A method for preparing high-purity glycidyl methacrylate using composite catalysis

By combining a composite catalyst with a two-stage fixed-bed reactor, the problems of limited reaction equilibrium and low purity in the preparation process of glycidyl methacrylate in the existing technology have been solved, realizing the efficient preparation and continuous production of high-purity glycidyl methacrylate.

CN123106584APending Publication Date: 2026-11-17WEICHENG NEW MATERIALS (SHANDONG) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611386798.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-08
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing methods for preparing glycidyl methacrylate suffer from problems such as limited transesterification equilibrium, insufficient glycidyl conversion, insufficient catalyst selectivity, numerous ring-opening side reactions of epoxy groups, and high product purification load, making it difficult to obtain high-purity glycidyl methacrylate.

Method used

A method for preparing high-purity glycidyl methacrylate using a composite catalyst includes preliminary treatment of the mixture under nitrogen-oxygen mixed gas protection, transesterification reaction in a two-stage fixed-bed reactor, and a vacuum flash distillation process to remove light components. A composite functional catalyst with imidazole and quaternary phosphonium groups covalently introduced onto a silicon-based support is used, combined with a macroporous strong-base anion exchange resin and cyclic flash distillation to remove methanol, to achieve continuous operation.

Benefits of technology

It improves the conversion and selectivity of glycidyl methacrylate, reduces side reactions, simplifies catalyst separation and product purification processes, and improves product purity and yield, making it suitable for continuous production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

This invention relates to the field of materials chemistry, specifically disclosing a method for preparing high-purity glycidyl methacrylate using a composite catalysis method. The method includes: mixing methyl methacrylate, glycidyl methacrylate, and p-hydroxyanisole under a nitrogen-oxygen mixture; dehydrating and filtering the mixture to obtain an ester exchange feedstock; passing the ester exchange feedstock into a primary circulating fixed bed packed with a first ester exchange catalyst for a primary ester exchange reaction; circulating the resulting reaction solution after vacuum flash evaporation; and passing the side stream effluent into a secondary fixed bed packed with a composite functional catalyst for a deep ester exchange reaction; subsequently, removing light components under vacuum, adding p-hydroxyanisole, and vacuum distilling to collect the main fraction, yielding high-purity glycidyl methacrylate. This preparation method can improve the conversion rate of glycidyl methacrylate, the selectivity and yield of glycidyl methacrylate, reduce the risk of side reactions and catalyst residue, and is suitable for continuous preparation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of materials chemistry, and more specifically, to a method for preparing high-purity glycidyl methacrylate using composite catalysis. Background Technology

[0002] Glycidyl methacrylate is an important functional methacrylate monomer containing both polymerizable carbon-carbon double bonds and reactive epoxy groups in its molecule. It is widely used in acrylic resins, powder coatings, adhesives, electronic materials, and polymer modification materials. With increasing demands from downstream materials for weather resistance, adhesion, crosslinking density, and electrical properties, higher requirements are being placed on the purity, color, and impurity content of glycidyl methacrylate.

[0003] Existing methods for preparing glycidyl methacrylate mainly include the reaction of methacrylic acid with epichlorohydrin and the transesterification method of methyl methacrylate with glycidyl methacrylate. Among these, the transesterification method has advantages such as low by-salt formation, stable raw material sources, and suitability for continuous production. However, in actual preparation, problems still exist, including insufficient methanol removal, high residual glycidyl methacrylate, insufficient catalyst selectivity, and the tendency for epoxy groups to undergo ring-opening side reactions. These problems can easily lead to limited reaction equilibrium, complex crude product composition, increased subsequent distillation load, and affect the purity and yield of the final product.

[0004] In addition, while single solid base catalysts are easy to separate and operate in fixed beds, they often cannot balance catalytic activity and epoxy group stability when deeply converting residual glycidyl. Homogeneous catalysts, although having high reactivity, have drawbacks such as difficulty in removal, complex recovery, and difficulty in controlling product impurities.

[0005] Therefore, there is an urgent need to develop a composite catalytic method for preparing high-purity glycidyl methacrylate, which can improve the conversion rate of residual glycidyl methacrylate while ensuring the efficiency of transesterification reaction, reduce side reactions such as epoxy ring opening, and facilitate catalyst separation, light component recovery and continuous purification, thereby obtaining high-purity glycidyl methacrylate products. Summary of the Invention

[0006] To address the problems in existing technologies, such as limited equilibrium of transesterification reaction, insufficient glycidyl conversion, insufficient catalyst selectivity, numerous ring-opening side reactions of epoxy groups, and high product purification load, this invention provides a method for preparing high-purity glycidyl methacrylate using composite catalysis.

[0007] A method for preparing high-purity glycidyl methacrylate using a composite catalysis method includes the following preparation steps: S1. Under the protection of nitrogen and oxygen mixed gas, methyl methacrylate, glycidyl ether and p-hydroxyanisole are mixed and stirred evenly to obtain a mixture. The mixture is then dehydrated and filtered to obtain the transesterification feed liquid. S2. After heating the transesterification feed liquid to 72-76℃, it is passed into a primary circulating fixed-bed reactor filled with the first transesterification catalyst to carry out the primary transesterification reaction and obtain the primary transesterification reaction liquid. S3. The primary transesterification reaction liquid is subjected to vacuum flash vapor-liquid separation to obtain the extracted gas phase and liquid phase. The extracted gas phase is condensed and separated into methanol and methyl methacrylate. The obtained methyl methacrylate is returned to step S1 for use. The liquid phase is sent to a circulating storage tank and divided into a circulating reflux stream and a side-stream collected stream by a circulating pump. The circulating reflux stream is returned to the feed end of the primary circulating fixed bed reactor and mixed with the transesterification feed liquid for primary transesterification reaction. The side-stream collected stream is led out via a side stream and used as the liquid to be reacted in the next step. S4. The solution to be deeply reacted is passed into a two-stage fixed-bed reactor filled with a composite functional catalyst to carry out a deep transesterification reaction and obtain a deep transesterification reaction solution. S5. The deep transesterification reaction solution is subjected to vacuum stripping to obtain crude glycidyl methacrylate; the methyl methacrylate obtained after stripping is condensed and returned to step S1 for use. S6. Add p-hydroxyanisole to the crude glycidyl methacrylate and stir until homogeneous to obtain the crude product to be distilled. Perform vacuum distillation on the crude product to be distilled and collect the main fraction to obtain high-purity glycidyl methacrylate.

[0008] Preferably, in step S1, the oxygen volume fraction in the nitrogen-oxygen mixture is 4.5-5.5%, with the remainder being nitrogen; the flow rate of the nitrogen-oxygen mixture is 15-25 mL / min.

[0009] Preferably, in step S1, the mass ratio of methyl methacrylate, glycidyl ether, and p-hydroxyanisole is 3.3-3.5:1:0.0010-0.0015.

[0010] Preferably, the term "stirring evenly" in step S1 refers to stirring for 25-35 minutes at room temperature and a rotation speed of 220-280 r / min.

[0011] Preferably, in step S1, the dehydration and filtration process refers to: passing the mixture through a dehydration column packed with 3A molecular sieves for dehydration at a temperature of 25-32°C and a residence time of 20-30 minutes until the moisture content of the material is ≤0.05%; subsequently, filtering is performed using a polytetrafluoroethylene filter element with a pore size of 3-5 μm at a pressure of 0.05-0.15 MPa, and the filtrate is collected.

[0012] Preferably, the first ester exchange catalyst in step S2 is a macroporous, strongly basic styrene-based type I anion exchange resin.

