Memory device and method of manufacturing the memory device

By using interlayer insulating layers and sacrificial layers with different etch rates in a three-dimensional non-volatile memory device, the problem of irregular cell plug shape was solved, improving integration density and performance.

CN123124362APending Publication Date: 2026-11-17SK HYNIX INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202511966437.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-14
Filing Date
2025-12-24
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the manufacturing process of existing three-dimensional non-volatile memory devices, the shape of the cell plugs is prone to developing an arc-shaped profile, which affects integration density and performance.

Method used

By alternately stacking interlayer insulating layers and sacrificial layers with different etch rates in the laminate, a cell plug is formed, and its shape is controlled. For example, using a second interlayer insulating layer with a lower etch rate than the first and third interlayer insulating layers avoids the formation of an arc-shaped profile.

Benefits of technology

This resulted in more regular shapes for the unit plugs, improved integration density and memory device performance, and reduced inhomogeneities during manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124362A_ABST
    Figure CN123124362A_ABST
Patent Text Reader

Abstract

This application relates to a memory device and a method of manufacturing the memory device. A memory device includes a stack of layers in which conductive layers and interlayer insulating layers are alternately stacked, and a cell plug extending through the stack. The interlayer insulating layers include a first interlayer insulating layer having a first etch rate and a second interlayer insulating layer having a second etch rate lower than the first etch rate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This disclosure generally relates to memory devices and methods of manufacturing memory devices, including but not limited to a memory device comprising a memory block having a three-dimensional structure and a method of manufacturing a memory device comprising a memory block having a three-dimensional structure. Background Technology

[0002] Memory devices can include non-volatile memory devices that retain stored data even during power outages. Depending on how the memory cells are arranged, non-volatile memory devices can have a two-dimensional or three-dimensional structure. In a two-dimensional structure, the memory cells are arranged in a single layer on a substrate, while in a three-dimensional structure, the memory cells are stacked vertically on the substrate. Because the integration density of three-dimensional non-volatile memory devices is higher than that of two-dimensional ones, more electronic devices can be manufactured using three-dimensional non-volatile memory devices. Summary of the Invention

[0003] A memory device according to embodiments of the present disclosure may include a stack in which conductive layers and interlayer insulating layers are alternately stacked, and a cell plug extending through the stack. The interlayer insulating layer may include a first interlayer insulating layer having a first etch rate and a second interlayer insulating layer having a second etch rate lower than the first etch rate.

[0004] A method of manufacturing a memory device according to embodiments of the present disclosure may include forming a laminate by alternately stacking a sacrificial layer and an interlayer insulating layer, and forming a cell plug extending through the laminate. The interlayer insulating layer may include a first interlayer insulating layer having a first etch rate and a second interlayer insulating layer having a second etch rate lower than the first etch rate.

[0005] A memory device according to embodiments of the present disclosure may include: a cell stack including conductive layers alternately stacked with interlayer insulating layers; a cell plug extending through the cell stack; a dummy stack disposed on a side of the cell stack and including sacrificial layers alternately stacked with dummy insulating layers; and peripheral circuit contacts extending through the dummy stack. The sacrificial layer may include a first sacrificial layer and a second sacrificial layer with an etch rate lower than that of the first sacrificial layer. Attached Figure Description

[0006] Figure 1 This is a diagram illustrating a memory device according to an embodiment of the present disclosure;

[0007] Figure 2 This is an isometric view showing a memory device according to an embodiment of the present disclosure;

[0008] Figure 3A This is a plan view showing the layout of a memory device according to an embodiment of the present disclosure;

[0009] Figure 3B This is a cross-sectional view of a memory device according to an embodiment of the present disclosure;

[0010] Figures 4A to 4E This is a cross-sectional view of a memory device formed using a method for manufacturing a memory device according to an embodiment of the present disclosure;

[0011] Figure 5A and Figure 5B This is a cross-sectional view of a memory device according to an embodiment of the present disclosure;

[0012] Figure 6 This is a diagram illustrating a memory card system including a memory device according to an embodiment of the present disclosure; and

[0013] Figure 7 This is a block diagram illustrating a solid-state drive (SSD) system including a memory device according to an embodiment of the present disclosure. Detailed Implementation

[0014] Embodiments of this disclosure are described in detail with reference to the accompanying drawings. Specific structural or functional descriptions of the embodiments are provided as examples to illustrate the concepts disclosed in this application. Examples or embodiments based on the concepts can be implemented in various forms, and the scope of this disclosure is not limited to the examples or embodiments described in this specification.

[0015] Terms such as “vertical,” “horizontal,” “top,” “bottom,” “above,” “below,” “over,” “overlapping,” “up,” “side,” “upper part,” “uppermost part,” “lower part,” “lower part,” “higher,” “high,” “lower,” “column,” “row,” “height,” and other terms that suggest relative spatial relationships or orientations are used for the convenience of description or reference to the accompanying drawings and are not intended to limit in any other way.

[0016] The intersecting shading lines running through the figures illustrate corresponding or similar areas between the figures, rather than indicating the material associated with those areas.

[0017] This disclosure relates to a memory device that can improve the shape of the cell plug and a method of manufacturing the memory device.

[0018] Figure 1 This is a diagram illustrating a memory device 100 according to an embodiment of the present disclosure.

[0019] Reference Figure 1The memory device 100 includes a memory cell array 110, peripheral circuitry 170, and control circuitry 180.

[0020] The memory cell array 110 includes first memory blocks BLK1 to i-th memory blocks BLKi, where i is an integer greater than 1. Each of the memory blocks BLK1 to BLKi includes a memory cell for storing data. Drain select line DSL, word line WL, source select line SSL, and source line SL are connected to each of the memory blocks BLK1 to BLKi. Bit line BL is collectively connected to memory blocks BLK1 to BLKi.

[0021] Memory blocks BLK1 to BLKi can have a three-dimensional structure. A memory block with a three-dimensional structure includes memory cells stacked on a substrate along a vertical or normal direction. Memory blocks BLK1 to BLKi include a material layer stacked in the vertical direction and cell plugs extending through the material layer. In this disclosure, the material layer can be formed to have various properties, thereby improving the shape of the cell plugs. For example, to reduce the arcuate profile in the cell plugs, material layers with different etch rates are formed. (Refer to...) Figure 3B Describe the etching rate of the material layer.

[0022] Memory cells store one, two, or more bits of data depending on the programming method. For example, storing one bit of data in a memory cell is called the single-level cell method, and storing two bits is called the multi-level cell method. Storing three bits of data in a memory cell is called the three-level cell method, and storing four bits is called the four-level cell method. Five or more bits of data can be stored in a single memory cell.

