A semiconductor reliability test structure and a reliability test method
By combining interconnect chains and comb-like structures on a semiconductor substrate, the problem of large area occupation and inability to monitor residues in existing test structures has been solved, achieving efficient and accurate reliability assessment of the dielectric layer and reducing production costs.
Patent Information
- Application Number
- CN202610289816.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-03-10
- Publication Date
- 2026-11-17
AI Technical Summary
Existing semiconductor reliability testing structures occupy a large area on the dicing track, which limits the number and coverage of testing structures, resulting in incomplete reliability assessments and an inability to effectively monitor the impact of residues on process reliability.
The test structure combines interconnect chain structure and comb structure. The interconnect chain structure is used to test the stress migration or electromigration parameter Rc, and the comb structure is used to test the breakdown voltage and breakdown over time. This reduces the area occupied by the test structure and can monitor residues.
It enables comprehensive monitoring of dielectric layer reliability within a limited area, reduces production costs, and accurately identifies weak areas of the dielectric layer, improving the accuracy and coverage of test results.
Smart Images

Figure CN123124750A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of semiconductor technology, and more specifically to a semiconductor reliability testing structure and a reliability testing method. Background Technology
[0002] In semiconductor manufacturing processes, reliability testing is typically used to monitor the process and ensure its stability. In back-end of line (BEOL) processes, the reliability of the dielectric layer has become a critical issue. Stress migration or electromigration parameters (Rc) are used to monitor the reliability of the metal layer, voltage breakdown (Vbd) testing is commonly used for rapid assessment of dielectric layer reliability, and time-dependent dielectric breakdown (TDDB) testing is used to estimate the dielectric layer's lifetime.
[0003] In related technologies, the Kelvin method or two-end method is usually used to test Rc, the two-end method is used to test Vbd, and a test chain is used for the Kevin method test, while a comb structure is used for the two-end method test. A total of 6 pads are required for Rc and Vbd testing. The test chain, comb structure and the corresponding multiple pads together constitute the reliability test structure, and the corresponding reliability test can be completed based on this reliability test structure.
[0004] However, in related technologies, the aforementioned test structures are generally placed on the cutting track. Due to the limited area of the cutting track, the number of test structures that can be placed is limited. This not only restricts the coverage area of the test structures but may also encroach on the space of other test items, leading to a reduction in test items, resulting in an incomplete reliability assessment and higher testing costs. Furthermore, because the test chain itself has a high resistance, if residues exist in the process, these residues will not cause a significant change in Rc. In other words, during reliability testing, the Rc test results cannot reflect the presence of residues. Therefore, the test chain cannot effectively monitor residues, which may affect process reliability. Summary of the Invention
[0005] The summary section introduces a series of simplified concepts, which will be further explained in detail in the detailed description section. This summary section is not intended to limit the key and essential technical features of the claimed technical solution, nor is it intended to determine the scope of protection of the claimed technical solution.
[0006] To address the existing problems, this application provides a semiconductor reliability testing structure, which includes: A semiconductor substrate, an interconnect chain structure and a comb structure disposed on the semiconductor substrate, wherein the interconnect chain structure and the comb structure are both embedded in a dielectric layer and spaced apart from each other; The interconnect chain structure includes an interconnect chain formed by multiple interconnect unit chains connected in series. The multiple interconnect unit chains are spaced apart along a first direction and extend along a second direction. The interconnect unit chain includes multiple first metal lines spaced apart along the second direction in the lower layer, multiple second metal lines spaced apart along the second direction in the upper layer, and multiple first conductive vias spaced apart along the second direction connecting the first metal lines and the second metal lines. The projection of the first conductive via on the semiconductor substrate is located within the overlapping portion of the projections of the first metal lines and the second metal lines on the semiconductor substrate. Both the first and second metal lines extend along the second direction, and the first conductive via extends along a third direction. The first direction and the second direction are perpendicular to each other and parallel to the semiconductor substrate, and the third direction is perpendicular to the semiconductor substrate. The comb-like structure includes a first comb-like portion and / or a second comb-like portion spaced apart from the interconnect chain structure. The first comb-like portion is on the same layer as the first metal wire, and the second comb-like portion is on the same layer as the second metal wire. Both the first comb-like portion and the second comb-like portion include a plurality of comb-tooth metal wires extending along the first direction and spaced apart along the second direction, and a comb handle metal wire connecting the plurality of comb-tooth metal wires and extending along the second direction. The comb-tooth metal wires are disposed between adjacent first metal wires or between second metal wires, and the comb handle metal wire is located on one side of the interconnect chain structure along the first direction.
[0007] In one embodiment, the interconnect chain structure further includes at least one connection structure for connecting adjacent interconnect unit chains. The connection structure includes a connecting metal line extending along the first direction and two second conductive vias extending along the third direction and arranged along the first direction. The connecting metal line is located on the same layer as the first metal line or the second metal line and is spaced apart with equal linewidth. The second conductive vias connect the connecting metal line and the second metal line or the first metal line. The projection of the second conductive via on the semiconductor substrate is located within the overlapping portion of the projection of the connecting metal line on the semiconductor substrate and the projection of the second metal line or the first metal line on the semiconductor substrate. All the connecting metal lines in the interconnect chain structure are spaced apart from each other, and the second conductive vias are the same size as the first conductive vias.
[0008] In one embodiment, the first metal wire and the second metal wire in the interconnect unit chain are offset in the second direction, and the first conductive via is connected between the end of the first metal wire and the corresponding end of the second metal wire.
[0009] In one embodiment, the comb-like structure includes a first comb-like portion and a second comb-like portion. The comb teeth metal wires of the first comb-like portion are located between adjacent first metal wires, and the comb teeth metal wires of the second comb-like portion are located between adjacent second metal wires. The lengths of the comb teeth metal wires of the first comb-like portion and the second comb-like portion are both greater than the dimensions of the interconnect chain structure along the first direction. The comb handle metal wires of the first comb-like portion and the comb handle metal wires of the second comb-like portion are located on both sides of the interconnect chain structure along the first direction.
[0010] In one embodiment, the comb teeth metal wires of the first comb portion and the comb teeth metal wires of the second comb portion are arranged alternately in the second direction.
[0011] In one embodiment, the linewidth of the comb teeth metal wire in the first comb-shaped portion is equal to the linewidth of the first metal wire, and the linewidth of the comb teeth metal wire in the second comb-shaped portion is equal to the linewidth of the second metal wire.
[0012] In one embodiment, the spacing between the comb teeth metal wires of the first comb-shaped portion and the adjacent first metal wires is set at equal intervals, and the spacing between the comb teeth metal wires of the second comb-shaped portion and the adjacent second metal wires is set at equal intervals.
[0013] In one embodiment, the spacing between adjacent first metal lines in the interconnect unit chain is equal to the spacing between the second metal lines.
[0014] In one embodiment, the interconnect chain structure further includes a first pad and a second pad, wherein the first pad is connected to one end of the interconnect chain and the second pad is connected to the other end of the interconnect chain; The comb-like structure further includes a third pad and / or a fourth pad, one end of the comb handle metal wire of the first comb-like portion is connected to the third pad, and one end of the comb handle metal wire of the second comb-like portion is connected to the fourth pad.
[0015] This application also provides a method for performing reliability testing using the above-described semiconductor reliability testing structure, the method comprising: In the first test mode, a test current signal is applied to one of the first pad and the second pad, while the other is grounded, and the voltage difference between the first pad and the second pad is tested to test the stress migration or electromigration parameter Rc. In the second test mode, a test voltage signal is applied to the third pad or the fourth pad, and at least one of the first pad and the second pad is grounded, for testing the breakdown voltage and / or breakdown over time between the interconnect chain and the first comb portion located in the layer where the first metal line is located, or the breakdown voltage and / or breakdown over time between the interconnect chain and the second comb portion located in the layer where the second metal line is located. In the third test mode, a test signal is applied to the third pad or the fourth pad, at least one of the first pad and the second pad is grounded, and the leakage current between the interconnect chain located on the layer where the first metal line is located and the first comb portion, or the leakage current between the interconnect chain located on the layer where the second metal line is located and the second comb portion, is tested to determine whether there is any contamination residue between the interconnect chain and the first comb portion and the second comb portion.