[0013] Preferably, the conditions for the primary transesterification reaction in step S2 are: a pressure of 0.1-0.2 MPa in the primary circulating fixed-bed reactor and a liquid hourly space velocity of 0.65-0.85 h⁻¹. -1 The reflux ratio is 3.0-3.8:1, and the reaction residence time is 60-70 min.

[0014] Preferably, the vacuum flash vapor-liquid separation in step S3 specifically involves: introducing the primary transesterification reaction liquid into a vacuum flash evaporator at a temperature of 58-64℃ and an absolute pressure of 12-18kPa, and allowing it to remain for 8-12 minutes to remove the methanol generated by the reaction and the entrained methyl methacrylate from the liquid phase; wherein the methanol content in the liquid phase is ≤0.45%.

[0015] Preferably, the preparation method of the composite functional catalyst in step S4 includes the following steps: A1. Porous silica is added to hydrochloric acid solution for acidification treatment. After the treatment is completed, it is cooled, filtered, washed and dried to obtain hydroxylated silicon-based carrier. A2. Under inert gas protection, the hydroxylated silicon-based support was added to anhydrous toluene and stirred until homogeneous. Then, 3-chloropropyltrimethoxysilane was added and stirred to react. After the reaction was completed, the mixture was cooled, filtered, washed, and dried to obtain the chloropropylated silicon-based support. A3. Add the chloropropylated silicon-based support to anhydrous N,N-dimethylformamide, stir until homogeneous, add imidazole and anhydrous potassium carbonate, stir to react, after the reaction is complete, cool, filter and wash to obtain the imidazole-based silicon-based support wet filter cake. A4. Add the imidazole-based silicon-based carrier wet filter cake to anhydrous acetonitrile, add triphenylphosphine, stir to react, after the reaction is completed, cool, filter and wash to obtain silicon-based quaternary phosphonium chloride-imidazole carrier wet filter cake; A5. The wet filter cake of silicon-based quaternary phosphonium chloride-imidazolium carrier was added to sodium methacrylate solution for anion exchange, followed by filtration, washing and drying to obtain a composite functional catalyst.

[0016] Preferably, the mass ratio of porous silica to hydrochloric acid solution in step A1 is 1:4.8-5.2.

[0017] Preferably, the mass fraction of the hydrochloric acid solution in step A1 is 4.5-5.5%.

[0018] Preferably, the acidification treatment in step A1 refers to stirring for 2.5-3.0 hours at a temperature of 55-60℃ and a rotation speed of 260-320 r / min.

[0019] Preferably, the filtration, washing, and drying in step A1 refers to: using a polypropylene filter cloth with a pore size of 20-30μm, filtering under a relative pressure of -0.075MPa to -0.085MPa, washing the filter cake with deionized water until the pH of the washing solution is neutral, and then drying it at a temperature of 105-110℃ for 4-5 hours.

[0020] Preferably, in step A2, the mass ratio of the hydroxylated silicon-based support, 3-chloropropyltrimethoxysilane, and anhydrous toluene is 1:0.78-0.88:5.0-5.5.

[0021] Preferably, the term "stirring evenly" in step A2 refers to stirring for 20-30 minutes at room temperature and a rotation speed of 240-300 r / min.

[0022] Preferably, the stirring reaction in step A2 refers to stirring the reaction for 7-8 hours at a temperature of 82-88℃ and a rotation speed of 260-320 r / min.

[0023] Preferably, in step A2, the filtration, washing, and drying process refers to: using a polytetrafluoroethylene filter membrane with a pore size of 10-20 μm, filtering under a relative pressure of -0.075 MPa to -0.085 MPa, washing the filter cake 2-3 times each with anhydrous toluene and anhydrous ethanol, and then drying it for 4-5 hours at a temperature of 60-65℃ and an absolute pressure of 3-5 kPa.

[0024] Preferably, in step A3, the mass ratio of chloropropyl silicon-based carrier, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide is 1:0.12-0.18:0.16-0.24:4.8-5.8.

[0025] Preferably, the term "stirring evenly" in step A3 refers to stirring for 20-30 minutes at room temperature and a rotation speed of 240-300 r / min.

[0026] Preferably, the stirring reaction in step A3 refers to stirring the reaction for 5.5-6.5 hours at a temperature of 72-76℃ and a rotation speed of 280-340 r / min.

[0027] Preferably, in step A3, the filtration and washing process refers to: using a polytetrafluoroethylene filter membrane with a pore size of 10-20 μm, filtering under a relative pressure of -0.075 MPa to -0.085 MPa, and washing the filter cake twice each with anhydrous N,N-dimethylformamide, anhydrous ethanol, and anhydrous acetonitrile.

[0028] Preferably, in step A4, the mass ratio of the imidazole-based silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile is 1:0.24-0.30:4.5-5.2.

[0029] Preferably, the stirring reaction in step A4 refers to stirring the reaction for 10-12 hours at a temperature of 78-82℃ and a rotation speed of 280-340 r / min.

[0030] Preferably, the filtration and washing in step A4 refers to: using a polytetrafluoroethylene filter membrane with a pore size of 10-20 μm, filtering under a relative pressure of -0.075 MPa to -0.085 MPa, and washing the filter cake with anhydrous acetonitrile and methyl methacrylate 2-3 times each.

[0031] Preferably, in step A5, the mass ratio of the silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake to the sodium methacrylate solution is 1:4.2-4.8.

[0032] Preferably, the sodium methacrylate solution in step A5 comprises the following components by mass percentage: 8.5-9.5% sodium methacrylate, 0.01-0.02% p-hydroxyanisole, 10-12% deionized water, and the balance being methanol.

[0033] Preferably, the anion exchange in step A5 refers to stirring for 2.5-3.5 hours under the protection of a nitrogen-oxygen mixture at a temperature of 30-35°C and a rotation speed of 240-300 r / min.

[0034] Preferably, the filtration, washing, and drying in step A5 refers to: using a polytetrafluoroethylene filter membrane with a pore size of 10-20 μm, filtering under a relative pressure of -0.075 MPa to -0.085 MPa, washing the filter cake first with a methanol-water mixture (prepared by mixing anhydrous methanol and deionized water in a volume ratio of 3:1) until the chloride ion content in the washing solution is ≤0.05%, then washing it 2-3 times with a sodium methacrylate solution, and then vacuum drying it for 4-5 hours under a temperature of 45-50℃ and an absolute pressure of 3-5 kPa.

[0035] Preferably, the conditions for the deep transesterification reaction in step S4 are: a pressure of 0.1-0.2 MPa in the two-stage fixed-bed reactor and a liquid hourly space velocity of 0.45-0.55 h⁻¹. -1 The reaction residence time is 100-120 min.

[0036] Preferably, the depressurization removal of light components in step S5 specifically involves: preheating the deep transesterification reaction solution to 55-65°C and then feeding it into the light component removal tower through the upper feed inlet. The light component removal tower is filled with structured stainless steel packing with a theoretical number of 12-18 plates. The absolute pressure at the top of the tower is controlled at 10-16 kPa, the top temperature at 38-46°C, the bottom temperature at 72-80°C, the reflux ratio at 0.8-1.3:1, and the residence time of the material in the bottom of the tower at 30-40 min. During the light component removal process, a nitrogen-oxygen mixture is introduced into the bottom of the tower, and the flow rate of the nitrogen-oxygen mixture is controlled at 10-20 mL / min. After the gas phase at the top of the tower is condensed at 5-10°C, a light component containing methanol and methyl methacrylate is obtained. When the content of methyl methacrylate in the bottom material is ≤0.5% and the content of methanol is ≤0.05%, the light component removal process is stopped, and the bottom product is crude glycidyl methacrylate.

[0037] Preferably, in step S6, the mass of p-hydroxyanisole is 0.05-0.06% of the crude glycidyl methacrylate mass.

