Molecularly imprinted resin, mulberry root extract and preparation method thereof

By preparing molecularly imprinted resin for oxidized resveratrol, the problem of separating and purifying oxidized resveratrol from mulberry root bark was solved, achieving efficient and environmentally friendly separation and purification, and improving product purity and mechanical strength.

CN123107009APending Publication Date: 2026-11-17GUANGZHOU MEIZHIYUAN NEW MATERIALS CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611015819.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-07-08
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies are insufficient for effectively separating and purifying oxidized resveratrol from mulberry root bark, and traditional resin adsorption has poor selectivity, affecting product purity and quality.

Method used

Oxidized resveratrol molecularly imprinted resin was prepared using molecular imprinting technology. Double bonds were grafted onto the surface of a functionalized silica carrier, combined with a multi-hydrogen bond synergistic network and fluorinated functional monomers, to enhance the specific recognition of stilbene aromatic rings. Deep eutectic solvent was used for recycling to improve separation efficiency.

Benefits of technology

It significantly improved the separation and purification efficiency of oxidized resveratrol, reduced non-specific adsorption, improved product purity and mechanical strength, and reduced production costs and environmental pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123107009A_ABST
    Figure CN123107009A_ABST
Patent Text Reader

Abstract

The application discloses an oxidized white resveratrol molecular imprinting resin, mulberry root extract and a preparation method thereof. The high-selectivity imprinting resin is prepared by using silica gel as a carrier and a bifunctional monomer and a deep eutectic solvent green system. The high-purity stilbene mulberry root extract is prepared through enzymolysis, low-temperature extraction of a compound extract solution and resin directional enrichment, has a high tyrosinase inhibition rate, has excellent whitening effect and can be used for cosmetics.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of cosmetics, and in particular to a molecularly imprinted resin, mulberry root extract, and a method for preparing the same. Background Technology

[0002] The dried root bark of the mulberry tree (Morus alba root bark) is rich in stilbene compounds, with resveratrol oxide and morin A as the core active ingredients. These components exert their whitening effects by inhibiting tyrosinase activity and scavenging free radicals, while also possessing anti-inflammatory and soothing properties, making them highly promising for development and application in the field of cosmetic whitening.

[0003] Chinese patent CN101591680B discloses a method for extracting oxidized resveratrol. This method uses mulberry bark (mulberry branch bark or mulberry root bark) as raw material and employs a direct enzymatic extraction process: first, the bark of fresh mulberry branches or roots is peeled, dried, and pulverized; then, it is enzymatically hydrolyzed using an ethanol solution containing glycoside hydrolase. After filtration and concentration, the solution is loaded onto a polyamide chromatography column and eluted using an ethanol gradient. The eluent is then recovered to obtain the target product. However, glycoside hydrolase is easily inactivated in ethanol solution, resulting in limited enzymatic hydrolysis efficiency. Furthermore, the purification method used in this approach is ordinary resin adsorption, which has poor selectivity and makes it difficult to efficiently separate structurally similar stilbene compounds from impurities such as flavonoids and phenolic acids, thus affecting the purity and quality of the product.

[0004] Molecular imprinting technology, as a highly efficient technique for preparing polymers with specific recognition capabilities for specific target molecules, has shown unique advantages in the field of natural product separation and purification. However, there are currently no mature reports on the development of molecular imprinted resins for oxidized resveratrol and their practical application in complex natural products (such as mulberry root bark), and there is still considerable room for research and development. Summary of the Invention

[0005] The first objective of this invention is to provide an oxidized resveratrol molecularly imprinted resin. The second objective of this invention is to use a molecularly imprinted resin to enrich the active ingredients in mulberry root bark, in order to obtain a mulberry root extract with significant whitening effects.

