Thermal field structure and silicon carbide crystal growth apparatus for silicon carbide crystal growth
By combining rigid support components and porous isolation components, the problems of thermal field drift, insulation failure and electromagnetic coupling instability in the thermal field structure of silicon carbide crystal growth were solved, realizing the long-term stability of the thermal field temperature gradient and the industrial-scale preparation of high-quality silicon carbide single crystals.
Patent Information
- Application Number
- CN202610934165.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-26
- Publication Date
- 2026-11-17
AI Technical Summary
Existing silicon carbide crystal growth thermal field structures suffer from problems such as physical sedimentation leading to thermal field drift, vapor phase erosion causing insulation failure, and electromagnetic coupling instability, which seriously affect the industrial-scale preparation of large-size, high-quality silicon carbide single crystals.
Rigid support components are used to support the heating components and crystal growth components. The isolation components construct a porous physical barrier to isolate corrosive gases and form a stable electromagnetic boundary buffer layer through a consumption reaction of porous materials, thus maintaining the stability of the thermal field temperature gradient.
It effectively prevents graphite soft felt from creeping and settling due to its own weight at high temperatures, extends the life of thermal insulation components, reduces the concentration of corrosive gases, stabilizes electromagnetic coupling efficiency, ensures long-term constant temperature gradient of the thermal field, and improves the purity and yield of silicon carbide single crystals.
Smart Images

Figure CN123108727A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the technical field of silicon carbide crystal growth, and more specifically, to a thermal field structure and a silicon carbide crystal growth apparatus for silicon carbide crystal growth. Background Technology
[0002] In the physical vapor transport (PVT) growth of silicon carbide (SiC) crystals, the thermal field temperature within the crystal growth furnace typically reaches 2000°C to 2300°C. The long-term absolute stability of the thermal field temperature gradient is a key factor determining the polymorphic purity, defect density, and yield of SiC single crystals. Graphite felt is usually used as the primary insulation material in the induction thermal field to maintain the axial and radial temperature gradients required for crystal growth.
[0003] In existing induction heating field structures for silicon carbide crystal growth furnaces, graphite felt is typically wrapped directly around the heating chamber or simply stacked, operating in a self-supporting state without rigid structural support. Due to the lack of effective physical barriers within the internal components, high-temperature corrosive gases escaping from the gaps in the heating chamber or crucible assembly directly erode the exposed graphite felt (especially the inner wall of the upper insulation layer and its junction with the side insulation layer). This traditional structure suffers from the following technical drawbacks during long-term high-temperature operation: First, physical settling leads to thermal field drift. Graphite felt exhibits significant creep under prolonged high temperatures, and under its own weight and alternating electromagnetic forces, it is highly susceptible to compaction and settling in the thickness direction. This not only disrupts the original geometric symmetry but also causes a sharp increase in local density and thermal conductivity of the felt, thereby triggering severe thermal field temperature gradient drift.
[0004] Secondly, vapor phase erosion leads to insulation failure. During crystal growth, highly reactive gaseous substances (such as Si, Si2C, and SiC2 vapors, with Si partial pressure typically above 10) escape from the crucible. - ²~10 - ¹ atm) will directly erode the graphite felt through the gaps. The fine carbon fibers on the surface of the felt are prone to react with high-temperature Si vapor to form SiC. The lattice mismatch with the bulk will lead to fiber pulverization and brittle fracture, which will not only cause a sharp drop in the thermal insulation performance of the insulation layer, but also generate carbon dust and cause crystal contamination.
[0005] Third, electromagnetic coupling instability. As the graphite felt is compacted and undergoes localized carbonization and silicification due to the absorption of silicon vapor, its dielectric constant and resistivity will also undergo uncontrollable changes. The felt transforms from a "magnetic permeable body" into a "locally absorbing and heating body," leading to drift in the distribution of induced eddy currents and fluctuations in heating power, making thermal field control extremely prone to instability.
[0006] The three problems mentioned above are interconnected and mutually reinforcing: physical sedimentation increases the gaps in the insulation layer, allowing more corrosive gases to penetrate (exacerbating problem two); vapor phase erosion alters the composition and density of the soft felt, further worsening its electromagnetic properties (exacerbating problem three); and temperature fluctuations caused by electromagnetic instability accelerate the thermal creep sedimentation of graphite fibers (exacerbating problem one). The combined effect of these three factors makes it difficult to maintain the temperature gradient stability of traditional thermal field structures, severely restricting the industrial-scale preparation of large-size, high-quality silicon carbide single crystals. Summary of the Invention
[0007] The purpose of this invention is to provide a thermal field structure and a silicon carbide crystal growth apparatus for silicon carbide crystal growth, so as to solve the technical problems of thermal field drift caused by physical sedimentation, thermal insulation failure caused by gas phase erosion, and electromagnetic coupling instability in the existing thermal field structure.