[0038] Preferably, the term "stirring evenly" in step S6 refers to stirring for 15-25 minutes at a temperature of 25-35℃ and a rotation speed of 180-250 r / min.

[0039] Preferably, the vacuum distillation in step S6 specifically involves: preheating the crude product to be distilled to 45-55°C, and then feeding it into the vacuum distillation column through the feed inlet in the middle of the column. The vacuum distillation column is filled with structured stainless steel packing, with a theoretical number of 18-25 plates. The absolute pressure at the top of the column is controlled at 0.7-1.0 kPa, the top temperature at 65-72°C, the bottom temperature at no higher than 92°C, the reflux ratio at 1.5-2.2:1, and the residence time of the material in the bottom of the column at 25-35 min. During the distillation process, the product is refluxed into the top reflux tank. A nitrogen-oxygen mixture is introduced, with a flow rate of 5-10 mL / min. The vapor phase at the top of the column is condensed at 5-10℃ and then enters the reflux tank. It is stabilized under total reflux conditions for 10-20 min, and then the fore fraction is collected at a reflux ratio of 1.5-2.2:1. When the content of methyl methacrylate in the fore fraction is ≤0.10%, methanol content is ≤0.01%, and glycidyl methacrylate content is ≤0.10%, the main fraction is switched to be collected. When the content of glycidyl methacrylate in the main fraction is <99.5%, the collection of the main fraction is stopped.

[0040] In summary, the present invention has the following beneficial effects: 1. This invention covalently introduces imidazole and quaternary phosphonium groups onto the surface of a silicon-based support, forming a composite functional catalyst through methacrylate anion exchange. The imidazole group serves as a weakly basic activation site, promoting the activation of glycidyl hydroxyl groups; the quaternary phosphonium methacrylate structure improves the ionic environment on the catalyst surface and helps stabilize the active intermediate state during the transesterification reaction. The immobilization of these two types of active sites on the same porous support surface enhances the contact efficiency of reactants within the catalyst channels, thereby increasing the conversion rate and selectivity of the deep transesterification reaction. Since the catalyst counterion is methacrylate, it exhibits good structural compatibility with the reaction system, reducing the adverse effects of residual foreign anions on product quality and lowering the risk of halogen impurity residues.

[0041] 2. This invention employs a two-stage reaction process combining a primary macroporous strong-base anion exchange resin fixed bed, a circulating flash evaporation for methanol removal, and a secondary composite functional catalyst fixed bed. The primary fixed bed mainly completes the main transesterification reaction and improves the contact efficiency between the material and the resin bed through reflux. After the primary reaction liquid undergoes vacuum flash evaporation to remove byproduct methanol, it can shift the transesterification equilibrium towards the formation of glycidyl methacrylate. The secondary fixed bed performs deep conversion of residual reactants under low methanol content conditions, avoiding the increase in side reactions caused by excessively increasing the temperature or extending the residence time in a single-stage reactor to improve the conversion rate.

[0042] 3. This invention employs a supported catalyst and a tubular fixed-bed reactor for continuous operation. The catalyst's active sites are covalently fixed to the support surface, and the reaction liquid separates from the catalyst after passing through the catalyst bed. This method reduces the risk of catalyst residue entering the product. Simultaneously, continuous fixed-bed operation helps maintain stable reaction conditions, facilitates integration with subsequent flash evaporation, reflux, and distillation units, and is suitable for continuous scale-up production.

[0043] 4. This invention incorporates polymerization inhibition protection and low-temperature, reduced-pressure operation conditions during the reaction, removal of light components, and distillation processes. By introducing oxygen-containing nitrogen gas and adding p-hydroxyanisole in stages, the free radical polymerization of glycidyl methacrylate under heated conditions can be inhibited. Lowering the operating temperature through reduced-pressure flash evaporation and reduced-pressure distillation, and controlling the residence time of materials in the high-temperature region, reduces thermal polymerization, ring-opening of epoxy groups, and the formation of heavy components. These measures help reduce product color and polymerization loss, and improve the purity and yield of glycidyl methacrylate. Detailed Implementation

[0044] The present invention will be further described in detail below with reference to the embodiments.

[0045] For experiments not specifically described in the examples, the procedures or conditions should be followed according to the conventional experimental procedures described in the literature in this field. Reagents or instruments whose manufacturers are not specified are all commercially available conventional reagent products.

[0046] The key raw materials used in the embodiments and comparative examples of this invention are sourced from the following sources: The porous silica was purchased from Rizhao KEPNO New Materials Co., Ltd., brand: KEPNO, particle size: 40 mesh; 3-Chloropropyltrimethoxysilane was purchased from Jiangsu Bost Chemical Technology Co., Ltd., CAS No.: 2530-87-2; The macroporous, strongly basic styrene-based type I anion exchange resin was purchased from Anhui Wanshu Chemical Sales Co., Ltd., grade: D231#.

[0047] Examples 1-3 provide a method for preparing high-purity glycidyl methacrylate using a composite catalysis.

