A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients.

By pre-wetting with carbonates, oxidizing with hydrogen peroxide, alkalizing, and flash steaming of weathered coal, combined with the phased regulation of carbon dioxide and ammonium dihydrogen phosphate, the contradiction between the alkalization and flash steaming activation of weathered coal and the retention of nitrogen-containing nutrients was resolved. This improved the water solubility of humic acid and the stability of compound fertilizers, and reduced nitrogen loss.

CN123106315APending Publication Date: 2026-11-17SHANDONG AIFUDI BIOLOGICAL TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611594356.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-15
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

How to coordinate the alkalization flash evaporation activation conditions of weathered coal with the low-temperature retention conditions of nitrogen-containing nutrients, while avoiding excessive oxidation of humic acid and high-temperature failure of nitrogen-containing raw materials, so as to improve the water solubility of humic acid in weathered coal and reduce nitrogen migration and loss during the production, drying and application of compound fertilizers.

Method used

Weathered coal is treated with carbonate pre-wetting, hydrogen peroxide oxidation, alkalization, and pressurized steam flash evaporation. The pH value of the material is controlled by staged adjustment of carbon dioxide and ammonium dihydrogen phosphate. Then, urea, ammonium sulfate, and ammonium-loaded clinoptilolite are coated at low temperature to form a nitrogen-containing outer layer, ensuring the activity of humic acid and the stability of nitrogen.

Benefits of technology

It improves the water solubility of humic acid, reduces nitrogen loss and migration, enhances the stability of compound fertilizer granules, avoids ammonia escape and clumping, and achieves effective utilization of humic acid and nitrogen.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention discloses a method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients, belonging to the field of fertilizer technology. The method includes: pre-wetting the weathered coal with carbonates, oxidizing it with hydrogen peroxide and alkalizing it, followed by flash activation with saturated steam; after cooling, adjusting the pH to 8.0-8.5 by introducing carbon dioxide, mixing it with organic materials, phosphate fertilizer, potassium fertilizer and trace elements, and steam granulation to obtain core particles; after cooling, spraying an ammonium dihydrogen phosphate aqueous solution to adjust the pH to 7.0-7.6; then coating the core particles with a film-forming solution of urea, ammonium sulfate and ammonium-loaded clinoptilolite, and drying at low temperature. This invention achieves spatial and temporal separation of high-temperature activation and low-temperature nitrogen retention processes by synergistically regulating residual alkalinity through carbon dioxide and ammonium dihydrogen phosphate in stages, effectively improving humic acid activity, reducing nitrogen loss, and resulting in stable finished particles.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of fertilizer technology, specifically to a method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients. Background Technology

[0002] Humic acid contains various active groups such as carboxyl, phenolic hydroxyl, alcoholic hydroxyl, and carbonyl groups. After being applied to the soil, it can participate in nutrient adsorption, ion exchange, and aggregate formation. Therefore, combining humic acid with nitrogen, phosphorus, potassium, and trace elements is a feasible approach to improve the comprehensive utilization performance of fertilizers.

[0003] Weathered coal is an important source of humic acid, but a significant portion of it exists as large molecular aggregates, bound to mineral components in the coal, resulting in low dissolution rates when directly extracted with water. Simply increasing the amount of alkaline substances can promote the ionization of acidic groups, but this can easily lead to excessively high residual alkalinity in the material. Furthermore, increasing the processing temperature or extending the processing time may cause excessive oxidation and molecularization of humic acid, affecting the retention of effective humic substances. Therefore, the activation process of weathered coal needs to balance structural depolymerization, exposure of active groups, humate formation, and control of excessive degradation.

[0004] In the production of organic-inorganic compound fertilizers, water vapor can provide both heat and moisture, which is beneficial for raw material mixing, wet-heat activation, and drum granulation. However, when nitrogen-containing materials such as urea and ammonium sulfate come into direct contact with weathered coal that has undergone alkalization treatment and undergo a high-temperature and high-humidity process together, the residual alkalinity in the materials will cause ammonium nitrogen to convert into free ammonia, increasing the risk of ammonia release. At the same time, nitrogen-containing materials are prone to dissolution and migration under wet-heat conditions, and after drying, they may concentrate on the surface of the granules, making the problems of fertilizer moisture absorption, agglomeration, and rapid nitrogen release more pronounced.

[0005] The alkalization and humid heat conditions required to improve the water solubility of humic acid present a technological contradiction with the near-neutral and low-temperature conditions needed to reduce nitrogen loss. Adding nitrogen-containing materials too early can easily lead to nitrogen loss; directly using strong acids to eliminate residual alkalinity may cause water-soluble humic acid to flocculate or revert to an insoluble form. Furthermore, simply feeding multiple raw materials into the rotary drum granulation process at once makes it difficult to simultaneously achieve full activation of weathered coal, uniform nutrient distribution, and slow nitrogen migration.

[0006] Therefore, the technical problem to be solved by the present invention is how to coordinate the alkalization flash evaporation activation conditions of weathered coal with the low-temperature retention conditions of nitrogen-containing nutrients, so as to improve the water solubility of humic acid in weathered coal and reduce nitrogen migration and loss during the production, drying and application of compound fertilizers, while avoiding excessive oxidation of humic acid and high-temperature failure of nitrogen-containing raw materials. Summary of the Invention

[0007] The purpose of this invention is to provide a method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients, so as to solve the technical problems mentioned in the background art.

[0008] To achieve the above objectives, the present invention provides the following technical solution:

[0009] A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients includes the following steps:

[0010] (1) The weathered coal is pre-wetted with at least one of sodium carbonate and potassium carbonate, and oxidized with hydrogen peroxide at 42-50℃; after the residual mass fraction of hydrogen peroxide in the wet material is not higher than 0.05%, at least one of sodium hydroxide and potassium hydroxide is added to make the pH of the 1:5 aqueous suspension of the material 10.0-11.0, and the moisture content of the material is adjusted to 30%-35%;

[0011] (2) Introduce saturated steam with a gauge pressure of 0.08 to 0.12 MPa into the material obtained in step (1) to make the actual temperature of the material reach 115 to 122°C and maintain it for 2 to 4 minutes. Then, depressurize it to atmospheric pressure within 5 seconds to obtain flash activated material.

[0012] (3) Cool the flash-activated material and introduce carbon dioxide in the powdered wet state to make the pH of the 1:5 aqueous suspension 8.0-8.5; mix the treated flash-activated material with organic materials, phosphate fertilizer, potassium fertilizer and micronutrient fertilizer without ammonium nitrogen, and granulate by drum granulation with steam without adding urea and ammonium nitrogen fertilizer to form core particles with a particle size of 0.8-1.5 mm; stop the steam, cool the core particles to below 40°C, and spray in ammonium dihydrogen phosphate aqueous solution so that the pH of the 1:5 aqueous suspension measured after the core particles are crushed as a whole is 7.0-7.6;

[0013] (4) Urea, ammonium sulfate and ammonium-loaded clinoptilolite obtained by partial ion exchange of sodium clinoptilolite with ammonium sulfate aqueous solution are coated on the outside of the core particles in batches with a film-forming solution containing pregelatinized starch and lignin sulfonate. The particles are dried under the condition that the actual temperature of the particles does not exceed 55°C during the drying process to obtain the organic-inorganic compound fertilizer containing humic acid.

[0014] The pH of the 1:5 aqueous suspension is the pH measured by mixing a representative powdered material or a material obtained by crushing a representative particle into deionized water at a mass ratio of 1:5.

