Chip Packaging Structure and Fabrication Method
By using solder components with melting points higher than the subsequent operating temperatures in the chip packaging structure, especially copper pillars and mating layers, the delamination problem caused by warpage and stress in large-size chip packaging is solved, improving the stability and reliability of the packaging structure.
Patent Information
- Application Number
- CN202611207336.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-10
- Publication Date
- 2026-11-17
AI Technical Summary
In large-size 2.5D CoWoS packages, there is a significant risk of delamination between the CoW die and the underfill due to warpage and stress, especially during pre-connection reflow and end-board SMT processes for package reliability, where the low melting point of existing solder components leads to insufficient bonding.
The system employs solder components with melting points higher than the subsequent operating temperatures of the packaging structure, including copper pillars and mating layers. By welding the solder components to the substrate at high temperatures, it ensures that the solder components do not melt in high-temperature environments, reducing the risk of delamination. Furthermore, the rectangular array layout reduces the high-temperature exposure time.
It effectively reduces the risk of delamination between the bottom filler material and the chip, improves the stability of the packaging structure, is suitable for large-size wafer-level chips and packaging structures, and avoids damage to the chip and substrate caused by prolonged high temperatures.
Smart Images

Figure CN123124856A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of chip packaging technology, and in particular to a chip packaging structure and its fabrication method. Background Technology
[0002] As the size of 2.5D CoWoS Packaging (Chip on Wafer on Substrate Packaging) increases, the CoW die also becomes larger, leading to a greater risk of delamination between the CoW die and the underfill due to warpage and stress.
[0003] Specifically, in existing chip packaging structures, the composition of the CoW die bump (wafer-level chip bump) is SnAg1.8, the composition of the sub-bump (substrate bump) is SAC305 / SnCu0.7, and the composition of the Package BGA Ball (ball grid array package ball) is SAC305, all with melting points below 230℃. However, during the ball mount process, the pre-con reflow process for packaging reliability, and the surface mount technology (SMT) process, the reflow soldering pin temperature (peak temperature) is between 240℃ and 260℃. Therefore, during the ball mount process, the pre-con reflow process for packaging reliability, and the SMT process for the final board, the bump that has been soldered between the CoW die and the substrate will melt again. As a result, in the above processes, the bonding ability between the CoW die and the substrate is provided only by the underfill, which greatly increases the risk of detachment between the underfill and the CoW die. Summary of the Invention
[0004] To address the aforementioned issues, the chip packaging structure and its fabrication method provided by this invention utilize a solder with a melting point higher than the subsequent operating temperature of the chip packaging structure to achieve chip-substrate bonding, thereby reducing the risk of delamination between the bottom filler material and the chip.
[0005] In a first aspect, the present invention provides a chip packaging structure, the chip packaging structure comprising: a chip and a substrate;
[0006] Multiple first welding components are provided between the chip and the substrate. The chip is welded to the substrate through the first welding components. The lowest melting point of the first welding components is higher than the subsequent operating temperature of the chip packaging structure. The bottom of the chip is also filled with underfill material to bond the chip to the substrate.
[0007] Optionally, the subsequent operating temperatures of the chip package structure include: the reflow temperature when solder balls are soldered onto the surface of the substrate away from the chip, and the reflow temperature when the substrate is soldered to the terminals via solder balls.
[0008] Optionally, a second welding element is provided between the chip and the substrate, and the chip is welded to the substrate through the second welding element. The lowest melting point of the second welding element is lower than the lowest melting point of the first welding element.
[0009] Optionally, the first weldment is located outside the second weldment in the horizontal direction.
[0010] Optionally, the first welding component includes a first upper bump fixed to the lower surface of the chip and a first lower bump fixed to the upper surface of the substrate; The first upper bump and the first lower bump are one-to-one correspondences. The first upper bump is welded to the corresponding lower bump. The melting points of the first upper bump and the first lower bump are both higher than the subsequent operating temperature of the chip packaging structure.
