A water-based cleaning agent and its preparation method

By chemically modifying rhamnosyl ester with organosilicon polyether, the problems of high environmental impact, poor safety and insufficient stability of water-based cleaning agents are solved, achieving a highly efficient and environmentally friendly cleaning effect, suitable for metal and glass substrates.

CN123107784APending Publication Date: 2026-11-17FUJIAN HUAXIALAN NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611300540.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-26
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

While existing water-based cleaning agents can ensure cleaning effectiveness, they suffer from high environmental impact, poor safety in use, insufficient storage stability, and poor compatibility, making it difficult to meet the cleaning needs under complex working conditions.

Method used

Using organosilicon polyether-modified rhamnosyl ester as the core component, organosilicon polyether is incorporated into the rhamnosyl ester molecule through a series of chemical reactions, which improves its encapsulation and emulsification of oil stains, reduces surface tension, enhances cleaning effect, and improves the stability of the system by selecting appropriate alkaline substances and defoamers.

Benefits of technology

It achieves low surface tension, good cleaning effect, low corrosion and high stability, and is suitable for cleaning metal and glass substrates, reducing the risk of environmental pollution and improving safety and storage stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123107784A_ABST
    Figure CN123107784A_ABST
Patent Text Reader

Abstract

This invention discloses a water-based cleaning agent and its preparation method, relating to the field of cleaning agent technology. It comprises the following raw materials in parts by weight: 5-25 parts of organosilicon polyether-modified rhamnosyl ester, 1-5 parts of alkali, 0.5-1 part of corrosion inhibitor, 0.5-1 part of defoamer, and 68-93 parts of water. The water-based cleaning agent of this invention uses rhamnosyl ester as a modified matrix, incorporating organosilicon polyether into the rhamnosyl ester molecules. This enhances the encapsulation and emulsification effect of rhamnosyl ester on oil stains, reduces surface tension, and provides excellent cleaning effect on heavy oil stains on optical glass and metal substrate surfaces with low corrosiveness. The organosilicon polyether-modified rhamnosyl ester is biodegradable, environmentally friendly, and causes minimal environmental pollution. Preferably, the organosilicon polyether-modified rhamnosyl ester does not contain ester groups in the system, exhibits strong alkali resistance, and is beneficial for removing oil stains under alkaline conditions.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of cleaning agent technology, specifically to a water-based cleaning agent and its preparation method. Background Technology

[0002] With the rapid development of industrial manufacturing and daily consumption, cleaning agents, as important chemicals for removing oil, dust, and inorganic scale from object surfaces, have been widely used in industrial processing, public facilities, household products, and medical and health fields. Traditional cleaning agent systems typically contain components such as surfactants, builders, solvents, and pH adjusters, among which surfactants are the core component that determines detergency.

[0003] While traditional solvent-based cleaning agents offer excellent cleaning performance and dissolve various types of oil stains, they are gradually being replaced by more environmentally friendly water-based cleaning agents due to pollution and exposure risks associated with their high emissions of volatile organic compounds (VOCs).

[0004] Currently, most mainstream water-based cleaning agents on the market use petroleum-based synthetic surfactants, such as alkylbenzene sulfonates, fatty alcohol polyoxyethylene ether sulfates, and nonylphenol polyoxyethylene ethers. While these products possess good emulsifying, wetting, and solubilizing abilities, they generally suffer from long degradation cycles in the natural environment, and some metabolites (such as nonylphenol) have endocrine-disrupting effects, posing ecotoxicity risks or strong irritation to operators. Furthermore, for heavy oil stains or specific industrial scenarios, existing water-based cleaning agents, due to their structural differences, often require the introduction of volatile organic solvents to enhance detergency. This not only increases the complexity of the process but also raises concerns about VOC emissions, flammability, explosiveness, and occupational health hazards.

[0005] To meet increasingly stringent environmental regulations, the field is gradually shifting towards developing environmentally friendly cleaning agents, such as using biosurfactants (e.g., glycolipids, lipopeptides) to replace some petroleum-based components. However, existing bio-based cleaning agents still face challenges in practical applications: unmodified biosurfactants often have drawbacks such as high critical micelle concentrations, insufficient temperature and salt resistance, and limited emulsification ability for heavy oil stains, making it difficult to meet cleaning needs under complex working conditions. Furthermore, to balance detergency and environmental safety, existing technologies often employ complex compounding systems, which can lead to poor compatibility between components, easy stratification during long-term storage, or gelation.

[0006] Therefore, how to significantly reduce the environmental impact, improve the safety of use, and enhance the storage stability of cleaning agents while ensuring their excellent detergency remains a pressing technical problem to be solved in this field. Summary of the Invention

[0007] Therefore, the present invention provides a water-based cleaning agent and a method for preparing the same.