[0008] To achieve the above objectives, the technical solution adopted by the present invention is as follows: On one hand, the present invention provides a thermal field structure for silicon carbide crystal growth, comprising: A heating element, wherein the heating element is used to provide the required high-temperature heat energy; A crystal growth module is provided inside the heating module to accommodate silicon carbide raw materials and fix seed crystals, so that sublimation gas condenses on the seed crystals to grow into single crystals. An isolation component, disposed above the heating component, is used to isolate corrosive gases; A heat insulation component is disposed around the heating component and the isolation component to form a heat insulation barrier; A rigid support assembly is disposed around the insulation assembly to support the heating assembly, the crystal growth assembly, the isolation assembly, and the insulation assembly, and to constrain the insulation assembly from the outside to prevent axial settlement and radial deformation of the insulation assembly.
[0009] According to the thermal field structure for silicon carbide crystal growth described above, the heating component is an induction heating barrel, which generates eddy currents and heats up under the action of an alternating electromagnetic field.
[0010] According to the above-described thermal field structure for silicon carbide crystal growth, the crystal growth assembly includes a crucible and a seed crystal holder. The crucible is disposed inside the heating assembly and is used to contain silicon carbide raw materials. The seed crystal holder is disposed above the crucible and is used to fix the seed crystal.
[0011] According to the thermal field structure for silicon carbide crystal growth described above, the isolation component includes a vertical isolation member and a horizontal isolation member. The vertical isolation member is cylindrically sleeved on the circumferential outer side above the heating component, and the horizontal isolation member is disposed at the bottom end of the vertical isolation member and extends radially outward.
[0012] According to the aforementioned thermal field structure for silicon carbide crystal growth, the thermal insulation component includes: A bottom insulation component is provided at the bottom of the heating element. The bottom insulation component is made of multiple pieces of insulating graphite soft felt stacked horizontally at the bottom of the heating element. The first side insulation component is disposed on the circumferential sidewall of the heating element. The first side insulation component is made of a whole piece of heat-insulating graphite soft felt vertically disposed on the circumferential sidewall of the heating element. The second side insulation component is disposed on the circumferential sidewall of the isolation component. The second side insulation component is made by horizontally stacking multiple pieces of insulating graphite soft felt on the circumferential sidewall of the isolation component.
[0013] According to the thermal field structure for silicon carbide crystal growth described above, a top insulation component is also provided on the top of the isolation assembly. And / or, a crucible insulation element is provided between the bottom of the crucible of the crystal growth component and the heating component.
[0014] According to the aforementioned thermal field structure for silicon carbide crystal growth, the rigid support assembly includes: A support base is disposed at the bottom of the bottom insulation component; The load-bearing support part has its lower end connected to the support base and its upper end supporting the heating element and the crystal growth element. The load-bearing support part passes through the bottom insulation part and is connected to the heating element. An external limiting member is provided on the radially outer side of the first side insulation member and the second side insulation member, for externally constraining the first side insulation member and the second side insulation member.
[0015] According to the thermal field structure for silicon carbide crystal growth described above, the load-bearing support includes a central support column, which is located at the center of the support base. Alternatively, the load-bearing support includes a central support column located at the center of the support base and a plurality of peripheral support columns evenly distributed around the central position on a concentric circle. The top surfaces of the central support and the peripheral support columns are flush and together support the heating component and the crystal growth component.
[0016] According to the aforementioned thermal field structure for silicon carbide crystal growth, the height of the load-bearing support is less than the thickness of the bottom insulation component.
[0017] On the other hand, the present invention also provides a silicon carbide crystal growth apparatus, including the thermal field structure for silicon carbide crystal growth described above.
[0018] The beneficial effects of the thermal field structure and silicon carbide crystal growth apparatus provided by this invention are at least as follows: (1) The present invention uses a rigid support component to bear the entire gravity load of the heating component and the crystal growth component, so that the insulation component (graphite soft felt) is completely free from pressure. This fundamentally avoids the compaction and settlement of the graphite soft felt due to high temperature creep and its own weight, maintains the long-term constant thickness and porosity of the insulation layer, thereby locking the macroscopic geometric dimensions of the thermal field, maintaining the constant thermal resistance and temperature gradient throughout the entire growth cycle, and preventing the thermal field temperature gradient from drifting.
[0019] (2) The present invention constructs a porous physical barrier between the heating component and the heat preservation component by means of an isolation component. The labyrinth effect greatly extends the diffusion path of corrosive gas. The huge internal surface area of the porous material reacts with the silicon-rich vapor in a sacrificial reaction, "intercepting and consuming" the corrosive gas inside the isolation component. This significantly reduces the concentration of corrosive gas reaching the heat preservation component, delays the siliconization and pulverization of the heat preservation component, extends the heat preservation life, avoids carbon dust contamination of the crystal, and reduces the cost of consumables.