[0023] The peripheral circuitry 170 is configured to perform programming operations that store data in the memory cell array 110, reading operations that output data stored in the memory cell array 110, and erasing operations that erase data stored in the memory cell array 110. The peripheral circuitry 170 includes a voltage generator 120, a row decoder 130, a page buffer group 140, a column decoder 150, and input / output circuitry 160.

[0024] Voltage generator 120 generates various operating voltages Vop used during programming, reading, and erasing operations in response to opcode OPCD. For example, voltage generator 120 is configured to generate programming voltage, turn-on voltage, turn-off voltage, negative voltage, pre-charge voltage, verification voltage, read voltage, pass voltage, and erase voltage in response to opcode OPCD. The operating voltage Vop generated at voltage generator 120 is applied via row decoder 130 to the drain select line DSL, word line WL, source select line SSL, and source line SL of the selected memory block.

[0025] The programming voltage is applied to the selected word line (WL) during programming operations to increase the threshold voltage of the memory cell connected to the selected word line. The turn-on voltage is applied to the drain select line (DSL) or the source select line (SSL) to turn on the drain select transistor (DST) or the source select transistor (SST). The cut-off voltage is applied to both the drain select line (DSL) and the source select line (SSL) to turn off the drain select transistor (DST) and the source select transistor (SST). For example, the cut-off voltage can be 0V. The precharge voltage can be higher than 0V and is applied to the bit line during read operations. During verification operations, a verification voltage is used to determine whether the threshold voltage of the selected memory cell has risen to the target level. The verification voltage varies depending on the target level and is applied to the selected word line.

[0026] During a read operation of the selected memory cell, a read voltage is applied to the selected word line. For example, the read voltage may be at various levels depending on the programming method of the selected memory cell. During a programming or read operation, a voltage is applied to the unselected word line in the word line WL to turn on the memory cells connected to the unselected word line. An erase voltage is used during an erase operation to erase the memory cells included in the selected memory block and is applied to the source line SL.

[0027] The row decoder 130 transmits the operating voltage Vop to the drain select line DSL, word line WL, source select line SSL, and source line SL connected to the selected memory blocks according to the row address RADD. For example, the row decoder 130 is connected to the voltage generator 120 via a global line and to memory blocks BLK1 to BLKi via the drain select line DSL, word line WL, source select line SSL, and source line SL.

[0028] Page buffer group 140 includes page buffers (not shown) respectively connected to memory blocks BLK1 to BLKi. Each page buffer is connected to memory blocks BLK1 to BLKi via bit lines BL. During a read operation, the page buffer senses the current or voltage of the bit lines that varies according to the threshold voltage of the selected memory cell in response to the page buffer control signal PBSIG and stores the sensed data.

[0029] The column decoder 150 transmits data between the page buffer group 140 and the input / output circuitry 160 in response to the column address CADD. For example, the column decoder 150 is connected to the page buffer group 140 via the column line CL and transmits an enable signal via the column line CL. The page buffers included in the page buffer group 140 receive or output data via the data line DL in response to the enable signal.

[0030] Input / output circuitry 160 receives or outputs commands (CMD), addresses (ADD), or data via input / output lines (I / O). For example, input / output circuitry 160 transmits commands (CMD) and addresses (ADD) received from an external controller via input / output lines (I / O) to control circuitry 180, and input / output circuitry 160 transmits data received from an external controller via input / output lines (I / O) to page buffer group 140. Alternatively, input / output circuitry 160 outputs data received from page buffer group 140 to an external controller via input / output lines (I / O).

[0031] Control circuit 180 responds to command CMD and address ADD by outputting at least one of the following: opcode OPCD, row address RADD, page buffer control signal PBSIG, or column address CADD. For example, when command CMD input to control circuit 180 corresponds to a programming operation, control circuit 180 controls peripheral circuit 170 to perform a programming operation on the memory block selected by address ADD. When command CMD input to control circuit 180 corresponds to a read operation, control circuit 180 controls peripheral circuit 170 to perform a read operation on the memory block selected by address ADD and output the read data. When command CMD input to control circuit 180 corresponds to an erase operation, control circuit 180 controls peripheral circuit 170 to perform an erase operation on the selected memory block.

[0032] Figure 2 This is an isometric view showing a memory device 100 according to an embodiment of the present disclosure.

[0033] Reference Figure 2 The memory device 100 includes peripheral circuitry PC disposed above the substrate SUB and memory blocks BLK1 to BLKi. Memory blocks BLK1 to BLKi may overlap with the peripheral circuitry PC.

[0034] The substrate SUB can be a single-crystal semiconductor layer. For example, the substrate SUB can be a bulk silicon substrate, a silicon-on-insulator substrate, a germanium substrate, a germanium-on-insulator substrate, a silicon-germanium substrate, or an epitaxial thin film formed by selective epitaxial growth.

[0035] The peripheral circuit PC includes a row decoder 130, a column decoder 150, a page buffer group 140, and a control circuit 180, which control the operation of memory blocks BLK1 to BLKi. For example, the peripheral circuit PC includes one or more NMOS transistors, PMOS transistors, resistors, capacitors, etc., electrically connected to memory blocks BLK1 to BLKi. In this embodiment, the peripheral circuit PC is disposed between the substrate SUB and the memory blocks BLK1 to BLKi.

[0036] Each of the memory blocks BLK1 to BLKi includes a source structure, a bit line, a cell string electrically coupled to the source structure and the bit line, a word line electrically coupled to the cell string, and a select line electrically coupled to the cell string. Each cell string includes memory cells and select transistors coupled in series with a cell plug. Each of the select lines serves as a gate of a corresponding select transistor, and each of the word lines serves as a gate of a corresponding memory cell. Interlayer insulating layers are disposed between the select lines, between the word lines, and between the select lines and the word lines. In the present disclosure, material properties of the interlayer insulating layers may be modified to improve the shape of the cell plugs. Reference is made to Figure 3B describing the material properties of the interlayer insulating layers.

[0037] In an embodiment, the substrate SUB, the peripheral circuit PC, and the memory blocks BLK1 to BLKi may be stacked in an order different from Figure 2 the order shown in the illustration. For example, the peripheral circuit PC may be located over the memory blocks BLK1 to BLKi.

[0038] In an embodiment, the peripheral circuit PC may be located in a region of the substrate SUB that does not overlap with the memory blocks BLK1 to BLKi. For example, the peripheral circuit PC and the memory blocks BLK1 to BLKi may be located in different non-overlapping regions on the substrate SUB.

[0039] Figure 3A is a plan view illustrating a layout of a memory device according to an embodiment of the present disclosure.

