A short-arc xenon lamp anode and its processing method
By printing heat sinks and heat dissipation structures on the electrode ends of the short-arc xenon lamp anode, the problems of poor heat dissipation and high processing costs are solved, achieving efficient heat dissipation and improved material utilization.
Patent Information
- Application Number
- CN202611283495.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-24
- Publication Date
- 2026-11-17
AI Technical Summary
Short-arc xenon lamps have poor anode heat dissipation and high processing costs. Existing processing methods are difficult to effectively improve heat dissipation performance and have low material utilization.
Laser 3D printing technology is used to form a heat sink on the electrode end of the anode of a short-arc xenon lamp. The heat sink has a through heat dissipation cavity and heat dissipation structure, which achieves efficient heat dissipation through heat conduction, radiation and convection, and improves material utilization by printing materials.
Without reducing structural strength, the heat dissipation effect of the short-arc xenon lamp anode is significantly improved, the service life is extended, processing costs and materials are saved, and the material utilization rate is improved.
Smart Images

Figure CN123120599A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of short-arc xenon lamp technology, and more particularly to a short-arc xenon lamp anode and its processing method. Background Technology
[0002] A short-arc xenon lamp is a high-intensity gas discharge light source. During operation, its anode is subjected to continuous bombardment by a high-energy electron beam, generating a large amount of heat. This heat must be dissipated through the anode's heat dissipation area via thermal radiation and convection. The heat dissipation performance of the anode directly affects the lamp's lifespan, luminous stability, and operational reliability.
[0003] In related technologies, there are generally two processing methods for short-arc xenon lamp anodes. One method is to increase the heat dissipation area of the product fins by laser grooving. The drawback of this method is that the external fin morphology can only rely on adjusting the depth and number of grooves to improve heat exchange efficiency. However, the groove depth is limited. Too deep a groove will affect the overall strength of the product and make it difficult to effectively dissipate internal heat. The other method is to coat the anode surface with tungsten powder and sinter it to increase the specific surface area by increasing the surface roughness. Both methods have low heat dissipation improvement effects. Moreover, tungsten products made by traditional powder metallurgy have finer grains and more grain boundaries per unit volume. Compared with coarse grains with fewer grain boundaries per unit volume, they have poorer heat dissipation performance. Furthermore, the processing method of milling tungsten rods and then laser grooving results in a large amount of material removal, low material utilization, and high processing costs. Summary of the Invention
[0004] The purpose of this invention is to provide a short-arc xenon lamp anode and its processing method to solve the problems of poor heat dissipation and high processing cost of short-arc xenon lamp anodes.
[0005] To achieve this objective, the present invention adopts the following technical solution: In a first aspect, a short-arc xenon lamp anode includes: an electrode end; a heat sink, wherein the heat sink is printed on one end face of the electrode end in a first direction, the heat sink has a heat dissipation cavity extending through the heat sink along the first direction, and the outer peripheral wall of the heat sink and / or the cavity wall of the heat dissipation cavity are provided with a heat dissipation structure; wherein, the first direction is the length direction of the short-arc xenon lamp anode.
[0006] Preferably, multiple heat sinks are provided, and the multiple heat sinks are coaxially arranged, with adjacent heat sinks spaced apart in a direction perpendicular to the first direction.
[0007] Preferably, the plurality of heat sinks have the same size in the first direction; or, the plurality of heat sinks have different sizes in the first direction; or, the plurality of heat sinks have not completely the same size in the first direction.
[0008] Preferably, there are two heat sinks, namely a first heat sink and a second heat sink, at least a portion of the second heat sink is located within the heat sink cavity of the first heat sink, and the dimension of the second heat sink in the first direction is greater than the dimension of the first heat sink in the first direction.
[0009] Preferably, the outer peripheral surface of the heat sink located on the outside in a direction perpendicular to the first direction is flush with the outer peripheral surface of the electrode end.
[0010] Preferably, the heat dissipation structure is a heat dissipation groove, which circumferentially surrounds the outer peripheral surface of the heat dissipation component.