[0016] The semiconductor reliability testing structure and method of this application embodiment simultaneously provide an interconnect chain structure and a comb structure on a semiconductor substrate. The interconnect chain structure includes multiple interconnect unit chains connected in series, each interconnect unit chain comprising multiple first metal lines on a lower layer, multiple second metal lines on an upper layer, and a first conductive via connecting the first and second metal lines. The comb structure includes a first comb portion and / or a second comb portion spaced apart from the interconnect chain structure. The first comb portion is on the same layer as the first metal line, and the second comb portion is on the same layer as the second metal line. This testing structure achieves the testing of stress migration or electromigration parameter Rc through the interconnect chain structure. Simultaneously, by combining the comb structure and the interconnect chain structure, the breakdown voltage and / or breakdown over time between the interconnect chain and the first comb portion, and between the interconnect chain and the second comb portion, can be tested. Thus, the testing structure of this application can be used to measure stress migration, electromigration parameter Rc, breakdown voltage, and / or breakdown over time, thereby saving the placement area of the testing structure. Furthermore, the implementation of this semiconductor reliability testing structure requires no additional process steps, thus avoiding additional cost burdens and keeping production costs controllable. Attached Figure Description
[0017] The following drawings, which are incorporated herein by reference and are used to understand this application, illustrate embodiments of the invention and their descriptions to explain the principles of the invention.
[0018] In the attached image: Figure 1 This illustrates a prior art reliability test structure that includes a test chain; Figure 2 It shows Figure 1 A schematic diagram of a partial cross-section of the reliability test structure on a plane perpendicular to the first direction; Figure 3 A top view of a reliability test structure including a test chain is shown, wherein residues exist in the reliability test structure; Figure 4 This illustrates a reliability test structure in the prior art that includes a comb-like structure; Figure 5 A schematic diagram of the wafer structure related to the present application is shown; Figure 6 A schematic diagram of a first semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 7A A partial cross-sectional schematic diagram of a first semiconductor reliability testing structure according to a specific embodiment of this application is shown on a plane perpendicular to a first direction; Figure 7B A partial cross-sectional schematic diagram of a first semiconductor reliability testing structure according to a specific embodiment of this application is shown on a plane perpendicular to the second direction; Figure 7C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a residue exists in the first semiconductor reliability test structure according to a specific embodiment of this application. Figure 8 A schematic diagram of a second semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 9A A partial cross-sectional schematic diagram of a second semiconductor reliability testing structure according to a specific embodiment of this application is shown on a plane perpendicular to the first direction; Figure 9B A partial cross-sectional schematic diagram of a second semiconductor reliability testing structure according to a specific embodiment of this application is shown on a plane perpendicular to the second direction; Figure 9C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a residue exists in the second semiconductor reliability test structure according to a specific embodiment of this application. Figure 10 A schematic diagram of a third semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 11A A partial cross-sectional schematic diagram of a third semiconductor reliability testing structure according to a specific embodiment of this application is shown on a plane perpendicular to the first direction; Figure 11BA partial cross-sectional schematic diagram of a third semiconductor reliability test structure according to a specific embodiment of this application is shown in a plane perpendicular to the second direction; Figure 11C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a third semiconductor reliability test structure according to a specific embodiment of this application has residual components. Figure 12 A schematic diagram of a fourth semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 13A A partial cross-sectional schematic diagram of the fourth semiconductor reliability test structure according to a specific embodiment of this application is shown on a plane perpendicular to the first direction; Figure 13B A partial cross-sectional schematic diagram of the fourth semiconductor reliability test structure according to a specific embodiment of this application is shown on a plane perpendicular to the second direction; Figure 13C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a residue exists in the fourth semiconductor reliability test structure according to a specific embodiment of this application. Figure 14 A schematic diagram of a fifth semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 15A This illustration shows a partial cross-sectional view of a fifth semiconductor reliability testing structure according to a specific embodiment of this application on a plane perpendicular to the first direction. Figure 15B This illustration shows a partial cross-sectional view of a fifth semiconductor reliability testing structure according to a specific embodiment of this application on a plane perpendicular to the second direction. Figure 15C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a residue exists in the fifth semiconductor reliability test structure according to a specific embodiment of this application. Figure 16 A schematic diagram of a sixth semiconductor reliability test structure according to a specific embodiment of this application is shown; Figure 17A This illustration shows a partial cross-sectional view of a sixth semiconductor reliability testing structure according to a specific embodiment of this application on a plane perpendicular to the first direction. Figure 17B This illustration shows a partial cross-sectional view of a sixth semiconductor reliability testing structure according to a specific embodiment of this application on a plane perpendicular to the second direction. Figure 17C This illustration shows a partial cross-sectional view on a plane perpendicular to the first direction when a sixth semiconductor reliability test structure according to a specific embodiment of this application has residual components. Figure 18 This is a top view schematic diagram showing the presence of residues in the first semiconductor reliability test structure according to a specific embodiment of this application. Detailed Implementation
[0019] The present application will now be described more fully with reference to the accompanying drawings, in which embodiments of the present application are illustrated. However, the present application can be implemented in various forms and should not be construed as limited to the embodiments set forth herein. Rather, providing these embodiments will make the disclosure thorough and complete, and will fully convey the scope of the present application to those skilled in the art. In the drawings, for clarity, the dimensions and relative dimensions of layers and regions may be exaggerated. The same reference numerals denote the same elements throughout.
[0020] It should be understood that when an element or layer is referred to as "on," "adjacent to," "connected to," or "coupled to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. Conversely, when an element is referred to as "directly on," "directly adjacent to," "directly connected to," or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc., may be used to describe various elements, components, areas, layers, and / or portions, these elements, components, areas, layers, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, area, layer, or portion from another element, component, area, layer, or portion. Therefore, without departing from the teachings of this application, the first element, component, area, layer, or portion discussed below may be referred to as the second element, component, area, layer, or portion.
[0021] Spatial relation terms such as “below,” “under,” “below,” “under,” “above,” “above,” etc., are used herein for convenience of description to describe the relationship between one element or feature shown in the figure and other elements or features. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms are intended to also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, then the element or feature described as “below” or “under” the other element or feature will be oriented “above” the other element or feature. Therefore, the exemplary terms “below” and “under” can include both upper and lower orientations. The device may be otherwise oriented (rotated 90 degrees or otherwise) and the spatial descriptive terms used herein will be interpreted accordingly.
[0022] The terminology used herein is for the purpose of describing particular embodiments only and is not intended to limit the scope of this application. When used herein, the singular forms “a,” “an,” and “the” are also intended to include the plural forms unless the context clearly indicates otherwise. It should also be understood that the terms “comprise” and / or “comprising,” when used in this specification, identify the presence of the stated features, integers, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and / or groups. When used herein, the term “and / or” includes any and all combinations of the associated listed items.
[0023] Unless otherwise defined, all terms used herein (including technical and scientific terms) shall have the same meaning as commonly understood by one of ordinary skill in the art. It will also be understood that terms as defined in commonly used dictionaries shall be interpreted as having a meaning consistent with their meaning in the relevant field and / or the context of this specification, and not as in an ideal or overly formal sense, unless expressly defined herein.
[0024] To fully understand this application, detailed steps and structures will be presented in the following description to illustrate the technical solutions proposed in this application. Preferred embodiments of this application are described in detail below; however, in addition to these detailed descriptions, this application may have other implementation methods.
[0025] In semiconductor manufacturing processes, reliability testing is typically used to monitor the process and ensure its stability. In back-end of line (BEOL) processes, the reliability of the dielectric layer has become a critical issue. Stress migration or electromigration parameters (Rc) are commonly used to monitor the reliability of the metal layer, while voltage breakdown (Vbd) testing is a common method for quickly assessing dielectric layer reliability. Time-dependent dielectric breakdown (TDDB) is used to predict the lifetime of the dielectric layer.
[0026] In related technologies, the above parameters are typically monitored using two independent test structures: 1. A test chain structure is typically used for Kevin's method testing to test Rc, such as... Figure 1 As shown, the test chain structure includes a test chain 10 and pads 11. One end of the test chain 10 is connected to two pads 11, namely PAD1 and PAD2, and the other end of the test chain 10 is connected to two more pads 11, namely PAD3 and PAD4. A test voltage signal is applied to PAD2, and PAD3 is grounded. The voltage is measured at PAD1 and PAD4. The Rc value is equal to the ratio of voltage to current, thereby passing through... Figure 1The structure shown completes the Rc test.
