Perovskite photovoltaic modules and their encapsulation methods, electronic devices
By using a filler material with a low coefficient of thermal expansion in the encapsulation layer to bond tightly with the encapsulation material, the problems of bubbles and delamination in perovskite photovoltaic modules during alternating hot and cold processes are solved, thus improving the stability of the modules.
Patent Information
- Application Number
- CN202510585886.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-05-08
- Publication Date
- 2026-11-17
AI Technical Summary
Perovskite photovoltaic modules are prone to developing bubbles and cell delamination during the alternating hot and cold aging process, leading to reduced stability.
Adding a filler material with a low coefficient of thermal expansion to the encapsulation layer reduces the overall coefficient of thermal expansion of the encapsulation layer. Through the tight bonding between the filler material and the encapsulation material, the interlayer stress caused by temperature changes is reduced.
This effectively reduces the probability of internal bubbles and cell layer delamination in perovskite photovoltaic modules, thus improving module stability.
Smart Images

Figure CN123124579A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of perovskite photovoltaic cell technology, and particularly to a perovskite photovoltaic module and its packaging method and electronic equipment. Background Technology
[0002] Perovskite photovoltaic (PV) modules have attracted much attention due to their high photoelectric conversion efficiency and good low-light performance. During manufacturing, perovskite PV modules require encapsulation to prevent water and oxygen intrusion. Currently, encapsulation of perovskite PV modules involves placing POE (polyolefin elastomer) between the cell layer and the protective layer, and applying butyl rubber around the perimeter of the perovskite PV cells. The perovskite PV modules are then hot-pressed in a laminator and cooled in air to obtain the encapsulated modules. However, during use, it has been found that perovskite PV modules are prone to internal air bubbles during alternating hot and cold aging processes, leading to reduced stability. Summary of the Invention
[0003] The main objective of this invention is to provide a perovskite photovoltaic module and its encapsulation method and electronic device, which aims to reduce the probability of bubbles appearing inside the perovskite photovoltaic module.
[0004] To achieve the above objectives, the present invention proposes a perovskite photovoltaic module, comprising: Base; A battery layer is disposed on the substrate; An encapsulation layer is disposed on the battery layer; A protective layer is disposed on the encapsulation layer; A sealing material is disposed between the protective layer and the substrate, and connects the protective layer and the substrate respectively. The substrate, the protective layer, and the sealing material enclose a sealed space, and the battery layer and the encapsulation layer are located within the sealed space. The encapsulation layer includes an encapsulation material and a filler material, wherein the encapsulation material and the filler material are tightly bonded together, and the coefficient of thermal expansion of the filler material is less than that of the encapsulation material.
[0005] In some embodiments of the present invention, the coefficient of thermal expansion of the filler material is less than or equal to 35 × 10⁻⁶. -6 / K.
[0006] In some embodiments of the present invention, the encapsulation material and the filling material are stacked, and the filling material has a plurality of pores.
[0007] In some embodiments of the present invention, the filling material is one of the following: metal mesh, cotton cloth, non-woven fabric, Kevlar fiber cloth, melamine sponge, alumina aerogel, and titanium dioxide aerogel.
[0008] In some embodiments of the present invention, the filler material is fibrous or granular; The encapsulation material is a curable solution; The encapsulation material and the filler material are mixed and cured together.
[0009] In some embodiments of the present invention, the encapsulation material is one of photocurable adhesive and thermocurable adhesive; The filling material is one or more of the following: carbon fiber, metal fiber, glass fiber, aluminum silicate fiber, PBO fiber, polytetrafluoroethylene fiber, polyoxymethylene fiber, polyphenylene sulfide fiber, polyetheretherketone fiber, polyaryletherketone fiber, polycarbonate fiber, and polyimide fiber; or the filling material is one or more of the following: carbon black powder, silicon oxide powder, aluminum oxide powder, silicon carbide powder, calcium carbonate powder, titanium oxide powder, cerium oxide powder, zirconium oxide powder, and iron oxide powder.
[0010] In some embodiments of the present invention, the sealing material is glass powder, the substrate and the protective layer are both made of glass, and the sealing material is connected to the substrate and the protective layer respectively by laser welding.
[0011] In some embodiments of the present invention, the sealing material is one of polyisoprene, polyolefin encapsulant, epoxy encapsulant, silicone encapsulant, and polyurethane encapsulant, ultraviolet light curing encapsulant, and infrared light curing encapsulant. And / or, the encapsulation material is one of the following: co-extruded POE film, polydimethylsiloxane, polyvinyl butyral, thermoplastic polyurethane, polyvinyl fluoride terpolymer, UV epoxy adhesive, and silicone.