[0011] Optionally, the first upper bump includes: a copper pillar and a mating layer; The top of the copper pillar is fixedly connected to the chip, and the bottom of the copper pillar is fixedly connected to the mating layer.
[0012] Optionally, the material of the mating layer includes an interface layer and a barrier layer stacked sequentially from bottom to top; The interface layer is used for bonding to the first lower bump, and the barrier layer is used to prevent the material on the bottom of the chip from diffusing with the material of the interface layer.
[0013] Alternatively, the material of the first lower bump may include tin, antimony, and nickel.
[0014] In a second aspect, the present invention provides a method for fabricating a chip packaging structure, the method comprising: A chip and a substrate are provided. The lower surface of the chip is fixedly provided with multiple first upper bumps, and the upper surface of the substrate is fixedly provided with multiple first lower bumps. The first upper bumps and the first lower bumps correspond one to one. The melting points of the first upper bumps and the first lower bumps are both higher than the subsequent operating temperature of the chip packaging structure. The first upper bump and the corresponding first lower bump are soldered together using a preset temperature, which is higher than the subsequent operating temperature of the chip package structure.
[0015] Optionally, a plurality of second upper bumps are fixedly provided on the lower surface of the chip, and a plurality of second lower bumps are fixedly provided on the upper surface of the substrate. The second upper bumps and the second lower bumps correspond one to one, and the melting point of the second lower bump is lower than the melting point of the first lower bump. The step of welding the first upper protrusion and the corresponding first lower protrusion together using a preset temperature includes: welding the first upper protrusion and the corresponding first lower protrusion together using a preset temperature, and welding the second upper protrusion and the corresponding second lower protrusion together.
[0016] The chip packaging structure and its fabrication method provided in this invention achieve chip-substrate bonding through soldering components with melting points higher than the subsequent operating temperature of the chip packaging structure. This ensures that some or all of the soldering components connecting the chip and the substrate will not melt during subsequent reflow soldering of the chip packaging structure. This avoids the situation where the bonding ability between the chip and the substrate relies solely on the underfill material during subsequent reflow soldering of the chip packaging structure, thereby reducing the risk of delamination between the underfill material and the chip. Attached Figure Description
[0017] To more clearly illustrate the technical solutions in the embodiments of this application or the conventional technology, the drawings used in the description of the embodiments or the conventional technology will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0018] Figure 1 This is a schematic cross-sectional view of a chip packaging structure according to an embodiment of this application; Figure 2 This is a schematic top view of a substrate according to an embodiment of this application; Figure 3 A schematic cross-sectional view of a chip according to an embodiment of this application. Figure 4 This is a schematic cross-sectional view of a substrate according to an embodiment of this application.
[0019] Figure label: 1. Chip; 2. Substrate; 31. First weldment; 311. First upper bump; 312. First lower bump; 32. Second weldment; 321. Second upper bump; 322. Second lower bump; 331. Copper pillar; 332. Butt layer; 4. Bottom filler material; 51. Solder ball; 52. Reinforcing sheet. Detailed Implementation
[0020] To facilitate understanding of this application, a more complete description will be provided below with reference to the accompanying drawings, which illustrate embodiments of the present application. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that the disclosure of this application will be thorough and complete.
[0021] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application.
[0022] Spatial relation terms such as "below," "under," "below," "below," "above," and "above" are used here to describe the relationship between one element or feature shown in the figure and other elements or features. Similarly, "directly above" can be used here to describe an element or feature shown in the figure that coincides in a vertical straight line direction, which may be partial or complete, depending on the actual situation or the content of the illustration. It should be understood that, in addition to the orientation shown in the figure, spatial relation terms also include different orientations of the device in use and operation. For example, if the device in the figure is flipped, the element or feature described as "below," "below," or "below" of other elements will be oriented "above" other elements or features. Therefore, the exemplary terms "below" and "below" can include both upper and lower orientations. Furthermore, the device may also include other orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptive terms used herein will be interpreted accordingly.
