Semiconductor devices and methods for detecting bonding defects in semiconductor devices
By designing specific structures and voltage measurement methods in semiconductor devices, the problem of detecting bonding interface defects has been solved, enabling early identification and prevention of bonding defects and ensuring the normal operation of the devices.
Patent Information
- Application Number
- CN202610269976.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-07
- Filing Date
- 2026-03-06
- Publication Date
- 2026-11-10
AI Technical Summary
In the bonding process of semiconductor devices, existing technologies have difficulty effectively detecting defects at the bonding interface, which may cause the device to malfunction.
A semiconductor device structure is designed, including first and second bonding pads, first and second test pads, and probe pads. Bonding defects are detected by applying different voltages to the probe pads and measuring the current values, and calculating the sheet resistance.
It can detect defects at the bonding interface at an early stage, ensuring normal electrical connection of semiconductor devices and improving device reliability and performance.
Smart Images

Figure CN123076217A_ABST
Abstract
Description
Cross-reference to related applications
[0001] This patent document claims priority to Korean Patent Application No. 10-2025-0058865, filed on May 7, 2025, the disclosure of which is incorporated herein by reference in its entirety. Technical Field
[0002] Embodiments of this disclosure relate to semiconductor devices and methods for detecting bonding defects in semiconductor devices. Background Technology
[0003] As semiconductor devices become increasingly integrated, technologies for stacking semiconductor devices vertically are constantly evolving. For example, integrated circuits can be formed on two separate wafers, and these two wafers can be bonded together using wafer bonding technology. When manufacturing semiconductor devices using wafer bonding technology, preventing defects at the bonding interface is crucial. Summary of the Invention
[0004] The purpose of this disclosure is not limited to the content described herein, and other unmentioned purposes will be clearly understood by those skilled in the art through the following description.
[0005] Embodiments of this disclosure may provide a semiconductor device and a method for detecting bonding defects in the semiconductor device, capable of detecting defects generated at the bonding interface.
[0006] Embodiments of this disclosure may provide a semiconductor device, comprising: a first bonding pad disposed on a substrate; a second bonding pad bonded to the first bonding pad; a first test pad located on the same layer as the second bonding pad, and including a first pad portion, a second pad portion spaced apart from the first pad portion, and a first connection portion connecting the first pad portion and the second pad portion; a first probe pad connected to the first pad portion via a first test contact disposed on the first pad portion; and a second probe pad connected to the second pad portion via a second test contact disposed on the second pad portion.
[0007] Embodiments of this disclosure may provide a semiconductor device, comprising: a first semiconductor structure including a first surface and a second surface opposite to the first surface in a direction perpendicular to the first surface; and a second semiconductor structure bonded to the first semiconductor structure and including a third surface contacting the second surface of the first semiconductor structure and a fourth surface opposite to the third surface in a direction perpendicular to the third surface. The second semiconductor structure may include: a first test pad disposed on the third surface and including a first pad portion, a second pad portion spaced apart from the first pad portion, and a first connection portion connecting the first pad portion and the second pad portion; a first probe pad disposed on the fourth surface and connected to the first pad portion via a first test contact disposed on the first pad portion; and a second probe pad disposed on the fourth surface and connected to the second pad portion via a second test contact disposed on the second pad portion.
[0008] Embodiments of this disclosure provide a method for detecting bonding defects in a semiconductor device, the semiconductor device comprising: a first bonding pad located on a substrate; a second bonding pad bonded to the first bonding pad; and a first test pad located on the same layer as the second bonding pad and having a first pad portion and a second pad portion spaced apart from each other. The method may include: applying a first voltage to a first probe pad connected to the first pad portion; applying a second voltage, different from the first voltage, to a second probe pad connected to the second pad portion; and determining whether a bonding defect has occurred by calculating a first sheet resistance value of the first test pad based on a current value between the first probe pad and the second probe pad.
[0009] According to embodiments of this disclosure, a semiconductor device and a method for detecting bonding defects in the semiconductor device can be provided, capable of detecting defects generated at the bonding interface.
[0010] The effects of the embodiments disclosed herein are not limited to those described above; those skilled in the art will clearly understand other unmentioned effects through the description in the claims. Attached Figure Description
[0011] This disclosure will be more fully understood through the following detailed description and accompanying drawings. The detailed description and accompanying drawings are for illustrative purposes only and are not intended to limit the scope of this disclosure.
[0012] Figure 1 This is a schematic diagram illustrating an example of a planar structure of a semiconductor device according to an embodiment of the present disclosure.
[0013] Figure 2 It shows along Figure 1 A schematic diagram of an example of a cross-sectional structure taken by the I-I' line.
[0014] Figure 3 This represents an example of a bonding defect. Figure 2 A magnified view of the central area 10.
[0015] Figures 4 to 7 This is a schematic diagram illustrating the process of bonding defect formation.
[0016] Figure 8 and Figure 9 It shows along Figure 1 A schematic diagram of other cross-sectional structures intercepted by the I-I' line.
[0017] Figure 10 This is a schematic diagram illustrating another example of a planar structure of a semiconductor device according to an embodiment of the present disclosure.
[0018] Figure 11 It shows along Figure 10 A schematic diagram illustrating examples of cross-sections taken by lines I-I' and II-II'.
[0019] Figures 12 to 14 It shows along Figure 10 Schematic diagrams of other examples of cross sections taken by lines I-I' and II-II'.
[0020] Figures 15 to 18 This is a schematic diagram illustrating an example of a method for detecting bonding defects in a semiconductor device according to an embodiment of the present disclosure. Detailed Implementation
[0021] In the following description of examples or embodiments of this disclosure, reference will be made to the accompanying drawings, which illustrate specific examples or embodiments that may be implemented by way of example, and the same reference numerals and symbols may be used to denote the same or similar components even if shown in different drawings. Furthermore, in the following description of examples or embodiments of this disclosure, detailed descriptions of well-known functions and components incorporated herein will be omitted where it is determined that such detailed descriptions might obscure the subject matter of certain embodiments of this disclosure. Terms such as “comprising,” “having,” “including,” “constituting,” “made of,” “formed from,” etc., as used herein, are generally intended to allow for the addition of additional components unless used with “only.” As used herein, the singular forms are intended to include the plural forms unless the context clearly indicates otherwise.
[0022] The terms “first,” “second,” “A,” “B,” “(A),” or “(B)” may be used in this document to describe elements of the disclosure. Each of these terms is not intended to define the nature, order, sequence, or number of elements, but only to distinguish the corresponding element from other elements.
[0023] When referring to a first element as "connected or coupled to," "in contact with," or "overlapping" with a second element, it should be understood that not only can the first element be "directly connected or coupled to" or "directly in contact with or overlap with" the second element, but a third element can also be "inserted" between the first and second elements, or the first and second elements can be "connected or coupled to," "in contact with," or "overlapped" with each other through a fourth element. Here, the second element can be included in at least one of two or more elements that are "connected or coupled to," "in contact with," or "overlap" with each other.
[0024] When using time-related terms such as “after,” “following,” “next,” or “before” to describe a process or operation of an element or structure, or a flow or step in an operation, processing, or manufacturing method, these terms may be used to describe discontinuous or non-sequential processes or operations unless used with “direct” or “immediate.”