[0020] (3) The present invention uses rigid support components to constrain the heat insulation components from the outside, suppressing the radial loosening and displacement of graphite soft felt under the action of alternating electromagnetic field, and maintaining the geometric symmetry of the thermal field; at the same time, the porous carbon-based material has stable electromagnetic properties (resistivity and dielectric constant do not change significantly with temperature and trace gas phase erosion), which can act as a stable electromagnetic boundary buffer layer in the induction field, avoid the electromagnetic property changes of the heat insulation components due to density and composition changes, stabilize the energy coupling efficiency between the induction coil and the thermal field, and ensure the thermodynamic balance of the crystal growth process. Attached Figure Description
[0021] To more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0022] Figure 1 A cross-sectional schematic diagram of the thermal field structure for silicon carbide crystal growth provided by the present invention. Figure 2This is a schematic diagram of the structure of the second central support column and the outer support column provided by the present invention.
[0023] The following are the labeling elements in the figure: 100. Thermal field structure for silicon carbide crystal growth; 10. Heating component; 20. Crystal growth component; 21. Crucible; 22. Seed crystal holder; 30. Isolation component; 31. Vertical isolation component; 32. Horizontal isolation component; 40. Thermal insulation component; 41. Bottom thermal insulation component; 42. First side thermal insulation component; 43. Second side thermal insulation component; 44. Top thermal insulation component; 45. Crucible thermal insulation component; 50. Rigid support component; 51. Support base; 52. Load-bearing support part; 521. First central support column; 522. Second central support column; 523. Peripheral support column; 53. Peripheral limiting component; 60. Infrared temperature measuring hole; 200. Silicon carbide raw material; 300. Seed crystal. Detailed Implementation
[0024] To make the technical problems to be solved, the technical solutions, and the beneficial effects of the present invention clearer, the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0025] It should be noted that when a component is referred to as "fixed to" or "set on" another component, it may be directly or indirectly located on that other component. When a component is referred to as "connected to" another component, it may be directly or indirectly connected to that other component. The terms "upper," "lower," "left," "right," "front," "rear," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate orientations or positions based on the accompanying drawings, and are for ease of description only, and should not be construed as limiting the technical solution. The terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features. "A plurality" means two or more, unless otherwise explicitly defined.
[0026] Please see Figure 1This embodiment provides a thermal field structure 100 for silicon carbide crystal growth, including a heating element 10, a crystal growth element 20, an isolation element 30, a heat insulation element 40, and a rigid support element 50. The heating element 10 provides the required high-temperature thermal energy; the crystal growth element 20 is disposed within the heating element 10, containing silicon carbide raw material 200 and fixing a seed crystal 300, allowing sublimation gas to condense and grow into a single crystal on the seed crystal 300; the isolation element 30 is disposed above the heating element 10 to isolate corrosive gases; the heat insulation element 40 is disposed around the heating element 10 and the isolation element 30 to form a heat insulation barrier; the rigid support element 50 is disposed around the heat insulation element 40 to support the heating element 10, the crystal growth element 20, the isolation element 30, and the heat insulation element 40, and externally constrains the heat insulation element 40 to prevent axial settlement and radial deformation. Optionally, the insulation component 40 uses graphite felt to prevent heat loss from the heating barrel and to resist external temperature fluctuations.
[0027] The working principle of the thermal field structure 100 for silicon carbide crystal growth provided in this embodiment is as follows: The thermal field structure 100 for silicon carbide crystal growth provided in this embodiment generates high-temperature heat energy when the heating element 10 is energized, causing the silicon carbide raw material 200 inside the crystal growth component 20 to sublimate into a silicon-containing gaseous substance. This gaseous substance condenses and grows into a silicon carbide single crystal at the seed crystal 300 of the crystal growth component 20 due to the temperature difference. Even if the crystal growth component 20 is sealed, corrosive gases can still escape from the gaps in the crystal growth component 20. The isolation component 30, which is set above the heating element 10, can isolate, block and consume the overflowing corrosive gases. Utilizing its porous structure, it forms a tortuous gas diffusion channel between the heating element 10 and the surrounding insulation component 40, which greatly lengthens the diffusion path of the corrosive gases escaping from the crystal growth component 20 when passing through the porous structure. A consumption-type reaction occurs on the huge inner surface of the porous material to generate a silicon carbide protective film, thereby significantly reducing the concentration of corrosive gases reaching the insulation component 40. Meanwhile, the rigid support component 50 bears the gravity load of the heating component 10, the crystal growth component 20, the isolation component 30 and the insulation component 40, and externally constrains the insulation component 40 to prevent it from axial settlement and radial deformation.
[0028] Based on the above-mentioned structural synergy, this embodiment achieves the following technical effects in response to the three major technical defects of the prior art: (1) In response to the problem of thermal field drift caused by physical settlement, this embodiment uses rigid support component 50 to bear all the gravity load of heating component 10 and crystal growth component 20, so that insulation component 40 (graphite soft felt) is completely free from pressure, fundamentally avoiding the compaction and settlement of graphite soft felt due to high temperature creep and its own weight, maintaining the long-term constant thickness and porosity of insulation layer, thereby locking the macroscopic geometric dimensions of thermal field, maintaining the constant thermal resistance and temperature gradient throughout the entire growth cycle, and preventing thermal field temperature gradient drift.