[0011] Preferably, the heat dissipation structure is provided in multiple ways, and the multiple heat dissipation structures are arranged along the first direction; the size of the heat dissipation structure in the first direction is in the range of 0.1mm-0.5mm; and / or the spacing between two adjacent heat dissipation structures is in the range of 1mm-2mm.
[0012] Preferably, the density of the heat sink is greater than or equal to 19.15 g / cm³. 3 ; and / or, the grain size of the heat sink in the cross section perpendicular to the first direction ranges from 0μm to 200μm; and / or, the grain size of the heat sink in the longitudinal section parallel to the first direction ranges from 0μm to 400μm.
[0013] Secondly, a method for processing a short-arc xenon lamp anode, used to process a short-arc xenon lamp anode as described above, the method comprising: S1. The electrode end is obtained through processing; S2. Using one end face of the electrode end in the first direction as the printing start face, print the printing material onto the printing start face to obtain a heat sink and a heat dissipation structure disposed on the heat sink; S3. Clean up any residual tungsten powder on the surface of the recycled product; S4. Perform heat treatment on the entire product.
[0014] Preferably, in step S2, the printing material includes tungsten, and the tungsten content in the printing material is greater than or equal to 99%. And / or, during the printing process in step S2, the layer thickness of the printing material ranges from 10μm to 50μm; And / or, during the printing process in step S2, the printing material is printed by laser 3D printing, and the laser spot size ranges from 20μm to 200μm, the laser power ranges from 100W to 500W, the laser scanning speed ranges from 100mm / s to 1000mm / s, and the laser scanning spacing ranges from 0.02mm to 0.1mm.
[0015] Preferably, after step S1 and before step S2, the short-arc xenon lamp anode processing method further includes: A printing substrate is provided, the printing substrate having a processing groove; The electrode end is assembled into the processing groove, and the end face of the electrode end used for printing the heat sink is controlled to be on the same horizontal plane as the top surface of the printing substrate.
[0016] Preferably, in step S4, the heat treatment atmosphere is a vacuum or hydrogen, the heat treatment temperature range of the product is 1500℃-2300℃, the product is heated to the set maximum temperature and then held at the temperature platform for 1 hour to 6 hours, and the product is cooled down with the furnace after the heat treatment is completed.
[0017] The beneficial effects of this invention are: The short-arc xenon lamp anode provided by the present invention includes an electrode end and a heat sink. The heat sink is printed on one end face of the electrode end in a first direction. The heat sink has a heat sink cavity extending through the heat sink in the first direction. The outer peripheral wall of the heat sink and / or the cavity wall of the heat sink cavity are provided with heat dissipation structures. The first direction is the length direction of the short-arc xenon lamp anode.
[0018] In this way, the heat dissipation cavity and heat dissipation structure on the heat sink can increase the heat dissipation area and improve the heat dissipation effect of the short-arc xenon lamp anode. When the short-arc xenon lamp anode is working, electrons collide with the working surface, and its temperature rises sharply. The heat from the electrode end is transferred to the heat sink connected to the electrode end through heat conduction. Then, the heat dissipation is completed through heat radiation and heat convection through the heat dissipation cavity and heat dissipation structure. Rapid heat dissipation is achieved without reducing the structural strength, extending the life of the short-arc xenon lamp. In addition, the printed heat sink has a rough surface, which can further increase the heat dissipation area, save the milling process, and improve the material utilization rate. Attached Figure Description
[0019] Figure 1 This is a front view of the anode of a short-arc xenon lamp in one embodiment of the present invention; Figure 2 This is a schematic diagram of the structure of the short-arc xenon lamp anode in one embodiment of the present invention; Figure 3 This is a cross-sectional view of the anode of a short-arc xenon lamp in one embodiment of the present invention; Figure 4This is a flowchart of a short-arc xenon lamp anode processing method in one embodiment of the present invention.
[0020] In the picture: 1. Electrode end; 11. Working surface; 2. Heat sink; 21. Heat sink cavity; 22. Heat sink structure; 23. First heat sink; 24. Second heat sink; 3. Assembly part; 31. Assembly groove; X, First direction. Detailed Implementation
[0021] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the present invention, and not all of the structures.