[0027] 2. Related technologies use the two-end method to test Vbd, such as... Figure 4 The comb-shaped structure shown is used to test Vbd. The comb-shaped structure includes two opposite and cross-spaced comb-shaped parts 12. Each comb-shaped part is connected to a pad 11 at one end, namely PAD5 and PAD6. During testing, a test voltage signal can be applied to PAD5 and PAD6 is grounded. The voltage signal applied to PAD5 is gradually increased until the dielectric layer is broken down, thereby measuring the breakdown voltage.
[0028] To monitor Rc and Vbd / TDDB during the semiconductor device fabrication process, the two test structures mentioned above need to be placed on the wafer, requiring a total of six pads to be brought out for the test chain structure and the comb structure.
[0029] However, as Figure 5 As shown, the reliability test structure is usually placed on the dicing area 14 between chip areas 101 on wafer 100. Due to the limited area of the dicing area 14, six pads are required to place the test structure in order to complete Rc test and Vbd / TDDB test. Therefore, the number of other process monitoring or reliability test structures that can be integrated in the same test area is limited. In order to meet the area constraints, some test structures are often forced to be removed, resulting in incomplete coverage of reliability assessment of the dielectric layer. That is, the area range of reliability test structure is limited and the cost is high.
[0030] In addition, such as Figure 2 and Figure 3 As shown, during the fabrication of semiconductor devices, when residue 13 remains in the reliability test structure, due to the large resistance of the test chain structure, the residue 13 will not cause a large change in resistance Rc. The small resistance change caused by the residue is difficult to be captured by the Rc test, which means that these residues 13 are "submerged" in the small changes in Rc.
[0031] For example, such as Figure 3 As shown, in the stress migration test, a test voltage signal is applied to PAD1, PAD2 is grounded, and the resistance R0 at time T0 is measured. After high-temperature baking for times T1 / T2 / T3, the resistances R1 / R2 / R3 at times T1 / T2 / T3 are measured respectively. The reliability of test chain 10 is determined by R = (Rn - R0 / R0) * 100% (n = 1, 2, 3). If residue 13 exists during the semiconductor device fabrication process, the stress migration (SM) test passes. R is used to determine reliability. Residue 13 may not cause [further issues] after stress migration testing at times T1 / T2 / T3. If R changes significantly, then the reliability test structure will be unable to monitor residue 13.
[0032] Residue 13 can adhere to various locations within the reliability testing structure, and as manufacturing processes become more advanced... Figure 2 and Figure 3 The residue 13 shown will become a hidden factor affecting process reliability, therefore Figure 1 The reliability testing structure of the related technologies shown cannot meet the reliability requirements of the product, ultimately affecting the product quality.
[0033] Therefore, in view of the aforementioned technical problems, this application proposes a semiconductor device reliability testing structure and a reliability testing method. The semiconductor reliability testing structure of this application includes: a semiconductor substrate, an interconnect chain structure and a comb-like structure disposed on the semiconductor substrate, wherein the interconnect chain structure and the comb-like structure are both embedded in a dielectric layer and spaced apart from each other; The interconnect chain structure includes an interconnect chain formed by multiple interconnect unit chains connected in series. The multiple interconnect unit chains are spaced apart along a first direction and extend along a second direction. The interconnect unit chain includes multiple first metal lines spaced apart along the second direction in the lower layer, multiple second metal lines spaced apart along the second direction in the upper layer, and multiple first conductive vias spaced apart along the second direction connecting the first metal lines and the second metal lines. The projection of the first conductive vias on the semiconductor substrate is located in the overlapping portion of the projections of the first metal lines on the semiconductor substrate and the projections of the second metal lines on the semiconductor substrate. Both the first metal lines and the second metal lines extend along the second direction, and the first conductive vias extend along a third direction. The first direction and the second direction are perpendicular to each other and both are parallel to the semiconductor substrate, and the third direction is perpendicular to the semiconductor substrate. The comb-like structure includes a first comb-like portion and / or a second comb-like portion spaced apart from the interconnect chain structure. The first comb-like portion is in the same layer as the first metal wire, and the second comb-like portion is in the same layer as the second metal wire. Both the first comb-like portion and the second comb-like portion include a plurality of comb-tooth metal wires extending along a first direction and spaced apart along a second direction, and a comb handle metal wire connecting the plurality of comb-tooth metal wires and extending along the second direction. Comb-tooth metal wires are provided between adjacent first metal wires or between second metal wires, and the comb handle metal wire is located on one side of the interconnect chain structure along the first direction.
[0034] The semiconductor reliability testing structure and method of this application embodiment simultaneously provide an interconnect chain structure and a comb structure on a semiconductor substrate. The interconnect chain structure includes multiple interconnect unit chains connected in series to form an interconnect chain. Each interconnect unit chain includes multiple first metal lines on a lower layer, multiple second metal lines on an upper layer, and a first conductive via connecting the first and second metal lines. The comb structure includes a first comb portion and / or a second comb portion spaced apart from the interconnect chain structure. The first comb portion is on the same layer as the first metal line, and the second comb portion is on the same layer as the second metal line. This testing structure achieves the testing of stress migration or electromigration parameter Rc through the interconnect chain structure. Simultaneously, by combining the comb structure and the interconnect chain structure, the breakdown voltage and / or breakdown over time between the interconnect chain and the first comb portion, and between the interconnect chain and the second comb portion, can be tested. Thus, the testing structure of this application can be used to measure stress migration, electromigration parameter Rc, breakdown voltage, and / or breakdown over time, thereby saving the placement area of the testing structure. Furthermore, the implementation of this semiconductor reliability testing structure requires no additional process steps, thus avoiding additional cost burdens and keeping production costs controllable.
[0035] Below, for reference Figures 6 to 18 The semiconductor reliability testing structure of this application is described in detail.
[0036] Example 1 like Figure 6 As shown, the semiconductor reliability test structure of this application includes a semiconductor substrate (not shown), an interconnect chain structure and a comb structure. The interconnect chain structure and the comb structure are disposed on the semiconductor substrate, and both the interconnect chain structure and the comb structure are embedded in a dielectric layer (not shown) and spaced apart from each other.
[0037] Exemplarily, the semiconductor reliability test structure includes a semiconductor substrate, the material of which includes, but is not limited to, at least one of the following: silicon (Si), germanium (Ge), silicon germanium (SiGe), silicon carbide (SiC), silicon germanium carbon (SiGeC), indium arsenide (InAs), gallium arsenide (GaAs), indium phosphide (InP), sapphire, or other III / V compound semiconductors; or silicon-on-insulator (SOI), silicon-on-insulator (SSOI), silicon-on-insulator (S-SiGeOI), silicon-on-insulator (SiGeOI), and germanium-on-insulator (GeOI); or it may be a double-sided polished wafer (DSP), a ceramic substrate such as alumina, a quartz, or a glass substrate, etc. Although several examples of materials that can form the substrate have been described herein, any material that can serve as a substrate falls within the spirit and scope of the invention. Exemplarily, the semiconductor substrate may be fabricated from single-crystal silicon material.
[0038] In this embodiment, the semiconductor reliability test structure is formed on a semiconductor substrate. The semiconductor substrate is typically a wafer 100, such as a silicon wafer, which is used to define multiple chip regions 101 through processes such as photolithography for fabricating integrated circuit chips. Adjacent chip regions 101 are separated by dicing areas 14, which are used for subsequent chip dicing and do not contain functional circuitry. To save chip area and fully utilize the blank areas on the wafer, the test structure can be located within the dicing area 14, thereby achieving process monitoring and reliability testing without affecting chip functionality. Furthermore, depending on testing requirements or design rules, the test structure can also be partially or entirely located in specific monitoring areas within the chip regions 101, such as the edge of the chip dicing groove or a reserved test element area. Through this layout, the test structure can effectively monitor the reliability parameters of the metal and dielectric layers during the wafer fabrication process, while avoiding occupying effective chip area and reducing production costs.
