A white-based photosensitive printing pad and its preparation method
By preparing a white-based photosensitive ink pad with a white body, the problem of the stamp surface being difficult to display color was solved, the ink color was made visible, and the stamp's recognizability was improved.
Patent Information
- Application Number
- CN202611285307.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-24
- Publication Date
- 2026-11-17
AI Technical Summary
The existing seals have a black surface, making it difficult to display other colors, which makes them hard to distinguish when there are many seals.
A white substrate is made from polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silica, white sugar and polymeric dispersant. The substrate is then mixed, extruded, dried, sliced and exposed to film to form a white-based photosensitive printing pad.
The seal surface is white, but the color will appear after the ink is applied, making it easy to distinguish.
Smart Images

Figure CN123104262A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of seal manufacturing technology, and more specifically to a white-based photosensitive ink pad and its preparation method. Background Technology
[0002] Currently, the seals on the market have black or light gray surfaces, which makes them difficult to distinguish once you have a lot of seals (because the surface does not display color).
[0003] Secondly, traditional stamp pads, through processes such as ingredient mixing, intensive mixing, crushing, granulation, drying, screw extrusion (mostly single-screw extrusion), soaking in water, air drying, and then exposure (using photosensitive stamp machines), produce a black stamp surface. Even after adding ink, the stamp surface remains black and does not display any other colors.
[0004] Traditional photosensitive stamp pads use strobe lamps to emit light, and the pad body uses carbon black to absorb heat and form an image. The pad body itself remains black, and the ink color will not be displayed after ink is added. Summary of the Invention
[0005] The purpose of this invention is to overcome the shortcomings of the prior art and provide a white photosensitive printing pad and its preparation method. The main body of the pad is white, so that its printing surface is white. When printing ink is injected into the main body of the pad, the white printing surface will display the color of the printing ink, which makes it easy to distinguish intuitively.
[0006] The solution of the present invention to the aforementioned technical problem is:
[0007] A white-based photosensitive printing pad includes a body composed of polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silica, white sugar, and a polymeric dispersant.
[0008] The main body contains 21% to 24% polyethylene resin, 2% to 3% dimethyl silicone oil, 0.5 parts per thousand infrared absorber, 1% to 2% glycerol, 0.5% to 0.75% silicon dioxide, 75% to 78% white sugar, and 0.1 parts per thousand polymeric dispersant.
[0009] A method for manufacturing a white-based photosensitive printing pad includes the following steps:
[0010] (1) Pour polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silicon dioxide, white sugar and polymeric dispersant into a high-speed mixer and mix and stir into powder;
[0011] (2) Pour the powder from step (1) into a twin-screw extruder and extrude the profile material;
[0012] (3) Soak the extruded material in water and then dry it;
[0013] (4) Slice the dried material to form slices;
[0014] (5) Expose one end of the slice through film to form the pattern required for the stamp, thus completing the processing.
[0015] The outstanding effects of this invention are:
[0016] Compared to existing technologies, its body is white, making its printing surface white. When ink is injected into the printing pad body, the white printing surface will display the color of the ink, making it very easy to distinguish. Attached Figure Description
[0017] Figure 1 This is a partial structural diagram of the conveyor belt section of the present invention;
[0018] Figure 2 yes Figure 1 A magnified view of a portion of the image;
[0019] Figure 3 This is a partial structural diagram of the conveyor belt. Detailed Implementation
[0020] For example, see below. Figures 1 to 3 As shown, a white-based photosensitive printing pad includes a body composed of polyethylene resin (in this embodiment, Mitsui Chemicals DF840 or Wanhua 5308 is used, which has the characteristics of high flow (high) MR index 30 and high temperature resistance), dimethyl silicone oil (500cs), infrared absorber (880nm), glycerin (food grade, such as Coconut Palm brand can be used), silica (A200), white sugar, and a polymeric dispersant (Span S80 dispersant).
[0021] The main body contains 21% to 24% polyethylene resin, 2% to 3% dimethyl silicone oil, 0.5 parts per thousand infrared absorber, 1% to 2% glycerol, 0.5% to 0.75% silicon dioxide, 75% to 78% white sugar, and 0.1 parts per thousand polymeric dispersant.
[0022] A method for manufacturing a white-based photosensitive printing pad includes the following steps:
[0023] (1) Pour polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silicon dioxide, white sugar and polymeric dispersant into a high-speed mixer and mix and stir into powder;
[0024] (2) Pour the powder from step (1) into a twin-screw extruder and extrude the profile material;
[0025] (3) Soak the extruded material in water and then dry it;
[0026] (4) Slice the dried material to form slices;
[0027] (5) Expose one end of the sliced body to film so that the pattern required for the stamp is formed on this end, and the processing is completed. At this time, the whole body is white.