[0008] A water-based cleaning agent comprises the following raw materials in parts by weight: 5-25 parts of organosilicon polyether modified rhamnosine ester, 1-5 parts of alkali, 0.5-1 part of corrosion inhibitor, 0.5-1 part of defoamer, and 68-93 parts of water.

[0009] The preparation method of the organosilicon polyether modified rhamnosine ester includes the following steps: (1) Dissolve rhamnosyl ester in deionized water, add epichlorohydrin and acid-binding agent, heat and react, and distill off excess epichlorohydrin under reduced pressure to obtain crude epioxidized rhamnosyl ester solution. (2) Add alkyl secondary amine, allyl polyether and allyl glycerol alkyl modified polyether to the crude epoxy modified rhamnosine ester solution obtained in step (1), heat the reaction, then cool down, adjust pH=4~6, add solvent for extraction, discard the aqueous phase, and obtain allyl polyether modified rhamnosine ester solution. (3) Add hydrogen-containing silane to the allyl polyether modified rhamnosine ester solution obtained in step (2), heat and add catalyst to react, remove solvent by vacuum distillation to obtain the organosilicon polyether modified rhamnosine ester. In steps (1)-(3), the molar ratio of rhamnosyl ester, deionized water, epichlorohydrin, acid-binding agent, alkyl secondary amine, allyl polyether, allyl glycerol alkyl modified polyether and hydrogen-containing silane is 1:50:(1.5-2.6):(3-4):(0.05-0.3):(0.62-1.5):(0.02-0.1):(0.95-1.65). Based on the effective components, the molar ratio of the catalyst added to the hydrogen-containing silane is 1:(1000-10000).

[0010] Furthermore, the rhamnose ester is one or more of the following: dirhamnose diester RL1, monorhamnose diester RL2, dirhamnose monoester RL3, or monorhamnose monoester RL4. The acid-binding agent is sodium hydroxide or potassium hydroxide; The alkyl secondary amine is any one of the alkyl secondary amines having 7-16 carbon atoms; The allyl polyether is one or more of allyl polyoxyethylene ether, allyl polyoxypropylene ether, or allyl polyoxyethylene polyoxypropylene ether, and the average molecular weight is ≤500 Da. The allylglycerol alkyl-modified polyether is a reactive nonionic emulsifier; preferably, the allylglycerol alkyl-modified polyether is Adeka's reactive nonionic emulsifier REASOAP. ® ER-10; The pH adjuster is dilute hydrochloric acid or dilute sulfuric acid; The solvent is dimethyl carbonate; The hydrogen-containing silane is 1,1,1,3,3-pentamethyldisiloxane or 1,1,1,3,5,5,5-heptamethyltrisiloxane; The catalyst is either a Speier catalyst or a Karstedt catalyst. Furthermore, the alkali is any one of sodium hydroxide, sodium bicarbonate, or ammonia water; The corrosion inhibitor is sodium metasilicate; The defoamer is a polyether-modified silicone emulsion defoamer, preferably Coadd from Puwei (Shanghai) New Material Technology Co., Ltd. TM DF2510, Coadd TM DF6050 or Coadd TM DF6904.

[0011] Furthermore, in step (1), the temperature is raised to 40-60℃ and the reaction is carried out for 4-12 hours.

[0012] Furthermore, in step (2), the temperature is raised to 50-80℃ and reacted for 2-6 hours, then cooled to 20-30℃.

[0013] Furthermore, in step (3), the temperature is raised to 60-80℃ and the catalyst is added. After reacting for 2-6 hours, the temperature is lowered to 20-30℃.

[0014] This invention also provides a method for preparing a water-based cleaning agent, comprising the following steps: (A) Weigh each raw material according to the specifications of the water-based cleaning agent; (B) Dissolve organosilicon polyether modified rhamnosyl ester, alkali and corrosion inhibitor in deionized water, add defoamer, and stir evenly to obtain water-based cleaning agent.

[0015] Compared with the prior art, the present invention has the following beneficial technical effects: This invention relates to a water-based cleaning agent using rhamnosyl ester as a modified matrix. Organosilicon polyether is incorporated into the rhamnosyl ester molecules, enhancing its encapsulation and emulsification of oil stains, reducing surface tension, and providing excellent cleaning effects on heavy oil stains on optical glass and metal substrates with low corrosiveness. The organosilicon polyether-modified rhamnosyl ester is biodegradable, environmentally friendly, and causes minimal pollution. When rhamnosyl monoester is preferred, the system does not contain ester groups, exhibiting strong alkali resistance, which is beneficial for removing oil stains under alkaline conditions.