[0006] To achieve the above objectives, the present invention provides the following technical solution: In a first aspect, the present invention provides an oxidized resveratrol molecularly imprinted resin, the preparation method of which includes the following steps: (A) Preparation of functionalized carrier: After activating spherical silica gel with hydrochloric acid, it was reacted with 3-(isobutenoyloxy)propyltrimethoxysilane under reflux in anhydrous toluene to obtain silica gel carrier with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxygenated resveratrol, methacrylic acid and acrylamide are dissolved in deep eutectic solvent porogen, ultrasonically dissolved and allowed to stand, so that the template and bifunctional monomer form hydrogen bond pre-assembled system. (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate, cumyl dithiobenzoate and the initiator azobisisobutyronitrile to the above pre-assembled system; degas in an ice bath using ultrasonication, introduce nitrogen to remove oxygen, and seal. (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica carrier prepared in step (A) and placed in a constant temperature water bath to react, so that the imprinted layer can be polymerized and grown in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol Soxhlet extract until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

[0007] In some embodiments, the spherical silica gel has a particle size of 5-10 μm.

[0008] In some embodiments, the molar ratio of resveratrol oxide, methacrylic acid, and acrylamide is 1:1-2:1-2; the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol at 80°C in a molar ratio of 1:2.

[0009] This invention uses both methacrylic acid and acrylamide as functional monomers. The two form a multi-hydrogen bond synergistic network with multiple phenolic hydroxyl groups of oxidized resveratrol, which has more binding sites and more stable binding than a single monomer, thus reducing non-specific adsorption.

[0010] This invention uses a choline chloride-ethylene glycol deep eutectic solvent, which is biodegradable, non-toxic, and non-volatile, to replace traditional volatile organic solvents such as toluene, acetonitrile, and acetone. This avoids health hazards to operators and environmental pollution, and conforms to the principles of green chemistry.

[0011] In some embodiments, the molar ratio of resveratrol oxide, methacrylic acid, acrylamide, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:1-2:1-2:0.5:8:0.2:0.1.

[0012] The purpose of the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate of the present invention is to enhance the specific recognition of stilbene aromatic rings and exclude flavonoid impurities.

[0013] In this invention, the imprinted layer is located on the surface of the carrier, allowing all recognition sites to quickly contact the template molecules. Compared to traditional bulk imprinted polymers (where sites are largely embedded internally), the adsorption equilibrium time is shortened, significantly improving separation efficiency.

[0014] This invention utilizes a silicone surface grafted with an imprinted layer, resulting in resin with uniform particle size, high mechanical strength, and rapid mass transfer rate. This shortens the adsorption equilibrium time and significantly improves separation and enrichment efficiency. It avoids problems such as irregular particles, excessive fine powder, and low yield caused by mechanical pulverization after bulk polymerization.

[0015] In some embodiments, each gram of silica carrier is added to 50 mL of the polymerization system; the volume ratio of acetic acid to methanol is 1:9.

[0016] In one embodiment, the method further includes step (F); recovery of deep eutectic solvent: the eluent from step (E) is distilled under reduced pressure to recover the acetic acid-methanol mixed solvent, the remaining residue is diluted with deionized water, the aqueous phase of the deep eutectic solvent porogen is recovered by centrifugation, and after being dehydrated by rotary evaporation, it is reused in step (B) to achieve the recycling of deep eutectic solvent porogen.

[0017] This invention integrates a deep eutectic solvent recovery step in the preparation of molecularly imprinted resins: after distillation, dilution, centrifugation, and rotary evaporation, the deep eutectic solvent can be reused for pre-assembly and polymerization, achieving recycling and significantly reducing production costs and waste emissions.

