Synthesis methods of bio-based solid fatty substances
By controlling the chain length distribution of straight-chain alkane mixtures, the environmental friendliness and safety issues of mineral paraffin and synthetic waxes have been resolved, providing a natural wax alternative with similar physicochemical characteristics for use in cosmetics and other fields.
Patent Information
- Application Number
- CN202580028160.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2024-04-17
- Filing Date
- 2025-04-17
- Publication Date
- 2026-11-17
AI Technical Summary
Existing mineral and synthetic waxes have issues with environmental friendliness and safety, and natural waxes cannot completely replace mineral or synthetic waxes in many applications, especially in cosmetics where they are deficient in stability, hardness, and melting point.
A mixture of straight-chain alkanes with a Gaussian distribution was prepared by metathesis of straight-chain terminal olefins in the presence of a non-isomerizing olefin metathesis catalyst, followed by isomerizing metathesis and hydrogenation in the presence of a catalyst. The chain length distribution was controlled to achieve specific melting points and hardness.
The obtained straight-chain alkane mixture has similar physicochemical characteristics to mineral waxes and can replace synthetic waxes in cosmetics and other fields, providing stability and hardness while also being environmentally friendly.
Smart Images

Figure CN123125221A_ABST
Abstract
Description
Technical Field
[0001] This specification relates to a method for preparing mixtures of straight-chain alkanes of natural, particularly plant, origin, in the form of solid fatty substances, particularly waxes or pastes. The invention also relates to straight-chain alkane mixtures obtainable according to this method and their uses in the fields of cosmetics, pharmaceuticals, coatings, inks, varnishes, paper, adhesives, candles, plastics, rubber, and / or food.
[0002] Existing technology Paraffin wax, also known as mineral wax, is a hydrocarbon-based compound derived from petroleum refining. Composed of various alkanes with a wide range of chain lengths, containing 18 to 60 carbon atoms, paraffin wax is a substance with a solid to semi-solid consistency at room temperature. It is typically characterized by a melting point of 40 to 90°C, excellent oxidation and temperature stability, odor neutrality, and clarity.
[0003] Synthetic waxes are synthetic products obtained from petroleum derivatives. They particularly include silicone polymers or waxes that typically have high melting points.
[0004] These properties make it popular for a wide range of applications, including the manufacture of matches, candles, paper, adhesives, paints, pharmaceuticals, and cosmetics.
[0005] However, mineral waxes and synthetic waxes or paraffins currently on the market have issues with environmental friendliness and safety.
[0006] Specifically, mineral paraffins, including MOSH (mineral oil saturated hydrocarbons) and / or MOAH (mineral oil aromatic hydrocarbons), are suspected of being toxic, particularly carcinogenic, and therefore regulations now require restrictions on their concentration in food.
[0007] Furthermore, due to their origin, mineral paraffins contribute to the increase in anthropogenic carbon dioxide. In addition, they are non-biodegradable and bioaccumulate in the environment.
[0008] This is why many industries are looking for environmentally friendly, biodegradable, and sustainable alternatives to replace mineral and synthetic paraffins.
[0009] “Natural” waxes derived from plants or animals, such as beeswax, candelilla wax, or carnauba wax, offer renewable alternatives to mineral paraffin.
[0010] However, in many applications, natural waxes cannot completely replace mineral or synthetic paraffins.
[0011] Recent scientific research has explored the possibility of replacing mineral paraffin with a naturally derived lipid blend in lipstick formulations, specifically a straight-chain C35-C38 ketene mixture derived from algal resources. However, low stability has been observed (Huynh, A). et al. Evaluation of alkenones, a renewably sourced, plant-derived wax as a structuring agent for lipsticks. Int. J. Cosmet. Sci. 42, 146-155 (2020).
[0012] Other recent scientific studies have shown that in the lipstick industry, replacing petroleum-based synthetic waxes with plant-based waxes can lead to problems such as product stability, lipstick strength, exudation, incompatibility, and / or oxidation, issues that increasingly demanding consumers are unwilling to tolerate. (de Clermont-Gallerande) et al. Substitution of synthetic waxes by plant-based waxes in lipsticks (OCL, 2022, 29, 19).
[0013] Therefore, the study indicates that when the composition obtained from plant waxes is in solid form, its hardness value is too low, which is reflected in excessively frequent breakage when applied in the case of rod-shaped products.
[0014] Furthermore, the stability over time is unsatisfactory. This may be reflected in the occurrence of oil separation, polymorphism, changes in the product surface appearance: unevenness, the presence of matte surface areas or coated areas, or even changes in sensory properties upon application over time (reduced spreadability and smoothness).
[0015] Furthermore, natural plant waxes with high melting points, around 80°C, do not provide sufficient sensory texture: they are very hard, lack softness, and feel unpleasant when applied to the skin or lips. Finally, plant waxes with melting points below 80°C cannot adequately structure the composition for molding lipstick sticks.
[0016] Therefore, it is indeed necessary to find ecological and sustainable alternatives from natural sources, especially plant sources, to replace mineral paraffin. Summary of the Invention
[0017] A method has been developed for preparing mixtures of straight-chain alkanes of natural, particularly plant, origin, in the form of solid aliphatic substances, whose physicochemical characteristics, particularly hardness, texture, and / or melting point, are very similar to those of existing mineral paraffins.
