An online detection method for polymerization inhibitors in styrene polymerization.

By combining ultraviolet spectroscopy and electrochemical detection, the problem of accurate measurement of inhibitor concentration in styrene polymerization has been solved, enabling real-time, online, and high-precision detection of inhibitor concentration, thus ensuring the safety and stability of the polymerization reaction.

CN123111997APending Publication Date: 2026-11-17JIANGSU TAIHU CHEM
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611368772.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-04
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In existing technologies, online detection methods for polymerization inhibitors in styrene polymerization reactions suffer from spectral interference and electrochemical drift, resulting in inaccurate concentration measurements and an inability to achieve high-precision real-time tracking.

Method used

By combining ultraviolet spectroscopy and electrochemical detection in a synergistic analysis method, the concentration of polymerization inhibitors can be accurately measured online in real time by extracting the fluctuation characteristics of ultraviolet absorbance and the acceleration of electrochemical potential changes.

Benefits of technology

It effectively suppresses spectral interference and electrochemical drift, enabling continuous, online, and high-precision detection of polymerization inhibitor concentration, reducing detection lag and deviation, and ensuring the safe and controllable polymerization reaction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123111997A_ABST
    Figure CN123111997A_ABST
Patent Text Reader

Abstract

This invention discloses an online detection method for polymerization inhibitors in styrene polymerization, belonging to the field of online polymerization inhibitor detection technology. The method acquires the ultraviolet absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths, generates an absorbance fluctuation vector, and extracts the fluctuation amplitude ratio of extreme points as a fluctuation characteristic parameter. The initial effective concentration is determined by querying a polymerization inhibitor concentration mapping table using the fluctuation characteristic parameter. When the initial effective concentration exceeds a threshold, an electrochemical detection probe is activated to acquire a redox potential sequence. The second-order difference of three consecutive potential values ​​is calculated to obtain the potential change acceleration. This acceleration is then weighted and fused with the initial effective concentration to obtain a concentration correction coefficient, which is used to correct the real-time effective concentration. This scheme can effectively eliminate background interference and sensitively capture changes in polymerization inhibitor activity, improving the accuracy of online detection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of online detection technology for polymerization inhibitors, specifically to an online detection method for polymerization inhibitors in styrene polymerization. Background Technology

[0002] In the polymerization of styrene, the concentration of the polymerization inhibitor directly affects the length of the polymerization induction period and the stability of the reaction. Online monitoring of this inhibitor is crucial for ensuring the safety and controllability of the polymerization process. Current technologies primarily employ a single ultraviolet (UV) spectroscopy method for online inhibitor monitoring, estimating the concentration by monitoring changes in absorbance at characteristic wavelengths. While this method meets basic measurement needs when the solution composition is relatively simple, it becomes problematic when styrene monomer, solvent, and trace impurities coexist in the polymerization system. The spectral absorptions of each component overlap, resulting in absorbance data containing numerous fluctuations unrelated to the inhibitor concentration, failing to accurately reflect the true changes in the effective inhibitor concentration. Furthermore, UV spectroscopy is insensitive to active state transitions caused by oxidation or complexation of the inhibitor, making it difficult to distinguish the differences in contribution of the effective and ineffective components to the spectral signal. This leads to significant lag and bias in concentration results derived solely from absorbance analysis.

[0003] Existing technologies also attempt to incorporate electrochemical methods to assess the activity of polymerization inhibitors by detecting the redox potential of the solution. However, electrochemical signals are easily affected by electrode surface contamination, fluctuations in solution ionic strength, and temperature drift during continuous monitoring, causing slow shifts in potential measurements. Using electrochemical detection alone makes it difficult to obtain a stable concentration conversion benchmark. More importantly, at low concentrations or when activity changes are gradual, the response sensitivity of electrochemical probes is insufficient to reflect the subtle degradation of the inhibitor's effectiveness in the early stages, thus preventing the achievement of high-precision online measurement throughout the entire process.

[0004] To address the aforementioned issues, a method is needed that can extract the essential characteristics of concentration changes from complex ultraviolet spectral signals, and then use electrochemical dynamic information to instantly correct the concentration results after the activity of the polymerization inhibitor enters the scope of interest. This would solve the problem that existing single detection methods have weak anti-interference capabilities and cannot accurately track the dynamic evolution of the effective concentration of the polymerization inhibitor. Summary of the Invention

[0005] This invention provides an online detection method for polymerization inhibitors in styrene polymerization. The method achieves stable acquisition of the initial effective concentration of the polymerization inhibitor by extracting the fluctuation characteristic parameters of ultraviolet spectral absorbance, and dynamically corrects the initial concentration by combining the acceleration of electrochemical potential change to obtain the real-time effective concentration, thereby overcoming the influence of spectral interference and electrochemical drift on the measurement accuracy.

[0006] To achieve the above objectives, the present invention provides the following technical solution: The present invention provides an online detection method for polymerization inhibitors in styrene polymerization, which achieves real-time online accurate determination of the polymerization inhibitor concentration through synergistic analysis of ultraviolet spectroscopy and electrochemical detection. The method includes the following steps: The ultraviolet (UV) absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths during the styrene polymerization reaction is obtained. Preferably, the UV spectrometer is controlled to continuously collect transmittance data of the polymerization inhibitor solution at wavelengths of 250 nm, 280 nm, and 310 nm according to a preset sampling period. The transmittance data are converted into absorbance values ​​at the corresponding wavelengths, and the UV absorbance sequence is constructed after aligning the data according to the sampling time. This method utilizes multi-wavelength absorbance information to sensitively capture subtle changes in the polymerization inhibitor caused by consumption or decomposition, providing a rich data foundation for subsequent dynamic feature extraction.

[0007] An absorbance fluctuation vector is generated based on the absorbance difference between adjacent sampling times in the ultraviolet spectral absorbance sequence. Specifically, absorbance values ​​between adjacent sampling times are extracted from the ultraviolet spectral absorbance sequence, the difference between the absorbance value at the next time moment and the absorbance value at the previous time moment is calculated, and these differences are arranged in chronological order to form the absorbance fluctuation vector. This fluctuation vector can highlight the dynamic behavior of absorbance changing over time, amplify the fluctuation signal of the effective concentration of the polymerization inhibitor, and suppress steady-state noise such as baseline drift.

[0008] The extreme points in the absorbance fluctuation vector are extracted, and the fluctuation amplitude ratio corresponding to the extreme points is calculated to obtain the fluctuation characteristic parameter. As a technical solution of this invention, each element in the absorbance fluctuation vector is traversed, and elements with values ​​greater than the two adjacent element values ​​are marked as maxima, and elements with values ​​less than the two adjacent element values ​​are marked as minima. The absolute value of the difference between the element values ​​of adjacent maxima and minima is calculated as the fluctuation amplitude value. The current fluctuation amplitude value is then divided by the previous fluctuation amplitude value to obtain the fluctuation amplitude ratio. This fluctuation characteristic parameter has a stable correlation with the inhibitor concentration, can reflect the activity decay trend of the inhibitor, and is insensitive to interference from other light-absorbing impurities in the solution system.