[0025] Furthermore, when referring to any size, relative size, etc., even without specific description, it should be assumed that the numerical values or corresponding information of the component or feature (e.g., level, range, etc.) include the range of tolerances or errors that may be caused by various factors (e.g., process factors, internal or external influences, noise, etc.). In addition, the term "may" fully encompasses all the meanings of the term "able to".
[0026] In the accompanying drawings, two directions on the top surface of the substrate 200 are defined as a first direction FD and a second direction SD, respectively, and a direction projecting vertically from the top surface of the substrate 200 is defined as a third direction VD. The first direction FD and the second direction SD may be substantially perpendicular to each other. The third direction VD is a direction perpendicular to both the first direction FD and the second direction SD. In the following description, the term "perpendicular" or "perpendicular direction" will be used to indicate a direction substantially the same as the third direction VD. The directions indicated by the arrows in the accompanying drawings and their opposite directions indicate the same direction.
[0027] Figure 1 This is a schematic diagram illustrating an example of a planar structure of a semiconductor device according to an embodiment of the present disclosure. Figure 2 It shows along Figure 1 A schematic diagram of an example of a cross-sectional structure taken by the I-I' line.
[0028] refer to Figure 1 The semiconductor device according to embodiments of this disclosure may include a chip region CHR and a scribe region SR. The chip region CHR may refer to an area containing various elements and circuits constituting a single semiconductor device (or chip). The scribe region SR may refer to an area located outside the chip region CHR, on which multiple bonds or test patterns are arranged. The scribe region SR may surround the chip region CHR.
[0029] The chip region CHR can include the cell region CR and the peripheral region PR. The cell region CR can refer to the area where memory cells are arranged. The peripheral region PR can refer to the area located outside the cell region CR, where circuitry for providing various voltages or signals to the memory cells is arranged. The peripheral region PR can be located around the cell region CR.
[0030] In one embodiment, the first test pad TP1 may be disposed in the peripheral region PR. The first test pad TP1 may be part of a test pattern used to verify whether the manufactured semiconductor device is functioning correctly. Alternatively, the first test pad TP1 may be part of a test pattern used to detect defects such as signal faults within the semiconductor device. In embodiments of this disclosure, the first test pad TP1 may be a pattern used to detect bonding defects generated in the bonding pads.
[0031] In one embodiment, a voltage supplied from outside the semiconductor device can be applied to the first test pad TP1. When a voltage is applied to the first test pad TP1, the resistance of the first test pad TP1 can be measured based on the current flowing through it. In one embodiment, the resistance of the first test pad TP1 can vary depending on whether bonding defects occur. This will be referred to later. Figure 8 and Figure 9 Describe it.
[0032] although Figure 1 An example is shown where the first test pad TP1 is located in the peripheral region PR, but this disclosure is not limited thereto. The first test pad TP1 may also be located in the cell region CR or the scribe region SR.
[0033] The first test pad TP1 may include a first pad portion PD1, a second pad portion PD2, and a first connection portion CN1. The first pad portion PD1 and the second pad portion PD2 may be spaced apart from each other in the second direction SD. For example, the first pad portion PD1 and the second pad portion PD2 may be separate and / or not in contact with each other. (Reference) Figure 1 and Figure 2 The first pad portion PD1 and the second pad portion PD2 can refer to the areas in the first test pad TP1 that are connected to the first probe pad 293 and the second probe pad 294, respectively. In one embodiment, the width W1 of the first pad portion PD1 in the first direction FD can be greater than the width W2 of the first connection portion CN1 in the first direction FD.
[0034] The first connection portion CN1 can connect the first pad portion PD1 and the second pad portion PD2. The first connection portion CN1 can be located between the first pad portion PD1 and the second pad portion PD2. In one embodiment, the length L2 of the first connection portion CN1 in the second direction SD can be greater than the length W2 of the first connection portion CN1 in the first direction FD.
[0035] In one embodiment, the area of the top surface of the first connection portion CN1 (i.e., the value obtained by multiplying the length W2 in the first direction FD by the length L2 in the second direction SD) can be greater than the area of the top surface of the first pad portion PD1 (i.e., the value obtained by multiplying the length W1 in the first direction FD by the length L1 in the second direction SD).
[0036] refer to Figure 2 The semiconductor device according to embodiments of this disclosure may include a first semiconductor structure S1 and a second semiconductor structure S2. The first semiconductor structure S1 may include a first surface S1a and a second surface S1b that are opposite to each other in the vertical direction VD. The second semiconductor structure S2 may include a third surface S2a and a fourth surface S2b that are opposite to each other in the vertical direction. The third surface S2a of the second semiconductor structure S2 may be in contact with the second surface S1b of the first semiconductor structure S1.
[0037] The first semiconductor structure S1 may include a substrate 200, a device isolation layer 201, a source region 200S, a drain region 200D, a gate insulating layer 202, a gate electrode 203, a source contact 204, a drain contact 205, a first wiring 206, a second wiring 207, a first contact 208, a third wiring 209, a first bonding contact 210, a first insulating layer 220, a first bonding insulating layer 230, and a first bonding pad 231.
[0038] The second semiconductor structure S2 may include an insulating pattern 241, an electrode layer 242, a channel structure 250, a first interlayer insulating layer 260, a bit line contact 261, a bit line BL, a first test wiring 271, a second interlayer insulating layer 272, a second bonding contact 273, a first test contact 274, a second bonding insulating layer 275, a second bonding pad 276, a first test pad TP1, a source plate 280, a second contact 281, a second test contact 282, a fourth wiring 283, a second test wiring 284, a second insulating layer 285, a third contact 290, a third test contact 291, a fifth wiring 292, a first probe pad 293, a second probe pad 294, and a third insulating layer 295.
[0039] The channel structure 250 may include a charge storage pattern 251, a channel pattern 252, a core insulating layer 253, and a drain pad 254. In one embodiment, the charge storage pattern 251 may include a tunnel insulating layer, a charge trapping layer, and a barrier layer. The tunnel insulating layer, the charge trapping layer, and the barrier layer may be sequentially located on the outer surface of the channel pattern 252.
[0040] The channel structure 250, insulating pattern 241, and electrode layer 242 can constitute a NAND memory cell array. However, the semiconductor device according to embodiments of this disclosure is not limited to a semiconductor device including a NAND memory cell array, but may also include any type of semiconductor device stacked by wafer bonding. In the following description, a semiconductor device including a NAND memory cell array will be used as an example.
