Battery cell packaging device
By using a mold structure with a support portion to limit thermal expansion and a beryllium copper heating block during the high-temperature sealing process of lithium secondary batteries, the problem of uneven sealing thickness was solved, and efficient production and stability of battery cells were achieved.
Patent Information
- Application Number
- CN202580027668.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-03-17
- Filing Date
- 2025-11-18
- Publication Date
- 2026-11-17
AI Technical Summary
During the high-temperature sealing process of lithium secondary batteries, the excessive thermal deformation of the bat-ear section and the degassing section leads to uneven sealing thickness, increasing the defect rate and rework burden.
The mold structure includes support components. Thermal expansion is limited by the first mold and the heating block. The heating block, made of beryllium copper, provides uniform heat. Multiple support components are combined on both sides of the mold to control thermal expansion deviation and ensure uniformity of the seal thickness.
This reduces thermal deformation deviation in the bat-ear section and degassing section, improves sealing quality and production efficiency, reduces defect rate and maintenance costs, and ensures the stability and reliability of battery cells.
Smart Images

Figure CN123125098A_ABST
Abstract
Description
Technical Field
[0001] Cross-references to related applications
[0002] This application claims priority and benefit to Korean Patent Application No. 10-2025-0033839, filed on March 17, 2025, the entire contents of which are incorporated herein by reference.
[0003] This disclosure relates to a battery cell packaging device for sealing battery cells, and more specifically, to a battery cell packaging device capable of reducing thermal deformation during high-temperature sealing and improving the uniformity of the seal thickness. Background Technology
[0004] In modern society, with the daily use of portable devices such as mobile phones, laptops, camcorders, and digital cameras, technological development in fields related to these mobile devices is very active. Furthermore, rechargeable / dischargeable secondary batteries are being used as power sources for electric vehicles (EVs), hybrid electric vehicles (HEVs), and plug-in hybrid electric vehicles (P-HEVs) in an attempt to address issues such as air pollution caused by existing gasoline vehicles using fossil fuels. Therefore, the need for developing secondary batteries is increasing.
[0005] Currently commercially available rechargeable batteries include nickel-cadmium (NiCd), nickel-metal hydride (NiMH), nickel-zinc (NiZn), and lithium-ion batteries. Among these, lithium-ion batteries have become the focus due to their advantages, such as exhibiting almost no memory effect compared to nickel-based batteries, allowing for free charging and discharging, and possessing a very low self-discharge rate and high energy density.
[0006] This type of lithium secondary battery primarily uses lithium-based oxide and carbon materials as the positive and negative electrode active materials, respectively. The lithium secondary battery includes an electrode assembly and a battery casing. In the electrode assembly, positive and negative electrode plates, respectively coated with positive and negative electrode active materials, are arranged with a separator inserted between them. The battery casing seals and houses the electrode assembly along with the electrolyte.
[0007] Generally, based on the shape of the external material, lithium secondary batteries can be classified into can-type secondary batteries in which the electrode components are built into a metal can, and bag-type secondary batteries in which the electrode components are built into a bag of aluminum laminate.
[0008] Pouch cells are manufactured by sealing electrode assemblies and electrolytes with aluminum laminates, where a sealing process is performed at the joints of the external materials under high temperature and pressure. However, during this high-temperature sealing process, thermal deformation resulting from combining materials with different thermal expansion properties may prevent the uniform maintenance of the seal thickness. In particular, structural deformation is likely to concentrate at the batwing or degassing areas of the cell, potentially leading to increased defect rates and rework burdens.
[0009] Therefore, the importance of technologies that can effectively control the amount of thermal deformation generated during the high-temperature sealing process of battery cells and uniformly maintain the seal thickness is becoming increasingly apparent. In response to this need, various studies have been conducted, such as utilizing the bimetallic effect to induce "desired deformation" at high temperatures by joining materials with different coefficients of thermal expansion. The battery cell packaging device disclosed herein relates to a technology designed to solve these problems and improve efficiency in the production process. Summary of the Invention
[0010] Technical issues
[0011] The purpose of this disclosure is to suppress defects in the batwing and degassing portions of battery cells caused by thermal deformation during the high-temperature sealing process, and to further ensure the uniformity of the seal thickness, thereby improving the efficiency of the production process.
[0012] However, the technical objectives to be addressed by the embodiments of this disclosure are not limited to the above objectives, but can be extended in various ways within the scope of the technical concepts included in this disclosure.