[0009] Using the aforementioned fluctuation characteristic parameters as an index, a pre-defined inhibitor concentration mapping table is consulted to determine the initial effective concentration of the inhibitor solution. Preferably, the inhibitor concentration mapping table is established by pre-collecting ultraviolet spectra of standard solutions of inhibitors with different known concentrations under the same conditions and extracting fluctuation characteristic parameters. The fluctuation characteristic parameters are matched with the standard fluctuation characteristic parameter intervals in the inhibitor concentration mapping table to determine the target standard fluctuation characteristic parameter interval to which they belong, and the standard concentration value corresponding to this interval is read as the initial effective concentration. This table lookup method quickly provides a preliminary estimate of the inhibitor concentration, avoiding the need for online solutions to complex models and meeting the response speed requirements of industrial polymerization reactions.

[0010] When the initial effective concentration exceeds a preset threshold, the electrochemical detection probe is activated to acquire the redox potential sequence of the polymerization inhibitor solution. When the initial effective concentration is low, it indicates that a large amount of polymerization inhibitor has been consumed, and UV spectroscopy alone may not provide sufficient resolution. In this case, electrochemical detection is introduced, and detection resources are rationally allocated by comparing the activation conditions. Specifically, the initial effective concentration is compared with the preset threshold. If the initial effective concentration is greater than the preset threshold, it indicates that there is still sufficient polymer inhibitor remaining. At this time, an activation command is sent to the electrochemical detection probe, which continuously acquires redox potential data according to a preset sampling period and generates a redox potential sequence in chronological order. The redox potential responds significantly to changes in the electrochemical activity of trace amounts of polymerization inhibitor, effectively compensating for the detection limitations of UV spectroscopy in the low concentration range.

[0011] The second-order difference of three consecutive potential values ​​in the redox potential sequence is calculated to obtain the potential change acceleration. Preferably, a first potential value E1, a second potential value E2, and a third potential value E3 are extracted from the redox potential sequence, and a first-order forward difference Δ1 = E2 - E1 and a first-order backward difference Δ2 = E3 - E2 are calculated. The second-order difference a = Δ2 - Δ1 is then calculated; this second-order difference characterizes the potential change acceleration. The potential change acceleration is directly related to the change in the electrochemical reaction rate of the polymerization inhibitor, enabling timely detection of inflection points in the inhibitor concentration and enhancing the sensitivity to abnormal concentration fluctuations.

[0012] The potential change acceleration is weighted and fused with the initial effective concentration to obtain a concentration correction coefficient. Preferably, the second-order difference 'a' is multiplied by a preset acceleration weighting factor 'α' to obtain the acceleration contribution value, and the initial effective concentration C0 is multiplied by a preset concentration weighting factor 'β' to obtain the concentration contribution value. The two are then added together to obtain the concentration correction coefficient k = α·a + β·C0. This fusion method organically integrates the overall concentration level obtained from ultraviolet spectroscopy with the instantaneous dynamic changes obtained from electrochemical detection, enabling the correction coefficient to reflect both the current concentration level and rapid changes during the reaction process, thus improving the accuracy and timeliness of the correction coefficient.

[0013] The initial effective concentration is corrected using the concentration correction coefficient to obtain the real-time effective concentration of the polymerization inhibitor solution. In a preferred embodiment of the invention, it is determined whether the value of the concentration correction coefficient k is greater than zero and less than or equal to two. If k is within this range, the initial effective concentration is multiplied by k to obtain the real-time effective concentration C = k·C0. If k is less than or equal to zero or greater than two, k is set to one, and the initial effective concentration is used as the real-time effective concentration to avoid over-correction due to abnormal fluctuations. This correction process uses electrochemical dynamic information to correct the static estimation of the ultraviolet spectrum, effectively suppressing the measurement deviation caused by temperature, pressure, and byproduct interference in the polymerization system to a single detection method. The output result truly reflects the actual effective content of the polymerization inhibitor at the current moment.

[0014] The above method sequentially extracts the absorbance fluctuation characteristics of ultraviolet spectra, performs initial concentration mapping, triggers electrochemical linkage, and performs weighted fusion correction. It achieves continuous, online, and high-precision detection of the concentration of polymerization inhibitor in styrene polymerization. The detection process does not require interruption of the reaction or offline sampling. It is simple to operate and has important guiding significance for the control of polymerization inhibitor addition and the safe operation of polymerization reaction.

[0015] The technical effects and advantages provided by the present invention in the above technical solution are as follows: An absorbance fluctuation vector is generated by analyzing the difference between adjacent sampling times in the UV absorbance sequence. The extreme points in this vector are then extracted to calculate the fluctuation amplitude ratio, which is used as a fluctuation characteristic parameter to look up the inhibitor concentration mapping table. This approach abandons the traditional method of directly using raw absorbance values ​​for calculation, instead focusing on the structural fluctuation information during absorbance changes. The spectral overlap of coexisting components in the inhibitor solution often forms relatively smooth and irregular baseline fluctuations. However, when the inhibitor concentration changes, the absorbance exhibits rhythmic transient increases and decreases at the corresponding wavelengths. This rhythm manifests as a continuous sequence of extreme values ​​in the fluctuation vector. Using the fluctuation amplitude ratio between extreme points as a characteristic parameter amplifies the unique dynamic profile of inhibitor concentration fluctuations while suppressing steady-state shifts and random noise caused by blending components. The resulting fluctuation characteristic parameter has a clearer correspondence with the actual effective concentration of the inhibitor. The initial effective concentration obtained from the table is less likely to be obscured by background interference, maintaining high concentration output stability even under complex spectral environments in the polymerization system.

[0016] When the initial effective concentration exceeds a preset threshold, the electrochemical detection probe is activated to acquire a redox potential sequence, and the second-order difference of three consecutive potential values ​​is calculated to obtain the potential change acceleration. When the activity of the polymerization inhibitor changes, its ability to participate in the electrode reaction will change accordingly. This change is not a slow drift, but rather manifested as a difference in the rate of potential change. The second-order difference operation is equivalent to extracting the acceleration information of the potential change, which is extremely sensitive to the local bending trend of the potential signal and can promptly capture the subtle transition of electrochemical activity during the transition of the polymerization inhibitor from the effective state to the inert state. Even if there is a slow baseline drift in the electrode itself, the second-order difference will filter it out because a slow linear drift will not produce a significant acceleration. By weighted and fused with the initial effective concentration, the accelerated activity change information is directly applied to the concentration correction coefficient, and the initial effective concentration is then corrected by the concentration correction coefficient. This is equivalent to giving the concentration benchmark provided by the ultraviolet spectroscopy an electrochemical dynamic sensitivity. The entire calibration process does not preset a fixed compensation amount, but rather adjusts adaptively based on the intensity of the activity change reflected by the potential acceleration at the current moment. This ensures that the final output real-time effective concentration can closely follow the actual effectiveness decay process of the polymerization inhibitor in the polymerization reaction system, reducing the process control delay caused by detection lag. Attached Figure Description

[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in this invention. For those skilled in the art, other drawings can be obtained based on these drawings.

