A plasma-resistant electrostatic chuck and its preparation method
By designing a multi-layer gradient composite structure and a modified ceramic matrix, the corrosion and interlayer cracking problems of electrostatic chucks in high-frequency plasma environments have been solved, resulting in a highly stable and high-precision electrostatic chuck suitable for high-end semiconductor processing equipment.
Patent Information
- Application Number
- CN202611446669.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-17
- Publication Date
- 2026-11-17
AI Technical Summary
Existing electrostatic chucks are prone to surface corrosion, grain shedding, and roughness deterioration under high-frequency, high-energy plasma bombardment and corrosive process gas environments. Poor matching between electrode structure and insulating transition layer leads to interlayer cracking and delamination. Furthermore, traditional fabrication processes lack sufficient density, failing to meet the high corrosion resistance, high stability, and high precision requirements of high-end semiconductor equipment.
The structure employs a multi-layer gradient composite structure, including a metal base, an insulating transition layer, an internal electrode layer, a ceramic substrate layer, and a corrosion-resistant protective surface layer. By using a doped modified alumina ceramic substrate and a dense amorphous alumina-silicon nitride composite film, combined with a patterned molybdenum electrode and a cooling channel design, the resistance to plasma bombardment and structural stability are enhanced.
It significantly improves the electrostatic chuck's resistance to plasma corrosion and its service life, ensures wafer temperature uniformity and adsorption stability, meets the needs of high-end semiconductor processing, and is suitable for mass production.
Smart Images

Figure CN123124739A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of semiconductor processing equipment technology, and more specifically, relates to a plasma corrosion resistant electrostatic chuck and its preparation method. Background Technology
[0002] Electrostatic chucks are core carrier components in plasma processing technologies such as semiconductor etching and thin film deposition. They are mainly used for electrostatic adsorption, fixation, temperature control, and gas backblowing support of wafers in a vacuum environment. Their performance directly determines the precision, yield, and equipment lifespan of semiconductor wafer processing.
[0003] Currently, commercial electrostatic chucks generally use conventional alumina ceramic as the substrate material, resulting in a simple surface protection structure. Under high-frequency, high-energy plasma bombardment and corrosive process gas atmospheres, they are highly susceptible to surface corrosion, grain shedding, and roughness degradation. This not only causes wafer surface contamination and reduced adsorption stability but also significantly shortens the chuck's lifespan and increases equipment maintenance costs. Furthermore, the electrode structure and insulating transition layer of existing electrostatic chucks have poor compatibility with the substrate. Differences in thermal expansion coefficients can easily lead to interlayer cracking and delamination defects under high-temperature processes. Additionally, ceramic substrates formed using traditional manufacturing processes lack sufficient density and have low surface precision, failing to meet the high corrosion resistance, high stability, and high precision requirements of advanced semiconductor equipment for electrostatic chucks.
[0004] In view of the many shortcomings of existing technologies, there is an urgent need to develop an electrostatic chuck with a reasonable structural hierarchy, strong material adaptability, excellent resistance to plasma corrosion and stable manufacturing process, so as to meet the application requirements of high-end semiconductor plasma processing technology. Summary of the Invention
[0005] To address the shortcomings of existing technologies, this invention provides a plasma-resistant electrostatic chuck and its preparation method, thereby solving the problems mentioned in the background section.
[0006] To achieve the above objectives, in a first aspect, the present invention provides a plasma corrosion resistant electrostatic chuck, comprising a metal base, an insulating transition layer, an internal electrode layer, a ceramic substrate layer, and a corrosion-resistant protective surface layer; the insulating transition layer is disposed on the upper surface of the metal base, the internal electrode layer is arranged between the insulating transition layer and the dense ceramic substrate layer, and the corrosion-resistant protective surface layer densely covers the wafer bearing surface of the ceramic substrate layer.