[0016] The reaction mechanism for preparing organosilicon polyether-modified rhamnosyl ester is as follows: First, the hydroxyl groups in the rhamnosyl ester react with epichlorohydrin under the action of an acid-binding agent, incorporating epoxy groups to obtain epoxy-modified rhamnosyl ester. Second, the epoxy groups in the epoxy-modified rhamnosyl ester react with the amino groups in the long-chain alkyl secondary amine and the hydroxyl groups in the allyl polyether, incorporating the long-chain alkyl and allyl groups into the rhamnosyl ester to obtain allyl polyether-modified rhamnosyl ester. The allyl groups in the allyl polyether-modified rhamnosyl ester have high reactivity and undergo hydrosilylation with the silane bonds in the hydrosilane, incorporating the silicon head into the rhamnosyl ester to obtain organosilicon polyether-modified rhamnosyl ester. The incorporation of organosilicon polyether in the reaction overcomes the shortcomings of rhamnosyl ester, which has good water solubility but is not sufficiently oleophilic, thus improving the encapsulation and emulsification effect of rhamnosyl ester on oil stains. Furthermore, the presence of organosilicon reduces surface tension, enhancing the penetration of oil stains and substrates, and improving the cleaning effect. Attached Figure Description

[0017] Figure 1 The infrared spectra of FRL T3, A1, B1 and C1 in Example 1 are shown. Detailed Implementation

[0018] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0019] Basic information and source of raw materials: WHAR TM -FRL15: Rhamnose ester, a product of Wanhua Chemical Group Co., Ltd., with an active ingredient content of 15wt%, including approximately 31.2wt% of dirhamnose diester RL1, approximately 19.6wt% of monorhamnose diester RL2, approximately 7.5% of dirhamnose monoester RL3, and approximately 1.7wt% of monorhamnose monoester RL4, with the remainder being water. The average molecular weight is approximately 557 g / mol. The calculation only includes the active ingredient. When using physical mixing, some water is removed by pre-vacuum distillation to increase the active ingredient content to 30wt%, resulting in a concentrated rhamnose ester solution.

[0020] WHAR TM -FRL T3: Dirhamnose monoester, a special sample prepared by Wanhua Chemical Group Co., Ltd., with an active ingredient content of 30wt%, dirhamnose monoester accounting for approximately 27.6wt%, monorhamnose monoester RL4 accounting for approximately 2.4wt%, and the remainder being water, with an average molecular weight of approximately 464g / mol; calculations only include the active ingredient.

[0021] HMS-238B: Allyl polyoxyethylene ether, Zhejiang Huangma Technology Co., Ltd., average molecular weight 204 g / mol.

[0022] A350: Allyl polyoxyethylene polyoxypropylene ether, Jiangsu Zhongshan New Materials Co., Ltd., average molecular weight 350 g / mol.

[0023] HMS-229B: Allyl polyoxyethylene polyoxypropylene ether, Zhejiang Huangma Technology Co., Ltd., average molecular weight 403 g / mol.

[0024] HMS-239B: Allyl alcohol polyoxyethylene ether, Zhejiang Huangma Technology Co., Ltd., average molecular weight 375 g / mol.

[0025] APPG300-4PO: Allyl polyoxypropylene ether, Hangzhou Danwei Technology Co., Ltd., average molecular weight 311 g / mol.

[0026] Coadd TM DF2510: Organosilicon polyether defoamer, Puwei (Shanghai) New Material Technology Co., Ltd.

[0027] Coadd TM DF6050: Organosilicon polyether defoamer, Puwei (Shanghai) New Material Technology Co., Ltd.

[0028] Coadd TM DF6904: Organosilicon polyether defoamer, Puwei (Shanghai) New Material Technology Co., Ltd.

[0029] Allylglycerol alkyl modified polyether is REASOAP, a reactive nonionic emulsifier from Adeka. ® ER-10; Example 1 The preparation method of water-based cleaning agents includes the following steps: (1) In a reaction vessel, 1 mol of dirhamnose monoester WHAR was added. TM -FRL T3 was dissolved in 50 mol of deionized water, and 2.6 mol of epichlorohydrin and 4 mol of NaOH were added. The mixture was heated to 60 °C and reacted for 4 hours. After the reaction was completed, excess epichlorohydrin was distilled off under reduced pressure to obtain a crude epoxy-modified rhamnosyl ester aqueous solution A1 containing NaOH and inorganic salts. Titration with sodium thiosulfate showed that an average of 1.63 hydroxyl groups were substituted with epoxy groups in one molecule of rhamnosyl ester. A small amount of A1 was taken to remove water and inorganic salts, and infrared spectroscopy was performed.