[0012] This invention also proposes a method for encapsulating perovskite photovoltaic modules, the encapsulation method comprising the following steps: S1. Lay the sealing material around the battery layer on the substrate; S2. Lay the encapsulation material onto the battery layer; S3. Lay the filler material on the encapsulation material; S4. Cover the encapsulation material with the protective layer; S5. Select a packaging process based on the packaging material and perform packaging.
[0013] In some embodiments of the present invention, in step S5, if the encapsulation material is a thermoplastic film, the perovskite photovoltaic module is placed in a laminator for hot-press encapsulation. If the encapsulation material is a photocurable adhesive, the perovskite photovoltaic module is placed under an ultraviolet lamp or an infrared lamp for curing and encapsulation. If the encapsulation material is a thermosetting adhesive, the perovskite photovoltaic module shall be stored in an environment of 25°C to 120°C for 0.25h to 72h.
[0014] The present invention also proposes an electronic device comprising an electronic device and a perovskite photovoltaic module as described above, wherein the electronic device and the perovskite photovoltaic module are electrically connected.
[0015] The reagents and raw materials used in this invention are all commercially available.
[0016] In the technical solution of this invention, by adding a filler material with a low coefficient of thermal expansion to the encapsulation layer, the overall coefficient of thermal expansion of the encapsulation layer is reduced, thereby reducing the interlayer stress caused by temperature changes. This reduces the probability of bubbles appearing inside the perovskite photovoltaic module and the probability of delamination of the stacked cell layers, thereby improving the stability of the perovskite photovoltaic module. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0018] Figure 1 This is a schematic diagram of the structure of an embodiment of the perovskite photovoltaic module provided by the present invention; Figure 2 This is a structural schematic diagram of a perovskite photovoltaic module cross-section; Figure 3 This is an exploded view of the encapsulation layer; Figure 4 The current decay curves for wet freeze (HF) tests in Examples 1 to 5 are shown. Figure 5 The current decay curves for the ultraviolet (UV) aging test in Examples 1 to 5 are shown. Figure 6 This is a current decay curve for the thermal cycling (TC) test. Figure 7 A schematic diagram of the structure of an embodiment of the electronic device provided by the present invention.
[0019] Explanation of icon numbers: 1000, Electronic equipment; 100, Perovskite photovoltaic module; 10, Substrate; 20, Cell layer; 30, Encapsulation layer; 31, Encapsulation material; 32, Filler material; 40, Protective layer; 50, Sealing material; 100a, Sealed space; 300, Electronic device.
[0020] The realization of the objective, functional features and advantages of the present invention will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation
[0021] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.
[0022] It should be noted that if the embodiments of the present invention involve directional indicators (such as up, down, left, right, front, back, etc.), the directional indicators are only used to explain the relative positional relationship and movement of the components in a specific posture. If the specific posture changes, the directional indicators will also change accordingly.
[0023] Furthermore, if the embodiments of this invention involve descriptions such as "first" or "second," these descriptions are for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with "first" or "second" may explicitly or implicitly include at least one of those features. Additionally, the use of "and / or" or "and / or" throughout the text includes three parallel solutions. For example, "A and / or B" includes solution A, solution B, or a solution where both A and B are satisfied simultaneously. Furthermore, the technical solutions of the various embodiments can be combined with each other, but this must be based on the ability of those skilled in the art to implement them. When the combination of technical solutions is contradictory or impossible to implement, it should be considered that such a combination of technical solutions does not exist and is not within the scope of protection claimed by this invention.
[0024] Encapsulation is one of the key technologies for improving the stability of perovskite solar cells. Traditional perovskite encapsulation methods typically use POE (polyolefin elastomer) combined with a glass layer. However, after the perovskite photovoltaic module is hot-pressed in a laminator, POE is prone to accumulating thermal stress during the cooling process. Simultaneously, due to the difference in the coefficient of thermal expansion between POE and the sealing material, bubbles can easily form in the perovskite module during alternating hot and cold cycles, leading to delamination of the cell layers. Therefore, developing a novel perovskite photovoltaic module that can reduce thermal stress and improve stability is of great significance.
[0025] This invention proposes a perovskite photovoltaic module, which aims to reduce the probability of bubbles appearing inside the perovskite photovoltaic module or delamination of the stacked cell layers.