[0040] Reference is made to Figure 3A , the a-th memory block BLKa is separated from consecutive memory blocks by a slit structure SI, where 1<a<i and a is a natural number. For example, the slit structure SI separates from the memory block BLKa in the Y direction. Each slit structure SI extends in the X direction. The memory block BLKa may be positioned consecutively with another memory block in the Y direction with the slit structure SI interposed therebetween.

[0041] The memory block BLKa includes a plurality of cell plugs CPL. The cell plugs CPL extend in the vertical direction (Z direction) from the substrate SUB. The cell plugs CPL may be arranged in a plurality of rows. Each row includes cell plugs CPL spaced apart in the X direction. The plurality of rows are spaced apart in the Y direction. The centers of the cell plugs CPL included in odd-numbered rows may be offset from the centers of the cell plugs CPL included in even-numbered rows.

[0042] Each unit plug CPL includes a barrier layer BX, a charge trapping layer CT, a tunneling layer TX, a channel layer CH, and a core post CO. The barrier layer BX may be cylindrical. The charge trapping layer CT contacts the inner surface of the barrier layer BX. The tunneling layer TX contacts the inner surface of the charge trapping layer CT. The channel layer CH contacts the inner surface of the tunneling layer TX. The barrier layer BX, charge trapping layer CT, tunneling layer TX, and channel layer CH may each be cylindrical. The core post CO is disposed within or fills the channel layer CH. For example, the core post CO is located in a region surrounded by the channel layer CH. The core post CO may be cylindrical. Figure 3B As shown, the capping layer CAP of the contact channel layer CH is disposed on the core post CO.

[0043] The barrier layer BX and tunneling layer TX may comprise an oxide layer such as silicon oxide or a oxynitride layer such as silicon oxynitride, or a combination thereof. The charge trapping layer CT may comprise a nitride layer or a variable resistance material. The channel layer CH may comprise an undoped silicon layer or a doped silicon layer. The core pillar CO may comprise an insulating layer or a conductive layer.

[0044] Figure 3B This is a cross-sectional view of a memory device according to an embodiment of the present disclosure. Figure 3B It shows along Figure 3A The cross section intercepted by line A-A'.

[0045] Reference Figure 3B Memory device 100, such as memory block BLKa, includes a stack STK. The stack STK includes alternating layers of interlayer insulating layer IIL and conductive layer CD. The conductive layer CD is alternately stacked with the interlayer insulating layer IIL in the Z direction. The stack STK includes an upper insulating layer UIL. In this example, the upper insulating layer UIL contacts the uppermost conductive layer CD.

[0046] The conductive layer CD corresponds to Figure 1 The drain select line DSL, word line WL, and source select line SSL are shown. The conductive layer CD corresponds to the reference. Figure 2 The selection lines and word lines are described. The conductive layer CD may include at least one of tungsten (W), cobalt (Co), nickel (Ni), molybdenum (Mo), silicon (Si), or polycrystalline silicon (poly-Si).

[0047] The interlayer insulation layer IIL includes a first interlayer insulation layer IIL1, a second interlayer insulation layer IIL2, and a third interlayer insulation layer IIL3. The second interlayer insulation layer IIL2 is disposed above the first interlayer insulation layer IIL1. For example, the lowermost second interlayer insulation layer IIL2 is positioned above the uppermost first interlayer insulation layer IIL1 in the Z-direction. The third interlayer insulation layer IIL3 is disposed above both interlayer insulation layers IIL1 and IIL2. For example, the lowermost third interlayer insulation layer IIL3 is positioned above the uppermost second interlayer insulation layer IIL2 in the Z-direction. The first interlayer insulation layer IIL1 surrounds the lower end of the cell plug CPL, and the third interlayer insulation layer IIL3 surrounds the upper end of the cell plug CPL.

[0048] In an embodiment, the second interlayer insulation layer IIL2 is located at a height corresponding to 70% to 85% of the total height of the laminate STK, measured from the bottom of the laminate STK. For example, when the laminate STK includes 100 interlayer insulation layers IIL, the second interlayer insulation layer IIL2 is located between the 70th and 85th layers. The number of first interlayer insulation layers IIL1 can be greater than the number of second interlayer insulation layers IIL2. The number of first interlayer insulation layers IIL1 can be greater than the number of third interlayer insulation layers IIL3. The number of first interlayer insulation layers IIL1 can be greater than the sum of the number of second interlayer insulation layers IIL2 and the number of third interlayer insulation layers IIL3. The number of second interlayer insulation layers IIL2 can be equal to the number of third interlayer insulation layers IIL3. In embodiments of this disclosure, the number of interlayer insulation layers IIL is equal to the number of interlayer insulation layers IIL.

[0049] In this embodiment, the second interlayer insulation layer IIL2 is located within 70% to 85% of the total height of the laminate STK as measured from the bottom of the laminate STK. For example, the second interlayer insulation layer IIL2 is located at a height corresponding to 75% to 80% of the total height of the laminate STK as measured from the bottom of the laminate STK, or at a height corresponding to 75% to 85% of the total height of the laminate STK.

[0050] In one embodiment, the second interlayer insulation layer IIL2 is located within a range that overlaps with at least a portion of the total height of the laminate STK as measured from the bottom of the laminate STK. For example, the second interlayer insulation layer IIL2 is located at a height corresponding to 65% to 80% of the total height of the laminate STK as measured from the bottom of the laminate STK, a height corresponding to 70% to 90% of the total height of the laminate STK, or a height corresponding to 65% to 90% of the total height of the laminate STK.

[0051] Interlayer insulating layers IIL have different etch rates. The second interlayer insulating layer IIL2 has a lower etch rate than the first interlayer insulating layer IIL1 and the third interlayer insulating layer IIL3. The first etch rate of the first interlayer insulating layer IIL1 is higher than the second etch rate of the second interlayer insulating layer IIL2. The second etch rate of the second interlayer insulating layer IIL2 can be lower than the third etch rate of the third interlayer insulating layer IIL3. The first etch rate can be substantially equal to the third etch rate.

[0052] Various methods can be used to control the etching rate of the interlayer insulating layer IIL. In an embodiment, the density of the second interlayer insulating layer IIL2 can be higher than the density of the first interlayer insulating layer IIL1 and the third interlayer insulating layer IIL3. For example, the interlayer insulating layers IIL can have different densities by utilizing differences in the deposition process of the interlayer insulating layers IIL. During the deposition process of the first interlayer insulating layer IIL1, heat treatment can be performed throughout a first time period, and during the deposition process of the second interlayer insulating layer IIL2, heat treatment can be performed throughout a second time period longer than the first time period. Alternatively, during the deposition process of the first interlayer insulating layer IIL1, heat treatment can be performed at a first temperature, and during the deposition process of the second interlayer insulating layer IIL2, heat treatment can be performed at a second temperature higher than the first temperature.