[0018] Figure 1 This is a flowchart of the online detection method for polymerization inhibitors in styrene polymerization. Figure 2 This is a flowchart of a method for detecting the initial effective concentration of polymerization inhibitors based on the characteristic parameters of ultraviolet spectral absorbance fluctuations. Figure 3 This is a flowchart of the process for monitoring the concentration of polymerization inhibitors and collecting electrochemical oxidation-reduction potentials. Figure 4 The absorbance curves of the polymerization inhibitor solution at wavelengths of 250 nm, 280 nm, and 310 nm during the polymerization of styrene are shown. Figure 5 This is a curve showing the change in redox potential of the polymerization inhibitor solution over sampling time; Figure 6 It is the acceleration curve of the potential change in the redox potential sequence; Figure 7 It is a curve showing the real-time effective concentration change of the polymerization inhibitor solution and the preset warning value. Detailed Implementation

[0019] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0020] See Figure 1 This invention provides an online detection method for polymerization inhibitors in styrene polymerization. The method includes: acquiring the ultraviolet absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths during the styrene polymerization reaction; generating an absorbance fluctuation vector based on the absorbance difference between adjacent sampling times in the ultraviolet absorbance sequence; extracting the extreme points in the absorbance fluctuation vector and calculating the fluctuation amplitude ratio corresponding to the extreme points to obtain fluctuation characteristic parameters; using the fluctuation characteristic parameters as an index to query a preset polymerization inhibitor concentration mapping table to determine the initial effective concentration of the polymerization inhibitor solution; under the condition that the initial effective concentration exceeds a preset threshold, activating an electrochemical detection probe to acquire the redox potential sequence of the polymerization inhibitor solution; calculating the second difference of three consecutive potential values ​​in the redox potential sequence to obtain the potential change acceleration; weighting and fusing the potential change acceleration with the initial effective concentration to obtain a concentration correction coefficient; and using the concentration correction coefficient to correct the initial effective concentration to obtain the real-time effective concentration of the polymerization inhibitor solution.

[0021] In specific implementation, the ultraviolet absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths during the styrene polymerization reaction is obtained, including controlling the ultraviolet spectrometer to continuously collect transmittance data of the polymerization inhibitor solution at wavelengths of 250nm, 280nm and 310nm according to a preset sampling period.

[0022] The ultraviolet spectrometer uses a deuterium lamp as its light source. The optical path passes through a flow cell. The polymerization inhibitor solution continuously flows into the flow cell from the sampling pipeline of the styrene polymerization reactor. After passing the detection site, it returns to the reactor or is discharged into a waste liquid collection device, ensuring a continuous renewal of the polymerization inhibitor solution in the flow cell. This allows the collected transmittance data to reflect the real-time optical characteristics of the polymerization inhibitor solution. The preset sampling period is set according to the consumption rate of the polymerization inhibitor in the styrene polymerization reaction, and the sampling period ranges from 5 seconds to 60 seconds. In some embodiments, the preset sampling period is set to 30 seconds, ensuring that the change in the polymerization inhibitor concentration between two adjacent acquisitions does not exceed 2% of the initial effective concentration. This guarantees that the ultraviolet spectral absorbance sequence can completely record the spectral change trend of the polymerization inhibitor as it is consumed during the reaction process. The ultraviolet spectrometer is connected to the industrial control computer via a data acquisition card. The acquisition software running in the industrial control computer sends a trigger signal to the ultraviolet spectrometer according to a preset sampling period. After receiving the trigger signal, the ultraviolet spectrometer simultaneously measures the transmittance data of the polymerization inhibitor solution at three wavelengths: 250 nm, 280 nm, and 310 nm. The selection of the three wavelengths is based on the characteristic absorption peak positions of the benzene ring and conjugated double bonds in the molecular structure of the polymerization inhibitor.

[0023] In practice, transmittance data is converted into absorbance values ​​at 250nm, 280nm, and 310nm, respectively. Transmittance data is recorded as a percentage, representing the ratio of transmitted light intensity to incident light intensity multiplied by 100%. The formula used to convert transmittance data to absorbance values ​​is:

[0024] in, This represents the absorbance value, which is dimensionless. The transmittance is the decimal value of the transmittance divided by 100, ranging from 0 to 1. When the transmittance is 100%, The value is 1, when the light transmittance is 0%. The value is 0.

[0025] After acquiring transmittance data each time, the acquisition software divides the transmittance data corresponding to the 250nm wavelength by 100 to obtain the 250nm transmittance ratio, and then substitutes this 250nm transmittance ratio into the above formula to calculate the 250nm absorbance value. Similarly, it divides the transmittance data corresponding to the 280nm wavelength by 100 to obtain the 280nm transmittance ratio, and then substitutes this 280nm transmittance ratio into the above formula to calculate the 280nm absorbance value. The transmittance data corresponding to the 310nm wavelength is divided by 100 to obtain the 310nm transmittance ratio, and then substitutes this 310nm transmittance ratio into the above formula to calculate the 310nm absorbance value. The absorbance values ​​at the three wavelengths are converted within one acquisition cycle, and the conversion results are stored in the data cache area of ​​the industrial control computer's memory. Each record contains a timestamp of the sampling time and the three absorbance values.

[0026] In practice, the absorbance values ​​at 250nm, 280nm, and 310nm are aligned according to the sampling time to construct a UV spectral absorbance sequence. The acquisition software uses the sampling time as an index to group the 250nm, 280nm, and 310nm absorbance values ​​obtained within the same acquisition cycle into a data triplet. All data triplets are arranged in chronological order to form the UV spectral absorbance sequence. The i-th data triplet in the UV spectral absorbance sequence is denoted as... , This represents the absorbance value at 250 nm at the i-th sampling time. This represents the absorbance value at 280 nm at the i-th sampling time. This represents the absorbance value at 310 nm at the i-th sampling time, where i is a positive integer sampling number starting from 1. The UV absorbance sequence is stored in the industrial control computer's memory using an array structure, supporting random access by sampling number or sampling time. The sequence length dynamically expands as the reaction time increases. Acquisition is terminated and the complete sequence is saved when the styrene polymerization reaction ends.

[0027] See Figure 4 In the graph, the horizontal axis represents the sampling time in minutes, ranging from 0 to 300 minutes, and the vertical axis represents the absorbance value (dimensionless). The legend indicates that the three curves correspond to the absorbance changes of the polymerization inhibitor solution at wavelengths of 250 nm, 280 nm, and 310 nm, respectively.

[0028] The trends of the three absorbance curves all show a gradual decrease with increasing sampling time, reflecting the continuous consumption of the inhibitor solution concentration during the styrene polymerization reaction. Specifically, the absorbance value at 280 nm is the highest, with an initial absorbance close to 1.4; the initial absorbance at 250 nm is approximately 0.95; and the absorbance at 310 nm is the lowest, with an initial value of approximately 0.7. The order of the initial absorbance values ​​is related to the characteristic absorption peaks of the benzene ring and conjugated double bonds in the inhibitor molecule.