[0018] Secondly, the present invention also provides a mulberry root extract, prepared using the above-mentioned molecularly imprinted resin, the specific preparation method including the following steps: (1) Pretreatment: Take mulberry root bark powder, add 3-5 times its weight of deionized water, adjust the pH to 4.5-5.0, add cellulase and pectinase, and enzymatically hydrolyze at a constant temperature of 40-45℃ for 30-40 min, then raise the temperature to 80-85℃ and keep warm for 10 min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Low temperature extraction: Take the pretreated mulberry root bark powder and add 10-15 times its weight of compound extract solution, which is composed of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water; adjust the pH to 5.5-6.0, place it in a constant temperature ultrasonic extractor, control the temperature at 35-40℃, the ultrasonic power at 250W, extract twice, each time for 40-50min, combine the extracts, centrifuge to take the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate is loaded onto a chromatography column packed with the molecularly imprinted resin at a loading rate of 2-3 BV / h. After loading, the resin is rinsed with deionized water at a rate of 1-2 BV / h. Then, impurities are removed by elution with a 30% ethanol solution at a rate of 2 BV / h. Finally, the resin is eluted with a 70% ethanol solution at a rate of 2-3 BV / h. 1-2 BV of eluent is collected to obtain a stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 45-50℃ and a vacuum of -0.07 to -0.08 MPa until no ethanol odor was detected, and the concentrate was obtained. The concentrate was placed in a vacuum freeze dryer, freeze-dried, and pulverized to obtain a mulberry root extract rich in stilbene.

[0019] In some embodiments, the cellulase has an enzyme activity of 100 u / mg, and the amount of cellulase used is 0.1-0.5% of the weight of mulberry root bark powder; the pectinase has an enzyme activity of 30 u / mg, and the amount of pectinase used is 0.1-0.5% of the weight of mulberry root bark powder.

[0020] In some embodiments, the betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water are mixed in a molar ratio of 1-5:1-5:1-5:0.01-0.05:15-20.

[0021] This invention utilizes 3-phenylpropionic acid, which simultaneously provides carboxyl hydrogen bonding sites and benzene ring π-π stacking sites, forming a bimodal recognition mechanism with the diphenyl ring structure of stilbene-based target molecules. The hydrophobic cavity of the hydroxypropyl-β-cyclodextrin used exhibits a natural affinity for stilbene-based molecules. Betaine provides hydrogen bonding sites. Through the synergistic combination of these three components—betaine providing hydrogen bonding sites, 3-phenylpropionic acid providing π-π recognition, and β-cyclodextrin providing molecular inclusion—multi-level recognition of target molecules is achieved.

[0022] In some embodiments, the freeze-drying parameters are: controlled temperature -40°C to -35°C, vacuum degree ≤0.08MPa, and drying time 12-16h.

[0023] A cosmetic product, wherein the cosmetic product is prepared by adding the above-mentioned mulberry root extract and excipients or auxiliary ingredients in the field of cosmetics.

[0024] The cosmetics mentioned can be in the form of creams, lotions, serums, masks, toners, shampoos, shower gels, etc. Attached Figure Description

[0025] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the accompanying drawings used in the description of the embodiments or the prior art are briefly introduced below.

[0026] Figure 1 The chromatograms of Experiment 1 and Example 3 are shown. Figure 2 The chromatograms of Experiment 1 and Example 4 are shown. Figure 3 The chromatogram of Experiment 1, Example 5 is shown; Figure 4 The chromatogram of Experiment 1, Example 6 is shown. Detailed Implementation

[0027] This invention discloses a molecularly imprinted resin, mulberry root extract, and a method for preparing the same. Those skilled in the art can refer to this document and appropriately modify the process parameters to achieve the desired results. It should be particularly noted that all similar substitutions and modifications are obvious to those skilled in the art and are considered to be included in this invention. The methods and applications of this invention have been described through preferred embodiments. Those skilled in the art can clearly modify or appropriately change and combine the methods and applications described herein without departing from the content, spirit, and scope of this invention to implement and apply the technology of this invention.

[0028] The raw materials and reagents used in the molecularly imprinted resin, mulberry root extract and their preparation method provided by this invention are commercially available.

