A manual preparation process for silk paintings

By employing low-temperature processing and multi-layer stacking techniques, combined with plant-based adhesives and preservatives, the problems of limited color and form in traditional silk paintings have been solved. This has resulted in richer colors and three-dimensional effects in silk paintings, along with anti-mildew and anti-insect properties, thus enhancing the artistic value and preservation quality of silk paintings.

CN123104273APending Publication Date: 2026-11-17程衍峰
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611300828.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-26
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional silk painting techniques suffer from insufficient color gradation, limited production methods, inadequate representation of the natural luster of silk, monotonous product forms, and a lack of anti-mildew and anti-insect treatments.

Method used

Low-temperature cocoon boiling and silk reeling processes preserve the luster of the silk. Plant-based adhesives are used to adhere the silk, which is then dyed and treated with dyes and preservatives for mildew and insect prevention. The artistic expression is enhanced through multi-layer stacking and three-dimensional sculpting techniques.

Benefits of technology

This technology has enabled silk paintings to achieve rich colors, strong three-dimensionality, and anti-mildew and anti-insect properties, thereby enhancing the artistic appeal and lifespan of the works.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a manual preparation process for silk paintings, including the following steps: obtaining silk floss by boiling cocoons at a low temperature of 75-80℃, and obtaining silk by reeling silk at a low temperature of 65-80℃. The silk and silk floss are then dyed for later use. A special glue is prepared by boiling a mixture of 10L water, 50-100g plant glue, 5-10g potassium sorbate, 5-10ml camphor oil, 30-50g chitosan, and 20-40g glycerin in a water bath to form a base coating. Linen or silk is fixed to a wooden canvas as a base. Silk, silk floss, and cocoon shells are laid out and shaped using either flat or three-dimensional stacking of silk. The surface of the finished silk painting is then soaked and sprayed with a mixture of camphor oil, chitosan, glycerin, and water at room temperature for anti-mildew and anti-insect treatment. This invention utilizes low-temperature cocoon boiling and silk reeling processes to retain more sericin in the silk, resulting in silk with good toughness and high luster. By stacking multiple layers of silk or silk floss, a three-dimensional relief effect can be created. The techniques are diverse and can be used to make flat, relief, and three-dimensional silk-shaped products, which also have anti-mildew and anti-insect properties.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of cultural and creative craft processing technology using silk, silk floss, and silkworm cocoon shells, specifically to a manual preparation process for silk paintings. Background Technology

[0002] Traditional silk painting techniques use readily available silk from the market. The silk is dyed and then directly adhered to a substrate with synthetic glue before the design is laid flat. This technique has several drawbacks: First, the single-layer flat application results in a lack of depth, limited color palette, coarse texture, and limited artistic expression. Second, the limited techniques make it difficult to achieve complex shapes and textures. Third, the high-temperature treatment and application of synthetic glue damage the natural luster of the silk, resulting in an imperfect and unnatural sheen. Fourth, traditional techniques can only produce flat silk paintings, failing to achieve relief effects or three-dimensional forms, leading to a limited product range. Fifth, the lack of effective anti-mold and anti-insect treatments makes the finished products susceptible to mold and insect damage during long-term storage, affecting the artwork's lifespan and aesthetic value.

[0003] Therefore, there is an urgent need to develop a silk painting preparation process that can preserve the natural luster and toughness of silk, produce rich color layers in the image, realize various forms such as flat, relief, and three-dimensional, and has anti-mildew and anti-insect properties. Summary of the Invention

[0004] In view of the shortcomings of existing technologies, such as insufficient color gradation, monotonous production techniques, inadequate representation of the natural luster of silk, limited product form, and lack of anti-mildew and anti-insect treatment, the purpose of this invention is to provide a manual preparation process for silk paintings.

