A polarizer and display device
By introducing a gradient interface layer and a dual bonding network into the polarizer, the optical performance degradation and warping problems of traditional polarizers under high temperature and high humidity environments are solved, achieving high bonding strength and long-term optical stability, making it suitable for display devices.
Patent Information
- Application Number
- CN202611603075.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-16
- Publication Date
- 2026-11-17
AI Technical Summary
Traditional polarizers are prone to hydrolysis in high temperature and high humidity environments, which leads to deterioration of optical performance and dimensional changes. Furthermore, stress concentration is likely to occur at the interface between the adhesive layer and the material, affecting the flatness and optical uniformity of the device.
A gradient interface layer is used to replace the adhesive layer. By forming a gradient interface layer in situ between the polarizing layer and the protective layer, an organic-inorganic dual bonding network is constructed using reactive compatibilizers and silicon-based composite materials to achieve covalent connection between the polarizing layer and the protective layer. Combined with a double-sided symmetrical protective layer design, stress is offset.
It significantly improves interfacial bonding and structural integrity, hydrolysis resistance and thermal stability, reduces warping tendency, maintains stable optical performance, and enhances the environmental reliability and service life of display devices.
Smart Images

Figure CN123113073A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of optical element technology, and in particular to a polarizer and display device. Background Technology
[0002] Polarizing film is one of the core optical components of liquid crystal display devices. Its basic structure usually consists of a protective film bonded to both sides of a polyvinyl alcohol polarizing layer with an adhesive. Traditional protective films are mainly made of cellulose triacetate film, but this material is not resistant to humidity and heat and is prone to hydrolysis in high temperature and high humidity environments, which leads to the deterioration of the optical performance of the polarizing film and changes in its size.
[0003] Currently, Chinese utility model patent CN208255574U discloses a liquid crystal electro-optical dimming mirror based on an absorption-reflection composite polarizer. This design places an absorption polarizer on one outer surface of a TN liquid crystal cell and an absorption-reflection composite polarizer on the other outer surface, attaching the reflective polarizing surface of the composite polarizer to the outer surface of the TN liquid crystal cell. This structure constitutes a normally white TN liquid crystal cell, exhibiting a semi-transparent glass appearance when no electric field is applied. After applying an electric field, it appears as a light-blocking black glass when viewed from one side and as a dark reflective mirror when viewed from the other, thus realizing the function of an electro-optical dimming mirror. This design emphasizes the combination of polarizer types and the optical effect design of the liquid crystal cell, expanding the liquid crystal cell from a simple display device into a decorative and functional integrated device with electro-optical dimming capabilities.
[0004] However, conventional polarizer structures in existing technologies leave an adhesive layer and abrupt material interfaces between the polarizing layer and the protective film. After prolonged use, the adhesive layer may yellow, and the interface area is prone to stress accumulation due to differences in modulus and coefficient of thermal expansion between the materials. When the polarizer area is large, these factors have a more significant impact on the flatness and optical uniformity of the device. For applications requiring both low warpage and long-term stable optical delay, conventional film bonding structures still have room for improvement in achieving these performance goals. Summary of the Invention
[0005] Therefore, it is necessary to provide a polarizer and display device to address the aforementioned technical problems.
[0006] This application provides a polarizer, employing the following technical solution: It includes a polarizing layer and a first composite protective layer directly bonded to a main surface of the polarizing layer; a first gradient interface layer is formed in situ between the polarizing layer and the first composite protective layer; the polarizing layer is composed of a polyvinyl alcohol-based resin; the first composite protective layer is formed of a resin composition containing polyolefin materials, a soft material, and a silicon-based composite material, wherein the polyolefin material is a cyclic olefin polymer, the soft material is a polyolefin elastomer, and the silicon-based composite material is a mixture of nano-silica with first reactive groups on its surface and cage-type silsesquioxane with first reactive groups on its surface; the first gradient interface layer is composed of the polarizing layer resin, cyclic olefin... The material is composed of a polymer, a polyolefin elastomer, a silicon-based composite material, and a reactive compatibilizer. Its composition changes continuously in a gradient along the thickness direction from the polarizing layer to the first composite protective layer, with the content of the polarizing layer resin gradually decreasing and the content of the cyclic olefin polymer gradually increasing. The reactive compatibilizer has a second reactive group and a non-polar segment compatible with the polyolefin material. The second reactive group forms a covalent bond with the hydroxyl group of the polarizing layer resin. The silicon-based composite material uses its first reactive group to chemically bond with the hydroxyl groups of both the reactive compatibilizer and the polarizing layer resin, thereby constructing an organic-inorganic dual-bonding network within the first gradient interface layer, with the reactive compatibilizer as the bridge and the silicon-based composite material as the node.