[0039] The interconnect chain structure includes an interconnect chain formed by multiple interconnect unit chains 20 connected in series, with the multiple interconnect unit chains 20 arranged at intervals along a first direction and extending along a second direction.
[0040] The interconnect unit chain 20 includes a plurality of first metal lines 21 spaced apart along a second direction in the lower layer, a plurality of second metal lines 23 spaced apart along a second direction in the upper layer, and a plurality of first conductive vias 22 spaced apart along a second direction connecting the first metal lines 21 and the second metal lines 23. Specifically, the interconnect unit chain 20 is composed of first metal lines 21, second metal lines 23, and first conductive vias 22. The first metal lines 21 and second metal lines 23 both extend along the second direction and are spaced apart along the second direction in their respective layers. The first conductive vias 22 extend along a third direction perpendicular to the semiconductor substrate, and the projection of the first conductive vias 22 on the semiconductor substrate falls within the overlapping area of the projections of the corresponding first metal lines 21 and second metal lines 23 on the semiconductor substrate, ensuring a reliable electrical connection between the upper and lower metal lines. The first conductive via 22, the first metal line 21, and the second metal line 23 are connected as a single unit, so that each interconnect unit chain 20 forms an integrated conductive chain spanning the upper and lower metal layers. When combined with the comb-like structure, a uniform and stable test electric field is formed, thereby accurately reflecting the reliability of the dielectric layer. The third direction is perpendicular to the semiconductor substrate, and the first direction, the second direction, and the third direction are mutually perpendicular.
[0041] For example, the first metal line 21 and the second metal line 23 in the interconnect unit chain 20 are staggered in the second direction. The first conductive via 22 is connected between the end of the first metal line 21 and the corresponding end of the second metal line 23, so that the first metal line 21, the first conductive via 22 and the second metal line 23 together form a continuous and bent conductive chain structure. This can not only achieve a stable electrical connection between the upper and lower layers, but also form an electric field distribution that is more in line with the actual circuit through staggered arrangement, thereby improving the accuracy of dielectric layer reliability testing.
[0042] Continue as Figure 6 As shown, the comb-like structure includes a first comb-like portion 31 and a second comb-like portion 32 spaced apart from the interconnect chain structure. Both the first comb-like portion 31 and the second comb-like portion 32 include a plurality of comb tooth metal lines 33 extending along a first direction and spaced apart along a second direction, and a comb handle metal line 34 connecting the plurality of comb teeth and extending along the second direction. Comb tooth metal lines 33 are provided between any adjacent first metal lines 21 and second metal lines 23, and the comb handle metal line 34 is located on one side of the interconnect chain structure along the first direction.
[0043] Specifically, taking the first comb-shaped portion 31 as an example, the first comb-shaped portion 31 has a comb-like layout. The comb handle metal line 34 extends along the second direction, serving as the main conductive structure. One end of the comb handle metal line 34 is electrically connected to the pad, and the other end extends along the second direction, providing support and a common current path for multiple comb tooth metal lines 33. Multiple comb tooth metal lines 33 are all connected to and electrically conductive with the comb handle metal line 34, extending along the first direction and arranged at intervals along the second direction, for example, evenly spaced along the second direction. This evenly spaced arrangement helps to form a consistent electric field environment between adjacent comb tooth metal lines, improving the uniformity and repeatability of the field strength distribution in the test area, thereby enhancing the accuracy of the dielectric layer reliability assessment. The first direction and the second direction are perpendicular to each other and both parallel to the surface of the semiconductor substrate. The structure and function of the second comb-shaped portion 32 are similar to those of the first comb-shaped portion 31 and will not be described in detail here.
[0044] Continue as Figure 6As shown, the first comb-shaped portion 31 is on the same layer as the first metal wire 21, and the second comb-shaped portion 32 is on the same layer as the second metal wire 23. Specifically, when the first comb-shaped portion 31 and the lower first metal wire 21 are on the same layer, the comb teeth 33 of the first comb-shaped portion 31 are arranged between adjacent first metal wires 21. When the second comb-shaped portion 32 and the upper second metal wire 23 are on the same layer, the comb teeth 33 of the second comb-shaped portion 32 are arranged between adjacent second metal wires 23. The above layout can be flexibly selected according to the testing requirements to complete the reliability testing of the dielectric layer at different layer positions. For example, when it is necessary to evaluate the reliability between the lower metal wire and the dielectric layer, the first comb-shaped portion 31 is set on the same layer as the first metal wire 21; when it is necessary to evaluate the reliability between the upper metal wire and the dielectric layer, the second comb-shaped portion 32 is set on the same layer as the second metal wire 23.
[0045] It is worth mentioning that the different comb-tooth metal wires 33 are separated by a dielectric layer, which includes, but is not limited to, silicon oxide, silicon nitride, or a low dielectric constant material.
[0046] Both the interconnect chain structure and the comb structure are embedded in the dielectric layer and spaced apart from each other. That is, the gap between the interconnect chain structure and the comb structure is filled by the dielectric layer to achieve electrical isolation. The dielectric layer includes, but is not limited to, silicon oxide, silicon nitride or low dielectric constant material.
[0047] For example, such as Figure 6 As shown, the comb teeth metal wires 33 of the first comb-shaped portion 31 are located between adjacent first metal wires 21, and the comb teeth metal wires 33 of the second comb-shaped portion 32 are located between adjacent second metal wires 23. The lengths of the comb teeth metal wires 33 of the first comb-shaped portion 31 and the second comb teeth metal wires 33 of the second comb-shaped portion 32 are both greater than the dimensions of the interconnect chain structure along the first direction. The comb handle metal wires 34 of the first comb-shaped portion 31 and the second comb handle metal wires 34 of the second comb-shaped portion 32 are located on both sides of the interconnect chain structure along the first direction.
[0048] For example, the comb-tooth metal wires 33 of the first comb-shaped portion 31 and the comb-tooth metal wires 33 of the second comb-shaped portion 32 are staggered in the second direction. This layout not only achieves a compact arrangement of the test structure, but also ensures the effective concentration of the electric field in the target gap area. At the same time, the L-shaped trunk connection improves the wiring efficiency and structural symmetry, which is beneficial to achieving multi-mode, high-density dielectric layer reliability testing within a limited cut area.
[0049] The linewidth of the comb-tooth metal line 33 of the first comb-shaped portion 31 is equal to the linewidth of the first metal line 21, and the linewidth of the comb-tooth metal line 33 of the second comb-shaped portion 32 is equal to the linewidth of the second metal line 23. In other words, the linewidth of the comb-tooth metal line 33 is equal to that of the metal lines in the same layer, so that the size of each metal line in the test area is consistent, thereby ensuring a uniform and stable electric field distribution.
[0050] For example, all the first conductive vias 22 are of equal size and arranged in an array along the first and second directions. Specifically, all the first conductive vias 22 have the same dimensions, such as the same cross-sectional shape and height. Multiple first conductive vias 22 are arranged at equal intervals along the first direction and also at equal intervals along the second direction, so that the projection positions of each first conductive via 22 on the semiconductor substrate are uniformly distributed in a matrix. This ensures that the connection structure between each first conductive via 22 and the first metal line 21 and the second metal line 23 is consistent, the electric field distribution within the test area is uniform, and the test conditions are consistent, improving the consistency and accuracy of the dielectric layer reliability test results. Each first conductive via 22 penetrates the dielectric layer between the first metal line 21 and the second metal line 23. Different first conductive vias 22 are insulated from each other by a dielectric layer, which includes, but is not limited to, silicon oxide, silicon nitride, or a low dielectric constant material. This ensures that adjacent conductive vias are not interconnected, avoiding leakage or short circuits during testing, ensuring a stable test electric field distribution and accurate test results.
[0051] For example, such as Figure 7A As shown, the spacing between the comb-tooth metal lines 33 of the first comb-shaped portion 31 and the adjacent first metal lines 21 is set at equal intervals, and the spacing between the comb-tooth metal lines 33 of the second comb-shaped portion 32 and the adjacent second metal lines 23 is set at equal intervals. For example, the spacing between the comb-tooth metal lines 33 of the first comb-shaped portion 31 and the adjacent first metal lines 21 is 'a', and the spacing between the comb-tooth metal lines 33 of the second comb-shaped portion 32 and the adjacent second metal lines 23 is 'b'. This design of equal spacing and equal linewidth ensures a uniform electric field distribution at each test gap, consistent electrical stress on the dielectric layer, and facilitates accurate identification of the weakest area of the dielectric layer, providing a reliable basis for process optimization.