[0053] In an implementation, the second interlayer insulating layer IIL2 may contain fewer defects than the first interlayer insulating layer IIL1 and the third interlayer insulating layer IIL3. For example, various processes such as plasma treatment, rapid temperature changes, or application of mechanical strain may be performed during the formation of interlayer insulating layers IIL1 and IIL3. During the formation of the second interlayer insulating layer IIL2, the described processes are not performed or may be performed to a lesser extent compared to interlayer insulating layers IIL1 and IIL3.

[0054] In one embodiment, the impurity concentration in the second interlayer insulating layer IIL2 is higher than the impurity concentration in the interlayer insulating layers IIL1 and IIL3. For example, impurities are not implanted into the interlayer insulating layers IIL1 and IIL3, but are implanted into the second interlayer insulating layer IIL2. The impurities may include carbon. The impurities can be implanted into the second interlayer insulating layer IIL2 by a doping process or an implantation process. In another example, impurities are implanted into the interlayer insulating layers IIL1 to IIL3, and the impurity concentration in the second interlayer insulating layer IIL2 is higher than the impurity concentration in the interlayer insulating layers IIL1 and IIL3. In yet another example, impurities are implanted into the interlayer insulating layers IIL1 to IIL3, and the types of impurities in the interlayer insulating layers IIL1 and IIL3 are different from the types of impurities in the second interlayer insulating layer IIL2.

[0055] Various methods can be used to make the second interlayer insulating layer IIL2 have a lower etch rate than the interlayer insulating layers IIL1 and IIL3.

[0056] The interlayer insulating layer IIL may include an oxide layer. For example, the interlayer insulating layer IIL may include a silicon oxide layer. The upper insulating layer UIL may include a material that is the same as or similar to at least a portion of the interlayer insulating layer IIL. For example, the upper insulating layer UIL may include a silicon oxide layer.

[0057] Memory device 100 (e.g., the a-th memory block BLKa) may include a cell plug CPL. The cell plug CPL may extend in a vertical direction (e.g., the Z-direction) within the stack-up STK. The cell plug CPL may penetrate the stack-up STK. For example, the cell plug CPL may be located in a first opening OP1 extending through the stack-up STK. (See reference...) Figure 1 and Figure 2 The memory cell or selection transistor described can be formed at the intersection of the cell plug CPL and the conductive layer CD.

[0058] The unit plug CPL includes a barrier layer BX, a charge trapping layer CT, a tunneling layer TX, a channel layer CH, a core post CO, and a capping layer CAP. The barrier layer BX, charge trapping layer CT, tunneling layer TX, and channel layer CH extend through the stack STK. The barrier layer BX, charge trapping layer CT, tunneling layer TX, and channel layer CH can have a cylindrical shape. The core post CO can also have a cylindrical shape. The barrier layer BX, charge trapping layer CT, tunneling layer TX, channel layer CH, and core post CO can extend in the Z direction.

[0059] Barrier layer BX contacts the side surface of stacked layer STK. Barrier layer BX contacts the side surface of conductive layer CD and interlayer insulating layer IIL. Charge trapping layer CT extends above the inner surface of barrier layer BX. Tunneling layer TX extends above the inner surface of charge trapping layer CT. Channel layer CH extends above the inner surface of tunneling layer TX. Core post CO is surrounded by channel layer CH. Core post CO contacts the inner surface of channel layer CH. Capping layer CAP is disposed on core post CO. Capping layer CAP contacts the end of the inner surface of channel layer CH. Capping layer CAP is surrounded by channel layer CH. Capping layer CAP and channel layer CH may comprise similar materials.

[0060] According to this disclosure, some of the interlayer insulating layers IILs included in the laminate STK (such as the second interlayer insulating layer IIL2) comprise a material with a low etch rate. When the interlayer insulating layers IILs have different etch rates, the cell plug CPL may not exhibit an arcuate profile in the Y direction. For example, the cell plug CPL has a first width W1 at a height corresponding to one or more of the first interlayer insulating layers IIL1, a second width W2 at a height corresponding to one or more of the second interlayer insulating layers IIL2, and a third width W3 at a height corresponding to one or more of the third interlayer insulating layers IIL3. The second width W2 may be greater than or equal to the first width W1, and the third width W3 may be greater than or equal to the second width W2. When the second width W2 is greater than the third width W3, the cell plug CPL exhibits an arcuate profile. When the cell plug CPL has a second width W2 that is greater than or equal to the first width W1 and narrower than or equal to the third width W3, the cell plug CPL does not exhibit an arcuate profile. For example, the unit plug CPL according to this disclosure has a cylindrical shape with a constant width along the Z direction or a tapered shape with a width that narrows toward the lower end of the unit plug CPL.

[0061] In the implementation, Figure 3B The stack-up STK shown corresponds to a segment of a memory block formed by two stack-ups. For example, the memory block includes an upper stack-up and a lower stack-up, and Figure 3B The STK in the stack corresponds to the upper or lower stack.

[0062] Figures 4A to 4E This is a cross-sectional view of a memory device formed using a method for manufacturing a memory device according to an embodiment of the present disclosure. Figures 4A to 4E Along during different stages of manufacturing Figure 3A A cross-sectional view taken from line A-A'.

[0063] Reference Figure 4A This forms a preliminary laminate pSTK. The preliminary laminate pSTK includes an interlayer insulating layer IIL and a sacrificial layer SF alternately laminated in the Z direction. The interlayer insulating layer IIL may include an insulating material. For example, the interlayer insulating layer IIL may include an oxide layer such as a silicon oxide layer. The sacrificial layer SF includes a material that can be selectively removed in subsequent processes. Therefore, the sacrificial layer SF includes a material with a different etch selectivity than the interlayer insulating layer IIL. For example, the sacrificial layer SF may include a nitride layer.

[0064] The preliminary laminate pSTK includes a first preliminary laminate pSTK1, a second preliminary laminate pSTK2 built on top of the first preliminary laminate pSTK1, and a third preliminary laminate pSTK3 built on top of the second preliminary laminate pSTK2. The first preliminary laminate pSTK1 includes a first sacrificial layer SF1 and a first interlayer insulating layer IIL1. The first sacrificial layer SF1 is alternately laminated with the first interlayer insulating layer IIL1 in the Z direction. The second preliminary laminate pSTK2 includes a second sacrificial layer SF2 and a second interlayer insulating layer IIL2. The second sacrificial layer SF2 is alternately laminated with the second interlayer insulating layer IIL2 in the Z direction. The third preliminary laminate pSTK3 includes a third sacrificial layer SF3 and a third interlayer insulating layer IIL3. The third sacrificial layer SF3 is alternately laminated with the third interlayer insulating layer IIL3 in the Z direction.