[0013] Technical solution
[0014] According to one aspect of this disclosure, a battery cell packaging apparatus is provided, comprising: a first mold; a first heating block coupled to the first mold; and a first sealing tool configured to attach to the first heating block and seal the battery cell, wherein the first mold includes a support portion that restricts thermal expansion.
[0015] In one embodiment, the support portion may be provided in multiple forms and may be positioned on both sides of the first mold.
[0016] In one embodiment, the support portion may be arranged to protrude from the periphery of the first mold.
[0017] In one embodiment, the first mold may be integrally formed with the support portion.
[0018] In one embodiment, the support portion may include an inclined shape in which its width gradually increases in the direction away from the first sealing tool.
[0019] In one embodiment, the first heating block may include beryllium copper (Be-Cu) material.
[0020] In one embodiment, the battery cell packaging device may further include: a second mold; a second heating block connected to the second mold; and a second sealing tool attached to the second heating block.
[0021] In one embodiment, the battery cell can be compressed and sealed between the first sealing tool and the second sealing tool.
[0022] Beneficial effects
[0023] According to embodiments of this disclosure, a mold structure including a support portion that restricts thermal expansion during the high-temperature sealing process is applied, thereby reducing deviations in thermal expansion and deformation of the batwing and degassing portions of the mold due to thermal expansion occurring at high temperatures. Therefore, uniform sealing quality of the battery cells can be ensured.
[0024] The effects of this disclosure are not limited to those mentioned above, and those skilled in the art will clearly understand from the description of the appended claims other additional effects not mentioned above. Attached Figure Description
[0025] Figure 1 This is a plan view showing a battery cell packaging device according to an embodiment of the present disclosure.
[0026] Figure 2 This is a plan view showing a battery cell according to an embodiment of the present disclosure.
[0027] Figure 3 This is a plan view showing a battery cell packaging device according to another embodiment of the present disclosure.
[0028] Figure 4 This is a plan view showing a conventional battery cell packaging device.
[0029] Figure 5 This is a plan view showing a battery cell packaging device according to another embodiment of the present disclosure. Detailed Implementation
[0030] In the following description, various embodiments of the present disclosure will be presented in detail with reference to the accompanying drawings, to the extent that those skilled in the art can readily practice the present disclosure. The present disclosure may be implemented in various different forms, and is not limited to the embodiments described herein.
[0031] Parts irrelevant to this description will be omitted in order to clearly describe this disclosure, and throughout the specification, the same reference numerals denote the same elements.
[0032] Furthermore, in the accompanying drawings, for ease of description, the dimensions and thicknesses of each element are arbitrarily shown, and this disclosure is not necessarily limited to those shown in the drawings. In the accompanying drawings, for clarity, the thicknesses of layers, regions, etc., are exaggerated. In the accompanying drawings, for ease of description, the thicknesses of portions and regions are exaggerated.
[0033] Furthermore, it will be understood that when an element such as a layer, film, region, or plate is referred to as being "on" or "above" another element, it can be directly on the other element, or there may be intermediate elements present. Conversely, when an element is referred to as being "directly on" another element, it means that there are no other intermediate elements present. Additionally, the statement that a portion is "above" or "on" a reference portion means that the portion is located above or below the reference portion, and does not specifically mean that the portion is located "above" or "on" in the direction opposite to gravity.
[0034] Furthermore, throughout the specification, when a section is referred to as "including" a certain component, it means that the section may also include other components, without excluding other components, unless otherwise stated.
[0035] Furthermore, throughout the instruction manual, when referred to as "planar," it means when viewing the target portion from above, and when referred to as "cross-section," it means when viewing the target portion from the side of a vertically cut cross-section.
[0036] Figure 1 This is a plan view showing a battery cell packaging device 100 according to an embodiment of the present disclosure. Figure 2 This is a plan view showing a battery cell 200 according to an embodiment of the present disclosure. Figure 3 This is a plan view showing a battery cell packaging device 100 according to another embodiment of the present disclosure. Figure 4 This is a plan view showing a conventional battery cell packaging device 100. Figure 5 This is a plan view showing a battery cell packaging device 100 according to another embodiment of the present disclosure.
[0037] Reference Figures 1 to 5 According to one embodiment of the present disclosure, a battery cell packaging apparatus 100 includes: a first mold 110; a first heating block 120 coupled to the first mold; and a first sealing tool 130 configured to attach to the first heating block and seal the battery cell. The first mold includes a support portion 111 for limiting thermal expansion.