[0005] To achieve the above objectives, the present invention is implemented through the following technical solution: a manual preparation process for silk paintings, comprising the following steps: 1. Obtaining silk, silk floss, and cocoon shells: Silkworm cocoons are selected as raw materials. Rotten and moldy cocoons are removed. The cocoons are then processed through low-temperature boiling, unwinding, and low-temperature reeling. The cocoons are then deflowered to obtain three types of raw materials: raw silk, fluffy silk floss, and cocoon shells. These are then stored separately for later use. At room temperature, the cocoons are boiled in a stainless steel pot at a low temperature of 75-80℃. Silk is then obtained using a low-temperature reeling machine at a water temperature of 65-80℃. The cocoons with the pupae removed are then sterilized at high temperature in a pressure cooker before being used directly. 2. Dyeing and anti-mildew / insect-proofing treatment of silk raw materials: The silk or silk floss obtained through the above process is placed in a water container with added surfactant and degreased and rinsed at a water temperature of 55-70℃ for 20 minutes; then the degreased silk or silk floss is placed in an aqueous solution with added dye and heated for dyeing at a bath temperature of 45-60℃. The dyeing process lasts for 40-50 minutes, during which the silk is gently turned to ensure even coloring. Once the dyed silk is fully colored, add a color-fixing agent and fix the color for 15 minutes. When the temperature cools naturally to room temperature, remove the silk and gently rinse it with room temperature water for the first time to remove any excess color. For the second rinse, add the prepared preservatives chitosan, citric acid, and camphor oil (liquor ratio: 10L water: 45g chitosan: 10g citric acid: 10ml camphor oil) to a container of water. Then add the silk or silk floss to be rinsed and soak for 20 minutes, gently turning and rinsing three times during this time. After rinsing, place the silk in a ventilated area to air dry naturally. The cocoon shells can be dyed or left to retain their original color depending on the needs of the artwork. 3. Preparation of silk painting glue: Using plant gum, the mixture consists of 10L water, 50-100g plant gum, 5-10g potassium sorbate, 5-10ml camphor essential oil, 30-50g chitosan, and 20-40g glycerin. It is then simmered in a ceramic or stainless steel container over a water bath for 40 minutes. The mixture is then filtered repeatedly through multiple layers of gauze to remove impurities and cooled to form a gel. When needed, it is dissolved in a water bath. 4. Pretreatment of the silk painting substrate Choose linen or silk as the base for your artwork. Evenly coat the surface of the wooden canvas with the glue prepared in step 3. Then, smoothly fix the fabric used as the base onto the wooden canvas, ensuring the surface is flat and wrinkle-free. Secure the sides of the canvas with nails. Once the glue under the fabric has dried completely, you can use silk or cocoon shells to create your artwork. 5. Pre-treatment of the silk 3D sculpture substrate When preparing a three-dimensional silk sculpture, the sculpture substrate is pre-treated. This step can be omitted when creating flat or relief silk paintings. A support base for the sculpture is pre-built, and the substrate material is selected to support the skeleton of the silk sculpture. First, build the shape of the substrate, then remove loose particles, dust and sharp edges from the surface. After cleaning, evenly apply the first layer of primer to the outer surface of the substrate and let it air dry in a ventilated place. Then, cover or apply a transition adhesion layer to make the surface of the substrate moderately rough and let it dry again for later use. 6. Wire fixing and shaping treatment Step 3: Prepare the homemade silk painting glue into a special water-based adhesive. Shape the silk by applying it evenly and lightly, or by spraying the setting glue. Complete the structural shaping of the silk picture by piecing together, crossing, and overlapping each other. Spray the surface layer for shaping. After shaping, place it in a ventilated and cool place to cure and dry naturally at room temperature for 12 to 24 hours. 7. Post-framing After the image has completely dried and stabilized, it is edged and framed to obtain the finished silk painting.

[0006] Preferably, in step 1, a silk reeling solution is used for reeling, which is an aqueous solution containing dried straw ash with a pH value of 6.5 to 7.2.