[0007] The ceramic substrate layer is a doped and modified alumina ceramic, formed by sintering alumina as the main raw material with silicon nitride and yttrium oxide. The density, mechanical properties, and resistance to plasma bombardment of the ceramic substrate are optimized through multi-element doping modification. The built-in electrode layer is a patterned molybdenum electrode, which has excellent conductivity, high temperature resistance, and chemical stability, and can ensure uniform and stable electrostatic adsorption performance. The corrosion-resistant protective surface layer is a dense amorphous composite ceramic film, specifically an alumina-silicon nitride composite film, which can effectively block plasma erosion and process gas corrosion, and protect the substrate structure.
[0008] Furthermore, the insulating transition layer is a high-purity alumina ceramic layer, whose coefficient of thermal expansion is precisely matched with that of the dense ceramic matrix layer. This can effectively alleviate interlayer thermal stress during high-temperature processes, avoid interlayer cracking and delamination, and improve the overall structural stability.
[0009] Furthermore, the metal base is equipped with cooling channels and back-blowing micropores, which can achieve precise temperature control and uniform back-blowing gas supply during wafer processing, ensuring wafer processing temperature uniformity and adsorption stability.
[0010] Secondly, the present invention provides a method for preparing a plasma-resistant electrostatic chuck, which includes the following steps: S1. Metal base pretreatment: The aluminum alloy substrate is precision machined to form an integrated cooling channel, air intake micro-holes and mounting positioning structure. Then, the substrate is subjected to hard anodizing treatment to remove surface impurities, improve the surface hardness and insulation compatibility of the substrate, and finally cleaned and dried for later use.
[0011] S2. Preparation of insulating transition layer: High-purity alumina ceramic green body is prepared by tape casting process. It then undergoes debinding, atmospheric pressure sintering, and precision grinding and polishing processes to prepare an insulating transition layer with uniform thickness and high flatness. The green body is then bonded and fixed to the upper surface of the metal base to ensure tight bonding between the layers without gaps.
[0012] S3. Fabrication of built-in electrode layer: A molybdenum metal thin film is uniformly deposited on the surface of the insulating transition layer, and then a patterned electrode structure is fabricated by photolithography and etching precision processes. After the electrode is shaped, a continuity test is performed to ensure that the electrode circuit is complete and the conductivity is uniform.
[0013] S4. Forming of Dense Ceramic Substrate Layer: Alumina, silicon nitride, yttrium oxide, and zirconium dioxide raw materials are ball-milled and mixed with anhydrous ethanol as the dispersion medium until the slurry particle size D50 ≤ 0.5 μm. Then, binder and dispersant are added and stirred to prepare a uniform and stable ceramic slurry. The slurry is then cast and stacked to obtain a ceramic green body. The green body is pretreated by warm isostatic pressing to improve its density. Finally, a nitrogen-protected segmented high-temperature sintering process is adopted. First, the internal organic additives are removed by low-temperature debinding, and then high-temperature sintering is performed to achieve integrated composite forming of the ceramic substrate layer and the electrode layer.
[0014] S5. Precision surface machining: The surface of the composite-molded ceramic substrate is subjected to rough grinding, fine grinding and nano-level polishing in sequence. The machining accuracy is strictly controlled to ensure that the flatness of the substrate surface is ≤5μm and the roughness Ra≤0.02μm, which meets the high-precision bearing requirements of the wafer.
[0015] S6. Preparation of corrosion-resistant protective surface layer: A dense amorphous alumina-silicon nitride composite protective film is deposited on the ceramic substrate wafer support surface using plasma-enhanced chemical vapor deposition process under a nitrogen and argon mixed protective atmosphere to form a complete corrosion-resistant protective structure.
[0016] S7. Post-processing and testing: The semi-finished chuck after the protective film is deposited is subjected to air atmosphere annealing to relieve stress. It is slowly cooled in the furnace to eliminate the internal stress generated during processing and deposition. Then, the electrode leads are welded, and the sealing performance, insulation performance and plasma corrosion resistance are tested in sequence. After all indicators are qualified, the finished electrostatic chuck is obtained.