[0023] It should be noted that when an element is referred to as "fixedly connected" to another element, it can be directly on the other element or there may be an intervening element. When an element is considered to be "connected" to another element, it can be directly connected to the other element or there may be an intervening element. Conversely, when an element is referred to as being "directly on" another element, there is no intervening element. The terms "vertical," "horizontal," "left," "right," and similar expressions used in this document are for illustrative purposes only.
[0024] It should also be understood that the terms “including / comprise” or “have” specify the presence of the stated features, wholes, steps, operations, components, parts, or combinations thereof, but do not preclude the possibility of the presence or addition of one or more other features, wholes, steps, operations, components, parts, or combinations thereof.
[0025] First, the technical terms involved in this invention will be explained as follows: CoW: Chip on Wafer, a chip bonding and reconfiguration technology for wafer fabrication. CoWoS: A 2.5D packaging structure; Sub: Substrate: The substrate used for I / O interconnection with the chip; Under-fill: Used to fill the gaps between chip bumps through capillary action; SAC305: Sn accounts for 96.5%, Ag accounts for 3%, and Cu accounts for 0.5%; SnCu0.7: Sn accounts for 99.3% and Cu accounts for 0.7%.
[0026] In a first aspect, one embodiment of the present invention provides a chip packaging structure, see [link to...]. Figure 1 The chip packaging structure includes: chip 1 and substrate 2.
[0027] A plurality of first solder joints 31 are disposed between the chip 1 and the substrate 2. The chip 1 is soldered to the substrate 2 through the first solder joints 31, and the lowest melting point of the first solder joints 31 is higher than the subsequent operating temperature of the chip package structure. The bottom of the chip 1 is also filled with an underfill material 4 to bond the chip 1 to the substrate 2.
[0028] Understandably, when the material used in the first weldment 31 is the same, its lowest melting point is the melting point of that material; when the first weldment 31 is composed of components made of different materials arranged vertically, the lowest melting point is the melting point corresponding to the component with the lowest melting point; in addition to being welded through the first weldment 31, the chip 1 and the substrate 2 can also be welded together with other weldments whose melting points are lower than the lowest melting point of the first weldment 31 and whose subsequent operating temperature is lower than the lowest melting point of the first weldment 31.
[0029] The chip packaging structure provided in this embodiment achieves the welding of chip 1 and substrate 2 through soldering components with melting points higher than the subsequent operating temperature of the chip packaging structure. This ensures that some or all of the soldering components connecting chip 1 and substrate 2 will not melt during subsequent reflow soldering of the chip packaging structure. This avoids the situation where the bonding ability between chip 1 and substrate 2 is provided solely by the underfill material 4 during subsequent reflow soldering of the chip packaging structure, thereby reducing the risk of delamination between the underfill material 4 and chip 1.
[0030] The subsequent operating temperatures of the chip package structure include, but are not limited to: the reflow temperature when the substrate 2 is soldered with solder balls 51 on the surface away from the chip 1, and the reflow temperature when the substrate 2 is soldered to the terminal via the solder balls 51. In addition, the subsequent operating temperatures may also include the temperatures generated when the chip package structure is used for package reliability certification and routine monitoring of samples. The terminal may be a circuit board on a device.
[0031] In this embodiment, a second solder joint 32 is also provided between the chip 1 and the substrate 2. The chip 1 is soldered to the substrate 2 through the second solder joint 32, and the lowest melting point of the second solder joint 32 is lower than the lowest melting point of the first solder joint 31. Compared with the scheme of using only the first solder joint 31 to solder the chip 1 to the substrate 2, the use of the first solder joint 31 and the second solder joint 32 can effectively reduce the number of first solder joints 31. Therefore, during the process of soldering the chip 1 to the substrate 2 together, the time required to solder the chip 1 to the substrate 2 using a temperature higher than the melting point of the first solder joint 31 and the first solder joint 31 and the second solder joint 32 can be effectively shortened, thereby avoiding damage to the chip 1 or the substrate 2 caused by prolonged high temperature.