[0015] Preferably, the weathered coal has a total humic acid content of not less than 45% on a dry basis, an initial water-soluble humic acid content of not more than 10%, and a raw material moisture content of not more than 20%; the weathered coal is crushed to a D90 of not more than 0.25 mm before pre-wetting.

[0016] As a preferred method, based on 100 parts by weight of dry-basis weathered coal, 2.0–3.0 parts by weight of potassium carbonate and water are added and mixed at 40–45°C for 20–30 minutes to bring the pH of the 1:5 aqueous suspension of the material to 8.8–9.3. Then, within 20–30 minutes, 4.0–6.0 parts by weight of a 30% hydrogen peroxide aqueous solution are added, and the reaction is continued at 42–50°C for 30–45 minutes. After the residual hydrogen peroxide mass fraction is no higher than 0.05%, 0.8–1.2 parts by weight of potassium hydroxide (pure weight) are added to bring the pH of the 1:5 aqueous suspension of the material to 10.3–10.8.

[0017] Preferably, the pressurized steam treatment is carried out in a pressure-bearing rotary wet heat activator, and the depressurized material enters a closed flash receiver; the flash activated material is cooled to below 40°C with air at a temperature not higher than 60°C and depolymerized to a D90 of not more than 0.25 mm, and its moisture content is adjusted to 25% to 32% before carbon dioxide is introduced.

[0018] Preferably, carbon dioxide with a volume fraction of not less than 95% is introduced under continuous material turning conditions, and the amount of carbon dioxide relative to the final dry basis of compound fertilizer is 3-8 kg / t; after stopping the aeration, mixing continues for no less than 10 minutes, and the treatment endpoint is when the pH of the 1:5 aqueous suspension of the material reaches 8.0-8.5.

[0019] 6. The method according to claim 1, wherein the organic material is decomposed plant-derived organic material, the phosphate fertilizer is dicalcium phosphate, and the potassium fertilizer is potassium sulfate; the micronutrient fertilizer is selected from at least two of magnesium sulfate, zinc sulfate, manganese sulfate, ferrous sulfate, boric acid, and sodium molybdate; the actual material temperature during the drum granulation process is 45-55℃, the material moisture content is 6%-9%, and the granulation time is 6-10 min.

[0020] Preferably, after stopping the steam supply and cooling the core particles to 35-40°C, a 10%-20% (w / w) ammonium dihydrogen phosphate aqueous solution is sprayed in; the amount of ammonium dihydrogen phosphate relative to the final compound fertilizer dry base is 4-6 kg / t. After spraying, the core particles are continuously rolled for 15-25 minutes so that the pH of the 1:5 aqueous suspension measured after the representative core particles are completely crushed is 7.0-7.6, and the pH is not higher than 7.8 when the pH is retested at 5-minute intervals.

[0021] Preferably, the ammonium-supported clinoptilolite is prepared according to the following method:

[0022] Natural clinoptilolite with a mineral content of not less than 70%, a cation exchange capacity of not less than 1.0 mmol / g, and a particle size of 100-200 mesh was selected. The natural clinoptilolite was mixed with an 8% sodium chloride aqueous solution at a dry basis mass ratio of 1:1.5. The mixture was treated at 55-60℃ for 60-90 min, filtered, washed, and dried at 70-80℃ to obtain sodium-type clinoptilolite with a water content of not more than 8%.

[0023] The sodium-type clinoptilolite is mixed with an aqueous solution of ammonium sulfate with a concentration of 1.0-1.3 mol / L at a liquid-to-solid ratio of 0.25-0.30 L / kg and treated at 30-40°C for 30-45 min to obtain ammonium-supported clinoptilolite that has undergone partial ion exchange. The ammonium-supported clinoptilolite is not subjected to high-temperature drying before coating.

[0024] Preferably, the dry weight ratio of urea to ammonium sulfate is 3:1 to 5:1, and the dry weight amount of ammonium-loaded clinoptilolite is 10% to 16% of the total dry weight of urea and ammonium sulfate; the film-forming solution comprises 12% to 18% pregelatinized starch, 4% to 6% sodium lignin sulfonate and the balance water by mass percentage.

[0025] Urea, ammonium sulfate (not used to prepare ammonium-supported clinoptilolite), and ammonium-supported clinoptilolite were divided into 2-3 batches. Before adding each batch of material, a portion of the film-forming liquid was sprayed onto the surface of the core particles. Then, the corresponding batch of urea, ammonium sulfate, and ammonium-supported clinoptilolite was added and rolled for 2-4 minutes. The above operation was repeated to form nitrogen-containing materials and ammonium-supported clinoptilolite on the outside of the core particles. The total coating time was 8-15 minutes, and the actual temperature of the particles during the coating process did not exceed 45°C.

[0026] Preferably, the coated granules are dried with low-humidity air at an inlet temperature not exceeding 60°C, and the actual temperature of the granules during the drying process does not exceed 55°C, until the moisture content of the granules does not exceed 3%; the dried granules are cooled to below 35°C, and granules with a particle size of 2.0 to 4.75 mm are screened as the finished product.

[0027] Compared with the prior art, the beneficial effects of the present invention are:

[0028] After undergoing carbonate pre-wetting, controlled hydrogen peroxide oxidation, alkalization, and pressurized steam flash treatment, the dense internal structure of weathered coal gradually loosens. Carbonate pre-wetting allows moisture to enter the pores of the weathered coal, providing a more uniform reaction environment for subsequent processing. Appropriate amounts of hydrogen peroxide, at controlled temperatures, increase the polarity of the coal's organic structure, exposing previously embedded hydrophilic groups such as carboxyl and phenolic hydroxyl groups. Subsequent alkalization facilitates the ionization and hydration of these acidic groups, thereby enhancing the dispersion of humic substances in water. Pressurized steam further promotes the transfer of moisture into the particles; rapid depressurization causes instantaneous vaporization of pore water, resulting in expansion and microcracks within the weathered coal, shortening the migration path of humic substances from the particle interior to the aqueous phase. By controlling the amount of hydrogen peroxide, treatment temperature, residual amount, and steam residence time, it is possible to improve the water solubility of humic acid while reducing the small-molecule formation of humic substances and the loss of effective organic carbon caused by excessive oxidation.

[0029] The aforementioned activation process requires alkaline conditions, while the stable loading of urea and ammonium nitrogen is more suitable for near-neutral, low-temperature environments, creating a clear process contradiction. After weathered coal undergoes alkalization and flash evaporation, a certain amount of free alkali and carbonate alkalinity may still remain in the material. Steam treatment may also cause alkaline components that have not yet fully balanced within the material to migrate back to the particle surface, resulting in a pH rise. If ammonium nitrogen sources such as ammonium sulfate are added directly at this point, the elevated pH will shift the ammonium nitrogen equilibrium towards free ammonia, and the generated ammonia is prone to escape during mixing, granulation, and drying. Clinoptilolite can retain ammonium ions through ion exchange, but it cannot effectively prevent the already converted and escaped gaseous ammonia. Therefore, reducing and stabilizing the residual alkalinity of the material before loading the main nitrogen source is a prerequisite for leveraging its subsequent nitrogen-retaining structural function.