[0029] The present invention will be further illustrated below with reference to the embodiments: Example 1 An oxidized resveratrol molecularly imprinted resin is obtained by the following preparation method: (A) Preparation of functionalized support: Spherical silica gel (average particle size of 5 μm) was activated with hydrochloric acid and then reacted with 3-(isobutenoyloxy)propyltrimethoxysilane in anhydrous toluene under reflux for 12 h to obtain silica gel support with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxyresveratrol, methacrylic acid and acrylamide are dissolved in a molar ratio of 1:1:2 in a deep eutectic solvent porogen, wherein the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol in a molar ratio of 1:2 at 80°C; ultrasonically dissolve and let stand for 30 min to allow the template and bifunctional monomer to form a hydrogen bond pre-assembled system; (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate (enhancing the specific recognition of stilbene aromatic rings and repelling flavonoid impurities), cumyl dithiobenzoate, and the initiator azobisisobutyronitrile to the above pre-assembled system; wherein the molar ratio of resveratrol oxide, methacrylic acid, acrylamide, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:1:2:0.5:8:0.2:0.1; degas in an ice bath using ultrasonication for 15 min, purge with nitrogen for 10 min to remove oxygen, and seal; (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica support prepared in step (A), with 50 mL of the mixture added per gram of support, and the mixture is placed in a constant temperature water bath at 65°C for 24 hours to allow the imprinted layer to grow in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol (1:9, v / v) by Soxhlet extraction until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

[0030] Example 2 An oxidized resveratrol molecularly imprinted resin is obtained by the following preparation method: (A) Preparation of functionalized support: Spherical silica gel (average particle size of 10 μm) was activated with hydrochloric acid and then reacted with 3-(isobutenoyloxy)propyltrimethoxysilane in anhydrous toluene under reflux for 12 h to obtain silica gel support with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxyresveratrol, methacrylic acid and acrylamide are dissolved in a molar ratio of 1:2:1 in a deep eutectic solvent porogen, wherein the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol in a molar ratio of 1:2 at 80°C; ultrasonic dissolution is performed and the mixture is allowed to stand for 30 min to allow the template and bifunctional monomer to form a hydrogen bond pre-assembled system. (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate (enhancing the specific recognition of stilbene aromatic rings and repelling flavonoid impurities), cumyl dithiobenzoate, and the initiator azobisisobutyronitrile to the above pre-assembled system; wherein the molar ratio of resveratrol oxide, methacrylic acid, acrylamide, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:2:1:0.5:8:0.2:0.1; degas in an ice bath using ultrasonication for 15 min, purge with nitrogen for 10 min to remove oxygen, and seal; (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica support prepared in step (A), with 50 mL of the mixture added per gram of support, and the mixture is placed in a constant temperature water bath at 65°C for 24 hours to allow the imprinted layer to grow in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol (1:9, v / v) by Soxhlet extraction until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

[0031] (F) Recovery of deep eutectic solvent: The eluent from step (E) is distilled under reduced pressure to recover the acetic acid-methanol mixed solvent. The remaining residue is diluted with deionized water, centrifuged to recover the aqueous phase of the deep eutectic solvent porogen, and then removed by rotary evaporation and reused in step (B) to achieve the recycling of the deep eutectic solvent porogen.

[0032] Comparative Example 1 An oxidized resveratrol molecularly imprinted resin is obtained by the following preparation method: (A) Preparation of functionalized support: Spherical silica gel (average particle size of 10 μm) was activated with hydrochloric acid and then reacted with 3-(isobutenoyloxy)propyltrimethoxysilane in anhydrous toluene under reflux for 12 h to obtain silica gel support with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxyresveratrol and methacrylic acid are dissolved in a deep eutectic solvent porogen at a molar ratio of 1:3, wherein the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol at a molar ratio of 1:2 at 80°C; ultrasonically dissolve and let stand for 30 min to allow the template and bifunctional monomer to form a hydrogen bond pre-assembled system; (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate (enhancing the specific recognition of stilbene aromatic rings and repelling flavonoid impurities), cumyl dithiobenzoate, and the initiator azobisisobutyronitrile to the above pre-assembled system; wherein the molar ratio of resveratrol oxide, methacrylic acid, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:3:0.5:8:0.2:0.1; degas in an ice bath using ultrasonication for 15 min, purge with nitrogen for 10 min to remove oxygen, and seal; (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica support prepared in step (A), with 50 mL of the mixture added per gram of support, and the mixture is placed in a constant temperature water bath at 65°C for 24 hours to allow the imprinted layer to grow in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol (1:9, v / v) by Soxhlet extraction until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