[0026] In one embodiment of the present invention, a perovskite photovoltaic module 100 includes a substrate 10, a cell layer 20, an encapsulation layer 30, a protective layer 40, and a sealing material 50. The cell layer 20 is disposed on the substrate 10, the encapsulation layer 30 is disposed on the cell layer 20, and the protective layer 40 is disposed on the encapsulation layer 30. The sealing material 50 is disposed between the protective layer 40 and the substrate 10, and connects the protective layer 40 and the substrate 10 respectively. The substrate 10, the protective layer 40, and the sealing material 50 enclose a sealed space 100a, within which the cell layer 20 and the encapsulation layer 30 are located. The encapsulation layer 30 includes an encapsulation material 31 and a filler material 32, which are tightly bonded together. The coefficient of thermal expansion of the filler material 32 is less than that of the encapsulation material 31.
[0027] Specifically, the substrate 10, serving as the supporting structure of the component, can be glass, transparent plastic, PET (polyethylene terephthalate) film, or other suitable materials. In this embodiment, the substrate 10 is glass, which possesses good mechanical strength and transparency. The battery layer 20 mainly consists of the transparent conductive substrate 10, an electron transport layer, a perovskite layer, a hole transport layer, and metal electrodes. The transparent conductive substrate 10 provides good light transmittance and conductivity and can be FTO (fluorine-doped tin oxide), ITO (indium tin oxide), or other suitable transparent conductive materials. The electron transport layer is used to transport electrons and suppress charge recombination, improving battery efficiency. The perovskite layer, as a light absorption layer, absorbs sunlight and converts it into electrons and holes. The hole transport layer is used to transport holes and prevent the reverse flow of electrons, improving battery performance. The metal electrodes, serving as the contact layer of the battery, are used to collect and transport current. The protective layer 40 provides protection and can be glass, transparent plastic, or other transparent materials. The specific structure of the battery layer 20 can adopt configurations known in the art. This invention does not limit the specific composition of the battery layer 20.
[0028] Understandably, by adding a filler material 32 with a low coefficient of thermal expansion to the encapsulation layer 30, the overall coefficient of thermal expansion of the encapsulation layer 30 is reduced, thereby reducing interlayer stress caused by temperature changes. This can further reduce the probability of bubbles appearing inside the perovskite photovoltaic module 100 and the probability of delamination of the stacked cell layers 20, thereby improving the stability of the perovskite photovoltaic module 100.
[0029] In one embodiment of the present invention, the coefficient of thermal expansion of the filler material 32 is less than or equal to 35 × 10⁻⁶. -6 / K. The coefficient of thermal expansion of the preferred filler material 32 is less than or equal to 35 × 10⁻⁶. -6 / K, to significantly reduce thermal stress. Specifically, the coefficient of thermal expansion is less than or equal to 35 × 10⁻⁶. -6The filler material 32 of / K effectively reduces the overall thermal expansion coefficient of the encapsulation layer 30. During the alternating use of hot and cold perovskite photovoltaic module 100, it can reduce the accumulated thermal stress of the encapsulation layer 30, thereby reducing the probability of bubbles appearing inside the perovskite photovoltaic module 100 and the probability of delamination of the stacked cell layers 20, thus improving the stability of the perovskite photovoltaic module 100.
[0030] In one embodiment of the present invention, an encapsulation material 31 and a filler material 32 are stacked, and the filler material 32 has a plurality of pores. Understandably, by providing pores in the filler material 32, the encapsulation material 31 can penetrate into the pores, thereby reducing the overall coefficient of thermal expansion of the encapsulation layer 30, which in turn reduces interlayer stress caused by temperature changes and helps to enhance the tight bonding between the encapsulation material 31 and the filler material 32. The filler material 32 can be a metal mesh, non-woven fabric, Kevlar fiber cloth, melamine sponge, alumina aerogel, or titanium dioxide aerogel, or other effective porous materials. For example, the filler material 32 is a stainless steel mesh with a coefficient of thermal expansion of approximately 10 × 10⁻⁶. -6 / K; The encapsulation material 31 is POE, with a coefficient of thermal expansion of approximately 100 × 10⁻⁶. -6 / K. During the encapsulation process, POE melts and fills the pores of the stainless steel mesh to form the encapsulation layer 30, thereby reducing the overall coefficient of thermal expansion of the encapsulation layer 30 and helping to enhance the tight bond between the encapsulation material 31 and the filler material 32.