[0038] According to this embodiment, the first mold 110 can be used as an upper structure to seal the battery cell 200 at high temperatures. The first mold 110 is a body that deforms at high temperatures, and its coefficient of thermal expansion is intentionally increased or appropriately designed so that the entire mold can be induced to expand only in a specific direction.
[0039] The first heating block 120 can be used to limit the thermal expansion of the first mold 110.
[0040] The first sealing tool 130 can directly contact the bonding surface of the bag film of the battery cell 200 to seal the battery cell 200. The first sealing tool 130 is capable of properly receiving the heat and pressure supplied by the first mold 110 and the first heating block 120 and uniformly transferring them to the sealing area.
[0041] Reference Figure 3 The first sealing tool 130 initially maintains a predetermined gap 130a at room temperature (e.g., 25°C), and during a temperature rise (e.g., 220°C), this gap deforms to a state represented by gap 130b. In this specification, the gap between the first sealing tool 130 and the reference line (or reference surface) in the initial stage (at room temperature) is defined as "gap 130a," and the gap between the first sealing tool 130 and the reference line after a temperature rise is defined as "gap 130b." Here, the amount of thermal deformation of the first sealing tool 130 can be defined as "gap 130a - gap 130b." That is, the degree to which the position of the first sealing tool 130 relative to the initially set reference line changes with temperature is evaluated by this gap difference, thereby enabling easy measurement of the vertical direction of the first sealing tool 130 generated during a temperature rise. Figure 3 The deformation along the Z-axis. In this case, such as... Figure 3 As shown, the stop can physically limit the excessive rise or fall of the first sealing tool 130, so that the actual range of thermal deformation can vary depending on the height and structure of the stop.
[0042] In this embodiment, when the first heating block 120 is heated to a high temperature (approximately 220°C), the first sealing tool 130 can be induced to move in the vertical direction ( Figure 3 The Z-axis of the sealing tool 130 expands or warps, causing the gap 130b to differ from the initial gap 130a. This difference can be quantitatively confirmed by calculating the difference using the formula "gap (130a) - gap (130b)". Furthermore, by repeatedly measuring the gaps 130a and 130b before and after a temperature rise, the accumulation of thermal stress and the durability of the sealing tool 130 can be monitored over a long period.
[0043] In other words, the method for measuring the thermal deformation of the first sealing tool 130 directly detects the change in the gap with the initially set reference line. As a result, the deformation of the first sealing tool 130 caused by temperature changes can be accurately determined, and this deformation can be used as the basis data for maintaining the required accuracy during the sealing process.
[0044] Reference Figure 2 and Figure 4 When sealing the battery bag at high temperatures using a conventional battery cell packaging device 10, the following problem arises: the conventional first sealing tool 13 causes excessive thermal deformation, and the amount of thermal deformation generated in the batwing portion 13-1 and the degassing portion 13-2 of the first sealing tool 13 increases. This problem occurs because the coefficient of thermal expansion of the first mold 11 is lower than that of the first sealing tool 13 and the first heating block 12. As a result, defects may occur in the sealing thickness of the battery cell 200, leading to rework and slowing down the sealing process.
[0045] According to this embodiment, the bat-ear portion 131 corresponds to the single-cell bat-ear portion 201 of the battery cell 200, and the degassing portion 132 can correspond to the single-cell degassing portion 202. The single-cell bat-ear portion 201 can refer to the area where a portion of the outer material of the battery cell 200 is extended or cut to allow the electrode leads 210 to extend to the outside. The single-cell bat-ear portion 201 is the area where the electrode leads 210 are bonded to the outer material; therefore, the bat-ear portion 131 corresponding to the single-cell bat-ear portion 201 is prone to thickness variations due to concentrated thermal deformation during high-temperature sealing. The single-cell degassing portion 202 can be a portion provided with a channel for venting residual gas or air in the battery cell 200. The single-cell degassing portion 202 is a path for venting gas or setting to a vacuum state during normal operation of the battery cell 200; therefore, the degassing portion 132 corresponding to the single-cell degassing portion 202 is prone to thickness variations due to concentrated thermal deformation during high-temperature sealing. Therefore, since the batwing portion 131 and the degassing portion 132 are areas where deformation is concentrated during the high-temperature sealing process, reducing the amount of deformation between the batwing portion 131 and the degassing portion 132 can reduce the defect rate and improve the durability and reliability of the battery cell 200. As a result, not only can the sealing quality of the battery cell 200 be improved and the defect rate reduced, but it can also be placed in an environment where uniform quality can be achieved even by operators with low skill levels. This can improve the efficiency of the production process and lead to cost reduction.
