Methods and apparatus for laser welding
By dynamically adjusting the power distribution between the core and ring regions of the laser spot during laser welding, the problem of inconsistent welding depth and quality under different welding conditions is solved, achieving an efficient and flexible laser welding process, reducing spatter and porosity, and shortening welding time.
Patent Information
- Application Number
- CN202580025346.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-04-05
- Filing Date
- 2025-03-18
- Publication Date
- 2026-11-10
AI Technical Summary
Existing laser welding technology struggles to maintain consistent welding depth and quality under different welding speeds and conditions, especially when machining along the primary direction and transverse directions, where the process is time-consuming and prone to spatter and porosity.
By dynamically adjusting the power distribution between the core and ring regions of the laser spot, the laser power is adjusted in real time according to changes in welding conditions. Optical multi-fiber and wedge beam splitter or laser module are used to adjust the power distribution, and the welding process is optimized by combining measurement equipment and artificial intelligence.
It achieves consistent weld depth and quality under different welding conditions, reduces spatter and porosity, shortens welding process time, and improves welding flexibility and efficiency.
Smart Images

Figure CN123076464A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to methods and apparatus for laser welding. It also relates to computer-readable storage media, computer program products, and data carrier signals. Background Technology
[0002] It is well known that in laser welding, laser power is increased during processing along the primary direction (Vorzugsrichtung) to reduce process time. Furthermore, it is well known that laser power is reduced during processing transverse to the primary direction, such as when moving at corners, to ensure a constant power input to the workpiece based on the reduced welding speed, or feed rate. That is, it should be ensured that a consistent weld depth is maintained even at different welding speeds. Summary of the Invention
[0003] The present invention aims to provide a laser welding method with shorter process time and consistent processing quality, particularly when processing along the primary direction and transversely to the primary direction.
[0004] The object of the present invention is achieved by a method having the features of claim 1. The method for laser welding at least two workpieces includes the following steps: Provide the first workpiece and the second workpiece.
[0005] At least one laser spot is generated on a first workpiece and / or a second workpiece, wherein the at least one laser spot has a core region that is particularly circular and a ring region that is particularly annular, preferably surrounding the core region.
[0006] The at least one laser spot is moved at a welding speed over the first and second workpieces to create a molten pool. Preferably, heat is introduced into the first and / or second workpieces, causing the workpieces to connect to each other along the weld seam.
[0007] The power distribution between the core region and the ring region is changed according to the position of the at least one laser spot on the first workpiece and / or the second workpiece, and / or according to the welding speed of the at least one laser spot, and / or according to at least one welding variable at the position of the at least one laser spot.
[0008] By varying the power distribution, the welding process can be adapted to changing welding conditions, such as laser spot position, welding speed, or welding variations. Therefore, in addition to consistent weld depth, consistent weld quality can be additionally guaranteed, even under varying welding conditions. This method offers exceptional flexibility in laser welding. Furthermore, it allows for the reduction of spatter and porosity.
[0009] It is advantageous to adjust the power distribution during laser welding. This allows for real-time response to changing welding conditions.
[0010] It is also advantageous if the switching time between successive power allocations is at most 20 milliseconds. Due to the short switching time, even short soldering processes, especially those shorter than 1 second, can be effectively adapted.
[0011] According to an extension of this method, the at least one laser spot can be generated using an optical multi-fiber. The optical multi-fiber can be constructed as a 2-in-1 fiber. Preferably, the core-to-loop fiber core diameter ratio is between 1:2 and 1:9, particularly between 1:4 and 1:6. The fiber core diameter is preferably 50 µm, and the fiber loop diameter is preferably 200 µm.
[0012] An advantageous extension of the invention is provided by means of a wedge-shaped beam splitter (Keilweiche) to adjust the power distribution between the core region and the ring region (e.g., see WO2011124671A1).
[0013] The wedge beam splitter can preferably be moved via a stepper motor configured for this purpose, moving over a range of 0 to 100% via up to 80 steps (or positions), particularly up to 60 steps, that can be individually controlled. Here, due to the step size, the step duration between two adjacent steps or positions is, for example, at most t = 360 microseconds. In this way, the wedge beam splitter can be configured such that the switching time between successive power distributions is at most 20 milliseconds.