[0007] Furthermore, the reactive compatibilizer is a graft copolymer, the main chain of which is selected from styrene-ethylene / butene-styrene block copolymer and maleic anhydride grafted polyolefin elastomer, and the side links are grafted with acrylate monomer units containing a second reactive group; the second reactive group is epoxy, amino, isocyanate group or mercapto group, and the first reactive group is epoxy, amino or methacryloyloxy.
[0008] Furthermore, in the first gradient interface layer, the concentration of silicon-based composite material increases first and then decreases from the polarizing layer toward the first composite protective layer, forming a concentration peak in the middle of the interface layer. The content of silicon-based composite material at this concentration peak accounts for 15-30 wt% of the total solid mass of the first gradient interface layer.
[0009] Furthermore, the thickness of the first gradient interface layer is 0.3-3 μm. When the first gradient interface layer is subjected to in-depth analysis using time-of-flight secondary ion mass spectrometry, the signal intensity ratio of silicon to carbon elements changes continuously within the thickness range without any abrupt changes.
[0010] Furthermore, the polarizing layer is a polyvinyl alcohol film dyed with iodine and uniaxially stretched, the cyclic olefin polymer is a norbornene ring-opening polymerized hydride, and the polyolefin elastomer is an ethylene-octene copolymer with a Shore A hardness of 65-80. After the polarizer is placed at 85°C and 85%RH for 500 hours, the peel strength retention rate between the polarizing layer and the first composite protective layer is greater than 90%, the in-plane retardation Ro of the first composite protective layer is ≤3nm, and the absolute value of the thickness direction retardation Rth is ≤8nm.
[0011] Furthermore, on the other main surface of the polarizing layer opposite to the first composite protective layer, a second composite protective layer and a second gradient interface layer are symmetrically disposed, the composition and thickness of the second gradient interface layer being the same as those of the first gradient interface layer.
[0012] Furthermore, the thickness of both the first and second composite protective layers is 20-50 μm, the thickness of the polarizing layer is 10-28 μm, the total thickness of the polarizer is 70-130 μm, and the warpage of the polarizer does not exceed 0.5 mm / 100 mm.
[0013] This application also provides a method for preparing the above-mentioned polarizer, comprising: S1, preparing a polarizing layer; S2, preparing a protective coating liquid, the coating liquid containing a cyclic olefin polymer, a polyolefin elastomer, a silicon-based composite material, a reactive compatibilizer, and an organic solvent; S3, coating the coating liquid onto a main surface of the polarizing layer to form a wet film; S4, subjecting the wet film to gradient heat treatment: first, treating it at a temperature T1 and a relative humidity RH1 for a time t1, causing the reactive compatibilizer to migrate directionally to the polarizing layer interface and partially swell the surface of the polarizing layer; then treating it at a temperature T2 and a relative humidity RH2 for a time t2, causing the reactive compatibilizer that migrated to the interface to simultaneously undergo a bonding reaction with the polarizing layer resin and the silicon-based composite material and complete curing, thereby forming a gradient interface layer in situ and bonding a composite protective layer; wherein T1 is 40-60℃, RH1 is 60-90%, and t1 is 1-5 minutes; T2 is 80-120℃, RH2≤10%, and t2 is 3-15 minutes.
[0014] Furthermore, the solvent used in the protective layer coating liquid is a mixed solvent of toluene and methyl isobutyl ketone, the solid content of the cyclic olefin polymer in the coating liquid is 10-25wt%, and the wet film coating thickness is 80-200μm; in the T1 treatment stage, the difference in the evaporation rate of the mixed solvent is used to form a viscosity gradient in the wet film thickness direction to assist the directional migration of the reactive compatibilizer.