[0018] Therefore, according to a first aspect, the present invention relates to a method for preparing a mixture of straight-chain alkanes of natural origin, preferably plant origin, comprising the following steps: i) Metathesis of at least one straight-chain terminal olefin containing 5 to 24 carbon atoms in the presence of a non-isomerizing olefin metathesis catalyst, wherein the straight-chain terminal olefin is derived from at least one natural source, preferably a plant source, of a fatty acid or fatty acid ester, thereby obtaining a first internal olefin mixture (I). ii) The internal olefin mixture (I) obtained in step i) isomerizes and metamorphoses in the presence of a catalyst or a mixture of catalysts to obtain a second internal olefin mixture (II), and iii) The mixture of inner olefins (II) is hydrogenated in the presence of a catalyst to obtain a mixture of straight-chain alkanes of natural origin (III).
[0019] Surprisingly, the inventors were able to observe that the method provides straight-chain alkane mixtures characterized by highly controlled chain length distribution in a very reproducible manner and with high yield.
[0020] Then, in a very advantageous manner, the inventors were able to demonstrate that by changing the composition of the starting and ending olefin mixture, particularly the chain lengths of these olefins, and / or their relative proportions in the mixture, the method makes it possible to control the distribution and thus the physicochemical characteristics of the resulting mixture, particularly the melting point of the resulting mixture. Thus, starting with an equimolar mixture of ending olefins, the method provides an alkane mixture with a symmetrical chain length distribution, i.e., a Gaussian distribution. Furthermore, the inventors were able to observe that the greater the proportion of short chains in the starting and ending olefin mixture, the more the Gaussian distribution shifts towards the smaller alkane chains (positive asymmetric distribution). Conversely, the greater the proportion of long chains in the mixture, the more the Gaussian distribution shifts towards the larger alkane chains (negative asymmetric distribution).
[0021] Highly advantageously, this method thus enables the production of mixtures of straight-chain alkanes from natural sources with melting points that vary over a wide range, particularly from 32°C to 90°C as measured by differential scanning calorimetry (DSC). These mixtures can be, in particular, in the form of waxes or pastes.
[0022] According to another aspect, the present invention relates to mixtures of straight-chain alkanes of natural origin, particularly of plant origin, which can be obtained by the method according to the invention.
[0023] According to another aspect, the present invention relates to mixtures of straight-chain alkanes of natural origin, particularly of plant origin, especially in the form of solid fatty substances, wherein: - Each straight-chain alkane constituting the mixture contains 8 to 90 carbon atoms, particularly 10 to 85 carbon atoms, more preferably 10 to 75 carbon atoms, even more preferably 10 to 70 carbon atoms, and even more preferably 24 to 60 carbon atoms. - The quantity distribution of each straight-chain alkane arranged in ascending order of carbon atom number is as follows: o Increasing from the minimum number of carbon atoms in straight-chain alkanes to the mode of distribution; and o Decreases between the mode of distribution and straight-chain alkanes with the largest number of carbon atoms. These quantities are calculated as a weight percentage relative to the total weight of the mixture of straight-chain alkanes from natural sources.
[0024] The quantity distribution can be characterized in particular by its span, which is defined as the difference between the maximum and minimum values of the distribution. It is always positive, and the more dispersed the series of values, the larger this value becomes proportionally.
[0025] In the context of this patent application, span is defined as the difference between the number of carbon atoms in a straight-chain alkane with the largest number of carbon atoms and the number of carbon atoms in a straight-chain alkane with the smallest number of carbon atoms.
[0026] The span defined in this way can be measured by gas chromatography (GC), which allows for the determination of the lengths of straight-chain alkanes in the distribution, including the lengths of the smallest and largest alkanes. Those skilled in the art can therefore adjust parameters such as column size, stationary phase properties, and measurement temperature to determine the nature of the alkanes present in the reaction mixture. In particular, those skilled in the art can adjust the experimental conditions of gas chromatography to determine the smaller and larger alkanes present in the mixture.
[0027] The larger the span, the wider the distribution of the straight-chain alkane mixture. Conversely, the smaller the span, the narrower the distribution of the straight-chain alkane mixture.
[0028] According to a preferred embodiment, the straight-chain alkane mixture according to the present invention is characterized in that the span is greater than 15, preferably greater than 20. The span may also preferably be less than 60, more preferably less than 55.
[0029] The distribution span of the straight-chain alkane mixture according to the present invention is related to the span of the melting range of the mixture.
[0030] The term "melting range" is used because the alkane mixture obtained by the method according to the claims is a collection of several alkanes with different chain lengths and therefore different melting points. In the case of alkane mixtures, the endothermic melting peaks observed by differential scanning calorimetry (DSC) are characterized by a "starting point" and a "terminating point," corresponding to the temperature at which melting is first observed and the temperature at which the mixture has completely melted, respectively.
[0031] The inventors can demonstrate that a narrower chain length distribution in alkane mixtures, as described, for example, in the prior art, results in a narrower melting range, and conversely, a wider chain length distribution in alkane mixtures described in this patent application reflects a wider melting range.
[0032] Examples in this patent application demonstrate that, by means of the method according to the invention, waxes with a significant melting temperature range (measured as the difference between the “end point” and the “start point”) can be obtained, reflecting the span of alkane distribution.
[0033] According to a preferred embodiment, the wax is characterized by a melting point of 79.6°C, and the melting range begins at 55.2°C and ends at 90.7°C.
[0034] According to another preferred embodiment, the wax is characterized by a melting point of 48.9°C and a melting range starting at 36.3°C and ending at 56.8°C.