[0046] The support portion 111 can be arranged on both side surfaces of the first mold 110 to reduce thermal expansion deviations occurring at high temperatures. The support portion 111 can correct the different thermal expansion between the bat-ear portion 131 and the degassing portion 132. That is, based on the structure that changes from the existing fan shape to a wing shape, the thermal expansion deviation occurring between the central portion 110-2 and the peripheral portion 110-1 can be mitigated.
[0047] The material of the first mold 110 can be selected taking into account the coefficient of thermal expansion to prevent excessive expansion during the temperature rise process. The first heating block 120 can be designed to achieve a process temperature of approximately 220°C, at which point the first sealing tool 130 can stably maintain the seal thickness while delivering uniform pressure to the battery cell. The expansion occurring at high temperatures is evenly distributed through the support portion 111, and a reduction in the deviation between the batwing portion 131 and the degassing portion 132 can be expected.
[0048] As a result of these effects, the sealing quality of the battery cell 200 becomes uniform, and a consistent thickness can be ensured without further adjustments. The deviation between the batwing portion 131 and the degassing portion 132 is reduced, making it possible to reduce the frequency of unnecessary mold reprocessing or replacements that may occur during high-temperature processes. As a result, the overall process time is shortened and production efficiency can be improved. Operators can ensure a stable sealing thickness without any additional correction operations, thereby improving both the yield and reliability of the battery cell 200. In addition, the durability of the mold is improved, maintenance costs are reduced, and large-scale production with uniform quality becomes possible.
[0049] Refer again Figures 1 to 3 and Figure 5 In the embodiments disclosed herein, the support portion 111 may be provided in multiple forms and positioned on both sides of the first mold 110.
[0050] Multiple support portions 111 are provided and positioned on both sides of the first mold 110, thereby distributing the thermal deformation that occurs during the sealing process more evenly. In conventional fan-shaped molds, only the central portion 110-2 may over-expand, resulting in a large difference in the cumulative deformation between the batwing portion 131 and the degassing portion 132. In contrast, in this embodiment, the support portions 111 on both sides each support the peripheral portion 110-1, thereby limiting or dispersing the expansion path. As a result, the areas where the batwing portion 131 and the degassing portion 132 are located do not allow thermal deformation to concentrate in only one direction, and the amount of thermal expansion between the batwing portion 131 and the degassing portion 132 is more uniform.
[0051] More specifically, multiple support portions 111 are symmetrically arranged on the left and right sides of the first mold 110, and help the entire mold expand uniformly when heated to a high temperature (e.g., about 220°C). For example, in a conventional fan-shaped mold, if the thickness or reinforcement of the outer portion 110-1 is insufficient, the central portion 110-2 may over-expand, thus posing a risk that the sealing gap will become significantly distorted. However, in this embodiment, support portions 111 are provided to firmly support each outer portion 110-1, thereby enabling balanced control of the amount of deformation between the central portion 110-2 and the outer portions 110-1. The shape of the support portions 111 can be designed as a "wing type," which can take the form of wings protruding from the side surface of the first mold 110, or can be structurally connected to surround the outer portions 110-1.
[0052] With multiple supports 111 positioned on both sides, the seal thickness deviation between the bat-ear portion 131 and the degassing portion 132 is significantly reduced, ensuring uniform seal thickness quality. Furthermore, due to the uniform seal, almost no further correction operations are required in subsequent processes, thus improving operational efficiency and extending mold changeover cycles, thereby reducing overall process costs and time consumption. Traditional problems of quality variation depending on operator skill level or individual corrections are also significantly reduced, minimizing quality deviations during mass production.
[0053] Refer again Figures 1 to 3 and Figure 5 In embodiments of this disclosure, the support portion 111 may be arranged to protrude from the periphery of the first mold 110.
[0054] As described above, the support portion 111 can be designed to suppress thermal expansion caused by the high-temperature process at the side surface of the first mold 110. If the support portion 111 reduces the expansion path acting from the peripheral portion 110-1 towards the central portion 110-2, the sealing thickness deviation between the batwing portion 131 and the degassing portion 132 can be alleviated. The support portion 111 can be integrally formed by selecting a material with a small coefficient of thermal expansion or by using a component with a coefficient similar to that of the mold material.