[0030] Carbon dioxide and ammonium dihydrogen phosphate are added in stages and sequentially to jointly regulate residual alkalinity. Carbon dioxide is first introduced while the flash-activated material is still in a powdery, wet state, ensuring sufficient contact with the activated material, which has a large specific surface area. After dissolving in the material's moisture, carbon dioxide creates a weakly acidic environment, which gently consumes free alkali and transforms the carbonate system into a less alkaline form, thus rapidly reducing the material's overall alkalinity. This treatment does not require the addition of strong acids or introduce polyvalent metal ions such as calcium and magnesium, thereby reducing the risk of flocculation of humic acid due to localized strong acidification or polyvalent ion bridging. However, the regulatory effect of carbon dioxide is somewhat reversible; carbon dioxide may escape during subsequent agitation and steam granulation, causing the pH to rise to varying degrees. Using carbon dioxide alone is insufficient for long-term stable acidity and alkalinity of the material.

[0031] Ammonium dihydrogen phosphate (MDP) is added after the core particles have undergone steam granulation and cooling. It serves to finely adjust and stabilize the pH after carbon dioxide treatment. MDP ions continue to consume residual or re-migrated alkaline components in the particles, forming a buffered phosphate system within a near-neutral range, preventing the material's pH from rising again due to carbon dioxide escape. Adding MDP after steam shutdown and cooling also avoids direct exposure of ammonium nitrogen to the steam granulation conditions. Carbon dioxide initially provides a mild reduction of most of the residual alkalinity, reducing the actual consumption of MDP and minimizing localized pH drops and salt concentrations caused by adding too much acidic fertilizer at once. MDP compensates for the tendency of carbon dioxide's regulatory effect to fade, further correcting for pH rises after granulation. The combination of these two components, following the sequence of "reducing alkalinity first in the powder stage, then stabilizing after nucleation and cooling," maintains a relatively stable near-neutral environment in the material before the addition of urea and ammonium sulfate. This is the core problem solved by their synergistic effect.

[0032] After controlling the residual alkalinity of the material, urea, ammonium sulfate, and ammonium-loaded clinoptilolite are placed on the outside of the core particles, and low-temperature layered coating is performed in conjunction with pregelatinized starch and sodium lignin sulfonate. The clinoptilolite framework has cation exchange sites, enabling reversible retention of ammonium ions and slowing the rapid migration of ammonium nitrogen with moisture. For uncharged urea, clinoptilolite primarily provides pore retention and surface adsorption space, and is not described as ion exchange. Pregelatinized starch and sodium lignin sulfonate, through bonding, hydrogen bonding, and drying film formation, fix the nitrogen-containing powder and clinoptilolite on the particle surface and extend the paths for moisture entry and nutrient diffusion. Controlling the actual particle temperature during coating and drying reduces the hygrothermal migration of nitrogen and ammonia volatilization, while also reducing the tendency of the finished product to absorb moisture, pulverize, and agglomerate.

[0033] Through the above process, the oxidation, alkalization, and flash activation of weathered coal are completed before the main nitrogen source is added. Nitrogen-containing nutrients are loaded after the core particles have cooled and their pH has stabilized, achieving spatial and temporal separation between the high-temperature alkaline activation process and the low-temperature nitrogen retention process. This process not only improves the water solubility of humic acid but also provides suitable pH and temperature conditions for ammonium-loaded clinoptilolite and the film-forming layer to exert their nitrogen retention effect, thus balancing the maintenance of humic acid activity, control of nitrogen loss, and stability of compound fertilizer particles. Detailed Implementation

[0034] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0035] All the following embodiments use a 10L pressurized rotary damp heat activator, a 30L closed flash receiver, and a 30L rotary drum granulator for preparation. A pressure relief pipe with an inner diameter of 20mm and a full-bore quick-opening valve are installed between the damp heat activator and the flash receiver.

[0036] All embodiments use 10,000 kg of theoretical finished product dry basis as the conversion basis for the dosage of carbon dioxide and ammonium dihydrogen phosphate; the dry basis mass includes weathered coal, alkaline substances, organic materials, nutrient fertilizers, clinoptilolite, and film-forming substances, but excludes process water, washing sodium chloride, and hydrogen peroxide. All moisture contents are wet basis moisture contents.

[0037] When determining the pH of a 1:5 aqueous suspension, 10.0 g of representative powdered material was taken; for granular material, the entire sample was first pulverized, then 10.0 g of the pulverized sample was taken, 50.0 g of deionized water was added, and the mixture was stirred at 25°C for 30 min before pH measurement. The residual mass fraction of hydrogen peroxide in the wet material was determined using the water extraction-iodometric method. The chloride ion content in the washed clinoptilolite was determined using the silver nitrate titration method.

[0038] Example 1

[0039] A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients includes the following steps:

[0040] (1) Activation of weathered coal

[0041] Weigh 1.875 kg of weathered coal with a moisture content of 20.0%, which is equivalent to 1.500 kg of dry-basis weathered coal. The total humic acid content of the weathered coal, on a dry basis, is 45.0%, and the initial water-soluble humic acid content is 10.0%. Crush it to a D90 of 0.25 mm.

[0042] Dissolve 30.0g of potassium carbonate in 186.0g of deionized water, add the resulting solution to weathered coal, mix at 40℃ for 20min, and use the pH of the 1:5 aqueous suspension reaching 8.8 as the pre-wetting endpoint.

[0043] In a mixer equipped with an exhaust port, the material temperature was controlled at 42℃. 60.0g of a 30% (w / w) hydrogen peroxide aqueous solution (containing 18.0g of hydrogen peroxide) was added dropwise over 30 minutes. After the addition was complete, the reaction continued for 45 minutes. Once the residual hydrogen peroxide content in the wet material was confirmed to be no higher than 0.05%, 60.0g of a 20% (w / w) potassium hydroxide aqueous solution (containing 12.0g of potassium hydroxide and 48.0g of water) was added to bring the pH of the 1:5 aqueous suspension of the material to 10.3 and the water content to 30.0%.

[0044] (2) Steam flashing and carbon dioxide treatment

[0045] All the alkalized material was loaded into a pressure-bearing rotary wet heat activator, and a total of 0.25 kg of saturated steam with a gauge pressure of 0.08 MPa was introduced. When the actual temperature of the material reached 115℃, the pressure was maintained for 2 minutes. Then, the quick-opening valve was fully opened, and the pressure was released to atmospheric pressure within 5 seconds, allowing the material to enter the closed flash receiver.

[0046] The flash-evaporated material was cooled to below 40°C and its moisture content adjusted to 25.0% using 25°C, low-humidity air, and then depolymerized to a D90 of 0.25 mm. Under continuous material turning conditions, carbon dioxide with a volume fraction of not less than 95% was introduced at a mass flow rate of 1.50 g / min for 20 min, with a cumulative introduction of 30.0 g of carbon dioxide. After stopping the aeration, mixing continued for 10 min, and the treatment endpoint was defined as the pH of the 1:5 aqueous suspension of the material reaching 8.5.

[0047] (3) Core particle preparation

[0048] Add 2.041 kg of well-rotted straw organic material with a moisture content of 2.0% to all the materials after carbon dioxide treatment, which is equivalent to 2.000 kg of dry basis organic material; then add 2.000 kg of dry basis dicalcium phosphate, 1.938 kg of dry basis potassium sulfate, 120.0 g of fertilizer grade magnesium sulfate, 50.0 g of fertilizer grade zinc sulfate and 30.0 g of fertilizer grade boric acid, and mix well.

[0049] The moisture content of the mixture is adjusted to 6.0% using 25℃ low-humidity air. This mixture is then fed into a rotary drum granulator rotating at 18 r / min, with a cumulative steam injection of 0.20 kg. Granulation takes 6 minutes at an actual material temperature of 45℃ and a moisture content of 6.0%. Core particles with a diameter of 0.8–1.0 mm are then sieved. Urea, ammonium sulfate, ammonia, ammonium bicarbonate, or other ammonium nitrogen fertilizers are not added in this step.