[0007] Preferably, the adhesive in step 4 is prepared by boiling 10L of water, 150g of plant glue, 8g of potassium sorbate, 5ml of camphor essential oil, 40g of chitosan, and 30g of glycerin in a water bath to make a special adhesive for use as a base coating or for bonding silk, silkworm cocoon shells, and the base.

[0008] The present invention has the following beneficial effects 1. Low-temperature cocoon boiling and silk reeling: Using low-temperature cocoon boiling at 75-80℃ and low-temperature silk reeling at 65-80℃ can retain more sericin on the surface of the silk, making the silk more resilient and lusterier. When multiple layers are stacked, the texture effect is more malleable, the three-dimensionality of the picture is stronger, and the artistic appeal is richer and more direct.

[0009] 2. Raw material dyeing: Dyeing silk and silk floss can be used to create colorful silk paintings, expanding the expressive power of color in the artwork.

[0010] 3. Diverse painting techniques: While retaining the traditional flat tiling, the plasticity of silk and silk floss is used to create multi-layered stacking, giving the image a three-dimensional relief effect. This combines artistry and aesthetics, significantly enhancing the value of the artwork. It also supports painting with a mixture of cocoon shells, silk, and silk floss, as well as painting with cocoon shells independently. The silk floss painting techniques include various methods such as pulling, picking, dragging, twisting, bridging, hanging, tiling, stacking, and multi-color mixing and tearing. It can produce various forms of products such as flat silk paintings, relief silk paintings, and three-dimensional silk sculptures.

[0011] 4. Anti-mildew and anti-insect: Camphor oil and chitosan are used for anti-mildew and anti-insect treatment. Combined with low-temperature impregnation, spraying and air drying at 50-55℃, it effectively prevents mold and insects while avoiding damage to the luster and toughness of silk caused by high temperature, thus extending the shelf life of the product. Detailed Implementation

[0012] To make the technical means, creative features, objectives and effects of this invention easier to understand, the invention will be further described below in conjunction with specific embodiments.

[0013] This specific embodiment adopts the following technical solution: a manual preparation process for silk paintings, including the following steps: 1. Obtaining silk, silk floss, and cocoon shells: Silkworm cocoons are selected as raw materials. Rotten and moldy cocoons are removed. The cocoons are then processed by low-temperature boiling, unwinding, and low-temperature reeling. The silkworm pupae inside the cocoons are removed to obtain three types of cocoon-derived raw materials: raw silk, fluffy silk floss, and intact cocoon shells. These are then classified and stored for later use. The operating environment is indoors at room temperature. The water temperature for boiling silkworm cocoons is 75-80℃ (which can be selectively adjusted according to the toughness of the silk floss). The water temperature for reeling silk is 65-80℃ (which can be selectively adjusted according to the toughness of the silk). Tools used: stainless steel pot and silk reeling machine.

[0014] After removing the cocoon shells from the silkworm pupae, the cocoons are sterilized at high temperature in a pressure cooker and then used directly.

[0015] 2. Dyeing and anti-mildew / anti-moth treatment of silk raw materials: The silk or silk floss obtained through the above process is placed in a water container with added surfactant and degreased and rinsed at a water temperature of 55-70℃ for 20 minutes.

[0016] Next, immerse the degreased silk or silk floss in an aqueous solution containing dye and heat it for dyeing. The water temperature should be 45–60℃. Immerse for 40–50 minutes, gently turning the silk or silk floss during this time to ensure even dyeing. After the dyed silk or silk floss has fully absorbed the color, add a color-fixing agent and fix the color for 15 minutes. Let it cool naturally to room temperature, then remove the silk or silk floss and gently rinse it with room temperature water for the first time to remove any excess color. For the second rinse, treat the silk or silk floss for mold and moth prevention. Add a pre-prepared preservative mixture of chitosan and citric acid (0.3% bath ratio) and camphor oil (for moth prevention) to a container of water. Add the silk or silk floss to the container and soak for 20 minutes, gently turning it over three times during this process. After rinsing, place it in a well-ventilated area to air dry naturally. Do not dry it at high temperatures or expose it to direct sunlight to avoid breaking the silk fibers. The cocoon shell can be dyed or left to retain its original color depending on the artwork's requirements.