[0029] (2) In response to the problem of thermal insulation failure caused by vapor phase erosion, this embodiment constructs a porous physical barrier between the heating component 10 and the thermal insulation component 40 by means of the isolation component 30. The diffusion path of corrosive gas is greatly extended by utilizing the maze effect. The huge internal surface area of the porous material is used to conduct a sacrificial reaction with the silicon-rich vapor, so that the corrosive gas is "intercepted and consumed" inside the isolation component 30. This significantly reduces the concentration of corrosive gas reaching the thermal insulation component 40, delays the siliconization and pulverization of the thermal insulation component 40, extends the thermal insulation life, avoids carbon dust contamination of the crystal, and reduces the cost of consumables.
[0030] (3) In response to the problem of electromagnetic coupling instability, this embodiment uses a rigid support component 50 to constrain the heat insulation component 40 from the outside, suppressing the radial loosening and displacement of the graphite soft felt under the action of alternating electromagnetic field, and maintaining the geometric symmetry of the thermal field; at the same time, the porous carbon-based material has stable electromagnetic properties (resistivity and dielectric constant do not change significantly with temperature and trace gas phase erosion), which can act as a stable electromagnetic boundary buffer layer in the induction field, avoiding the electromagnetic property changes of the heat insulation component 40 due to changes in density and composition, stabilizing the energy coupling efficiency between the induction coil and the thermal field, and ensuring the thermodynamic balance of the crystal growth process.
[0031] As can be seen, this embodiment forms a positive feedback loop of "axial support to prevent settlement → reducing gas leakage channels → gas phase barrier to protect the stability of graphite felt composition → maintaining electromagnetic property stability → electromagnetic stability to ensure temperature controllability → slowing down graphite felt creep". The rigid support component 50 axially supports and prevents the insulation component 40 from settling, maintaining the density of the insulation layer and the sealing of gaps, and reducing the leakage channels of corrosive gases. The gas phase barrier formed by the isolation component 30 significantly reduces the erosion of the insulation component 40 by corrosive gases, maintaining the stability of the graphite felt composition and electromagnetic properties. The electromagnetic coupling stability ensures the long-term controllability of the thermal field temperature and avoids the negative impact of temperature fluctuations on the creep rate of the felt. It breaks the vicious cycle of "settling-erosion-instability" described in the prior art and jointly achieves the long-term absolute stability of the thermal field temperature gradient, providing a reliable guarantee for the industrial preparation of large-size, high-quality silicon carbide single crystals.
[0032] In one embodiment, the heating component 10 is an induction heating barrel, which generates eddy currents and heats up under the action of an alternating electromagnetic field. The induction heating barrel generates strong induced eddy currents under the action of an external alternating electromagnetic field, resulting in intense heating due to the Joule heating effect. This heating method provides uniform heating, rapid response, and eliminates the need for easily damaged heating elements. It is particularly suitable for ultra-high temperature crystal growth environments of 2000°C to 2300°C, providing continuous, stable, and uniform high-temperature thermal energy for the 200% sublimation of silicon carbide raw materials.
[0033] In one embodiment, see Figure 1 The crystal growth assembly 20 includes a crucible 21 and a seed crystal holder 22. The crucible 21 is disposed inside the heating chamber and is used to contain silicon carbide raw material 200. A very small thermal expansion gap is left between the heating chamber and the sidewall of the crucible 21. The seed crystal holder 22 is disposed above the crucible 21 and is used to fix the seed crystal 300. The crucible 21 contains the silicon carbide raw material 200 and sublimates at high temperature to produce silicon-containing vapor phase material. The seed crystal holder 22 fixes the seed crystal 300 as a condensation substrate. During the rising process, the silicon-containing vapor reaches the seed crystal 300 at a slightly lower temperature, and due to supersaturation, it recondenses on the lower surface of the seed crystal 300 and gradually grows along the axial direction into a complete silicon carbide single crystal ingot.
[0034] In one embodiment, see Figure 1 The isolation assembly 30 includes a vertical isolation member 31 and a horizontal isolation member 32. The vertical isolation member 31 is cylindrically sleeved on the circumferential outer side above the heating assembly 10. The horizontal isolation member 32 is disposed at the bottom end of the vertical isolation member 31 and extends radially outward to connect with the vertical isolation member 31. Optionally, the horizontal isolation member 32 may also be disposed at the top end of the vertical isolation member 31.
[0035] Optionally, both the vertical isolation element 31 and the horizontal isolation element 32 are made of porous graphite with a porosity controlled at 40%~60% and an average pore size of 50μm~150μm. They possess a complex three-dimensional interconnected microchannel structure, a physical labyrinth structure. When gases come into contact with the vertical isolation element 31 and the horizontal isolation element 32, they are forced to pass through their 50μm-150μm tortuous pores. During this process, the gas reacts with the large specific surface area of the porous graphite, generating a self-healing microscopic SiC coating. This significantly consumes silicon vapor and prevents the silicification and pulverization of the soft felt. This structure acts as a physical barrier, blocking the straight-line jet path of corrosive gases. By utilizing the labyrinth effect of the porous structure and the sacrificial reaction, it actively intercepts and consumes corrosive gases, achieving the effects of blocking gas diffusion and extending the insulation life.