[0065] The etching rate of the second interlayer insulating layer IIL2 is lower than that of the interlayer insulating layers IIL1 and IIL3. The etching rate of the first interlayer insulating layer IIL1 can be substantially equal to that of the third interlayer insulating layer IIL3.

[0066] Various methods can be used to control the etching rate of the interlayer insulating layer IIL. In one embodiment, the density of the second interlayer insulating layer IIL2 is higher than that of the interlayer insulating layers IIL1 and IIL3. For example, the interlayer insulating layers IIL can have different densities by using different deposition processes for them. During the deposition process of the first interlayer insulating layer IIL1, heat treatment is performed for a first time period, and during the deposition process of the second interlayer insulating layer IIL2, heat treatment is performed for a second time period longer than the first time period. Alternatively, during the deposition process of the first interlayer insulating layer IIL1, heat treatment is performed at a first temperature, and during the deposition process of the second interlayer insulating layer IIL2, heat treatment is performed at a second temperature higher than the first temperature.

[0067] In this embodiment, the second interlayer insulating layer IIL2 has fewer defects than the interlayer insulating layers IIL1 and IIL3. For example, defects may be generated during the formation of interlayer insulating layers IIL1 and IIL3 due to plasma processing, rapid temperature changes, or the application of mechanical strain. During the formation of the second interlayer insulating layer IIL2, the described defect-causing processes may be omitted or performed to a lesser extent compared to performing such processes on interlayer insulating layers IIL1 and IIL3.

[0068] In one embodiment, the impurity concentration in the second interlayer insulating layer IIL2 is higher than the impurity concentration in the interlayer insulating layers IIL1 and IIL3. For example, impurities are not implanted into the interlayer insulating layers IIL1 and IIL3, but are implanted into the second interlayer insulating layer IIL2. The impurities may include carbon. The impurities can be implanted into the second interlayer insulating layer IIL2 by a doping process or an implantation process. In another example, impurities are implanted into the interlayer insulating layers IIL1 to IIL3, and the impurity concentration in the second interlayer insulating layer IIL2 is higher than the impurity concentration in the interlayer insulating layers IIL1 and IIL3. In yet another example, impurities are implanted into the interlayer insulating layers IIL1 to IIL3, and the type of impurities implanted into the interlayer insulating layers IIL1 and IIL3 is different from the type of impurities implanted into the second interlayer insulating layer IIL2.

[0069] Various methods can be used to make the second interlayer insulating layer IIL2 have a lower etch rate than the first interlayer insulating layer IIL1 and the third interlayer insulating layer IIL3.

[0070] The etch rate of the second sacrificial layer SF2 can be lower than the etch rates of the first sacrificial layer SF1 and the third sacrificial layer SF3. The etch rate of the first sacrificial layer SF1 can be substantially equal to the etch rate of the third sacrificial layer SF3. To form sacrificial layers SF with different etch rates, the described method is provided as an example of a method for controlling the etch rate of the interlayer insulating layer IIL, and this disclosure is not limited to these examples.

[0071] The position of the second preliminary laminate pSTK2 within the preliminary laminate pSTK (e.g., the range occupied by the second preliminary laminate pSTK2 on the Z-axis) corresponds to the middle to upper section of the preliminary laminate pSTK. For example, the second preliminary laminate pSTK2 may be located at a height corresponding to 70% to 85% of the total height of the preliminary laminate pSTK, measured from the bottom of the preliminary laminate pSTK. For example, when the preliminary laminate pSTK comprises 100 interlayer insulating layers IIL, the second interlayer insulating layer IIL2 is located between layers 70 and 85. When the preliminary laminate pSTK comprises 100 sacrificial layers SF, the second sacrificial layer SF2 is located between layers 70 and 85. The height of the second preliminary laminate pSTK2 in the Z-direction may be shorter than the height of the first preliminary laminate pSTK1. The height of the third preliminary laminate pSTK3 may be less than the height of the first preliminary laminate pSTK1, but may be similar to the height of the second preliminary laminate pSTK2.

[0072] Reference Figure 4AThe lowermost second sacrificial layer SF2 of the second sacrificial layer SF2 is disposed between the uppermost first interlayer insulation layer IIL1 and the lowermost second interlayer insulation layer IIL2, and the uppermost second sacrificial layer SF2 of the second sacrificial layer SF2 is disposed between the uppermost second interlayer insulation layer IIL2 and the lowermost third interlayer insulation layer IIL3. In an alternative embodiment, with Figure 4A The configuration shown is different; the second sacrificial layer SF2 can be disposed between the second interlayer insulation layers IIL2 and may not contact the first interlayer insulation layer IIL1 or the third interlayer insulation layer IIL3.

[0073] Reference Figure 4B A first opening OP1 is formed extending through the preliminary laminate pSTK. The first opening OP1 extends through the sacrificial layer SF and the interlayer insulating layer IIL of the preliminary laminate pSTK. The first opening OP1 extends in the Z direction. The first opening OP1 extends through the first preliminary laminate pSTK1, the second preliminary laminate pSTK2, and the third preliminary laminate pSTK3. The first opening OP1 has a first width W1 in the first preliminary laminate pSTK1, a second width W2 in the second preliminary laminate pSTK2, and a third width W3 in the third preliminary laminate pSTK3. The first width W1 may be narrower than or equal to the second width W2, and the third width W3 may be greater than or equal to the second width W2.

[0074] An anisotropic dry etching process can be performed to form a first opening OP1 extending through the initial stack pSTK. During the anisotropic dry etching process, interlayer insulating layers IIL1 to IIL3 and sacrificial layers SF1 to SF3 can be etched.

[0075] In an embodiment, the position of the second preliminary laminate pSTK2 within the preliminary laminate pSTK is determined by the etching process that forms the first opening OP1, such as the range occupied by the second preliminary laminate pSTK2 along the Z-axis. For example, the position of the second preliminary laminate pSTK2 can be determined based on the activation energy of the etchant used to etch the first opening OP1, which varies with the depth within the preliminary laminate pSTK. Relative to the total height of the preliminary laminate pSTK, the second preliminary laminate pSTK2 lies within a range where the activation energy of the etchant used to etch the preliminary laminate pSTK is equal to or greater than a threshold. For example, the etchant may have an activation energy greater than or equal to the threshold at a depth corresponding to 15% to 30% of the top of the preliminary laminate pSTK. In this disclosure, the threshold may be a reference value determined during the manufacturing process of the memory device 100.