[0030] (2) Add 0.05 mol di-n-octylamine, 1.5 mol allyl polyoxyethylene ether HMS-238B and 0.1 mol AdekaREASOAP ®ER-10 was added to crude epoxy-modified rhamnosyl ester aqueous solution A1, heated to 50℃, reacted for 6 hours, cooled to 20℃, and the pH was adjusted to 4 with dilute hydrochloric acid. Dimethyl carbonate was added for extraction, and the aqueous phase was discarded to obtain allyl polyether-modified rhamnosyl ester solution B1. The average number of double bonds in one molecule of rhamnosyl ester was determined by iodometric titration. A small amount of B1 was taken to evaporate the solvent and subjected to infrared spectroscopy.

[0031] (3) Mix allyl polyether modified rhamnosyl ester solution B1 with 1.65 mol 1,1,1,3,5,5,5-heptamethyltrisiloxane, heat to 80°C, add 0.165 mmol Speier catalyst, react for 2 hours, cool to 25°C, remove dimethyl carbonate by vacuum distillation to obtain organosilicon polyether modified rhamnosyl ester C1; take a small amount of C1 and perform infrared spectroscopy test.

[0032] (4) Dissolve 25g of organosilicon polyether modified rhamnosyl ester C1, 5g of sodium hydroxide, and 0.5g of corrosion inhibitor sodium metasilicate in 68g of deionized water, and add 0.5g of defoamer Coadd. TM DF2510, stir well to obtain water-based cleaning agent D1.

[0033] The infrared spectra of the products obtained in each step are shown below. Figure 1 . Figure 1 In the middle, FRL T3 at 3400cm -1 A distinct hydroxyl peak appears on both sides, at 1710 cm⁻¹. -1 The left and right sides are the characteristic absorption peaks of the carboxyl group, at 1735 cm⁻¹. -1 The absence of obvious characteristic peaks for ester groups on the left and right indicates that FRLT3 is a rhamnose monoester.

[0034] In A1, 1267cm -1 and 830cm -1 The absorption peak is a characteristic absorption peak of the epoxy group, at 1606 cm⁻¹. -1 The absorption peak is a characteristic absorption peak of carboxylate, indicating that epoxy-modified rhamnose ester was obtained, and the titration results also confirm the success of epoxy modification.

[0035] In B1, 1641cm -1 The characteristic absorption peak for unsaturated carbon-carbon double bonds is 1108 cm⁻¹. -1 The characteristic absorption peak of the COC bond in allyl polyether is 1712 cm⁻¹. -1 The characteristic absorption peak of the carboxyl group is observed, while the characteristic absorption peak of the epoxy group disappears, indicating that the reaction produces the allyl polyether-modified rhamnose ester, which is consistent with the result of iodometric titration.

[0036] In C1, 1641cm -1 The absorption peak disappears at 1002 cm⁻¹. -1The presence of a characteristic absorption peak of siloxane indicates that step 3 involves the addition of a hydrogen-containing silane to an allyl group via a hydrosilylation reaction, yielding organosilicon polyether-modified rhamnosyl ester.

[0037] Example 2 The preparation method of water-based cleaning agents includes the following steps: (1) In the reaction vessel, 1 mol of rhamnosyl ester WHAR TM -FRL15 was dissolved in 50 mol of deionized water, and 1.5 mol of epichlorohydrin and 3 mol of KOH were added to the reaction vessel. The mixture was heated to 40 °C and reacted for 12 hours. After the reaction was completed, excess epichlorohydrin was distilled off under reduced pressure to obtain crude epioxidized rhamnosyl ester aqueous solution A2. According to the titration results of sodium thiosulfate, an average of 0.92 hydroxyl groups in 1 molecule of rhamnosyl ester were replaced by epoxy groups.

[0038] (2) Add 0.30 mol di-n-butylamine, 0.62 mol allyl polyoxyethylene polyoxypropylene ether A350 and 0.02 mol Adeka REASOAP ® ER-10 was added to crude epoxy-modified rhamnosyl ester aqueous solution A2, heated to 80℃, reacted for 2 hours, cooled to 30℃, pH was adjusted to 6 with dilute sulfuric acid, and dimethyl carbonate was added for extraction. The aqueous phase was discarded to obtain allyl polyether-modified rhamnosyl ester solution B2. The average number of double bonds in one molecule of rhamnosyl ester was determined by iodometric titration.