[0048] Example 1 The preparation method of the composite functional catalyst includes the following steps: A1. The mass ratio of porous silica to hydrochloric acid solution was controlled at 1:4.8. Porous silica was added to a 4.5% hydrochloric acid solution and stirred for 3.0 h at 55℃ and 260 r / min. After treatment, the solution was cooled to room temperature and filtered using a 20 μm pore size polypropylene filter cloth at a relative pressure of -0.075 MPa. The filter cake was washed with deionized water until the pH of the washing solution was neutral and then dried at 105℃ for 5 h to obtain a hydroxylated silica-based support. A2. The mass ratio of hydroxylated silicon-based support, 3-chloropropyltrimethoxysilane, and anhydrous toluene was controlled at 1:0.78:5.0. Under nitrogen protection, the hydroxylated silicon-based support was added to anhydrous toluene and stirred for 30 min at room temperature and 240 r / min. Then, 3-chloropropyltrimethoxysilane was added, and the mixture was stirred for 8 h at 82 °C and 260 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 10 μm at a relative pressure of -0.075 MPa. The filter cake was washed twice each with anhydrous toluene and anhydrous ethanol, and then dried for 5 h at 60 °C and 3 kPa to obtain the chloropropylated silicon-based support. A3. The mass ratio of chloropropylated silicon-based support, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide was controlled at 1:0.12:0.16:4.8. The chloropropylated silicon-based support was added to anhydrous N,N-dimethylformamide and stirred for 30 min at room temperature and 240 r / min. Imidazole and anhydrous potassium carbonate were added, and the mixture was stirred for 6.5 h at 72 °C and 280 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 10 μm at a relative pressure of -0.075 MPa. The filter cake was washed twice each with anhydrous N,N-dimethylformamide, anhydrous ethanol, and anhydrous acetonitrile to obtain a wet filter cake of imidazoleized silicon-based support. A4. The mass ratio of imidazole-based silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile was controlled at 1:0.24:4.5. The imidazole-based silicon-based carrier wet filter cake was added to anhydrous acetonitrile, and triphenylphosphine was added. The mixture was stirred and reacted for 12 hours at a temperature of 78℃ and a rotation speed of 280 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 10 μm at a relative pressure of -0.075 MPa. The filter cake was washed twice each with anhydrous acetonitrile and methyl methacrylate to obtain a silicon-based quaternary phosphonium chloride-imidazole carrier wet filter cake. A5. The mass ratio of the silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake to the sodium methacrylate solution was controlled at 1:4.2. The silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake was added to the sodium methacrylate solution (the sodium methacrylate solution contains the following components by mass percentage: sodium methacrylate 8.5%, p-hydroxyanisole 0.01%, deionized water 10%, and the balance being methanol). Under the protection of nitrogen and oxygen mixed gas, the mixture was stirred for 3.5 h at 30℃ and 240 r / min for anion exchange. Then, it was filtered using a polytetrafluoroethylene filter membrane with a pore size of 10 μm at a relative pressure of -0.075 MPa. The filter cake was first washed with a methanol-water mixture (prepared by mixing anhydrous methanol and deionized water at a volume ratio of 3:1) until the chloride ion content in the washing solution was ≤0.05%. Then, it was washed twice with the sodium methacrylate solution. Finally, it was vacuum dried for 5 h at 45℃ and 3 kPa to obtain the composite functional catalyst. A method for preparing high-purity glycidyl methacrylate using a composite catalysis method includes the following preparation steps: S1. The mass ratio of methyl methacrylate, glycidyl ether, and p-hydroxyanisole is controlled at 3.3:1:0.0010. Under the protection of a nitrogen-oxygen mixture (oxygen volume fraction of 4.5%, balance nitrogen, and flow rate of 15 mL / min), methyl methacrylate, glycidyl ether, and p-hydroxyanisole are mixed and stirred for 35 min at room temperature and 220 r / min to obtain a mixture. The mixture is then dehydrated through a dehydration column packed with 3A molecular sieves at a dehydration temperature of 25℃ and a residence time of 30 min until the moisture content of the material is ≤0.05%. Subsequently, the mixture is filtered using a polytetrafluoroethylene filter with a pore size of 3 μm at a pressure of 0.05 MPa, and the filtrate is collected to obtain the transesterification feed solution. S2. After heating the ester exchange feed solution to 72°C, it is passed from bottom to top into a primary circulating fixed-bed reactor packed with macroporous strong-base styrene-based type I anion exchange resin. The pressure inside the reactor is controlled at 0.1 MPa and the liquid hourly space velocity is 0.65 h⁻¹. -1 The primary transesterification reaction was carried out with a circulation-reflux ratio of 3.0:1 and a reaction residence time of 70 min to obtain the primary transesterification reaction solution. S3. The primary transesterification reaction liquid is introduced into a vacuum flash evaporator at a temperature of 58°C and an absolute pressure of 12 kPa, and held for 12 minutes to allow the methanol and entrained methyl methacrylate generated in the reaction to be removed from the liquid phase, resulting in a gas phase and a liquid phase. The removed gas phase is condensed at 5°C to separate methanol and methyl methacrylate, and the obtained methyl methacrylate is returned to step S1 for use. The methanol content in the liquid phase is ≤0.45%. The liquid phase is sent to a circulating storage tank and divided into a circulating reflux stream and a side-stream sampled stream by a circulating pump. The circulating reflux stream is returned to the feed end of the primary circulating fixed-bed reactor, mixed with the transesterification feed liquid, and then subjected to the primary transesterification reaction. The side-stream sampled stream is led out via a side stream and used as the liquid for further reaction in the next step. S4. After preheating the reaction solution to 76°C, introduce it into a two-stage fixed-bed reactor packed with a composite functional catalyst. Control the pressure inside the reactor at 0.1 MPa and the liquid hourly space velocity at 0.45 h⁻¹. -1 The reaction residence time was 120 min to carry out a deep transesterification reaction and obtain a deep transesterification reaction solution. S5. After preheating the deep transesterification reaction solution to 55°C, it is fed into the light component removal tower from the upper feed inlet. The light component removal tower is filled with stainless steel structured packing, with a theoretical number of 12 plates. The absolute pressure at the top of the tower is controlled at 10 kPa, the top temperature at 38°C, the bottom temperature at 72°C, the reflux ratio at 0.8:1, and the residence time of the material in the bottom of the tower at 40 min. During the light component removal process, a nitrogen-oxygen mixture is introduced into the bottom of the tower at a flow rate of 10 mL / min. After the gas phase at the top of the tower is condensed at 5°C, a light component containing methanol and methyl methacrylate is obtained. When the methyl methacrylate content in the bottom material is ≤0.5% and the methanol content is ≤0.05%, the light component removal process is stopped, and the bottom product is crude glycidyl methacrylate. S6. Add p-hydroxyanisole (mass equal to 0.05% of the crude glycidyl methacrylate mass) to the crude glycidyl methacrylate, and stir for 25 minutes at 25℃ and 180 r / min to obtain the crude product to be refined. Preheat the crude product to 45℃, and then feed it into the vacuum distillation column through the feed inlet in the middle of the column. The vacuum distillation column is packed with structured stainless steel packing, with a theoretical number of 18 plates. Control the absolute pressure at the top of the column to 0.7 kPa, the top temperature to 65℃, the bottom temperature to no higher than 92℃, the reflux ratio to 1.5:1, and the residence time of the material in the bottom of the column. The interval is 35 min; during the distillation process, a nitrogen-oxygen mixture is introduced into the reflux tank at the top of the column, and the flow rate of the nitrogen-oxygen mixture is controlled at 5 mL / min. The gas phase at the top of the column is condensed at 5℃ and then enters the reflux tank. It is first stabilized under total reflux conditions for 10 min, and then the fore fraction is collected at a reflux ratio of 1.5:1. When the content of methyl methacrylate in the fore fraction is ≤0.10%, the content of methanol is ≤0.01%, and the content of glycidyl methacrylate is ≤0.10%, the main fraction is switched to be collected. When the content of glycidyl methacrylate in the main fraction is <99.5%, the collection of the main fraction is stopped. The obtained main fraction is high-purity glycidyl methacrylate.