[0015] In addition, this application also provides a display device including a liquid crystal display panel, the liquid crystal display panel having a first substrate, a second substrate disposed opposite to each other and a liquid crystal layer located between the two, and a polarizer attached at one or both of the outer sides of the first substrate and the second substrate, the polarizer being the polarizer described above.
[0016] In summary, this application includes the following beneficial technical effects: 1. The polarizer provided in this application replaces the adhesive layer and sharp interface between the polarizing layer and the protective layer in traditional polarizers with an in-situ generated gradient interface layer. In this gradient interface layer, the content of the polarizing layer resin continuously decreases along the thickness direction, while the content of the cyclic olefin polymer continuously increases, so that the modulus and coefficient of thermal expansion gradually transition in the interface region, fundamentally avoiding stress concentration caused by abrupt changes in material properties. At the same time, an organic-inorganic dual-bonding network is constructed in the gradient interface layer, with reactive compatibilizers as bridges and silicon-based composite materials as nodes, which firmly connects the polarizing layer resin and the polyolefin protective material through covalent bonds, significantly improving the interfacial bonding force and structural integrity.
[0017] 2. The silicon-based particles in the double-bonded network of this application, as multifunctional cross-linking nodes, have excellent hydrolysis resistance and thermal stability. They can maintain the density and strength of interfacial chemical bonds for a long time in humid and hot environments, effectively resisting the erosion of the interface by water molecules. The symmetrical arrangement of the double-sided protective layer allows the shrinkage or expansion stress generated on both sides of the polarizer to cancel each other out when the temperature and humidity change, which greatly reduces the warping tendency of the polarizer. After long-term high temperature and high humidity aging, the polarizer can still maintain stable in-plane retardation and thickness direction retardation, with no significant degradation in optical performance, demonstrating excellent environmental reliability.
[0018] 3. In terms of preparation, the method of this application integrates the preparation of the coating solution, coating, and gradient heat treatment into a continuous process. It utilizes the difference in evaporation rate of the mixed solvent to naturally form a viscosity gradient in the wet film, driving the reactive compatibilizer to spontaneously migrate to the polarizing layer interface. It can construct a continuously changing interface layer without additional coating steps or pre-coating layers. The two-stage heat treatment of low temperature and high humidity and high temperature and low humidity respectively complete the directional enrichment of the compatibilizer and the chemical bonding of the interface. The process parameters are clear and controllable, which is suitable for continuous industrial production. In addition, the display device containing this polarizer is less prone to problems such as edge light leakage and uneven image during long-term use due to the polarizer's low warpage and high humidity and heat stability, thus improving the display quality and service life. Attached Figure Description
[0019] Figure 1 This is a schematic diagram of the structure of the polarizer in this application; Figure 2This is a schematic diagram showing the concentration distribution of each component along the thickness direction within the first gradient interface layer of this application; Figure 3 This is a schematic diagram of the TOF-SIMS depth profile of the first gradient interface layer in this application; Figure 4 This is a flowchart of the preparation method of the polarizer in this application; Figure 5 This is a schematic diagram illustrating the measurement of polarizer warpage in this application; Figure 6 This is a schematic diagram of the structure of the display device of this application.
[0020] Explanation of reference numerals in the attached figures: 10, polarizing layer; 20, first composite protective layer; 30, first gradient interface layer; 40, second composite protective layer; 50, second gradient interface layer; 100. Polarizing film; 1. First substrate; 2. Second substrate; 3. Liquid crystal layer. Detailed Implementation
[0021] To make the objectives, technical solutions, and advantages of this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the scope of this application.
[0022] For the fabrication of polarizing layer 10, please refer to [link / reference]. Figure 4 The polarizing layer 10 is made of polyvinyl alcohol resin. The polyvinyl alcohol resin used in this embodiment has an average degree of polymerization of approximately 2400 and a degree of saponification of approximately 99.9 mol%. These two parameters directly affect the polarizing performance and water resistance of the polarizing layer. If the polymerization is too low, the molecular chains are prone to breakage during stretching and orientation, resulting in a decrease in polarization efficiency. If the saponification is too low, the residual acetyl groups will hydrolyze under humid and hot conditions, altering the hydroxyl content and cross-linking state of the polarizing layer, thereby affecting the chemical bonding density with the subsequent gradient interface layer.