[0039] (3) Mix allyl polyether modified rhamnosyl ester solution B2 with 0.95 mol 1,1,1,3,3-pentamethyldisiloxane, heat to 60°C, add 0.05 mmol Karstedt catalyst, react for 6 hours, cool to 30°C, remove dimethyl carbonate by vacuum distillation, and obtain organosilicon polyether modified rhamnosyl ester C2.

[0040] (4) Dissolve 5g of organosilicon polyether modified rhamnosyl ester C2, 1g of ammonia water, and 0.5g of corrosion inhibitor sodium metasilicate in 93g of deionized water, and add 0.5g of defoamer Coadd. TM DF6050, stir well to obtain water-based cleaning agent D2.

[0041] Example 3 The preparation method of water-based cleaning agents includes the following steps: (1) In the reaction vessel, 1 mol of rhamnosyl ester WHAR TM-FRL15 was dissolved in 50 mol of deionized water, and 2 mol of epichlorohydrin and 3.6 mol of NaOH were added to the reaction vessel. The mixture was heated to 55 °C and reacted for 6 hours. After the reaction was completed, excess epichlorohydrin was distilled off under reduced pressure to obtain crude epioxidized rhamnosyl ester aqueous solution A3. According to the titration results of sodium thiosulfate, an average of 1.27 hydroxyl groups in 1 molecule of rhamnosyl ester were replaced by epoxy groups.

[0042] (2) Add 0.15 mol N-methylhexylamine, 1.1 mol allyl polyoxyethylene polyoxypropylene ether HMS-229B and 0.05 mol Adeka REASOAP ® ER-10 was added to crude epoxy-modified rhamnosyl ester aqueous solution A3, heated to 65℃, reacted for 4 hours, cooled to 25℃, pH was adjusted to 5 with dilute sulfuric acid, and extracted with dimethyl carbonate. The aqueous phase was discarded to obtain allyl polyether-modified rhamnosyl ester solution B3. The average number of double bonds in one molecule of rhamnosyl ester was determined by iodometric titration.

[0043] (3) Mix allyl polyether modified rhamnosyl ester solution B3 with 1.3 mol 1,1,1,3,5,5,5-heptamethyltrisiloxane, heat to 70°C, add 0.13 mmol Speier catalyst, react for 4 hours, cool to 25°C, remove dimethyl carbonate by vacuum distillation, and obtain organosilicon polyether modified rhamnosyl ester C3.

[0044] (4) Dissolve 18g of organosilicon polyether modified rhamnosyl ester C3, 1g of sodium bicarbonate, and 0.5g of corrosion inhibitor sodium metasilicate in 80g of deionized water, and add 0.5g of defoamer Coadd. TM DF6904, after being stirred evenly, yields water-based cleaning agent D3.

[0045] Example 4 The preparation method of water-based cleaning agents includes the following steps: (1) In the reaction vessel, 1 mol of rhamnosyl ester WHAR TM -FRL15 was dissolved in 50 mol of deionized water, and 1.7 mol of epichlorohydrin and 3.3 mol of KOH were added to the reaction vessel. The mixture was heated to 50 °C and reacted for 8 hours. After the reaction was completed, excess epichlorohydrin was distilled off under reduced pressure to obtain crude epioxidized rhamnosyl ester aqueous solution A4. According to the titration results of sodium thiosulfate, an average of 1.16 hydroxyl groups in 1 molecule of rhamnosyl ester were replaced by epoxy groups.

[0046] (2) Add 0.25 mol N-methyldodecylamine, 0.85 mol HMS-239B and 0.07 mol Adeka REASOAP ®ER-10 was added to crude epoxy-modified rhamnosyl ester aqueous solution A4, heated to 70℃, reacted for 3 hours, cooled to 25℃, pH adjusted to 4.5 with dilute sulfuric acid, extracted with dimethyl carbonate, and the aqueous phase was discarded to obtain allyl polyether-modified rhamnosyl ester solution B4; by iodometric determination, one molecule of rhamnosyl ester contained an average of 1.15 double bonds.

[0047] (3) Mix allyl polyether modified rhamnosyl ester solution B4 with 1.18 mol 1,1,1,3,3-pentamethyldisiloxane, heat to 75°C, add 0.2 mmol Karstedt catalyst, react for 3 hours, cool to 25°C, remove dimethyl carbonate by vacuum distillation, and obtain organosilicon polyether modified rhamnosyl ester C4.

[0048] (4) Dissolve 10g of organosilicon polyether modified rhamnosyl ester C4, 2g of sodium bicarbonate, and 1g of corrosion inhibitor sodium metasilicate in 86g of deionized water, and add 0.5g of defoamer Coadd. TM DF6904, after being stirred evenly, yields water-based cleaning agent D4.