[0036] Optionally, the transverse isolation element 32 has a porosity gradient in the thickness direction, with the porosity on the side closer to the heating element being greater than that on the side farther from the heating element. Optionally, the vertical isolation element 31 has a porosity gradient in the thickness direction, with the porosity on the side farther from the insulation component 40 being greater than that on the side closer to the insulation component 40. Larger porosity provides a larger specific surface area for sufficient contact and reaction with corrosive gases, fully utilizing the interception efficiency of the "consumable sacrificial layer"; smaller porosity forms a denser barrier layer, enhancing sealing. This achieves gradient protection with "large-aperture adsorption reaction on the inner side and fine-pore barrier penetration on the outer side," maximizing protection efficiency with minimal material volume.
[0037] Optionally, an infrared temperature measuring hole 60 is provided in the middle of the horizontal isolation component 32 at the top and bottom. The function of the infrared temperature measuring hole 60 is to open an observation window for the infrared thermometer, so that it can pass through the shielding of the isolation component 30 and monitor the key temperature near the seed crystal 300 in real time, providing data support for closed-loop temperature control.
[0038] During the PVT crystal growth process, silicon carbide raw material 200 sublimates at a high temperature of 2000°C~2300°C to generate highly active silicon-rich vapors (Si, Si2C, SiC2, etc.). Since the seed crystal holder 22 and the crucible 21 are mechanically overlapped, there are unavoidable assembly gaps. Driven by thermal buoyancy and concentration gradient, these high-temperature corrosive gases first escape from the overlap gap between the seed crystal holder 22 and the crucible 21 and enter the upper space of the heating chamber.
[0039] At this point, the transverse isolator 32 positioned above the heating element forms the first line of defense. Corrosive gases attempting to escape towards the upper insulation component 40 must first pass through the porous graphite transverse isolator 32. Once inside its tortuous micropores, the diffusion path is lengthened several to tens of times (maze effect), resulting in a significant decrease in flow rate and diffusion flux. Simultaneously, the large internal surface area of the porous graphite (derived from its high porosity of 40%–60%) provides ample active sites for the gas-solid reaction. Silica-rich vapor reacts chemically with carbon atoms on the pore walls to generate a silicon carbide protective film, fixing the corrosive gases as solid products within the porous graphite (a sacrificial reaction). Thus, most of the corrosive gases are intercepted and consumed at the first line of defense.
[0040] An infrared temperature measuring hole 60 is provided in the middle of the horizontal isolation component 32. The function of this infrared temperature measuring hole 60 is to provide an unobstructed optical path for the infrared thermometer, allowing the temperature probe to pass through the obstruction of the isolation component 30 and monitor the temperature at the top of the heating barrel or near the seed crystal holder 22 in real time, providing data support for closed-loop temperature control. However, this infrared temperature measuring hole 60 also provides a vertical escape channel for a small amount of corrosive gas. To address this, this embodiment sets up a vertical isolation component 31 as a second line of defense. Residual corrosive gas escaping upward from the bottom horizontal isolation component 32 and the infrared temperature measuring hole 60 undergoes a labyrinth effect and a sacrificial reaction upon entering the microporous structure of the vertical isolation component 31 and the top horizontal isolation component 32, further reducing the gas concentration.
[0041] This embodiment implements a multi-stage interception path, where corrosive gases are intercepted and consumed step by step, achieving a stepped protection effect of "gradually decreasing gas concentration." After multiple consumptions by the porous graphite isolation component 30, the concentration of corrosive gases reaching the outer insulation component 40 is reduced to an extremely low level, significantly slowing down the siliconization and pulverization rate of the graphite felt. In actual crystal growth production (150-300 hours of single-furnace operation), the service life of the insulation component 40 is significantly extended compared to traditional non-isolated structures, greatly reducing the consumable costs of single-furnace operation. Simultaneously, it prevents carbon dust generated by the pulverization of the felt from falling into the crucible 21 and causing crystal defects, directly ensuring the improvement of the purity and yield of silicon carbide single crystals.
[0042] In one embodiment, see Figure 1 The heat insulation component 40 includes a bottom heat insulation component 41, a first side heat insulation component 42, and a second side heat insulation component 43. The bottom heat insulation component 41 is located at the bottom of the outer side of the heating component 10, and the bottom heat insulation component 41 is composed of multiple pieces of heat-insulating graphite soft felt stacked horizontally at the bottom of the heating component 10; the first side heat insulation component 42 is located on the circumferential side wall of the heating component 10, and the first side heat insulation component 42 is composed of a single piece of heat-insulating graphite soft felt stacked vertically on the circumferential side wall of the heating component 10; the second side heat insulation component 43 is located on the circumferential side wall of the isolation component 30, and the second side heat insulation component 43 is composed of multiple pieces of heat-insulating graphite soft felt stacked horizontally on the circumferential side wall of the isolation component 30.