[0076] According to an embodiment, the second preliminary stack pSTK2 is positioned at a depth corresponding to 15% to 30% of the height of the preliminary stack pSTK, from the top of the preliminary stack pSTK, at which the activation energy of the etchant is greater than or equal to a threshold. Because the second preliminary stack pSTK2 has a lower etch rate than the first preliminary stack pSTK1 and the third preliminary stack pSTK3, the width of the first opening OP1 may not be excessively extended even when the activation energy of the etchant is high. For example, when the etch rates of the preliminary stacks pSTK1 to pSTK3 are equal, the preliminary stack pSTK may be over-etched at a depth corresponding to 15% to 30% from the top of the preliminary stack pSTK, thereby causing the first opening OP1 to exhibit an arcuate profile. According to this disclosure, the first opening OP1 without an arcuate profile can be formed by forming the second preliminary stack pSTK2 at a low etch rate.

[0077] Reference Figure 4C Cell plugs (CPL) are formed in the first opening (OP1). Barrier layer (BX), charge trapping layer (CT), tunneling layer (TX), and channel layer (CH) are sequentially deposited on the side surfaces of the sacrificial layer (SF) and interlayer insulation layer (IIL) of the preliminary stack pSTK exposed through the first opening (OP1). Core post (CO) and capping layer (CAP) are surrounded by the channel layer (CH).

[0078] The unit plug CPL extends through the initial laminate pSTK1 to pSTK3. In one embodiment, the unit plug CPL is formed in the initial laminate pSTK with a constant width along the Z direction. In another embodiment, the unit plug CPL has a tapered shape, and its width increases in the Z direction from the bottom of the unit plug CPL toward the top of the unit plug. In yet another embodiment, the unit plug CPL does not exhibit an arcuate profile.

[0079] Reference Figure 4D The sacrificial layer SF is removed, thereby forming a groove RC between the interlayer insulating layers IIL. For example, a slit extending through the initial laminate pSTK1 to pSTK3 is formed, and the sacrificial layers SF1 to SF3 are removed through the slit. When the sacrificial layer SF is removed, the groove RC is formed between the interlayer insulating layers IIL. The cell plug CPL supports the spaced interlayer insulating layers IIL.

[0080] Reference Figure 4E A conductive layer CD is formed between the interlayer insulating layers IIL, thereby forming a laminate STK. The conductive layer CD is formed in the groove RC created by removing the sacrificial layers SF1 to SF3. The conductive layer CD may include a conductive material.

[0081] Figure 5A and Figure 5B This is a cross-sectional view of a memory device according to an embodiment of the present disclosure.

[0082] Reference Figure 5A and Figure 5B Such as Figure 3A The storage block BLKa includes a contact CTT. The contact CTT is connected to the conductive layer CD. Each contact CTT contacts its corresponding conductive layer CD.

[0083] Reference Figure 5A The stacked component STK can be formed as a stepless structure. A contact CTT extends through the conductive layer CD. A spacer SP is formed on the side surface of the contact CTT. The spacer SP insulates the contact CTT from the conductive layer CD. For example, a first contact CTT contacts a corresponding conductive layer CD within the conductive layer CD, and the first contact CTT extends through other conductive layers CD located above the corresponding conductive layer CD within the conductive layer CD. The spacer SP is located between the first contact CTT and the other conductive layers CD.

[0084] Reference Figure 5B The stacked component STK can be formed with a stepped structure. The upper insulating layer UIL covers the stepped structure. The contact CTT extends through the upper insulating layer UIL and contacts the conductive layer CD. When the stacked component STK has a stepped structure, the contact CTT does not extend through the conductive layer CD.

[0085] Reference Figure 5A and Figure 5B A dummy laminate DSTK is formed on one side of the laminate STK in the horizontal direction. The dummy laminate DSTK includes interlayer insulation layers IIL1 to IIL3 and sacrificial layers SF1 to SF3. Figure 5A and Figure 5B Interlayer insulation layers IIL1 to IIL3 and sacrificial layers SF1 to SF3 correspond to the reference. Figure 3B , Figure 4A and Figure 4B Interlayer insulating layers IIL1 to IIL3 and sacrificial layers SF1 to SF3 are described. The second interlayer insulating layer IIL2 has a lower etch rate than interlayer insulating layers IIL1 and IIL3. The second sacrificial layer SF2 has a lower etch rate than sacrificial layers SF1 and SF3. Interlayer insulating layers IIL1 to IIL3 included in the dummy stack DSTK are referred to as dummy insulating layers.

[0086] The peripheral circuit contact PCT extends through the dummy laminate DSTK. The peripheral circuit contact PCT extends through interlayer insulation layers IIL1 to IIL3 and sacrificial layers SF1 to SF3. (Example) Figure 2As shown, the peripheral circuit contact PCT is connected to the peripheral circuit PC located below the stack-up STK and the dummy stack-up DSTK. The peripheral circuit contact PCT may not have an arcuate profile. For example, the peripheral circuit contact PCT has a constant width along the Z direction. In another example, the peripheral circuit contact PCT has a tapered shape, and its width increases in the Z direction from the bottom of the peripheral circuit contact PCT toward the top of the peripheral circuit contact PCT.

[0087] An isolation structure IS is positioned between the stacked component STK and the dummy stacked component DSTK. The isolation structure IS separates the stacked component STK from the dummy stacked component DSTK. For example, the isolation structure IS surrounds the dummy stacked component DSTK.

[0088] Reference Figure 5A , Figure 5B and Figure 4D An isolation structure IS extending through the initial laminate pSTK can be formed before removing the sacrificial layers SF1 to SF3 of the initial laminate pSTK. When removing the sacrificial layers SF1 to SF3 of the initial laminate pSTK, the portion of the sacrificial layers SF1 to SF3 surrounded by the isolation structure IS may not be removed. The unremoved and thus retained portions of the sacrificial layers SF1 to SF3 form the dummy laminate DSTK.

[0089] Figure 6 This is a diagram illustrating a memory card system 3000 including a memory device 3200 according to an embodiment of the present disclosure.

[0090] Reference Figure 6 The memory card system 3000 includes a controller 3100, a memory device 3200, and a connector 3300.

[0091] Controller 3100 is coupled to memory device 3200. Controller 3100 is configured to access memory device 3200. For example, controller 3100 is configured to control programming operations, read operations, erase operations, and background operations of memory device 3200. Controller 3100 is configured to provide an interface between memory device 3200 and a host. Controller 3100 is configured to run firmware to control memory device 3200. For example, controller 3100 may include components such as random access memory (RAM), a processing unit, a host interface, a memory interface, and error correction components.