[0055] In this embodiment, a temperature of approximately 200°C to 250°C can be applied via the first heating block 120 to seal the battery cell 200 at a high temperature. At this time, the first sealing tool 130 compresses the battery cell 200, and the support portion 111 enables a uniform distribution of thermal expansion between the central portion 110-2 and the peripheral portion 110-1. Because the support portion 111 has a protruding shape in the peripheral direction, it can improve the fan-shaped structure where thermal expansion is concentrated and maintain uniform pressure.
[0056] This design suppresses thermal expansion of the outer 110-1 portion during cell sealing, thus reducing overall thickness variation. Ensuring a uniform seal thickness maintains consistent quality even during repeated operations. It also extends mold changeover cycles and shortens calibration time, thereby improving production efficiency.
[0057] Refer again Figures 1 to 3 and Figure 5 In one embodiment of this disclosure, the first mold 110 may be integrally formed with the support portion 111.
[0058] Therefore, when the first mold 110 and the support portion 111 form a single structure during high-temperature processing, thermal expansion can be distributed uniformly rather than concentrated locally. In other words, the difference in expansion between the central portion 110-2 and the peripheral portion 110-1 of the first mold 110 can be reduced. The support portion 111 can be made of a material with the same or similar coefficient of thermal expansion as the first mold 110 in order to control the expansion occurring in the peripheral portion 110-1.
[0059] This reduces thickness deviations caused by thermal expansion during the sealing of the battery cell 200. Even when the process is repeated, uniform sealing quality is achieved, extending mold changeover cycles and reducing the time required for calibration operations. Furthermore, since the support portion 111 has a structure integrally connected to the first mold 110, it maintains stable behavior even under stress generated during high-temperature processes. Therefore, the thickness deviation between the batwing portion 201 and the degassing portion 202 of the battery cell 200 can be stably maintained on the production line, reducing the defect rate and thus improving overall production efficiency and quality reliability.
[0060] Refer again Figures 1 to 3 and Figure 5 In embodiments of this disclosure, the support portion 111 may include an inclined shape: its width gradually increases in the direction away from the first sealing tool 130.
[0061] The inclined shape according to this embodiment enables the expansion that occurs during the high-temperature process to be evenly distributed. That is, since the inclination is applied to the support portion 111, the overall thermal expansion of the first mold 110 is evenly distributed, thereby improving sealing stability. Therefore, deviations caused by uneven expansion are reduced, thus achieving a constant thickness even when the process is repeated. This extends the mold changeover cycle, reduces the need for correction processes, and improves production efficiency. Furthermore, since the peripheral portion 110-1 is adequately supported, mold deformation is stabilized, and the defect rate occurring in the batwing portion 201 and degassing portion 202 of the battery cell 200 is reduced, thereby improving product reliability.
[0062] In embodiments of this disclosure, the first heating block 120 may include beryllium copper (Be-Cu) material.
[0063] Compared to regular copper, beryllium copper possesses superior mechanical strength and high thermal conductivity, enabling it to maintain a stable heat supply at high temperatures. In particular, when used in battery packaging processes requiring temperatures above a certain range, beryllium copper can transfer heat uniformly without localized temperature deviations. Its high abrasion resistance and thermal shock resistance also help minimize deformation and achieve uniform seal quality, even during repetitive processes.
[0064] In this embodiment, the first heating block 120 can be designed to consistently provide a temperature above approximately 200°C and below 250°C. Even when using beryllium copper material and the temperature rises or falls rapidly, biased thermal stress or deformation within the material is unlikely to occur. Therefore, the effect of rapidly reaching the temperature required for battery encapsulation and shortening operating time can be expected. Furthermore, beryllium copper, due to its high thermal diffusivity, can maintain a uniform temperature throughout the heating block and can meet the purpose of uniformly sealing the protective portion of the battery cell 200.
[0065] Refer again Figures 1 to 3 and Figure 5 The battery cell packaging device 100 according to an embodiment of the present disclosure may further include: a second mold 150; a second heating block 160 connected to the second mold; and a second sealing tool 170 attached to the second heating block.
[0066] The second mold 150 according to this embodiment can be manufactured using a material with a suitable coefficient of thermal expansion at high temperatures. A second heating block 160 is attached to the second mold 150 and can thus be heated to a constant temperature via heating elements inserted internally or externally. A second sealing tool 170 is attached to the second heating block 160 and can directly participate in the operation of sealing the battery cell 200 in a heated state. By utilizing alloys with different coefficients of thermal expansion, warping and twisting occurring at high temperatures can be predicted and controlled.
