A method for preparing a high-performance ceramic plate with a pre-crack barrier structure and a composite protective structure.

By introducing a pre-formed crack barrier structure into the ceramic plate, a gradient match between the hard ceramic unit and the interface barrier zone is achieved, which solves the problem of crack propagation in ceramic materials after bullet impact, improves the ceramic plate's resistance to multiple hits and yield, and reduces production costs.

CN123111012APending Publication Date: 2026-11-17杭州智元研究院有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611601085.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-16
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing ceramic materials are prone to large-area crack propagation and breakage after being hit by bullets, resulting in reduced protective capabilities. Furthermore, large-size ceramics have low yield rates, high production costs, and low bonding strength at the physical splicing interface, making it impossible to effectively prevent crack propagation.

Method used

High-performance ceramic plates with pre-fabricated crack-blocking structures achieve a gradient matching of "high hardness-high toughness" and "high modulus-low modulus" by setting interfacial barrier zones between hard ceramic units and forming a metallurgical bond through secondary sintering. The crack propagation is cut off by using a grid-like crack-blocking system.

Benefits of technology

It effectively blocks crack propagation, improves resistance to multiple impacts, enhances the integrity and yield of ceramic plates, reduces production costs, prevents softening and deformation of ceramic units, and forms a continuous interface bond.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123111012A_ABST
    Figure CN123111012A_ABST
Patent Text Reader

Abstract

This invention discloses a high-performance ceramic plate with a pre-formed crack-blocking structure and a method for preparing a composite protective structure, comprising hard ceramic units and an interface barrier region. The hard ceramic units are formed into high-density, high-hardness ceramics through a first sintering process. The interface barrier region is disposed within the gaps between multiple hard ceramic units and is formed through a second sintering process, metallurgically / sinteringly bonding with the hard ceramic units to form a dense whole. This solution, through the design of the formulation and sintering method of the hard ceramic units and the interface barrier region, as well as the matching of their performance parameters, can eliminate interface microcracks, voids, shrinkage mismatch, and debonding, preventing the barrier region from becoming a weak penetration channel. The resulting interface barrier region is tough yet not weak, with no drastic drop in hardness, and does not experience through-hole failure, achieving "tough yet not weak, hard yet not brittle." It confines impact damage to a single unit, preventing crack propagation and penetration, thus improving resistance to multiple impacts.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of high-performance protective materials and composite protective structures, specifically relating to a high-performance ceramic plate with a pre-formed crack barrier structure and a method for preparing a composite protective structure. Background Technology

[0002] Lightweighting and improved protective capabilities are crucial indicators for evaluating the performance of protective equipment. The core value of protective equipment lies in effectively resisting lethal threats without significantly increasing its weight. Materials technology, as the core foundation for the development of protective equipment, is key to overcoming performance bottlenecks. High-performance ceramic materials, with their ultra-high hardness and low density, are among the most critical materials in protective equipment. However, due to the inherent brittleness of ceramic materials, a single bullet impact often results in large-scale fractures and breakage of the ceramic layer, and extensive deformation and delamination of the fiber layer, significantly reducing its protective capabilities. Therefore, improving the resistance to multiple projectiles while ensuring the lightweight nature of the ceramic fiber composite structure is a pressing technical problem. Furthermore, reducing the crack propagation range is crucial for achieving resistance to multiple projectiles.

[0003] Traditional one-piece molded ceramic plates, such as alumina, silicon carbide, and boron carbide ceramics, all suffer from the following drawbacks, regardless of whether they are sintered using hot pressing, pressureless sintering, or reaction sintering processes:

[0004] 1) The whole piece of ceramic is brittle, and the crack propagation area is large after impact.

[0005] Radial cracks caused by impact can penetrate the entire ceramic piece, leading to large-area failure, loss of continued protective ability, and poor resistance to multiple consecutive impacts.

[0006] 2) Large-size ceramics are difficult to sinter in one step.

[0007] Solid ceramic blocks of 300 mm to 500 mm size are prone to warping, internal cracking, uneven density, and abnormal grain growth during high-temperature sintering, resulting in low yield and high production costs.

[0008] 3) Conventional physical splicing of ceramics has fatal defects.

[0009] Simply splicing ceramic interfaces involves physical contact, resulting in extremely low bonding strength. After being struck, the ceramics are prone to delamination, detachment, and chipping, making it impossible to form an overall load-bearing structure and posing a very high risk of protective failure.