[0041] In the cell region CR, a channel structure 250 can be connected to a bit line BL via a bit line contact 261. A first test wiring 271 may be located on the same layer as the bit line BL. In one embodiment, the first test wiring 271 may be formed in the same process step as the bit line BL. The first test wiring 271 and the bit line BL may comprise conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0042] Below the bit line BL and the first test trace 271, a second bonding contact 273 and a first test contact 274 can be respectively provided. The second bonding contact 273 can connect the bit line BL and the second bonding pad 276. The first test contact 274 can connect the first test trace 271 and the first test pad TP1. Although... Figure 2 Three first test contacts 274 are shown, but this is merely an example, and the number of first test contacts 274 can be many. In one embodiment, when the number of first test contacts 274 is sufficiently large, the resistance of the first test contacts 274 can be neglected. Reference Figure 1 and Figure 2 The first test contact 274 can be connected to the first pad portion PD1 and the second pad portion PD2. The second bonding contact 273 and the first test contact 274 can include conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0043] Below the second bonding contact 273 and the first test contact 274, a first bonding pad 231 and a first test pad TP1 can be respectively disposed. The first test pad TP1 can be located on the same layer as the second bonding pad 276. For example, the first test pad TP1 and the second bonding pad 276 can be disposed on the third surface S2a of the second semiconductor structure S2. The second bonding insulating layer 275 can surround the sides of the first test pad TP1 and the second bonding pad 276.
[0044] In one embodiment, the first test pad TP1 and the second bonding pad 276 can be formed in the same process step. For example, the first test pad TP1 may include the same material as the material used to form the second bonding pad 276. The first test pad TP1 and the second bonding pad 276 may include copper (Cu), tantalum (Ta), tantalum nitride (TaN), manganese (Mn), or a combination thereof.
[0045] The bottom surface of the first test pad TP1 can be substantially coplanar with the bottom surface of the second bonding pad 276. The bottom surface of the first test pad TP1 can contact the top surface of the first bonding insulating layer 230. In one embodiment, the bottom surface of the first test pad TP1 can be substantially coplanar with the bottom surface of the second bonding insulating layer 275.
[0046] The second semiconductor structure S2 can be bonded to the first semiconductor structure S1 via the first bonding pad 231, the second bonding pad 276, the first bonding insulating layer 230, and the second bonding insulating layer 275. For example, the first bonding pad 231 and the second bonding pad 276 can be bonded to each other. The first bonding insulating layer 230 and the second bonding insulating layer 275 can be bonded to each other. The first bonding insulating layer 230 can surround the side of the first bonding pad 231.
[0047] In the cell region CR, a channel structure 250 can be connected to the drain region 200D of the transistor via bit line contact 261, bit line BL, second bonding contact 273, second bonding pad 276, first bonding pad 231, first bonding contact 210, third wiring 209, first contact 208, second wiring 207 and drain contact 205.
[0048] A second test contact 282, a second test wiring 284, and a third test contact 291 can be sequentially configured on the first test wiring 271. Although Figure 2Three second test contacts 282 and three third test contacts 291 are shown, but this is merely an example, and the number of second test contacts 282 and third test contacts 291 can be many. The second test contacts 282 and third test contacts 291 may include the same material as the first test contact 274. The second test wiring 284 may include the same material as the first test wiring 271.
[0049] The first probe pad 293 and the second probe pad 294 can be disposed on the third test contact 291. The first probe pad 293 and the second probe pad 294 can be disposed on the fourth surface S2b of the second semiconductor structure S2. The first probe pad 293 and the second probe pad 294 can be connected to the first test pad TP1 through the third test contact 291, the second test wiring 284, the second test contact 282, the first test wiring 271, and the first test contact 274.
[0050] A voltage supplied from outside the semiconductor device can be applied to the first probe pad 293 and the second probe pad 294. The voltage applied to the first probe pad 293 can be different from the voltage applied to the second probe pad 294. For example, a ground voltage (0V) can be applied to the first probe pad 293, and a voltage equal to or greater than 0.1V can be applied to the second probe pad 294. Alternatively, a ground voltage can be applied to the second probe pad 294, and a voltage equal to or greater than 0.1V can be applied to the first probe pad 293.
[0051] The first probe pad 293 and the second probe pad 294 may include conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0052] In one embodiment, when no bonding defects occur, the bottom surface of the second bonding pad 276 can be in complete contact with the top surface of the first bonding pad 231. However, when bonding defects occur, the bottom surface of the second bonding pad 276 can be spaced apart from the top surface of the first bonding pad 231. Alternatively, when bonding defects occur, at least a portion of the second bonding insulating layer 275 can be spaced apart from the first bonding insulating layer 230.
[0053] Figure 3 yes Figure 2 A magnified view of region 10 shows an example of bonding defects. Figure 3 The diagram shows a case where bonding occurs normally (Case 1) and a case where bonding defects occur (Case 2).
[0054] Bonding defects may include bonding defects between the first bonding pad 231 and the second bonding pad 276, bonding defects between the first bonding insulating layer 230 and the second bonding insulating layer 275, or combinations thereof. For example, bonding defects may include defects caused by excessive depression of the top surface of the first bonding pad 231 or the second bonding pad 276 during the formation of the first bonding pad 231 or the second bonding pad 276. Alternatively, bonding defects may include defects caused by slight depressions on the top surface of the first bonding pad 231 or the second bonding pad 276, or inherent defects formed in the first bonding pad 231 or the second bonding pad 276.
[0055] The following description will take the defect caused by excessive etching (depression) on the top surface of the first bonding pad 231 or the second bonding pad 276 as an example.
[0056] refer to Figure 3 As shown in Case 1, when the first bonding pad 231 and the second bonding pad 276 are normally bonded, the bottom surface of the second bonding pad 276 can be in complete contact with the top surface of the first bonding pad 231. However, as shown in Case 2, when the top surface of the second bonding pad 276 is excessively recessed, the bottom surface of the second bonding pad 276 can be spaced apart from the top surface of the first bonding pad 231. The following will refer to... Figures 4 to 7 Describe in detail the phenomenon caused by excessive indentation.
[0057] Figures 4 to 7 This is a schematic diagram illustrating the process of bonding defect formation. Figures 4 to 7 It shows Figure 3 The formation process of the first bonding pad 231 and the second bonding pad 276 in Case 2.
[0058] refer to Figure 4 The first bonding insulating layer 230 can be formed on the first insulating layer 220 and the first bonding contact 210 included in the first semiconductor structure S1. The first trench TH1 can be formed in the first bonding insulating layer 230. The second bonding insulating layer 275 can be formed on the second interlayer insulating layer 272 and the second bonding contact 273 included in the second semiconductor structure S2. The second trench TH2 can be formed in the second bonding insulating layer 275.
[0059] refer to Figure 5 The first bonding pad 231 and the second bonding pad 276 can be formed in the first trench TH1 and the second trench TH2, respectively.
[0060] The process of forming the first bonding pad 231 and the second bonding pad 276 may include: depositing conductive material in the first trench TH1 and the second trench TH2, and then removing the top of the conductive material by a grinding or chemical mechanical polishing (CMP) process. The conductive material may include copper (Cu), tantalum (Ta), tantalum nitride (TaN), or a combination thereof.
[0061] In some embodiments, more conductive material deposited in the second trench TH2 may be removed than that deposited in the first trench TH1. For example, the conductive material deposited in the second trench TH2 may cause excessive indentation. Therefore, the vertical thickness t2 of the first bonding pad 231 may be greater than the vertical thickness t3 of the second bonding pad 276.
[0062] refer to Figure 6 The second semiconductor structure S2 can be stacked on the first semiconductor structure S1. The second bonding insulating layer 275 can be stacked on the first bonding insulating layer 230. The second bonding pad 276 can be spaced apart from the first bonding pad 231.