[0052] For example, such as Figure 7B As shown, in the interconnect unit chain 20, the spacing d between adjacent first metal lines 21 in the first direction is equal to the spacing c between second metal lines 23, i.e., d=c. This design ensures that the electric field distribution between the upper and lower metal lines is uniform and consistent in the vertical direction, so that the electric field strength of the entire test area is basically the same when voltage stress is applied.
[0053] For example, such as Figure 6As shown, the interconnect chain structure also includes at least one connection structure for connecting adjacent interconnect unit chains 20. The connection structure includes a connecting metal line 24 extending along a first direction and two second conductive vias 25 extending along a third direction and arranged along the first direction. The connecting metal line 24 and the first metal line 21 are located in the same layer and are spaced apart with equal line widths. The connecting metal line 24 and the second metal line 23 are connected through the second conductive vias 25. The projection of the second conductive via 25 on the semiconductor substrate is located within the overlapping portion of the projection of the connecting metal line 24 on the semiconductor substrate and the projection of the second metal line 23 on the semiconductor substrate. All connecting metal lines 24 in the interconnect chain structure are spaced apart from each other. Optionally, the second conductive via 25 and the first conductive via 22 are substantially equal in size.
[0054] In another example, the connecting metal line 24 and the second metal line 23 are located on the same layer and are spaced apart with equal linewidths. The connecting metal line 24 and the first metal line 21 are connected through a second conductive via 25. The projection of the second conductive via 25 onto the semiconductor substrate is located within the overlapping portion of the projections of the connecting metal line 24 and the first metal line 21 onto the semiconductor substrate. It is worth mentioning that the equal linewidth spacing refers to the metal lines on the same layer having equal linewidths and being spaced apart from each other.
[0055] For example, such as Figure 6 As shown, the interconnect chain structure also includes a first pad 41 and a second pad 42. The first pad 41 is connected to one end of the interconnect chain, and the second pad 42 is connected to the other end of the interconnect chain. The comb structure also includes a third pad 43 and a fourth pad 44. One end of the comb handle metal line 34 of the first comb portion 31 is connected to the third pad 43, and one end of the comb handle metal line 34 of the second comb portion 32 is connected to the fourth pad 44.
[0056] The first pad 41 can apply a test voltage to the interconnect structure, and the second pad 42 can provide a reference potential (such as ground) to the interconnect structure; or the second pad 42 can apply a test voltage to the interconnect structure, and the first pad 41 can provide a reference potential (such as ground) to the interconnect structure, thereby completing the Rc test.
[0057] The third pad 43 can apply a test voltage to the first comb section 31, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect chain structure, thereby testing the Vbd / TDDB between the lower interconnect chain structure and the comb structure; or the fourth pad 44 can apply a test voltage to the second comb section 32, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect chain structure, thereby testing the Vbd / TDDB between the upper interconnect chain structure and the comb structure.
[0058] For example, the semiconductor reliability test structure also includes a fifth pad (not shown) and a sixth pad (not shown), which are connected to an interconnect chain and are connected to the same end of the interconnect chain as the first pad. The sixth pad is close to the second pad and is connected to the same end of the interconnect chain as the second pad, so that the semiconductor reliability test structure can test stress migration / electromigration parameters using the Kelvin four-terminal method.
[0059] Example 2 The semiconductor reliability test structure in Example 2 is basically the same as the semiconductor reliability test structure in Example 1, such as... Figure 8 As shown, the semiconductor reliability testing structure in Embodiment 2 also includes an interconnect chain structure and a comb structure. The interconnect chain structure includes an interconnect chain formed by multiple interconnect unit chains 20 connected in series. The comb structure includes a first comb portion 31 and a second comb portion 32 spaced apart from the interconnect chain structure. The specific structures of the interconnect unit chain 20, the first comb portion 31, and the second comb portion 32 can be found in the description of Embodiment 1, and will not be repeated here.
[0060] like Figure 8 As shown, the main difference between Embodiment 2 and Embodiment 1 is that the linewidth of the second metal line 23 is greater than the linewidth of the first metal line 21. In other words, the linewidth of the upper metal line is greater than the linewidth of the lower metal line. The linewidth of the comb-tooth metal line 33 of the first comb-shaped portion 31 is equal to the linewidth of the first metal line 21, and the linewidth of the comb-tooth metal line 33 of the second comb-shaped portion 32 is equal to the linewidth of the second metal line 23. Figure 9A and Figure 9B As shown, B=C>D=A.
[0061] In embodiment two, since the linewidth of the second metal line 23 is greater than the linewidth of the first metal line 21, therefore, as Figure 9B In the interconnection unit chain 20 shown, the spacing d between adjacent first metal lines 21 in the first direction is greater than the spacing c between second metal lines 23.
[0062] Other structures not described in the semiconductor reliability test structure of Example 2 are the same as the corresponding structures in the semiconductor reliability test structure of Example 1. For details, please refer to the description of Example 1, which will not be repeated here.
[0063] In the structure of semiconductor devices, the width of the metal usually increases from bottom to top. Therefore, the design of the upper metal line being wider than the lower metal line in Embodiment 2 is closer to the structure of commonly used semiconductor devices and more in line with the actual semiconductor device traces. The reliability test data is closer to the actual product.
[0064] Example 3 The difference between the semiconductor reliability test structure in Example 3 and the semiconductor reliability test structure in Example 1 lies in the different comb-shaped structure. For example... Figure 10 As shown, the comb-like structure includes a first comb-like portion 31 spaced apart from the interconnect chain structure. In other words, the comb-like structure of Embodiment 3 only includes the first comb-like portion 31 on the same layer as the first metal line 21. Since the comb-like structure of Embodiment 2 only includes the first comb-like portion 31, the comb-like structure of Embodiment 3 also includes a third pad 43. One end of the comb handle metal line 34 of the first comb-like portion 31 is connected to the third pad 43.
[0065] The first pad 41 can apply a test voltage to the interconnect structure, and the second pad 42 can provide a reference potential (such as ground) to the interconnect structure; or the second pad 42 can apply a test voltage to the interconnect structure, and the first pad 41 can provide a reference potential (such as ground) to the interconnect structure, thereby completing the Rc test.
[0066] The third pad 43 can apply a test voltage to the first comb section 31, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect structure, thereby testing the Vbd / TDDB between the lower interconnect structure and the comb structure.
[0067] In Embodiment 3, the comb handle metal wire 34 of the first comb-shaped portion 31 is located on one side of the interconnect chain structure along the first direction. The other structures of Embodiment 3 are the same as those of Embodiment 1, and can be referred to the detailed description of Embodiment 1, which will not be repeated here.
[0068] like Figure 11A As shown, the spacing between the comb-shaped metal lines 33 of the first comb-shaped portion 31 and the adjacent first metal lines 21 is set at equal intervals, for example, the spacing is a.
[0069] like Figure 11B As shown, in the interconnect unit chain 20, the spacing d between adjacent first metal lines 21 in the first direction is equal to the spacing c between second metal lines 23.
[0070] The linewidth of the first metal wire 21 is equal to the linewidth of the second metal wire 23, meaning the linewidth of the upper metal wire is the same as the linewidth of the lower metal wire. The linewidth of the comb-tooth metal wire 33 of the first comb-shaped portion 31 is equal to the linewidth of the first metal wire 21, that is... Figure 11A and Figure 11B As shown, A=C=D.