[0035] According to another preferred embodiment, the wax is characterized by a melting point of 75.2°C, and the melting range begins at 66.9°C and ends at 79.2°C.
[0036] According to another preferred embodiment, the wax is characterized by a melting point of 68.5°C, and a melting range starting at 56.8°C and ending at 75.1°C.
[0037] According to another preferred embodiment, the wax is characterized by a melting point of 74°C, and the melting range begins at 32°C and ends at 86.4°C.
[0038] This invention differs from known methods in the prior art, which cannot provide a straight-chain alkane mixture characterized by a Gaussian distribution. For example, patent application WO 2021 / 183330 A1 discloses a two-step method based on an isomerization metathesis step followed by hydrogenation of the inner alkene obtained by metathesis. The straight-chain alkane mixture obtained after these two steps is not characterized by a Gaussian distribution (see in particular Comparative Example 16, which reproduces Example 4 of WO 2021 / 183330 A1, and related […]). Figure 21Furthermore, the mixture described in patent application WO 2021 / 183330 A1 is characterized by a span of 8 carbon atoms between the largest and smallest straight-chain alkanes. Therefore, such a span is significantly narrower than the span of the straight-chain alkane distribution obtained by practicing this invention.
[0039] The inventors have demonstrated that producing a mixture of straight-chain alkanes characterized by a Gaussian distribution, particularly with a significant span of at least 15 carbon atoms, faithfully reproduces the characteristics of commercially available synthetic waxes, and thus allows for the substitution of synthetic waxes with bio-based waxes. Specifically, using a mixture of straight-chain alkanes that does not have a Gaussian distribution, and particularly has a narrow span, as a substitute for synthetic waxes in cosmetic compositions fails to reproduce all the properties of synthetic waxes and may lead to various problems during their formulation, such as composition gelation and / or uneven surface crystallization.
[0040] The distinctive feature of the method according to the invention lies in the combination of the first non-isomerization metathesis step and the isomerization metathesis step preceding the hydrogenation step. As demonstrated by the inventors in Comparative Example 16, it is precisely by adding the intermediate isomerization metathesis step that the method according to the invention results in a Gaussian distribution, particularly with a significant span.
[0041] This effect is even more unexpected because prior art seeks to avoid or reduce any isomerization reactions during metathesis to maximize the yield of the target product. Several prior art documents describe technical solutions that allow for the avoidance or reduction of isomerization reactions. For example, Buutilkov D. et al. The title is " Jojoba oil olefin metathesis: a A valuable source for bio-renewable materials: Jojoba oil olefin metathesis: bio-renewable materials [A valuable source] This is the case with the publication in "Green Chemistry" (vol. 16, No. 11, 2014, pp. 4728-4733). The publication describes strategies for avoiding or minimizing isomerization metathesis reactions, which occur, for example, when a catalyst is degraded under extreme reaction conditions.
[0042] Therefore, the inventors have done a good job by implementing a second isomerization metathesis step, despite the prior art teaching to avoid any isomerization during metathesis, in order to obtain a Gaussian straight-chain alkane distribution, particularly with a significant span and rich in straight-chain alkanes with different chain lengths.
[0043] In a particularly advantageous manner, and compared with existing technologies, the inventors have been able to develop naturally derived C24 to C60 straight-chain alkane mixtures in wax form, possessing physicochemical characteristics very similar to those of synthetic mineral waxes commonly used in the lipstick industry. Specifically, the inventors have demonstrated that the wax obtained according to this method is compatible with oils commonly used in the cosmetics industry, and enables the production of lipsticks with textures, hardness, and stability comparable to lipsticks containing mineral paraffin waxes used in this industry.
[0044] More generally, these straight-chain alkane mixtures particularly enable the production of compositions, especially anhydrous and solid compositions, and more particularly in rod form, whose physicochemical properties are similar to those of similar compositions prepared from mineral waxes in terms of hardness, sensory properties, and stability over time, while being free of mineral waxes and / or synthetic waxes. The mixtures also enable the production of mascara compositions (water-in-wax emulsions) that impart similar volume to eyelashes as obtained with similar compositions prepared from mineral waxes, while being free of mineral waxes and / or synthetic waxes.
[0045] In a particularly advantageous manner, through a sequence of two consecutive selective metathesis steps (one non-isomerization, the other isomerization), the method according to the invention enables the production of a mixture of straight-chain alkanes with sufficiently high melting points (very close to the melting points of synthetic waxes) by using terminal olefins (i.e., fewer than or equal to 20 carbon atoms) with shorter chains than those used in prior art methods. The advantage of shorter terminal olefins is their lower cost compared to longer olefins. The method according to this application, for example, enables the production of C24 to C60 alkanes from terminal olefins having 16 to 20 carbon atoms (Example 1, […]). Figure 8 [ ]), thereby reproducing the melting point of the target synthetic wax at a lower cost.
[0046] According to another aspect, the present invention relates to a composition comprising a mixture of straight-chain alkanes according to the invention.
[0047] According to another aspect, the present invention relates to the use of straight-chain alkane mixtures according to the invention in the fields of cosmetics, pharmaceuticals, coatings, inks, varnishes, paper, adhesives, candles, plastics, rubber and / or food.
[0048] The features disclosed in the following paragraphs may be implemented independently of each other or in combination with each other.