[0092] Controller 3100 communicates with external devices via connector 3300. Controller 3100 communicates with external devices, such as a host, based on communication protocols. For example, controller 3100 is configured to communicate with external devices via at least one communication protocol such as: Universal Serial Bus (USB), Multimedia Card (MMC), Embedded MMC (eMMC), Peripheral Component Interconnect (PCI), Fast PCI (PCI-E), Advanced Technology Attachment (ATA), Serial ATA, Parallel ATA, Small Computer System Interface (SCSI), Enhanced Small Disk Interface (ESDI), Integrated Drive Electronics (IDE), FireWire, Universal Flash Memory (UFS), Wi-Fi, Bluetooth, or High-Speed ​​Non-Volatile Memory (NVMe). For example, connector 3300 is configured according to at least one of these communication protocols.

[0093] Memory device 3200 includes multiple memory cells and can be similar to Figures 1 to 5B The memory device 100 illustrated herein is configured.

[0094] The controller 3100 and the memory device 3200 can be integrated into a single semiconductor device to form a memory card. For example, the controller 3100 and the memory device 3200 can be integrated into a single semiconductor device within a memory card such as the Personal Computer Memory Card International Association (PCMCIA), Compact Flash (CF) cards, Smart Media Cards (SM, SMC), Memory Sticks, Multimedia Cards (MMC, RS-MMC, MMCmicro, eMMC), SD cards (SD, Mini SD, Micro SD, SDHC), Universal Flash Memory (UFS), etc.

[0095] Figure 7 This is a block diagram illustrating a solid-state drive (SSD) system 4000 including a memory device according to an embodiment of the present disclosure.

[0096] Reference Figure 7 The SSD system 4000 includes a host 4100 and an SSD 4200. The SSD 4200 exchanges signals with the host 4100 through a signal connector 4001, and the SSD 4200 receives power through a power connector 4002. The SSD 4200 includes a controller 4210, a plurality of memory devices 4221 to 422n, an auxiliary power supply 4230, and a cache memory 4240.

[0097] Controller 4210 controls multiple memory devices 4221 to 422n in response to signals received from host 4100. For example, the signals are based on the interface between host 4100 and SSD 4200. For example, the signals may include at least one interface such as: Universal Serial Bus (USB), Multimedia Card (MMC), Embedded MMC (eMMC), Peripheral Component Interconnect (PCI), Fast PCI (PCI-E), Advanced Technology Attachment (ATA), Serial ATA, Parallel ATA, Small Computer System Interface (SCSI), Enhanced Small Disk Interface (ESDI), Integrated Drive Electronics (IDE), FireWire, Universal Flash Memory (UFS), Wi-Fi, Bluetooth, High-Speed ​​Non-Volatile Memory (NVMe), etc.

[0098] The plurality of memory devices 4221 to 422n include a plurality of memory cells configured to store data. Each of the plurality of memory devices 4221 to 422n may be similar to Figures 1 to 5B The memory device 100 shown is configured. Multiple memory devices 4221 to 422n communicate with the controller 4210 via channels CH1 to CHn.

[0099] Auxiliary power supply 4230 is connected to host 4100 via power connector 4002. Auxiliary power supply 4230 receives power from host 4100 and is rechargeable. When the power supply from host 4100 is unstable or inconsistent, auxiliary power supply 4230 can provide power to SSD 4200. Auxiliary power supply 4230 may be located inside or outside SSD 4200. For example, auxiliary power supply 4230 may be located on the motherboard and can provide auxiliary power to SSD 4200.

[0100] Buffer memory 4240 serves as a buffer for SSD 4200. For example, buffer memory 4240 stores data received from host 4100 or from multiple memory devices 4221 to 422n, or buffer memory 4240 stores metadata such as a mapping table for memory devices 4221 to 422n. Buffer memory 4240 may include volatile memory such as DRAM, SDRAM, DDR SDRAM, or LPDDR SDRAM, or non-volatile memory such as FRAM, ReRAM, STT-MRAM, or PRAM.

[0101] According to this disclosure, the shape of the cell plug can be improved and the quality of the memory device can be enhanced by diversifying the properties of the material layers included in the laminate.

[0102] The concepts have been disclosed in conjunction with examples and embodiments. Those skilled in the art will understand that various modifications, additions, combinations, and substitutions are possible without departing from the scope and technical concepts of this disclosure. The embodiments disclosed in this specification should be considered from an illustrative rather than a restrictive perspective. Therefore, the scope of this disclosure is not limited to these descriptions. All changes within the meaning and scope of equivalents of the claims are included within its scope.

[0103] Cross-references to related applications

[0104] This application claims priority to Korean Patent Application No. 10-2025-0062488, filed on May 14, 2025, with the Korean Intellectual Property Office, the entire contents of which are incorporated herein by reference.

Claims

1. A memory device, the memory device comprising: A laminate, the laminate comprising alternating layers of interlayer insulating layers and conductive layers; as well as Unit plug, the unit plug extending through the stack; The interlayer insulation layer includes: A first interlayer insulating layer, the first interlayer insulating layer having a first etch rate; and A second interlayer insulating layer has a second etch rate lower than the first etch rate.

2. The memory device according to claim 1, wherein, The second interlayer insulation layer is disposed above the first interlayer insulation layer.

3. The memory device according to claim 1, wherein, The lowest second interlayer insulation layer in the second interlayer insulation layer is disposed above the highest first interlayer insulation layer in the first interlayer insulation layer.

4. The memory device according to claim 1, wherein, The interlayer insulation layer further includes a third interlayer insulation layer located above the first interlayer insulation layer and the second interlayer insulation layer; and The second etch rate is lower than the third etch rate of the third interlayer insulating layer.

5. The memory device according to claim 4, wherein, The lowest third interlayer insulation layer is disposed above the highest second interlayer insulation layer in the second interlayer insulation layer.

6. The memory device according to claim 4, wherein, The first etch rate is substantially equal to the third etch rate.

7. The memory device according to claim 4, wherein, The first interlayer insulation layer surrounds the first end of the unit plug; and The third interlayer insulation layer surrounds the second end of the unit plug.

8. The memory device according to claim 4, wherein, The number of the first interlayer insulating layers is greater than the number of the second interlayer insulating layers; and The number of the first interlayer insulation layers is greater than the number of the third interlayer insulation layers.

9. The memory device according to claim 4, wherein, The number of the first interlayer insulation layer is greater than the sum of the number of the second interlayer insulation layer and the number of the third interlayer insulation layer.