[0063] refer to Figure 7 A heating process can be performed on the first bonding pad 231 and the second bonding pad 276. The first bonding pad 231 and the second bonding pad 276 can expand after heating. The top surface of the expanded first bonding pad 231 can be substantially on the same plane as the top surface of the first bonding insulating layer 230.
[0064] However, the bottom surface of the expanded second bonding pad 276 may be located at a higher position than the bottom surface of the second bonding insulating layer 275. The second bonding pad 276 may be spaced apart from the first bonding pad 231. The second bonding pad 276 and the first bonding pad 231 may be physically and electrically separated. That is, due to excessive recess, the second bonding pad 276 may develop bonding defects.
[0065] Refer again Figure 2 When a bonding defect occurs and the second bonding pad 276 separates from the first bonding pad 231, the channel structure 250 included in the second semiconductor structure S2 may fail to make an electrical connection with the transistor included in the first semiconductor structure S1. In other words, a proper electrical connection may not be established between the first semiconductor structure S1 and the second semiconductor structure S2. Therefore, the semiconductor device may malfunction.
[0066] According to one embodiment of this disclosure, since a first test pad TP1, test contacts 274, 282, 291, test wiring 271, 284, a first probe pad 293, and a second probe pad 294 are provided inside the second semiconductor structure S2, bonding defects between the first bonding pad 231 and the second bonding pad 276 can be detected in advance.
[0067] Refer again Figure 1 and Figure 2 The first test pad TP1 can be formed in the same process step as the second bonding pad 276. That is, when no such test pad TP1 is formed in the second bonding pad 276... Figures 4 to 7 In the event of a bonding defect, the bottom surface of the first test pad TP1 can be substantially flush with the bottom surface of the second bonding insulating layer 275. Furthermore, the bottom surface of the first test pad TP1 can be in complete contact with the top surface of the first bonding insulating layer 230.
[0068] When a bonding defect occurs, the vertical thickness of the first test pad TP1 may differ from the vertical thickness t1 of the first test pad TP1 when no bonding defect occurs. When the thickness of the first test pad TP1 changes, the sheet resistance of the first test pad TP1 may change as shown in Formula 1 below.
[0069] [Formula 1]
[0070] Rs=ρ / t
[0071] In Formula 1, Rs represents sheet resistance, ρ represents resistivity, and t represents the vertical thickness of the object.
[0072] Since ρ is an inherent property of the material, the sheet resistance of the first test pad TP1 will change accordingly when bonding defects such as depressions occur and the thickness of the first test pad TP1 decreases.
[0073] In one embodiment of this disclosure, the occurrence of bonding defects can be detected by comparing the sheet resistance of the first test pad TP1 when bonding defects occur with the sheet resistance of the first test pad TP1 when no bonding defects occur.
[0074] When no bonding defects occur, the sheet resistance of the first test pad TP1 corresponds to the sheet resistance when the entire bottom surface of the first test pad TP1 is on the same plane as the bottom surface of the second bonding insulating layer 275. When no bonding defects occur, the vertical thickness t1 of the first test pad TP1 can be substantially the same as the vertical thickness of the second bonding insulating layer 275. Therefore, if the vertical thickness of the second bonding insulating layer 275 is known, the sheet resistance of the first test pad TP1 can be calculated using Formula 1.
[0075] In one embodiment, during the manufacturing of a semiconductor device, the second bonding insulating layer 275 can be formed to have a predetermined thickness. Therefore, referring to Formula 1, the sheet resistance of the first test pad TP1 when no bonding defects occur can be the value obtained by dividing the resistivity of the material forming the first test pad TP1 by the predetermined thickness of the second bonding insulating layer 275.
[0076] The sheet resistance of the first test pad TP1 when no bonding defects occur will be referred to as the first reference value.
[0077] Once the first reference value is obtained, the sheet resistance of the first test pad TP1 in any semiconductor device, regardless of whether bonding defects have occurred, can be measured and compared with the first reference value. By comparing the measured sheet resistance of the first test pad TP1 with the first reference value, it can be determined whether a bonding defect has occurred. This will be discussed later. Figure 8 and Figure 9 To provide a more detailed description.
[0078] Figure 8 and Figure 9 It shows along Figure 1 Schematic diagrams of other examples of cross-sectional structures cut by the I-I' line.
[0079] refer to Figure 8 The first test pad TP1 can be connected to Figure 2 The second bonding pad 276 is formed in the same process step. For example... Figure 3 As shown in Case 2, when excessive depression occurs in the second bonding pad 276, such as Figure 8 As shown, bonding defects may also occur in the first test pad TP1. The vertical thickness t4 of the first test pad TP1 can be less than... Figure 2 The vertical thickness t1 of the first test pad TP1.
[0080] As described above, different voltages can be applied between the first probe pad 293 and the second probe pad 294, and the current between the first probe pad 293 and the second probe pad 294 can be measured. Based on this current, the resistance between the first probe pad 293 and the second probe pad 294 can be calculated. Once the resistance between the first probe pad 293 and the second probe pad 294 is calculated, the sheet resistance of the first test pad TP1 included in any semiconductor device can be calculated based on Formula 1 and the following Formula 2.
[0081] [Formula 2]
[0082] R = Rs × L / W
[0083] In Formula 2, R represents the resistance of the first test pad TP1, Rs represents the sheet resistance of the first test pad TP1, L represents the length of the first test pad TP1 in the second direction SD, and W represents the width of the first test pad TP1 in the first direction FD.
[0084] Since the values of L and W are predetermined, the sheet resistance of the first test pad TP1 can be calculated by measuring the resistance of the first test pad TP1 included in any semiconductor device.
[0085] The resistance of the first test pad TP1 can be calculated based on the current flowing between the first probe pad 293 and the second probe pad 294. The specific explanation is as follows.
[0086] For example, a positive voltage can be applied to the first probe pad 293, and a ground voltage can be applied to the second probe pad 294. Current can flow from the first probe pad 293 along the test contact, test wiring, and the first test pad TP1 to the second probe pad 294. In this case, the resistance between the first probe pad 293 and the second probe pad 294 can be the series sum of the resistances of the test contacts 274, 282, and 291, the resistances of the test wirings 271 and 284, and the resistance of the first test pad TP1, and the contact resistance between the test contacts and the test wiring.
[0087] As per the above reference Figure 2 The number of test contacts 274, 282, and 291 can be large, and the test contacts 274, 282, and 291 and the test wirings 271 and 284 can all be made of the same material. In this case, the resistance of the test contacts 274, 282, and 291, as well as the contact resistance between the test contacts 274, 282, and 291 and the test wirings 271 and 284, can be relatively small. Furthermore, the length of the first connection portion CN1 of the first test pad TP1 can be very large. In one embodiment, the length L2 of the first connection portion CN1 in the second direction SD can be more than 100 times greater than the length of the first pad portion PD1 or the second pad portion PD2 in the second direction SD. In this case, the resistance measured between the first probe pad 293 and the second probe pad 294 can be considered to be substantially the same as the resistance of the first test pad TP1.
[0088] Therefore, the resistance of the first test pad TP1 can be calculated by measuring the current flowing between the first probe pad 293 and the second probe pad 294.