[0029] During the first 150 minutes of sampling, all three curves showed a relatively flat and gradual downward trend, indicating that the concentration of the polymerization inhibitor decreased slowly and uniformly. After 150 minutes, the rate of decrease in absorbance value accelerated, especially the decrease in the 280nm absorbance curve, which gradually approached the absorbance levels of the 250nm and 310nm wavelengths, reflecting the changes in the optical properties of the polymerization inhibitor as the reaction progressed.

[0030] In specific implementation, please refer to Figure 2The absorbance values ​​at adjacent sampling times are extracted from the ultraviolet (UV) absorbance sequence. The difference between the absorbance values ​​at the next sampling time and the absorbance values ​​at the previous sampling time is calculated as the absorbance difference between adjacent sampling times. The UV absorbance sequence contains triplets arranged according to sampling time. Processing is performed separately for the 250nm, 280nm, and 310nm absorbance value sequences. Taking the 250nm absorbance value sequence as an example, let the 250nm absorbance value sequence be... ,in This represents the total number of sampling points in the sequence. For the sampling sequence number... From 1 to Calculate the first The absorbance value at 250nm at the first sampling time minus the absorbance value at the second sampling time. The absorbance value at 250 nm at the sampling time is obtained to obtain the first... The difference in absorbance at 250 nm between adjacent sampling times ,Right now The 280nm absorbance value sequence and the 310nm absorbance value sequence were processed in the same way to obtain the 280nm absorbance difference sequence and the 310nm absorbance difference sequence, respectively.

[0031] In practice, the absorbance differences between adjacent sampling times are arranged chronologically to generate an absorbance fluctuation vector. The same sampling sequence number is then used... The corresponding absorbance differences at 250nm, 280nm, and 310nm are combined into a triplet of differences, represented as follows: According to the sampling sequence number Arrange all difference triplets in ascending order to generate an absorbance fluctuation vector. The absorbance fluctuation vector is a vector of length [missing value]. The sequence, where the first... Each element records the absorbance difference across three wavelengths, reflecting the amplitude and direction of absorbance fluctuations in the inhibitor solution within adjacent sampling intervals.

[0032] In practice, each element in the absorbance fluctuation vector is traversed, and elements with values ​​greater than their two adjacent values ​​are marked as maxima, while elements with values ​​less than their two adjacent values ​​are marked as minima. Since the absorbance fluctuation vector contains difference information for three wavelengths, the marking of extrema is performed separately for the absorbance difference sequence at each wavelength. For the 250nm absorbance difference sequence, starting from the second element to the... After each element is counted, the value of each element is compared with the values ​​of its preceding and following elements. If the condition is met... and Then This is marked as a maximum point in the 250nm absorbance difference sequence. If it satisfies... and Then This is marked as a minimum point in the 250nm absorbance difference sequence. For the first and last elements of the absorbance fluctuation vector, compare only with one existing adjacent element: if... Then Marked as a maximum point; if Then Mark the point as the minimum; for the last element ,like If, then mark it as a maximum point; if If the value is within a certain range, it is marked as a minimum point. The same rules are applied to the 280nm absorbance difference sequence and the 310nm absorbance difference sequence to obtain the set of extreme points for each wavelength.

[0033] In practice, the absolute value of the difference between the element values ​​of adjacent maxima and minima is calculated as the fluctuation amplitude. For the absorbance difference sequence at each wavelength, the marked extreme points are extracted in chronological order, with the types of extreme points alternating. Taking the 250nm absorbance difference sequence as an example, let the marked extreme points in chronological order be... ,in Let be the total number of extreme points. Starting from the first extreme point, group adjacent extreme points into groups, each group containing one maximum and one minimum. Calculate the absolute value of the difference between the element values ​​of the two extreme points in each group to obtain the fluctuation range. Let be the th extreme point. Group fluctuation amplitude value , Values ​​range from 1 to The integer. If the total number of extreme points is an integer. If the number is odd, the last extreme point is not included in the fluctuation amplitude calculation. The same operation is performed on the 280nm absorbance difference sequence and the 310nm absorbance difference sequence to obtain their respective fluctuation amplitude value sequences.

[0034] In practice, the fluctuation amplitude ratio is obtained by dividing the current fluctuation amplitude value by the previous fluctuation amplitude value. This is the fluctuation amplitude value sequence obtained from the 250nm absorbance difference sequence. ,in Starting from the second fluctuation amplitude value, calculate , obtained the The ratio of fluctuation amplitude, Values ​​range from 2 to The integer. The formula for calculating the fluctuation ratio is:

[0035] in, The first value in the 250nm absorbance difference sequence The ratio of fluctuation amplitudes is dimensionless. The first value in the 250nm absorbance difference sequence Each fluctuation range value; The first value in the 250nm absorbance difference sequence Each fluctuation range value; The value range is 1 to The integer, consisting of the total number of fluctuation amplitude values ​​in the 250nm absorbance difference sequence. Subtract 1 to confirm. Calculate the fluctuation amplitude ratios of the 280nm absorbance difference sequence and the 310nm absorbance difference sequence in the same way, and combine all the fluctuation amplitude ratios calculated at the three wavelengths into a set of fluctuation characteristic parameters. These fluctuation characteristic parameters reflect the decay rate of the UV spectral absorbance fluctuation amplitude during the consumption of the polymerization inhibitor.

[0036] In practice, the initial effective concentration of the polymerization inhibitor solution is determined by querying a pre-defined inhibitor concentration mapping table using the fluctuation characteristic parameters as an index. The inhibitor concentration mapping table is pre-stored in the industrial control computer's database and contains the correspondence between standard fluctuation characteristic parameter intervals and standard concentration values. The arithmetic mean of all fluctuation amplitude ratios in the fluctuation characteristic parameter set obtained in the above steps is calculated to obtain an average fluctuation amplitude ratio. This average fluctuation amplitude ratio is then matched one by one with the standard fluctuation characteristic parameter intervals in the inhibitor concentration mapping table. Each standard fluctuation characteristic parameter interval corresponds to a standard concentration value, and the interval is defined by a lower limit and an upper limit. If the average fluctuation amplitude ratio is greater than or equal to the lower limit of a standard fluctuation characteristic parameter interval and less than the upper limit of that interval, then the average fluctuation amplitude ratio is determined to belong to the target standard fluctuation characteristic parameter interval. The standard concentration value corresponding to the target standard fluctuation characteristic parameter interval is read as the initial effective concentration, with the unit of the initial effective concentration being milligrams per liter.

[0037] In practice, the inhibitor concentration mapping table is established by pre-collecting ultraviolet spectra of standard solutions of inhibitors with different known concentrations under the same conditions and extracting fluctuation characteristic parameters. The specific establishment process is as follows: Inhibitor standards are accurately weighed, and a series of standard solutions of inhibitors with known concentrations are prepared using styrene monomer or the same solvent as the reaction system. The concentration gradient covers the effective concentration range of the inhibitor in actual production; for example, 20 concentration points are uniformly selected from 10 mg / L to 500 mg / L. For each standard solution of inhibitor with known concentration, under the same temperature, optical path length, sampling period, and wavelength conditions, the ultraviolet absorbance sequence is obtained according to the aforementioned steps. An absorbance fluctuation vector is generated, extreme points are marked, and the fluctuation amplitude value and fluctuation amplitude ratio are calculated to obtain the set of fluctuation characteristic parameters corresponding to that concentration. The arithmetic mean of all fluctuation amplitude ratios in the set of fluctuation characteristic parameters corresponding to each known concentration is recorded as the standard fluctuation characteristic parameter. Repeat the above process multiple times for each known concentration, and obtain the statistical distribution of the standard fluctuation characteristic parameters to determine the standard fluctuation characteristic parameter interval for each standard concentration. The interval width is set to three times the standard deviation of the standard fluctuation characteristic parameter. Store the standard fluctuation characteristic parameter intervals and their corresponding standard concentration values ​​in a pair in the polymerization inhibitor concentration mapping table. The polymerization inhibitor concentration mapping table supports rapid indexing of the initial effective concentration through fluctuation characteristic parameters during online detection.