[0031] In one embodiment of the present invention, the filler material 32 is one of the following: metal mesh, cotton cloth, non-woven fabric, Kevlar fiber cloth, melamine sponge, alumina aerogel, and titanium dioxide aerogel. The filler material 32, being one of the above materials, has abundant pores, which facilitates a tight bond between the filler material 32 and the encapsulation material 31.
[0032] In one embodiment of the invention, the filler material 32 is fibrous or granular. The encapsulating material 31 is a curable solution, such as a photocurable adhesive, a thermocurable adhesive, or other effective curable solution. The encapsulating material 31 and the filler material 32 are mixed and cured integrally. It is understood that by mixing and curing the encapsulating material 31 and the filler material 32 to form the encapsulation layer 30, the filler material 32 can penetrate into the encapsulation material 31, thereby effectively reducing the overall coefficient of thermal expansion of the encapsulation layer 30. Furthermore, this method allows the filler material 32 to be fixed within the encapsulation material 31, resulting in a more reliable bond between the encapsulation material 31 and the filler material 32.
[0033] Specifically, the filler material 32 is fibrous and can be carbon fiber, metal fiber, glass fiber, aluminosilicate fiber, or other effective fibrous materials. The filler material 32 is also granular and can be carbon black powder, silicon oxide powder, alumina powder, silicon carbide powder, or other effective particulate materials. The liquid encapsulation material 31 can be... In one embodiment of the present invention, the encapsulation material 31 is one of a photocurable adhesive and a thermocurable adhesive. The filler material 32 is one or more combinations of carbon fiber, metal fiber, glass fiber, aluminum silicate fiber, PBO fiber, polytetrafluoroethylene fiber, polyoxymethylene fiber, polyphenylene sulfide fiber, polyetheretherketone fiber, polyaryletherketone fiber, polycarbonate fiber, and polyimide fiber. It is understood that using the above-mentioned fiber materials as the filler material 32 can improve the mechanical strength of the encapsulation layer 30.
[0034] In one embodiment of the present invention, the encapsulating material 31 is one of a photocurable adhesive and a thermocurable adhesive. The filler material 32 is one or more combinations of carbon black powder, silicon oxide powder, alumina powder, silicon carbide powder, calcium carbonate powder, titanium oxide powder, cerium oxide powder, zirconium oxide powder, and iron oxide powder. Understandably, using the above-mentioned powder materials as filler material 32 can increase the solid content of the liquid encapsulating material 31, improve its mechanical properties, and the addition of powder can fill the voids in the liquid encapsulating material 31, reduce volume shrinkage during curing, and reduce internal stress and warpage.
[0035] It should be noted that the UV-curable adhesive can be an acrylic UV-curable adhesive, a polyurethane UV-curable adhesive, or other effective UV-curable adhesive. The thermosetting adhesive can be an epoxy resin adhesive, a phenolic resin adhesive, or other effective thermosetting adhesive.
[0036] In one embodiment of the present invention, the sealing material 50 is glass powder, and both the substrate 10 and the protective layer 40 are made of glass. The sealing material 50 is connected to the substrate 10 and the protective layer 40 respectively by laser welding. Understandably, the glass powder is melted during the laser welding process, filling the tiny gaps between the substrate 10 and the protective layer 40 to form a dense seal. By using glass powder as the sealing material 50 and connecting the glass substrate 10 and the protective layer 40 using laser welding technology, the reliability of the connection can be improved, and it also has good barrier properties against harmful substances such as water vapor and oxygen, effectively preventing the external environment from corroding the battery layer 20 and improving the stability of the perovskite photovoltaic module 100.
[0037] In one embodiment of the present invention, the sealing material 50 is one of polyisoprene, polyolefin encapsulant, epoxy encapsulant, silicone encapsulant, polyurethane encapsulant, UV-curable encapsulant, and infrared-curable encapsulant. Understandably, using the above-mentioned materials, the sealing material 50 can provide excellent sealing performance, prevent water and oxygen intrusion, and has strong compatibility, enabling it to firmly bond to various substrates and ensuring encapsulation quality.
[0038] In one embodiment of the present invention, the encapsulation material 31 is one of EPE (co-extruded POE film), polydimethylsiloxane, polyvinyl butyral, thermoplastic polyurethane, polyvinyl fluoride terpolymer, UV epoxy adhesive, and silicone. It is understood that the encapsulation material 31, using the above-mentioned materials, is stable and reliable.
