An impact-resistant silicon carbide ceramic impeller and its impeller body
By setting stress guiding grooves and protrusions on the front and rear liners of the silicon carbide ceramic impeller, and connecting them with adhesive, the cracking problem of the impeller under impact and vibration conditions was solved, thereby improving its impact resistance and reliability.
Patent Information
- Application Number
- CN202611276524.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-12-18
- Filing Date
- 2026-08-21
- Publication Date
- 2026-11-17
AI Technical Summary
Existing silicon carbide ceramic impellers are prone to cracking and breakage under strong impact and vibration conditions, especially vertical and arc cracks on the outer ring of the front cover plate, resulting in poor impeller reliability.
Stress guiding grooves and protrusions are set on the front and rear liners of the impeller body and connected by adhesive to form multiple sub-liners integral with the skeleton, reducing stress concentration, improving bending strength, and reducing processing costs by plasma or laser cutting.
It significantly improves the impeller's impact resistance, reduces the probability of cracks and fractures, and enhances product qualification rate and reliability.
Smart Images

Figure CN123110133A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of centrifugal pump technology, and in particular to an impact-resistant silicon carbide ceramic impeller and its impeller body. Background Technology
[0002] The impeller of a slurry pump is the most severely worn component, and is generally made of wear-resistant alloy or wear-resistant rubber. However, in some severely worn operating conditions, wear-resistant alloy impellers and wear-resistant rubber impellers often fail to meet the requirements. To improve impeller life, silicon carbide ceramic materials with better wear resistance have been used to make impellers in recent years, but poor impeller reliability has been observed in use. To improve the strength of the impeller, CN202420821399.9 discloses a silicon carbide ceramic impeller, as shown in the attached figure. Figure 21 , 22 As shown, in Embodiment 2 of this application, a skeleton is added to both the front and rear cover plates of the impeller, and an axially protruding outer ring 101' is provided on the radially outer side of the impeller body corresponding to the skeleton of the front cover plate to protect the outer edge of the skeleton from erosion. This structure can significantly improve the strength of the impeller and has achieved good performance in applications with low impact and vibration. However, the silicon carbide impeller of this solution still has a high probability of breakage when used in applications with strong impact and vibration.
[0003] Analysis of numerous impellers damaged by impact fracture as described in Example 2 of CN202420821399.9 revealed that the primary cause of most impeller failures was cracks or latent cracks in the outer ring 101' of the impeller body's front cover plate. These cracks or latent cracks are mainly of two types: vertical cracks (CW) that are approximately perpendicular to the outer circumference of the impeller, and arc-shaped cracks (YW) that develop along the inner edge of the outer ring 101'. Vertical cracks (CW) are more likely to occur because the front and rear cover plates have the largest area and dimensions. During the forming, drying, sintering, and use of the impeller, cracks or latent cracks extending inward from the largest outer ring 101' are easily generated, or stress concentration is likely to occur in this area. Since the radial bending strength perpendicular to the outer ring tangent is relatively weak in the local area of the outer ring 101', these cracks or latent cracks are highly likely to be approximately perpendicular to the outer circumference of the impeller, hence the term "vertical crack." The reason why arc-shaped cracks (YW) are prone to occur is that the outer ring 101' of the front cover plate has an L-shaped structure designed to accommodate the front frame. The cross-sectional area of this L-structure changes abruptly at the inner corner 103', easily causing stress concentration at this point. Arc-shaped cracks (YW) then develop at this stress concentration location. Because these cracks develop roughly along the circumference, they are called arc-shaped cracks (YW). Due to the large size of the impeller body, especially its axial and thickness, existing flaw detection equipment such as X-ray flaw detectors are unable to penetrate the thick impeller body, making it difficult to detect some impeller bodies with hidden arc-shaped cracks (YW), which can easily flow into the subsequent use site. When the slurry pump is working, solid particles enter the axial gap between the impeller and the pump body. If the particle diameter is larger than the axial gap, it will generate axial compressive force on the impeller and pump body. If this axial compressive force acts directly on the location of the arc-shaped crack (YW), even a small compressive force can easily cause the part to detach, leading to rapid overall impeller failure.
[0004] Therefore, existing technologies need further improvement and refinement. Summary of the Invention
[0005] The purpose of this invention is to overcome the shortcomings of the prior art and provide an impact-resistant silicon carbide ceramic impeller to solve the problem of insufficient impact resistance of silicon carbide ceramic impellers in the prior art.
[0006] Another object of the present invention is to provide an impeller body using the impeller body technical features of the above-mentioned impact-resistant silicon carbide ceramic impeller.
[0007] To achieve the above objectives, the technical solution provided by this invention is as follows:
[0008] An impact-resistant silicon carbide ceramic impeller includes an impeller body, a frame, a front liner, and a rear liner. The impeller body is made of silicon carbide and includes a front cover plate, blades, and a rear cover plate arranged sequentially from front to back. The frame includes a rear frame and a front frame. The rear frame is disposed between the rear cover plate and the rear liner, and the front frame is disposed between the front cover plate and the front liner.