[0049] The method according to the present invention may include the following additional features: - The non-isomeric olefin metathesis catalyst in step i) is selected from transition metal complexes, especially alkylene complexes of transition metals, particularly alkylene complexes of ruthenium; - The non-isomeric olefin metathesis catalyst is selected from Ru-1a, Ru-1b or a mixture thereof; [Chemical Formula 1] [Chemical Formula 2] - The catalyst or mixture of catalysts used in step ii) is a transition metal complex, especially a ruthenium complex; - The isomerization olefin metathesis catalyst is a mixture of Ru-2 and Ru-3.
[0050] [Chemical Formula 3] [Chemical Formula 4] - The terminal olefin used in step i) is prepared from fatty acid esters of jojoba oil; - The at least one linear terminal olefin used in step i) is a mixture of at least two different linear terminal olefins, each containing 5 to 24 carbon atoms, particularly 16 to 24 carbon atoms, preferably 16 to 20 carbon atoms; - The at least two linear terminal olefins differ from each other by at least two carbon atoms; - The at least one linear terminal olefin used in step i) is a mixture of three linear terminal olefins, preferably C6 / C7 / C8, C8 / C9 / C10, C10 / C12 / C14, or C16 / C18 / C20, and the mixture may in particular contain: o 0.5% to 10%, preferably 1% to 10%, or even more preferably 1% to 5% of C16 terminal olefins; o 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C18 terminal olefins; and o 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C20 terminal olefins; The percentage is expressed in moles relative to the total molar weight of the terminal olefin mixture.
[0051] Generally, the higher the proportion of short-chain (C16) straight-chain terminal olefins in the mixture, the lower the melting point of the alkane mixture obtained after the two metathesis steps and the hydrogenation step. Therefore, those skilled in the art will select the composition of the straight-chain terminal olefin mixture to obtain the desired melting point of the final alkane mixture.
[0052] A mixture of straight-chain alkanes of natural origin that can be obtained according to the method of the invention may contain at least two different straight-chain alkanes, each of which contains 8 to 90 carbon atoms, particularly 10 to 85 carbon atoms, preferably 10 to 75 carbon atoms, even more preferably 10 to 70 carbon atoms, and even more preferably 24 to 60 carbon atoms.
[0053] According to the invention, a mixture of straight-chain alkanes of natural, particularly plant, origin, especially in the form of solid fatty substances, may also contain any one or more of the following additional features: - Each straight-chain alkane in the distribution differs from every consecutive straight-chain alkane in the distribution by one carbon atom; - Each straight-chain alkane that makes up the mixture contains 24 to 60 carbon atoms; - The mode of distribution is between 40 and 45 carbon atoms; - The median distribution is between 40 and 45 carbon atoms; - The melting point of the mixture is between 75°C and 85°C; - The characteristics of this mixture are: o The straight-chain alkanes with the smallest number of carbon atoms have 15 to 19 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 42 to 46 carbon atoms; or o The straight-chain alkanes with the smallest number of carbon atoms have 20 to 24 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 52 to 56 carbon atoms; or o The straight-chain alkanes with the smallest number of carbon atoms have 10 to 14 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 45 to 49 carbon atoms; or o The straight-chain alkanes with the smallest number of carbon atoms have 9 to 13 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 48 to 52 carbon atoms; or The straight-chain alkanes with the smallest number of carbon atoms have 9 to 13 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 52 to 56 carbon atoms, or The straight-chain alkanes with the smallest number of carbon atoms have 16 to 20 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 63 to 67 carbon atoms, or o The straight-chain alkanes with the smallest number of carbon atoms have 13 to 17 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 66 to 70 carbon atoms, or The straight-chain alkanes with the smallest number of carbon atoms have 19 to 23 carbon atoms, while the straight-chain alkanes with the largest number of carbon atoms have 49 to 53 carbon atoms.
[0054] Compositions comprising a mixture of straight-chain alkane compounds according to the present invention may further comprise and / or feature one or more of the following additional features: - Contains less than 3% by weight, particularly less than 1% by weight, preferably free of solid fatty substances of mineral and / or synthetic origin, these weight percentages are expressed relative to the total weight of the composition; - The composition is characterized as a cosmetic or pharmaceutical composition, particularly a fragrance, care or cosmetic product for use on the skin, mucous membranes or body surface; - The composition is characterized as an anhydrous composition; - The composition is characterized as a solid composition; - The composition is characterized as a solid composition in rod form; - The composition is characterized as a mascara composition. Attached Figure Description
[0055] Other features, details, and advantages will become apparent upon reading the following detailed description and analyzing the accompanying drawings, in which: Figure 1 [ Figure 1 The method according to the invention is schematically illustrated, corresponding to a targeted sequential catalytic method leading to a mixture of alkanes from terminal olefins. The reaction conditions are as follows: (i) metathesis: Ru-1a / Ru-1b 3 / 7 (0.3 mol%), THF (9M), 75°C, 2 days; (ii) isomerization / metathesis: Ru-2 (0.5 mol%), Ru-3 (1 mol%), MeOH (100 equivalents / catalyst), THF (1.3M), 75°C, 2 h; (iii) hydrogenation: H2 (1 bar), Pd / C (0.4 wt% Pd / substrate), cyclohexane (0.2 g / mL), 50°C, 16 h.
[0056] Figure 2 [ Figure 2 This schematically illustrates a method for producing a mixture of terminal olefins from saturated and unsaturated fatty acid esters.