[0050] Stop the steam supply and cool the core particles to 35°C. Dissolve 40.0g of ammonium dihydrogen phosphate in 360.0g of deionized water to prepare 400.0g of a 10% (w / w) ammonium dihydrogen phosphate aqueous solution. Spray this solution into the core particles in four applications, 100.0g each time. After spraying, continue rolling for 15 minutes. The treatment endpoint is defined as the pH of the 1:5 aqueous suspension after whole-body crushing of representative core particles reaching 7.6, and the pH not exceeding 7.8 when retested at 5-minute intervals. Adjust the moisture content of the core particles to 7.0% using low-humidity air at a temperature not exceeding 40°C.

[0051] (4) Preparation of ammonium-supported clinoptilolite

[0052] Weigh 200.0g of dry-basis natural clinoptilolite, which has a clinoptilolite mineral content of 70.0%, a cation exchange capacity of 1.0mmol / g, and a particle size of 100 mesh.

[0053] 24.0 g of sodium chloride was dissolved in 276.0 g of deionized water to prepare a 300.0 g sodium chloride aqueous solution with a mass fraction of 8%. 200.0 g of dry-basis natural clinoptilolite was mixed with the 300.0 g sodium chloride aqueous solution and treated at 55 °C for 60 min. After filtration, it was washed five times with 1000.0 g of deionized water, using 200.0 g of deionized water each time. After confirming that the chloride ion content in the dry-basis clinoptilolite was not higher than 0.30%, it was dried at 70 °C until the moisture content was 8.0%, yielding sodium-type clinoptilolite.

[0054] 6.607 g of ammonium sulfate was dissolved in deionized water and brought to a final volume of 50.0 mL at 25 °C to prepare a 1.0 mol / L ammonium sulfate aqueous solution. The 50.0 mL solution was then uniformly sprayed into all of the sodium-type clinoptilolite and forcibly mixed at 30 °C for 30 min to obtain an ammonium-loaded clinoptilolite wet material. This wet material was not filtered or dried and was used entirely for subsequent coating.

[0055] (5) Construction and drying of nitrogen-containing outer layer

[0056] In this embodiment, the total dry weight of urea and ammonium sulfate is 2.000 kg, including 1.500 kg of urea and 500.000 g of ammonium sulfate. Of the 500.000 g of ammonium sulfate, 6.607 g of ammonium sulfate is used to prepare ammonium-supported clinoptilolite, and the remaining 493.393 g of powdered ammonium sulfate is used for direct coating. The dry weight ratio of urea to ammonium sulfate is 3:1. The 200.0 g dry weight clinoptilolite is 10.0% of the total dry weight of urea and ammonium sulfate.

[0057] 60.0g of low-viscosity pregelatinized cassava starch, 20.0g of sodium lignin sulfonate and 420.0g of deionized water were stirred at 40℃ for 20min to prepare a film-forming solution of 500.0g.

[0058] 1.500 kg of urea, 493.393 g of powdered ammonium sulfate, all of the ammonium-loaded clinoptilolite wet material, and 500.0 g of film-forming solution were divided into two equal portions. For the first part, 250.0 g of film-forming solution was sprayed onto the surface of the rotating core particles. Then, 750.0 g of urea, 246.697 g of powdered ammonium sulfate, and half of the ammonium-loaded clinoptilolite wet material were added, and the mixture was rolled for 2 minutes. The remaining materials were added in the same order and rolled for 2 minutes each time. Finally, rolling continued for 4 minutes, for a total coating time of 8 minutes. During the coating process, the actual temperature of the particles did not exceed 40℃, and the particles gradually grew through rolling and agglomeration.

[0059] The particles are dried using low-humidity air with an inlet temperature of 45℃, and the actual temperature of the particles is controlled not to exceed 45℃ until the moisture content is 3.0%. Then, the particles are cooled to 35℃ and sieved with 2.0mm and 4.75mm sieves to obtain particles with a particle size of 2.0 to 4.75mm, thus obtaining humic acid-containing organic-inorganic compound fertilizer.

[0060] Example 2

[0061] A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients includes the following steps:

[0062] (1) Activation of weathered coal

[0063] Weigh 1.667 kg of weathered coal with a moisture content of 10.0%, which is equivalent to 1.500 kg of dry-basis weathered coal. The total humic acid content of the weathered coal, on a dry basis, is 52.0%, and the initial water-soluble humic acid content is 7.0%. Crush it to a D90 of 0.20 mm.

[0064] Dissolve 37.5g of sodium carbonate in 456.0g of deionized water, add the resulting solution to weathered coal, mix at 43℃ for 25min, and use the pH of the 1:5 aqueous suspension reaching 9.0 as the pre-wetting endpoint.

[0065] The material temperature was controlled at 46℃. 75.0 g of a 30% (w / w) hydrogen peroxide aqueous solution (containing 22.5 g of hydrogen peroxide) was added dropwise over 25 minutes. After the addition was complete, the reaction continued for 38 minutes. Once the residual hydrogen peroxide content in the wet material was confirmed to be no higher than 0.05%, 75.0 g of a 20% (w / w) sodium hydroxide aqueous solution (containing 15.0 g of sodium hydroxide and 60.0 g of water) was added to bring the pH of the 1:5 aqueous suspension of the material to 10.5 and the water content to 32.5%.

[0066] (2) Steam flashing and carbon dioxide treatment

[0067] All the alkalized material was loaded into a pressure-bearing rotary wet heat activator, and a total of 0.30 kg of saturated steam with a gauge pressure of 0.10 MPa was introduced. When the actual temperature of the material reached 119°C, the pressure was maintained for 3 minutes, and then the pressure was released to atmospheric pressure within 3 seconds, allowing the material to enter a closed flash receiver.

[0068] The flash-evaporated material was cooled to below 40°C and its moisture content adjusted to 28.5% using 30°C, low-humidity air, and then depolymerized to a D90 of 0.20 mm. Under continuous material turning conditions, carbon dioxide with a volume fraction of not less than 95% was introduced at a mass flow rate of 2.20 g / min for 25 min, with a cumulative introduction of 55.0 g of carbon dioxide. After stopping the aeration, mixing continued for 10 min, and the treatment endpoint was defined as the pH of the 1:5 aqueous suspension of the material reaching 8.2.

[0069] (3) Core particle preparation

[0070] Add 2.041 kg of well-rotted straw organic material with a moisture content of 2.0% to all the materials after carbon dioxide treatment, which is equivalent to 2.000 kg of dry basis organic material; then add 2.000 kg of dry basis dicalcium phosphate, 1.8375 kg of dry basis potassium sulfate, 120.0 g of fertilizer grade magnesium sulfate, 50.0 g of fertilizer grade zinc sulfate and 30.0 g of fertilizer grade boric acid, and mix well.

[0071] The moisture content of the mixture is adjusted to 7.0% using 30℃ low-humidity air. This mixture is then fed into a rotary drum granulator at a speed of 20 r / min, with a cumulative steam injection of 0.25 kg. Granulation is carried out for 8 minutes at an actual material temperature of 50℃ and a moisture content of 7.5%. Core particles with a diameter of 1.0–1.3 mm are then sieved. Urea, ammonium sulfate, ammonia, ammonium bicarbonate, or other ammonium nitrogen fertilizers are not added in this step.