[0067] By integrating the second mold 150, the second heating block 160, and the second sealing tool 170, thermal expansion deviations can be actively controlled in environments subject to repeated high temperatures and cooling. As a result, the defect rate during the battery sealing process can be reduced, and operation time can be shortened. Furthermore, even operators with low skill levels can seal the battery while maintaining a uniform thickness, which is expected to be beneficial in terms of production process stability and quality control. Even during repeated use, mold warpage and surface damage are reduced, further improving the durability and maintenance efficiency of the device.
[0068] Refer again Figures 1 to 3 and Figure 5 According to embodiments of the present disclosure, the battery cell 200 can be compressed and sealed between a first sealing tool and a second sealing tool.
[0069] According to this embodiment, the first sealing tool 130 and the second sealing tool 170 can be heated to high temperatures by their respective heating blocks 120 and 160, and this heat can be used to uniformly compress the battery cell 200. By using sealing tools made of alloys with different coefficients of thermal expansion, thermal deformation occurring at high temperatures can be predicted and controlled.
[0070] After the battery cell 200 is positioned between the first sealing tool 130 and the second sealing tool 170, each sealing tool is heated to a high temperature and pressed under constant pressure to perform the sealing process. During this time, heating rods inserted into the first heating block 120 and the second heating block 160 can operate simultaneously to minimize temperature deviation. During compression, due to the bimetallic effect, the warping direction can be intentionally guided, thereby achieving a uniform seal thickness at the periphery and throughout the interior of the battery cell 200.
[0071] The battery cell 200 is compressed and simultaneously sealed at high temperature between the first sealing tool 130 and the second sealing tool 170, thereby ensuring a uniform thickness of the seal. As a result, the durability and performance of the battery cell 200 can be stably maintained, and the production process efficiency can also be improved. By reducing the amount of thermal deformation caused by temperature conditions, the replacement cycle of the battery cell packaging device 100 can be extended, rework can be reduced, and an overall cost reduction can be expected.
[0072] In this embodiment, directional terms such as "front," "back," "left," "right," "up," and "down" have been used. These terms are used only for ease of description and may vary, for example, depending on the position of the target object or the observer.
[0073] Although preferred embodiments of the present disclosure have been shown and described above, the scope of the disclosure is not limited thereto, and many other variations and modifications can be made to the embodiments by those skilled in the art using the basic principles of the invention as defined in the appended claims, which also fall within the spirit and scope of the invention.
[0074] [Explanation of reference numerals in the attached figures]
[0075] 10: Traditional battery cell packaging devices
[0076] 100: Battery cell packaging device
[0077] 110: First mold
[0078] 110-1: Peripheral Area
[0079] 110-2: Central Department
[0080] 120: First heating block
[0081] 130: First sealing tool
[0082] 131: Bat ears
[0083] 132: Degassing section
[0084] 150: Second mold
[0085] 160: Second heating block
[0086] 170: Second sealing tool
[0087] 200: Battery cell
[0088] 201: Single bat ear
[0089] 202: Monomer Degassing Section
[0090] 210: Electrode lead
Claims
1. A battery cell packaging device, comprising: First mold; A first heating block is connected to the first mold; as well as A first sealing tool is configured to attach to the first heating block and seal the battery cell. The first mold includes a support portion that restricts thermal expansion.
2. The battery cell packaging device according to claim 1, wherein The support portion is provided in multiple parts and is positioned on both sides of the first mold.
3. The battery cell packaging device according to claim 1, wherein The support portion is arranged to protrude from the periphery of the first mold.
4. The battery cell packaging device according to claim 1, wherein The first mold is integrally formed with the support portion.
5. The battery cell packaging device according to claim 1, wherein The support portion includes an inclined shape in which its width gradually increases in the direction away from the first sealing tool.
6. The battery cell packaging device according to claim 1, wherein The first heating block comprises beryllium copper (Be-Cu) material.
7. The battery cell packaging device according to claim 1, further comprising: Second mold; A second heating block is connected to the second mold; as well as The second sealing tool is attached to the second heating block.
8. The battery cell packaging device according to claim 7, wherein, The battery cell is compressed and sealed between the first sealing tool and the second sealing tool.
Citation Information
Patent Citations
Dry-type cleaning apparatus