[0010] Current technologies cannot simultaneously achieve effective crack prevention, high yield of large-size products, and stable protection against multiple cracks while ensuring the high hardness and penetration resistance of ceramic units. Therefore, developing a high-performance ceramic suitable for industrial production that can effectively prevent crack propagation has significant engineering value. Summary of the Invention

[0011] This invention addresses the problems existing in the prior art by providing a high-performance ceramic plate with a pre-formed crack barrier structure and a method for preparing a composite protective structure, which can solve the following key problems:

[0012] 1) Eliminate interfacial microcracks, voids, shrinkage mismatch, and debonding;

[0013] 2) Prevent the barrier area from becoming a weak penetration channel, and achieve "tough but not weak, hard but not brittle";

[0014] 3) Avoid secondary sintering, which can cause over-firing, softening, and grain coarsening of ceramic units;

[0015] 4) Improve the dimensional accuracy, flatness, and yield of large-size ceramics;

[0016] 5) It achieves forced isolation, localization, and non-penetration of projectile-induced cracks, significantly improving the ability to resist multiple strikes.

[0017] The specific technical solution for the objective of this invention is as follows:

[0018] A high-performance ceramic plate with a pre-formed crack barrier structure includes hard ceramic units and an interface barrier region.

[0019] The hard ceramic unit is formed into a high-density, high-hardness ceramic through a first sintering process. The interface barrier region is set in the gap between multiple hard ceramic units and is formed through a second sintering process, forming a dense whole with the hard ceramic unit through metallurgical / sintering bonding.

[0020] The hard ceramic units and interface barrier regions are formulated with different formulations and sintering methods to create gradient differences in mechanical properties;

[0021] The difference in wave impedance between the hard ceramic unit and the interface barrier region leads to a reduction in the stress transmission intensity between the ceramic units.

[0022] The interface barrier region forms a grid-like crack barrier system to cut off the propagation of cracks caused by impact.

[0023] Furthermore, a gradient matching of "high hardness - high toughness" and "high modulus - low modulus" is formed between the hard ceramic unit and the interface barrier region:

[0024] The ratio of the elastic modulus of the interface barrier region to the elastic modulus of the hard ceramic unit, Ei / Eu, ranges from 0.70 to 0.90.

[0025] The ratio of the hardness of the interface barrier region to the hardness of the hard ceramic unit, Hi / Hu, ranges from 0.50 to 0.70.

[0026] The fracture toughness of the interface barrier region is between 1.5 and 2.5 times that of the ceramic unit.

[0027] Furthermore, the hard ceramic unit is square, rectangular, hexagonal, or circular in shape, and is made of boron carbide ceramic, silicon carbide, or other high-performance ceramics.

[0028] The thickness of the ceramic unit ranges from 6 mm to 25 mm, and the length and width range from 30 mm to 130 mm.

[0029] Furthermore, the thickness of the interface barrier region ranges from 0.5 mm to 2 mm, and it is prepared using SiC or... As the base, add Phase transformation toughening, SiCw whisker toughening, One or more composite materials in particle toughening form toughened multiphase ceramics.

[0030] Furthermore, the fabrication process of the hard ceramic unit includes:

[0031] High-density hard ceramic units are obtained by mixing, ball milling, molding, and first sintering according to a preset formula;

[0032] The first sintering is densification sintering, which adopts any one of hot pressing sintering, pressureless sintering, and reaction sintering to obtain hard ceramic units with a density ≥ 97%, Vickers hardness ≥ 28 GPa, and flexural strength ≥ 400 MPa.

[0033] The hard ceramic unit is subjected to micro-roughening treatment through one or more of the following methods: sandblasting, laser etching, and acid etching, to form a dual reinforcement of mechanical interlocking and sintering.

[0034] Furthermore, the hard ceramic units are arranged in an array as required and fixed to a special graphite mold, with uniform gaps reserved.

[0035] Ceramic powder from the interface barrier zone is evenly filled into the gap. The filling is achieved through dry filling, vibration compaction, and light cold pressing to ensure dense filling without voids or bridging, forming a continuous grid-like interface barrier zone. This effectively prevents crack propagation and confines the damage to a single hard ceramic unit.

[0036] The filled interface barrier region and hard ceramic unit are sintered a second time to make the powder in the interface barrier region dense and form a strong sintered bond with the hard ceramic unit, thus obtaining an integrated high-performance ceramic plate.

[0037] Furthermore, the temperature of the second sintering is 100-200°C lower than that of the first sintering to ensure that the hard ceramic unit does not soften, deform, recrystallize, or have a coarse reaction layer.