[0089] If the first test pad TP1 exhibits excessive depression, the measured resistance of the first test pad TP1 will be relatively high. Therefore, based on Formula 2, the calculated sheet resistance of the first test pad TP1 can be greater than the first reference value. In one embodiment, when the calculated sheet resistance of the first test pad TP1 exceeds 105% of the first reference value, it can be determined that... Figure 2 Bonding defects occurred in the second bonding pad 276.
[0090] Therefore, even when the thickness of the first bonding pad 231 or the second bonding pad 276 is unknown, bonding defects can be detected by measuring the current between the first probe pad 293 and the second probe pad 294.
[0091] refer to Figure 9 Different voltages can be applied between the first probe pad 293 and the second probe pad 294 to measure the current between them. Once the current between the first probe pad 293 and the second probe pad 294 has been measured, the sheet resistance of the first test pad TP1 can be calculated based on Formulas 1 and 2 as described above.
[0092] like Figure 9 As shown, insufficient depression can also lead to bonding defects. (Reference) Figure 5 and Figure 6 When the degree of depression during the formation of the bonding pad is extremely small, the thickness of the second bonding pad 276 may be greater than t2. In this case, when heat is applied in subsequent processes, the second bonding pad 276 may expand to a thickness greater than the thickness of the second bonding insulating layer 275. Since the thickness of the first test pad TP1 can be the same as the thickness of the second bonding pad 276, therefore Figure 9 The vertical thickness t5 of the first test pad TP1 shown can be greater than Figure 2 The vertical thickness t1 (e.g., optimal vertical thickness) of the first test pad TP1 shown.
[0093] If the depressions on the first test pad TP1 are significantly reduced, the resistance of the first test pad TP1 will be measured as smaller. Therefore, the sheet resistance of the first test pad TP1 can be calculated to be less than a first reference value. In one embodiment, when the sheet resistance of the first test pad TP1 is less than 95% of the first reference value, it can be determined that... Figure 2 Bonding defects occurred in the second bonding pad 276.
[0094] Figure 10 This is a schematic diagram illustrating another example of a planar structure of a semiconductor device according to an embodiment of the present disclosure. Figure 11 It shows along Figure 10 A schematic diagram illustrating examples of cross-sections taken by lines I-I' and II-II'.
[0095] refer to Figure 10 The first test pad TP1 and the second test pad TP2 can be disposed in the peripheral region PR. In one embodiment of this disclosure, the first test pad TP1 and the second test pad TP2 can be patterns used to detect bonding defects generated in the bond pads. The first test pad TP1 can be related to the above reference. Figure 1 The first test pad TP1 described is basically the same.
[0096] In one embodiment, a voltage supplied from outside the semiconductor device can be applied to a first test pad TP1 and a second test pad TP2. When a voltage is applied to the first test pad TP1 and the second test pad TP2, the resistance of the first test pad TP1 and the second test pad TP2 can be measured based on the current flowing through the first test pad TP1 and the second test pad TP2, respectively. In one embodiment, the resistance of the first test pad TP1 and the second test pad TP2 can vary depending on whether bonding defects occur. This will be referred to later. Figures 12 to 14 Describe it.
[0097] although Figure 10 The illustration shows a first test pad TP1 and a second test pad TP2 located in the peripheral region PR, but this disclosure is not limited thereto. At least one of the first test pad TP1 and the second test pad TP2 may be located in the cell region CR or the scribe region SR.
[0098] The second test pad TP2 may include a third pad portion PD3, a fourth pad portion PD4, and a second connection portion CN2. The third pad portion PD3 and the fourth pad portion PD4 may be spaced apart from each other in the second direction SD. (Reference) Figure 10 and Figure 11 The third pad portion PD3 and the fourth pad portion PD4 can refer to the areas in the second test pad TP2 that are connected to the third probe pad 1193 and the fourth probe pad 1194, respectively. In one embodiment, the width of the third pad portion PD3 in the first direction FD can be greater than the width of the second connection portion CN2 in the first direction FD.
[0099] The second connection portion CN2 can connect the third pad portion PD3 and the fourth pad portion PD4. The second connection portion CN2 can be located between the third pad portion PD3 and the fourth pad portion PD4. In one embodiment, the length L2 of the second connection portion CN2 in the second direction SD can be greater than the length W2 of the second connection portion CN2 in the first direction FD.
[0100] In one embodiment, the area of the top surface of the second connection portion CN2 (i.e., the value obtained by multiplying the length W2 in the first direction FD by the length L2 in the second direction SD) can be greater than the area of the top surface of the third pad portion PD3 (i.e., the value obtained by multiplying the length W1 in the first direction FD by the length L1 in the second direction SD).
[0101] refer to Figure 11 The semiconductor device according to the embodiments of this disclosure may include a first semiconductor structure S1 and a second semiconductor structure S2.
[0102] The first semiconductor structure S1 may include a substrate 200, a first insulating layer 220, a first bonding insulating layer 230, and a second test pad TP2.
[0103] The second test pad TP2 can be set on the first insulating layer 220. The second test pad TP2 can be... Figure 2 The first bonding pad 231 is located on the same layer. For example, the second test pad TP2 and the first bonding pad 231 can be disposed on the second surface S1b of the first semiconductor structure S1. The first bonding insulating layer 230 can surround the side of the second test pad TP2.
[0104] The bottom surface of the second test pad TP2 can be substantially coplanar with the bottom surface of the first bonding insulating layer 230. The top surface of the second test pad TP2 can contact the bottom surface of the second bonding insulating layer 275. In one embodiment, the top surface of the second test pad TP2 can be substantially coplanar with the top surface of the first bonding insulating layer 230.
[0105] The second semiconductor structure S2 may include a first test wiring 271, a third test wiring 1171, a first test contact 274, a fourth test contact 1174, a second bonding insulating layer 275, a first test pad TP1, a first dummy bonding pad DBP1, a second dummy bonding pad DBP2, a second test contact 282, a fifth test contact 1182, a second test wiring 284, a fourth test wiring 1184, a second insulating layer 285, a third test contact 291, a sixth test contact 1191, a first probe pad 293, a second probe pad 294, a third probe pad 1193, a fourth probe pad 1194, and a third insulating layer 295.
[0106] The third test wiring 1171 may be located on the same layer as the first test wiring 271. In one embodiment, the third test wiring 1171 may be formed in the same process step as the first test wiring 271. The third test wiring 1171 may include conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0107] A fourth test contact 1174 can be provided below the third test trace 1171. The fourth test contact 1174 can connect the third test trace 1171 and the first dummy bonding pad DBP1. Although Figure 11 Three fourth test contacts 1174 are shown, but this is merely an example, and the number of fourth test contacts 1174 can be many. (Reference) Figure 10 and Figure 11The fourth test contact 1174 can be connected to the first dummy bonding pad DBP1 and the second dummy bonding pad DBP2. The fourth test contact 1174 may include conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0108] A first dummy bond pad DBP1 and a second dummy bond pad DBP2 can be disposed below the fourth test contact 1174. The first dummy bond pad DBP1 and the second dummy bond pad DBP2 can be located on the same layer as the first test pad TP1. For example, a second bonding insulating layer 275 can surround the sides of the first dummy bond pad DBP1 and the second dummy bond pad DBP2.