[0038] In specific implementation, please refer to Figure 3 The initial effective concentration is compared with a preset threshold, which is set according to the minimum concentration required for the inhibitor to effectively suppress polymerization. The inhibitor must maintain a minimum effective inhibition concentration in the styrene polymerization system. When the actual concentration is lower than this minimum effective inhibition concentration, the self-polymerization reaction of styrene monomers cannot be effectively suppressed, and the reaction system faces the risk of explosive polymerization. The specific value of the preset threshold is determined experimentally, ranging from 20 mg / L to 50 mg / L in different production processes. In some embodiments, the preset threshold is set to 30 mg / L. This setting is based on experimental data on the half-inhibition concentration of the inhibitor on the thermally initiated polymerization of styrene monomers at 100°C. At an inhibitor concentration of 30 mg / L, the polymerization induction period is extended to more than the designed safe duration. The industrial control computer reads the initial effective concentration value determined by ultraviolet spectroscopy from the storage unit and sends the initial effective concentration value and the preset threshold value to the value comparison module for comparison. If the initial effective concentration is less than or equal to the preset threshold, the industrial control computer determines that the inhibitor concentration is in the normal consumption stage, does not generate a start command, and the electrochemical detection probe remains in standby mode. If the initial effective concentration is greater than the preset threshold, the industrial control computer determines that the concentration of the polymerization inhibitor is too high and there may be spectral detection deviation caused by system disturbance, and generates a start command signal.

[0039] In practice, if the initial effective concentration is greater than a preset threshold, the industrial control computer sends a start command to the electrochemical detection probe. The digital output port of the industrial control computer generates a rising edge pulse signal with a pulse width of 100 milliseconds. The pulse signal is transmitted to the control interface of the electrochemical detection probe after passing through an opto-isolator. After receiving the start command, the electrochemical detection probe executes the power-on initialization sequence, connecting the constant potential circuit and the signal acquisition channels of the working electrode, reference electrode, and auxiliary electrode. The electrochemical detection probe adopts a three-electrode system, where the working electrode is a glassy carbon electrode, the reference electrode is a silver-silver chloride electrode, and the auxiliary electrode is a platinum wire electrode. After each start command, the working electrode first performs a surface cleaning procedure. The cleaning procedure includes cyclic voltammetry scanning of the working electrode surface using a 0.5 mol / L sulfuric acid solution, with a scanning potential range of -0.2V to 1.2V, a scanning rate of 100mV / s, and five consecutive scans. Afterward, the working electrode surface is rinsed with deionized water to maintain the working electrode's response sensitivity to the redox reaction of the polymerization inhibitor.

[0040] In specific implementation, the electrochemical detection probe continuously collects redox potential data of the polymerization inhibitor solution according to a preset sampling period. The preset sampling period is synchronized with the UV spectroscopy acquisition period, meaning that each sampling moment of the electrochemical detection probe coincides with each sampling moment of the UV spectrometer, and the trigger signals of both originate from the same clock reference. In some embodiments, the preset sampling period is maintained at 30 seconds, exactly the same as the sampling period of the UV spectrometer. At each sampling moment, the electrochemical detection probe records the open-circuit potential between the working electrode and the reference electrode. The open-circuit potential value is directly used as the redox potential data of the polymerization inhibitor solution, and the unit of recording the redox potential data is millivolts. After the polymerization inhibitor solution is drawn from the styrene polymerization reactor through the sampling pipeline, it first flows through the UV spectroscopy detection flow cell, and then flows into the measurement chamber of the electrochemical detection probe. The solution in the measurement chamber remains still for 15 seconds before the potential measurement is performed. After the measurement is completed, the measurement chamber is emptied and the polymerization inhibitor solution for the next time period is introduced, ensuring that the redox potential data collected each time reflects the state of the polymerization inhibitor solution at the corresponding moment.

[0041] In practice, redox potential (OP) data are arranged according to the sampling time sequence to generate an OP sequence. After receiving the OP data, the acquisition software combines the OP data with the timestamp of the current sampling time into a single record, which is then stored in the OP data buffer. The OP data are arranged into a one-dimensional sequence according to the ascending order of the timestamps. The redox potential data corresponding to each sampling time is denoted as . , This indicates the order of sampling times. Each redox potential value The sampling sequence number has a value from 1 to... positive integers, This represents the total number of data points collected in the redox potential sequence. The redox potential sequence is stored in the industrial control computer's memory as an array. The array index corresponds to the sampling number, and the array element value is the redox potential value at the corresponding sampling time, which is used for index retrieval when calculating the acceleration of potential change.

[0042] See Figure 5 The figure shows the trend of the redox potential of the polymerization inhibitor solution over time during the polymerization of styrene, with sampling time (in minutes) on the x-axis and redox potential (in millivolts, mV) on the y-axis. The curve represents the redox potential data of the polymerization inhibitor solution collected by the electrochemical detection probe in the above embodiment.

[0043] As shown in the figure, the redox potential initially starts at approximately 220 mV. With increasing sampling time, the potential exhibits a trend of first decreasing and then increasing. Specifically, it can be divided into three stages: In the initial stage (0 to approximately 150 minutes), the redox potential decreases slowly, from 220 mV to approximately 195 mV, indicating that the electrochemical activity of the polymerization inhibitor solution gradually decreases in the early stages of the reaction; in the intermediate stage (approximately 150 to 200 minutes), the potential reaches its lowest point of approximately 193 mV and then maintains a relatively stable low level, reflecting that the change in the polymerization inhibitor concentration tends to level off or reach a certain equilibrium state; in the final stage (200 to 300 minutes), the potential begins to rise, reaching nearly 201 mV by 300 minutes, indicating that the electrochemical properties of the polymerization inhibitor solution have recovered or changed, possibly suggesting fluctuations in the concentration or activity of the polymerization inhibitor.

[0044] The potential change curve is used to calculate the potential change acceleration. Combined with the initial effective concentration and acceleration weighting factor described in the previous embodiment, a weighted fusion is performed to obtain the concentration correction coefficient, enabling real-time correction of the polymerization inhibitor concentration. The obvious stage fluctuations and trend changes in the curve provide important dynamic information for the calculation of potential change acceleration, helping to accurately reflect the actual concentration state and changes of the polymerization inhibitor solution.

