate oxide layer 600 covering the surface of the target active region 301.

[0057] To adapt to different device designs and performance requirements, the thermal oxidation process used to form the gate oxide layer 600 on the surface of the target active region 301 can be flexibly selected. For example, the thermal oxidation process can be selected from at least one of wet oxidation, in-situ steam generation (ISSG), rapid thermal oxidation (RTO), and dry oxidation. These diverse thermal oxidation processes can provide different oxygen partial pressures, reaction kinetic rates, and thermal treatment environments, thereby controlling the thickness distribution of the gate oxide layer 600 and effectively improving its interface quality, ensuring that the gate oxide layer 600 has good electrical performance and reliability, and thus improving the reliability of semiconductor devices.

[0058] It should be noted that the various embodiments in this specification are described in a progressive manner, and the same or similar parts between the various embodiments can be referred to mutually. Each embodiment focuses on describing the differences from other embodiments. The embodiments described above are merely illustrative, and some or all of the features can be selected to achieve the purpose of this embodiment according to actual needs. Those skilled in the art can understand and implement this without creative effort.

[0059] The above description is merely one specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.

Claims

1. A method for fabricating a semiconductor device, characterized in that, The method includes: An initial structure is provided; the initial structure has an exposed silicon surface with initial sharp corners at the edges; The silicon surface is oxidized using an oxidation process to form a sacrificial layer covering the silicon surface, and the silicon material is consumed to form a protruding sharp corner based on the initial sharp corner; the radius of curvature of the protruding sharp corner is smaller than the radius of curvature of the initial sharp corner; An etching process is performed to etch the sacrificial layer until the protruding sharp corners of the silicon surface edge are exposed, and then etching continues to etch the protruding sharp corners into rounded corners.

2. The method according to claim 1, characterized in that, The top of the rounded corner is lower than the top of the silicon surface.

3. The method according to claim 1, characterized in that, The radius of curvature of the fillet is selected from 30-50 nm.

4. The method according to claim 1, characterized in that, The etching process is a reactive ion etching process.

5. The method according to claim 4, characterized in that, The gases introduced into the reactive ion etching process include: A mixture of sulfur hexafluoride and oxygen.

6. The method according to claim 1, characterized in that, The etching process, which involves etching the sacrificial layer to expose the protruding sharp corners at the edge of the silicon surface, and then continuing etching to round off the protruding sharp corners, includes: An etching process is performed to etch the sacrificial layer down to the protruding sharp corners of the exposed silicon surface edge, resulting in a residual sacrificial layer; The residual sacrificial layer is passivated by the etching process to form a passivation layer, and the protruding sharp corners are etched into rounded corners.

7. The method according to claim 6, characterized in that, After passivating the residual sacrificial layer through the etching process to form a passivation layer, and etching the protruding sharp corners into rounded corners, the method further includes: The passivation layer is removed by wet cleaning to obtain the target silicon surface.

8. The method according to claim 7, characterized in that, The silicon surface is an active region surface. After removing the passivation layer using wet cleaning to obtain the target silicon surface, the method further includes: The target silicon surface is oxidized to form a gate oxide layer covering the active region surface.

9. The method according to claim 1, characterized in that, The oxidation process is selected from any one of wet oxidation, dry oxygen oxidation, chlorine-containing wet oxidation, or in-situ steam growth oxidation.

10. A semiconductor device, characterized in that, The device is prepared by the method for preparing a semiconductor device according to any one of claims 1 to 9, and the device comprises: A silicon surface with rounded edges; the rounded edges are obtained by etching raised sharp corners at the edges of the silicon surface.