[0043] The bottom uses multiple graphite soft felts stacked horizontally. By utilizing the extremely low thermal conductivity in the thickness direction of the soft felt and the interlayer contact thermal resistance, the axial thermal resistance is greatly increased, effectively locking in the heat at the bottom to maintain the high temperature of the raw material area. At the same time, the number of layers can be adjusted to flexibly adjust the axial temperature gradient, which is convenient for precise temperature control. It also makes it easy to replace the damaged insulation graphite soft felt layer during use, which greatly reduces maintenance costs and spare parts expenses.
[0044] The first side insulation component 42 is made of a single piece of soft felt vertically placed on the circumferential side wall of the heating element 10, which reduces splicing gaps, continuously and uniformly wraps the main heat source laterally, ensures the continuity and uniformity of the temperature field around the heating barrel, reduces heat loss to the surrounding environment, avoids local hot spots, improves thermal efficiency, and stabilizes the lateral temperature field of the heater area.
[0045] Most of the heat generated by the heating chamber is used to heat the crystal growth components 20 (crucible 21, etc.) inside, but the heat will naturally radiate and conduct upwards. A second side insulation component 43 is installed around the isolation component 30, which is equivalent to adding a heat insulation barrier to the top region of the thermal field, effectively reducing useless heat loss to the upper part of the furnace body through the side wall of the isolation component 30, thus reducing top heat loss. Multiple soft felt layers are horizontally stacked, allowing for flexible adjustment of the number of insulation layers according to actual process requirements, enabling fine-tuning of the top insulation strength. Each layer can be replaced independently, reducing maintenance costs. Optionally, the thickness of each insulating graphite soft felt layer is 8mm to 12mm.
[0046] The overall insulation component 40 described above significantly improves thermal energy utilization and enhances the adjustability and maintainability of the thermal field structure, providing a reliable guarantee for the high repeatability and high quality growth of the seed crystal 300.
[0047] Optionally, a top insulation component 44 is also provided on the top of the isolation component 30. The top insulation component 44 acts as a thermal barrier at the top of the thermal field, reducing heat loss upwards from the top of the thermal field. The top insulation component 44 covers the top isolation component, providing thermal insulation coverage for the isolation component 30, and together with the side insulation layer protected by the isolation component 30, forms a closed thermal insulation chamber. At the same time, a high-temperature buffer zone is formed between the top insulation component 44 and the isolation component 30. After the isolation component 30 blocks most of the corrosive gases, the top insulation component 44 only needs to perform a pure thermal insulation function and does not need to withstand the impact of gas phase erosion.
[0048] Optionally, a crucible insulation component 45 is provided between the bottom of the crucible 21 and the heating chamber of the crystal growth component 20. The crucible insulation component 45 reduces heat loss downwards from the bottom of the crucible 21, concentrating heat in the raw material area, improving temperature uniformity and thermal efficiency in the raw material area, promoting full sublimation of the silicon carbide raw material 200, and increasing the bottom thermal resistance to raise the actual temperature of the raw material area, further widening the axial temperature difference between the raw material area (hot end) and the seed crystal area (cold end), providing a more sufficient thermodynamic driving force for the directional condensation of silicon vapor on the seed crystal 300. The crucible insulation component 45 is made of graphite felt, combining thermal insulation and flexible buffering functions, absorbing dimensional changes caused by the difference in thermal expansion coefficients between the crucible 21 and the heating chamber at high temperatures, and avoiding localized stress concentration or damage caused by rigid contact.
[0049] In one embodiment, see Figure 1 The rigid support assembly 50 includes a support base 51, a load-bearing support part 52, and a peripheral limiting member 53. The support base 51 is disc-shaped and is disposed at the bottom of the bottom insulation member 41. The lower end of the load-bearing support part 52 is connected to the support base 51, and the upper end supports the heating element 10 and the crystal growth component 20. The load-bearing support part 52 passes through the through hole of the bottom insulation member 41 and is connected to the heating element 10. The peripheral limiting member 53 is disposed radially outside the first side insulation member 42 and the second side insulation member 43, and is used to constrain the first side insulation member 42 and the second side insulation member 43 from the outside.
[0050] Optionally, the support base 51 is made of carbon / carbon composite material, which utilizes its extremely high strength and rigidity to support the enormous weight of all the components above. The load-bearing support part 52 is made of porous graphite material, which has excellent high-temperature compressive and bending strength (>20MPa), and the outer limiting part 53 is made of porous graphite material.