[0049] Example 5 The preparation method of water-based cleaning agents includes the following steps: (1) In the reaction vessel, 1 mol of rhamnosyl ester WHAR TM -FRL15 was dissolved in 50 mol of deionized water, and 2.3 mol of epichlorohydrin and 4 mol of NaOH were added to the reaction vessel. The mixture was heated to 55 °C and reacted for 6 hours. After the reaction was completed, excess epichlorohydrin was distilled off under reduced pressure to obtain crude epioxidized rhamnosyl ester aqueous solution A5. According to the titration results of sodium thiosulfate, an average of 1.45 hydroxyl groups in 1 molecule of rhamnosyl ester were replaced by epoxy groups.

[0050] (2) Add 0.1 mol di-n-hexylamine, 1.3 mol allyl polyoxypropylene ether APPG300-4PO and 0.05 mol AdekaREASOAP ® ER-10 was added to crude epoxy-modified rhamnosyl ester aqueous solution A5, heated to 55℃, reacted for 6 hours, cooled to 20℃, pH adjusted to 5.5 with dilute hydrochloric acid, extracted with dimethyl carbonate, and the aqueous phase was discarded to obtain allyl polyether-modified rhamnosyl ester solution B5; by iodometric determination, an average of 1.42 double bonds were found in one molecule of rhamnosyl ester.

[0051] (3) Mix allyl polyether modified rhamnosyl ester solution B5 with 1.45 mol 1,1,1,3,3-pentamethyldisiloxane, heat to 70°C, add 0.6 mmol Karstedt catalyst, react for 5 hours, cool down, and remove dimethyl carbonate by vacuum distillation to obtain organosilicon polyether modified rhamnosyl ester C5.

[0052] (4) Dissolve 20g of organosilicon polyether modified rhamnosyl ester C5, 2g of ammonia water, and 1g of corrosion inhibitor sodium metasilicate in 76g of deionized water, and add 1g of defoamer Coadd. TM DF6050, stir well to obtain water-based cleaning agent D5.

[0053] Comparative Example 1 Comparative Example 1 is based on the formulation of Example 1, with the active ingredient, organosilicon polyether modified rhamnose ester, as a dirhamnose monoester WHAR. TM -FRL T3 replacement. Its preparation process is described below: 86g of dirhamnose monoester WHAR TM -FRL T3, 5g sodium hydroxide, 0.5g corrosion inhibitor sodium metasilicate dissolved in 8g deionized water, add 0.5g defoamer Coadd TM DF2510, after being stirred evenly, yields water-based cleaning agent D6.

[0054] Comparative Example 2 Comparative Example 2 is based on the formulation of Comparative Example 1, with the addition of dirhamnose monoester WHAR TM -FRL T3 and sodium hydroxide in equal amounts of rhamnosyl ester WHAR TM -FRL15 and sodium bicarbonate are used as substitutes. The preparation process is described below: 86g of rhamnosyl ester WHAR TM - FRL15 concentrate (30wt% active ingredient), 5g sodium bicarbonate, 0.5g sodium metasilicate corrosion inhibitor dissolved in 8g deionized water, and 0.5g Coadd defoamer added. TM DF2510, after thorough mixing, yields water-based cleaning agent D7.

[0055] Comparative Example 3 Comparative Example 3 is based on the formulation of Example 1, with the active ingredient, organosilicon polyether modified rhamnose ester, as a dirhamnose monoester WHAR. TM -FRL T3, di-n-octylamine, allyl polyoxyethylene ether HMS-238B and 2g Adeka REASOAP ® ER-10 was substituted at approximately the same ratio as in Example 1. The preparation process is described below: 15g of dirhamnose monoester WHAR TM -FRL T3, 1g di-n-octylamine, 5g sodium hydroxide, 7g allyl polyoxyethylene ether HMS-238B, 2g Adeka REASOAP ® ER-10, 0.5g of corrosion inhibitor sodium metasilicate dissolved in 68g of deionized water, and 0.5g of defoamer Coadd added. TM DF2510, after being stirred evenly, yields water-based cleaning agent D8.

[0056] Comparative Example 4 Comparative Example 4 is based on the formulation of Comparative Example 3, with the addition of dirhamnose monoester WHAR TM -FRL T3 with rhamnose ester WHAR TM - A concentrated solution of FRL15 (30wt% active ingredient) is used as a substitute. Its preparation process is described below: 50g of rhamnosyl ester WHAR TM - FRL15 concentrate (30wt% active ingredient), 1g di-n-octylamine, 5g sodium hydroxide, 7g allyl polyoxyethylene ether HMS-238B, 2g Adeka REASOAP ® ER-10, 0.5g of corrosion inhibitor sodium metasilicate dissolved in 33g of deionized water, and 0.5g of defoamer Coadd added. TM DF2510, after thorough mixing, yields water-based cleaning agent D9.