[0032] It is understandable that chip 1 is not only welded to substrate 2 through first welding component 31 and second welding component 32, but also electrically connected to substrate 2 through first welding component 31 and second welding component 32.
[0033] Furthermore, combined Figure 1 and Figure 2 The first weldment 31 is located outside the second weldment 32 in the horizontal direction. Taking the weldment components for welding chip 1 and substrate 2 as an example, which are arranged in a rectangular array between chip 1 and substrate 2, the outer weldment component is the first weldment 31, and the inner area of the first weldment 31 is the second weldment 32. That is, the weldment components from the outside to the inside are the first weldment 31 and the second weldment 32.
[0034] It should be noted that the number of outer rings of the first welding component 31 is determined by the size of the chip 1 being welded. The larger the size of the chip 1, the more outer rings the first welding component 31 needs to have. This embodiment does not impose a specific limitation on this. The welding component used to weld the chip 1 to the substrate 2 employs 11... Taking the rectangular array arrangement of 11 between chip 1 and substrate 2 as an example, the outer two rings of welding parts are all first welding parts 31, and the inner area of the first welding parts 31 is all second welding parts 32.
[0035] By limiting the relative positions of the first weldment 31 and the second weldment 32, deformation of the edge parts of the chip 1 where stress is concentrated can be effectively avoided in the subsequent high-temperature environment, thereby further reducing the risk of delamination between the bottom filler material 4 and the chip 1.
[0036] In a further optional embodiment of this embodiment, combined with Figure 1 , Figure 3 and Figure 4The first welding component 31 includes a first upper bump 311 fixed to the lower surface of the chip 1 and a first lower bump 312 fixed to the upper surface of the substrate 2. The first upper bump 311 and the first lower bump 312 correspond one-to-one. The first upper bump 311 is welded to the corresponding lower bump. The melting points of the first upper bump 311 and the first lower bump 312 are both higher than the subsequent operating temperature of the chip packaging structure.
[0037] The first upper bump 311 includes a copper pillar 331 and a mating layer 332. The top end of the copper pillar 331 is fixedly connected to the chip 1, and the bottom end of the copper pillar 331 is fixedly connected to the mating layer 332. The mating layer 332 is used to improve the stability of the welding between the copper pillar 331 and the first lower bump 312. The melting point of the first lower bump 312 is not lower than 265 degrees Celsius, and the material of the first lower bump 312 includes, but is not limited to, tin, antimony, and nickel. In this embodiment, the lowest melting point of the first weldment 31 is the melting point of the first lower bump 312, and the material of the mating layer 332 includes an interface layer and a barrier layer stacked sequentially from bottom to top.
[0038] Among them, the copper pillar 331, as the main structure of the first upper bump 311, can reduce the manufacturing cost of the first upper bump 311, and its material is copper; the interface layer is used to weld with the first lower bump 312 so that the first upper bump 311 has a high-quality welding interface, thereby improving the stability of the welding between the copper pillar 331 and the first lower bump 312; the barrier layer is used to prevent the material at the bottom of the chip from diffusing with the material of the interface layer.
[0039] In this embodiment, the barrier layer is made of materials including, but not limited to, nickel, and the interface layer is made of gold. The top of the copper pillar is fixedly connected to the pads on chip 1, and the pads are made of aluminum. This barrier layer prevents the materials of the pads and the interface layer from diffusing into each other, thereby avoiding the formation of high-resistivity intermetallic compounds, such as Al-Au alloys, between the pads and the interface layer. This prevents the resistance of the first solder joint 31 from spiked or from breaking.