[0028] In step (1), the high-speed mixer is heated to 100 degrees. First, slow stirring is started and stirred for 1 to 2 minutes to make the material evenly mixed. Then, the high-speed crushing function is started to make the material rub at high speed under high temperature. The running time is 6 to 8 minutes.
[0029] Note that if the current indicator of the high-speed mixer reaches or approaches 30A during operation, the material should be immediately unloaded, spread out and allowed to cool naturally. The material should only proceed to the next process (i.e., into the twin-screw extruder) when the material temperature is below 50 degrees Celsius.
[0030] In step (2), the material extruded by the twin-screw extruder through the die is pushed onto the conveyor belt, where forced air cooling is applied to both the top and bottom of the conveyor belt, and the cooled material is placed into a plastic basket.
[0031] In this embodiment, the conveyor belt structure includes a frame, two drive shafts located between the front and rear side plates of the frame, the two ends of the drive shafts being movably connected to the front and rear side plates of the frame via bearings, a drive roller 10 fixed in the middle of the two drive shafts, a conveyor belt 11 tensioned on the two drive rollers 10, a motor frame fixed on the outer side wall of one side plate of the frame, a drive motor fixed thereon, one end of the drive shaft extending out of the outer side wall of the side plate of the frame and fixed to the output shaft of the drive motor via a coupling, a plurality of front and rear extending air guide grooves 12 formed on the conveyor belt 11, a middle support plate 13 located between the front and rear side plates of the frame, the front and rear side walls of the middle support plate 13 fixed to the inner side walls of the two side plates, the middle support plate 13 located between the upper belt body and the lower belt body of the conveyor belt 11, a plurality of fan frames fixed on the top surface of the middle support plate 13, a lower fan 14 fixed on the fan frame, its air outlet facing the bottom surface of the upper belt body of the conveyor belt 11;
[0032] Multiple upper support frames 20 are fixed on the top surface of the two side plates. An upper rotary motor 21 is fixed in the middle of the top surface of the top plate of the upper support frame 20. The bottom end of the rotating shaft of the upper rotary motor 21 extends out of the bottom surface of the top plate of the upper support frame 20 and is movably connected to the top of the lower support frame through a hinge shaft. A horizontal plate is fixed at the bottom of the lower support frame, and an upper ventilator 22 is fixed on it. The air outlet of the upper ventilator 22 faces the top surface of the upper belt of the conveyor belt 11 below.
[0033] One side of the horizontal plate is movably connected to the bottom connecting block of the electric push rod 30 via a hinge shaft. The top of the push rod of the electric push rod 30 is movably connected to the moving block 31 via a hinge shaft. The top surface of the moving block 31 is fixed with a sliding ball 32. The bottom surface of the top plate of the upper support frame 20 is fixed with an annular guide rail 23. An annular groove is formed in the middle of the bottom surface of the annular guide rail 23. The inner sidewall of the annular groove is larger than a semi-circular arc surface. A self-lubricating layer 24 is fixed on its inner sidewall. The sliding ball 32 is inserted into the annular groove, and its outer sidewall is close to or in close contact with the inner sidewall of the self-lubricating layer 24.
[0034] In use, the upper fan 22 and the lower fan 14 blow air to cool the material placed on the top surface of the conveyor belt 11 in both directions. The upper fan 22 can be rotated horizontally by the shaft of the upper rotary motor 21 and pushed or retracted by the push rod of the electric push rod 30, so that the blowing direction of the upper fan 22 can be changed to meet different blowing requirements.
[0035] After cooling with air, the plastic frame is placed in a stainless steel water tank filled with water, with the water level submerging the plastic frame. The water temperature is controlled below 45 degrees Celsius using a mold temperature controller. After soaking for 48 hours, the water is changed again, and the process is repeated for another 48 hours until the sugar content in the water is below 0.5 grams per 100 ml, which meets the requirements. The sugar content in the water is then tested using a sugar content analyzer, and if it is below 0.5 grams per 100 ml, it meets the requirements.
[0036] In further, the material in the profile shape after drainage in step (3) is squeezed out of water by a double roller machine, and then the material is placed on the corresponding placement layer of the multilayer rack. Each layer of the multilayer rack is placed with a 5mm thick breathable sponge, which is placed at the bottom of the material. Then the multilayer rack is moved into the drying room for baking.