[0033] (F) Recovery of deep eutectic solvent: The eluent from step (E) is distilled under reduced pressure to recover the acetic acid-methanol mixed solvent. The remaining residue is diluted with deionized water, centrifuged to recover the aqueous phase of the deep eutectic solvent porogen, and then removed by rotary evaporation and reused in step (B) to achieve the recycling of the deep eutectic solvent porogen.

[0034] Comparative Example 2 An oxidized resveratrol molecularly imprinted resin is obtained by the following preparation method: (A) Preparation of functionalized support: Spherical silica gel (average particle size of 10 μm) was activated with hydrochloric acid and then reacted with 3-(isobutenoyloxy)propyltrimethoxysilane in anhydrous toluene under reflux for 12 h to obtain silica gel support with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxyresveratrol and acrylamide are dissolved in a deep eutectic solvent porogen at a molar ratio of 1:3, wherein the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol at a molar ratio of 1:2 at 80°C; ultrasonic dissolution is performed, and the mixture is allowed to stand for 30 min to allow the template and bifunctional monomer to form a hydrogen bond pre-assembled system. (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate (enhancing the specific recognition of stilbene aromatic rings and repelling flavonoid impurities), cumyl dithiobenzoate, and the initiator azobisisobutyronitrile to the above pre-assembled system; wherein the molar ratio of resveratrol oxide, acrylamide, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:3:0.5:8:0.2:0.1; degas in an ice bath using ultrasonication for 15 min, purge with nitrogen for 10 min to remove oxygen, and seal; (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica support prepared in step (A), with 50 mL of the mixture added per gram of support, and the mixture is placed in a constant temperature water bath at 65°C for 24 hours to allow the imprinted layer to grow in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol (1:9, v / v) by Soxhlet extraction until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

[0035] (F) Recovery of deep eutectic solvent: The eluent from step (E) is distilled under reduced pressure to recover the acetic acid-methanol mixed solvent. The remaining residue is diluted with deionized water, centrifuged to recover the aqueous phase of the deep eutectic solvent porogen, and then removed by rotary evaporation and reused in step (B) to achieve the recycling of the deep eutectic solvent porogen.

[0036] Example 3 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 3 times its weight of deionized water, adjust the pH to 5.0 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.1% of the weight of mulberry root bark powder and the amount of pectinase is 0.5% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 40℃ for 40min, then raise the temperature to 80℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 15 times its weight of the compound extract solution, which is composed of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 1:5:1:0.05:15; adjust the pH to 6.0, place it in a constant temperature ultrasonic extractor, control the temperature at 35℃, the ultrasonic power at 250W, extract twice, 50min each time, combine the extracts, centrifuge to collect the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 1 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 2 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 2 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-enriched solution was concentrated at 45°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -40°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 16 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0037] Example 4 A method for preparing mulberry root extract, using the molecularly imprinted resin obtained in Example 2, is otherwise the same as in Example 3.

[0038] Example 5 A method for preparing mulberry root extract, using the molecularly imprinted resin prepared in Comparative Example 1, is the same as in Example 3.

[0039] Example 6 A method for preparing mulberry root extract, using the molecularly imprinted resin obtained in Comparative Example 2, is the same as in Example 3.

[0040] Experiment 1 The oxidized resveratrol in the mulberry root extracts prepared in Examples 3-6 was determined by chromatographic method as described in the literature "Wei Min, Tuo Yangling, Du Xiaoyue, et al. Determination of the content of 7 components in mulberry bark from different origins and chemometric evaluation [J]. Chinese Medicinal Herbs, 2020, 43(01):125-129."