[0017] 3. Preparation of silk painting glue: The core requirements for silk painting glue are: it should not be brittle, should not turn yellow, and should not damage the luster of the silk. It should be able to firmly adhere the fibers when laying the silk. Silk is a protein fiber, which is highly susceptible to insect infestation and mold. There are two solutions: traditional ancient method and modern process.

[0018] Special glue for silk painting is prepared (for applying to the base plate, laying and fixing the silk). Ingredients: 10L water, 50-100g plant gum, 5-10g potassium sorbate, 5-10ml camphor oil, 30-50g chitosan, 20-40g glycerin. Use a ceramic / stainless steel container and cook in a water bath (boiling in water allows for temperature control to prevent burning and loss of flavor).

[0019] The mixture is repeatedly filtered through multiple layers of gauze to remove impurities. It is then cooled to form a gel, which is thawed in a water bath before use.

[0020] 4. Pretreatment of the silk painting substrate Choose linen or silk as the base for your artwork. Apply glue evenly to the surface of the wooden canvas, then smooth and fix the fabric (used as the base) to the canvas, ensuring the surface is flat and wrinkle-free. Secure the sides of the canvas with nails. Once the glue under the fabric has dried completely, you can then use silk, silk floss, or cocoon shells to create your artwork.

[0021] 5. Pre-treatment of the silk 3D sculpture substrate When preparing a three-dimensional silk sculpture, the sculptural substrate undergoes pretreatment. This step can be omitted when creating flat or relief silk paintings.

[0022] A sculpture support base is pre-built. The base material can be any material that can support the silk or silk floss sculpture skeleton, such as: steel wire skeleton, bamboo skeleton, foam base, wooden skeleton, plaster base, composite sculpting skeleton, etc.

[0023] First, build and trim the shape of the substrate, removing loose particles, dust, and sharp edges from the surface. After cleaning, evenly apply the first layer of primer to the outer surface of the substrate and let it air dry naturally in a ventilated place. Then, cover or apply a transition adhesion layer to create a moderately rough adhesion surface on the substrate, and let it dry again for later use.

[0024] The pre-treated sculpting substrate can improve the adhesion of silk, silk floss, and cocoon shell materials. When the silk is laid and shaped, the fibers are less likely to slip or shift, and the finished product is less likely to peel or crack during long-term storage.

[0025] 6. Wire fixing and shaping treatment Based on the pattern lines drawn on the base, water-based adhesive is applied to the base surface using brushing or atomized spraying. Then, the obtained silk, silk floss, or cocoon shell is adhered to the base according to the pattern lines. It is then allowed to cure and dry naturally at room temperature, resulting in a silk painting. The drying time is 12–24 hours, allowing for natural setting without the use of heat or baking.

[0026] 7. Post-framing After the image has completely dried and stabilized, the edges are sealed, sealed (with a sponge), and framed to obtain the finished silk painting.

[0027] The pretreatment of the three-dimensional sculpture substrate in step 5 is as follows: build a three-dimensional sculpture support substrate, trim the edges and corners, remove loose debris from the surface, apply a base coat to the whole, then set a transition adhesion layer, and after it dries, lay silk material layer by layer on the outer surface of the substrate to form a three-dimensional shape.

[0028] In the creative process, silk, silk floss, and cocoon shells can be used individually for painting; they can also be used individually to create three-dimensional sculptures; or they can be mixed and matched to enrich the texture and three-dimensionality of the image.