[0014] The alternative expansion scheme of the present invention is configured to adjust the power distribution between the core region and the ring region by fusing a first input fiber to the core region of the multi-fiber array and fusing at least one second input fiber to at least one ring region of the multi-fiber array. Therefore, the core region and the ring region are supplied by different laser modules (see, for example, WO2014118516A1).
[0015] Preferably, the welding variables include one or more, in particular all, of the following variables: the material of the first workpiece and / or the second workpiece, and / or the workpiece geometry of the first workpiece and / or the second workpiece, and / or the gap width between the first workpiece and the second workpiece, and / or the surface condition of the first workpiece and / or the second workpiece, in particular the average roughness, and / or the occurrence and / or amount of spatter during laser welding, and / or the positional tolerance of the first workpiece and / or the second workpiece, in particular the lateral misalignment of the parts, and / or the total power during laser welding, and / or the focal position of the laser beam, and / or the beam diameter of the laser beam on the first workpiece and / or the second workpiece, and / or the intensity of the laser beam, and / or the energy density of the laser beam.
[0016] When spatter occurs, the power distribution between the core and ring regions can be set to an optimal value related to the material. For materials such as copper, the optimal power ratio between the core and ring regions is in the range of 20:80 to 50:50. It is advantageous if the optimal value can be adjusted.
[0017] It is advantageous to detect the at least one welding variable during laser welding using measuring equipment, particularly optical measuring equipment. Therefore, the process can be adjusted in real time as needed. The measuring equipment can preferably be constructed as a camera-based sensor system, particularly VisionLine Detect. The measuring equipment can record the position and positional deviation of the various components to be welded. Alternatively, an interferometric sensor system, particularly VisionLine OCT Detect, can be used.
[0018] An advantageous extension of the invention involves changing the power distribution between the core and ring regions of the at least one laser spot, as well as altering the total power sum of the core and ring regions of the laser spot. Therefore, the process can be individually adjusted according to local welding requirements or joining conditions.
[0019] Another advantageous extension of the invention involves altering the power distribution when the laser spot's movement speed decreases, resulting in a decrease in the average laser power density in the core region and / or an increase in the average laser power density in the ring region. Therefore, consistent welding results can be achieved even when making sharp or slow turns.
[0020] Another advantageous extension of the invention involves altering the power distribution as the laser spot's movement speed increases, thereby increasing the average laser power density in the core region and / or decreasing the average laser power density in the ring region. This ensures consistent welding results even during rapid longitudinal movement.
[0021] It is advantageous to adjust the power distribution at the beginning of the laser processing so that the average laser power density in the core region is greater than that in the annular region. Alternatively, it is also advantageous to adjust the power distribution at the end of the laser processing so that the average laser power density in the core region is less than that in the annular region. Therefore, optimal welding results can be achieved either at the beginning, particularly with less spatter and a shorter process time, or at the end, particularly with less porosity and a shorter process time.
[0022] It is advantageous to adjust the power distribution so that the average laser power density oscillates between the core and ring regions. This improves the molten pool dynamics.
[0023] Another advantageous extension of the invention involves improving the gap bridging by increasing the laser power density in the annular region and / or decreasing the laser power density in the core region, depending on the gap width between the first and second workpieces. A larger gap width more preferably results in a higher laser power density in the annular region and / or a lower laser power density in the core region. Therefore, optimal bonding results can be achieved even with a large gap width between the first and second workpieces.
[0024] Preferably, in order to improve the gap between the first workpiece and the second workpiece, the power distribution is changed, so that the average laser power density in the core region is reduced and / or the average laser power density in the ring region is increased.
[0025] Furthermore, it is advantageous to use artificial intelligence and / or machine learning to alter the power distribution between the core and ring regions.
[0026] It is advantageous if the core region has multiple core segment regions. It is advantageous if the ring region has multiple ring segment regions. It is advantageous if the core region and the ring region are directly adjacent to each other. Alternatively, it is conceivable to provide a gap separating the core region and the ring region. In the context of this invention, the core region and the ring region relate to laser spots projected onto a workpiece, wherein the core region and the ring region are formed at a focal position on the workpiece.
[0027] Alternatively, it can be envisioned that two overlapping, preferably coaxially arranged, laser spots with different diameters are set to form a core region and a ring region, wherein the core region is set within the overlapping region and the ring region is set outside the overlapping region.
[0028] The object of the present invention is also achieved by a laser welding apparatus for laser welding at least two workpieces, the laser welding apparatus having the features described in claim 13. The laser welding apparatus is configured to perform the method described above.