[0051] It should be noted that the porous graphite used in the load-bearing support 52, the peripheral limiting component 53, the vertical isolation component 31, and the horizontal isolation component 32 is not ordinary graphite felt or high-density, high-purity graphite block, but a rigid porous carbon-based material sintered through a specific process. Pore characteristics: Porosity is controlled at 40%-60%, preferably 40%-50%, with an average pore size of 50μm-500μm, preferably 50μm-150μm. This porosity characteristic ensures the formation of complex three-dimensional interconnected microchannels (maze effect) internally. Mechanical properties: High-temperature (2000°C) flexural strength is greater than 20MPa, ensuring no creep or fracture under high-temperature heavy loads. Electrothermal characteristics: Resistivity is maintained at 10... -4 It is on the order of Ω•m, falling between conductive heating elements and insulating materials.
[0052] A rigid load-bearing system consisting of a support base 51 and a load-bearing support 52 is set at the bottom of the thermal field. The load-bearing support 52 vertically penetrates the bottom insulation layer, with its lower end connected to the support base 51 and its upper end directly bearing the entire gravity load of the heating barrel and the crystal growth module 20, transferring the load directly to the support base 51, bypassing the bottom insulation component 41. This "load transfer" mechanism completely removes the bottom insulation component 41 from the pressure-bearing state, fundamentally cutting off the physical driving force for the graphite soft felt to be compacted and settled due to high-temperature creep and its own weight, thus achieving anti-axial settlement. The thickness and porosity of the bottom insulation component 41 remain unchanged during the growth cycle of hundreds of hours (150-200 hours), maintaining a constant thermal conductivity at the bottom, thereby preventing the downward shift of the temperature at the center of the thermal field and the drift of the axial temperature gradient, ensuring the stable axial growth of silicon carbide single crystals.
[0053] The outermost limiting member 53 clamps the first side insulation member 42 and the second side insulation member 43 from the outermost side, providing rigid radial constraint to prevent radial loosening, expansion, and flange formation of the first side insulation member 42 and the second side insulation member 43 under the action of alternating electromagnetic field, ensuring the long-term constant radial geometry of the thermal field. The porous graphite material constituting the rigid skeleton has a stable resistivity (10⁻⁶). -4 With a dielectric constant on the order of Ωm, it does not change significantly with temperature and trace amounts of vapor phase erosion. It acts as a stable "electromagnetic boundary buffer layer" in the radio frequency induction field. Even if it absorbs a small amount of silicon vapor, the overall electrical performance drift is minimal, thereby stabilizing the induction heating efficiency, suppressing the fluctuation of induction heating power to a very low range, and improving the macroscopic controllability of the thermal field.
[0054] As can be seen, this embodiment ensures that the macroscopic geometry of the thermal field remains constant during the growth cycle of hundreds of hours through the above-mentioned axial and radial dual locking.
[0055] Optionally, the outer limiting member 53 has a resistivity gradient in the thickness direction, with a higher resistivity (>5×10) near the heating element. -4 Ω•m), the resistivity is lower further away from the heating element (i.e., closer to the induction coil) (<<2×10 Ω•m). -4 (Ω•m), by controlling the distribution of induced current through resistivity gradient, the peripheral limiting component 53 is kept in a "weak heating" state.
[0056] In one embodiment, see Figure 1 The load-bearing support 52 includes a first central support column 521, which is located at the center of the support base 51. Using a single central support column 521 requires less material, is simpler to manufacture, and, being located at the center of the support base 51, ensures the most direct and even distribution of force, preventing uneven weight distribution. A single central support column is suitable for conventionally sized thermal fields.
[0057] In one embodiment, see Figure 2 The load-bearing support 52 includes a second central support column 522 disposed at the center of the support base 51 and a plurality of peripheral support columns 523 evenly distributed on a concentric circle around the center. The top surfaces of the second central support column 522 and the peripheral support columns 523 are flush and together support the heating component 10 and the crystal growth component 20.
[0058] To address the issue of a sharp increase in the total weight of the crucible 21 and raw materials during large-size crystal growth, a multi-point array layout is adopted to distribute the gravity load across multiple peripheral support pillars 523. This significantly reduces stress concentration on individual pillars, avoids the risk of high-temperature fracture, and substantially improves the stability and reliability of the entire thermal field bottom support structure. It ensures that the thermal conductivity of the large-size bottom insulation component 41 remains consistent throughout the entire crystal growth cycle, both at the center and the edges. This is of decisive technical significance for avoiding radially uneven stress and improving crystal crack control during large-size crystal growth. Optionally, the load-bearing support 52 includes one central support pillar and four peripheral support pillars 523.
[0059] In traditional crystal growth furnace designs, dense bulk graphite support rings are sometimes used to support heavy components such as the heating chamber or crucible 21. These rings are sturdy solid rings. This embodiment uses a group of point-distributed porous graphite support pillars. Porous graphite has stable electromagnetic buffering properties. The multi-point distributed porous graphite support pillar group not only achieves rigid support but also avoids the introduction of uneven induced eddy current interference that can occur with dense graphite support rings.
[0060] In one embodiment, see Figure 1 The height of the load-bearing support 52 is less than the thickness of the bottom insulation component 41, and the difference ranges from 10% to 20% of the height of the load-bearing support 52.