[0072] Stop the steam supply and cool the core particles to 38°C. Dissolve 50.0g of ammonium dihydrogen phosphate in 283.3g of deionized water to prepare a 333.3g (w / w) ammonium dihydrogen phosphate aqueous solution. Spray this solution into the core particles in three applications, 111.1g each time. After spraying, continue rolling for 20 minutes. The treatment endpoint is defined as the pH of the 1:5 aqueous suspension after whole-body crushing of representative core particles reaching 7.3, and the pH not exceeding 7.8 when retested at 5-minute intervals. Adjust the moisture content of the core particles to 7.0% using low-humidity air at a temperature not exceeding 40°C.

[0073] (4) Preparation of ammonium-supported clinoptilolite

[0074] Weigh 260.0g of dry-basis natural clinoptilolite, which has a mineral content of 80.0%, a cation exchange capacity of 1.2mmol / g, and a particle size of 150 mesh.

[0075] 31.2 g of sodium chloride was dissolved in 358.8 g of deionized water to prepare 390.0 g of an 8% sodium chloride aqueous solution. 260.0 g of dry-basis natural clinoptilolite was mixed with the 390.0 g of the sodium chloride aqueous solution and treated at 57.5 °C for 75 min. After filtration, it was washed five times with 1300.0 g of deionized water, using 260.0 g of deionized water each time. After confirming that the chloride ion content in the dry-basis clinoptilolite was no higher than 0.30%, it was dried at 75 °C until the moisture content was 7.0%, yielding sodium-type clinoptilolite.

[0076] 10.865 g of ammonium sulfate was dissolved in deionized water and brought to a final volume of 71.5 mL at 25 °C to prepare a 1.15 mol / L ammonium sulfate aqueous solution. The 71.5 mL of this ammonium sulfate aqueous solution was uniformly sprayed into all of the sodium-type clinoptilolite, and forced mixing was carried out at 35 °C for 38 min to obtain an ammonium-loaded clinoptilolite wet material. The resulting wet material was not filtered or dried and was used entirely for subsequent coating.

[0077] (5) Construction and drying of nitrogen-containing outer layer

[0078] In this embodiment, the total dry weight of urea and ammonium sulfate is 2.000 kg, including 1.600 kg of urea and 400.000 g of ammonium sulfate. Of the 400.000 g of ammonium sulfate, 10.865 g of ammonium sulfate is used to prepare ammonium-supported clinoptilolite, and another 389.135 g of powdered ammonium sulfate is used for direct coating. The dry weight ratio of urea to ammonium sulfate is 4:1. The 260.0 g dry weight clinoptilolite accounts for 13.0% of the total dry weight of urea and ammonium sulfate.

[0079] 75.0g of low-viscosity pregelatinized cassava starch, 25.0g of sodium lignin sulfonate and 400.0g of deionized water were stirred at 42℃ for 20min to prepare a film-forming solution of 500.0g.

[0080] 1.600 kg of urea, 389.135 g of powdered ammonium sulfate, all of the ammonium-loaded clinoptilolite wet material, and 500.0 g of film-forming solution were divided into three equal portions. Each time, 166.7 g of film-forming solution was sprayed in sequence, followed by 533.3 g of urea, 129.7 g of powdered ammonium sulfate, and one-third of the ammonium-loaded clinoptilolite wet material, and the mixture was rolled for 3 minutes. This process was repeated three times, with a total coating time of 9 minutes. During the coating process, the actual temperature of the particles did not exceed 43℃, and the particles gradually grew through rolling and agglomeration.

[0081] The particles were dried using low-humidity air with an inlet temperature of 52℃, and the actual temperature of the particles was controlled to be no higher than 50℃ until the moisture content was 2.5%. Then, the particles were cooled to 30℃ and sieved with 2.0mm and 4.75mm sieves to obtain particles with a particle size of 2.0 to 4.75mm, thus obtaining a humic acid-containing organic-inorganic compound fertilizer.

[0082] Example 3

[0083] A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients includes the following steps:

[0084] (1) Activation of weathered coal

[0085] Weigh 1.765 kg of weathered coal with a moisture content of 15.0%, which is equivalent to 1.500 kg of dry-basis weathered coal. The total humic acid content of the weathered coal, on a dry basis, is 60.0%, and the initial water-soluble humic acid content is 5.0%. Crush it to a D90 of 0.15 mm.

[0086] Dissolve 45.0g of potassium carbonate in 428.0g of deionized water, add the resulting solution to the weathered coal, mix at 45℃ for 30min, and use the pH of the 1:5 aqueous suspension reaching 9.3 as the pre-wetting endpoint.

[0087] The material temperature was controlled at 50℃. 90.0g of a 30% (w / w) hydrogen peroxide aqueous solution (containing 27.0g of hydrogen peroxide) was added dropwise over 20 minutes. After the addition was complete, the reaction continued for 30 minutes. Once the residual hydrogen peroxide content in the wet material was confirmed to be no higher than 0.05%, 90.0g of a 20% (w / w) potassium hydroxide aqueous solution (containing 18.0g of potassium hydroxide and 72.0g of water) was added to bring the pH of the 1:5 aqueous suspension of the material to 10.8 and the water content to 35.0%.

[0088] (2) Steam flashing and carbon dioxide treatment

[0089] All the alkalized material was loaded into a pressure-bearing rotary wet heat activator, and a total of 0.35 kg of saturated steam with a gauge pressure of 0.12 MPa was introduced. When the actual temperature of the material reached 122℃, the pressure was maintained for 4 minutes, and then the pressure was released to atmospheric pressure within 2 seconds, allowing the material to enter a closed flash receiver.

[0090] The flash-evaporated material was cooled to below 40°C and its moisture content adjusted to 31.5% using 35°C, low-humidity air, followed by depolymerization to a D90 of 0.15 mm. Under continuous material turning conditions, carbon dioxide with a volume fraction of not less than 95% was introduced at a mass flow rate of 2.67 g / min for 30 minutes, with a cumulative introduction of 80.0 g of carbon dioxide. After stopping the aeration, mixing continued for 10 minutes, and the treatment endpoint was defined as the pH of a 1:5 aqueous suspension of the material reaching 8.0.

[0091] (3) Core particle preparation

[0092] Add 2.041 kg of well-rotted straw organic material with a moisture content of 2.0% to all the materials after carbon dioxide treatment, which is equivalent to 2.000 kg of dry basis organic material; then add 2.000 kg of dry basis dicalcium phosphate, 1.737 kg of dry basis potassium sulfate, 120.0 g of fertilizer grade magnesium sulfate, 50.0 g of fertilizer grade zinc sulfate and 30.0 g of fertilizer grade boric acid, and mix well.

[0093] The moisture content of the mixture is adjusted to 8.0% using 35℃ low-humidity air. This mixture is then fed into a rotary drum granulator at a speed of 22 r / min, with a cumulative steam injection of 0.30 kg. Granulation is carried out for 10 minutes at an actual material temperature of 55℃ and a moisture content of 9.0%. Core particles with a diameter of 1.2–1.5 mm are then sieved out. Urea, ammonium sulfate, ammonia, ammonium bicarbonate, or other ammonium nitrogen fertilizers are not added in this step.

[0094] Stop the steam supply and cool the core particles to 40°C. Dissolve 60.0g of ammonium dihydrogen phosphate in 240.0g of deionized water to prepare 300.0g of a 20% (w / w) ammonium dihydrogen phosphate aqueous solution. Spray this solution into the core particles in three applications, 100.0g each time. After spraying, continue rolling for 25 minutes. The treatment endpoint is defined as the pH of the 1:5 aqueous suspension after whole-body crushing of representative core particles reaching 7.0, and the pH not exceeding 7.8 when retested at 5-minute intervals. Adjust the moisture content of the core particles to 7.0% using low-humidity air at a temperature not exceeding 40°C.