[0029] To generate a laser spot, a beam quality of less than or equal to 4 mm SPP (beam parameter product) can be used. mrad (millimeters) A laser with a radius of milliradians (milliradians).
[0030] To generate a laser spot, a multimode NIR (near-infrared) laser with a power greater than or equal to 4 kW, particularly greater than 8 kW, and preferably 12 kW, can be used.
[0031] Alternatively, lasers with wavelengths in the visible light range (VIS lasers), especially green or blue, can be used.
[0032] According to an extended version of the method, the at least one laser spot can be moved by means of a scanner optics device. The scanner optics device can have an imaging ratio of 1.7:1. The scanner optics device can preferably be equipped with an optical sensor, such as a camera device. Accordingly, gap tolerances or positional deviations can be identified, thereby allowing for real-time adjustment of power distribution. The scanner optics device can preferably be constructed to be ultra-lightweight to reduce non-productive time.
[0033] This method is advantageous if used for welding hair clips and / or battery casings.
[0034] The object of the present invention is also achieved by a computer-readable storage medium having the features of claim 14. For this purpose, the computer-readable storage medium includes a command that, when executed by a computer, causes the computer to perform the described method.
[0035] The object of the present invention is also achieved by a computer program product having the features of claim 15. This computer program product includes commands that, when executed by a computer, cause the computer to perform the methods described above.
[0036] The object of the present invention is also achieved by a data carrier signal having the features of claim 16. This data carrier signal transmits and / or characterizes the aforementioned computer program product.
[0037] The specification also includes the use of laser welding methods in welding processes shorter than 5 s, particularly shorter than 3 s, preferably shorter than 2 s, and most preferably shorter than 1 s.
[0038] Further details and advantageous embodiments of the invention can be found in the following description, which further describes and illustrates exemplary embodiments of the invention. Attached Figure Description
[0039] Figure 1 A schematic top view of the workpieces to be joined is shown; Figure 2 It shows that according to Figure 1 A schematic side view of the workpieces to be joined; Figure 3 It shows that according to Figure 1 and Figure 2 The graph shows the power curves of the core and ring regions, as well as the welding speed of the laser spot. Detailed Implementation
[0040] To illustrate the method according to the present invention, Figure 1 and Figure 2 The diagram illustrates, by way of example, a first workpiece 10 and a second workpiece 12 that should be welded to each other. The first workpiece 10 also has a first base section 10A and a first cover section 10B, which should also be welded to each other. The second workpiece 12 also has a second base section 12A and a second cover section 12B, which should also be welded to each other. Alternatively, it may be conceivable that workpieces 10 and 12 are integrally constructed and should be welded to each other, and / or that base sections 10A, 12A and cover sections 10B, 12B should be welded to each other. In this case, base sections 10A, 12A can form the first workpiece, and cover sections 10B, 12B can form the second workpiece.
[0041] In laser welding, a laser beam 14 is used to generate a laser spot 16 on a first workpiece 10 and / or a second workpiece 12. The laser beam 14 is configured such that the laser spot 16 projected onto the first workpiece 10 and / or the second workpiece 12 has a circular core region 18 and an annular region 20 surrounding the core region 18.
[0042] exist Figure 2 In the diagram, laser beam 14 is shown in a simplified form, with core region 18 and ring region 20 already formed along laser beam 14. It is conceivable that core region 18 and ring region 20 are formed in this manner only at the focal point, or in other words, within laser spot 16, and are formed particularly clearly separated. Along laser beam 14, the two regions 18 and 20 may overlap and become blurred.
[0043] Laser spot 16 at welding speed v (e.g. Figure 3 (As shown) it moves on the first workpiece 10 and the second workpiece 12. The energy input of the laser beam 14 generates a molten pool 22. Figure 1 and Figure 2The welding process is illustrated at different time points t0 to t7, where the laser spot 16 is positioned at different locations. The laser spot 16 travels from the upper left (t0) to the upper right (t2) and crosses the gap 24 (t1) between the first workpiece 10 and the second workpiece 12. The laser spot 16 then performs a corner movement (t2). The laser spot then travels along the primary direction (t3) to the lower right (t4). The corner movement (t4, t6), gap crossing (t5), and primary direction (t7) are repeated until a full circle is completed.