10. The memory device according to claim 4, wherein, The number of the second interlayer insulation layers is equal to the number of the third interlayer insulation layers.

11. The memory device according to claim 4, wherein, The unit plug has a first width at a height corresponding to one or more of the first interlayer insulation layers; Wherein, at a height corresponding to one or more of the second interlayer insulating layers, the unit plug has a second width; Wherein, at a height corresponding to one or more of the third interlayer insulating layers, the unit plug has a third width; Wherein, the second width is greater than or equal to the first width; and The third width is greater than or equal to the second width.

12. The memory device according to claim 1, wherein, The second interlayer insulation layer is disposed at a height of 70% to 85% of the height of the laminate.

13. The memory device according to claim 1, wherein, The density of the second interlayer insulation layer is higher than that of the first interlayer insulation layer.

14. The memory device according to claim 1, wherein, The defects included in the second interlayer insulation layer are fewer than the defects included in the first interlayer insulation layer.

15. The memory device according to claim 1, wherein, The concentration of impurities in the second interlayer insulation layer is higher than the concentration of impurities in the first interlayer insulation layer.

16. The memory device of claim 1, wherein the memory device further comprises a contact coupled to the conductive layer.

17. The memory device of claim 1, further comprising: A dummy stacked component is arranged horizontally relative to the stacked component; as well as Peripheral circuit contacts that extend through the dummy stack.

18. The memory device according to claim 17, wherein, The virtual stack-up component includes: The first dummy insulation layer corresponds to the first interlayer insulation layer; The second dummy insulation layer corresponds to the second interlayer insulation layer; A first sacrificial layer, the first sacrificial layer being in contact with the first dummy insulating layer; and A second sacrificial layer is in contact with the second dummy insulating layer; and The etching rate of the second sacrificial layer is lower than that of the first sacrificial layer.

19. The memory device according to claim 18, wherein, The dummy stack-up further includes: A third dummy insulating layer, wherein the third dummy insulating layer is located above the first dummy insulating layer and the second dummy insulating layer; and The third sacrificial layer is in contact with the third dummy insulating layer, and The etching rate of the second sacrificial layer is lower than that of the third sacrificial layer.

20. A method of manufacturing a memory device, the method comprising the steps of: Laminated components are formed by alternately stacking sacrificial layers and interlayer insulating layers; as well as Forming a unit plug that extends through the laminate; The interlayer insulation layer includes: A first interlayer insulating layer, the first interlayer insulating layer having a first etch rate; and A second interlayer insulating layer has a second etch rate lower than the first etch rate.

21. The method according to claim 20, wherein, The steps for forming the laminated component include the following: The first laminate is formed by alternately stacking the first sacrificial layer and the first interlayer insulating layer; A second laminate is formed on top of the first laminate by alternately laminating a second sacrificial layer and a second interlayer insulating layer; and A third laminate is formed on top of the second laminate by alternately laminating a third sacrificial layer and a third interlayer insulating layer; and The second etch rate is lower than the third etch rate of the third interlayer insulating layer.

22. The method according to claim 21, wherein, The first etch rate is substantially equal to the third etch rate.

23. The method according to claim 21, wherein, The height of the second layer is shorter than the height of the first layer.

24. The method according to claim 21, wherein, The height of the third layer is shorter than the height of the first layer and is substantially equal to the height of the second layer.

25. The method according to claim 21, wherein, The second laminate is formed at a height of 70% to 85% of the height of the laminate, measured from the bottom of the laminate.

26. The method according to claim 21, wherein, The etch rate of the second sacrificial layer is lower than that of the first sacrificial layer and also lower than that of the third sacrificial layer.

27. The method of claim 21, further comprising the following steps: Forming a slit that extends through the first laminate, the second laminate, and the third laminate; A groove is formed by removing the first sacrificial layer, the second sacrificial layer, and the third sacrificial layer via the slit; and A conductive layer is formed in the groove.

28. The method of claim 27, the method further comprising forming an isolation structure extending through the first laminate, the second laminate, and the third laminate; in, When the first sacrificial layer, the second sacrificial layer, and the third sacrificial layer are removed, the sections of the first sacrificial layer, the second sacrificial layer, and the third sacrificial layer surrounded by the isolation structure are not removed.

29. The method of claim 20, further comprising the following steps: The first interlayer insulation layer is subjected to heat treatment during the first time period; and During a second time period longer than the first time period, the second interlayer insulation layer is subjected to heat treatment.

30. The method of claim 20, further comprising the following steps: Defects are generated in the first interlayer insulation layer; as well as Defects are generated in the second interlayer insulation layer; The defects included in the second interlayer insulation layer are fewer than the defects included in the first interlayer insulation layer.

31. The method according to claim 20, further comprising the following steps: Impurities are injected into the first interlayer insulating layer; as well as The impurities are injected into the second interlayer insulating layer; The concentration of impurities in the second interlayer insulation layer is higher than the concentration of impurities in the first interlayer insulation layer.

32. A memory device, the memory device comprising: A unit stack comprising alternating layers of interlayer insulating layers and conductive layers; A unit plug extending through the unit stack; A dummy laminate is disposed on the side of the unit laminate and includes alternately stacked dummy insulating layers and sacrificial layers; as well as Peripheral circuit contact, the peripheral circuit contact extending through the dummy stack; The sacrificial layer includes: The first layer of sacrifice; and A second sacrificial layer has an etch rate that is lower than that of the first sacrificial layer.

33. The memory device according to claim 32, wherein, The interlayer insulation layer includes: First interlayer insulation layer; and A second interlayer insulating layer has an etch rate that is lower than that of the first interlayer insulating layer.

34. The memory device according to claim 33, wherein, The dummy insulation layer includes: The first dummy insulating layer; and The second dummy insulating layer has an etch rate that is lower than that of the first dummy insulating layer.

35. The memory device according to claim 34, wherein, The first dummy insulating layer is disposed in a first direction relative to the first interlayer insulating layer; and The second dummy insulating layer is disposed in the first direction relative to the second interlayer insulating layer.

36. The memory device according to claim 32, wherein, The sacrificial layer is disposed relative to the conductive layer in a first direction.

37. The memory device according to claim 32, wherein, The density of the second sacrificial layer is higher than that of the first sacrificial layer.

38. The memory device according to claim 32, wherein, The number of defects in the second sacrificial layer is less than the number of defects in the first sacrificial layer.

39. The memory device according to claim 32, wherein, The concentration of impurities in the second sacrificial layer is higher than that in the first sacrificial layer.

Citation Information

Patent Citations

  • Pharmacokinetics analysis method using multi-organ on a chip

    KR1020250062488A