[0095] (4) Preparation of ammonium-supported clinoptilolite

[0096] Weigh 320.0g of dry-basis natural clinoptilolite, which has a mineral content of 90.0%, a cation exchange capacity of 1.5mmol / g, and a particle size of 200 mesh.

[0097] 38.4 g of sodium chloride was dissolved in 441.6 g of deionized water to prepare a sodium chloride aqueous solution of 480.0 g with a mass fraction of 8%. 320.0 g of dry-basis natural clinoptilolite was mixed with the aforementioned sodium chloride aqueous solution and treated at 60 °C for 90 min. After filtration, it was washed five times with 1600.0 g of deionized water, using 320.0 g of deionized water each time. After confirming that the chloride ion content in the dry-basis clinoptilolite was not higher than 0.30%, it was dried at 80 °C until the moisture content was 5.0%, yielding sodium-type clinoptilolite.

[0098] 16.491 g of ammonium sulfate was dissolved in deionized water and brought to a final volume of 96.0 mL at 25 °C to prepare a 1.3 mol / L ammonium sulfate aqueous solution. The 96.0 mL solution was then uniformly sprayed into all of the sodium-type clinoptilolite and forcibly mixed at 40 °C for 45 min to obtain an ammonium-loaded clinoptilolite wet material. This wet material was not filtered or dried and was used entirely for subsequent coating.

[0099] (5) Construction and drying of nitrogen-containing outer layer

[0100] In this embodiment, the total dry weight of urea and ammonium sulfate is 2.000 kg, including 1.667 kg of urea and 333.333 g of ammonium sulfate. Of the 333.333 g of ammonium sulfate, 16.491 g was used to prepare ammonium-supported clinoptilolite, and the remaining 316.842 g of powdered ammonium sulfate was used for direct coating. The dry weight ratio of urea to ammonium sulfate was 5:1. The 320.0 g dry weight clinoptilolite represents 16.0% of the total dry weight of urea and ammonium sulfate.

[0101] 90.0g of low-viscosity pregelatinized cassava starch, 30.0g of sodium lignin sulfonate and 380.0g of deionized water were forcibly stirred at 45℃ for 30min and then sprayed using a large-diameter nozzle to prepare a film-forming solution of 500.0g.

[0102] 1.667 kg of urea, 316.842 g of powdered ammonium sulfate, all of the ammonium-loaded clinoptilolite wet material, and 500.0 g of film-forming solution were divided into three equal portions. Each time, 166.7 g of film-forming solution was sprayed in sequence, followed by 555.6 g of urea, 105.6 g of powdered ammonium sulfate, and one-third of the ammonium-loaded clinoptilolite wet material, and the mixture was rolled for 4 minutes. This process was repeated three times, followed by another 3 minutes of rolling, for a total coating time of 15 minutes. During the coating process, the actual temperature of the particles did not exceed 45℃, and the particles gradually grew through rolling and agglomeration.

[0103] The particles are dried using low-humidity air with an inlet temperature of 60℃, and the actual temperature of the particles is controlled to be no higher than 55℃, until the moisture content is 2.0%. Then, the particles are cooled to 25℃ and sieved with 2.0mm and 4.75mm sieves to obtain particles with a particle size of 2.0 to 4.75mm, thus obtaining humic acid-containing organic-inorganic compound fertilizer.

[0104] Comparative Example 1

[0105] Compared with Example 1, Comparative Example 1 used 60.0g of deionized water instead of 60.0g of 30% hydrogen peroxide aqueous solution, and did not perform hydrogen peroxide oxidation treatment. The remaining steps were the same as in Example 1.

[0106] Comparative Example 2

[0107] Compared with Example 1, Comparative Example 2 adopted a slow depressurization to atmospheric pressure for 10 minutes after the pressurized steam treatment, and the flash steaming operation of rapid depressurization within 5 seconds was cancelled. The remaining steps were the same as those in Example 1.

[0108] Comparative Example 3

[0109] Compared with Example 1, Comparative Example 3 did not introduce 30.0g of carbon dioxide during the alkali adjustment stage of the activation material, and after the core particles were cooled, 360.0g of deionized water replaced 400.0g of 10% ammonium dihydrogen phosphate aqueous solution. The remaining steps were the same as in Example 1.

[0110] Comparative Example 4

[0111] Compared with Example 1, Comparative Example 4 retains the 30.0g carbon dioxide treatment step, but after the core particles are cooled, 360.0g of deionized water replaces 400.0g of 10% ammonium dihydrogen phosphate aqueous solution. The remaining steps are the same as in Example 1.

[0112] Comparative Example 5

[0113] Compared with Example 1, Comparative Example 5 did not introduce 30.0g of carbon dioxide during the alkali adjustment stage of the activation material, but only maintained the same time of stirring and mixing, and retained 400.0g of 10% ammonium dihydrogen phosphate aqueous solution after the core particles were cooled. The remaining steps were the same as in Example 1.

[0114] Comparative Example 6

[0115] Compared with Example 1, Comparative Example 6 adjusted the addition of 400.0g of 10% ammonium dihydrogen phosphate aqueous solution to be added after carbon dioxide treatment and before steam granulation. After the core particles were cooled, no more ammonium dihydrogen phosphate was added. The remaining steps were the same as in Example 1.

[0116] Comparative Example 7

[0117] Compared with Example 1, Comparative Example 7 omits the sodium chloride sodiumization and ammonium sulfate partial ion exchange treatment, and instead uses 200.0g of untreated natural clinoptilolite. 6.607g of ammonium sulfate in the original exchange solution is added to the ammonium sulfate for direct coating, so that the total amount of ammonium sulfate for direct coating is 500.000g. The remaining steps are the same as in Example 1.

[0118] Comparative Example 8

[0119] Compared with Example 1, Comparative Example 8 did not add 60.0g of pregelatinized cassava starch and 20.0g of sodium lignin sulfonate to the film-forming solution, and only sprayed 420.0g of deionized water for batch rolling loading. The remaining steps were the same as in Example 1.

[0120] Comparative Example 9

[0121] Compared with Example 1, Comparative Example 9 added 1,500 kg of urea, 500,000 g of ammonium sulfate and all ammonium-loaded clinoptilolite wet material during the steam drum granulation stage, and no longer carried out low-temperature post-loading of nitrogen-containing materials after the core particles cooled. The remaining steps were the same as in Example 1.

[0122] Performance testing

[0123] 1. Sample preparation, sampling points and statistical processing

[0124] Examples 1-3 and Comparative Examples 1-9 each prepared three batches independently, with the batch preparation order randomized; each batch of finished product was reduced according to GB / T 8571—2008. Chemical analysis samples were ground and passed through a 0.50 mm sieve; unground particles were used for particle size and compressive strength tests. Five sampling points were uniformly set: T0 (after flash evaporation, cooling, and depolymerization), T1 (after carbon dioxide treatment and continued mixing for 10 min), T2 (after steam nucleation and cessation of steam supply), T3 (T3 being the samples obtained before coating after each experimental group completed its preset post-treatment, reached the same final cooling temperature and cumulative mixing time; for experimental groups with ammonium dihydrogen phosphate treatment, samples were taken after spraying and mixing; for experimental groups without this treatment, samples were taken after isothermal and isochronous blank mixing), and T4 (finished product after coating, drying, and sieving). Chemical indicators for each batch were measured twice in parallel, and the average value was used as the statistical value for that batch. The final results are expressed as the mean ± standard deviation of the three independent batches. Example 2 and Comparative Examples 3-5 were analyzed using a two-way ANOVA including CO2, ammonium dihydrogen phosphate and their interaction term. The comparisons between the remaining groups were analyzed using a one-way ANOVA with Holm correction. The significance level was set at P < 0.05.