[0017] This invention provides a plasma-resistant electrostatic chuck and its preparation method, which has the following beneficial effects: 1. This invention adopts a multi-layer gradient composite structure with matching performance and clear division of labor among the functional layers. The high-purity alumina insulating transition layer with thermal expansion matching effectively solves the problems of delamination and cracking between layers at high temperatures, and significantly improves the overall structural stability and reliability.
[0018] 2. This invention uses a multi-doped modified alumina ceramic matrix combined with a dense amorphous alumina-silicon nitride composite protective film, which greatly improves the chuck's resistance to plasma bombardment and process gas corrosion, effectively inhibits grain shedding and surface deterioration, and extends its service life.
[0019] 3. The use of patterned molybdenum electrodes ensures uniform and stable electrostatic adsorption. Combined with a metal base cooling and back-blowing structure, it can achieve uniform wafer temperature and reliable adsorption, meeting the needs of high-precision semiconductor processing.
[0020] 4. This invention utilizes wet ultrafine ball milling, warm isostatic pressing densification, segmented atmosphere sintering, and nanoscale precision polishing processes to produce products with high density and excellent surface precision. Combined with stress relief annealing and a full set of performance tests, the products exhibit good consistency and stability, meeting the requirements of high-end semiconductor equipment and suitable for mass production. Attached Figure Description
[0021] Figure 1 This is a schematic diagram of the overall layered structure of the plasma corrosion resistant electrostatic chuck of the present invention; Figure 2 This is a process flow diagram of the electrostatic chuck preparation method of the present invention.
[0022] In the diagram: 1. Metal base; 11. Cooling channel; 12. Back-blowing air intake micropores; 2. Insulating transition layer; 3. Built-in electrode layer; 4. Ceramic substrate layer; 5. Corrosion-resistant protective surface layer. Detailed Implementation
[0023] The embodiments of the present invention will be described in further detail below with reference to the accompanying drawings and examples. The following examples are for illustrative purposes only and should not be construed as limiting the scope of the invention.
[0024] In the description of this invention, unless otherwise stated, "a plurality of" means two or more; the terms "upper," "lower," "left," "right," "inner," "outer," "front end," "rear end," "head," "tail," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, and are only for the convenience of describing the invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation of the invention. Furthermore, the terms "first," "second," "third," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance.
[0025] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "connected" and "linked" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0026] A plasma-resistant electrostatic chuck, such as Figure 1 As shown, it is composed of a metal base 1, an insulating transition layer 2, an internal electrode layer 3, a ceramic substrate layer 4, and a corrosion-resistant protective surface layer 5 from top to bottom.
[0027] The metal base 1 is made of aluminum alloy, with pre-fabricated integrated cooling channels 11 and back-blowing air intake micro-holes 12. Precision machining ensures structural dimensional accuracy, and hard anodizing enhances surface compatibility. The insulating transition layer 2 is a high-purity alumina ceramic layer with a thermal expansion coefficient perfectly matched to the ceramic substrate layer 4, and is fixedly attached to the upper surface of the metal base 1. The built-in electrode layer 3 is a patterned molybdenum electrode, deposited on the surface of the insulating transition layer 2, resulting in a regular circuit structure and stable conductivity. The ceramic substrate layer 4 is a dense ceramic layer modified and sintered from a composite of alumina, silicon nitride, yttrium oxide, and zirconium dioxide. The corrosion-resistant protective surface layer 5 is a dense amorphous alumina-silicon nitride composite film, fully covering the ceramic substrate wafer support surface.
[0028] like Figure 2 As shown, its preparation method specifically includes the following steps: S1. Metal base pretreatment: 6061 aluminum alloy base material is used. The cooling channel 11, back blow air inlet micro hole 12 and installation positioning structure are formed by five-axis precision machining. After processing, hard anodizing treatment is performed to remove surface burrs, oxide scale and oil stains. After cleaning with deionized water, it is dried for later use.