[0041] The mulberry root extracts obtained in Examples 3-6 were diluted 10 times with the mobile phase, and the content of oxidized resveratrol in each sample was determined by HPLC according to the literature method.

[0042] The specific test results are shown in Table 1 below, and the detailed chromatograms are attached. Figures 1-4 .

[0043] Table 1. Oxidized resveratrol content in each test group As shown in Table 1, the content of oxidized resveratrol in the mulberry root extracts prepared in Examples 3-4 of this invention is significantly higher than that in Examples 5-6. This indicates that the methacrylic acid and acrylamide used simultaneously in the molecularly imprinted resins employed in Examples 3-4, as functional monomers, form a multi-hydrogen bond synergistic network with multiple phenolic hydroxyl groups of oxidized resveratrol. This network has more binding sites and is more stable than that of a single monomer, thus reducing non-specific adsorption.

[0044] Example 7 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 5 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.5% of the weight of mulberry root bark powder and the amount of pectinase is 0.1% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 45℃ for 30min, then raise the temperature to 85℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 10 times its weight of the compound extract solution, which is composed of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 5:1:5:0.01:20; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 40℃, the ultrasonic power at 250W, extract twice, 40min each time, combine the extracts, centrifuge to collect the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 3 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 3 BV / h, and 1 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 50°C and a vacuum of -0.07 MPa until no ethanol odor was detected, and the concentrate was obtained. The concentrate was placed in a vacuum freeze dryer, and the temperature was controlled at -35°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 12 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0045] Example 8 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 12 times its weight of the compound extract solution, which is a mixture of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 3:2:3:0.03:15; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃ and the ultrasonic power at 250W, extract twice, 45min each time, combine the extracts, centrifuge to collect the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 1.5 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 48°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0046] Comparative Example 3 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 12 times its weight of the compound extract solution, which is composed of betaine, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 3:3:0.03:15; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃ and the ultrasonic power at 250W, extract twice, 45min each time, combine the extracts, centrifuge to collect the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 1.5 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 48°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0047] Comparative Example 4 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 12 times its weight of the compound extract solution, which is composed of betaine, 3-phenylpropionic acid, glycerol and deionized water in a molar ratio of 3:2:3:15; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃ and the ultrasonic power at 250W, extract twice, 45min each time, combine the extracts, centrifuge to take the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 1.5 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 48°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0048] Comparative Example 5 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 12 times its weight of the compound extract solution, which is a mixture of 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 2:3:0.03:15; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃ and the ultrasonic power at 250W, extract twice, 45min each time, combine the extracts, centrifuge to collect the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 1.5 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 48°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0049] Comparative Example 6 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder and add 12 times its weight of the compound extract solution, which is composed of betaine, glycerol and deionized water in a molar ratio of 3:3:15; adjust the pH to 5.5, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃ and the ultrasonic power at 250W, extract twice, 45min each time, combine the extracts, centrifuge to take the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate was loaded onto a chromatography column packed with the molecularly imprinted resin prepared in Example 2 at a loading rate of 2 BV / h. After loading, the resin was rinsed with deionized water at a rate of 1 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it was eluted with 70% ethanol solution at a rate of 2 BV / h, and 1.5 BV of eluent was collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 48°C and a vacuum of -0.08 MPa until no ethanol odor was detected, and a concentrated solution was obtained. The concentrated solution was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08 MPa. The solution was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene.

[0050] Comparative Example 7 A method for preparing mulberry root extract includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 4 times its weight of deionized water, adjust the pH to 4.5 with citric acid, add cellulase with an enzyme activity of 100u / mg and pectinase with an enzyme activity of 30u / mg, wherein the amount of cellulase is 0.3% of the weight of mulberry root bark powder, and the amount of pectinase is 0.3% of the weight of mulberry root bark powder; enzymatically hydrolyze at a constant temperature of 42℃ for 35min, then raise the temperature to 82℃ and keep warm for 10min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Extraction: Take the pretreated mulberry root bark powder, add 12 times its mass of 70% ethanol solution, place it in a constant temperature ultrasonic extractor, control the temperature at 36℃, ultrasonic power at 250W, extract twice, each time for 45min, combine the extracts, centrifuge to take the supernatant, filter through a membrane to obtain the permeate; (3) Concentration: The permeate was concentrated at 48°C and a vacuum of -0.08MPa until no ethanol odor was detected, and the concentrate was obtained. The concentrate was placed in a vacuum freeze dryer, and the temperature was controlled at -36°C and the vacuum degree was ≤0.08MPa. It was dried for 14 hours and then pulverized to obtain a mulberry root extract rich in stilbene compounds.