[0009] The front liner includes at least three front sub-liners, the outer edges of which extend axially rearward and pass over the outer end face of the front frame; the front sub-liners are provided with a plurality of radially inwardly extending front first extensions at the corresponding radial portion of the front frame, and a front first stress guiding groove is formed between adjacent front first extensions; the front frame is provided with a front protrusion that fits into the front first stress guiding groove to facilitate the connection between the front frame and the front sub-liners, and an adhesive is filled between the front protrusion and the front first stress guiding groove.
[0010] And / or the rear liner includes at least three rear sub-liners, the outer edges of which extend forward axially and pass over the outer end face of the rear frame; the rear sub-liners are provided with a plurality of rear first extensions extending radially inward at the corresponding radial portion of the rear frame, and a rear first stress guiding groove is formed between adjacent rear first front extensions; the rear frame is provided with a rear protrusion that engages with the rear first stress guiding groove to facilitate connection between the rear frame and the rear sub-liners, and an adhesive is filled between the rear protrusion and the rear first stress guiding groove.
[0011] As a preferred embodiment of the present invention, the impeller body is integrally formed.
[0012] As a preferred embodiment of the present invention, the impeller body includes at least three sub-impeller bodies, which are bonded together as a whole by an adhesive.
[0013] As a preferred embodiment of the present invention, the outer edge of the front liner extends axially rearward to the flow channel or blade and is bonded to the blade as a whole; the diameter of the front cover plate is 0.75-0.95 times the diameter of the impeller.
[0014] And / or the outer edge of the rear liner extends axially forward to the flow channel or blade and is bonded to the blade as a whole, wherein the diameter of the rear cover plate is 0.75-0.95 times the diameter of the impeller.
[0015] As a preferred embodiment of the present invention, the outer edge of the front cover plate of the impeller body is connected to a plurality of radially inwardly extending front second extensions, the axial projections of the front second extensions and the front first extensions overlap between the adjacent front protrusions; a front second stress guiding groove is formed between the adjacent front second extensions, the front second stress guiding groove is adapted to the front protrusions, and is bonded together by an adhesive.
[0016] And / or the rear cover plate of the impeller body is connected to a plurality of rear second extensions extending radially inward, the axial projections of the rear second extensions and the rear first extensions overlapping between adjacent rear protrusions; a rear second stress guide groove is formed between adjacent rear second extensions, the rear second stress guide groove is adapted to the rear protrusions and is bonded together by an adhesive.
[0017] As a preferred embodiment of the present invention, the diameter of the front frame is 0.75-0.95 times the diameter of the impeller;
[0018] And / or the diameter of the rear frame is 0.75-0.95 times the diameter of the impeller.
[0019] As a preferred embodiment of the present invention, the front skeleton is made of metal or polymer composite material, or a combination of metal and polymer composite material;
[0020] And / or the rear skeleton is made of metal or polymer composite material, or a combination of metal and polymer material.
[0021] As a preferred embodiment of the present invention, the area of a cross section parallel to the radial outer axis in the first stress guide groove is greater than the area of a cross section parallel to the radial inner axis on the other side.
[0022] And / or the area of the cross section in the first stress guide groove on one radially outer side parallel to the axis is greater than its area on another radially inner side parallel to that cross section;
[0023] And / or the area of the cross section in the pre-second stress guide groove that is radially outer parallel to the axis is greater than its area on the other radially inner cross section that is parallel to the cross section;
[0024] And / or the area of the cross section in the second stress guide groove on one radially outer side parallel to the axis is greater than its area on another radially inner side parallel to that cross section.
[0025] As a preferred embodiment of the present invention, the number of front sub-liners is 3-25;
[0026] Or the number of the rear sub-liners is 3-25.
[0027] As a preferred embodiment of the present invention, the number of the front protrusions is 15-150;
[0028] And / or the number of the rear protrusions is 15-150.
[0029] As a preferred embodiment of the present invention, the number of the front liner plates is an integer multiple of 1 to 5 times the number of blades;
[0030] Or the number of rear sub-liners is an integer multiple of 1 to 5 times the number of blades.
[0031] To achieve the other objective mentioned above, the technical solution provided by this invention is as follows:
[0032] An impeller body having all the technical features of the aforementioned impact-resistant silicon carbide ceramic impeller.