[0038] The ceramic unit and the barrier region have different material systems, different sintering regimes, and matched toughness gradients, with no obvious gaps or weak bonding surfaces.

[0039] The second sintering process employs hot pressing and static isobaric methods to compensate for shrinkage stress and achieve defect-free metallurgical bonding in the interface barrier zone.

[0040] Furthermore, after the integrated high-performance ceramic plate is prepared, it undergoes surface grinding, chamfering, and surface sealing treatment.

[0041] Furthermore, it includes, in sequence, a crack-arresting layer, a high-performance ceramic plate layer, and a fiber composite material layer;

[0042] The crack-arresting layer has a surface density of 80~140 g / cm³. 3 Woven fabrics made of aramid II or aramid III;

[0043] The fiber composite material layer is composed of one or more high-performance fibers, such as aramid fiber UD composite material, ultra-high molecular weight polyethylene UD composite material, carbon fiber UD composite material, and PBO fiber composite material.

[0044] The crack-resistant layer, the high-performance ceramic plate layer, and the fiber composite material layer are connected by an adhesive film.

[0045] This solution also provides a method for preparing the above-mentioned high-performance ceramic composite protective structure, wherein the crack-arresting layer, adhesive film, high-performance ceramic plate layer, adhesive film, and fiber composite material layer are stacked sequentially, and the whole structure is subjected to hot pressing treatment to obtain the high-performance ceramic composite protective structure.

[0046] The hot pressing process is carried out in an autoclave according to the following steps:

[0047] (1) Raise the temperature from room temperature to 60±3℃, pressurize to 0KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 15 minutes;

[0048] (2) Increase the temperature from 60±3℃ to 120±3℃, pressurize to 1000KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 45 minutes;

[0049] (3) Maintain 120±3℃, maintain pressure of 1000KPa, maintain vacuum value of -0.1~-0.09MPa, and keep warm for 60 minutes;

[0050] (4) Cool down to room temperature, maintain pressure of 1000 kPa, vacuum value of -0.1 to -0.09 MPa, and keep warm for 10 minutes;

[0051] (5) Maintain room temperature, reduce pressure to 0 kPa, keep vacuum value at -0.1~-0.09 MPa, and keep warm for 20 minutes.

[0052] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0053] (1) The high-performance ceramic plate with prefabricated crack barrier structure proposed in this invention forms an integrated hard ceramic unit and interface barrier area through secondary sintering. By setting the ratio of elastic modulus, hardness and fracture toughness between the ceramic unit and the interface barrier area, a gradient matching of "high hardness - high toughness" and "high modulus - low modulus" is achieved between the ceramic unit and the interface barrier area. This enables the impact damage to be confined to a single unit, and the cracks do not propagate or penetrate, thus improving the resistance to multiple impacts.

[0054] (2) The high-performance ceramic plate with pre-crack barrier structure proposed in this invention is formed by secondary sintering, which has higher integrity than the physical splicing structure. The second sintering temperature of this scheme is 100~200℃ lower than the first sintering temperature to ensure that the ceramic unit does not soften, deform, recrystallize, or have a coarse reaction layer. The ceramic unit and the interface barrier region have different material systems, different sintering regimes, and matching toughness gradients. There are no obvious gaps or weak bonding surfaces. The secondary sintering adopts a multiphase system with a lower sintering temperature and higher toughness. The chemical composition of the two is different. By controlling the sintering aid and high-temperature diffusion reaction, the powder of the interface barrier region and the surface of the ceramic unit undergo solid-phase diffusion or transient liquid-phase sintering during the secondary sintering to form a metallurgical bonding layer. The two can still form a continuous interface bond. The interface barrier region formed is tough but not weak, the hardness does not drop sharply, and there is no through-through failure.

[0055] The present invention will be further described below with reference to specific embodiments. Attached Figure Description

[0056] Figure 1 This is a schematic diagram of a high-performance ceramic plate structure with a pre-fabricated crack barrier structure in an embodiment of the present invention.

[0057] Figure 2 This is a schematic diagram of the shape of the hard ceramic unit in an embodiment of the present invention.

[0058] Figure 3 This is a schematic diagram of a high-performance ceramic composite protective structure in an embodiment of the present invention. Detailed Implementation

[0059] Example

[0060] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. The described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0061] As indicated in this application and claims, unless the context clearly indicates otherwise, the words "a," "an," "an," and / or "the" do not specifically refer to the singular and may also include the plural. Generally speaking, the terms "comprising" and "including" only indicate the inclusion of explicitly identified steps and elements, which do not constitute an exclusive list, and the method or apparatus may also include other steps or elements.