[0044] Different time points in the welding process are characterized by different welding variables. The requirements differ at the start of the welding process (t0), at the end of the welding process (after t7), during the gap bridging (t1, t5), and / or during corner movement (t2, t4, t6).
[0045] According to the present invention, during laser welding, the power distribution between the core region 18 and the ring region 20 is adjusted according to position and / or time and / or at least one welding variable. Figure 3 The variation of power distribution over time is shown. Alternatively, the power distribution can be plotted with respect to location, where one or more coordinates are projected on the y-axis. These two variations can be used together in this method, or they can be used separately.
[0046] Power distribution is preferably determined by the average laser power density of the core region 18 (hereinafter referred to as core power P). K The average laser power density of the ring region 20 (hereinafter referred to as the ring power P) R The ratio between ) is used to determine this.
[0047] Workpieces 10, 12 and / or the welding process are configured to cause welding variables to change rapidly, particularly at time intervals of less than 50 milliseconds, and especially less than 30 milliseconds. Therefore, it is advantageous if the switching time between two successive power distributions of the core power and ring power is at most 20 milliseconds. The welding process (after t1 to t7) can preferably last for a maximum of 3 seconds, particularly a maximum of 2 seconds, and preferably a maximum of 1 second.
[0048] At time point t0, the welding speed v is 0. For this reason, if the core power P in core region 18... K The ring power P in ring region 20 is greater than R That would be advantageous.
[0049] The welding speed v is increased until time point t1, at which time gap 24 is bridged. To improve the gap bridging of gap 24, if the ring power P in ring region 20... R A core power PK greater than that in core region 18 is advantageous. Here, the core power P of core region 18...K The ring power P in ring region 20 R The total power of the sum of these is at least essentially constant.
[0050] At time point t2, a corner movement is performed, during which the welding speed v decreases. Due to the changing welding speed v, if the core power P... K Greater than the ring power P R That would be advantageous.
[0051] At time point t3, the welding speed v reaches its maximum value because the laser beam moves in a straight line along the primary direction. Due to the higher welding speed v, it is advantageous if the power in the core region 18 is greater than the power in the ring region 20. Furthermore, it is advantageous if the total power increases compared to the start of the welding process (t0) and / or gap bridging (t1) and / or corner movement (t2).
[0052] Preferably, the core power P can also be set at other time points (t4 to t7). K With ring power P R Changes in power distribution between them.
[0053] Furthermore, at the end of the welding process (after t7), if the ring power P R Greater than core power P K That would be advantageous.
[0054] exist Figure 3 As shown, between time points t4 and t5, in order to improve molten pool dynamics, the core power P... K And ring power P R Oscillation. If the core power P K With the ring power P R The same magnitude of oscillation is advantageous. In this case, the power distribution is variable, but the total power is constant. It can also be envisioned that the core power P... K It will briefly exceed the ring power P R Furthermore, it can be envisioned that power distribution and / or ring power P R and / or core power P K And / or the total power may oscillate. Such oscillations can preferably also be set at other points in time.
[0055] exist Figure 1 and Figure 2In this design, the first workpiece 10 and the second workpiece 12 are made of the same material. Therefore, the power curves and welding speed curves v for the first workpiece 10 (i.e., t0 to t1 and t5 to t7) and the second workpiece 12 (i.e., t1 to t5) are identical in terms of the corresponding welding variables. Alternatively, it can be envisioned that these workpieces are made of different materials, such that the power distribution and / or total power for the corresponding workpieces 10 and 12, or rather, the materials of workpieces 10 and 12, will vary. The power distribution and / or total power can also be adjusted based on variations in workpiece geometry and / or gap width and / or surface condition, and / or when spatter occurs and / or when there is a maximum amount of spatter.
[0056] To obtain the at least one welding variable in real time, an optical and / or tactile measuring device (not shown) may preferably be provided. Furthermore, a control unit (not shown) may be provided, configured to adjust the power distribution and / or total power of the core region 18 and the ring region 20 during laser welding based on the at least one welding variable detected by the measuring device, with a maximum switching time of 20 milliseconds.