[0023] The preparation process involves first dissolving polyvinyl alcohol resin in deionized water to prepare an 8% (w / w) aqueous solution. This solution is then cast onto a mirror-finished metal strip and dried with hot air to obtain a primary film approximately 75 μm thick. This thickness allows for sufficient stretching to ensure the uniformity of the final polarizing layer thickness. The primary film is then immersed in a dyeing bath containing iodine and potassium iodide, where iodine molecules diffuse into the polyvinyl alcohol matrix. The dyed film is then uniaxially stretched in a boric acid bath at a stretching ratio of 5 to 6 times its original length. During stretching, boric acid cross-links with the hydroxyl groups of polyvinyl alcohol, causing the iodine molecules to be highly oriented and fixed along the stretching direction. The stretched film is then washed with water to remove unreacted boric acid and free iodine, and then dried to obtain a polarizing layer 10 approximately 12 μm thick. The drying temperature is controlled between 60 and 80 °C; excessively high temperatures will cause over-hardening of the polarizing layer surface, which is detrimental to the penetration and swelling of reactive compatibilizers during subsequent gradient heat treatment.
[0024] The surface and near-surface regions of the polarizing layer 10 contain a large number of active hydroxyl groups, which are the main sites for forming covalent bonds in subsequent steps. The polarizing layer 10 should be kept away from high humidity environments during storage and transportation to prevent the surface hydroxyl groups from being overhydrated and reducing the reactivity.
[0025] Preparation of protective coating liquid The solid components of the coating liquid, by weight, include: 70 parts of cyclic olefin polymer, 15 parts of polyolefin elastomer, 10 parts of silicon-based composite material, and 5 parts of reactive compatibilizer.
[0026] The cyclic olefin polymer selected is a norbornene ring-opening polymerized hydride, which is currently one of the commercially available cyclic olefin polymers with a relatively balanced light transmittance and heat resistance. Its glass transition temperature is approximately 165℃, and its number-average molecular weight is approximately 50,000. The selection of the glass transition temperature needs to consider two factors: first, it must be higher than the highest temperature the polarizer might encounter in actual use to prevent the protective layer from softening and deforming at high temperatures; second, it must be lower than the second-stage curing temperature in the subsequent gradient heat treatment to ensure that the cyclic olefin polymer in the coating solution can fully level and form a film during the curing stage. Molecular weight mainly affects the viscosity of the coating solution and the mechanical strength of the film after formation; a molecular weight of around 50,000 achieves a good balance between the two.
[0027] The polyolefin elastomer selected is an ethylene-octene copolymer with a Shore A hardness of 72. The function of this elastomer is to give the composite protective layer a certain degree of flexibility, while acting as a stress buffer segment in the gradient interface layer. Ethylene-octene copolymers with a hardness between 65 and 80 can be used. If the hardness is too low, the surface of the protective layer will become sticky, and if the hardness is too high, the compatibilization effect will decrease. If the chain segments that are too hard are too different from the molecular chain mobility of the polarizing layer resin, it will not be conducive to molecular chain entanglement and stress transfer at the interface.
[0028] The silicon-based composite material is composed of two types of particles. The first is nano-silica with an average particle size of 30 nm, treated with 3-glycidyl etheroxypropyltrimethoxysilane, and bearing epoxy groups on its surface; the second is a cage-like silsesquioxane with methacryloyloxy groups on its surface; the mass ratio of the two is 3:1. Nano-silica provides the main reinforcing nodes and crosslinking points, while the cage-like silsesquioxane, due to its unique cage-like structure and multiple reaction sites, can introduce local organic-inorganic hybrid regions into the crosslinked network, improving the toughness of the nodes. If all nano-silica is used without cage-like silsesquioxane, the crosslinked network will be brittle; conversely, if all cage-like silsesquioxane is used, the cost is higher and the spatial distribution uniformity of the particles is not as good as that of nano-silica.
[0029] The preparation of the reactive compatibilizer involves two steps. First, a maleic anhydride-grafted ethylene-octene copolymer is used as the base resin. Second, glycidyl methacrylate is grafted onto this base resin via free radical initiation to obtain a graft copolymer with epoxy groups in the side chains. The main chain segment of this compatibilizer has a similar structure to the polyolefin elastomer in the protective layer, exhibiting good compatibility. The epoxy groups on the side chains act as reactive groups, undergoing a ring-opening reaction with the hydroxyl groups of the polarizing layer resin.