[0062] Unless otherwise specifically stated, the relative arrangement, numerical expressions, and values ​​of the components and steps described in these embodiments do not limit the scope of this application. It should also be understood that, for ease of description, the dimensions of the various parts shown in the drawings are not drawn to actual scale. Techniques, methods, and devices known to those skilled in the art may not be discussed in detail, but where appropriate, such techniques, methods, and devices should be considered part of the specification. In all examples shown and discussed herein, any specific values ​​should be interpreted as merely exemplary and not as limitations. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters in the following drawings denote similar items; therefore, once an item is defined in one drawing, it need not be further discussed in subsequent drawings.

[0063] Combination Figure 1 A high-performance ceramic plate with a pre-fabricated crack barrier structure includes a hard ceramic unit 1 and an interface barrier region 2.

[0064] The hard ceramic unit 1 is formed into a high-density, high-hardness ceramic through a first sintering process. The interface barrier region 2 is disposed in the gap between multiple hard ceramic units 1 and is formed through a second sintering process, forming a dense whole with the hard ceramic unit 1 through metallurgical bonding / sintering bonding.

[0065] The hard ceramic unit 1 and the interface barrier region 2 are formulated with different formulations and sintering methods to form a gradient difference in mechanical properties;

[0066] The difference in wave impedance between the hard ceramic unit 1 and the interface barrier region 2 leads to a reduction in the stress transmission intensity between the ceramic units 1.

[0067] The interface barrier zone 2 forms a grid-like crack barrier system to cut off the propagation of cracks caused by impact.

[0068] Furthermore, a gradient matching of "high hardness - high toughness" and "high modulus - low modulus" is formed between the hard ceramic unit 1 and the interface barrier region 2:

[0069] The ratio of the elastic modulus of the interface barrier region 2 to that of the hard ceramic unit 1, Ei / Eu, ranges from 0.70 to 0.90.

[0070] The ratio of the hardness of the interface barrier region 2 to the hard ceramic unit 1, Hi / Hu, ranges from 0 to 0.50 to 0.70.

[0071] The fracture toughness of the interface barrier region 2 is between 1.5 and 2.5 times that of the ceramic unit 1.

[0072] Combination Figure 2 The hard ceramic unit 1 is square, rectangular, hexagonal or circular in shape, and is made of boron carbide ceramic, silicon carbide or other high-performance ceramic.

[0073] The thickness of the ceramic unit 1 ranges from 6 mm to 25 mm, and its length and width range from 30 mm to 130 mm.

[0074] Furthermore, the thickness of the interface barrier region 2 ranges from 0.5 mm to 2 mm, and it is prepared using SiC or... As the base, add Phase transformation toughening, SiCw whisker toughening, One or more composite materials in particle toughening form toughened multiphase ceramics.

[0075] Furthermore, the preparation process of the hard ceramic unit 1 includes:

[0076] High-density hard ceramic unit 1 was obtained by mixing, ball milling, molding, and first sintering according to the preset formula;

[0077] The first sintering is densification sintering, which adopts any one of hot pressing sintering, pressureless sintering, and reaction sintering to obtain a hard ceramic unit 1 with a density ≥ 97%, Vickers hardness ≥ 28 GPa, and bending strength ≥ 400 MPa. Its function is to undertake the main anti-penetration function, break the core of the projectile, and dissipate kinetic energy.

[0078] The hard ceramic unit 1 is subjected to micro-roughening treatment through one or more of the following methods: sandblasting, laser etching, and acid etching, to form a dual reinforcement of mechanical interlocking and sintering.

[0079] The hard ceramic units 1 are arranged in an array as required and fixed in a special graphite mold with uniform gaps reserved.

[0080] Ceramic powder in interface barrier zone 2 is uniformly filled into the gap. The filling is achieved by dry filling, vibration compaction, and light cold pressing to ensure dense filling without voids or bridging, forming a continuous grid-like interface barrier zone 2. This achieves forced prevention of crack propagation and confines the damage to a single hard ceramic unit 1.

[0081] The filled interface barrier region 2 and the hard ceramic unit 1 are sintered a second time to make the powder of the interface barrier region 2 sintered dense and form a strong sintered bond with the hard ceramic unit 1, thus obtaining an integrated high-performance ceramic plate.