[0033] Compared with existing technologies, the principles and advantages of this technical solution are as follows:
[0034] The diameter of the front liner is the same as that of the impeller, and it includes at least three front sub-liners. This prevents the outer edge of the impeller body's front cover from being directly subjected to axial compressive force. Even if there are undetected hidden cracks in the front cover, the probability of the impeller breaking is reduced to a certain extent compared to existing technologies. Furthermore, the front liner is composed of multiple front sub-liners, and its reduced dimensions decrease the probability of deformation and cracking. It also facilitates the use of flaw detection equipment to inspect the front liner. The outer edge of the front liner extends axially rearward and beyond the outer end face of the front frame, which allows the outer edge of the impeller body front cover plate to avoid the L-shaped structure that encloses the front frame or reduces the axial dimension of the L-shaped structure, thus reducing the probability of cracks or latent cracks in the impeller body front cover plate. The front liner plate has several radially inwardly extending front first extensions at the radial portion corresponding to the front frame, forming a front first stress guiding groove between adjacent front first extensions. This structure guides the stress generated in the front liner plate during sintering along the first stress guiding groove, reducing the likelihood of vertical cracks (CW) and stress release. The probability of arc-shaped cracks (YW) is reduced. Since the probability of two or more vertical cracks forming within a stress guiding groove is very low, and the first forward extension can block stress development at the L-section of the front sub-liner, this structure significantly reduces the probability of arc-shaped cracks (YW) forming on the front sub-liner. A corresponding forward protrusion is provided within the first forward stress guiding groove and is integrated with the front frame; an adhesive is filled between the forward protrusion and the first forward stress guiding groove. This structure further reduces the probability of arc-shaped cracks (YW) forming on the front sub-liner during operation, thereby improving the impeller's impact resistance. Another beneficial effect of this structure is that the front sub-liner can be manufactured using ceramic materials with better impact resistance, increasing the impeller's impact resistance with only a limited increase in cost.
[0035] When the structure of the rear liner, rear sub-liner, and rear cover plate is the same as that of the front liner, front sub-liner, and front cover plate, the same effect will be achieved.
[0036] When the outer edge of the front liner extends axially rearward to the flow channel, the diameter of the front cover plate will decrease accordingly. Simultaneously, the L-shaped structure causing stress concentration on the outer edge of the front cover plate will no longer exist, which helps reduce the formation of arc-shaped cracks (YW) in this area. Of course, this will increase the axial dimension of the L-shaped structure on the front liner plate, which is not conducive to reducing the probability of arc-shaped cracks (YW) on the front liner plate. However, because the front liner plate is smaller in size and it is easier to remove products with hidden cracks through flaw detection or to use materials with better impact resistance, it can generally improve the product qualification rate and impact resistance compared to existing technologies. When the diameter of the front cover plate is too large, approaching the impeller diameter, the cross-sectional dimension of the axial arm of the L-shaped structure on the front liner plate is too small, making it prone to breakage. Conversely, a long cantilever structure will form on the radially outer side of the blade, making it prone to cracking on the radially outer side of the blade during sintering. When the diameter of the front cover plate is 0.75-0.95 times the impeller diameter, the above contradictions can be better balanced. The front liner and blades are bonded together, which can improve the stress on the blades and front liner, increase their strength, and improve the impeller's impact resistance.
[0037] When the rear liner and rear cover plate have the same structure, the same effect as the front liner and front cover plate can be obtained.
[0038] The front cover plate of the impeller body is provided with several radially inwardly extending front second extensions. A front second stress guiding groove is formed between adjacent front second extensions. The front second stress guiding groove is adapted to the front protrusion. When the axial projections of the front second extensions and the front first extensions overlap between adjacent front protrusions, this structure can place both the front first extensions and the front second extensions in the gap between adjacent front protrusions. The front frame can achieve the required precision by plasma or laser cutting, without the need for mechanical cutting, thereby reducing costs. At the same time, it simplifies the geometry of the front liner and the front cover plate of the impeller body, which is beneficial for molding and reduces the probability of cracks or hidden cracks. They are bonded together with adhesive, improving the impact resistance of the impeller.
[0039] The rear cover plate of the impeller body is connected to several radially inwardly extending rear second extensions along its outer edge, and has a similar structure to the front cover plate, thus achieving the same effect.
[0040] The greater the difference between the diameter of the front frame and the impeller, the greater the radial thickness of the front liner plate on the outer radial side of the frame, resulting in increased bending strength of the outer ring. The smaller the difference in bending strength between areas with and without extensions, the higher the probability of vertical cracks not developing along the stress-guiding grooves. Simultaneously, it increases the likelihood of arc-shaped cracks (YW) forming along the L-shaped structure, all of which reduce the impeller's impact resistance. Conversely, if the cross-sectional area of the axial cantilever section of the front liner plate at the L-shape is too small, it is prone to fracture upon impact. Setting the diameter of the front frame to 0.75-0.95 times the impeller diameter can effectively balance these contradictions. Setting the diameter of the rear frame to 0.75-0.95 times the impeller diameter achieves the same effect.
[0041] The front or rear frame is made of metal or polymer composite material, or a combination of metal and polymer composite material, which can significantly improve the impeller's impact resistance.