[0049] Example 2 The preparation method of the composite functional catalyst includes the following steps: A1. The mass ratio of porous silica to hydrochloric acid solution was controlled at 1:5. Porous silica was added to a 5% hydrochloric acid solution and stirred for 2.75 h at 58℃ and 290 r / min. After treatment, the solution was cooled to room temperature and filtered using a 25 μm pore size polypropylene filter cloth at a relative pressure of -0.080 MPa. The filter cake was washed with deionized water until the pH of the washing solution was neutral, and then dried at 108℃ for 4.5 h to obtain a hydroxylated silica-based support. A2. The mass ratio of hydroxylated silicon-based support, 3-chloropropyltrimethoxysilane, and anhydrous toluene was controlled at 1:0.83:5.3. Under nitrogen protection, the hydroxylated silicon-based support was added to anhydrous toluene and stirred for 25 min at room temperature and 270 r / min. Then, 3-chloropropyltrimethoxysilane was added, and the mixture was stirred for 7.5 h at 85 °C and 290 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a 15 μm polytetrafluoroethylene filter membrane at a relative pressure of -0.080 MPa. The filter cake was washed three times each with anhydrous toluene and anhydrous ethanol, and then dried for 4.5 h at 63 °C and 4 kPa to obtain the chloropropylated silicon-based support. A3. The mass ratio of chloropropylated silicon-based support, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide was controlled at 1:0.15:0.20:5.3. The chloropropylated silicon-based support was added to anhydrous N,N-dimethylformamide and stirred for 25 min at room temperature and 270 r / min. Imidazole and anhydrous potassium carbonate were added, and the mixture was stirred for 6 h at 74℃ and 310 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 15 μm at a relative pressure of -0.080 MPa. The filter cake was washed twice each with anhydrous N,N-dimethylformamide, anhydrous ethanol, and anhydrous acetonitrile to obtain a wet filter cake of imidazoleized silicon-based support. A4. The mass ratio of imidazole-based silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile was controlled at 1:0.27:4.8. The imidazole-based silicon-based carrier wet filter cake was added to anhydrous acetonitrile, and triphenylphosphine was added. The mixture was stirred and reacted for 11 hours at a temperature of 80℃ and a rotation speed of 310 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 15 μm at a relative pressure of -0.080 MPa. The filter cake was washed three times each with anhydrous acetonitrile and methyl methacrylate to obtain a silicon-based quaternary phosphonium chloride-imidazole carrier wet filter cake. A5. The mass ratio of the silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake to the sodium methacrylate solution was controlled at 1:4.5. The silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake was added to the sodium methacrylate solution (the sodium methacrylate solution includes the following components by mass percentage: sodium methacrylate 9%, p-hydroxyanisole 0.015%, deionized water 11%, and the balance being methanol). Anion exchange was carried out under nitrogen-oxygen mixed gas protection at a temperature of 33℃ and a rotation speed of 270 r / min for 3 h. Then, the filter cake was filtered using a polytetrafluoroethylene filter membrane with a pore size of 15 μm at a relative pressure of -0.080 MPa. The filter cake was first washed with a methanol-water mixture (prepared by mixing anhydrous methanol and deionized water at a volume ratio of 3:1) until the chloride ion content in the washing solution was ≤0.05%. Then, it was washed three times with the sodium methacrylate solution. Finally, it was vacuum dried at a temperature of 48℃ and an absolute pressure of 4 kPa for 4.5 h to obtain the composite functional catalyst. A method for preparing high-purity glycidyl methacrylate using a composite catalysis method includes the following preparation steps: S1. The mass ratio of methyl methacrylate, glycidyl ether, and p-hydroxyanisole is controlled at 3.4:1:0.0013. Under the protection of a nitrogen-oxygen mixture (the volume fraction of oxygen in the nitrogen-oxygen mixture is 5.0%, and the balance is nitrogen, with an inflow rate of 20 mL / min), methyl methacrylate, glycidyl ether, and p-hydroxyanisole are mixed and stirred for 30 min at room temperature and a rotation speed of 250 r / min to obtain a mixture. The mixture is then dehydrated by passing it through a dehydration column packed with 3A molecular sieves at a dehydration temperature of 28℃ and a residence time of 25 min until the moisture content of the material is ≤0.05%. Subsequently, the mixture is filtered using a polytetrafluoroethylene filter element with a pore size of 4 μm at a pressure of 0.1 MPa, and the filtrate is collected to obtain the transesterification feed solution. S2. After heating the ester exchange feed solution to 74°C, it is passed from bottom to top into a primary circulating fixed-bed reactor packed with macroporous strong-base styrene-based type I anion exchange resin. The pressure inside the reactor is controlled at 0.15 MPa and the liquid hourly space velocity is 0.75 h⁻¹. -1 The primary transesterification reaction was carried out with a circulation-reflux ratio of 3.4:1 and a reaction residence time of 65 min to obtain the primary transesterification reaction solution. S3. The primary transesterification reaction liquid is introduced into a vacuum flash evaporator at a temperature of 61°C and an absolute pressure of 15 kPa, and held for 10 minutes to allow the methanol and entrained methyl methacrylate generated in the reaction to be removed from the liquid phase, resulting in a gas phase and a liquid phase. The removed gas phase is condensed at 8°C to separate methanol and methyl methacrylate, and the obtained methyl methacrylate is returned to step S1 for use. The methanol content in the liquid phase is ≤0.45%. The liquid phase is sent to a circulating storage tank and divided into a circulating reflux stream and a side-stream sampled stream by a circulating pump. The circulating reflux stream is returned to the feed end of the primary circulating fixed-bed reactor, mixed with the transesterification feed liquid, and then subjected to the primary transesterification reaction. The side-stream sampled stream is led out via a side stream and used as the liquid for further reaction in the next step. S4. After preheating the reaction solution to 79°C, introduce it into a two-stage fixed-bed reactor packed with a composite functional catalyst. Control the reactor pressure at 0.15 MPa and the liquid hourly space velocity at 0.5 h⁻¹. -1 The reaction residence time was 110 min, and a deep transesterification reaction was carried out to obtain a deep transesterification reaction solution. S5. After preheating the deep transesterification reaction solution to 60°C, it is fed into the light component removal tower from the upper feed inlet. The light component removal tower is filled with stainless steel structured packing, with a theoretical number of 15 plates. The absolute pressure at the top of the tower is controlled at 13 kPa, the top temperature at 42°C, the bottom temperature at 76°C, the reflux ratio at 1:1, and the residence time of the material in the bottom of the tower at 35 min. During the light component removal process, a nitrogen-oxygen mixture is introduced into the bottom of the tower at a flow rate of 15 mL / min. After the gas phase at the top of the tower is condensed at 8°C, a light component containing methanol and methyl methacrylate is obtained. When the methyl methacrylate content in the bottom material is ≤0.5% and the methanol content is ≤0.05%, the light component removal process is stopped, and the bottom product is crude glycidyl methacrylate. S6. Add p-hydroxyanisole (mass equal to 0.055% of the crude glycidyl methacrylate mass) to the crude glycidyl methacrylate, and stir for 20 minutes at 30℃ and 220 r / min to obtain the crude product to be refined. Preheat the crude product to 50℃ and then feed it into the vacuum distillation column through the feed inlet in the middle of the column. The vacuum distillation column is packed with structured stainless steel packing, with a theoretical number of 22 plates. Control the absolute pressure at the top of the column to 0.8 kPa, the top temperature to 69℃, the bottom temperature to no higher than 92℃, the reflux ratio to 1.9:1, and the residence time of the material in the bottom of the column. The interval is 30 min; during the distillation process, a nitrogen-oxygen mixture is introduced into the reflux tank at the top of the column, and the flow rate of the nitrogen-oxygen mixture is controlled at 8 mL / min. The gas phase at the top of the column is condensed at 8℃ and then enters the reflux tank. It is first stabilized under total reflux conditions for 15 min, and then the fore fraction is collected at a reflux ratio of 1.8:1. When the content of methyl methacrylate in the fore fraction is ≤0.10%, the content of methanol is ≤0.01%, and the content of glycidyl methacrylate is ≤0.10%, the main fraction is switched to be collected. When the content of glycidyl methacrylate in the main fraction is <99.5%, the collection of the main fraction is stopped. The obtained main fraction is high-purity glycidyl methacrylate.