[0029] This specific implementation method uses silkworm silk and silk floss as the main raw materials for making silk paintings. Silk floss is obtained by boiling cocoons at a low temperature (75-80℃), and silkworm silk is obtained by reeling at a low temperature (65-80℃). The low-temperature process allows for better retention of the sericin on the silk surface, resulting in better toughness and higher luster. In silk painting, multiple layers of silk or silk floss create more malleable textural effects, a stronger three-dimensional effect, and a richer, more direct artistic expression. The obtained silk and silk floss are dyed, allowing for the creation of richly colored silk paintings. This silk painting technique adds diversity to the art form. By utilizing the malleability of silk and silk floss to create multiple layers while maintaining the initial flat surface of the silk, the silk painting can present a three-dimensional relief effect, possessing high artistic and aesthetic value, significantly enhancing the value of the work. This is a clear distinction from ordinary silk paintings.

[0030] Building upon the foundation of creating artworks using silk, silk floss, and cocoon shells independently, techniques have been added to create artworks using a mixture of these materials. Alternatively, cocoon shells, silk, and silk floss can be used as raw materials to create independent artworks, possessing unique aesthetic and artistic value. The painting techniques are diverse, including 72 different methods such as: pulling, picking, dragging, twisting, bridging, hanging, laying flat, stacking, and multi-color mixing and tearing.

[0031] Example 1: Preparation and permeation treatment of low-temperature silk reeling unwinding solution In this embodiment, the silkworm cocoons are subjected to low-temperature unwinding and permeation treatment before silk reeling in step (1), and the unwinding solution is prepared according to the following formula: Using 10L of clean water as a base, add a solution of dried straw ash to prepare a solution with a pH value of 6.5-7.2 to obtain a low-temperature silk reeling unwinding solution.

[0032] Qualified silkworm cocoons are immersed in the above-mentioned solubilizing solution, with the solution temperature controlled at 28–32°C. The solution is then used for permeation under vacuum conditions to ensure it fully penetrates the cocoon layer. After permeation, the cocoons are removed and then reeled at a low temperature of 65–80°C to obtain silk.

[0033] This embodiment uses low-temperature permeation instead of the traditional high-temperature boiling of cocoons to loosen them. The cocoon layer can be fully loosened under the low temperature of 28-32℃, avoiding the excessive dissolution of sericin and damage to silk fibers caused by high temperature. This allows more sericin to be retained on the surface of the silk, resulting in silk with good toughness and high luster, which is more suitable for subsequent multi-layer stacking and shaping, and will not cause problems such as the silk fibers being overcooked or increased silk breakage. Example

[0034] Using 10L of clean water as a base, a solution of dried straw ash was added to adjust the pH to 6.8, resulting in a low-temperature silk reeling solution. Silkworm cocoons were immersed in this solution and treated at a controlled temperature of 30℃ for 15 minutes. After removal, the silk was reeled at a low temperature of 65-80℃. The resulting silk had a high sericin retention rate, intact fibers, and a natural luster.

[0035] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely illustrative of the principles of the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of this invention is defined by the appended claims and their equivalents.