[0045] In practical implementation, continuous first, second, and third potential values ​​are extracted from the redox potential sequence. Redox potential sequence The samples have been stored in the industrial computer's memory in the order of their sampling time. Indicates the sampling sequence number is The redox potential value, This represents the total number of potential values ​​in the redox potential sequence. The data processing module within the industrial computer uses a sliding window with a fixed length of three consecutive potential values ​​and a sliding step size of 1. The data processing module then... Start sliding the window to extract the first... The first potential value is taken as the redox potential value and denoted as . Extract the first The first redox potential value is taken as the second potential value and denoted as . Extract the first The redox potential value is taken as the third potential value, denoted as . When the sliding window iterates to... At that time, the extraction of all three consecutive potential combinations in the redox potential sequence was completed, yielding a total of Group potential data.

[0046] In practice, the first difference value is obtained by subtracting the first potential value from the second potential value using the first-order forward difference. The calculation method is as follows:

[0047] in, This represents the first difference value, in millivolts. This represents the second potential value extracted by the current sliding window, in millivolts. This represents the first potential value extracted by the current sliding window, in millivolts. The first difference value reflects the change in redox potential from the first sampling time to the second sampling time.

[0048] In practice, the second difference value is obtained by subtracting the first-order backward difference of the second potential value from the third potential value. The calculation method is as follows:

[0049] in, This represents the second difference value, in millivolts. This represents the third potential value extracted by the current sliding window, in millivolts. This represents the second potential value extracted by the current sliding window, in millivolts. The second difference value reflects the change in redox potential from the second sampling time to the third sampling time.

[0050] In practice, the difference between the second difference value and the first difference value is calculated to obtain the second-order difference, which is the acceleration due to the change in electrical potential. The formula for calculating the acceleration due to the change in electrical potential is:

[0051] in, This represents the acceleration due to a change in electrical potential, measured in millivolts. This represents the second difference value, in millivolts. This represents the first difference value, in millivolts. The acceleration of the potential change reflects the direction and magnitude of the rate of change of the redox potential over three consecutive sampling times. A positive acceleration indicates an accelerating rate of change of the redox potential, while a negative acceleration indicates a decelerating rate of change. For each sliding window position in the redox potential sequence, a corresponding acceleration of the potential change is calculated. The potential change acceleration of the last window in the potential change acceleration calculated from all sliding windows of the redox potential sequence is taken as the representative value of the potential change acceleration participating in subsequent calculations.

[0052] In practice, the potential change acceleration is weighted and fused with the initial effective concentration to obtain a concentration correction coefficient. The representative value of the potential change acceleration is multiplied by a preset acceleration weighting factor to obtain the acceleration contribution value. The acceleration weighting factor is determined based on the sensitivity characteristics of the electrochemical detection probe and the electrochemical activity of the polymerization inhibitor. The acceleration weighting factor is obtained as follows: under laboratory conditions, the redox potential of a series of standard solutions of the polymerization inhibitor with known concentrations is collected using an electrochemical detection probe. The standard value of the potential change acceleration at each concentration is calculated, and a linear regression model is established between the potential change acceleration and the change in the polymerization inhibitor concentration. The slope of the linear regression model is dimensionless and used as the benchmark value of the acceleration weighting factor. In some embodiments, the acceleration weighting factor is set to 0.65. This value is determined based on calibration experimental data of the acceleration response to potential change caused by a 10 mg / L change in the concentration of the polymerization inhibitor in the styrene system. The calibration experiment shows that the sensitivity coefficient of the acceleration response to the concentration change is 0.65 mV-L / mg. After normalizing the sensitivity coefficient to the dimensionless acceleration weighting factor, the value of 0.65 is retained.

[0053] In practice, the initial effective concentration is multiplied by a preset concentration weighting factor to obtain the concentration contribution value. The concentration weighting factor is calibrated using a combination of UV spectroscopy and electrochemical response analysis of standard polymerization inhibitor solutions at multiple concentration gradients. The calibration method for the concentration weighting factor is as follows: multiple standard solutions covering the effective concentration range of the polymerization inhibitor are prepared, and the initial effective concentration of each standard solution is obtained using UV spectroscopy. Simultaneously, the redox potential data of each standard solution is obtained using electrochemical methods. Using the concentration value directly measured by the electrochemical method as a reference standard, a deviation distribution between the initial effective concentration of the UV spectroscopy method and the reference standard is established. The statistical mean of the ratio of the initial effective concentration of the UV spectroscopy method to the reference standard concentration is used as 1 minus the corresponding value of the concentration weighting factor, thus deriving the value of the concentration weighting factor. In some embodiments, the concentration weighting factor is set to 0.35. This value is determined based on the average deviation rate between the concentration detected by UV spectroscopy of 20 standard polymerization inhibitor solutions and the electrochemical reference concentration. The average deviation rate is 35%, indicating that the contribution of the concentration detected by UV spectroscopy alone accounts for 0.65% in the weighted fusion, and the contribution of electrochemical correction accounts for 0.35%.

[0054] In practice, the acceleration contribution value and the concentration contribution value are added together to obtain the concentration correction coefficient. The calculation method is as follows:

[0055] in, This represents the concentration correction factor, which is dimensionless. This represents the acceleration weighting factor, which is dimensionless and has a value of 0.65. This represents the representative value of the acceleration due to change in electrical potential, in millivolts. This represents the unit potential, with a value of 1 millivolt. This represents the concentration weighting factor, which is dimensionless and has a value of 0.35, with the unit being the reciprocal of millivolt-deciliters per milligram. Indicates the initial effective concentration, in milligrams per liter; This represents the unit concentration, with a value of 1 mg / L. The concentration correction factor integrates the potential dynamic change information obtained from electrochemical detection and the concentration reference information obtained from ultraviolet spectroscopy detection, and is used to correct the initial effective concentration.

[0056] See Figure 6 The figure shows the potential change acceleration curve calculated by the sliding window based on the redox potential sequence acquired by the electrochemical detection probe in one of the above embodiments. The horizontal axis represents the sliding window number, ranging from 0 to 600, representing the starting position index of three consecutive potential values ​​extracted sequentially; the vertical axis represents the potential change acceleration of the corresponding sliding window, in millivolts, with a value range of approximately -0.4 mV to 0.4 mV.

[0057] The curves generally fluctuate near zero, with the acceleration reflecting the rate of change of redox potential mostly maintaining small positive and negative fluctuations, indicating that the electrochemical state of the inhibitor solution is relatively stable. At certain points in the sliding window, significant peaks appear in the potential change acceleration, with the maximum peak value approaching 0.39 mV and the minimum valley value approximately -0.4 mV. These abrupt changes may correspond to instantaneous acceleration or deceleration of the redox reaction in the inhibitor solution, reflecting transient changes in the inhibitor concentration or electrochemical activity.