[0022] In the description of this invention, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0023] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.
[0024] In the description of this embodiment, the terms "upper," "lower," "left," and "right," etc., refer to the orientation or positional relationship shown in the accompanying drawings. They are used only for ease of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the present invention. In addition, the terms "first" and "second" are used only for distinction in description and have no special meaning.
[0025] See Figures 1 to 3The present invention provides a short-arc xenon lamp anode, including an electrode end 1 and a heat sink 2. The heat sink 2 is printed on one end face of the electrode end 1 in a first direction X. The heat sink 2 is provided with a heat sink cavity 21 extending through the heat sink 2 along the first direction X. The outer peripheral wall of the heat sink 2 and / or the cavity wall of the heat sink cavity 21 are provided with a heat sink structure 22. The first direction X is the length direction of the short-arc xenon lamp anode.
[0026] In this embodiment, the short-arc xenon lamp anode also includes an assembly part 3. The end of the electrode end 1 facing away from the heat sink 2 is a working surface 11. The electrode end 1 has a frustum structure. The diameter of the working surface 11 of the electrode end 1 is smaller than the diameter of the end face connected to the heat sink 2. The assembly part 3 is disposed inside the heat sink cavity 21 and has an assembly groove 31 for assembling the tungsten rod. The heat dissipation structure 22 is disposed on the outer peripheral wall of the heat sink 2 and the cavity wall of the heat sink cavity 21 to increase the heat dissipation area of the heat sink 2.
[0027] Thus, by opening a heat dissipation cavity 21 and setting a heat dissipation structure 22 on the heat sink 2, the heat dissipation effect of the short-arc xenon lamp anode can be improved through the heat dissipation structure 22 and the heat dissipation cavity 21. When the short-arc xenon lamp anode is working, electrons collide with the working surface 11, and its temperature rises sharply. The heat is transferred to the heat sink 2 connected to the electrode end 1 through thermal conduction. Then, the heat dissipation is completed by the heat dissipation cavity 21 and the heat dissipation structure 22 set on the inner and outer surfaces, and heat dissipation is completed by thermal radiation and thermal convection. Rapid heat dissipation is achieved without reducing the structural strength, thus extending the service life of the short-arc xenon lamp. The heat sink 2 is printed on the electrode end 1, which can save the milling process and improve the material utilization rate. In addition, the printed heat sink 2 has a rough surface, which can further increase the heat dissipation area.
[0028] See Figure 2 In some embodiments, multiple heat sinks 2 are provided, and the multiple heat sinks 2 are coaxially arranged, with adjacent heat sinks 2 spaced apart in a direction perpendicular to the first direction X.
[0029] In this embodiment, the heat sink 2 and the heat sink cavity 21 are arranged in a one-to-one correspondence. The heat sink 2 is a hollow cylindrical structure, so that there is an annular space between adjacent heat sinks 2. The end faces of the heat sink 2 on the same side are printed and set on the electrode end 1.
[0030] In this way, the volume of the heat dissipation cavity 21 can be increased within a limited axial space, thereby increasing the heat dissipation area of the short-arc xenon lamp anode. Heat dissipation is achieved through radiation from the cavity wall of the heat dissipation cavity 21, which is conducive to the continuous transfer of heat from the high-temperature zone to the low-temperature zone, improving the heat dissipation efficiency of the short-arc xenon lamp anode, and making the overall structure of the short-arc xenon lamp anode more compact.
[0031] It is understandable that the number of heat sink 2 can be adjusted according to actual processing needs, which will not be elaborated here.
[0032] See Figure 2 In some embodiments, the multiple heat sinks 2 have the same size in the first direction X; or, the multiple heat sinks 2 have different sizes in the first direction X; or, the multiple heat sinks 2 have not completely the same size in the first direction X.
[0033] In this embodiment, the multiple heat sinks 2 have different dimensions in the first direction X. Among adjacent heat sinks 2, the inner heat sink 2 has a larger dimension than the outer heat sink 2.