[0051] Experiment 2 Melanin synthesis is influenced by tyrosinase, which catalyzes the hydroxylation of L-tyrosine to dopa and then oxidizes dopa to dopaquinone, which forms the final product, melanin. Test substances that inhibit tyrosinase activity can slow down the tyrosinase-catalyzed conversion of L-tyrosine to dopaquinone. The inhibitory effect of the test substance on tyrosinase activity is evaluated by measuring the absorbance of dopaquinone at 475 nm and analyzing the changes in absorbance.

[0052] The mulberry root extracts obtained in Examples 7-8 and Comparative Examples 3-7 were first dissolved and diluted 10 times with dimethyl sulfoxide, and the tyrosinase inhibition rate was determined according to the method described in the group standard "T / GDCA 006—2021 Test Method for Inhibition of Tyrosinase Activity by Cosmetic Raw Materials (In Vitro Method)". The specific test results are shown in Table 2.

[0053] Table 2 Tyrosinase inhibition rate of each test group

[0054] As shown in Table 2, the tyrosinase inhibition rate of the mulberry root extract prepared in Examples 7-8 of this invention was significantly higher than that of any missing group (Comparative Examples 3-6); moreover, it was higher than the expected value of the sum of the inhibition rates of any two or three groups in Comparative Examples 3-6. This confirms that through the synergistic combination of the ternary components, betaine provides hydrogen bond binding sites, 3-phenylpropionic acid provides π-π recognition, and β-cyclodextrin provides molecular inclusion, achieving multi-level recognition of the target molecule.

[0055] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A molecularly imprinted resin for oxidized resveratrol, characterized in that, The preparation method includes the following steps: (A) Preparation of functionalized carrier: After activating spherical silica gel with hydrochloric acid, it was reacted with 3-(isobutenoyloxy)propyltrimethoxysilane under reflux in anhydrous toluene to obtain silica gel carrier with surface grafted double bonds. (B) Preparation of pre-assembled system: Oxygenated resveratrol, methacrylic acid and acrylamide are dissolved in deep eutectic solvent porogen, ultrasonically dissolved and allowed to stand, so that the template and bifunctional monomer form hydrogen bond pre-assembled system. (C) Preparation of the polymerization system: Add the crosslinking agent ethylene glycol dimethacrylate, the fluorinated functional monomer 2,2,2-trifluoroethyl methacrylate, cumyl dithiobenzoate and the initiator azobisisobutyronitrile to the above pre-assembled system; degas in an ice bath using ultrasonication, introduce nitrogen to remove oxygen, and seal. (D) Surface imprinting polymerization: The polymerization system obtained in step (C) is added to the silica carrier prepared in step (A) and placed in a constant temperature water bath to react, so that the imprinted layer can be polymerized and grown in a controlled manner on the silica surface. (E) Product separation and elution: After the reaction, the solid was collected by centrifugation and extracted with acetic acid-methanol Soxhlet extract until there was no UV absorption peak of oxidized resveratrol in the eluent. Then it was washed with pure methanol and dried under vacuum to constant weight to obtain oxidized resveratrol surface molecular imprinted resin.

2. The oxidized resveratrol molecularly imprinted resin according to claim 1, characterized in that, The spherical silica gel has a particle size of 5-10 μm.