[0058] In practice, it is determined whether the concentration correction factor is greater than zero and less than or equal to two. The industrial control computer's data processing module calculates the concentration correction factor. Then, the concentration correction factor The numerical value is sent to the numerical range determination unit. The numerical range determination unit internally stores two boundary values: a lower boundary value of zero and an upper boundary value of two. The numerical range determination unit then inputs the concentration correction coefficient. The concentration correction factor is compared with the lower limit boundary value of zero. Compare with the upper boundary value two. If the lower boundary value of zero is less than the concentration correction factor... The value, and the concentration correction factor If the value is less than or equal to the upper limit boundary value of 2, the value range determination unit outputs "within the range"; if the concentration correction coefficient The value is less than or equal to the lower limit boundary value of zero, or the concentration correction factor. If the value is greater than the upper limit boundary value of 2, the numerical range determination unit will output "out of range".

[0059] In practical implementation, if the numerical range determination unit outputs "within range," meaning the concentration correction coefficient is greater than zero and less than or equal to two, the industrial control computer performs a multiplication operation, multiplying the initial effective concentration by the concentration correction coefficient to obtain the real-time effective concentration. Initial effective concentration With concentration correction factor The product of these is used as the real-time effective concentration. ,Right now Real-time effective concentration This represents the concentration of the polymerization inhibitor solution after correction using electrochemical redox potential dynamic information, expressed in milligrams per liter. Multiplication operations use floating-point multiplication instructions, and the result is rounded to two decimal places.

[0060] In practical implementation, if the numerical range determination unit outputs "out of range," meaning the concentration correction coefficient is less than or equal to zero or greater than two, the industrial control computer will set the concentration correction coefficient to one. The procedure for setting the concentration correction coefficient to one is as follows: The concentration correction coefficient is stored in the industrial control computer's memory... The variable address is written to the floating-point value 1.0. After completing the setting operation, the industrial control computer uses the initial effective concentration as the real-time effective concentration, that is... A concentration correction factor less than or equal to zero or greater than two indicates abnormal fluctuations in the redox potential data acquired by the electrochemical detection probe, or unexpected changes in the electrochemical properties of the polymerization inhibitor solution. In this case, the electrochemical correction information is discarded, and the initial effective concentration obtained from UV spectroscopy is directly used as the real-time effective concentration output.

[0061] In practice, the real-time effective concentration is continuously recorded and displayed. The industrial control computer stores the real-time effective concentration value calculated for each sampling period along with the corresponding sampling time timestamp into a real-time concentration database on the industrial control computer's hard drive. The database adopts a time-series storage structure and supports querying historical real-time effective concentration curves by time range. The display unit connected to the industrial control computer refreshes and displays the current real-time effective concentration value in real time. The display format is a combination of numerical and trend curve interfaces. The trend curve plots the trajectory of real-time effective concentration over time with time as the horizontal axis and real-time effective concentration as the vertical axis.

[0062] In practice, when the real-time effective concentration falls below a preset warning value, an alarm is triggered to prompt the replenishment of the polymerization inhibitor. The preset warning value is set according to the styrene polymerization process requirements and is 1.2 times the minimum effective inhibitory concentration of the polymerization inhibitor. In some embodiments, the minimum effective inhibitory concentration is 30 mg / L, and the preset warning value is set to 36 mg / L. This multiple is chosen to allow a 20% concentration margin before the inhibitor concentration drops to the minimum effective inhibitory concentration, giving operators sufficient time to replenish the inhibitor before it becomes completely ineffective. After obtaining the real-time effective concentration in each sampling cycle, the industrial control computer compares the real-time effective concentration value with the preset warning value. If the real-time effective concentration value is less than the preset warning value, the industrial control computer's digital output port outputs a high-level signal, driving the alarm device to issue an audible and visual alarm, prompting the operator to replenish the polymerization inhibitor in the styrene polymerization system.

[0063] In practice, the process of establishing the inhibitor concentration mapping table is as follows: Under the simulated conditions of styrene polymerization, a series of standard solutions of inhibitors with known concentrations are prepared. The simulated conditions for styrene polymerization refer to heating the styrene monomer to the same temperature as the actual polymerization reaction without adding an initiator, maintaining the same stirring speed, and introducing a protective gas of the same purity. This ensures the system is in a thermal and flow environment consistent with the actual reaction, without initiating the polymerization reaction, thus eliminating interference from polymer formation on spectral detection. A series of standard solutions of inhibitors with known concentrations cover the entire possible concentration range of the inhibitor in the styrene polymerization reaction, with a minimum concentration of 5 mg / L and a maximum concentration of 500 mg / L. The concentration difference between adjacent concentration points does not exceed 20 mg / L, resulting in the preparation of 25 standard solutions of different concentrations.

[0064] In practice, spectral data is acquired according to the ultraviolet spectral absorbance sequence. The ultraviolet spectrometer continuously acquires the transmittance data of the polymerization inhibitor standard solution at wavelengths of 250nm, 280nm, and 310nm according to a preset sampling period of 30 seconds. The transmittance data is converted into absorbance values, and the absorbance values ​​at the three wavelengths are aligned according to the sampling time to construct an ultraviolet spectral absorbance sequence.

[0065] In practical implementation, fluctuation characteristic parameters are extracted. The absorbance difference between adjacent sampling times is extracted from the ultraviolet spectral absorbance sequence to generate an absorbance fluctuation vector. Each element in the absorbance fluctuation vector is traversed, and its maximum and minimum values ​​are marked. The absolute value of the difference between the element values ​​of adjacent maximum and minimum values ​​is calculated as the fluctuation amplitude value. The current fluctuation amplitude value is divided by the previous fluctuation amplitude value to obtain the fluctuation amplitude ratio. All fluctuation amplitude ratios calculated for all wavelengths form a set of fluctuation characteristic parameters.

[0066] In practice, the fluctuation characteristic parameter interval corresponding to each standard concentration is recorded. For each standard solution of polymerization inhibitor with a known concentration, spectral data is repeatedly collected and fluctuation characteristic parameters are extracted a total of 10 times, resulting in 10 sets of fluctuation characteristic parameters. The arithmetic mean of all fluctuation amplitude ratios in each fluctuation characteristic parameter set is calculated to obtain 10 average fluctuation amplitude ratios. The arithmetic mean of the 10 average fluctuation amplitude ratios is used as the center value of the standard fluctuation characteristic parameter, and the sample standard deviation of the 10 average fluctuation amplitude ratios is calculated. The center value of the standard fluctuation characteristic parameter minus three times the sample standard deviation is used as the lower limit of the fluctuation characteristic parameter interval, and the center value of the standard fluctuation characteristic parameter plus three times the sample standard deviation is used as the upper limit of the fluctuation characteristic parameter interval. These lower and upper limits constitute the standard fluctuation characteristic parameter interval for the corresponding standard concentration.

[0067] In practice, a correspondence is established between standard fluctuation characteristic parameter ranges and standard concentration values, and this correspondence is stored in a mapping table for online detection. Each standard concentration value, along with its corresponding lower and upper limits of the standard fluctuation characteristic parameter range, is written as a record into the polymerization inhibitor concentration mapping table. The polymerization inhibitor concentration mapping table uses a two-dimensional table structure: the first column stores the standard concentration value in milligrams per liter; the second column stores the lower limit of the standard fluctuation characteristic parameter range; and the third column stores the upper limit of the standard fluctuation characteristic parameter range. The polymerization inhibitor concentration mapping table is stored as a binary file in the non-volatile memory of the industrial control computer. The online detection program of the industrial control computer loads the polymerization inhibitor concentration mapping table into memory upon startup, for use when querying the initial effective concentration using the fluctuation characteristic parameters as an index.