Claims
1. A method for laser welding at least two workpieces (10, 12), comprising the following steps: - Provide the first workpiece (10) and the second workpiece (12); - Generate at least one laser spot (16) on the first workpiece (10) and / or the second workpiece (12), wherein the at least one laser spot (16) has a core region (18) and a ring region (20), the core region being particularly circular and the ring region being particularly annular; - Move the at least one laser spot (16) over the first workpiece (18) and the second workpiece (20) at a welding speed (v) to generate a molten pool (22). - The power distribution between the core region (18) and the ring region (20) is changed according to the position of the at least one laser spot (16) on the first workpiece (10) and / or the second workpiece (12), and / or according to the welding speed (v) of the at least one laser spot (16), and / or according to at least one welding variable at the position of the at least one laser spot (16).
2. The method according to claim 1, wherein, The power distribution is adjusted during laser welding.
3. The method according to claim 1 or 2, wherein, The maximum switching time between successive power allocations is 20 milliseconds.
4. The method according to claim 1, 2 or 3, wherein, The power distribution between the core region (18) and the ring region (20) is adjusted by means of a wedge beam splitter.
5. The method according to claim 1, 2 or 3, wherein, The first input fiber is fused to the core region (18) of the multi-fiber, and at least one second input fiber is fused to at least one loop region (20) of the multi-fiber, wherein the power distribution between the core region (18) and the loop region (20) is adjusted by changing the power at the respective input fiber.
6. The method according to any one of the preceding claims, wherein, The at least one welding variable includes one or more, and in particular all of, the following variables: - The materials of the first workpiece (10) and / or the second workpiece (12), - The workpiece geometry of the first workpiece (10) and / or the second workpiece (20), - The gap width between the first workpiece (10) and the second workpiece (12), - The surface condition of the first workpiece (10) and / or the second workpiece (12), - The presence and / or amount of spatter during laser welding. - Positional tolerances of the first workpiece (10) and / or the second workpiece (12), particularly lateral component misalignment. - Total power during laser welding - The focal position of the laser beam (14), - The beam diameter of the laser beam (14) on the first workpiece (12) and / or the second workpiece (20), - The intensity of the laser beam (14), - Energy density of the laser beam (14).
7. The method according to any one of the preceding claims, wherein, During laser welding, at least one welding variable is detected by means of measuring equipment, particularly optical and / or tactile measuring equipment.
8. The method according to any one of the preceding claims, wherein, When the power distribution of the core region (18) and the ring region (20) of the at least one laser spot (16) is changed, the total power, which is the sum of the power of the core region (18) and the ring region (18) of the at least one laser spot (16), is also changed.
9. The method according to any one of the preceding claims, wherein, When the speed (v) of the laser spot (16) decreases, the power distribution is changed, such that the average laser power density in the core region (18) decreases and / or the average laser power density in the ring region (20) increases.
10. The method according to any one of the preceding claims, wherein, When the speed (v) of the laser spot (16) increases, the power distribution is changed, such that the average laser power density in the core region (18) increases and / or the average laser power density in the ring region (20) decreases.
11. The method according to any one of the preceding claims, in, At the start of the laser processing, the power distribution is adjusted such that the average laser power density in the core region (18) is greater than the average laser power density in the ring region (20), and / or At the end of the laser processing process, the power distribution is adjusted such that the average laser power density in the core region (18) is less than the average laser power density in the ring region (20).
12. The method according to any one of the preceding claims, wherein, The power distribution is adjusted such that the average laser power density oscillates between the core region (18) and the ring region (20).
13. The method according to any one of the preceding claims, wherein, To improve the gap bridging, the laser power density in the ring region (20) and / or the laser power density in the core region (18) are increased and / or decreased according to the gap width between the first workpiece (10) and the second workpiece (12).
14. The method according to any one of the preceding claims, wherein, Artificial intelligence and / or machine learning are used to change the power distribution between the core region (18) and the ring region (20).
15. A laser welding apparatus for laser welding at least two workpieces (10, 12), wherein, The laser welding apparatus is configured to perform the method according to any one of the preceding claims.
16. A computer-readable storage medium comprising commands that, when executed by a computer, cause the computer to perform the method according to at least one of claims 1 to 14.
17. A computer program product comprising commands that, when executed by a computer, cause the computer to perform the method according to at least one of claims 1 to 14.
18. A data carrier signal, said data carrier signal transmitting and / or characterizing the computer program product according to claim 17.
Citation Information
Patent Citations
Method and arrangement for generating a laser beam having a differing beam profile characteristic by means of a multi-clad fibre
WO2011124671A1
Fibre optical laser combiner
WO2014118516A1