[0057] Figure 3 [ Figure 3This diagram schematically illustrates example methods for producing C16, C18, and C20 terminal alkenes, respectively. The reaction conditions are as follows: Grignard reagent preparation: alkyl bromide (1.5 equivalents), Mg (3 equivalents), I₂ (0.1 mol%), THF (1.3 M), 0 °C to 20 °C, 1 h; Cross-coupling: CuCl₂ (2 mol%), 1-phenylpropyne (10 mol%), THF (0.9 M), 0 °C to 20 °C, 1.5 h; Yield: C 16 (1.7 g; 77%); C 18 (2.3 g, 90%; 63.5 g, 91%); C 20 (9.9 g, 99%; 69.5 g, 99%).
[0058] Figure 4 [ Figure 4 [This refers to the cross-metathesis step of step i) according to the method of the present invention, starting from a specific mixture of C16, C18, and C20 straight-chain terminal olefins, according to Example 1. The reaction conditions are as follows: Starting terminal olefin: C 16 (0.01 equivalent), C 18 (0.495 equivalent), C 20 (0.495 equivalents); Double displacement: Ru-1a / Ru-1b 3 / 7 (0.3 mol%), THF (9M), 75℃, 2 days.
[0059] Figure 5 [ Figure 5 [ ] indicates the isomerization metathesis step ii) of the method according to the invention, which begins with a specific mixture of C16, C18, and C20 linear terminal olefins carried out in step i). The reaction conditions are as follows: Ru-2 (0.5 mol%), Ru-3 (1 mol%), MeOH (100 equivalents / catalyst), THF (2.4 M), 75 °C, 15 h.
[0060] Figure 6 [ Figure 6 [This refers to the GC analysis of the inner olefin mixture obtained in step ii) of Example 1, starting from a specific mixture of C16, C18, and C20 straight-chain terminal olefins used in step i).
[0061] Figure 7 [ Figure 7 [ ] indicates the hydrogenation step in step iii) of the method according to the present invention. The reaction conditions are as follows: H2 (1 bar), Pd / C (0.4 wt% Pd / substrate), cyclohexane (0.2 g / mL), 50 °C, 16 h.
[0062] Figure 8 [ Figure 8 [] indicates, according to Example 1, a specific mixture (C16, C18, and C20 straight-chain terminal olefins) used in step i) 16 (0.01 equivalent), C 18 (0.495 equivalent), C 20 (0.495 equivalents) Begin with GC analysis of the straight-chain alkane mixture obtained in step iii).
[0063] Figure 9 [ Figure 9 This schematically illustrates the ethyleneolysis of jojoba oil according to Example 2, yielding dec-1-ene. The reaction conditions are as follows: ethyleneolysis: ethylene (10 bar), Ru-4 (100 ppm), 40 °C, 6 h.
[0064] Figure 10 [ Figure 10 [] indicates the method of the present invention, according to Example 2, starting from dec-1-ene: (i) metathesis: Ru-1a / Ru-1b3 / 7 (0.3 mol%), THF (1M), 75°C, 4 days; (ii) isomerization / metathesis: Ru-2 (0.5 mol%), Ru-3 (1 mol%), MeOH (100 equivalents / catalyst), THF (0.7M), 75°C, 2 h; (iii) hydrogenation: H2 (1 bar), Pd / C (0.4 wt% Pd / substrate), cyclohexane (0.2 g / mL), 50°C, 6 h.
[0065] Figure 11 [ Figure 11 [] indicates the GC analysis of the straight-chain alkane mixture obtained in step iii), starting from the dec-1-ene used in step i), according to Example 2.
[0066] Figure 12 [ Figure 12 [] indicates, according to Example 3, a specific mixture (C16, C18, and C20 straight-chain terminal olefins) used in step i). 16 (0.01 equivalent), C 18 (0.495 equivalent), C 20 (0.495 equivalents) Begin with GC analysis of the straight-chain alkane mixture obtained in step iii).
[0067] Figure 13 [ Figure 13 [] indicates the GC analysis of the straight-chain alkane mixture obtained in step iii) starting from a specific mixture of C6, C7 and C8 straight-chain terminal olefins (C6 (0.33 equivalent), C7 (0.33 equivalent), C8 (0.33 equivalent)) according to Example 4.
[0068] Figure 14 [ Figure 14 [This refers to a specific mixture of C8, C9, and C10 linear terminal olefins according to Example 5 (C8 (0.33 equivalents), C9 (0.33 equivalents), C...] 10 (0.33 equivalents) Start with GC analysis of the straight-chain alkane mixture obtained in step iii).
[0069] Figure 15 [ Figure 15 [] indicates a specific mixture of C10, C12 and C14 straight-chain terminal olefins (C10, C12 and C14) according to Example 6. 10 (0.33 equivalent), C 12 (0.33 equivalent), C 14 (0.33 equivalents) Start with GC analysis of the straight-chain alkane mixture obtained in step iii).
[0070] Figure 16 [ Figure 16 This schematically illustrates a method for producing a mixture of terminal olefins from jojoba oil. The reaction conditions are as follows: isomerization: Fe(CO)5 (50 mol%), hexane (0.1 M), UV lamp (2 x λ = 365 nm), 24 h, 50 °C, pyridine (20 equivalents / catalyst); ethylene hydrolysis: ethylene (20 bar), Ru-4 (0.5 mol%), 40 °C, 16 h.