[0034] Thus, since the heat sink 2 is printed on the electrode end 1, it is convenient to process heat sinks 2 of different sizes, and the heat dissipation structure 22 and heat dissipation cavity 21 are processed by printing, which reduces the processing difficulty, saves milling process, improves assembly efficiency, saves printing material, and improves material utilization.
[0035] See Figure 3 In some embodiments, there are two heat sinks 2, namely a first heat sink 23 and a second heat sink 24. At least a portion of the second heat sink 24 is located in the heat dissipation cavity 21 of the first heat sink 23. The size of the second heat sink 24 in the first direction X is larger than the size of the first heat sink 23 in the first direction X.
[0036] In this embodiment, one end of the second heat sink 24 away from the electrode end 1 protrudes from the first heat sink 23. The outer diameter of the second heat sink 24 is smaller than the inner diameter of the first heat sink 23. The assembly part 3 is disposed in the heat dissipation cavity 21 of the second heat sink 24. The surface of the assembly part 3 away from the electrode end 1 is flush with the surface of the second heat sink 24 away from the electrode end 1.
[0037] In this way, a heat dissipation space can be formed between the first heat sink 23 and the second heat sink 24, and between the second heat sink 24 and the assembly part 3. This space, in conjunction with the heat dissipation structure 22 located inside the cavity wall of the heat dissipation cavity 21, improves the heat dissipation capacity of the short-arc xenon lamp anode and prevents heat from accumulating inside the heat sink 2.
[0038] It is understandable that the number of heat sink 2 can be adjusted according to actual needs, which will not be elaborated here.
[0039] See Figure 3 In some embodiments, the outer peripheral surface of the heat sink 2 located on the outer side in a direction perpendicular to the first direction X is flush with the outer peripheral surface of the electrode end 1. That is, the outer diameter of the first heat sink 23 is equal to the outer diameter of the end of the electrode end 1 facing the first heat sink 23.
[0040] In this way, the surface space of the electrode end 1 can be fully utilized to print the first heat sink 23, the second heat sink 24 and the assembly part 3, making the structure of the short arc xenon lamp anode more compact while increasing its heat dissipation capacity and reducing the processing cost of the short arc xenon lamp anode.
[0041] See Figure 3 In some embodiments, the heat dissipation structure 22 is a heat dissipation groove, which surrounds the outer peripheral surface of the heat dissipation component 2.
[0042] In this embodiment, heat dissipation grooves are disposed on the outer peripheral surface of the heat dissipation component 2 and the cavity wall of the heat dissipation cavity 21. The heat dissipation grooves disposed on the first heat dissipation component 23 and the second heat dissipation component 24 have the same width and the spacing between adjacent heat dissipation grooves is the same.
[0043] Thus, the heat dissipation grooves surrounding the first heat sink 23 and the second heat sink 24 can reduce dead corners on the heat dissipation surface, allowing the first heat sink 23 and the second heat sink 24 to fully participate in heat radiation. The heat dissipation grooves are located on the inner wall of the heat dissipation cavity 21, which can further increase the heat dissipation area. The heat dissipation grooves in the heat dissipation cavity 21 can dissipate the heat from the anode core of the short-arc xenon lamp to the space inside the heat dissipation cavity 21 in the form of radiation, thereby improving the heat dissipation efficiency. The heat dissipation grooves arranged at equal intervals can avoid the concentration of thermal stress caused by uneven local heat dissipation, thereby improving the stability and reliability of the short-arc xenon lamp anode under long-term high-temperature operation.
[0044] It is understandable that the heat dissipation structure 22 can also be a porous structure, heat dissipation fins, etc., and is not limited to heat dissipation slots, so we will not list them in detail here.
[0045] See Figure 3 In some embodiments, multiple heat dissipation structures 22 are provided, and the multiple heat dissipation structures 22 are arranged along the first direction X; the size of the heat dissipation structure 22 in the first direction X ranges from 0.1mm to 0.5mm; and / or the spacing between two adjacent heat dissipation structures 22 ranges from 1mm to 2mm.