[0061] The bottom insulation component 41 is higher than the load-bearing support part 52. After assembly, when the heating component 10 is supported on the top of the load-bearing support part 52, the bottom soft felt is slightly compressed and flush with the top surface of the load-bearing support part 52. This ensures that the load-bearing support part 52 can effectively bear the load, and also prevents the bottom insulation component 41 from losing its insulation performance due to excessive compression. In other words, it ensures that the bottom insulation component 41 is tight and not loose.
[0062] The present invention also provides a silicon carbide crystal growth apparatus, including an induction coil and the thermal field structure 100 for silicon carbide crystal growth described above. Since the thermal field structure 100 for silicon carbide crystal growth has been described in detail above, it will not be repeated here.
[0063] An alternating electromagnetic field generated by energizing the induction coil serves as the energy input source, working in conjunction with the aforementioned thermal field structure. Under the positive feedback loop of the triple mechanism of axial support, vapor barrier, and electromagnetic buffer, the graphite soft felt of the insulation component 40 remains in a state of "no force and no wave absorption," achieving long-term absolute stability of the thermal field temperature gradient over a continuous growth cycle of 150 to 300 hours. This makes it suitable for the industrial-scale preparation of high-quality, large-size silicon carbide single crystals.
[0064] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the protection scope of the present invention.
Claims
1. A thermal field structure for silicon carbide crystal growth, characterized in that, include: A heating element for providing the required heat energy; A crystal growth module is disposed within the heating module to accommodate silicon carbide raw materials and fix seed crystals, so that sublimation gas condenses on the seed crystals to grow into single crystals. An isolation component, disposed above the heating component, is used to isolate corrosive gases; A heat insulation component is disposed around the heating component and the isolation component to form a heat insulation barrier; A rigid support assembly is disposed around the insulation assembly to support the heating assembly, the crystal growth assembly, the isolation assembly, and the insulation assembly, and to constrain the insulation assembly from the outside to prevent axial settlement and radial deformation of the insulation assembly.
2. The thermal field structure for silicon carbide crystal growth as claimed in claim 1, wherein The heating component is an induction heating barrel, which generates eddy currents and heats up under the action of an alternating electromagnetic field.
3. The thermal field structure for silicon carbide crystal growth as claimed in claim 1, wherein The crystal growth assembly includes a crucible and a seed crystal holder. The crucible is disposed inside the heating assembly and is used to contain silicon carbide raw materials. The seed crystal holder is disposed above the crucible and is used to fix the seed crystal.
4. The thermal field structure for silicon carbide crystal growth as claimed in claim 1, wherein The isolation assembly includes a vertical isolation member and a horizontal isolation member. The vertical isolation member is cylindrical and sleeved on the circumferential outer side above the heating assembly. The horizontal isolation member is disposed at the bottom end of the vertical isolation member and extends radially outward.
5. The thermal field structure for silicon carbide crystal growth as claimed in claim 1, wherein The thermal insulation component includes: A bottom insulation component is provided at the bottom of the heating element. The bottom insulation component is made of multiple pieces of insulating graphite soft felt stacked horizontally at the bottom of the heating element. The first side insulation component is disposed on the circumferential sidewall of the heating element. The first side insulation component is made of a whole piece of heat-insulating graphite soft felt vertically disposed on the circumferential sidewall of the heating element. The second side insulation component is disposed on the circumferential sidewall of the isolation component. The second side insulation component is made by horizontally stacking multiple pieces of insulating graphite soft felt on the circumferential sidewall of the isolation component.
6. The thermal field structure for silicon carbide crystal growth of claim 5, wherein, The top of the isolation component is also provided with a top insulation component; And / or, a crucible insulation element is provided between the bottom of the crucible of the crystal growth component and the heating component.
7. The thermal field structure for silicon carbide crystal growth as claimed in claim 5, wherein The rigid support component includes: A support base is disposed at the bottom of the bottom insulation component; The load-bearing support part has its lower end connected to the support base and its upper end supporting the heating element and the crystal growth element. The load-bearing support part passes through the bottom insulation part and is connected to the heating element. An external limiting member is provided on the radially outer side of the first side insulation member and the second side insulation member, for externally constraining the first side insulation member and the second side insulation member.
8. The thermal field structure for silicon carbide crystal growth of claim 7, wherein, The load-bearing support includes a central support column, which is located at the center of the support base; Alternatively, the load-bearing support includes a central support column located at the center of the support base and a plurality of peripheral support columns evenly distributed around the central position on a concentric circle. The top surfaces of the central support and the peripheral support columns are flush and together support the heating component and the crystal growth component.
9. The thermal field structure for silicon carbide crystal growth according to claim 7, characterized in that, The height of the load-bearing support is less than the thickness of the bottom insulation component.
10. A silicon carbide crystal growth apparatus, characterized in that, A thermal field structure for silicon carbide crystal growth according to any one of claims 1 to 9.