[0071] Example 4 The semiconductor reliability test structure in Example 4 is similar to that in Example 3, with the main difference from the semiconductor reliability test structure in Example 1 being the different comb-like structure. For example... Figure 12As shown, the comb-like structure includes a second comb-like portion 32 spaced apart from the interconnect chain structure. In other words, the comb-like structure of the semiconductor reliability test structure in Embodiment 4 only includes the second comb-like portion 32 on the same layer as the second metal line 23. Since the comb-like structure of Embodiment 4 only includes the second comb-like portion 32, the comb-like structure of the semiconductor reliability test structure in Embodiment 4 also includes a fourth pad 44. One end of the comb handle metal line 34 of the second comb-like portion 32 is connected to the fourth pad 44. The first pad 41 can apply a test voltage to the interconnect chain structure, and the second pad 42 can provide a reference potential (such as ground) to the interconnect chain structure; or the second pad 42 can apply a test voltage to the interconnect chain structure, and the first pad 41 can provide a reference potential (such as ground) to the interconnect chain structure, thereby completing the Rc test.
[0072] The fourth pad 44 can apply a test voltage to the second comb section 32, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect structure, thereby testing the Vbd / TDDB between the upper interconnect structure and the comb structure.
[0073] In Embodiment 4, the comb handle metal wire 34 of the second comb portion 32 is located on one side of the interconnect chain structure along the first direction. Similar to Embodiment 3, the other structures of Embodiment 4 are the same as those of Embodiment 1. Please refer to the detailed description of Embodiment 1, which will not be repeated here.
[0074] like Figure 13A As shown, the spacing between the comb-shaped metal lines 33 of the second comb-shaped portion 32 and the adjacent second metal lines 23 is set at equal intervals, for example, the spacing is b.
[0075] like Figure 13B As shown, in the interconnect unit chain 20, the spacing d between adjacent first metal lines 21 in the first direction is equal to the spacing c between second metal lines 23.
[0076] The linewidth of the first metal wire 21 is equal to the linewidth of the second metal wire 23, meaning the linewidth of the upper metal wire is the same as the linewidth of the lower metal wire. Similarly, the linewidth of the comb-tooth metal wire 33 of the second comb-shaped portion 32 is equal to the linewidth of the second metal wire 23. Figure 13A and Figure 13B As shown, B=C=D.
[0077] Example 5 The difference between the semiconductor reliability test structure in Example 5 and the semiconductor reliability test structure in Example 2 lies in the different comb-shaped structure. For example... Figure 14As shown, the comb-like structure includes a first comb-like portion 31 spaced apart from the interconnect chain structure. In other words, the comb-like structure of Embodiment 5 only includes the first comb-like portion 31 on the same layer as the first metal line 21. Since the comb-like structure of Embodiment 5 only includes the first comb-like portion 31, the comb-like structure of Embodiment 5 also includes a third pad 43. One end of the comb handle metal line 34 of the first comb-like portion 31 is connected to the third pad 43.
[0078] The first pad 41 can apply a test voltage to the interconnect structure, and the second pad 42 can provide a reference potential (such as ground) to the interconnect structure; or the second pad 42 can apply a test voltage to the interconnect structure, and the first pad 41 can provide a reference potential (such as ground) to the interconnect structure, thereby completing the Rc test.
[0079] The third pad 43 can apply a test voltage to the first comb section 31, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect structure, thereby testing the Vbd / TDDB between the lower interconnect structure and the comb structure.
[0080] In Embodiment 5, the comb handle metal wire 34 of the first comb-shaped portion 31 is located on one side of the interconnect chain structure along the first direction. The other structures of Embodiment 5 are the same as those of Embodiment 2, and can be referred to the detailed description of Embodiment 2, which will not be repeated here.
[0081] like Figure 15A As shown, the spacing between the comb-shaped metal lines 33 of the first comb-shaped portion 31 and the adjacent first metal lines 21 is set at equal intervals, for example, the spacing is a.
[0082] like Figure 15B As shown, the linewidth D of the first metal line 21 is smaller than the linewidth C of the second metal line 23, meaning the linewidth of the lower metal line is smaller than the linewidth of the upper metal line. However, the linewidth of the comb-tooth metal line 33 of the first comb-shaped portion 31 is equal to the linewidth of the first metal line 21. Figure 15A and Figure 15B As shown, A=D <C。
[0083] like Figure 15B As shown, since the linewidth D of the first metal line 21 is smaller than the linewidth C of the second metal line 23, the spacing d between adjacent first metal lines 21 in the first direction in the interconnect unit chain 20 is greater than the spacing c between second metal lines 23.
[0084] Example 6 The semiconductor reliability test structure in Example 6 is similar to that in Example 5, and its difference from the semiconductor reliability test structure in Example 2 lies in the different comb-like structure. For example... Figure 16As shown, the comb-like structure includes a second comb-like portion 32 spaced apart from the interconnect chain structure. In other words, the comb-like structure of the semiconductor reliability test structure in Embodiment Six only includes the second comb-like portion 32 on the same layer as the second metal line 23. Since the comb-like structure in Embodiment Three only includes the second comb-like portion 32, the comb-like structure of the semiconductor reliability test structure in Embodiment Six also includes a fourth pad 44. One end of the comb handle metal line 34 of the second comb-like portion 32 is connected to the fourth pad 44. The first pad 41 can apply a test voltage to the interconnect chain structure, and the second pad 42 can provide a reference potential (such as ground) to the interconnect chain structure; or the second pad 42 can apply a test voltage to the interconnect chain structure, and the first pad 41 can provide a reference potential (such as ground) to the interconnect chain structure, thereby completing the Rc test.
[0085] The fourth pad 44 can apply a test voltage to the second comb section 32, and the first pad 41 or the second pad 42 can provide a reference potential (such as ground) to the interconnect structure, thereby testing the Vbd / TDDB between the upper interconnect structure and the comb structure.
[0086] In Embodiment Six, the comb handle metal wire 34 of the second comb-shaped portion 32 is located on one side of the interconnect chain structure along the first direction. Similar to Embodiment Five, the other structures of Embodiment Six are the same as those of Embodiment Two, and can be referred to the detailed description of Embodiment Two, which will not be repeated here.
[0087] like Figure 17A As shown, the spacing between the comb-shaped metal lines 33 of the second comb-shaped portion 32 and the adjacent second metal lines 23 is set at equal intervals, for example, the spacing is b.
[0088] like Figure 17B As shown, the linewidth D of the first metal line 21 is smaller than the linewidth C of the second metal line 23, meaning the linewidth of the upper metal line is greater than the linewidth of the lower metal line. The linewidth of the comb-tooth metal line 33 of the second comb-shaped portion 32 is equal to the linewidth of the second metal line 23, i.e., as shown... Figure 17A and Figure 17B As shown, B=C>D.
[0089] The linewidth D of the first metal line 21 is smaller than the linewidth C of the second metal line 23, and the spacing d between adjacent first metal lines 21 in the first direction of the interconnection unit chain 20 is greater than the spacing c between second metal lines 23.
[0090] The linewidth of the first metal wire 21 is equal to the linewidth of the second metal wire 23, that is, the linewidth of the upper metal wire is the same as the linewidth of the lower metal wire, while the linewidth of the comb-shaped metal wire 33 of the second comb-like portion 32 is equal to the linewidth of the second metal wire 23, such as Figure 17A and Figure 17B As shown.
[0091] This concludes the description of the key structures of the semiconductor reliability testing structure of this application. Other structures may also be included in the complete semiconductor reliability testing structure, which will not be elaborated here.
[0092] The semiconductor reliability testing structure of this application embodiment simultaneously provides an interconnect chain structure and a comb structure on a semiconductor substrate. The interconnect chain structure includes multiple interconnect unit chains connected in series, each interconnect unit chain comprising multiple first metal lines in the lower layer, multiple second metal lines in the upper layer, and a first conductive via connecting the first and second metal lines. The comb structure includes a first comb portion and / or a second comb portion spaced apart from the interconnect chain structure. The first comb portion is on the same layer as the first metal lines, and the second comb portion is on the same layer as the second metal lines. This testing structure uses the interconnect chain structure to test the stress migration or electromigration parameter Rc, while simultaneously utilizing the comb structure... The combination of the structure and the interconnect chain structure allows for testing the breakdown voltage and / or breakdown over time between the interconnect chain and the first comb portion, and between the interconnect chain and the second comb portion. This enables the measurement of stress migration, electromigration parameter Rc, breakdown voltage, and / or breakdown over time using the test structure of this application, thereby saving the placement area of the test structure. Furthermore, the implementation of this semiconductor reliability test structure requires no additional process steps, thus avoiding additional cost burdens and keeping production costs controllable. Additionally, the design of the upper metal line width being greater than the lower metal line width in the embodiments of this application better matches the actual product structure and routing, resulting in reliability test data that is closer to the actual product.