[0046] In this embodiment, all heat dissipation structures 22 are coaxially arranged with the anode of the short-arc xenon lamp. The dimension of the heat dissipation structure 22 in the first direction X can be any value between 0.1mm and 0.5mm or any range between any two values, such as 0.1mm, 0.2mm, 0.3mm, 0.4mm, 0.5mm, etc. The distance between two adjacent heat dissipation structures 22 can be any value between 1mm and 2mm or any range between any two values, such as 1mm, 1.2mm, 1.4mm, 1.6mm, 1.8mm, 2mm, etc.
[0047] In this way, the heat dissipation grooves are evenly distributed, which can reduce the difference in heat dissipation capacity at different positions of the first heat dissipation component 23 and the second heat dissipation component 24, and avoid uneven heat dissipation leading to local overheating. By limiting the size of the heat dissipation structure 22 in the first direction X and the spacing between two adjacent heat dissipation structures 22, while ensuring that the first heat dissipation component 23 and the second heat dissipation component 24 have sufficient structural strength, the heat dissipation area is increased by processing multiple heat dissipation structures 22, which is conducive to achieving rapid heat dissipation of the short-arc xenon lamp anode.
[0048] Understandably, the dimensions of the heat dissipation structure 22 in the first direction X cannot be too small. If it is too small, the spacing between the walls of the heat dissipation grooves will be too close, affecting the improvement of heat dissipation effect. The dimensions of the heat dissipation structure 22 in the first direction X cannot be too large either. If it is too large, it will reduce the structural strength of the short-arc xenon lamp anode, making it prone to thermal deformation or breakage. The spacing between two adjacent heat dissipation structures 22 cannot be too small. If it is too small, it will increase the processing difficulty, and the ribs between adjacent heat dissipation structures 22 will be too thin, reducing the structural strength. The spacing between two adjacent heat dissipation structures 22 cannot be too large either. If it is too large, it will reduce the number of heat dissipation structures 22, reduce the total heat dissipation area, and make it difficult to dissipate heat in time.
[0049] See Figure 3 In some embodiments, the density of the heat sink 2 is greater than or equal to 19.15 g / cm³. 3 ; and / or, the grain size of the heat sink 2 in the cross section perpendicular to the first direction X ranges from 0μm to 200μm; and / or, the grain size of the heat sink 2 in the longitudinal section parallel to the first direction X ranges from 0μm to 400μm.
[0050] In this embodiment, the grain size of the cross section of the heat sink 2 perpendicular to the first direction X can be any value between 0μm and 200μm or any range between any two values, such as 0μm, 10μm, 50μm, 100μm, 150μm, 200μm, etc.; the grain size of the longitudinal section of the heat sink 2 parallel to the first direction X can be any value between 0μm and 400μm or any range between any two values, such as 0μm, 10μm, 100μm, 200μm, 300μm, 400μm, etc.
[0051] In this way, while ensuring that the heat sink 2 has sufficient structural strength, it can also have good heat dissipation capacity, avoid heat accumulation inside the heat sink 2, and facilitate connection with the electrode end 1 through printing, thereby improving the material utilization rate and heat dissipation capacity of the short arc xenon lamp anode.
[0052] Understandably, the cross-sectional grain size of heat sink 2 cannot be too small, as this would affect the heat dissipation effect. Conversely, the cross-sectional grain size of heat sink 2 cannot be too large, as this would increase the brittleness of the material and increase the probability of cracking.
[0053] See Figure 3 and Figure 4 The present invention also provides a method for processing short-arc xenon lamp anodes, used for processing short-arc xenon lamp anodes in any of the above embodiments. The method for processing short-arc xenon lamp anodes includes: S1. Electrode end 1 is obtained through processing; S2. Using one end face of electrode end 1 in the first direction X as the printing start face, print the printing material onto the printing start face to obtain heat sink 2 and heat dissipation structure 22 disposed on heat sink 2. S3. Clean up any residual tungsten powder on the surface of the recycled product; S4. Perform heat treatment on the entire product.
[0054] Furthermore, in some embodiments, the short-arc xenon lamp anode processing method further includes: S5. Inspect the shape and dimensions of the heat-treated product.