[0042] The area of a cross section parallel to the radial outer axis within the first stress guide groove is greater than the area of a cross section parallel to that cross section on the other radial inner side. This structure increases the probability of vertical cracks CW being distributed within the first stress guide groove and reduces the probability of circular cracks YW by releasing stress through the generation of vertical cracks CW. On the other hand, this structure can increase the constraint on the radial outer edge of the two vertical cracks CW between the two vertical cracks CW in the front liner when it is impacted during operation, thereby improving the impeller's impact resistance.
[0043] The same structure can be installed in the first stress guide groove, the second stress guide groove, and the second stress guide groove to achieve the same effect.
[0044] If the number of front liners is too small, the yield rate of front liners with larger external dimensions will decrease when the impeller diameter is large. Conversely, if too many front liners are assembled, not only will the assembly process become more difficult, but the reliability will also decrease. Depending on the impeller diameter, setting the number of front liners to 3-25 can better balance the above contradictions. Setting the number of rear liners to 3-25 can also achieve the same effect.
[0045] The width of the first stress guide groove has a significant impact on the internal stress of the impeller body. When the groove is wider, the probability of generating two or more vertical cracks CW within a single groove increases. In this case, the impeller body portion between the vertical cracks CW is less constrained, and the probability of generating arc cracks YW in the L-shaped structure also increases. This significantly increases the probability of the impeller body portion between the cracks detaching from the impeller body and causing impeller fracture and disintegration. If the first stress guide groove is narrower, the vertical crack generated in the outer ring is more likely to extend into the impeller along one of the first stress guide grooves, releasing the internal stress on both sides of the crack. Thus, the probability of vertical cracks generating near the crack is much lower than that of cracks farther away. Clearly, a narrower front stress guide groove width helps reduce the probability of two or more vertical cracks forming within a single groove, thus lowering the probability of impeller breakage and disintegration. From this perspective, a smaller front stress guide groove width is better. However, an excessively small width is detrimental to the arrangement of the front protrusions in the front frame and ensuring sufficient strength. Furthermore, it places higher demands on the dimensional accuracy of the front frame and front sub-liner, increasing manufacturing complexity. When the impeller diameter is fixed, the width of the front stress guide groove is primarily determined by its number. Based on the impeller diameter, setting the total number of front stress guide grooves to 15-150 can effectively balance the aforementioned contradictions. Since the front protrusions correspond to the front stress guide grooves, their number can be set to 15-150; a larger impeller diameter requires more protrusions, and vice versa. Similarly, the number of rear protrusions can be set to 15-150 to achieve the same effect.
[0046] For large impellers, the impeller body includes at least three separately manufactured sub-impeller bodies, which are bonded together as a whole by an adhesive. This structure can improve the yield of impeller body sintering and reduce manufacturing costs. Attached Figure Description
[0047] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0048] Figure 1 This is a cross-sectional view of the impeller in Embodiment 1 of the present invention;
[0049] Figure 2 This is a cross-sectional view of the impeller body in Embodiment 1 of the present invention;
[0050] Figure 3This is one of the perspective views of the impeller body in Embodiment 1 of the present invention;
[0051] Figure 4 This is a second perspective view of the impeller body in Embodiment 1 of the present invention;
[0052] Figure 5 This is one of the perspective views of the assembled front liner plate in Embodiment 1 of the present invention;
[0053] Figure 6 This is a second perspective view of the assembled front liner plate in Embodiment 1 of the present invention;
[0054] Figure 7 This is one of the perspective views of the front sub-liner in Embodiment 1 of the present invention;
[0055] Figure 8 This is a second perspective view of the front sub-liner in Embodiment 1 of the present invention;
[0056] Figure 9 This is a perspective view of the rear skeleton in Embodiment 1 of the present invention;
[0057] Figure 10 This is a perspective view of the anterior skeleton in Embodiment 1 of the present invention;
[0058] Figure 11 This is a perspective view of the assembled rear liner plate in Embodiment 1 of the present invention;
[0059] Figure 12 This is a perspective view of the rear sub-liner in Embodiment 1 of the present invention;
[0060] Figure 13 This is a cross-sectional view of the impeller in Embodiment 2 of the present invention;
[0061] Figure 14 This is a perspective view of the impeller body in Embodiment 2 of the present invention;
[0062] Figure 15 This is a perspective view of the assembled front liner plate in Embodiment 2 of the present invention;
[0063] Figure 16 This is a perspective view of the front sub-liner in Embodiment 2 of the present invention;
[0064] Figure 17 This is a perspective view of the rear skeleton in Embodiment 3 of the present invention;
[0065] Figure 18 for Figure 17 A magnified view of a portion at point A;
[0066] Figure 19 A perspective view of the rear skeleton in Embodiment 4 of the present invention;
[0067] Figure 20This is a perspective view of the assembled impeller body in Embodiment 5 of the present invention;
[0068] Figure 21 A perspective view of the impeller body in the prior art (patent number 202420821399.9);
[0069] Figure 22 for Figure 21 A partial view at point B.