[0125] 2. Total humic acid content and total humic acid retention rate

[0126] T0 activated material and T4 finished product were taken separately and determined according to GB / T 34766—2017 "Determination of Total Humic Acid Content from Mineral Sources": The pulverized and mixed sample was extracted with sodium pyrophosphate alkaline extract to allow the mineral-derived humic acid to enter the extract. After acidification and separation of acid-soluble components, the humic acid carbon was determined according to the standard and converted into the total humic acid mass fraction. The results were uniformly converted to dry basis. The total humic acid retention rate was calculated as "(total mass of material at the corresponding sampling point × dry basis mass fraction of total humic acid at the sampling point) ÷ (mass of weathered coal input × dry basis mass fraction of total humic acid in weathered coal) × 100%"; this indicator is based on T0 and is used to identify whether controlled oxidation has caused excessive degradation. The finished product state was retested at T4.

[0127] 3. Content of water-soluble humic acid and water solubility rate of humic acid

[0128] Take T0 activated material and T4 finished product, and determine the soluble humic acid content according to GB / T 35107—2017 "Determination of Soluble Humic Acid Content in Mineral-Derived Humic Acid Fertilizers": Extract the pulverized and mixed sample with water, acidify the extract to the standard specified conditions to precipitate humic acid, separate, wash, dry, and deduct ash content before calculating the mass fraction of water-soluble humic acid. The same dry and wet standard and carbon coefficient caliber are used for total humic acid and water-soluble humic acid; the water solubility rate of humic acid is calculated as "mass fraction of water-soluble humic acid ÷ mass fraction of total humic acid × 100%", and the result of T4 finished product is used as the reported value in the table.

[0129] 4. pH, titratable residual alkalinity, and pH recovery value

[0130] pH was determined according to Clause 6.7 of GB / T 18877—2020: Weigh 10.00g of the pulverized sample, add 50.0mL of CO2-free water, stir for 1min and let stand for 5min, and measure using a pH meter with two-point calibration and a scale division of 0.01. The absolute difference between two parallel measurements should not exceed 0.10. Samples T0 to T4 were measured separately. Sample T3 was placed in an open environment at 25±1℃ and 60±5% relative humidity, and independent samples were taken at 0, 1, 3, and 7 days to measure pH. The pH rise was the difference between the highest pH during the storage period and the pH on day 0. The titrable residual alkalinity was determined as follows: Weigh 5.000g of the pulverized T3 sample, add 100.0mL of CO2-free water, stir at 25℃ for 30min, and titrate with 0.1000mol / L hydrochloric acid to pH=7.00. After subtracting the water blank, the pH was converted to mmol H based on the dry basis sample mass. + / kg.

[0131] 5. Total nitrogen content and solid nitrogen recovery rate

[0132] The total nitrogen content of the T4 finished product was determined according to GB / T 17767.1—2008 "Determination of Organic-Inorganic Compound Fertilizers Part 1: Total Nitrogen Content": Samples passing through a 0.50 mm sieve were digested using a sulfuric acid system to convert organic nitrogen and amide nitrogen into ammonium nitrogen. The digestion solution was then alkalized and distilled. The released ammonia was absorbed with boric acid solution, followed by titration with a standard acid and blank correction. The dry basis total nitrogen mass fraction was calculated. After each batch of production, qualified finished products, sieve feed, sieve underfeed, and recyclable dust were collected separately. The mass of each part was weighed, and the total nitrogen content was determined. The total solid nitrogen recovery rate was calculated as "the sum of the products of the mass of each solid part and its total nitrogen mass fraction ÷ the total nitrogen input of all nitrogen-containing raw materials × 100%".

[0133] 6. Process ammonia loss rate

[0134] A sealed gas collection hood was installed at the exhaust end of the small-scale rotary drum granulation device. A stable total exhaust flow rate Q was maintained using ammonia-removed air, and samples were continuously collected from the thoroughly mixed exhaust at a constant rate of 0.50 L / min. The sampling tube was kept warm throughout the process to prevent condensation before the absorption bottle. Two impact absorption bottles, each containing 50.0 mL of 0.010 mol / L sulfuric acid absorbent, were connected in series at the outlet. Samples were collected for the steam granulation, outer nitrogen source loading, and low-temperature drying stages, respectively. NH3-N in the absorbent was determined according to Nessler's reagent spectrophotometry as per HJ 533—2009. Quantitative dilution was performed if the absorbance exceeded the calibration range. The second-stage absorbance should be less than 5% of the total of the two stages; otherwise, the number of absorption stages was increased and the measurement was repeated. Ammonia loss at each stage was calculated by multiplying the absorbed NH3-N by the ratio of Q to the sampling flow rate. The process ammonia loss rate was the percentage of the sum of NH3-N losses at each stage to the total nitrogen input from the nitrogen-containing raw materials.

[0135] 7. 14-day cumulative ammonia volatilization rate in soil

[0136] Following the airflow sampling principle of GB / T 47215—2026 "Determination of Ammonia Volatilization in Soils", 500.0g of air-dried calcareous soil from the same batch was weighed and placed in a sealed incubator. Fertilizer samples were applied with an equal total nitrogen content, resulting in 200.0mg of total nitrogen per incubator. A blank soil sample without fertilizer was also included. The moisture content was adjusted to 60% of field capacity with deionized water and incubated at 25±1℃. Ammonia-removed air was continuously passed through at 1.00L / min. Two absorption bottles, each containing 50.0mL of 0.050mol / L sulfuric acid, were connected in series at the outlet. The absorbent solution was replaced and water was added to the original mass on days 1, 2, 3, 5, 7, 10, and 14. The NH4+ content of the absorbent solution was measured. + -N, sum after subtracting blanks. The cumulative ammonia volatilization rate over 14 days is calculated as "cumulative NH3-N over 14 days ÷ total nitrogen applied × 100%"; if this value is subtracted from 100%, it can only be expressed as the nitrogen retention rate through the ammonia volatilization pathway, which is not the same as the total nitrogen retention rate.

[0137] 8. Particle size compliance rate

[0138] Referring to GB / T 24891—2010 "Determination of Particle Size of Compound Fertilizers", approximately 200g of unground T4 finished product was weighed, accurate to 0.5g. A 4.75mm test sieve was placed on top of a 2.00mm test sieve, and a base plate was installed. The sample was placed on the upper sieve and mechanically vibrated for 5 minutes. The mass of particles that passed through the 4.75mm sieve and remained on the 2.00mm sieve was weighed. Particles trapped in the sieve holes were treated as not passing through the sieve. The pass rate for particles with a size of 2.00–4.75mm was calculated as the percentage of the mass of particles between the sieves to the total mass of the sample.

[0139] 9. Average compressive strength of particles

[0140] Referring to GB / T 44750—2024 "Measurement of Compressive Strength of Particles", 30 intact particles were randomly selected from the qualified particle size range of 2.00–4.75 mm. After equilibration for 24 hours at 25±1℃ and 50±5% relative humidity, each particle was placed between two parallel pressure plates of a particle strength tester and loaded at a constant beam speed of 5.0 mm / min until the particle first fractured. The peak load was recorded. Only invalid results caused by particle slippage or instrument instability were discarded and the test was repeated. The average compressive strength, standard deviation, and coefficient of variation of the 30 particles were reported, in N / particle.