[0109] In one embodiment, the first dummy bond pad DBP1 and the second dummy bond pad DBP2 can be formed in the same process step as the first test pad TP1. For example, the first dummy bond pad DBP1 and the second dummy bond pad DBP2 may include the same material as the first test pad TP1. The first dummy bond pad DBP1 and the second dummy bond pad DBP2 may include copper (Cu), tantalum (Ta), tantalum nitride (TaN), or a combination thereof.
[0110] The bottom surfaces of the first dummy bonding pad DBP1 and the second dummy bonding pad DBP2 can be substantially coplanar with the bottom surface of the first test pad TP1. The bottom surfaces of the first dummy bonding pad DBP1 and the second dummy bonding pad DBP2 can contact the top surface of the second test pad TP2. In one embodiment, the bottom surfaces of the first dummy bonding pad DBP1 and the second dummy bonding pad DBP2 can be substantially coplanar with the bottom surface of the second bonding insulating layer 275.
[0111] The second semiconductor structure S2 can be bonded to the first semiconductor structure S1.
[0112] The fifth test contact 1182, the fourth test contact 1184, and the sixth test contact 1191 can be sequentially set on the third test wiring 1171. Although Figure 11 Three fifth test contacts 1182 and three sixth test contacts 1191 are shown, but this is merely an example, and the number of fifth and sixth test contacts can be many. The fifth test contacts 1182 and sixth test contacts 1191 may comprise the same material as the fourth test contact 1174. The fourth test wiring 1184 may comprise the same material as the third test wiring 1171.
[0113] The third probe pad 1193 and the fourth probe pad 1194 can be located on the sixth test contact 1191. (See reference) Figure 2 and Figure 11The third probe pad 1193 and the fourth probe pad 1194 can be disposed on the fourth surface S2b of the second semiconductor structure S2. The third probe pad 1193 and the fourth probe pad 1194 can be connected to the second test pad TP2 through the sixth test contact 1191, the fourth test wiring 1184, the fifth test contact 1182, the third test wiring 1171, the fourth test contact 1174, the first dummy bonding pad DBP1, and the second dummy bonding pad DBP2.
[0114] A voltage supplied from outside the semiconductor device can be applied to the third probe pad 1193 and the fourth probe pad 1194. The voltage applied to the third probe pad 1193 can be different from the voltage applied to the fourth probe pad 1194 (e.g., by a predetermined minimum value). For example, a ground voltage can be applied to the third probe pad 1193, and a voltage equal to or greater than 0.1V can be applied to the fourth probe pad 1194. Alternatively, a ground voltage can be applied to the fourth probe pad 1194, and a voltage equal to or greater than 0.1V can be applied to the third probe pad 1193.
[0115] The third probe pad 1193 and the fourth probe pad 1194 may include conductive materials such as metal, metal oxide, metal nitride, metal silicide, polysilicon, conductive carbon, or combinations thereof.
[0116] In one embodiment of this disclosure, the second test pad TP2 can be with Figure 2 The first bonding pad 231 is formed in the same process step. When no bonding pad 231 is formed as described above... Figures 4 to 7 In the event of a bonding defect, the top surface of the second test pad TP2 can be substantially flush with the top surface of the first bonding insulating layer 230. Furthermore, the top surface of the second test pad TP2 can contact the bottom surface of the second bonding insulating layer 275.
[0117] When no bonding defects occur, the vertical thickness t6 of the second test pad TP2 can be substantially the same as the vertical thickness of the first bonding insulating layer 230. Therefore, if the vertical thickness of the first bonding insulating layer 230 is known, the sheet resistance of the second test pad TP2 can be calculated with reference to Formula 1.
[0118] In one embodiment, during the manufacturing of a semiconductor device, the first bonding insulating layer 230 can be formed to have a predetermined thickness. Therefore, referring to Formula 1, the sheet resistance of the second test pad TP2 when no bonding defects occur can be the value obtained by dividing the resistivity of the material forming the second test pad TP2 by the predetermined thickness of the first bonding insulating layer 230. Since the thickness of the second test pad TP2 can be substantially the same as the thickness of the first test pad TP1, the sheet resistance of the second test pad TP2 when no bonding defects occur can be a first reference value.
[0119] Once the first reference value is obtained, the sheet resistance of the second test pad TP2 included in any semiconductor device, regardless of whether bonding defects have occurred, can be measured and compared with the first reference value. By comparing the measured sheet resistance of the second test pad TP2 with the first reference value, it can be determined whether a bonding defect has occurred. This will be discussed later. Figures 12 to 14 Provide a detailed description.
[0120] Figures 12 to 14 It shows along Figure 10 Schematic diagrams of other examples of cross sections taken by lines I-I' and II-II'.
[0121] refer to Figures 12 to 14 The second test pad TP2 can be connected to Figure 2 The first bonding pad 231 is formed in the same process step. When Figure 2 When excessive depression occurs in the first bonding pad 231, such as Figure 12 As shown, the second test pad TP2 may also have bonding defects.
[0122] refer to Figure 12 The second test pad TP2 can be spaced apart from the first dummy bond pad DBP1 and the second dummy bond pad DBP2. In this case, the third probe pad 1193 and the fourth probe pad 1194 can be electrically isolated. The vertical thickness t7 of the second test pad TP2 can be less than the vertical thickness t1 of the first test pad TP1.
[0123] As described above, different voltages can be applied between the third probe pad 1193 and the fourth probe pad 1194, and the current between the third probe pad 1193 and the fourth probe pad 1194 can be measured. Once the current between the third probe pad 1193 and the fourth probe pad 1194 has been measured, the sheet resistance of the second test pad TP2 included in any semiconductor device can be calculated based on Formulas 1 and 2. Since the values of L and W are predetermined, the sheet resistance of the second test pad TP2 included in any semiconductor device can be calculated by measuring its resistance.
[0124] The resistance of the second test pad TP2 can be calculated based on the current flowing between the third probe pad 1193 and the fourth probe pad 1194. The method for calculating the resistance of the second test pad TP2 is similar to the method described above for calculating the resistance of the first test pad TP1. Since the first dummy bond pad DBP1 and the second dummy bond pad DBP2 can contain the same material as the second test pad TP2, the contact resistance between the first dummy bond pad DBP1, the second dummy bond pad DBP2, and the second test pad TP2 can be ignored.
[0125] When excessive depression occurs in the second test pad TP2, the third probe pad 1193 and the fourth probe pad 1194 can be electrically isolated, resulting in a very small measured current. That is, the measured resistance of the second test pad TP2 can be very high. Therefore, the sheet resistance of the second test pad TP2 can be greater than the first reference value. In one embodiment, when the calculated sheet resistance of the second test pad TP2 exceeds 105% of the first reference value, it can be determined that... Figure 2 A bonding defect occurred in the first bonding pad 231.
[0126] refer to Figure 13 The second test pad TP2 can be partially connected to the first dummy bond pad DBP1 and the second dummy bond pad DBP2. In this case, current can flow between the third probe pad 1193 and the fourth probe pad 1194. The resistance of the second test pad TP2 can be calculated based on the current between the third probe pad 1193 and the fourth probe pad 1194.