[0082] In addition, the temperature of the second sintering is 100~200℃ lower than that of the first sintering to ensure that the hard ceramic unit 1 does not soften, deform, recrystallize, or have a coarse reaction layer.

[0083] The ceramic unit 1 has a different material system, sintering regime, and toughness gradient matching with the barrier region, and has no obvious gaps or weak bonding surfaces.

[0084] The second sintering process employs hot pressing and static isobaric methods to compensate for shrinkage stress and achieve defect-free metallurgical bonding in the interface barrier zone 2.

[0085] After the integrated high-performance ceramic plate is prepared, it undergoes surface grinding, chamfering, and surface sealing.

[0086] On the other hand, the present invention also provides the above-mentioned high-performance ceramic composite protective structure method, including a crack-arresting layer a, a high-performance ceramic plate layer c, and a fiber composite material layer e arranged in sequence.

[0087] The crack-arresting layer has a surface density of 80~140 g / cm³. 3 Woven fabrics made of aramid II or aramid III;

[0088] The fiber composite material layer is composed of one or more high-performance fibers, such as aramid fiber UD composite material, ultra-high molecular weight polyethylene UD composite material, carbon fiber UD composite material, and PBO fiber composite material.

[0089] The crack-resistant layer a, the high-performance ceramic plate layer c, and the fiber composite material layer e are connected by adhesive films (b and d).

[0090] Combination Figure 3 This solution also provides a method for preparing the above-mentioned high-performance ceramic composite protective structure, wherein the crack-arresting layer a, the adhesive film b, the high-performance ceramic plate layer c, the adhesive film d, and the fiber composite material layer e are stacked in sequence and the whole is subjected to hot pressing treatment to obtain the high-performance ceramic composite protective structure.

[0091] The hot pressing process is carried out in an autoclave according to the following steps:

[0092] (1) Raise the temperature from room temperature to 60±3℃, pressurize to 0KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 15 minutes;

[0093] (2) Increase the temperature from 60±3℃ to 120±3℃, pressurize to 1000KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 45 minutes;

[0094] (3) Maintain 120±3℃, maintain pressure of 1000KPa, maintain vacuum value of -0.1~-0.09MPa, and keep warm for 60 minutes;

[0095] (4) Cool down to room temperature, maintain pressure of 1000 kPa, vacuum value of -0.1 to -0.09 MPa, and keep warm for 10 minutes;

[0096] (5) Maintain room temperature, reduce pressure to 0 kPa, keep vacuum value at -0.1~-0.09 MPa, and keep warm for 20 minutes.

[0097] As shown in Table 1: Table 1

[0098] The high-performance ceramic plate and corresponding composite protective structure prepared by the method of this solution with pre-fabricated crack barrier structure can eliminate interfacial microcracks, pores, shrinkage mismatch, and debonding by designing the formulation and sintering method of the hard ceramic unit 1 and the interface barrier zone 2, as well as matching the performance parameters between the two. It can prevent the barrier zone from becoming a weak penetration channel. The interface barrier zone formed is tough but not weak, the hardness does not drop sharply, and there is no through-through failure. It achieves "tough but not weak, hard but not brittle". It can limit impact damage to a single unit, prevent crack propagation and penetration, and improve the ability to resist multiple impacts.

[0099] The embodiments described above are merely one implementation method of this application, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of the invention patent. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.

Claims

1. A high-performance ceramic plate with a pre-fabricated crack-barrier structure, characterized in that, Includes hard ceramic units and interface barrier regions; The hard ceramic unit is formed into a high-density, high-hardness ceramic through a first sintering process. The interface barrier region is set in the gap between multiple hard ceramic units and is formed through a second sintering process, forming a dense whole with the hard ceramic unit through metallurgical / sintering bonding. The hard ceramic units and interface barrier regions are formulated with different formulations and sintering methods to create gradient differences in mechanical properties; The difference in wave impedance between the hard ceramic unit and the interface barrier region leads to a reduction in the stress transmission intensity between the ceramic units. The interface barrier region forms a grid-like crack barrier system to cut off the propagation of cracks caused by impact.

2. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 1, characterized in that, A gradient match of "high hardness - high toughness" and "high modulus - low modulus" is formed between the hard ceramic unit and the interface barrier region: The ratio of the elastic modulus of the interface barrier region to the elastic modulus of the hard ceramic unit, Ei / Eu, ranges from 0.70 to 0.

90. The ratio of the hardness of the interface barrier region to the hardness of the hard ceramic unit, Hi / Hu, ranges from 0.50 to 0.