[0071] Figure 17 [ Figure 17 This schematically illustrates a method for producing a mixture of terminal olefins from erucic acid esters (methyl erucic acid). The reaction conditions are as follows: isomerization: Fe(CO)5 (10 mol%), hexane (0.04 M), UV lamp (2 x λ = 365 nm), 7 h, 50 °C, pyridine (20 equivalents / catalyst); ethylene hydrolysis: ethylene (20 bar), Ru-4 (0.3 mol%), 40 °C, 16 h.
[0072] Figure 18 [ Figure 18[This refers to the GC analysis of the straight-chain alkane mixture obtained in step iii), starting from the straight-chain terminal olefin mixture obtained by isomerization of jojoba oil followed by ethylene hydrolysis in step i), according to Example 14.
[0073] Figure 19 [ Figure 19 [This refers to the GC analysis of the straight-chain alkane mixture obtained in step iii), starting from the straight-chain terminal olefin mixture obtained by isomerization of methyl erucate followed by ethylene hydrolysis in step i), according to Example 15.
[0074] Figure 20 [ Figure 20 This schematically illustrates the method described in Example 4 of patent application WO 2021 / 183330 A1.
[0075] Figure 21 [ Figure 21 The diagram illustrates the GC analysis of a mixture of straight-chain alkanes obtained according to the method described in Example 4 of patent application WO 2021 / 183330 A1, the overall scheme of which is as follows [ Figure 20 As shown in the image. Detailed Implementation
[0076] The invention will now be described in more detail in a non-limiting manner in the following description.
[0077] Unless otherwise stated, all percentages of quantities are mass percentages.
[0078] For the purposes of this specification, the term "mineral wax" refers to a refined or semi-refined product obtained from the processing and refining of crude oil, primarily composed of saturated hydrocarbons. This is particularly true of paraffin wax or microcrystalline wax.
[0079] For the purposes of this specification, the term "synthetic wax" refers to waxes synthesized from hydrocarbons derived from petroleum refining. These are primarily polymers of fossil (petrochemical) origin. For example, polyolefin waxes synthesized from ethylene (polyethylene wax), propylene (propylene wax), and other fossil-derived monomers may be mentioned.
[0080] For the purposes of this specification, the term "linear terminal olefin" refers to a linear hydrocarbon chain, specifically containing 5 to 24 carbon atoms, and having one or two double bonds ((-CH=CH2)) at the end of the hydrocarbon chain. Therefore, a linear terminal olefin is one having the formula (C... n1 H 2n1+1 CH=CH2 or CH2=CH(C) n2 H 2n2α-Alkenes of CH=CH2, wherein n1 is an integer from 4 to 22 and n2 is an integer from 1 to 5.
[0081] For the purposes of this specification, the term "naturally derived straight-chain alkanes" refers to alkanes obtained from biomass, particularly plants, and therefore includes carbon from renewable sources.
[0082] Unlike components derived from fossil materials, components derived from renewable resources contain... 14 C. All carbon samples obtained from living organisms (animals or plants) are actually a mixture of three isotopes: 12 C (approximately 98.892%) 13 C (approximately 1.108%) and 14 C (trace level: 1.2 × 10⁻⁶) -12 %). In living tissue 14 C / 12 The C ratio is the same as in the atmosphere. In the environment, 14 Carbon exists in two main forms: the mineral form, namely carbon dioxide (CO2), and the organic form, namely carbon incorporated into organic molecules.
[0083] In living organisms 14 C / 12 The carbon ratio remains constant through metabolism because carbon is constantly exchanged with the environment. This is due to the carbon content in the atmosphere. 14 The proportion of C is constant, and as long as the organism is alive, the proportion within its body remains similarly constant because it absorbs C. 14 C is like absorption. 12 Same as C. 14 C / 12 The average ratio of C is equal to 1.2 x 10. -12 .
[0084] 12 C is stable, meaning that in a given sample 12 The number of carbon atoms remains constant over time. On the other hand, 14 C is radioactive (each gram of carbon from living organisms contains sufficient...) 14 Carbon isotopes decay 13.6 times per minute, and the number of such atoms in the sample decreases with time (t) according to the following law: n = no exp(-at) in: - no is the initial state (when an organism, animal, or plant dies). 14 The number of C, - n is the number of 14C atoms remaining at the end of time t. - a is the decay constant (or radioactivity constant); it is related to the half-life.
[0085] Half-life (or period) is the time required for any number of radioactive nuclei or unstable particles of a given species to decay by half; half-life T 1 / 2 Through the formula aT 1 / 2 = ln 2 is related to the decay constant a. 14 The half-life of C is 5730 years.
[0086] Considering 14 The half-life of C (T) 1 / 2 This refers to the process from extraction of animal or plant raw materials to formulation manufacturing, and even until the end of their use. 14 The C content is constant.
[0087] The applicant believes that if a mixture of straight-chain alkanes contains at least 20% by mass of renewable source C relative to the total mass of carbon, preferably at least 50% by mass of renewable source C relative to the total mass of carbon, more preferably at least 80% by mass of renewable source C relative to the total mass of carbon, and even more preferably at least 90% by mass of renewable source C relative to the total mass of carbon, then the mixture is of natural origin, i.e. derived from renewable feedstock, and this percentage is preferably measured according to standard ASTM D 6866.
[0088] In other words, if the alkane contains at least 0.2 × 10 -10 quality% 14 C, preferably 0.6×10 -10 quality% 14 C is derived from renewable raw materials.