[0055] In this embodiment, in step S1, a tungsten electrode tip 1 is fabricated using powder metallurgy, pressure processing, and machining. The tungsten content of the electrode tip 1 material is ≥99%, and its density is ≥19.15 g / cm³. 3 The cross-sectional grain size is ≤30μm, which is beneficial for the rapid conduction of the electron beam heat received by the working surface 11 to the heat sink 2, and for heat dissipation through the heat dissipation structure 22 and the heat dissipation cavity 21.
[0056] In step S2, before printing the printing material onto the printing start surface, the printing start surface is polished and cleaned. Printing the printing material onto the printing start surface includes using laser positioning or the grafting printing function built into the 3D printing equipment.
[0057] In step S3, cleaning the residual tungsten powder on the surface of the recycled product includes cleaning the powder on the surface of the heat dissipation structure 22 by manual or mechanically assisted vibration until there is no powder residue on the surface of the short-arc xenon lamp anode.
[0058] In step S5, the appearance and dimensions of the heat-treated product are inspected, including by means of image measuring instruments and visual inspection.
[0059] Thus, by grafting and printing pure tungsten heat sink 2 and assembly part 3 onto forged tungsten rods, and processing heat dissipation structure 22 and heat dissipation cavity 21, the heat exchange efficiency of short-arc xenon lamp anode is improved and its service life is extended. Grafting printing can achieve the processing of complex shapes. During the processing, heat dissipation structure 22 and heat dissipation cavity 21 can be formed, saving the milling process and improving material utilization. When the printing material is grafted and printed to the printing starting surface, there are fewer grain boundaries per unit volume and better thermal conductivity. In addition, during the grafting printing process, the first heat sink 23, the second heat sink 24, and assembly part 3 naturally form rough surfaces, further improving the heat dissipation effect of short-arc xenon lamp anode.
[0060] It should be noted that the pressure processing in step S1 includes, but is not limited to, forging, rolling, etc. The processing of electrode end 1 is existing technology and will not be described in detail here.
[0061] See Figure 3 and Figure 4 In some embodiments, when multiple heat sinks 2 are provided; In step S2, heat sink 2 is printed one by one along a direction perpendicular to the first direction X and from the inside out; or, In step S2, heat sink 2 is printed one by one along a direction perpendicular to the first direction X and from the outside in; or, In step S2, multiple heat sinks 2 are printed simultaneously in a direction that gradually moves away from the electrode end 1.
[0062] In this way, the printing direction can be adapted according to the setting position of the heat sink 2, which improves the flexibility of short-arc xenon lamp anode processing, facilitates the processing of short-arc xenon lamp anodes of various sizes and shapes, saves milling processes, and improves material utilization and processing efficiency.
[0063] See Figure 4 In some embodiments, in step S2, the printing material includes tungsten, and the tungsten content in the printing material is greater than or equal to 99%. And / or, during the printing process in step S2, the layer thickness of the printing material ranges from 10μm to 50μm; And / or, during the printing process in step S2, the printing material is printed by laser 3D printing, and the laser spot size ranges from 20μm to 200μm, the laser power ranges from 100W to 500W, the laser scanning speed ranges from 100mm / s to 1000mm / s, and the laser scanning spacing ranges from 0.02mm to 0.1mm.
[0064] In step S2, the laser particle size range of the printing material is 5μm-100μm. After the printing material is vacuum dried at 200℃ for 2 hours, the powder Hall flow rate is ≤30s / 50g, and the oxygen content of the printing material powder is ≤300ppm. The laser particle size can be any value between 5μm and 100μm or any range between two values, such as 5μm, 20μm, 40μm, 60μm, 80μm, 100μm, etc.