[0030] The organic solvent used is a mixture of toluene and methyl isobutyl ketone (MBE) in a mass ratio of 85:15. Toluene has good solubility for cyclic olefin polymers and a fast evaporation rate; MBE has a relatively slow evaporation rate and a certain degree of polarity, which helps to stabilize the dispersion of the silicon-based composite material in the coating solution. The combination of these two solvents can create a controllable difference in evaporation rates during the initial drying stage after coating, facilitating subsequent viscosity gradient-driven migration.
[0031] Add all the above solid components into the mixed solvent and stir until completely dissolved and uniformly dispersed to obtain a coating liquid with a solid content of 20wt%. The coating liquid needs to be defoamed before coating and allowed to stand to remove bubbles in order to avoid air bubbles in the wet film affecting the uniformity of the interface layer.
[0032] Coating and gradient heat treatment The coating solution was applied to one main surface of the polarizing layer 10 using a wire bar coater, with the wet film thickness controlled at approximately 120 μm. The coating was carried out in a clean coating chamber at a temperature of 25°C and a relative humidity not exceeding 50%.
[0033] The coated film is immediately sent into a tunnel furnace for a two-stage gradient heat treatment process.
[0034] The first stage of processing is conducted at 50°C, 85% relative humidity, and for 3 minutes. The core objective of this stage is to achieve the directional migration of the reactive compatibilizer and the pre-swelling of the polarizing layer surface. Toluene has a boiling point of approximately 110°C, while methyl isobutyl ketone (Methyl isobutyl ketone) has a boiling point of approximately 116°C, a relatively small difference. However, at 50°C, the saturated vapor pressure of toluene is significantly higher than that of Methyl isobutyl ketone, thus toluene preferentially evaporates from the upper surface of the wet film. Due to solvent loss, the viscosity of the upper surface of the wet film increases rapidly, while the viscosity is relatively lower on the lower surface near polarizing layer 10 because more Methyl isobutyl ketone is retained, forming a viscosity gradient that increases from bottom to top. Driven by this viscosity difference, reactive compatibilizer molecules migrate from the lower layer to the upper layer. However, due to their affinity for the hydroxyl groups on the polarizing layer surface and the physical trapping effect of the swollen surface of the polarizing layer, the compatibilizer ultimately accumulates on the surface of the polarizing layer rather than continuing to migrate upwards to the surface of the wet film. Since 50℃ is below the glass transition temperature of polyvinyl alcohol (PVA), dry heat alone is insufficient to effectively swell the polarizing layer. Therefore, high humidity is introduced, allowing water molecules to penetrate into the surface of the polarizing layer, increasing the activity of the PVA chain segments and providing space for the penetration of compatibilizer molecules and the contact of chemical groups. If the processing time is too short, migration and swelling will be insufficient; if it is too long, the wet film may form a skin due to excessive solvent evaporation, affecting the uniformity of subsequent curing. Three minutes is an optimal value that balances efficiency and effectiveness.
[0035] The second stage of treatment is conducted at a temperature of 110℃, a relative humidity below 5%, and a time of 10 minutes. Upon entering the second stage, the temperature rapidly increases, and the residual toluene and methyl isobutyl ketone in the mixed solvent evaporate completely. When the temperature exceeds 100℃, the epoxy groups on the side chains of the reactive compatibilizer undergo a ring-opening reaction with the hydroxyl groups of the polarizing layer resin, generating stable ether bonds and achieving covalent bonding between the compatibilizer and the polarizing layer. Simultaneously, the epoxy groups on the surface of nano-silica and the methacryloxy groups on the surface of cage-like silsesquioxane undergo bonding reactions with the hydroxyl groups of the polarizing layer resin and the already ring-opened epoxy groups on the compatibilizer, respectively, forming a double cross-linked network with the compatibilizer molecular chains as bridges and silicon-based particles as nodes. Methacryloxy groups can also undergo self-polymerization at high temperatures, further increasing the cross-linking density. Below 100℃, the epoxy ring-opening reaction rate is too slow, resulting in incomplete curing; above 120℃, the iodine in the polarizing layer may undergo pyrolysis, reducing polarization performance. The relative humidity is controlled below 5% to prevent water molecules from competitively consuming epoxy groups, thus reducing bonding efficiency. A curing time of 10 minutes is sufficient to achieve a reaction rate of over 95% in the interfacial region.