[0050] Example 3 The preparation method of the composite functional catalyst includes the following steps: A1. The mass ratio of porous silica to hydrochloric acid solution was controlled at 1:5.2. The porous silica was added to a 5.5% hydrochloric acid solution and stirred for 2.5 h at 60℃ and 320 r / min. After treatment, the solution was cooled to room temperature and filtered using a 30 μm pore size polypropylene filter cloth at a relative pressure of -0.085 MPa. The filter cake was washed with deionized water until the pH of the washing solution was neutral, and then dried at 110℃ for 4 h to obtain a hydroxylated silica-based support. A2. The mass ratio of hydroxylated silicon-based support, 3-chloropropyltrimethoxysilane, and anhydrous toluene was controlled at 1:0.88:5.5. Under nitrogen protection, the hydroxylated silicon-based support was added to anhydrous toluene and stirred for 20 min at room temperature and 300 r / min. Then, 3-chloropropyltrimethoxysilane was added, and the mixture was stirred for 7 h at 88 °C and 320 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 20 μm at a relative pressure of -0.085 MPa. The filter cake was washed three times each with anhydrous toluene and anhydrous ethanol, and then dried for 4 h at 65 °C and 5 kPa to obtain the chloropropylated silicon-based support. A3. The mass ratio of chloropropylated silicon-based support, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide was controlled at 1:0.18:0.24:5.8. The chloropropylated silicon-based support was added to anhydrous N,N-dimethylformamide and stirred for 20 min at room temperature and 300 r / min. Then, imidazole and anhydrous potassium carbonate were added, and the mixture was stirred for 5.5 h at 76 °C and 340 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 20 μm at a relative pressure of -0.085 MPa. The filter cake was washed twice each with anhydrous N,N-dimethylformamide, anhydrous ethanol, and anhydrous acetonitrile to obtain a wet filter cake of imidazoleized silicon-based support. A4. The mass ratio of imidazole-based silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile was controlled at 1:0.30:5.2. The imidazole-based silicon-based carrier wet filter cake was added to anhydrous acetonitrile, and triphenylphosphine was added. The mixture was stirred and reacted for 10 h at a temperature of 82℃ and a rotation speed of 340 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a polytetrafluoroethylene filter membrane with a pore size of 20 μm at a relative pressure of -0.085 MPa. The filter cake was washed three times each with anhydrous acetonitrile and methyl methacrylate to obtain a silicon-based quaternary phosphonium chloride-imidazole carrier wet filter cake. A5. The mass ratio of the silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake to the sodium methacrylate solution was controlled at 1:4.8. The silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake was added to the sodium methacrylate solution (the sodium methacrylate solution includes the following components by mass percentage: sodium methacrylate 9.5%, p-hydroxyanisole 0.02%, deionized water 12%, and the balance being methanol). Under the protection of nitrogen and oxygen mixed gas, the mixture was stirred for 2.5 h at 35℃ and 300 r / min for anion exchange. Then, it was filtered using a polytetrafluoroethylene filter membrane with a pore size of 20 μm at a relative pressure of -0.085 MPa. The filter cake was first washed with a methanol-water mixture (prepared by mixing anhydrous methanol and deionized water at a volume ratio of 3:1) until the chloride ion content in the washing solution was ≤0.05%. Then, it was washed three times with the sodium methacrylate solution. Finally, it was vacuum dried for 4 h at 50℃ and 5 kPa to obtain the composite functional catalyst. A method for preparing high-purity glycidyl methacrylate using a composite catalysis method includes the following preparation steps: S1. The mass ratio of methyl methacrylate, glycidyl ether, and p-hydroxyanisole is controlled at 3.5:1:0.0015. Under the protection of a nitrogen-oxygen mixture (the volume fraction of oxygen in the nitrogen-oxygen mixture is 5.5%, and the balance is nitrogen, with an inflow rate of 25 mL / min), methyl methacrylate, glycidyl ether, and p-hydroxyanisole are mixed and stirred for 25 min at room temperature and a rotation speed of 280 r / min to obtain a mixture. The mixture is then dehydrated by passing it through a dehydration column packed with 3A molecular sieves at a dehydration temperature of 32℃ and a residence time of 20 min until the moisture content of the material is ≤0.05%. Subsequently, the mixture is filtered using a polytetrafluoroethylene filter element with a pore size of 5 μm at a pressure of 0.15 MPa, and the filtrate is collected to obtain the transesterification feed solution. S2. After heating the ester exchange feed solution to 76°C, it is fed from bottom to top into a primary circulating fixed-bed reactor packed with macroporous strong-base styrene-based type I anion exchange resin. The pressure inside the reactor is controlled at 0.2 MPa and the liquid hourly space velocity is 0.85 h⁻¹. -1 The primary transesterification reaction was carried out with a circulation-reflux ratio of 3.8:1 and a reaction residence time of 60 min to obtain the primary transesterification reaction solution. S3. The primary transesterification reaction liquid is introduced into a vacuum flash evaporator at a temperature of 64℃ and an absolute pressure of 18kPa, and held for 8 minutes to allow the methanol and entrained methyl methacrylate generated in the reaction to be removed from the liquid phase, resulting in a gas phase and a liquid phase. The removed gas phase is condensed at 10℃ to separate methanol and methyl methacrylate, and the obtained methyl methacrylate is returned to step S1 for use. The methanol content in the liquid phase is ≤0.45%. The liquid phase is sent to a circulating storage tank and divided into a circulating reflux stream and a side-stream sampled stream by a circulating pump. The circulating reflux stream is returned to the feed end of the primary circulating fixed-bed reactor, mixed with the transesterification feed liquid, and then carried out a primary transesterification reaction. The side-stream sampled stream is led out via a side stream and used as the liquid for further reaction in the next step. S4. After preheating the reaction solution to 82°C, introduce it into a two-stage fixed-bed reactor packed with a composite functional catalyst. Control the pressure inside the reactor at 0.2 MPa and the liquid hourly space velocity at 0.55 h⁻¹. -1 The reaction residence time was 100 min, and a deep transesterification reaction was carried out to obtain a deep transesterification reaction solution. S5. After preheating the deep transesterification reaction solution to 65°C, it is fed into the light component removal tower from the upper feed inlet. The light component removal tower is filled with stainless steel structured packing, with a theoretical number of 18 plates. The absolute pressure at the top of the tower is controlled at 16 kPa, the top temperature at 46°C, the bottom temperature at 80°C, the reflux ratio at 1.3:1, and the residence time of the material in the bottom of the tower at 30 min. During the light component removal process, a nitrogen-oxygen mixture is introduced into the bottom of the tower at a flow rate of 20 mL / min. After the gas phase at the top of the tower is condensed at 10°C, a light component containing methanol and methyl methacrylate is obtained. When the methyl methacrylate content in the bottom material is ≤0.5% and the methanol content is ≤0.05%, the light component removal process is stopped, and the bottom product is crude glycidyl methacrylate. S6. Add p-hydroxyanisole (mass equal to 0.06% of the crude glycidyl methacrylate) to the crude glycidyl methacrylate, and stir for 15 minutes at 35℃ and 250 r / min to obtain the crude product to be refined. Preheat the crude product to 55℃ and then feed it into the vacuum distillation column through the feed inlet in the middle of the column. The vacuum distillation column is packed with structured stainless steel packing, with a theoretical number of 25 plates. Control the absolute pressure at the top of the column to 1.0 kPa, the top temperature to 72℃, the bottom temperature to no higher than 92℃, the reflux ratio to 2.2:1, and the residence time of the material in the bottom of the column. The distillation process takes 25 minutes. During the distillation, a nitrogen-oxygen mixture is introduced into the reflux tank at the top of the column, with the flow rate controlled at 10 mL / min. The vapor phase at the top of the column is condensed at 10°C and then enters the reflux tank. The reflux is stabilized for 20 minutes under total reflux conditions, and then the fore fraction is collected at a reflux ratio of 2.2:1. When the content of methyl methacrylate in the fore fraction is ≤0.10%, the content of methanol is ≤0.01%, and the content of glycidyl methacrylate is ≤0.10%, the main fraction is switched to be collected. When the content of glycidyl methacrylate in the main fraction is <99.5%, the collection of the main fraction is stopped, and the obtained main fraction is high-purity glycidyl methacrylate.

[0051] To verify the overall performance of the glycidyl methacrylate prepared in Examples 1-3 of this invention, the inventors set up Comparative Examples 1-6, as follows: Comparative Example 1 The difference between this comparative example and Example 1 is that step A3 is omitted, and the imidazole silicon-based carrier wet filter cake in the original step A4 is replaced with the chloropropyl silicon-based carrier in step A2. The remaining steps and raw materials are the same as in Example 1.

[0052] Comparative Example 2 The difference between this comparative example and Example 1 is that the composite functional catalyst is replaced by an imidazole silicon-based support of equal mass, while the remaining steps and raw materials are the same as in Example 1. Specifically: A3. The mass ratio of chloropropylated silicon-based support, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide was controlled at 1:0.08:0.10:4.5. The chloropropylated silicon-based support was added to anhydrous N,N-dimethylformamide and stirred for 30 min at room temperature and 240 r / min. Imidazole and anhydrous potassium carbonate were then added, and the mixture was stirred for 6.5 h at 72 °C and 280 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a 10 μm polytetrafluoroethylene filter membrane at a relative pressure of -0.075 MPa. The filter cake was washed twice each with anhydrous N,N-dimethylformamide, anhydrous ethanol, and anhydrous acetonitrile to obtain a wet filter cake of imidazole-based silicon-based support. The wet filter cake of imidazole-based silicon-based support was vacuum dried for 5 h at 45 °C and 3 kPa to obtain the imidazole-based silicon-based support.