[0089] Currently, at least two different techniques are used to measure samples. 14 C content: - Liquid scintillation spectroscopy The method includes counting by 14 'Beta' particles produced by C decay: measurements taken from samples of known mass over a certain period of time. 12 β radiation (number of C atoms). This "radioactivity" is related to... 14 The number of C atoms is proportional, therefore it can be determined. The sample contains... 14 C emits beta radiation, which produces photons when it comes into contact with scintillating fluid (scintillator). These photons have different energies (between 0 and 156 keV), forming what is called... 14 C-spectroscopy. Depending on two variations of this method, the analysis involves either CO2 previously generated in a suitable absorption solution from a carbonaceous sample, or benzene previously converted from a carbonaceous sample.
[0090] - Mass spectrometryThe sample is reduced to graphite or gaseous CO2 and analyzed in a mass spectrometer. This technique uses an accelerator and a mass spectrometer to... 14 C ions and 12 C ions were separated to determine the ratio of the two isotopes.
[0091] All these measuring materials 14 Methods for determining carbon content are precisely described in standards ASTM D 6866 (specifically D6866-06) and ASTM D7026 (specifically 7026-04). These methods measure the carbon content of a sample. 14 C / 12 The C ratio was compared with that of a reference sample from a 100% renewable source. 14 C / 12 The C ratios are compared to give the relative percentage of renewable C sources in the sample.
[0092] In the case of straight-chain alkane mixtures of the present invention, the preferred measurement method is mass spectrometry as described in standard ASTM D6866-06 (“accelerator mass spectrometry”).
[0093] For the purposes of this invention, the term "fatty substance" refers to any oily organic substance containing at least one carbon chain with at least 11 carbon atoms and having a solubility of less than 0.1 wt% in water at 25°C (1 atm).
[0094] The "solid fatty substance" preferably has a melting point greater than or equal to 35°C, and / or a melting point at 40°C and 1 s. -1 The viscosity at the shear rate is greater than or equal to 1 Pa·s, particularly from 1 Pa·s to 1,000,000 Pa·s, and preferably from 10 to 1,000 Pa·s. Viscosity measurements can be performed on a Carri-Med CSL2-500 instrument at a temperature of approximately 40°C.
[0095] The solid fatty substance according to the invention can be crystalline, amorphous, or paste-like. The melting point is preferably from 35°C to 250°C, and more particularly from 40°C to 150°C. The melting point can be measured by differential scanning calorimetry (DSC), particularly at a heating rate of 10°C / min. The melting point is therefore the temperature corresponding to the peak of the endothermic melting point obtained during the measurement.
[0096] The prior art describes a mixture of straight-chain alkanes having the same melting point as commercially available synthetic waxes.
[0097] However, measuring the melting point is insufficient to characterize all the physicochemical properties of wax.
[0098] This is because, as mentioned above, straight-chain alkane mixtures are complex mixtures in which each alkane has different physicochemical properties.
[0099] The inventors have made a contribution by developing a method that produces straight-chain alkane mixtures that not only reproduce the melting point of commercially available synthetic waxes but also all their physicochemical properties, such as melting range, hardness, oil separation, and stability.
[0100] The solid fatty substances according to the present invention may in particular be waxy or paste-like fatty substances.
[0101] For the purposes of this invention, "wax" refers to a lipophilic compound that is solid at room temperature (about 25°C), exhibits a reversible solid / liquid phase transition, has a melting point above about 40°C and possibly up to 200°C, and possesses an anisotropic crystalline structure in the solid state. Typically, the size of wax crystals causes them to diffract and / or scatter light, giving compositions containing them a cloudy, more or less opaque appearance. Heating wax to its melting point allows it to be miscible with oil and form a microscopically homogeneous mixture, but by cooling the mixture to room temperature, recrystallization of the wax in the oil mixture is obtained, which is detectable microscopically and macroscopically (opalescent). For a definition of wax, one may refer, for example, to PDDorgan, Drug and Cosmetic Industry, December 1983, pp. 30-33.
[0102] For the purposes of this invention, the term "paste-like fatty substance" refers to a lipophilic fatty compound having a reversible solid / liquid state change, having an anisotropic crystalline structure in the solid state, and containing liquid and solid fractions at a temperature of 23°C.
[0103] In other words, the initial melting point of the paste-like fatty substance can be below 23°C. The liquid fraction of the paste-like fatty substance, measured at 23°C, can account for 9 to 97% by weight of the paste-like fatty substance. This liquid fraction at 23°C preferably accounts for 15 to 85% by weight, and more preferably 40 to 85% by weight.
[0104] For the purposes of this invention, the melting point corresponds to the temperature of the most endothermic peak observed in thermal analysis (DSC), as described in standard ISO 11357-3; 1999. The melting point of a paste-like fatty substance can be measured using a differential scanning calorimeter (DSC), such as the calorimeter sold by TA Instruments under the name "MDSC 2920".
[0105] The measurement plan is as follows: A 5 mg sample of paste-like fatty substance placed in a crucible was first heated from -20°C to 100°C at a heating rate of 10°C / min, then cooled from 100°C to -20°C at a cooling rate of 10°C / min, and finally heated from -20°C to 100°C again at a heating rate of 5°C / min. During the second heating, the power difference absorbed by the empty crucible and the crucible containing the paste-like fatty substance was measured as a function of temperature. The melting point of the paste-like fatty substance is the temperature value corresponding to the peak of the curve representing the power difference as a function of temperature.