[0036] After the above two processes, the solvent completely evaporates and the resin matrix is cured, and a first gradient interface layer 30 and a first composite protective layer 20 are simultaneously formed on a main surface of the polarizing layer 10. The first gradient interface layer 30 is generated in situ and there is no adhesive layer or physical boundary between it and the polarizing layer 10 and the first composite protective layer 20.
[0037] Preparation of symmetrical structures Reference Figure 1 The polarizer 100 of this application adopts a double-sided protective structure. Based on the single-sided protective structure described above, the polarizing layer 10 is flipped, and the same coating and gradient heat treatment steps are performed on the other main surface to form a second gradient interface layer 50 and a second composite protective layer 40. The composition and thickness of the second gradient interface layer 50 are the same as those of the first gradient interface layer 30, and the composition and thickness of the second composite protective layer 40 are the same as those of the first composite protective layer 20. The double-sided symmetrical arrangement allows the shrinkage stress generated on both sides of the polarizer to cancel each other out when temperature and humidity change, effectively suppressing warping.
[0038] Characterization of gradient interface layer The first gradient interface layer 30 and the second gradient interface layer 50 have essentially the same chemical composition and physical structure. The following explanation uses the first gradient interface layer 30 as an example.
[0039] Reference Figure 2 The concentrations of each component in the first gradient interface layer 30 along the thickness direction were analyzed by using X-ray photoelectron spectroscopy combined with argon ion layer-by-layer etching. Figure 2 The zero point on the horizontal axis corresponds to the junction between the first gradient interface layer 30 and the polarizing layer 10, while the right side corresponds to the junction between the first gradient interface layer 30 and the first composite protective layer 20. The curve trend shows that the resin concentration of the polarizing layer 10 continuously decreases from the side of the interface layer closer to the polarizing layer 10 towards the side closer to the first composite protective layer 20, while the concentration of the cyclic olefin polymer continuously increases, and the two curves intersect smoothly. The concentration of the silicon-based composite material first increases and then decreases, reaching a peak in the middle region of the interface layer. At this peak, the silicon-based composite material content accounts for approximately 22 wt% of the total solid mass of the first gradient interface layer 30.
[0040] Reference Figure 3 The first gradient interface layer 30 was depth-profiled using time-of-flight secondary ion mass spectrometry (TOF-SIMS). The x-axis represents sputtering time corresponding to the depth direction, and the y-axis represents the ratio of Si signal intensity to C signal intensity. The curve shows a smooth, single-peak shape with symmetrical peaks, transitioning gently at both ends to the bulk levels of the polarizing layer 10 and the first composite protective layer 20, respectively. The curve shows no abrupt changes or plateau regions, indicating that the composition is continuously and gradually changing throughout the entire interface layer thickness, without the formation of new independent phase layers. Based on the full width at half maximum (FWHM) of the Si / C intensity ratio curve, the thickness of the first gradient interface layer 30 is defined as approximately 1.5 μm. If the thickness is less than 0.3 μm, the gradient transition effect is not significant, and the stress buffering capacity is insufficient; if the thickness is greater than 3 μm, the gradient interface layer itself may form a thicker high-modulus cross-linked region, which could increase brittleness.
[0041] Polarizer performance testing The following performance tests were performed on the polarizer 100 manufactured according to the above embodiments.
[0042] Optical retardation testing. The in-plane retardation Ro and thickness direction retardation Rth of the first composite protective layer 20 and the second composite protective layer 40 were measured using a phase difference meter. The Ro values of both protective layers did not exceed 2 nm, and the absolute values of Rth did not exceed 6 nm. This indicates that the cyclic olefin polymer did not produce obvious molecular chain orientation during film formation, and the composite protective layer maintained good optical isotropy.