[0093] Example 7 This application also provides a method for performing reliability testing using the above-described semiconductor reliability testing structure, the method comprising: In the first test mode, a test current signal is applied to one of the first pad and the second pad, while the other is grounded. The voltage difference between the first pad and the second pad is tested to test the stress migration or electromigration parameter Rc. This parameter is an important indicator for evaluating the reliability of metal interconnects and is used to monitor the failure risk of metal lines due to current stress or thermal stress.
[0094] Specifically, first, the test structure is placed in a preset test environment. For stress migration testing, the test structure is usually placed in a high-temperature environment to bake and accelerate stress; for electromigration testing, a constant current density stress is applied to the test structure.
[0095] In the electrical measurement stage, such as Figure 6As shown, test signals are applied to the first pad 41 and the second pad 42, which are connected to both ends of the interconnect chain structure. Specifically, a test current signal I is applied to the first pad 41, while the second pad 42 is grounded, thereby forming a test current path in the interconnect chain structure. At this time, the voltage difference V between the first pad 41 and the second pad 42 is measured by a voltage measuring device such as a voltmeter.
[0096] According to Ohm's law, the resistance Rc of an interconnect structure can be calculated using the formula Rc = V / I. This resistance Rc is a characterizing parameter for stress migration or electromigration.
[0097] For stress migration testing, it is necessary to measure the resistance change at multiple time points. For example, before high-temperature baking, the initial resistance value R0 is measured; after high-temperature storage for preset times (such as T1, T2, T3), the corresponding resistance values R1, R2, and R3 are measured respectively. The reliability performance of the interconnect structure under thermal stress is evaluated by calculating the resistance change rate ΔR = (Rn - R0) / R0 × 100% (n=1,2,3). If the resistance change rate exceeds a preset threshold, it indicates that there is a risk of failure such as voids or grain boundary migration in the metal layer.
[0098] For electromigration testing, resistance changes are continuously monitored under constant current stress. When the resistance value changes abruptly or reaches a preset failure criterion (such as a 10% increase in resistance), the failure time is recorded to evaluate the lifetime distribution and electromigration failure mechanism of the metal interconnect.
[0099] It should be noted that the first and second pads serve as the current application terminal and the ground terminal, respectively, while the voltage measurement path is independent of the current path. This effectively eliminates the influence of the test leads and contact resistance on the measurement results and improves the testing accuracy of the Rc parameter.
[0100] Through the first test mode described above, the embodiments of this application can accurately monitor the reliability of the metal layer, providing data support for the stability assessment of the process.
[0101] The method for performing reliability testing using the above-mentioned semiconductor reliability test structure also includes: in a second test mode, such as Figure 6 As shown, a test voltage signal is applied to the third pad 43 or the fourth pad 44, and at least one of the first pad 41 and the second pad 42 is grounded, for testing the breakdown voltage and / or breakdown over time between the interconnect chain located in the layer where the first metal line 21 is located and the first comb portion 31, or the breakdown voltage and / or breakdown over time between the interconnect chain located in the layer where the second metal line 23 is located and the second comb portion 32.
[0102] In this embodiment, the second test mode is used to evaluate the reliability of the dielectric layer, specifically including breakdown voltage testing and / or time-lapse breakdown testing. This mode utilizes the same-layer correspondence between the comb structure and the interconnect chain structure to achieve the breakdown characteristics and lifetime assessment of the dielectric layer between different metal layers.
[0103] In the first example, such as Figure 6 As shown, when it is necessary to evaluate the reliability of the dielectric layer of the layer where the first metal line is located, the test object is the dielectric region between the lower layer of the interconnect chain structure (e.g., the first metal line 21) and the first comb-shaped portion 31. Specifically, the first metal line 21 located in the lower layer of the interconnect chain structure and the comb-shaped metal line 33 interlaced between adjacent first metal lines 21 in the first comb-shaped portion 31 constitute a pair of test electrodes, and the dielectric layer between them is the object under test.
[0104] During testing, a test voltage signal is applied to the third pad 43 connected to the first comb-shaped portion 31, while at least one of the first pad 41 and the second pad 42 connected at both ends of the interconnect chain structure is grounded. Preferably, to form a complete test circuit, the first pad 41 and the second pad 42 can be grounded simultaneously, or either one of them can be grounded. At this time, the test voltage is applied between the comb tooth metal line 33 of the first comb-shaped portion 31 and the first metal line 21 and the connecting metal line 24 of the interconnect chain, and the electric field is distributed in the dielectric layer between them.
[0105] In the second example, when it is necessary to evaluate the reliability of the dielectric layer of the layer containing the second metal line 23, the test object is the dielectric region between the upper part of the interconnect chain structure and the second comb-shaped portion 32. Specifically, the second metal line 23 located in the upper layer of the interconnect chain structure and the comb-shaped metal lines 33 interlaced between adjacent second metal lines 23 in the second comb-shaped portion 32 constitute a test electrode pair.
[0106] During testing, a test voltage signal is applied to the fourth pad 44 connected to the second comb section 32, while at least one of the first pad 41 and the second pad 42 is grounded. The test voltage is applied between the comb tooth metal line 33 of the second comb section 32 and the second metal line 23 of the interconnect chain to evaluate the breakdown characteristics of the upper dielectric layer.
[0107] It should be noted that since the first comb-shaped part and the second comb-shaped part are located on both sides of the interconnect chain structure along the first direction, and the comb tooth metal lines of the two are staggered in the second direction, the above two test configurations do not interfere with each other and can be carried out independently according to test requirements.
[0108] Breakdown voltage testing is used to quickly assess the breakdown strength of the dielectric layer, and is typically performed using the voltage ramp method. In one example, the specific test steps are as follows: First, place the test structure in a room temperature test environment, and complete the test connection according to the first or second example described above.
[0109] Subsequently, the test program is initiated, applying a gradually increasing DC voltage signal to the corresponding third or fourth pad. During the voltage scan, leakage current changes are monitored in real time by a current monitoring unit connected to the first and / or second pad.
[0110] In the initial stage, as the applied voltage increases, the leakage current increases slowly, and the dielectric layer is in a normal insulating state. When the voltage rises to a certain critical value, the dielectric layer breaks down, and the leakage current rises sharply, usually manifesting as a sudden change in the order of magnitude of the current. The applied voltage value at this point is recorded as the breakdown voltage Vbd.
[0111] The test structure of this application can also be used for time-delay breakdown testing, which is used to evaluate the lifetime characteristics of the dielectric layer under long-term operating stress, and is typically performed using the constant voltage stress method or the constant current stress method. In one example, the specific test steps are as follows: The test connection method is the same as the breakdown voltage test. Select the corresponding third or fourth pad according to the location of the layer under test, apply the test signal, and ground at least one of the first and second pads.
[0112] Regarding the selection of test stress, the stress level for the time-lapse test can be set based on the Vbd value obtained from the breakdown voltage test. A constant voltage below Vbd is typically chosen as the test stress. The test structure is placed in a high-temperature environment to accelerate the aging process; the temperature can be set according to the test specifications.
[0113] During the test, the leakage current is continuously monitored, and the time from the application of stress to dielectric breakdown, i.e., the failure time Tbd, is recorded. The criteria for determining dielectric breakdown can be set according to the test specification. For example, when the leakage current exceeds a preset threshold or a sudden change in magnitude occurs, it is determined to be a breakdown failure.
[0114] The method for performing reliability testing using the above-mentioned semiconductor reliability testing structure further includes: in the third test mode, applying a test signal to the third pad or the fourth pad, grounding at least one of the first pad and the second pad, testing the leakage current between the interconnect chain located in the layer where the first metal line is located and the first comb portion, or the leakage current between the interconnect chain located in the layer where the second metal line is located and the second comb portion, and determining whether there is any contamination residue between the interconnect chain and the first comb portion and the second comb portion.