[0029] S2. Preparation of insulating transition layer: High-purity alumina powder is selected, and ceramic green body is prepared by tape casting process. The green body is placed in a high-temperature furnace for segmented debinding, followed by high-temperature sintering at normal pressure. After sintering, double-sided precision grinding and mirror polishing are performed to obtain a high-purity alumina insulating transition layer 2 with uniform thickness and smooth surface. It is then bonded and fixed to the upper surface of the metal base 1 by high-temperature bonding process.
[0030] S3. Preparation of built-in electrode layer: A uniform molybdenum metal thin film is deposited on the surface of insulating transition layer 2 using magnetron sputtering. A pre-patterned electrode structure is prepared by photolithography and wet etching. After completion, continuity test and resistance uniformity test are performed to eliminate products with electrode defects.
[0031] S4. Forming of Dense Ceramic Substrate Layer: Weigh the main raw material alumina according to the mass ratio, and compound appropriate amounts of silicon nitride, yttrium oxide, and zirconium dioxide. Mix them in a high-energy ball mill using anhydrous ethanol as the dispersion medium until the slurry particle size D50 ≤ 0.5 μm. Add polyvinyl alcohol binder and polyethylene glycol dispersant to the slurry and stir at high speed to prepare a uniform and stable ceramic slurry. Prepare a ceramic green film by tape casting, and press multiple layers together to obtain a dense green body. Perform warm isostatic pressing pretreatment on the green body, with the pressure controlled at 150 MPa and the temperature at 80℃. Then transfer it to a nitrogen-protected sintering furnace and adopt a segmented sintering process. First, hold at a low temperature of 450℃ for 2 hours to remove the binder, and then raise the temperature to 1650℃ for 4 hours to form a tight composite of the ceramic substrate and the electrode layer.
[0032] S5. Precision surface machining: The surface of the composite ceramic substrate is subjected to rough grinding, fine grinding and nano-diamond polishing in sequence to finally control the surface flatness ≤5μm and roughness Ra≤0.02μm. After machining, the surface dust and impurities are removed by cleaning.
[0033] S6. Preparation of corrosion-resistant protective surface layer: Using plasma-enhanced chemical vapor deposition equipment, a nitrogen and argon mixed process atmosphere is set to deposit an amorphous alumina-silicon nitride composite protective film on the ceramic substrate bearing surface. The film layer has uniform thickness and a dense, non-porous structure.
[0034] S7. Post-processing and testing: The deposited chuck is placed in an air atmosphere annealing furnace and held at 500℃ for 3 hours. It is then allowed to cool naturally in the furnace to remove internal stress. After laser welding of the electrode leads, air tightness test, insulation withstand voltage test, resistance stability test and plasma corrosion acceleration test are performed in sequence. The finished product is obtained after all indicators meet the standards.
[0035] The electrostatic chuck prepared in this embodiment has high interlayer bonding strength and no delamination or cracking defects; the surface precision meets the requirements of high-end wafer processing; under continuous high-energy plasma bombardment, there is no obvious corrosion or peeling; the plasma corrosion resistance life is more than twice that of traditional alumina ceramic electrostatic chucks; and the insulation performance, adsorption stability, and temperature control uniformity all meet the standards for use in 12-inch advanced process semiconductor processing equipment.
[0036] The device embodiments described above are merely illustrative. The units described as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this embodiment according to actual needs. Those skilled in the art can understand and implement this without any creative effort.
[0037] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A plasma-resistant electrostatic chuck, characterized in that, The device includes a metal base (1), an insulating transition layer (2), an internal electrode layer (3), a ceramic substrate layer (4), and a corrosion-resistant protective surface layer (5). The insulating transition layer (2) is disposed on the upper surface of the metal base (1), the internal electrode layer (3) is arranged between the insulating transition layer (2) and the dense ceramic substrate layer (4), and the corrosion-resistant protective surface layer (5) densely covers the wafer bearing surface of the ceramic substrate layer (4). The ceramic substrate layer (4) is a doped modified alumina ceramic. The internal electrode layer (3) is a patterned molybdenum electrode. The corrosion-resistant protective surface layer (5) is a dense amorphous composite ceramic film.