Claims

1. A handcrafting process of silk painting, characterized in that, Includes the following steps: (1). Obtaining silk, silk floss, and cocoon shells: Silkworm cocoons are selected as raw materials. Rotten and moldy cocoons are removed. The cocoons are boiled at low temperature, unwound, and reeled at low temperature. The cocoons are then processed to remove the silkworm pupae and produce three types of cocoon-derived raw materials: raw silk, fluffy silk floss, and cocoon shells. These are then classified and stored for later use. At room temperature, the cocoons are boiled at low temperature in a stainless steel pot at 75-80℃. The silk is then reeled at low temperature in a reeling machine at 65-80℃. The cocoon shells, after removing the silkworm pupae, are sterilized at high temperature in a pressure cooker and then used directly. (2). Dyeing and anti-mildew and anti-moth treatment of silk raw materials: The silk or silk floss obtained through the above process is placed in a water container with an active agent and degreased and rinsed at a water temperature of 55-70℃ for 20 minutes; then the degreased silk or silk floss is placed in an aqueous solution with dye and heated for dyeing at a bath temperature of 45-60℃ for 40-50 minutes, during which time the silk or silk floss is gently turned over to ensure even coloring. Once the dyed silk or silk floss has fully absorbed the color, add a color-fixing agent and fix the color for 15-20 minutes. When the temperature has naturally cooled to room temperature, remove the silk or silk floss and gently rinse it with room temperature water for the first time to remove any loose dye. For the second rinse and to treat the silk or silk floss for mold and moth prevention, add pre-prepared preservatives such as chitosan, citric acid, and camphor oil to a container of water, then add the silk or silk floss to be rinsed and soak for 20 minutes, gently turning it over and rinsing it 3 times during the process. After rinsing, place it in a ventilated place to air dry naturally. The cocoon shell can be dyed or left to retain its original color depending on the needs of the artwork. (3). Preparation of glue for silk painting: Using plant gum, 10L of water: 50-100g of plant gum: 5-10g of potassium sorbate: 5-10ml of camphor essential oil: 30-50g of chitosan: 20-40g of glycerin. Use a ceramic or stainless steel container, simmer in a water bath over low heat for 40 minutes, filter repeatedly through multiple layers of gauze to remove impurities, cool to form a gel, and dissolve in a water bath when needed. (4) Pretreatment of silk painting substrate Choose flax or silk as the base for the painting. Apply the glue prepared in step (3) evenly to the surface of the wooden board. Then, fix the flax or silk fabric used as the base flat on the wooden board. Use a scraper to evenly scrape the surface to keep the board flat and wrinkle-free. Fix it with nails on the side of the board. After the glue under the fabric dries, you can use silk or cocoon shell to paint. (5) Pretreatment of silk 3D sculpture substrate When preparing a three-dimensional silk sculpture, the sculpture substrate is pre-treated; this step can be omitted when making flat or relief silk paintings; the sculpture support substrate is built in advance, and the substrate material is selected to support the skeleton of the silk sculpture. First, build the shape of the substrate, then remove loose particles, dust and sharp edges from the surface. After cleaning, evenly apply the first layer of primer to the outer surface of the substrate and let it air dry in a ventilated place. Then, cover or apply a transition adhesion layer to make the surface of the substrate moderately rough and let it dry again for later use. (6) Wire fixing and shaping treatment For the silk fixation, the silk painting glue made in step (3) is prepared into a special water-based adhesive. The silk is shaped by evenly and lightly applying the adhesive and fixing it. The homemade glue is diluted with pure water and can be used as a setting glue spray to fix it. The structure of the silk painting is completed by splicing, crossing, and overlapping each other. The surface is sprayed for fixing. After the setting is completed, it is placed in a ventilated and cool place to cure and dry naturally at room temperature. The drying time is 12 to 24 hours. (7) Post-framing After the image has completely dried and stabilized, it is edged and framed to obtain the finished silk painting.

2. A handcrafting process of silk painting as claimed in claim 1 wherein, In step (1), a silk reeling solution was used for reeling. The silk reeling solution is an aqueous solution containing dried straw ash with a pH value of 6.5 to 7.

2.

3. A handcrafting process of silk painting as claimed in claim 1 wherein, The special water-based adhesive is prepared by boiling 10L of water, 50-100g of plant glue, 5-10g of potassium sorbate, 5-10ml of camphor essential oil, 30-50g of chitosan, and 20-40g of glycerin in a water bath. It is used as a base coating or for bonding silk, silk floss, and cocoon shells to a base.

4. A handcrafting process of silk painting as claimed in claim 1 wherein, The pretreatment of the three-dimensional sculpture substrate in step (5) is as follows: build a three-dimensional sculpture support substrate, trim the edges and corners, remove loose debris from the surface, apply a base coat to the whole, and then set a transition adhesion layer. After it dries, lay silk material layer by layer on the outer surface of the substrate to form a three-dimensional shape.