[0043] Peel strength test. According to JIS K 6854 standard, the peel strength between the polarizing layer 10 and the first composite protective layer 20 was tested using the 90° peel method at a tensile speed of 300 mm / min. The initial peel strength was 38 N / 25 mm. Samples from the same batch were placed in a constant temperature and humidity chamber at 85°C and 85% RH for 500 hours of aging. After being removed and placed at room temperature and humidity for 2 hours, the peel strength was tested, and the peel strength was 36 N / 25 mm, with a retention rate of approximately 95%. As a comparative example, using the same cyclic olefin polymer and polarizing layer material, but employing corona treatment followed by direct hot-press bonding without adhesive, the peel strength retention rate was only about 60% under the same aging conditions.
[0044] Warpage measurement. (Refer to...) Figure 5 The polarizer 100 was cut into 100mm × 100mm samples and placed flat on a 90℃ hot plate. After one hour, the height distribution on the sample surface was scanned using a laser displacement sensor, and the elevation difference between the highest and lowest points was taken as the warpage amount H. The measured warpage amount in this embodiment was 0.2mm / 100mm. As a comparative example, a polarizer with a gradient interface layer and a composite protective layer on only one side of the polarizing layer had a warpage amount of approximately 1.5mm / 100mm under the same conditions, demonstrating that the symmetrical structure had a very significant effect on suppressing warpage.
[0045] Display device Reference Figure 6 The display device includes a liquid crystal display panel, which is composed of a first substrate 1, a second substrate 2 and a liquid crystal layer 3 sandwiched between the two substrates. The first substrate 1 and the second substrate 2 are typically flexible substrates with transparent electrodes and alignment films. Polarizers 100 are respectively attached to the outside of the first substrate 1 and the outside of the second substrate 2 by means of an acrylic pressure-sensitive adhesive layer. The light absorption axis direction of the polarizers 100 is matched with the alignment direction of the liquid crystal layer 3.
[0046] The polarizer 100 has low warpage, so it is not easy to generate bubbles and edge lifting during the bonding process, resulting in a high bonding yield. After the display device is assembled, it undergoes a durability test at 85°C, 85%RH and 500 hours. After the test, it is powered on and checked. No light leakage was observed in the four corners of the screen, and the brightness uniformity of the whole surface meets the factory standard.
[0047] The embodiments described above are merely illustrative of the technical concept and features of this application, intended to enable those skilled in the art to understand the content of this application and implement it accordingly, and should not be construed as limiting the scope of protection of this application. All equivalent changes or modifications made in accordance with the spirit and essence of this application should be included within the scope of protection of this application.
Claims
1. A polarizer, comprising a polarizing layer (10) and a first composite protective layer (20) directly bonded to a main surface of the polarizing layer (10). Its features are, A first gradient interface layer (30) is formed in situ between the polarizing layer (10) and the first composite protective layer (20). The polarizing layer (10) is composed of polyvinyl alcohol resin; The first composite protective layer (20) is formed of a resin composition containing polyolefin materials, soft materials and silicon-based composite materials. The polyolefin materials are cyclic olefin polymers, the soft materials are polyolefin elastomers, and the silicon-based composite materials are a mixture of nano-silica with first reactive groups on the surface and cage-type silsesquioxane with first reactive groups on the surface. The first gradient interface layer (30) is composed of the polarizing layer (10) resin, cyclic olefin polymer, polyolefin elastomer, silicon-based composite material and reactive compatibilizer. Its composition changes continuously in the thickness direction from the polarizing layer (10) to the first composite protective layer (20). The content of the polarizing layer (10) resin gradually decreases and the content of the cyclic olefin polymer gradually increases. The reactive compatibilizer has a second reactive group and a non-polar segment compatible with the polyolefin material. The second reactive group forms a covalent bond with the hydroxyl group of the polarizing layer (10) resin. The silicon-based composite material uses its first reactive group to chemically bond with both the reactive compatibilizer and the hydroxyl group of the polarizing layer (10) resin, thereby constructing an organic-inorganic dual bonding network in the first gradient interface layer (30) with the reactive compatibilizer as the bridge and the silicon-based composite material as the node.
2. The polarizer according to claim 1, characterized in that, The reactive compatibilizer is a graft copolymer, the main chain of which is selected from styrene-ethylene / butene-styrene block copolymer and maleic anhydride grafted polyolefin elastomer, and the side links are grafted with acrylate monomer units containing a second reactive group; the second reactive group is epoxy, amino, isocyanate or mercapto, and the first reactive group is epoxy, amino or methacryloyloxy.