[0053] Comparative Example 3 The difference between this comparative example and Example 1 is that the composite functional catalyst is replaced by a silicon-based quaternary phosphonium chloride-imidazolium support by the same mass, while the remaining steps and raw materials are the same as in Example 1. Specifically: A4. The mass ratio of imidazole-modified silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile was controlled at 1:0.24:4.5. The imidazole-modified silicon-based carrier wet filter cake was added to anhydrous acetonitrile, followed by triphenylphosphine. The mixture was stirred and reacted for 12 hours at 78°C and 280 r / min. After the reaction was completed, the mixture was cooled to room temperature and filtered using a 10 μm PTFE membrane at a relative pressure of -0.075 MPa. The filter cake was washed twice each with anhydrous acetonitrile and methyl methacrylate, with each wash using 1.2 times the mass of the filter cake. This yielded a silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake. The silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake was then vacuum dried for 5 hours at 45°C and 3 kPa to obtain the silicon-based quaternary phosphonium chloride-imidazolium carrier.

[0054] Comparative Example 4 The difference between this comparative example and Example 1 is that the side stream sampled in step S3 is not sent to the secondary fixed-bed reactor, that is, the secondary fixed-bed reactor in step S4 is cancelled, and the deep transesterification reaction liquid in the original step S5 is replaced with the liquid to be reacted in the deep transesterification process. The remaining steps and raw materials are the same as in Example 1.

[0055] Comparative Example 5 The difference between this comparative example and Example 1 is that step S3 is omitted, and the original reaction liquid to be further reacted in step S4 is replaced by the same mass of the primary transesterification reaction liquid, which is directly fed into the secondary fixed-bed reactor filled with the composite functional catalyst. The remaining steps and raw materials are the same as in Example 1.

[0056] Comparative Example 6 The difference between this comparative example and Example 1 is that the nitrogen-oxygen mixture is replaced with nitrogen, while the remaining steps and raw materials are the same as in Example 1.

[0057] Performance testing The overall properties of glycidyl methacrylate prepared in Examples 1-3 and Comparative Examples 1-6 of this invention were tested respectively.

[0058] ①Product purity testing The composition of the products was determined by gas chromatography (GC) using a gas chromatograph equipped with a flame ionization detector (FID) and a DB-WAX capillary column (30 m × 0.32 mm × 0.5 μm). High-purity nitrogen was used as the carrier gas at a flow rate of 1.0 mL / min. The injection port temperature was 220 °C, the detector temperature was 250 °C, the injection volume was 0.2 μL, and the split ratio was 50:1. The column temperature was programmed, starting at 60 °C and holding for 2 min, then increasing to 180 °C at a rate of 10 °C / min and holding for 5 min. The mass percentage of each component was calculated using the area normalization method. The purity of glycidyl methacrylate (GMA) was calculated using the formula: Glycidyl methacrylate (GMA) purity (%) = 100% - ∑ percentage of each impurity peak area.

[0059] ② Determination of transesterification conversion, selectivity and yield The contents of glycidol, methyl methacrylate, glycidyl methacrylate, methanol, and byproducts in the reaction solution were determined by gas chromatography. A flame ionization detector was used for detection, and quantification was performed using the area normalization method.

[0060] The glycidyl ether conversion rate is calculated using the formula: X = (n0 - n1) / n0 × 100%; where X is the glycidyl ether conversion rate, %; n0 is the molar amount of glycidyl ether entering the reaction unit; and n1 is the molar amount of unreacted glycidyl ether in the material after the reaction.

[0061] The selectivity of glycidyl methacrylate (GMA) is calculated by the formula: S = n2 / (n0 - n1) × 100%; where S is the selectivity of glycidyl methacrylate, %; and n2 is the molar amount of glycidyl methacrylate produced in the reaction.

[0062] The yield of glycidyl methacrylate (GMA) is calculated using the formula: Y = X × S / 100%.

[0063] The values ​​of n0, n1, and n2 are calculated based on the feed and discharge flow rates and the corresponding component contents per unit time.

[0064] ③ Determination of catalyst stability during continuous operation The composite functional catalyst was loaded into a two-stage fixed-bed reactor and operated continuously under the same temperature, pressure, liquid hourly space velocity, and feed composition conditions as in the corresponding embodiment. After the system reached a steady state, the conversion rate after 12 hours of continuous operation was taken as the initial conversion rate X0; thereafter, samples were taken every 24 hours to detect the composition of the outlet material and the corresponding conversion rate Xt was calculated.

[0065] The catalyst activity retention rate is calculated using the formula: A = Xt / X0 × 100%; where A is the catalyst activity retention rate, %; and Xt is the glycidyl conversion rate after t hours of continuous operation. In this invention, t is taken as 240.

[0066] ④ Determination of chloride ion content The chloride ion content in glycidyl methacrylate was determined by ion chromatography. 5.000 g of the sample was accurately weighed and placed in a 50 mL polypropylene centrifuge tube. 25.00 mL of ultrapure water was added, and the tube was sealed. After extraction by shaking at room temperature for 15 min, the tube was sonicated for 10 min to ensure sufficient transfer of soluble chloride ions to the aqueous phase. The tube was then centrifuged at 4000 rpm for 5 min, and the supernatant was collected and filtered through a 0.22 μm microporous membrane as the test solution. The blank test solution was prepared by adding only 25.00 mL of ultrapure water without glycidyl methacrylate, following the same shaking extraction, sonication, centrifugation, and filtration procedures as the test sample.

[0067] The test was performed using an ion chromatograph equipped with a suppressed conductivity detector. The chromatographic column was an anion exchange column, the eluent was a sodium carbonate-sodium bicarbonate mixture, the flow rate was 1.0 mL / min, the column temperature was 30 °C, and the injection volume was 25 μL. A standard curve was established using chloride ion standard solutions, and the chloride ion concentration in the test solution was calculated using the external standard method.

[0068] Chloride ion content is calculated using the formula: C Cl = (c-c0)×V×f / m; where, C Cl c represents the chloride ion content in the sample, in mg / kg; c represents the chloride ion concentration in the test solution, in mg / L; c0 represents the chloride ion concentration in the blank solution, in mg / L; V represents the volume of the extract, in mL; f represents the dilution factor; and m represents the sample mass, in g. Each sample group was measured in triplicate, and the average value was taken as the test result.

[0069] The specific test results are shown in Table 1.

[0070] Table 1: Performance parameters of glycidyl methacrylate in Examples 1-3 and Comparative Examples 1-6 Note: "-" indicates that a secondary fixed-bed reactor filled with composite functional catalyst was not set up, and the activity retention rate of composite functional catalyst was not evaluated.

[0071] As shown in Table 1, the glycidyl methacrylate prepared in Examples 1-3 of this invention is superior to Comparative Examples 1-6 in terms of glycidyl methacrylate conversion rate, glycidyl methacrylate selectivity, glycidyl methacrylate yield, glycidyl methacrylate purity, chloride ion content, and retention rate of composite functional catalyst activity.

[0072] The data from Example 1 and Comparative Example 1 show that: Comparative Example 1 did not introduce an imidazole group, which resulted in the lack of a weak basic auxiliary action site in the catalyst, leading to insufficient activation of the glycidyl hydroxyl group and weakened synergistic catalytic effect. Consequently, the conversion rate of glycidyl methacrylate, the selectivity of glycidyl methacrylate, the yield of glycidyl methacrylate, and the retention rate of the activity of the composite functional catalyst decreased.