[0037] The drying room is equipped with an industrial dryer. The dryer is set to a temperature not exceeding 55 degrees Celsius. After baking for 18 hours, the relative humidity inside the drying room should be below 18%. The data from the dryer system should be the standard. As long as the humidity is below 18%, it meets the requirements and the drying is complete.
[0038] The dried material is sliced, and the slices are generally made of six standard thicknesses: 2mm, 3mm, 3.5mm, 4mm, 5.5mm and 7mm.
[0039] In this embodiment, the profile-shaped material is generally determined by the shape of the mold forming opening, and conventionally the cross-section is circular, elliptical, or rectangular. It can also be made into irregular shapes as needed.
[0040] The sliced body is the white photosensitive printing pad (at this point, it has many fine pores inside to ensure that ink can flow out). It can then be used to create the pattern to be printed using film exposure. The principle is to attach the film with black text to the corresponding end face of the printing pad body, and then expose it (using a high-frequency xenon lamp). The areas without black text melt due to the heat absorbed by the high-frequency xenon lamp, sealing all the pores. Then, the film is removed. Ink can flow out from the end face of the pad where the black text is, but not from the rest, thus allowing the pattern to be printed. The exposed end face is concave inwards, making the end face of the pad where the black text is located approximately 0.2mm higher than the rest.
[0041] Finally, the above embodiments are only used to illustrate the present invention and are not intended to limit the present invention. Those skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, all equivalent technical solutions also fall within the scope of the present invention, and the patent protection scope of the present invention should be defined by the claims.
Claims
1. A white-based photosensitive printing pad, comprising a body, characterized in that: The main body is composed of polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silicon dioxide, white sugar and polymeric dispersant.
2. The white-based photosensitive printing pad according to claim 1, characterized in that: The main body contains 21% to 24% polyethylene resin, 2% to 3% dimethyl silicone oil, 0.5 parts per thousand infrared absorber, 1% to 2% glycerol, 0.5% to 0.75% silicon dioxide, 75% to 78% white sugar, and 0.1 parts per thousand polymeric dispersant.
3. A method for manufacturing a white-based photosensitive printing pad according to any one of claims 1 or 2, characterized in that: Includes the following steps: (1) Pour polyethylene resin, dimethyl silicone oil, infrared absorber, glycerin, silicon dioxide, white sugar and polymeric dispersant into a high-speed mixer and mix and stir into powder; (2) Pour the powder from step (1) into a twin-screw extruder and extrude the profile material; (3) Soak the extruded material in water and then dry it; (4) Slice the dried material to form slices; (5) Expose one end of the slice through film to form the pattern required for the stamp, thus completing the processing.
4. The method for manufacturing a white-based photosensitive printing pad according to claim 3, characterized in that: In step (1), the high-speed mixer is heated to 100 degrees, and the slow stirring is started first. The stirring lasts for 1 to 2 minutes to make the material evenly mixed. Then the high-speed crushing function is started to make the material rub at high speed under high temperature. The running time is 6 to 8 minutes.
5. A white-based photosensitive printing pad according to claim 3, characterized in that: In step (2), the material extruded by the twin-screw extruder through the die is pushed onto the conveyor belt, where forced air cooling is applied to both the top and bottom of the conveyor belt, and the cooled material is placed into a plastic basket.
6. A white-based photosensitive printing pad according to claim 5, characterized in that: The plastic frame is placed in a stainless steel water tank, and the tank is filled with water. The water level should be enough to submerge the plastic frame. The water temperature is controlled below 45 degrees Celsius using a mold temperature controller. After soaking for 48 hours, the water is changed again. This process is repeated for another 48 hours until the sugar content in the water is less than 0.5 grams per 100 ml, which meets the requirements.
7. A white-based photosensitive printing pad according to claim 3, characterized in that: In step (3), the material in the shape of the profile after drainage is squeezed out of water by a double roller machine. Then the material is placed on the corresponding layer of the multilayer rack. Each layer of the multilayer rack is placed with a 5mm thick breathable sponge, which is placed under the material. Then the multilayer rack is moved into the drying room for baking.
8. A white-based photosensitive printing pad according to claim 3, characterized in that: The drying room is equipped with an industrial dryer. The dryer is set to a temperature not exceeding 55 degrees Celsius. After 18 hours of continuous baking, the relative humidity inside the drying room should be below 18%, based on the data from the dryer system.
9. A white-based photosensitive printing pad according to claim 6, characterized in that: The sugar content in the stainless steel water tank is detected by a sugar content detector, and it is considered to meet the requirements if it is less than 0.5 grams per 100ml.