[0070] Figure label:
[0071] 1-Impeller body; 11-Sub-impeller body; 101-Front cover plate; 102-Blade; 103-Rear cover plate; 1011-Front second extension; 1012-Front second stress guide groove; 1013-Front L-section of impeller body; 1031-Rear second extension; 1032-Rear second stress guide groove; 1033-Rear L-section of impeller body; 2-Rear liner; 21-Rear sub-liner; 211-Rear first extension; 212-Rear first stress guide groove; 213-Rear sub-liner L-section; 3-Front liner; 31-Front sub-liner; 311-Front first extension; 312-Front first stress guide groove; 313-Front sub-liner L-section; 4-Front frame; 41-Front outer frame; 42-Front inner frame; 401-Front protrusion; 5-Rear frame; 501-Rear protrusion; CW-Vertical crack; YW-Circular arc crack. Detailed Implementation
[0072] The present invention will be further described below with reference to specific embodiments:
[0073] Example 1
[0074] After analysis, the applicant discovered that in the prior art CN202420821399.9, when the impeller body, frame, and liner are bonded together with adhesive, vertical cracks (CW), circular cracks (YW), or latent cracks on the impeller body are reinforced. Centrifugal force and slight vibration during operation will not cause further development of these cracks or latent cracks, and stress concentration points will not develop into cracks. Because silicon carbide ceramics have high bending strength, the impeller can still operate safely under these conditions. However, when the impeller is subjected to significant impact or vibration, the relatively smooth surface of silicon carbide ceramics results in lower adhesive strength, making the bonded surfaces prone to peeling. This can lead to further development of cracks or latent cracks, or the development of cracks at stress concentration points. However, if there is only one vertical crack in a certain part of the impeller body, even if it is subjected to a certain impact, it will generally not cause the impeller to disintegrate and break apart. This is because when the crack develops to a certain length, after the internal stress is released, the impeller body is protected by the adhesive, and the crack will not continue to extend and cause the impeller to split in two along the crack. Only when two vertical cracks on the front or rear cover plate of the impeller body intersect, or when an arc-shaped crack YW appears between two vertical cracks, the part of the impeller body between these cracks loses the direct connection of ceramic material to the impeller body body, and is only fixed to the side end face or outer edge of the front or rear frame by adhesive force; under the action of strong impact vibration, the adhesive is continuously peeled off, and the already insufficient adhesive force will further decrease, causing this part to fall off. Under the action of centrifugal force, it flies out from the impeller body. If the volume of this part is large and cannot be discharged from the pump body in time, it will collide violently with the impeller body, further causing the impeller to disintegrate and break apart.
[0075] Furthermore, analysis and research revealed certain patterns in the distribution and development of cracks and latent cracks on the impeller body. For example, cracks tend to originate and develop along sections with lower bending strength, which is the main reason for the formation of vertical cracks. Additionally, the distance between the origin points of two adjacent and intersecting vertical cracks or vertical latent cracks is likely not less than a certain value, which is related to the diameter and thickness of the front or rear cover plate, the thickness of the outer ring, etc. Analysis suggests that the main reason is that when a crack is generated in the impeller body during molding, drying, or sintering, the internal stress in the area close to the crack is released or decreases, making it difficult for new vertical cracks to originate in the area close to the crack.
[0076] Furthermore, analysis and research have revealed that cracks located radially inside the impeller body are less likely to propagate after bonding due to greater constraint. Even if the impeller is subjected to significant impact and vibration during operation, the cracks are less likely to develop, thus reducing the probability of the impeller undergoing disintegration. In other words, increasing the constraint on various parts of the impeller body is beneficial to improving the impeller's impact resistance.
[0077] This embodiment, based on the above analysis and research, achieves the following through technical improvements: Figure 1-12 The impact-resistant silicon carbide ceramic impeller shown has a diameter of 1500mm and includes an integrally formed impeller body 1, a frame, a front liner 3, and a rear liner 2. The impeller body 1 includes a front cover plate 101, blades 102, and a rear cover plate 103 arranged sequentially from front to back. The frame includes a rear frame 5 and a front frame 4. The rear frame 5 is disposed between the rear cover plate 103 and the rear liner 2, and the front frame 4 is disposed between the front cover plate 101 and the front liner 3.
[0078] In this article, the terms front, back, inside, and outside are defined as follows: the impeller suction side is front, the opposite side is back, the side closer to the flow channel is inside, and the side farther from the flow channel is outside. Radial inward refers to approaching the main axis radially, and radial outward refers to moving away from the main axis radially.