[0068] See Figure 7 In the graph, the vertical axis represents the inhibitor concentration (mg / L), and the horizontal axis represents the sampling time (minutes). The solid blue line indicates the real-time effective concentration change over time, and the dashed red line represents the preset warning value of 36 mg / L. The real-time effective concentration curve starts from approximately 210 mg / L and shows a continuous decreasing trend as the sampling time progresses, indicating that the inhibitor concentration gradually decreases as the polymerization reaction proceeds. The curve shows a smooth decrease overall, without any sudden fluctuations, reflecting the stability of the inhibitor consumption.

[0069] Around the 270-minute mark of the sampling period, the real-time effective concentration curve first dropped to near the preset warning value of 36 mg / L, indicating that the inhibitor concentration had approached 1.2 times the minimum effective inhibition concentration warning limit. At this point, the system may trigger an alarm mechanism, prompting operators to replenish the inhibitor to ensure the safe and stable operation of the polymerization reaction. At the end of the 300-minute sampling period, the real-time effective concentration further decreased to approximately 28 mg / L, below the preset warning value, reflecting that the inhibitor had been consumed to a critical state.

[0070] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application.

Claims

1. An online detection method for polymerization inhibitors in styrene polymerization, characterized in that, The method includes: Obtain the UV absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths during the styrene polymerization reaction; An absorbance fluctuation vector is generated based on the absorbance difference between adjacent sampling times in the ultraviolet spectral absorbance sequence. Extract the extreme points in the absorbance fluctuation vector and calculate the fluctuation amplitude ratio corresponding to the extreme points to obtain the fluctuation characteristic parameters; Using the fluctuation characteristic parameters as an index, a preset inhibitor concentration mapping table is queried to determine the initial effective concentration of the inhibitor solution; When the initial effective concentration exceeds a preset threshold, the electrochemical detection probe is activated to acquire the redox potential sequence of the polymerization inhibitor solution; Calculate the second-order difference of three consecutive potential values ​​in the redox potential sequence to obtain the potential change acceleration; The concentration correction coefficient is obtained by weighting and fusing the potential change acceleration with the initial effective concentration. The initial effective concentration is corrected using the concentration correction coefficient to obtain the real-time effective concentration of the polymerization inhibitor solution.

2. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The acquisition of the ultraviolet absorbance sequence of the polymerization inhibitor solution at multiple preset wavelengths during the styrene polymerization reaction specifically includes: The ultraviolet spectrometer is controlled to continuously collect transmittance data of the polymerization inhibitor solution at wavelengths of 250 nm, 280 nm and 310 nm according to a preset sampling cycle; The transmittance data were converted into absorbance values ​​at 250 nm, 280 nm, and 310 nm, respectively. The ultraviolet spectral absorbance sequence is constructed by aligning the 250nm absorbance value, the 280nm absorbance value, and the 310nm absorbance value according to the sampling time.

3. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The step of generating an absorbance fluctuation vector based on the absorbance difference between adjacent sampling times in the ultraviolet spectral absorbance sequence specifically includes: Extract the absorbance values ​​of adjacent sampling times from the ultraviolet spectral absorbance sequence, and calculate the difference between the absorbance value of the next time time and the absorbance value of the previous time time, as the absorbance difference between adjacent sampling times. The absorbance difference between adjacent sampling times is arranged in chronological order to generate the absorbance fluctuation vector.

4. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The step of extracting the extreme points in the absorbance fluctuation vector and calculating the fluctuation amplitude ratio corresponding to the extreme points to obtain the fluctuation characteristic parameters specifically includes: Traverse each element in the absorbance fluctuation vector, mark the element with an element value greater than the two adjacent element values ​​as the maximum value point, and mark the element with an element value less than the two adjacent element values ​​as the minimum value point; Calculate the absolute value of the difference between the element values ​​of adjacent maximum and minimum points, and use it as the fluctuation range value; The fluctuation ratio is obtained by dividing the current fluctuation amplitude value by the previous fluctuation amplitude value.

5. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The step of using the fluctuation characteristic parameter as an index to query a preset inhibitor concentration mapping table to determine the initial effective concentration of the inhibitor solution specifically includes: The fluctuation characteristic parameter is matched with the standard fluctuation characteristic parameter range in the polymerization inhibitor concentration mapping table to determine the target standard fluctuation characteristic parameter range to which the fluctuation characteristic parameter belongs; Read the standard concentration value corresponding to the target standard fluctuation characteristic parameter range, and use it as the initial effective concentration.

6. The online detection method for polymerization inhibitors in styrene polymerization according to claim 2, characterized in that, The step of activating an electrochemical detection probe to acquire the redox potential sequence of the polymerization inhibitor solution when the initial effective concentration exceeds a preset threshold specifically includes: Compare the initial effective concentration with the preset threshold. If the initial effective concentration is greater than the preset threshold, send a start command to the electrochemical detection probe. The electrochemical detection probe is controlled to continuously collect the redox potential data of the polymerization inhibitor solution according to the preset sampling cycle; The redox potential data are arranged in the order of sampling time to generate the redox potential sequence.

7. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The calculation of the second-order difference of three consecutive potential values ​​in the redox potential sequence to obtain the potential change acceleration specifically includes: Extract consecutive first potential value, second potential value, and third potential value from the redox potential sequence; Calculate the first-order forward difference of the second potential value minus the first potential value to obtain the first difference value; The second difference value is obtained by subtracting the first-order backward difference of the second potential value from the third potential value. The second difference is obtained by calculating the difference between the second difference value and the first difference value.

8. The online detection method for polymerization inhibitors in styrene polymerization according to claim 7, characterized in that, The step of weighting and fusing the potential change acceleration with the initial effective concentration to obtain the concentration correction coefficient specifically includes: The second-order difference is multiplied by a preset acceleration weighting factor to obtain the acceleration contribution value; The initial effective concentration is multiplied by a preset concentration weighting factor to obtain the concentration contribution value; The concentration correction coefficient is obtained by adding the acceleration contribution value to the concentration contribution value.

9. The online detection method for polymerization inhibitors in styrene polymerization according to claim 1, characterized in that, The step of correcting the initial effective concentration using the concentration correction coefficient to obtain the real-time effective concentration of the polymerization inhibitor solution specifically includes: Determine whether the value of the concentration correction coefficient is greater than zero and less than or equal to two; If the value of the concentration correction coefficient is greater than zero and less than or equal to two, then the initial effective concentration is multiplied by the concentration correction coefficient to obtain the real-time effective concentration; If the value of the concentration correction coefficient is less than or equal to zero or greater than two, then the concentration correction coefficient is set to one, and the initial effective concentration is taken as the real-time effective concentration.

10. The online detection method for polymerization inhibitors in styrene polymerization according to claim 5, characterized in that, The polymerization inhibitor concentration mapping table was established by pre-collecting ultraviolet spectra of standard solutions of polymerization inhibitors with different known concentrations under the same conditions and extracting fluctuation characteristic parameters.