[0057] Comparative Example 5 Comparative Example 5 was based on Example 1, in which an organosilicon-modified polyether mixture was prepared and then reacted with bisrhamnose monoester WHAR. TM -FRL T3 undergoes physical mixing without reacting. Its preparation method is described below: Step 1: Add 1.5 mol of allyl polyoxyethylene ether HMS-238B and 0.1 mol of Adeka REASOAP ® ER-10 and 1.65 mol of 1,1,1,3,5,5,5-heptamethyltrisiloxane were mixed, heated to 80°C, a small amount of Speier catalyst was added, and after reacting for 2 hours, the temperature was lowered to 25°C. Dimethyl carbonate was removed by vacuum distillation to obtain a silicone-modified polyether mixture C6.

[0058] Step 2: Add 15g of dirhamnosyl monoester WHAR TM -FRL T3, 1g di-n-octylamine, 5g sodium hydroxide, 10g organosilicon-modified polyether mixture C6, 0.5g corrosion inhibitor sodium metasilicate dissolved in 68g deionized water, with 0.5g defoamer Coadd added. TM DF2510, when stirred evenly, yields water-based cleaning agent D10.

[0059] Effect Experiment: The water-based cleaning agents D1-D10 obtained in Examples 1-5 and Comparative Examples 1-5 were subjected to tests for surface tension, stability, corrosivity, and detergency. The test conditions are described below: Surface tension: The water-based cleaning agent was diluted with deionized water to a surfactant content of 0.2 wt%, and the surface tension of the water-based cleaning agent was determined according to GB / T 22237-2008 "Determination of Surface Tension of Surfactants". The results are shown in Table 1.

[0060] Stability: The cleaning agent was placed in a sealed transparent container and stored at (-5±2)℃ for 24 hours and (60±2)℃ for 6 hours, respectively. After being taken out and brought to room temperature, its appearance was visually inspected, i.e., low temperature stability and high temperature stability. The results are shown in Table 2.

[0061] Corrosivity: According to the specifications in GB / T 35759-2017 Metal Cleaning Agents, 45# steel, Z30 grade I cast iron, H62 brass, and 1Cr18Ni9Ti stainless steel were used. Metal test pieces were immersed in a cleaning agent solution at a specified temperature. After a specified time, the corrosivity of the metal cleaning agent to the metal was evaluated based on the appearance changes and the amount of corrosion on the metal test pieces. Appearance grades were: Grade 0: No obvious change; Grade 1: Slight discoloration or loss of gloss; Grade 2: Uneven discoloration; Grade 3: Surface discoloration or large-area corrosion. The results are shown in Table 3.

[0062] Cleaning power: According to the provisions of GB / T 35759-2017 Metal Cleaning Agents, metal test pieces coated with artificial heavy oil stains were ultrasonically cleaned for 30 seconds with a 3% cleaning agent solution. The cleaning power was calculated based on the amount of oil stains removed. The results are shown in Table 4.

[0063] Table 1. Surface tension results of cleaning agents D1-D10

[0064] Table 2. Stability results of cleaning agents D1-D10

[0065] Table 3. Corrosivity results of cleaning agents D1-D10

[0066] Table 4. Cleaning power results of cleaning agents D1-D10

[0067] As can be seen from Table 1, the surface tension of the cleaning agent D1-D5 aqueous solution obtained in Examples 1-5 is lower than that in Comparative Examples 1-4, indicating that the surface tension of the organosilicon polyether modified rhamnosyl ester in Examples 1-5 is lower than that of rhamnosyl ester and allyl polyether, etc.; the surface tension of Comparative Example 5 is low because the system contains a mixture of organosilicon modified polyether with low surface tension.

[0068] Table 2 shows that the cleaning agents D1-D5 obtained in Examples 1-5 and the cleaning agents D6 and D7 obtained in Comparative Examples 1-2 all passed the low-temperature and high-temperature stability tests, and the systems were homogeneous without stratification or precipitation. However, Comparative Examples 2-5 all showed stratification, indicating poor stability. This may be due to poor compatibility of the components. The presence of a large amount of sodium hydroxide in Example 1 and Comparative Example 1 indicates strong alkalinity, and their good stability suggests that the selected dirhamnose monoester RL3, which does not contain ester groups, exhibits strong hydrolysis resistance. The stability of Comparative Example 2 indicates that even under weak alkalinity, the rhamnose ester mixture, although containing a certain amount of ester groups, remains relatively stable.