[0079] The diameter of the front liner 3 is the same as the impeller diameter, equal to the diameter of the outer edge of the blade 102, and is made of pressureless sintered silicon carbide. Figure 5 As shown, it includes 5 front sub-liners 31, as Figure 1 As shown, the outer edge of the front sub-liner 31 extends axially rearward and passes over the outer end face of the front frame 4. The front sub-liner 31 has a plurality of radially inwardly extending front first front extensions 311 at the radial portion corresponding to the front frame 4, and a front first stress guiding groove 312 is formed between adjacent front first front extensions 311. The front frame 4 has a front protrusion 401 that fits into the front first stress guiding groove 312 to facilitate the connection between the front frame 4 and the front sub-liner 31. The front protrusion 401 and the front first stress guiding groove 312 are filled with adhesive. In this embodiment, the front frame 4 is composed of a front outer frame 41 made of polymer material and a front inner frame 42 made of metal material, which are bonded together as a whole by adhesive.
[0080] The diameter of the rear liner 2 is the same as that of the impeller, and includes five rear sub-liners 21 made of zirconia ceramic. The outer edge of each rear sub-liner 21 extends forward axially and passes over the outer end face of the rear frame 5. Each rear sub-liner 21 has several radially inwardly extending rear first forward extensions 211 on the radially outer side corresponding to the rear frame 5. Adjacent rear first forward extensions 211 form rear first stress guiding grooves 212. The rear frame 5 has rear protrusions 501 that engage with the rear first stress guiding grooves 211 to facilitate connection between the rear frame 5 and the rear sub-liners 21. Adhesive is filled between the rear protrusions 501 and the rear first stress guiding grooves 212. In this embodiment, the rear frame 5 is made of carbon steel.
[0081] In this embodiment, since the front liner 3 is assembled from multiple front sub-liners 31, the reduction in its external dimensions can reduce the probability of deformation and cracking of the ceramic parts. It also facilitates the use of flaw detection equipment to inspect the front sub-liners 31. The front sub-liner 31 has several radially inwardly extending front first extensions 311 on its radially outer side corresponding to the front frame 4. Adjacent front first extensions 311 form front first stress guiding grooves 312. This structure can guide the stress generated in the front sub-liner 31 during sintering along the first stress guiding grooves 312 and release the stress. Due to the arrangement of the front first extensions 311, the bending strength along the front sub-liner L portion 313 is significantly greater than that along the front first stress guiding grooves 312, thereby reducing the probability of arc cracks YW forming in the front sub-liner 31 along the front sub-liner L portion 313. The first stress guiding groove 312 is provided with a front protrusion 401 that is adapted to it and connected to the front frame 4 as an integral whole. An adhesive is filled between the front protrusion 401 and the first stress guiding groove 312. This structure can further reduce the probability of arc cracks YW forming in the front sub-liner 31 during operation, thereby improving the impeller's impact resistance. Obviously, due to the provision of the first stress guiding groove 312, the probability of vertical cracks CW forming on the front sub-liner 31 increases, while the probability of arc cracks forming along the L portion 313 of the front sub-liner is greatly reduced. Thus, even if... Figure 8 Two intersecting vertical cracks CW are generated within the two stress guide grooves 312 of a front liner 31. However, due to the presence of the front protrusion 401 on the front frame 4, the protrusion 401 can reliably restrain the broken ceramic pieces between the two vertical cracks from falling off using adhesive. This significantly improves the impeller's impact resistance.
[0082] By using the same principle, the same effect can be achieved by setting structures such as the rear first stress guide groove 212, the rear first extension 211, and the rear sub-liner L part 213 on the rear sub-liner 21.
[0083] In this embodiment, the impeller body 1 is made of reaction-sintered silicon carbide. The outer edge of the front cover plate 101 is connected with several radially inwardly extending front second extensions 1011, similar to the front first extensions 311 provided on the sub-front liner 31. This can reduce the probability of arc cracks YW generated along the front L portion 1013 of the impeller body. The axial projections of the front second extensions 1011 and the front first extensions 311 overlap and are both located between adjacent front protrusions 401 on the front frame 4. A front second stress guide groove 1012 is formed between adjacent front second extensions 1011. The front second stress guide groove 1012 is adapted to the front protrusions 401. This structure allows the front frame 3 to achieve the required precision through plasma or laser cutting without mechanical cutting, thereby reducing costs. At the same time, it simplifies the geometry of the front sub-liner 31 and the front cover plate 101 of the impeller body 1, which is beneficial for molding and reduces the probability of generating cracks or hidden cracks, thus improving the impact resistance of the impeller.
[0084] The rear cover plate 103 of the impeller body 1 is connected to a plurality of rear second extensions 1031 extending radially inward. The axial projections of the rear second extensions 1031 and the rear first extensions 211 overlap. A rear second stress guide groove 212 is formed between adjacent rear second extensions 1031. The rear second stress guide groove 212 is adapted to the rear protrusion 501 and is bonded together with an adhesive. Its effect is the same as that of the aforementioned front cover plate of the impeller body.