[0141] Table 1:

[0142]

[0143] Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing embodiments or make equivalent substitutions for some of the technical features. Any modifications, equivalent substitutions, improvements, etc., made within the essence and principles of the present invention should be included within the protection scope of the present invention.

Claims

1. A method for preparing humic acid-containing organic-inorganic compound fertilizer by steam flash activation of weathered coal coupled with multiple nutrients, characterized in that, Includes the following steps: (1) The weathered coal is pre-wetted with at least one of sodium carbonate and potassium carbonate, and oxidized with hydrogen peroxide at 42-50℃; after the residual mass fraction of hydrogen peroxide in the wet material is not higher than 0.05%, at least one of sodium hydroxide and potassium hydroxide is added to make the pH of the 1:5 aqueous suspension of the material 10.0-11.0, and the moisture content of the material is adjusted to 30%-35%; (2) Introduce saturated steam with a gauge pressure of 0.08 to 0.12 MPa into the material obtained in step (1) to make the actual temperature of the material reach 115 to 122°C and maintain it for 2 to 4 minutes. Then, depressurize it to atmospheric pressure within 5 seconds to obtain flash activated material. (3) Cool the flash-activated material and introduce carbon dioxide in the powdered wet state to make the pH of the 1:5 aqueous suspension 8.0-8.5; mix the treated flash-activated material with organic materials, phosphate fertilizer, potassium fertilizer and micronutrient fertilizer without ammonium nitrogen, and granulate by drum granulation with steam without adding urea and ammonium nitrogen fertilizer to form core particles with a particle size of 0.8-1.5 mm; stop the steam, cool the core particles to below 40°C, and spray in ammonium dihydrogen phosphate aqueous solution so that the pH of the 1:5 aqueous suspension measured after the core particles are crushed as a whole is 7.0-7.6; (4) Urea, ammonium sulfate and ammonium-loaded clinoptilolite obtained by partial ion exchange of sodium clinoptilolite with ammonium sulfate aqueous solution are coated on the outside of the core particles in batches with a film-forming solution containing pregelatinized starch and lignin sulfonate. The particles are dried under the condition that the actual temperature of the particles does not exceed 55°C during the drying process to obtain the organic-inorganic compound fertilizer containing humic acid. The pH of the 1:5 aqueous suspension is the pH measured by mixing a representative powdered material or a material obtained by crushing a representative particle into deionized water at a mass ratio of 1:

5.

2. The method according to claim 1, characterized in that, The weathered coal has a total humic acid content of not less than 45% on a dry basis, an initial water-soluble humic acid content of not more than 10%, and a raw material moisture content of not more than 20%; the weathered coal is crushed to a D90 of not more than 0.25 mm before pre-wetting.

3. The method according to claim 2, characterized in that, Based on 100 parts by weight of dry-basis weathered coal, add 2.0–3.0 parts by weight of potassium carbonate and water, and mix at 40–45°C for 20–30 minutes to make the pH of the 1:5 aqueous suspension of the material 8.8–9.3; then add 4.0–6.0 parts by weight of 30% hydrogen peroxide aqueous solution within 20–30 minutes, and continue the reaction at 42–50°C for 30–45 minutes; after the residual hydrogen peroxide mass fraction is not higher than 0.05%, add 0.8–1.2 parts by weight of potassium hydroxide (pure weight) to make the pH of the 1:5 aqueous suspension of the material 10.3–10.

8.

4. The method according to claim 3, characterized in that, The pressurized steam treatment is carried out in a pressure-bearing rotary wet heat activator. After depressurization, the material enters a closed flash receiver. The flash activated material is cooled to below 40°C using air at a temperature not higher than 60°C and depolymerized to a D90 of not more than 0.25 mm. Before introducing carbon dioxide, its moisture content is adjusted to 25% to 32%.

5. The method according to claim 4, characterized in that, Under continuous material turning conditions, carbon dioxide with a volume fraction of not less than 95% is introduced, and the amount of carbon dioxide relative to the final dry basis of compound fertilizer is 3-8 kg / t; after stopping the aeration, continue mixing for no less than 10 minutes, and take the pH of the 1:5 aqueous suspension of the material reaching 8.0-8.5 as the treatment endpoint.

6. The method according to claim 1, characterized in that, The organic material is decomposed plant-derived organic material, the phosphate fertilizer is dicalcium phosphate, and the potassium fertilizer is potassium sulfate; the micronutrient fertilizer is selected from at least two of magnesium sulfate, zinc sulfate, manganese sulfate, ferrous sulfate, boric acid, and sodium molybdate; the actual material temperature during the drum granulation process is 45-55℃, the material moisture content is 6%-9%, and the granulation time is 6-10 min.

7. The method according to claim 1, characterized in that, After stopping the steam supply and cooling the core particles to 35-40°C, spray in an aqueous solution of ammonium dihydrogen phosphate with a mass fraction of 10%-20%. The amount of ammonium dihydrogen phosphate relative to the final dry base of the compound fertilizer is 4-6 kg / t. After spraying, continuously roll the core particles for 15-25 minutes so that the pH of the 1:5 aqueous suspension after whole crushing of the representative core particles is 7.0-7.

6. When retesting at 5-minute intervals, the pH should not be higher than 7.

8.

8. The method according to claim 1, characterized in that, The ammonium-supported clinoptilolite was prepared according to the following method: Natural clinoptilolite with a mineral content of not less than 70%, a cation exchange capacity of not less than 1.0 mmol / g, and a particle size of 100-200 mesh was selected. The natural clinoptilolite was mixed with an 8% sodium chloride aqueous solution at a dry basis mass ratio of 1:1.

5. The mixture was treated at 55-60℃ for 60-90 min, filtered, washed, and dried at 70-80℃ to obtain sodium-type clinoptilolite with a water content of not more than 8%. The sodium-type clinoptilolite is mixed with an aqueous solution of ammonium sulfate with a concentration of 1.0-1.3 mol / L at a liquid-to-solid ratio of 0.25-0.30 L / kg and treated at 30-40°C for 30-45 min to obtain ammonium-supported clinoptilolite that has undergone partial ion exchange. The ammonium-supported clinoptilolite is not subjected to high-temperature drying before coating.

9. The method according to claim 8, characterized in that, The dry basis mass ratio of urea to ammonium sulfate is 3:1 to 5:1, and the dry basis amount of ammonium-loaded clinoptilolite is 10% to 16% of the total dry basis mass of urea and ammonium sulfate; the film-forming solution includes 12% to 18% pregelatinized starch, 4% to 6% sodium lignin sulfonate and the balance water by mass percentage. Urea, ammonium sulfate (not used to prepare ammonium-supported clinoptilolite), and ammonium-supported clinoptilolite were divided into 2-3 batches. Before adding each batch of material, a portion of the film-forming liquid was sprayed onto the surface of the core particles. Then, the corresponding batch of urea, ammonium sulfate, and ammonium-supported clinoptilolite was added and rolled for 2-4 minutes. The above operation was repeated to form nitrogen-containing materials and ammonium-supported clinoptilolite on the outside of the core particles. The total coating time was 8-15 minutes, and the actual temperature of the particles during the coating process did not exceed 45°C.

10. The method according to claim 9, characterized in that, The coated granules are dried with low-humidity air at an inlet temperature not exceeding 60°C, and the actual temperature of the granules does not exceed 55°C during the drying process, until the moisture content of the granules does not exceed 3%. The dried granules are cooled to below 35°C, and granules with a particle size of 2.0 to 4.75 mm are screened out as finished products.