[0065] In this embodiment, the thickness of the printing material layer can be any value between 10μm and 50μm, or any range between any two values, such as 10μm, 20μm, 30μm, 40μm, 50μm, etc.; the laser spot size can be any value between 20μm and 200μm, or any range between any two values, such as 20μm, 100μm, 120μm, 140μm, 160μm, 180μm, 200μm, etc.; the laser power can be any value between 100W and 500W, or any range between any two values, such as 100W, 2... 00W, 300W, 400W, 500W, etc.; the laser scanning speed can be any value between 100mm / s and 1000mm / s or any two values, such as 100mm / s, 300mm / s, 500mm / s, 700mm / s, 900mm / s, 1000mm / s, etc.; the laser scanning spacing can be any value between 0.02mm and 0.1mm or any two values, such as 0.02mm, 0.04mm, 0.06mm, 0.08mm, 0.1mm, etc.
[0066] This improves the reliability of grafting printing, allows the printing material to be stably bonded to the electrode end 1, facilitates the formation of heat dissipation structure 22 and heat dissipation cavity 21 during the grafting printing process, improves the yield of short-arc xenon lamp anode, and gives the first heat dissipation component 23 and the second heat dissipation component 24 good heat dissipation effect.
[0067] It is understandable that the layer thickness, laser spot size, laser power, laser scanning speed, and scanning spacing of the grafting print can be adjusted according to the size of the short-arc xenon lamp anode, which will not be elaborated here.
[0068] See Figure 3 and Figure 4 In some embodiments, after step S1 and before step S2, the short-arc xenon lamp anode processing method further includes: A printing substrate is provided, which has processing grooves; The electrode end 1 is assembled into the processing groove, and the end face of the electrode end 1 used for printing the heat sink 2 is controlled to be on the same horizontal plane as the top surface of the printing substrate.
[0069] In this embodiment, the material of the printing substrate is any one of iron, aluminum, titanium, tungsten, molybdenum, tantalum, and niobium, or an alloy thereof; or, the material of the printing substrate is at least one of alumina and zirconium oxide. Preferably, the material of the printing substrate is a refractory metal such as tungsten, molybdenum, tantalum, or niobium.
[0070] Thus, a large amount of heat is generated during the laser powder bed 3D printing process. The coefficient of thermal expansion of the electrode end 1 needs to be matched with the material of the printing substrate to avoid deformation of the electrode end 1 located in the processing groove during the processing, improve the positional accuracy of the printing starting surface, and thus improve the bonding quality between the heat sink 2 and the electrode end 1 during the grafting printing process.
[0071] It is understandable that the material of the printing substrate can be adjusted according to actual needs, which will not be elaborated here.
[0072] See Figure 4 In some embodiments, in step S4, the heat treatment atmosphere is a vacuum or hydrogen, the heat treatment temperature range of the product is 1500℃-2300℃, after the product is heated to the set maximum temperature, it is kept at the temperature platform for 1 hour to 6 hours, and after the heat treatment is completed, the product is cooled down with the furnace.
[0073] In this embodiment, the heat treatment temperature of the product can be any value or any two values between 1500℃ and 2300℃, such as 1500℃, 1700℃, 2000℃, 2100℃, 2200℃, 2300℃, etc. The holding time at the set maximum temperature platform can be any value or any two values between 1 hour and 6 hours, such as 1 hour, 2 hours, 3 hours, 4 hours, 5 hours, 6 hours, etc.
[0074] In this way, residual thermal stress accumulated during the grafting printing process can be eliminated, allowing the product's grains to grow and achieve better thermal conductivity. This prevents the short-arc xenon lamp anode from deforming or cracking due to residual stress release under subsequent high-temperature operating conditions, improves heat dissipation efficiency, reduces heat accumulation, and ensures that the short-arc xenon lamp anode has sufficient structural strength.
[0075] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation of the present invention. Those skilled in the art will be able to make various obvious changes, readjustments, and substitutions without departing from the scope of protection of the present invention. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the claims of the present invention.
Claims
1. A short arc xenon lamp anode, characterized in that, include: Electrode end (1); A heat sink (2) is printed on one end face of the electrode end (1) in a first direction (X). The heat sink (2) is provided with a heat dissipation cavity (21) that runs through the heat sink (2) along the first direction (X). The outer peripheral wall of the heat sink (2) and / or the cavity wall of the heat dissipation cavity (21) are provided with a heat dissipation structure (22). The first direction (X) is the length direction of the short arc xenon lamp anode.