[0073] The data from Example 1 and Comparative Example 2 show that Comparative Example 2 only uses an imidazole-based silicon support, which has insufficient transesterification reaction activity and reduced deep conversion capacity. Consequently, the purity of glycidyl methacrylate, the yield of glycidyl methacrylate, and the retention rate of the composite functional catalyst are all lower than those of Example 1.

[0074] The data from Example 1 and Comparative Example 3 show that Comparative Example 3 did not undergo methacrylate anion exchange, resulting in an increase in chloride ion residue, which in turn led to a decrease in the selectivity, yield, purity, and activity retention rate of glycidyl methacrylate and the composite functional catalyst.

[0075] Data from Example 1 and Comparative Example 4 show that Comparative Example 4 eliminated the secondary fixed-bed reactor, resulting in the inability of the residual reactants to undergo further deep conversion. At the same time, the side reactions increased, and therefore the overall reaction effect and the purity of glycidyl methacrylate were lower than those of Example 1.

[0076] Data from Example 1 and Comparative Example 5 show that Comparative Example 5 did not perform vacuum flash evaporation to remove methanol from the primary reaction solution, and the by-product methanol could not be removed in time. This restricted the shift of the transesterification equilibrium, which in turn led to a decrease in the conversion rate of glycidyl methacrylate, the selectivity of glycidyl methacrylate, the yield of glycidyl methacrylate, and the purity of glycidyl methacrylate.

[0077] The data from Example 1 and Comparative Example 6 show that replacing oxygen-containing nitrogen with pure nitrogen in Comparative Example 6 weakens the synergistic polymerization inhibition effect of p-hydroxyanisole and trace oxygen, increases polymerization side reactions during the reaction and distillation process, and leads to a decrease in the selectivity, yield, purity, and activity retention rate of glycidyl methacrylate and glycidyl methacrylate.

[0078] This specific embodiment is merely an explanation of the present invention and is not intended to limit the invention. After reading this specification, those skilled in the art can make modifications to this embodiment without contributing any inventive step, but such modifications are protected by patent law as long as they are within the scope of the claims of the present invention.

Claims

1. A method for preparing high-purity glycidyl methacrylate using a composite catalysis, characterized in that, The preparation steps include the following: S1. Under the protection of nitrogen and oxygen mixed gas, methyl methacrylate, glycidyl ether and p-hydroxyanisole are mixed and stirred evenly to obtain a mixture. The mixture is then dehydrated and filtered to obtain the transesterification feed liquid. S2. After heating the transesterification feed liquid to 72-76℃, it is passed into a primary circulating fixed-bed reactor filled with the first transesterification catalyst to carry out the primary transesterification reaction and obtain the primary transesterification reaction liquid. S3. The primary transesterification reaction liquid is subjected to vacuum flash vapor-liquid separation to obtain the extracted gas phase and liquid phase. The extracted gas phase is condensed and separated into methanol and methyl methacrylate. The obtained methyl methacrylate is returned to step S1 for use. The liquid phase is sent to a circulating storage tank and divided into a circulating reflux stream and a side-stream sampled stream by a circulating pump. The circulating reflux stream is returned to the feed end of the primary circulating fixed bed reactor and mixed with the transesterification feed liquid for primary transesterification reaction. The side-stream sampled stream is led out via a side stream and used as the liquid to be reacted in the next step. S4. The solution to be deeply reacted is passed into a two-stage fixed-bed reactor filled with a composite functional catalyst to carry out a deep transesterification reaction and obtain a deep transesterification reaction solution. S5. The deep transesterification reaction solution is subjected to vacuum stripping to obtain crude glycidyl methacrylate; the methyl methacrylate obtained after stripping is condensed and returned to step S1 for use. S6. Add p-hydroxyanisole to the crude glycidyl methacrylate and stir until homogeneous to obtain the crude product to be distilled. Perform vacuum distillation on the crude product to be distilled and collect the main fraction to obtain high-purity glycidyl methacrylate.

2. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 1, characterized in that, In step S1, the mass ratio of methyl methacrylate, glycidyl ether, and p-hydroxyanisole is 3.3-3.5:1:0.0010-0.0015.

3. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 1, characterized in that, The conditions of the primary ester exchange reaction in step S2 are: the pressure in the primary circulation fixed bed reactor is 0.1-0.2 MPa, the liquid hourly space velocity is 0.65-0.85 h -1 -1, the circulation reflux ratio is 3.0-3.8:1, and the reaction residence time is 60-70 min.

4. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 1, characterized in that, The vacuum flash vapor-liquid separation in step S3 specifically involves: introducing the primary transesterification reaction liquid into a vacuum flash evaporator at a temperature of 58-64℃ and an absolute pressure of 12-18kPa, and allowing it to remain for 8-12 minutes to remove the methanol generated by the reaction and the entrained methyl methacrylate from the liquid phase; the methanol content in the liquid phase is ≤0.45%.

5. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 1, characterized in that, The preparation method of the composite functional catalyst in step S4 includes the following steps: A1. Porous silica is added to hydrochloric acid solution for acidification treatment. After the treatment is completed, it is cooled, filtered, washed and dried to obtain hydroxylated silicon-based carrier. A2. Under inert gas protection, the hydroxylated silicon-based support was added to anhydrous toluene and stirred until homogeneous. Then, 3-chloropropyltrimethoxysilane was added and stirred to react. After the reaction was completed, the mixture was cooled, filtered, washed, and dried to obtain the chloropropylated silicon-based support. A3. Add the chloropropylated silicon-based support to anhydrous N,N-dimethylformamide, stir until homogeneous, add imidazole and anhydrous potassium carbonate, stir to react, after the reaction is complete, cool, filter and wash to obtain the imidazole-based silicon-based support wet filter cake. A4. Add the imidazole-based silicon-based carrier wet filter cake to anhydrous acetonitrile, add triphenylphosphine, stir to react, after the reaction is completed, cool, filter and wash to obtain silicon-based quaternary phosphonium chloride-imidazole carrier wet filter cake; A5. The silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake was added to a sodium methacrylate solution for anion exchange, followed by filtration, washing, and drying to obtain a composite functional catalyst.

6. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 5, characterized in that, In step A1, the mass ratio of porous silica to hydrochloric acid solution is 1:4.8-5.

2.

7. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 5, characterized in that, In step A2, the mass ratio of the hydroxylated silicon-based support, 3-chloropropyltrimethoxysilane, and anhydrous toluene is 1:0.78-0.88:5.0-5.

5.

8. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 5, characterized in that, In step A3, the mass ratio of chloropropylated silicon-based carrier, imidazole, anhydrous potassium carbonate, and anhydrous N,N-dimethylformamide is 1:0.12-0.18:0.16-0.24:4.8-5.

8.

9. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 5, characterized in that, In step A4, the mass ratio of the imidazole-based silicon-based carrier wet filter cake, triphenylphosphine, and anhydrous acetonitrile is 1:0.24-0.30:4.5-5.

2. In step A5, the mass ratio of the silicon-based quaternary phosphonium chloride-imidazolium carrier wet filter cake to the sodium methacrylate solution is 1:4.2-4.

8.

10. The method for preparing high-purity glycidyl methacrylate using composite catalysis according to claim 1, characterized in that, The conditions for the deep transesterification reaction in step S4 are as follows: pressure in the two-stage fixed-bed reactor is 0.1-0.2 MPa, and liquid hourly space velocity is 0.45-0.55 h⁻¹. -1 The reaction residence time is 100-120 min.