[0040] Simultaneously, the barrier layer can react with the tin in the solder during the welding process of the first upper bump 311 and the first lower bump 312 to form a uniform and dense IMC (such as Ni3Sn4) structure. This IMC structure has high strength and stable conductivity, which can significantly improve the bonding force between the first welded component 31 and the chip and substrate, avoiding problems such as poor soldering or detachment at the welding interface. In addition, using nickel as a barrier layer also improves the mechanical strength of the first upper bump 311, especially in scenarios such as thermal cycling and vibration after chip packaging, which can reduce the risk of cracking of the first welded component 31 due to the difference in thermal expansion coefficients.
[0041] The second welding component 32 includes a second upper bump 321 fixed to the lower surface of the chip 1 and a second lower bump 322 fixed to the upper surface of the substrate 2. The second upper bump 321 and the second lower bump 322 correspond one-to-one, and the second upper bump 321 is welded to the corresponding lower bump.
[0042] The lowest melting point of the second welded part 32 is the melting point of the second lower protrusion 322. The material and structure of the second upper protrusion 321 are the same as those of the first upper protrusion 311. The material of the second lower protrusion 322 includes, but is not limited to, SAC305 or SnCu0.7.
[0043] In this embodiment, the subsequent operating temperature of the chip packaging structure is below 265 degrees Celsius. A plurality of solder balls 51 are fixedly disposed on the lower surface of the substrate 2. The material of the solder balls 51 is SAC305. A reinforcing sheet 52 is fixedly disposed on the upper surface of the substrate 2. The reinforcing sheet 52 is fixedly connected to the substrate 2 by an adhesive.
[0044] The chip packaging structure provided in this embodiment has high stability and effectively reduces the risk of delamination between the bottom filler material 4 and the chip 1. It is particularly suitable for large-size wafer-level chips and large-size packaging structures.
[0045] In a second aspect, an embodiment of the present invention provides a method for fabricating a chip packaging structure as described in the first aspect, the method comprising steps S101 to S102.
[0046] Step S101: Provide chip 1 and substrate 2.
[0047] In this chip, a plurality of first upper bumps 311 are fixedly disposed on the lower surface of the chip 1, and a plurality of first lower bumps 312 are fixedly disposed on the upper surface of the substrate 2. The first upper bumps 311 and the first lower bumps 312 correspond one to one, and the melting points of the first upper bumps 311 and the first lower bumps 312 are both higher than the subsequent operating temperature of the chip packaging structure.
[0048] Step S102: Weld the first upper protrusion 311 and the corresponding first lower protrusion 312 together using a preset temperature.
[0049] The preset temperature is higher than the subsequent operating temperature of the chip packaging structure and not lower than the melting point of the first lower bump 312; the melting points of the first upper bump 311 and the second upper bump 321 are both higher than the preset temperature and the subsequent operating temperature.
[0050] In this embodiment, the preset temperature is not lower than the lowest melting point of the first lower protrusion 312, and the lowest melting point of the first lower protrusion 312 is not lower than 265 degrees Celsius.
[0051] Furthermore, a plurality of second upper bumps 321 are fixedly disposed on the lower surface of the chip 1, and a plurality of second lower bumps 322 are fixedly disposed on the upper surface of the substrate 2. The second upper bumps 321 and the second lower bumps 322 correspond one to one, and the melting point of the second lower bumps 322 is lower than the melting point of the first lower bumps 312.
[0052] The step of welding the first upper protrusion 311 and the corresponding first lower protrusion 312 together using a preset temperature includes: welding the first upper protrusion 311 and the corresponding first lower protrusion 312 together using a preset temperature, and welding the second upper protrusion 321 and the corresponding second lower protrusion 322 together.
[0053] It should be noted that during the process of welding the first upper protrusion 311 to the corresponding first lower protrusion 312 and the second upper protrusion 321 to the corresponding second lower protrusion 322 at a preset temperature, only the first lower protrusion 312 and the second lower protrusion 32 change from a solid state to a molten state in order to be welded to the corresponding first upper protrusion 311 and the second upper protrusion 321.