2. The short arc xenon lamp anode of claim 1, wherein The heat sink (2) is provided in multiple ways, and the multiple heat sinks (2) are coaxially arranged, with two adjacent heat sinks (2) arranged at intervals in a direction perpendicular to the first direction (X).
3. The short arc xenon lamp anode of claim 2, wherein The multiple heat sinks (2) have the same size in the first direction (X); or, the multiple heat sinks (2) have different sizes in the first direction (X); or, the multiple heat sinks (2) have not completely the same size in the first direction (X).
4. The short arc xenon lamp anode of claim 2, wherein The heat sink (2) is provided in two parts, namely a first heat sink (23) and a second heat sink (24). At least a portion of the second heat sink (24) is located in the heat sink cavity (21) of the first heat sink (23). The size of the second heat sink (24) in the first direction (X) is greater than the size of the first heat sink (23) in the first direction (X).
5. The short arc xenon lamp anode of claim 2, wherein The outer peripheral surface of the heat sink (2) located on the outside in the direction perpendicular to the first direction (X) is flush with the outer peripheral surface of the electrode end (1).
6. The short arc xenon lamp anode of claim 1, wherein The heat dissipation structure (22) is a heat dissipation groove, which surrounds the outer peripheral surface of the heat dissipation component (2) in the circumferential direction.
7. The short arc xenon lamp anode of claim 1, wherein The heat dissipation structure (22) is provided in multiple ways, and the multiple heat dissipation structures (22) are arranged along the first direction (X); The dimensions of the heat dissipation structure (22) in the first direction (X) range from 0.1 mm to 0.5 mm; and / or the spacing between two adjacent heat dissipation structures (22) ranges from 1 mm to 2 mm.
8. The short arc xenon lamp anode of claim 1, wherein, The density of the heat sink (2) is greater than or equal to 19.15 g / cm³. 3 ; and / or, the grain size of the heat sink (2) in the cross section perpendicular to the first direction (X) is in the range of 0μm-200μm; and / or, the grain size of the heat sink (2) in the longitudinal section parallel to the first direction (X) is in the range of 0μm-400μm.
9. A method of processing an anode of a short arc xenon lamp, characterized in that The method for processing the short-arc xenon lamp anode as described in any one of claims 1-8 includes: S1. The electrode end (1) is obtained by processing; S2. Using one end face of the electrode end (1) in the first direction (X) as the printing start face, print the printing material onto the printing start face to obtain the heat sink (2) and the heat dissipation structure (22) disposed on the heat sink (2); S3. Clean up any residual tungsten powder on the surface of the recycled product; S4. Perform heat treatment on the entire product.
10. The short arc xenon lamp anode processing method according to claim 9, characterized by, In step S2, the printing material includes tungsten, and the tungsten content in the printing material is greater than or equal to 99%. And / or, during the printing process in step S2, the layer thickness of the printing material ranges from 10μm to 50μm; And / or, during the printing process in step S2, the printing material is printed by laser 3D printing, and the laser spot size ranges from 20μm to 200μm, the laser power ranges from 100W to 500W, the laser scanning speed ranges from 100mm / s to 1000mm / s, and the laser scanning spacing ranges from 0.02mm to 0.1mm.
11. The short arc xenon lamp anode processing method according to claim 9, characterized by, After step S1 and before step S2, the short-arc xenon lamp anode processing method further includes: A printing substrate is provided, the printing substrate having a processing groove; The electrode end (1) is assembled into the processing groove, and the end face of the electrode end (1) used for printing the heat sink (2) is controlled to be on the same horizontal plane as the top surface of the printing substrate.
12. The short-arc xenon lamp anode processing method according to claim 9, characterized in that, In step S4, the heat treatment atmosphere is vacuum or hydrogen, and the heat treatment temperature range of the product is 1500℃-2300℃. After the product is heated to the set maximum temperature, it is kept at the temperature platform for 1 hour to 6 hours. After the heat treatment is completed, the product is cooled down with the furnace.