2. The plasma-resistant electrostatic chuck according to claim 1, characterized in that, The dense ceramic matrix layer (4) is mainly composed of alumina, combined with silicon nitride and yttrium oxide and sintered.
3. The plasma-resistant electrostatic chuck according to claim 1, characterized in that, The insulating transition layer (2) is a high-purity alumina ceramic layer, and its coefficient of thermal expansion matches that of the dense ceramic matrix layer (4).
4. The plasma-resistant electrostatic chuck according to claim 1, characterized in that, The metal base (1) is provided with a cooling channel (11) and a back-blowing air inlet micro-hole (12).
5. A plasma-resistant electrostatic chuck according to claim 1, characterized in that, The corrosion-resistant protective surface layer (5) is an aluminum oxide-silicon nitride composite film.
6. A method for preparing a plasma-resistant electrostatic chuck, used to prepare the plasma-resistant electrostatic chuck according to any one of claims 1 to 5, characterized in that, Includes the following steps: S1. Metal base pretreatment: The aluminum alloy substrate is precision machined to form cooling channels, back-blowing air inlet micro-holes and installation positioning structure, followed by hard anodizing treatment, cleaning and drying for later use. S2. Preparation of insulating transition layer: High-purity alumina ceramic green body is prepared by tape casting process, and after debinding, atmospheric pressure sintering, and precision grinding and polishing, a uniform insulating transition layer is obtained and bonded to the upper surface of the metal base. S3. Fabrication of built-in electrode layer: A molybdenum metal thin film is deposited on the surface of the insulating transition layer, and patterned electrodes are fabricated by photolithography and etching processes to complete electrode shaping and conduction detection. S4. Forming of dense ceramic matrix layer: Alumina, silicon nitride, yttrium oxide and zirconium dioxide raw materials are ball-milled and mixed, and binder and dispersant are added to prepare a uniform slurry. The slurry is then cast and pressed to obtain a ceramic green body. After pretreatment by warm isostatic pressing, it is sintered at high temperature to prepare a dense ceramic matrix layer and composite it with the electrode layer. S5. Precision surface machining: The surface of the composite ceramic substrate is subjected to rough grinding, fine grinding, and nano-level polishing to ensure that the surface flatness is ≤5μm and the roughness Ra is ≤0.02μm. S6. Preparation of corrosion-resistant protective surface layer: An amorphous alumina-silicon nitride composite protective film is deposited on the ceramic substrate wafer bearing surface using plasma-enhanced chemical vapor deposition process. S7. Post-processing and inspection: Annealing to relieve stress, electrode lead welding, sealing test, insulation performance test, and random inspection of plasma corrosion resistance are performed on the finished product. After passing the inspection, the finished electrostatic chuck is obtained.
7. The method for preparing a plasma-resistant electrostatic chuck according to claim 6, characterized in that, In step S4, anhydrous ethanol is used as the dispersion medium to ball mill and mix the ceramic raw materials; the particle size D50 of the slurry after ball milling is ≤0.5μm; and then a warm isostatic pressing pretreatment is performed.
8. The method for preparing a plasma-resistant electrostatic chuck according to claim 6, characterized in that, In step S4, nitrogen protection is used for segmented high-temperature sintering. First, the binder is removed at a low temperature, and then it is sintered at a high temperature to form the shape.
9. The method for preparing a plasma-resistant electrostatic chuck according to claim 6, characterized in that, Step S6 employs plasma-enhanced chemical vapor deposition to prepare a corrosion-resistant protective surface layer in a mixed atmosphere of nitrogen and argon.
10. The method for preparing a plasma-resistant electrostatic chuck according to claim 6, characterized in that, Step S7 involves air-atmosphere annealing to relieve stress on the chuck after the protective film has been deposited, followed by furnace cooling.