70. The fracture toughness of the interface barrier region is between 1.5 and 2.5 times that of the ceramic unit.

3. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 1, characterized in that, The hard ceramic unit is square, rectangular, regular hexagonal or circular in shape, and is made of boron carbide ceramic, silicon carbide or other high-performance ceramics. The thickness of the ceramic unit ranges from 6 mm to 25 mm, and the length and width range from 30 mm to 130 mm.

4. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 1, characterized in that, The thickness of the interface barrier region ranges from 0.5 mm to 2 mm, and it is prepared using SiC or... As the base, add Phase transformation toughening, SiCw whisker toughening, One or more composite materials in particle toughening form toughened multiphase ceramics.

5. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 1, characterized in that, The fabrication process of the hard ceramic unit includes: High-density hard ceramic units are obtained by mixing, ball milling, molding, and first sintering according to a preset formula; The first sintering is densification sintering, which adopts any one of hot pressing sintering, pressureless sintering, and reaction sintering to obtain hard ceramic units with a density ≥ 97%, Vickers hardness ≥ 28 GPa, and flexural strength ≥ 400 MPa. The hard ceramic unit is subjected to micro-roughening treatment through one or more of the following methods: sandblasting, laser etching, and acid etching, to form a dual reinforcement of mechanical interlocking and sintering.

6. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 4, characterized in that, The hard ceramic units are arranged in an array as required and fixed in a special graphite mold with uniform gaps reserved. Ceramic powder from the interface barrier zone is evenly filled into the gap. The filling is achieved through dry filling, vibration compaction, and light cold pressing to ensure dense filling without voids or bridging, forming a continuous grid-like interface barrier zone. This effectively prevents crack propagation and confines the damage to a single hard ceramic unit. The filled interface barrier region and hard ceramic unit are sintered a second time to make the powder in the interface barrier region dense and form a strong sintered bond with the hard ceramic unit, thus obtaining an integrated high-performance ceramic plate.

7. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 6, characterized in that, The second sintering temperature is 100-200°C lower than the first sintering temperature to ensure that the hard ceramic unit does not soften, deform, recrystallize, or have a coarse reaction layer. The ceramic unit and the barrier region have different material systems, different sintering regimes, and matched toughness gradients, with no obvious gaps or weak bonding surfaces. The second sintering process employs hot pressing and static isobaric methods to compensate for shrinkage stress and achieve defect-free metallurgical bonding in the interface barrier zone.

8. The high-performance ceramic plate with a pre-fabricated crack barrier structure according to claim 6, characterized in that, After the integrated high-performance ceramic plate is prepared, it undergoes surface grinding, chamfering, and surface sealing.

9. The high-performance ceramic composite protective structure of the high-performance ceramic plate according to any one of claims 1-8, characterized in that, It includes a crack-arresting layer, a high-performance ceramic plate layer, and a fiber composite material layer arranged in sequence; The crack-arresting layer has a surface density of 80~140 g / cm³. 3 woven fabrics of aramid II or aramid III; The fiber composite material layer is composed of one or more high-performance fibers, such as aramid fiber UD composite material, ultra-high molecular weight polyethylene UD composite material, carbon fiber UD composite material, and PBO fiber composite material. The crack-resistant layer, the high-performance ceramic plate layer, and the fiber composite material layer are connected by an adhesive film.

10. The method for preparing the high-performance ceramic composite protective structure according to claim 9, characterized in that, The crack-arresting layer, adhesive film, high-performance ceramic plate layer, adhesive film, and fiber composite material layer are stacked in sequence and then hot-pressed as a whole to obtain a high-performance ceramic composite protective structure. The hot pressing process is carried out in an autoclave according to the following steps: (1) Raise the temperature from room temperature to 60±3℃, pressurize to 0KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 15 minutes; (2) Increase the temperature from 60±3℃ to 120±3℃, pressurize to 1000KPa, set the vacuum value to -0.1~-0.09MPa, and keep warm for 45 minutes; (3) Maintain 120±3℃, maintain pressure of 1000KPa, maintain vacuum value of -0.1~-0.09MPa, and keep warm for 60 minutes; (4) Cool down to room temperature, maintain pressure of 1000 kPa, vacuum value of -0.1 to -0.09 MPa, and keep warm for 10 minutes; (5) Maintain room temperature, reduce pressure to 0 kPa, keep vacuum value at -0.1~-0.09 MPa, and keep warm for 20 minutes.