3. The polarizer according to claim 1, characterized in that, In the first gradient interface layer (30), the concentration of silicon-based composite material increases first and then decreases from the polarizing layer (10) toward the first composite protective layer (20), forming a concentration peak in the middle of the interface layer. The content of silicon-based composite material at the concentration peak accounts for 15-30 wt% of the total solid mass of the first gradient interface layer (30).
4. A polarizer according to claim 1, characterized in that, The thickness of the first gradient interface layer (30) is 0.3-3 μm. When the first gradient interface layer (30) is subjected to in-depth analysis using time-of-flight secondary ion mass spectrometry, the signal intensity ratio of silicon to carbon elements changes continuously within the thickness range without any abrupt change.
5. A polarizer according to claim 1, characterized in that, The polarizing layer (10) is a polyvinyl alcohol film dyed with iodine and stretched uniaxially. The cyclic olefin polymer is a norbornene ring-opening polymer hydride. The polyolefin elastomer is an ethylene-octene copolymer with a Shore A hardness of 65-80. After the polarizer is placed at 85°C and 85%RH for 500 hours, the peel strength retention rate between the polarizing layer (10) and the first composite protective layer (20) is greater than 90%. The in-plane retardation Ro of the first composite protective layer (20) is ≤3nm, and the absolute value of the thickness direction retardation Rth is ≤8nm.
6. A polarizer according to claim 1, characterized in that, On the other main surface of the polarizing layer (10) opposite to the first composite protective layer (20), a second composite protective layer (40) and a second gradient interface layer (50) are symmetrically disposed. The composition and thickness of the second gradient interface layer (50) are the same as those of the first gradient interface layer (30).
7. A polarizer according to claim 6, characterized in that, The thickness of the first composite protective layer (20) and the second composite protective layer (40) is 20-50μm, the thickness of the polarizing layer (10) is 10-28μm, the total thickness of the polarizer is 70-130μm, and the warpage of the polarizer does not exceed 0.5mm / 100mm.
8. A method for preparing the polarizer according to any one of claims 1 to 7, characterized in that, include: S1. Prepare the polarizing layer (10); S2. Prepare a protective coating solution containing cyclic olefin polymers, polyolefin elastomers, silicon-based composite materials, reactive compatibilizers, and organic solvents. S3. The coating liquid is applied to one of the main surfaces of the polarizing layer (10) to form a wet film; S4. Gradient heat treatment of wet film: First, treat at temperature T1 and relative humidity RH1 for time t1 to promote the directional migration of reactive compatibilizer to the polarizing layer (10) interface and partially swell the surface of polarizing layer (10); then treat at temperature T2 and relative humidity RH2 for time t2 to allow the reactive compatibilizer that has migrated to the interface to simultaneously undergo bonding reaction with the polarizing layer (10) resin and silicon-based composite material and complete curing, thereby forming a gradient interface layer (30) in situ and bonding the first composite protective layer (20). The T1 is 40-60℃, RH1 is 60-90%, and t1 is 1-5 minutes; the T2 is 80-120℃, RH2≤10%, and t2 is 3-15 minutes.
9. The method according to claim 8, characterized in that, The solvent used in the protective coating solution is a mixture of toluene and methyl isobutyl ketone. The solid content of the cyclic olefin polymer in the coating solution is 10-25 wt%, and the wet film coating thickness is 80-200 μm. In the T1 treatment stage, the difference in the evaporation rate of the mixed solvent is used to form a viscosity gradient in the wet film thickness direction to assist the directional migration of the reactive compatibilizer.
10. A display device comprising a liquid crystal display panel, the liquid crystal display panel having a first substrate (1), a second substrate (2) disposed opposite to each other and a liquid crystal layer (3) located between the two, wherein a polarizer (100) is attached at one or both of the outer sides of the first substrate (1) and the second substrate (2), characterized in that, The polarizer (100) is the polarizer according to any one of claims 1 to 7.
Citation Information
Patent Citations
Automatically controlled mirror of adjusting luminance of liquid crystal based on compound polaroid is absorbed, reflected