[0085] In this embodiment, the diameter of the front frame 4 is 0.85 times the diameter of the impeller; the diameters of the front frame 4 and the rear frame 5 refer to their diameters at their furthest points from the axis, and the diameter of the rear frame 5 is 0.95 times the diameter of the impeller.
[0086] like Figure 8 As shown, the area of the first stress guiding groove 312 on a radially outer CC section parallel to the axis is greater than its area on a radially inner DD section parallel to the plane. This structure increases the probability of vertical cracks CW being distributed within the first stress guiding groove, thereby reducing the probability of circular cracks YW being generated. On the other hand, the wedge-shaped structure formed after the first stress guiding groove 312 and the front protrusion 401 are filled with adhesive can further increase the constraint force of the front frame 4 on the front liner 31, preventing the front liner 31 from coming off due to cracking. The same structure can be provided in the rear first stress guiding groove, the front second stress guiding groove, and the second stress guiding groove to achieve the same effect.
[0087] In this embodiment, the number of front sub-liners 31 and rear sub-liners are both 5 pieces, and the number of blades 102 is 5 pieces, with the number of the former being 1 times the number of blades 102.
[0088] In this embodiment, there are 30 front protrusions 401 and 30 rear protrusions 501.
[0089] Comparative studies show that when the silicon carbide ceramic impeller of this embodiment is used under the same conditions of significant vibration and impact, the probability of impeller breakage is reduced by about 90%.
[0090] Example 2
[0091] like Figure 13-16 As shown, the main difference between this embodiment and Embodiment 1 is that the impeller diameter is 1200mm, and the outer edge of the front sub-liner 31 extends axially rearward to the flow channel or blade 102; it is partially bonded to the blade 102. With this structure, the diameter of the front cover plate 101 is correspondingly smaller than the diameter of the outer edge of the blade 102, and there is no L-shaped structure on the outer edge of the front cover plate 101, which helps reduce the generation of arc-shaped cracks YW in this area. Of course, this leads to an increase in the axial dimension of the L-shaped structure 313 on the front sub-liner 31, which is not conducive to reducing the probability of arc-shaped cracks YW on the front sub-liner 31. However, since the front sub-liner 31 is smaller in size and it is easier to remove products with hidden cracks through flaw detection, it can generally improve the product qualification rate and impact resistance compared to the prior art. The front liner 3 is composed of 5 front sub-liners 31, which solves the problem of how the protrusion 401 is inserted into the front first stress guide groove 312. In this embodiment, the diameter of the front cover plate 101 refers to its average diameter, which is 0.85 times the impeller diameter. The diameter of the rear cover plate 103 is also 0.85 times the impeller diameter. Obviously, in similar embodiments of this embodiment, depending on the different application conditions of the impeller, the diameter of the front cover plate 101 or the rear cover plate 103 can also be selected as 0.75-0.95 times the impeller diameter.
[0092] Example 3
[0093] As shown in Figures 17 and 18, the structure of this embodiment is roughly the same as that of Embodiment 1, except that the impeller diameter is 2000 mm, the number of rear protrusions 51 on the rear frame 5 is 150, and the number of front sub-liners 31 is 25, which is 5 times the number of blades 102. The diameter of the rear frame 51 is 1900 mm, which is 0.95 times the impeller diameter.
[0094] Example 4
[0095] like Figure 19As shown, the structure of this embodiment is largely the same as that of Embodiment 1. The main differences are that the impeller diameter is 500mm, the number of rear protrusions 51 on the rear frame 5 is 15, the number of front liner plates 31 is 3, and the number of blades 102 is 3, the former being twice that of the latter. The diameter of the rear frame 5 is 375mm, which is 0.75 times the impeller diameter.
[0096] Example 5
[0097] like Figure 20 As shown, the structure of this embodiment is largely the same as that of Embodiment 1, with the main difference being that the impeller diameter is 2200mm, the number of blades 102 is 5, and the impeller body 1 is composed of 5 silicon carbide sub-impeller bodies 11 assembled and bonded together. This structure can greatly reduce the external dimensions of the impeller body and improve the yield of the sub-impeller bodies 11. When the number of sub-impeller bodies 11 and the number of blades 102 are the same, the sub-impeller bodies 11 can be easily standardized for production.
[0098] Example 6
[0099] This embodiment is largely the same as Embodiment 5, with the main difference being that the impeller diameter is 800mm, the impeller body 1 is composed of 3 sub-impeller bodies 11, and the impeller is provided with 3 blades 102. The number of front sub-liners is 3, and the number of rear sub-liners is 3.
[0100] The above-described embodiments are merely preferred embodiments of the present invention and are not intended to limit the scope of the present invention. Therefore, any changes made in accordance with the shape and principle of the present invention should be covered within the protection scope of the present invention.