[0069] Table 3 shows that the cleaning agents obtained in each embodiment and comparative example have relatively slight corrosion on 45 steel, Z30 grade 1 cast iron, H62 brass and 1Cr18Ni9Ti stainless steel, which can be considered to meet the usage standards of the above metals.

[0070] Table 4 shows that the cleaning agents D1-D5 obtained in Examples 1-5 have significantly better cleaning power than the cleaning agents D6-D10 obtained in Comparative Examples 1-5.

[0071] In summary, the water-based cleaning agent of the present invention has low surface tension, is suitable for cleaning metal and glass substrates, has high cleaning power, low corrosiveness, good cleaning effect, is green and environmentally friendly, and causes little pollution to the environment.

[0072] The above description of the disclosed embodiments enables those skilled in the art to make or use the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A water-based cleaning agent, characterized by, The raw materials include the following parts by weight: 5-25 parts of organosilicon polyether modified rhamnose ester, 1-5 parts of alkali, 0.5-1 part of corrosion inhibitor, 0.5-1 part of defoamer, and 68-93 parts of water. The preparation method of the organosilicon polyether modified rhamnosine ester includes the following steps: (1) Dissolve rhamnosyl ester in deionized water, add epichlorohydrin and acid-binding agent, heat and react, and distill off excess epichlorohydrin under reduced pressure to obtain crude epioxidized rhamnosyl ester solution. (2) Add alkyl secondary amine, allyl polyether and allyl glycerol alkyl modified polyether to the crude epoxy modified rhamnosine ester solution obtained in step (1), heat the reaction, then cool down, adjust pH=4~6, add solvent for extraction, discard the aqueous phase, and obtain allyl polyether modified rhamnosine ester solution. (3) Add hydrogen-containing silane to the allyl polyether modified rhamnosine ester solution obtained in step (2), heat and add catalyst to react, remove solvent by vacuum distillation to obtain the organosilicon polyether modified rhamnosine ester. In steps (1)-(3), the molar ratio of rhamnosyl ester, deionized water, epichlorohydrin, acid-binding agent, alkyl secondary amine, allyl polyether, allyl glycerol alkyl modified polyether and hydrogen-containing silane is 1:50:(1.5-2.6):(3-4):(0.05-0.3):(0.62-1.5):(0.02-0.1):(0.95-1.65). Based on the effective components, the molar ratio of the catalyst added to the hydrogen-containing silane is 1:(1000-10000).

2. The water-based cleaning agent according to claim 1, characterized in that, The rhamnose ester is one or more of the following: dirhamnose diester RL1, monorhamnose diester RL2, dirhamnose monoester RL3 or monorhamnose monoester RL4. The acid-binding agent is sodium hydroxide or potassium hydroxide; The alkyl secondary amine is any one of the alkyl secondary amines having 7-16 carbon atoms; The allyl polyether is one or more of allyl polyoxyethylene ether, allyl polyoxypropylene ether, or allyl polyoxyethylene polyoxypropylene ether, and the average molecular weight is ≤500 Da. The allylglycerol alkyl modified polyether is a reactive nonionic emulsifier; The pH adjuster is dilute hydrochloric acid or dilute sulfuric acid; The solvent is dimethyl carbonate; The hydrogen-containing silane is 1,1,1,3,3-pentamethyldisiloxane or 1,1,1,3,5,5,5-heptamethyltrisiloxane; The catalyst is either a Speier catalyst or a Karstedt catalyst.

3. The water-based cleaning agent according to claim 1, characterized in that, The alkali is any one of sodium hydroxide, sodium bicarbonate, or ammonia water; The corrosion inhibitor is sodium metasilicate; The defoamer is a polyether-modified silicone emulsion defoamer.

4. The water-based cleaning agent according to claim 1, characterized in that, In step (1), the temperature is raised to 40-60℃ and the reaction is carried out for 4-12 hours.

5. The water-based cleaning agent according to claim 1, characterized in that, In step (2), the temperature is raised to 50-80℃ and reacted for 2-6 hours, then cooled to 20-30℃.

6. The water-based cleaning agent according to claim 1, characterized in that, In step (3), the temperature is raised to 60-80℃ and the catalyst is added. After reacting for 2-6 hours, the temperature is lowered to 20-30℃.

7. A method for preparing a water-based cleaning agent, characterized in that, Includes the following steps: (A) Weigh each raw material according to any one of claims 1-6 for the water-based cleaning agent; (B) Dissolve organosilicon polyether modified rhamnosyl ester, alkali and corrosion inhibitor in deionized water, add defoamer, and stir evenly to obtain water-based cleaning agent.