[0039] The present invention also proposes a packaging method for a perovskite photovoltaic module 100, the packaging method comprising the following steps: S1. The sealing material 50 is laid around the battery layer 20 on the substrate 10; S2. Lay the encapsulation material 31 on the battery layer 20; S3. Lay the filler material 32 on the encapsulation material 31; S4. Cover the protective layer 40 onto the encapsulation material 31; S5. Select the packaging process according to the packaging material 31 and perform packaging.
[0040] In step S5, if the encapsulation material 31 is a thermoplastic film, the perovskite photovoltaic module 100 is placed in a laminator for hot-press encapsulation; if the encapsulation material 31 is a photocurable adhesive, the perovskite photovoltaic module 100 is placed under an ultraviolet lamp or an infrared lamp for curing and encapsulation; if the encapsulation material 31 is a thermocurable adhesive, the perovskite photovoltaic module 100 is stored in an environment of 25°C to 120°C for 0.25h to 72h.
[0041] Understandably, the perovskite photovoltaic module 100 prepared by the above encapsulation method can reduce the interlayer stress caused by temperature changes, thereby reducing the probability of bubbles appearing inside the perovskite photovoltaic module 100 and the probability of delamination of the stacked cell layers 20, so as to improve the stability of the perovskite photovoltaic module 100.
[0042] The present invention will be further described in detail below with reference to specific embodiments. Example 1
[0043] S1. Prepare a 0.32 cm thick battery layer 20 on the backplate glass; S2. Apply multiple strips of 1cm wide and 0.08cm thick butyl tape to the four sides of the back glass, with the edges of the butyl tape overlapping each other. S3. Apply a 0.06cm thick non-crosslinked POE film to the perovskite photovoltaic module 100, with the edge in contact with the butyl adhesive. Ensure a seamless splicing between the POE and the butyl adhesive. S4. Place a 0.02cm thick cleanroom cloth on top of the POE, with the edge in contact with the butyl adhesive. Make sure the cleanroom cloth and the butyl adhesive are seamlessly joined. S5. Cover with the back glass and use a vacuum laminator to laminate to obtain the encapsulated perovskite photovoltaic module 100. Example 2
[0044] The difference from Example 1 is that step S3 uses a 0.06 cm thick non-crosslinked TPU (Thermoplastic polyurethanes) film, while the rest of the process is the same as in Example 1. Example 3
[0045] The difference from Example 1 is that step S4 uses a 0.25mm thick glass fiber cloth instead of a cleanroom cloth, while the rest of the process is the same as in Example 1. Example 4
[0046] The difference from Example 1 is that step S4 uses 9.5 kg / m 3 The density and thickness of the 1mm melamine sponge were used instead of the cleanroom cloth, and the rest of the process was the same as in Example 1. Example 5
[0047] The difference from Example 1 is that step S4 uses 220g / m 2 The process is the same as in Example 1, except that the Kevlar fiber knitted fabric is used instead of a cleanroom cloth.
[0048] Comparative Example The difference from Example 1 is that step S4 is omitted, while the rest of the process is the same as in Example 1.
[0049] The perovskite photovoltaic modules 100 manufactured according to Comparative Examples, Examples 1, 2, 3, 4, and 5 were subjected to wet freeze test (HF), ultraviolet aging test (UV), and thermal cycling test (TC) according to the IEC 61215:2021 test standard, respectively, to obtain the following results: Figure 4 , Figure 5 , Figure 6 The current decay curves shown are illustrated. The current decay in Examples 1 to 5 is less than that in the comparative example, indicating that the packaging structure has a more stable effect.
[0050] In summary, the encapsulation structure designed in this invention can effectively slow down the aging rate of the perovskite photovoltaic module 100 and has a significant benefit to the long-term stability of the perovskite photovoltaic module 100.
[0051] The present invention also proposes an electronic device 1000, which includes an electronic device 300 and a perovskite photovoltaic module 100, the electronic device 300 and the perovskite photovoltaic module 100 being electrically connected. The specific structure of the perovskite photovoltaic module 100 is as described in the above embodiments. Since the electronic device 1000 adopts all the technical solutions of all the above embodiments, it possesses at least all the beneficial effects brought about by the technical solutions of the above embodiments, which will not be elaborated further here.
[0052] The electronic device 300 may be, but is not limited to, an electronic calculator, an e-book reader, a wearable device, a camera, an electronic scale, etc.