Claims
1. A shock resistant silicon carbide ceramic impeller comprising an impeller body, a skeleton, a front liner and a rear liner, characterized in that: The impeller body is made of silicon carbide and includes a front cover plate, blades and a rear cover plate arranged sequentially from front to back; the frame includes a rear frame and a front frame; the rear frame is disposed between the rear cover plate and the rear liner plate, and the front frame is disposed between the front cover plate and the front liner plate; The front liner includes at least three front sub-liners, the outer edges of which extend axially rearward and pass over the outer end face of the front frame; the front sub-liners are provided with a plurality of radially inwardly extending front first extensions at the corresponding radial portion of the front frame, and a front first stress guiding groove is formed between adjacent front first extensions; the front frame is provided with a front protrusion that fits into the front first stress guiding groove to facilitate the connection between the front frame and the front sub-liners, and an adhesive is filled between the front protrusion and the front first stress guiding groove. And / or the rear liner includes at least three rear sub-liners, the outer edges of which extend forward axially and pass over the outer end face of the rear frame; the rear sub-liners are provided with a plurality of rear first extensions extending radially inward at the corresponding radial portion of the rear frame, and a rear first stress guiding groove is formed between adjacent rear first front extensions; the rear frame is provided with a rear protrusion that engages with the rear first stress guiding groove to facilitate connection between the rear frame and the rear sub-liners, and an adhesive is filled between the rear protrusion and the rear first stress guiding groove.
2. The impact resistant silicon carbide ceramic impeller of claim 1, wherein: The impeller body is integrally formed.
3. The impact resistant silicon carbide ceramic impeller of claim 1, wherein: The impeller body includes at least three sub-impeller bodies, which are bonded together as a whole by an adhesive.
4. The impact resistant silicon carbide ceramic impeller of claim 1, wherein: The outer edge of the front liner extends axially rearward to the flow channel or blade and is bonded to the blade as a whole; the diameter of the front cover plate is 0.75-0.95 times the diameter of the impeller; And / or the outer edge of the rear liner extends axially forward to the flow channel or blade and is bonded to the blade as a whole, wherein the diameter of the rear cover plate is 0.75-0.95 times the diameter of the impeller.
5. The impact resistant silicon carbide ceramic impeller of claim 1, wherein: The front cover plate of the impeller body is connected to a plurality of radially inwardly extending front second extensions, the axial projections of the front second extensions and the front first extensions overlap between the adjacent front protrusions; a front second stress guide groove is formed between the adjacent front second extensions, the front second stress guide groove is adapted to the front protrusions and is bonded together by an adhesive; And / or the rear cover plate of the impeller body is connected to a plurality of rear second extensions extending radially inward, the axial projections of the rear second extensions and the rear first extensions overlapping between adjacent rear protrusions; a rear second stress guide groove is formed between adjacent rear second extensions, the rear second stress guide groove is adapted to the rear protrusions and is bonded together by an adhesive.
6. The impact resistant silicon carbide ceramic impeller of claim 1, wherein The diameter of the front frame is 0.75-0.95 times the diameter of the impeller; And / or the diameter of the rear frame is 0.75-0.95 times the diameter of the impeller.
7. The impact resistant silicon carbide ceramic impeller of claim 1 wherein, The front skeleton is made of metal or polymer composite material, or a combination of metal and polymer composite material. And / or the rear skeleton is made of metal or polymer composite material, or a combination of metal and polymer material.
8. The impact resistant silicon carbide ceramic impeller of claim 1 wherein, The area of the cross section parallel to the radial outer axis in the first stress guide groove is greater than its area on the other radial inner side and parallel to that cross section. And / or the area of the cross section in the first stress guide groove on one radially outer side parallel to the axis is greater than its area on another radially inner side parallel to that cross section; And / or the area of the cross section in the pre-second stress guide groove that is radially outer parallel to the axis is greater than its area on the other radially inner cross section that is parallel to the cross section; And / or the area of the cross section in the second stress guide groove on one radially outer side parallel to the axis is greater than its area on another radially inner side parallel to that cross section.
9. The impact resistant silicon carbide ceramic impeller of claim 1 wherein, The number of the front sub-liner plates is 3-25; Or the number of the rear sub-liners is 3-25.
10. The impact resistant silicon carbide ceramic impeller of claim 1 wherein, The number of the front protrusions is 15-150; And / or the number of the rear protrusions is 15-150.
11. The impact resistant silicon carbide ceramic impeller of claim 1 wherein, The number of the front liner plates is an integer multiple of 1 to 5 times the number of blades; Or the number of rear sub-liners is an integer multiple of 1 to 5 times the number of blades.
12. An impeller body characterized by, The impeller body has all the technical features of an impact-resistant silicon carbide ceramic impeller as described in any one of claims 1 to 5.
Citation Information
Patent Citations
Silicon carbide ceramic impeller
CN222046207U