[0115] like Figure 7C , Figure 9C , Figure 11C , Figure 13C , Figure 15C , Figure 17C and Figure 18As shown, there may be residue 13 in the semiconductor reliability test structure. In the third test mode, a test signal is applied to the third pad or the fourth pad, and at least one of the first pad and the second pad is grounded. The leakage current between the interconnect chain and the first comb portion in the layer where the first metal line is located, or the leakage current between the interconnect chain and the second comb portion in the layer where the second metal line is located, is tested to determine whether there is contamination residue between the interconnect chain and the first comb portion and the second comb portion.
[0116] For example, taking the semiconductor reliability test structure of Embodiment 1 as an example, such as Figure 6 As shown and Figure 18 As shown, a test signal is applied to the fourth pad 44, and the first pad 41 is grounded. If there is residue 13 between the second metal line 23 and the comb-shaped metal line 33 of the second comb portion 32, this residue connects the second metal line 23 and the comb-shaped metal line 33 of the second comb portion 32 together, thus establishing a conductive path between the interconnect structure and the comb structure. At this time, the leakage current will be significantly abnormal. For example, if a 1V voltage is applied and the current reaches the current limit of 1mA, it indicates a short circuit in the reliability test structure, i.e., there is an abnormal leakage current. Therefore, by checking whether the current is normal, it is possible to determine whether there is an abnormal leakage current, and thus whether there is residual contamination between the second metal line 23 and the second comb portion 32. Based on the same principle, the leakage current can be used to determine whether there is residual contamination between the first metal line 21 and the first comb portion 31.
[0117] When leakage current anomalies are detected during testing, subsequent stress migration tests will no longer be performed. Instead, failure analysis will be conducted on the structure with abnormal leakage current values to identify process defects and provide feedback, which can significantly save process iteration time.
[0118] This concludes the description of the key steps of the reliability testing method of this application. A complete reliability testing method may include other steps, which will not be elaborated here.
[0119] The reliability testing method of this application embodiment can not only use a test structure to complete stress migration or electromigration parameter Rc testing and breakdown voltage and / or time-dependent breakdown testing between interconnect chains and comb structures, but also determine whether there is contamination residue between interconnect chains and comb structures by the leakage current between interconnect chains and comb structures, thereby effectively reducing the impact of contamination residue on process reliability and improving the accuracy of reliability testing.
[0120] Although several embodiments have been described herein, it should be understood that many other modifications and embodiments will arise in the mind of those skilled in the art, all of which will fall within the spirit and scope of the concept disclosed herein. More specifically, various modifications and changes may be made in terms of the arrangement and / or components of the subject matter within the scope of this disclosure, the drawings, and the appended claims. In addition to modifications and changes in the components and / or arrangement, the use of alternative methods will also be obvious to those skilled in the art.
Claims
1. A semiconductor reliability testing structure, characterized in that, The semiconductor reliability testing structure includes: A semiconductor substrate, an interconnect chain structure and a comb structure disposed on the semiconductor substrate, wherein the interconnect chain structure and the comb structure are both embedded in a dielectric layer and spaced apart from each other; The interconnect chain structure includes an interconnect chain formed by multiple interconnect unit chains connected in series. The multiple interconnect unit chains are spaced apart along a first direction and extend along a second direction. The interconnect unit chain includes multiple first metal lines spaced apart along the second direction in the lower layer, multiple second metal lines spaced apart along the second direction in the upper layer, and multiple first conductive vias spaced apart along the second direction connecting the first metal lines and the second metal lines. The projection of the first conductive via on the semiconductor substrate is located within the overlapping portion of the projections of the first metal lines and the second metal lines on the semiconductor substrate. Both the first and second metal lines extend along the second direction, and the first conductive via extends along a third direction. The first direction and the second direction are perpendicular to each other and parallel to the semiconductor substrate, and the third direction is perpendicular to the semiconductor substrate. The comb-like structure includes a first comb-like portion and / or a second comb-like portion spaced apart from the interconnect chain structure. The first comb-like portion is on the same layer as the first metal wire, and the second comb-like portion is on the same layer as the second metal wire. Both the first comb-like portion and the second comb-like portion include a plurality of comb-tooth metal wires extending along the first direction and spaced apart along the second direction, and a comb handle metal wire connecting the plurality of comb-tooth metal wires and extending along the second direction. The comb-tooth metal wires are disposed between adjacent first metal wires or between second metal wires, and the comb handle metal wire is located on one side of the interconnect chain structure along the first direction.
2. The reliability testing structure as described in claim 1, characterized in that, The interconnect chain structure further includes at least one connection structure for connecting adjacent interconnect unit chains. The connection structure includes a connecting metal line extending along the first direction and two second conductive vias extending along the third direction and arranged along the first direction. The connecting metal line is located on the same layer as the first metal line or the second metal line and is spaced apart with equal linewidth. The second conductive vias connect the connecting metal line and the second metal line or the first metal line. The projection of the second conductive via on the semiconductor substrate is located within the overlapping portion of the projection of the connecting metal line on the semiconductor substrate and the projection of the second metal line or the first metal line on the semiconductor substrate. All the connecting metal lines in the interconnect chain structure are spaced apart from each other, and the second conductive vias are the same size as the first conductive vias.
3. The reliability testing structure as described in claim 1, characterized in that, The first metal wire and the second metal wire in the interconnect unit chain are staggered in the second direction, and the first conductive via is connected between the end of the first metal wire and the corresponding end of the second metal wire.
4. The reliability testing structure as described in claim 1, characterized in that, The comb-like structure includes a first comb-like portion and a second comb-like portion. The comb teeth metal wires of the first comb-like portion are located between adjacent first metal wires, and the comb teeth metal wires of the second comb-like portion are located between adjacent second metal wires. The lengths of the comb teeth metal wires of the first comb-like portion and the second comb-like portion are both greater than the dimensions of the interconnect chain structure along the first direction. The comb handle metal wires of the first comb-like portion and the comb handle metal wires of the second comb-like portion are located on both sides of the interconnect chain structure along the first direction.
5. The reliability testing structure as described in claim 4, characterized in that, The comb-shaped metal wires of the first comb portion and the comb-shaped metal wires of the second comb portion are arranged alternately in the second direction.
6. The reliability testing structure as described in claim 1, characterized in that, The linewidth of the comb teeth metal wire in the first comb-shaped portion is equal to the linewidth of the first metal wire, and the linewidth of the comb teeth metal wire in the second comb-shaped portion is equal to the linewidth of the second metal wire.
7. The reliability test structure as described in claim 6, characterized in that, The spacing between the comb teeth metal wires of the first comb-shaped portion and the adjacent first metal wires is set at equal intervals, and the spacing between the comb teeth metal wires of the second comb-shaped portion and the adjacent second metal wires is set at equal intervals.
8. The reliability test structure as described in claim 7, characterized in that, The spacing between adjacent first metal lines in the interconnect unit chain is equal to the spacing between the second metal lines.
9. The reliability testing structure as described in claim 1, characterized in that, The interconnect chain structure further includes a first pad and a second pad, wherein the first pad is connected to one end of the interconnect chain and the second pad is connected to the other end of the interconnect chain; The comb-like structure further includes a third pad and / or a fourth pad, one end of the comb handle metal wire of the first comb-like portion is connected to the third pad, and one end of the comb handle metal wire of the second comb-like portion is connected to the fourth pad.
10. A method for performing reliability testing using the semiconductor reliability testing structure as described in claim 9, characterized in that, The method includes: In the first test mode, a test current signal is applied to one of the first pad and the second pad, while the other is grounded, and the voltage difference between the first pad and the second pad is tested to test the stress migration or electromigration parameter Rc. In the second test mode, a test voltage signal is applied to the third pad or the fourth pad, and at least one of the first pad and the second pad is grounded, for testing the breakdown voltage and / or breakdown over time between the interconnect chain and the first comb portion located in the layer where the first metal line is located, or the breakdown voltage and / or breakdown over time between the interconnect chain and the second comb portion located in the layer where the second metal line is located. In the third test mode, a test signal is applied to the third pad or the fourth pad, at least one of the first pad and the second pad is grounded, and the leakage current between the interconnect chain located on the layer where the first metal line is located and the first comb portion, or the leakage current between the interconnect chain located on the layer where the second metal line is located and the second comb portion, is tested to determine whether there is any contamination residue between the interconnect chain and the first comb portion and the second comb portion.