[0054] In this embodiment, after step S102, the preparation method further includes: fixing the solder ball 51 to the lower surface of the substrate 2 at a temperature lower than a preset temperature; and fixing the solder ball 51 to the terminal at a temperature lower than a preset temperature.
[0055] The chip packaging structure fabrication method provided in this embodiment is simple to operate and effectively reduces the risk of delamination between the bottom filler material 4 and the chip 1. It is particularly suitable for large-size wafer-level chips and large-size packaging structures.
[0056] In the description of this specification, the references to terms such as "some embodiments," "other embodiments," "ideal embodiments," etc., refer to specific features, structures, materials, or characteristics described in connection with that embodiment or example that are included in at least one embodiment or example of this application. In this specification, the illustrative descriptions of the above terms do not necessarily refer to the same embodiments or examples.
[0057] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0058] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of this patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.
Claims
1. A chip packaging structure, characterized in that, The chip packaging structure includes: a chip and a substrate; A plurality of first welding components are disposed between the chip and the substrate, and the chip is welded to the substrate through the first welding components. The lowest melting point of the first welding components is higher than the subsequent operating temperature of the chip packaging structure. The bottom of the chip is also filled with an underfill material to bond the chip to the substrate.
2. The chip packaging structure according to claim 1, characterized in that, The subsequent operating temperatures of the chip packaging structure include: the reflow temperature when solder balls are soldered onto the surface of the substrate away from the chip, and the reflow temperature when the substrate is soldered to the terminal through the solder balls.
3. The chip packaging structure according to claim 1, characterized in that, A second welding element is also provided between the chip and the substrate. The chip is welded to the substrate through the second welding element, and the lowest melting point of the second welding element is lower than the lowest melting point of the first welding element.
4. The chip packaging structure according to claim 3, characterized in that, The first welded component is located outside the second welded component in the horizontal direction.
5. The chip packaging structure according to claim 1, characterized in that, The first welding component includes a first upper bump fixed to the lower surface of the chip and a first lower bump fixed to the upper surface of the substrate; The first upper bump and the first lower bump are in one-to-one correspondence. The first upper bump is welded to the corresponding lower bump. The melting point of the first upper bump and the first lower bump are both higher than the subsequent operating temperature of the chip packaging structure.
6. The chip packaging structure according to claim 5, characterized in that, The first upper protrusion includes: a copper pillar and a mating layer; The top end of the copper pillar is fixedly connected to the chip, and the bottom end of the copper pillar is fixedly connected to the mating layer.
7. The chip packaging structure according to claim 6, characterized in that, The material of the docking layer includes an interface layer and a barrier layer stacked sequentially from bottom to top; The interface layer is used for welding to the first lower bump, and the barrier layer is used to prevent the material on the bottom of the chip from diffusing with the material of the interface layer.
8. The chip packaging structure according to claim 5, characterized in that, The materials of the first lower bump include tin, antimony, and nickel.
9. A method for fabricating a chip packaging structure, characterized in that, The preparation method includes: A chip and a substrate are provided. The lower surface of the chip is fixedly provided with a plurality of first upper bumps, and the upper surface of the substrate is fixedly provided with a plurality of first lower bumps. The first upper bumps and the first lower bumps correspond one to one. The melting points of the first upper bumps and the first lower bumps are both higher than the subsequent operating temperature of the chip packaging structure. The first upper bump and the corresponding first lower bump are soldered together at a preset temperature, which is higher than the subsequent operating temperature of the chip package structure.
10. The preparation method according to claim 9, characterized in that, The lower surface of the chip is also fixedly provided with a plurality of second upper bumps, and the upper surface of the substrate is also fixedly provided with a plurality of second lower bumps. The second upper bumps and the second lower bumps correspond one to one, and the melting point of the second lower bump is lower than the melting point of the first lower bump. The step of welding the first upper protrusion and the corresponding first lower protrusion together using a preset temperature includes: welding the first upper protrusion and the corresponding first lower protrusion together using a preset temperature, and welding the second upper protrusion and the corresponding second lower protrusion together.