[0053] Understandably, by electrically connecting the electronic device 300 and the perovskite photovoltaic module 100, the perovskite photovoltaic module 100 can supply power to the electronic device 300, thereby allowing the electronic device 1000 to operate without charging or with fewer charging cycles throughout its service life.
[0054] The above description is merely an exemplary embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformations made using the contents of the present invention specification and drawings under the technical concept of the present invention, or direct / indirect applications in other related technical fields, are included within the patent protection scope of the present invention.
Claims
1. A perovskite photovoltaic module, characterized in that, include: Base; A battery layer is disposed on the substrate; An encapsulation layer is disposed on the battery layer; A protective layer is disposed on the encapsulation layer; A sealing material is disposed between the protective layer and the substrate, and connects the protective layer and the substrate respectively. The substrate, the protective layer, and the sealing material enclose a sealed space, and the battery layer and the encapsulation layer are located within the sealed space. The encapsulation layer includes an encapsulation material and a filler material, wherein the encapsulation material and the filler material are tightly bonded together, and the coefficient of thermal expansion of the filler material is less than that of the encapsulation material.
2. The perovskite photovoltaic module as described in claim 1, characterized in that, The coefficient of thermal expansion of the filler material is less than or equal to 35 × 10⁻⁶. -6 / K.
3. The perovskite photovoltaic module as described in claim 1, characterized in that, The encapsulation material and the filling material are stacked, and the filling material has a plurality of pores.
4. The perovskite photovoltaic module as described in claim 3, characterized in that, The filling material is one of the following: metal mesh, cotton cloth, non-woven fabric, Kevlar fiber cloth, melamine sponge, alumina aerogel, and titanium dioxide aerogel.
5. The perovskite photovoltaic module as described in claim 1, characterized in that, The filler material is fibrous or granular; The encapsulation material is a curable solution; The encapsulation material and the filler material are mixed and cured together.
6. The perovskite photovoltaic module as described in claim 5, characterized in that, The encapsulation material is one of photocurable adhesive and thermocurable adhesive; The filling material is one or more of the following: carbon fiber, metal fiber, glass fiber, aluminum silicate fiber, PBO fiber, polytetrafluoroethylene fiber, polyoxymethylene fiber, polyphenylene sulfide fiber, polyetheretherketone fiber, polyaryletherketone fiber, polycarbonate fiber, and polyimide fiber; or the filling material is one or more of the following: carbon black powder, silicon oxide powder, aluminum oxide powder, silicon carbide powder, calcium carbonate powder, titanium oxide powder, cerium oxide powder, zirconium oxide powder, and iron oxide powder.
7. The perovskite photovoltaic module as described in claim 1, characterized in that, The sealing material is glass powder, and both the substrate and the protective layer are made of glass. The sealing material is connected to the substrate and the protective layer respectively by laser welding.
8. The perovskite photovoltaic module as described in claim 1, characterized in that, The sealing material is one of the following: polyisoprene, polyolefin encapsulant, epoxy encapsulant, silicone encapsulant, polyurethane encapsulant, ultraviolet curable encapsulant, and infrared curable encapsulant. And / or, the encapsulation material is one of polydimethylsiloxane, polyvinyl butyral, thermoplastic polyurethane, polyvinyl fluoride terpolymer, UV epoxy adhesive, and silicone.
9. A method for encapsulating a perovskite photovoltaic module as described in any one of claims 1 to 8, characterized in that, The packaging method includes the following steps: S1. Lay the sealing material around the battery layer on the substrate; S2. Lay the encapsulation material onto the battery layer; S3. Lay the filler material on the encapsulation material; S4. Cover the encapsulation material with the protective layer; S5. Select a packaging process based on the packaging material and perform packaging.
10. The packaging method as described in claim 9, characterized in that, In step S5, if the encapsulation material is a thermoplastic film, the perovskite photovoltaic module is placed in a laminator for hot-press encapsulation. If the encapsulation material is a photocurable adhesive, the perovskite photovoltaic module is placed under an ultraviolet lamp or an infrared lamp for curing and encapsulation. If the encapsulation material is a thermosetting adhesive, the perovskite photovoltaic module shall be stored in an environment of 25°C to 120°C for 0.25h to 72h.
11. An electronic device, characterized in that, The electronic device includes an electronic device and a perovskite photovoltaic module as described in any one of claims 1 to 8, wherein the electronic device and the perovskite photovoltaic module are electrically connected.