3. The oxidized resveratrol molecularly imprinted resin according to claim 1, characterized in that, The molar ratio of resveratrol oxide, methacrylic acid, and acrylamide is 1:1-2:1-2; the deep eutectic solvent porogen is prepared by stirring choline chloride and ethylene glycol at 80°C in a molar ratio of 1:

2.

4. The oxidized resveratrol molecularly imprinted resin according to claim 1, characterized in that, The molar ratio of resveratrol oxide, methacrylic acid, acrylamide, 2,2,2-trifluoroethyl methacrylate, ethylene glycol dimethacrylate, cumyl dithiobenzoate, and azobisisobutyronitrile is 1:1-2:1-2:0.5:8:0.2:0.

1.

5. The oxidized resveratrol molecularly imprinted resin according to claim 1, characterized in that, Each gram of silica carrier is added to 50 mL of the polymerization system; the volume ratio of acetic acid to methanol is 1:

9.

6. The oxidized resveratrol molecularly imprinted resin according to claim 1, characterized in that, It also includes step (F); recovery of deep eutectic solvent: the eluent from step (E) is distilled under reduced pressure to recover the acetic acid-methanol mixed solvent, the remaining residue is diluted with deionized water, the deep eutectic solvent porogen aqueous phase is recovered by centrifugation, and after being dehydrated by rotary evaporation, it is reused in step (B) to realize the recycling of deep eutectic solvent porogen.

7. A mulberry root extract, characterized in that, The specific preparation method includes the following steps: (1) Pretreatment: Take mulberry root bark powder, add 3-5 times its weight of deionized water, adjust the pH to 4.5-5.0, add cellulase and pectinase, and enzymatically hydrolyze at a constant temperature of 40-45℃ for 30-40 min, then raise the temperature to 80-85℃ and keep warm for 10 min to inactivate the enzyme, centrifuge to collect the precipitate, wash and dry to obtain pretreated mulberry root bark powder; (2) Low temperature extraction: Take the pretreated mulberry root bark powder and add 10-15 times its weight of compound extract solution, which is composed of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water; adjust the pH to 5.5-6.0, place it in a constant temperature ultrasonic extractor, control the temperature at 35-40℃, the ultrasonic power at 250W, extract twice, each time for 40-50min, combine the extracts, centrifuge to take the supernatant, filter through a membrane to obtain the permeate; (3) Directional enrichment: The permeate is loaded onto a chromatography column packed with the molecularly imprinted resin according to any one of claims 1-6 at a loading rate of 2-3 BV / h. After loading, the resin is rinsed with deionized water at a rate of 1-2 BV / h, and then eluted with 30% ethanol solution at a rate of 2 BV / h to remove impurities. Finally, it is eluted with 70% ethanol solution at a rate of 2-3 BV / h, and 1-2 BV of eluent is collected to obtain stilbene-based enrichment solution. (4) Concentration: The stilbene-rich solution was concentrated at 45-50℃ and a vacuum of -0.07 to -0.08 MPa until no ethanol odor was detected, and the concentrate was obtained. The concentrate was placed in a vacuum freeze dryer, freeze-dried, and pulverized to obtain a mulberry root extract rich in stilbene.

8. The mulberry root extract according to claim 7, characterized in that, The cellulase has an enzyme activity of 100 u / mg, and the amount of cellulase used is 0.1-0.5% of the weight of mulberry root bark powder; the pectinase has an enzyme activity of 30 u / mg, and the amount of pectinase used is 0.1-0.5% of the weight of mulberry root bark powder; the mixture is composed of betaine, 3-phenylpropionic acid, glycerol, hydroxypropyl-β-cyclodextrin and deionized water in a molar ratio of 1-5:1-5:1-5:0.01-0.05:15-20.

9. The mulberry root extract according to claim 7, characterized in that, The freeze-drying parameters are: temperature controlled at -40℃ to -35℃, vacuum degree ≤0.08MPa, and drying time 12-16h.

10. The use of the mulberry root extract according to any one of claims 7-9 in the preparation of cosmetics.

Citation Information

Patent Citations

  • Method for extracting oxidized resveratrol

    CN101591680B