[0127] When excessive recess occurs on the second test pad TP2, its sheet resistance may exceed the first reference value. In one embodiment, if the calculated sheet resistance of the second test pad TP2 exceeds 105% of the first reference value, it can be determined that... Figure 2 A bonding defect occurred in the first bonding pad 231.
[0128] Therefore, even in the unknown Figure 2 In cases where the thickness of the first bonding pad 231 or the second bonding pad 276 is known, bonding defects can also be detected by measuring the current between the third probe pad 1193 and the fourth probe pad 1194.
[0129] refer to Figure 14 Different voltages can be applied between the third probe pad 1193 and the fourth probe pad 1194 to measure the current between them. Once the current between the third probe pad 1193 and the fourth probe pad 1194 has been measured, the sheet resistance of the second test pad TP2 can be calculated based on Formulas 1 and 2 as described above.
[0130] like Figure 14 As shown, insufficient depression can also lead to bonding defects. (See again...) Figure 5 and Figure 6 If the depression during the formation of the bonding pad is minimal, the thickness of the first bonding pad 231 can be greater than t2. In this case, when heat is applied in subsequent processes, the first bonding pad 231 can expand to a thickness greater than the thickness of the first bonding insulating layer 230. Since the thickness of the second test pad TP2 can be the same as the thickness of the first bonding pad 231, the vertical thickness t8 of the second test pad TP2 can be greater than the vertical thickness t1 of the first test pad TP1.
[0131] When the depression in the second test pad TP2 is very small, its measured resistance can be relatively small. Therefore, the calculated sheet resistance of the second test pad TP2 can be less than the first reference value. If the sheet resistance of the second test pad TP2 is less than 95% of the first reference value, then it can be determined that... Figure 2 A bonding defect occurred in the first bonding pad 231.
[0132] Figures 15 to 18 This is a schematic diagram illustrating an example of a method for detecting bonding defects in a semiconductor device according to an embodiment of the present disclosure.
[0133] refer to Figure 15 The bonding defect detection method for a semiconductor device according to embodiments of the present disclosure may include: applying a first voltage to a first probe pad 293 (S101); applying a second voltage to a second probe pad 294 (S102); and determining whether a bonding defect has occurred by calculating a first sheet resistance value of a first test pad TP1 (S103).
[0134] Figure 15 The bonding defect detection method shown can be applied to the above reference. Figure 1 and Figure 2 The semiconductor device described.
[0135] refer to Figure 1 , Figure 2 and Figure 15 The semiconductor device may include: a substrate 200; a first bonding pad 231 disposed on the substrate 200; a second bonding pad 276 bonded to the first bonding pad 231; a first test pad TP1 located on the same layer as the second bonding pad 276 and including a first pad portion PD1 and a second pad portion PD2 spaced apart from each other; a first probe pad 293; and a second probe pad 294.
[0136] The first probe pad 293 can be connected to the first pad portion PD1, and the second probe pad 294 can be connected to the second pad portion PD2. A first voltage can be applied to the first probe pad 293, and a second voltage different from the first voltage can be applied to the second probe pad 294.
[0137] Referring to Formula 2, the first sheet resistance value of the first test pad TP1 can be calculated based on the current value between the first probe pad 293 and the second probe pad 294.
[0138] In one embodiment, if the first sheet resistance value differs from a first reference value, a bonding defect can be determined. The first reference value can be the sheet resistance of the first test pad TP1 when the entire bottom surface of the first test pad TP1 is on the same plane as the bottom surface of the second bonding insulation layer 275.
[0139] refer to Figure 16 The operation of determining whether a bonding defect has occurred by calculating the first sheet resistance value of the first test pad TP1 (S103) may further include determining whether the first sheet resistance value is within the range of 95% to 105% of the first reference value (S1501).
[0140] If the first sheet resistance value is within 95% to 105% of the first reference value (S1501, Yes), it can be determined that no bonding defect has occurred in the second bonding pad 276 (S1502). If the first sheet resistance value is less than 95% of the first reference value or greater than 105% of the first reference value (S1501, No), it can be determined that a bonding defect has occurred in the second bonding pad 276 (S1503).
[0141] refer to Figure 17 The bonding defect detection method for a semiconductor device according to embodiments of the present disclosure may include: applying a first voltage to a first probe pad 293 (S101); applying a second voltage to a second probe pad 294 (S102); determining whether a bonding defect has occurred by calculating a first sheet resistance value of a first test pad TP1 (S103); applying a first voltage to a third probe pad 1193 (S104); applying a second voltage to a fourth probe pad 1194 (S105); and determining whether a bonding defect has occurred by calculating a second sheet resistance value of a second test pad TP2 (S106).
[0142] Figure 17 The bonding defect detection method shown can be applied to the above reference. Figure 10 and Figure 11 The semiconductor device described.
[0143] refer to Figure 10 , Figure 11 and Figure 17The semiconductor device may include a substrate 200; a first test pad TP1; a first probe pad 293; a second probe pad 294; a second test pad TP2, which is located on the same layer as the first test pad TP1 and includes a third pad portion PD3 and a fourth pad portion PD4 spaced apart from each other; a third probe pad 1193; a fourth probe pad 1194; a first dummy bonding pad DBP1; and a second dummy bonding pad DBP2.
[0144] The third probe pad 1193 can be connected to the third probe pad portion PD3. The fourth probe pad 1194 can be connected to the fourth probe pad portion PD4. A first voltage can be applied to the third probe pad 1193, and a second voltage different from the first voltage can be applied to the fourth probe pad 1194.
[0145] Referring to Formula 2, the second square resistance value of the second test pad TP2 can be calculated based on the current value between the third probe pad 1193 and the fourth probe pad 1194.
[0146] In one embodiment, if the second sheet resistance value differs from the first reference value, a bonding defect can be determined. The first reference value can be the sheet resistance value of the second test pad TP2 when the entire top surface of the second test pad TP2 is in the same plane as the top surface of the first bonding insulation layer 230.
[0147] In one embodiment, if it is determined that no bonding defects have occurred in the second bonding pad 276, then it can be further determined whether bonding defects have occurred in the first bonding pad 231.
[0148] refer to Figure 18 The operation of determining whether a bonding defect has occurred by calculating the second sheet resistance value of the second test pad TP2 (S106) may include determining whether the second sheet resistance value is within the range of 95% to 105% of the first reference value (S1701).
[0149] If the second sheet resistance value is within 95% to 105% of the first reference value (S1701, Yes), it can be determined that no bonding defect has occurred in the first bonding pad 231 (S1702). If the second sheet resistance value is less than 95% of the first reference value or greater than 105% of the first reference value (S1701, No), it can be determined that a bonding defect has occurred in the first bonding pad 231 (S1703).
[0150] According to embodiments of this disclosure, a semiconductor device may include a first test pad TP1, a first probe pad 293, a second probe pad 294, a second test pad TP2, a third probe pad 1193, and a fourth probe pad 1194. The first test pad TP1 and the second test pad TP2 may be formed in the same process step as the second bonding pad 276 and the first bonding pad 231, respectively.
[0151] When a bonding defect occurs in either the first bonding pad 231 or the second bonding pad 276, the same bonding defect may also occur in either the first test pad TP1 or the second test pad TP2. Therefore, by measuring the sheet resistance value of the first test pad TP1 or the second test pad TP2 and comparing it with a predetermined reference value, the disclosed embodiments provide the ability to determine whether a bonding defect has occurred in either the first bonding pad 231 or the second bonding pad 276. Thus, bonding defects occurring at the bonding interface can be accurately detected even when the exact thickness of the bonding pad is unknown.
[0152] The above description is merely an illustration of the technical features of this disclosure. Those skilled in the art to which this disclosure pertains can make various modifications and changes without departing from the scope and concept of this disclosure. Furthermore, the embodiments described herein are for illustrative purposes only and are not intended to limit the scope of this disclosure. The scope of protection of this disclosure should be interpreted according to the claims, and all equivalent technical concepts should be interpreted as included within the scope of this disclosure.
Claims
1. A semiconductor device, comprising: The first bonding pad is disposed on the substrate; The second bonding pad is bonded to the first bonding pad; The first test pad is located on the same layer as the second bonding pad and includes a first pad portion, a second pad portion spaced apart from the first pad portion, and a first connection portion connecting the first pad portion and the second pad portion. A first probe pad is connected to the first pad portion via a first test contact disposed on the first pad portion; and The second probe pad is connected to the second pad portion via a second test contact disposed on the second pad portion.
2. The semiconductor device of claim 1, further comprising a first bonding insulating layer, the first bonding insulating layer surrounding the side surface of the first bonding pad, wherein, The first test pad is in contact with the top surface of the first bonding insulation layer.
3. The semiconductor device of claim 1, further comprising a first bonding insulating layer, the first bonding insulating layer surrounding the side surface of the first bonding pad, wherein, The first test pad is spaced apart from the first bonding insulation layer.
4. The semiconductor device according to claim 1, in, The area of the top surface of the first connection portion is greater than the area of the top surface of the first pad portion or the area of the top surface of the second pad portion.
5. The semiconductor device according to claim 1, in, The width of the first pad portion on the top surface of the substrate in a first direction is greater than the width of the first connection portion in the first direction.
6. The semiconductor device according to claim 1, in, Apply a first voltage to the first probe pad, and Specifically, a second voltage, which differs from the first voltage by a predetermined minimum value, is applied to the second probe pad.
7. The semiconductor device according to claim 1, in, The substrate includes a chip region and a scribe region, the scribe region being located around the chip region, and The first test pad is located in the chip area.
8. The semiconductor device according to claim 1, further comprising: The second test pad is located on the same layer as the first bonding pad and is spaced apart from the first test pad. The second test pad includes a third pad portion, a fourth pad portion spaced apart from the third pad portion, and a second connection portion connecting the third pad portion and the fourth pad portion. A third probe pad is connected to the third pad portion via a test contact disposed on the third pad portion; and The fourth probe pad is connected to the fourth pad portion via a test contact disposed on the fourth pad portion.
9. The semiconductor device according to claim 8, further comprising: A first bonding insulating layer surrounds the side of the first bonding pad; and A second bonding insulating layer is bonded to the first bonding insulating layer. The second test pad is in contact with the bottom surface of the second bonding insulating layer.
10. The semiconductor device according to claim 8, further comprising: A first bonding insulating layer surrounds the side of the first bonding pad; and A second bonding insulating layer is bonded to the first bonding insulating layer. The second test pad is spaced apart from the second bonding insulating layer.
11. The semiconductor device according to claim 8, further comprising: A first dummy bonding pad is disposed between the test contact and the third pad portion and is connected to the third pad portion; as well as The second dummy bonding pad is disposed between the test contact and the fourth pad portion and is connected to the fourth pad portion.
12. The semiconductor device according to claim 11, in, The first dummy bonding pad and the second dummy bonding pad are in contact with the top surface of the second test pad.
13. The semiconductor device according to claim 11, in, The first dummy bonding pad and the second dummy bonding pad are spaced apart from the second test pad.
14. A semiconductor device, comprising: A first semiconductor structure includes a first surface and a second surface opposite to the first surface in a direction perpendicular to the first surface; and A second semiconductor structure, bonded to the first semiconductor structure, includes a third surface in contact with the second surface of the first semiconductor structure and a fourth surface opposite to the third surface in a direction perpendicular to the third surface. The second semiconductor structure includes: A first test pad is disposed on the third surface and includes a first pad portion, a second pad portion spaced apart from the first pad portion, and a first connection portion connecting the first pad portion and the second pad portion; A first probe pad, disposed on the fourth surface and connected to the first pad portion via a first test contact disposed on the first pad portion; and A second probe pad is disposed on the fourth surface and connected to the second pad portion via a second test contact disposed on the second pad portion.
15. The semiconductor device according to claim 14, in, The first semiconductor structure includes: A second test pad is disposed on the second surface and includes a third pad portion, a fourth pad portion spaced apart from the third pad portion, and a second connection portion connecting the third pad portion and the fourth pad portion. The second test pad is spaced apart from the first test pad. The second semiconductor structure further includes: A third probe pad, disposed on the fourth surface and connected to the third pad portion via a third test contact disposed on the third pad portion; and A fourth probe pad is disposed on the fourth surface and connected to the fourth pad portion via a fourth test contact disposed on the fourth pad portion.
16. A method for detecting bonding defects in a semiconductor device, the semiconductor device comprising: The first bonding pad is located on the substrate; The second bonding pad is bonded to the first bonding pad; The method includes a first test pad, which is located on the same layer as the second bonding pad and has a first pad portion and a second pad portion spaced apart from each other. A first voltage is applied to the first probe pad that is connected to the first pad portion; A second voltage, different from the first voltage, is applied to a second probe pad that is partially connected to the second pad; and Whether a bonding defect has occurred is determined by calculating the first sheet resistance value of the first test pad based on the current value between the first probe pad and the second probe pad.
17. The method according to claim 16, in, Determining whether a bonding defect has occurred by calculating the first sheet resistance value includes: when the first sheet resistance value is less than 95% of the first reference value or greater than 105% of the first reference value, it is determined that a bonding defect has occurred in the second bonding pad.
18. The method according to claim 17, in, The first reference value is the sheet resistance of the first test pad when the entire bottom surface of the first test pad is in the same plane as the bottom surface of the bonding insulation layer surrounding the side of the first test pad.
19. The method according to claim 17, in, The semiconductor device further includes a second test pad, which is located on the same layer as the first bonding pad and includes a third pad portion and a fourth pad portion spaced apart from each other. The method further includes: The first voltage is applied to the third probe pad that is partially connected to the third pad. Apply the second voltage to the fourth pad portion; and Whether a bonding defect has occurred is determined by calculating the second block resistance value of the second test pad based on the current value between the third probe pad and the fourth probe pad.
20. The method according to claim 19, wherein, Determining whether a bonding defect has occurred by calculating the second block resistance value includes: when the second block resistance value is less than 95% of the first reference value or greater than 105% of the first reference value, it is determined that a bonding defect has occurred in the first bonding pad.
Citation Information
Patent Citations
Portable holder for pets