[0106] The liquid fraction of a paste-like fatty substance at 23°C, by weight, is equal to the ratio of the enthalpy of fusion consumed at 23°C to the enthalpy of fusion of the paste-like fatty substance. The enthalpy of fusion of a paste-like fatty substance is the enthalpy consumed when the substance changes from a solid to a liquid state. When the entire mass of a paste-like fatty substance is in crystalline solid form, it is said to be in a solid state. When the entire mass of a paste-like fatty substance is in liquid form, it is said to be in a liquid state.
[0107] The enthalpy of fusion of a paste-like fatty substance is equal to the area under the thermal analysis curve obtained using a differential scanning calorimeter (DSC) (such as the calorimeter sold by TA Instruments under the name MDSC 2920) at a heating rate of 5 or 10 °C / min, according to standard ISO 11357-3:1999.
[0108] The enthalpy of fusion of a paste-like fatty substance is the energy required to transform it from a solid to a liquid state. It is expressed in J / g.
[0109] The enthalpy of fusion consumed at 23℃ is the amount of energy absorbed by a sample as it changes from a solid state to its state at 23℃, which consists of liquid and solid fractions.
[0110] The liquid fraction of the paste-like fatty substance, measured at 32°C, preferably accounts for 30-100% by weight, more preferably 50-100% by weight, and even more preferably 60-100% by weight. When the liquid fraction of the paste-like fatty substance measured at 32°C is equal to 100%, the melting range termination temperature of the paste-like fatty substance is less than or equal to 32°C.
[0111] The liquid fraction of a paste-like fatty substance measured at 32°C is equal to the ratio of the enthalpy of fusion consumed at 32°C to the enthalpy of fusion of the paste-like fatty substance. The calculation method for the enthalpy of fusion consumed at 32°C is similar to that for enthalpy of fusion consumed at 23°C.
[0112] Alkene metathesis is a well-known reaction in organic chemistry. This reaction, carried out in the presence of a suitable catalytic system, involves the exchange of alkylene groups between two alkenes according to the following equation: 1. The first case is called "self-metathesis" or "isometathesis" (i.e., the metathesis of one olefin molecule with another olefin molecule of the same kind): [Chemical Formula 5] 2. The second case is called "cross metathesis" (i.e., metathesis between two different alkenes): [Chemical Formula 6] The metathesis of olefins is an equilibrium reaction. It can occur in the presence of a variety of catalysts, typically based on group IVA to VIII transition metals, including tungsten, molybdenum, rhenium, and ruthenium, and can be homogeneous or heterogeneous.
[0113] The term "isomeric metathesis" refers to an olefin metathesis reaction in the presence of a metal hydride, which either a) originates from the intrinsic decomposition of a metathesis catalyst or b) originates from a metal hydride catalyst added to the reaction medium; its role is to isomerize the double bonds present in the starting compound and / or the metathesis reaction products.
[0114] Generally, "distribution" is a function that associates frequency of occurrence with a class of values. In this specification, the term refers to the chain length distribution of the straight-chain alkanes constituting the mixture obtained by this method; in other words, it refers to the distribution of the number of carbon atoms in the straight-chain alkanes constituting the mixture. Therefore, each straight-chain alkane in the mixture is associated with its quantity, particularly its weight percentage relative to the total weight of the mixture. Analysis of this distribution can be performed, in particular, using gas chromatography (GC), optionally coupled with mass spectrometry (GC-MS).
[0115] This distribution is characterized in particular by its central value, namely the mode, median, and mean.
[0116] The mode, or dominant value, corresponds to the most frequent value in the distribution. In this paper, it corresponds to the most representative straight-chain alkane in the mixture, and therefore has the largest weight content in the mixture.
[0117] Since the chain lengths are arranged in ascending order, the median corresponds to the chain length that divides the population into two equal subsets: 50% of the alkane chain lengths are greater than the median, and 50% of the alkane chain lengths are less than the median.
[0118] The average is the sum of the values divided by the number of elements.
[0119] When these three central values coincide (mode = mean = median), the distribution is called a normal or Gaussian distribution. The graphical representation of this distribution is a bell curve, symmetrical about the mean.
[0120] This distribution can also have positive or negative asymmetry.
[0121] When the distribution is positively asymmetric, the tails extend further above the mean. In other words, there are more extreme values on the higher side of the mean, and the tails on the lower side are shorter.
[0122] Conversely, when the distribution is negatively asymmetric, the tails of the distribution are longer on the side with values below the mean. There are more extreme values on the lower side, and the tails on the higher side are shorter.
[0123] These types of asymmetric distributions are characterized by a metric called skewness, which quantifies the degree of asymmetry. Zero skewness corresponds to a perfectly symmetrical distribution, while positive or negative skewness indicates asymmetry on the corresponding side.
[0124] Method for preparing mixtures of straight-chain alkanes from natural sources According to a first aspect, the present invention relates to a method for preparing a mixture of straight-chain alkanes of natural origin, preferably plant origin, comprising the following steps: i) At least one linear terminal olefin containing 5 to 24 carbon atoms is metathesisd in the presence of a non-isomerizing olefin metathesis catalyst, wherein the linear terminal olefin is derived from at least one natural, preferably plant-derived fatty acid or fatty acid ester, thereby obtaining a first internal olefin mixture (I). ii) The internal olefin mixture (I) obtained in step i) isomerizes and metamorphoses in the presence of a catalyst or a mixture of catalysts to obtain a second internal olefin mixture (II), and iii) The mixture of inner olefins (II) is hydrogenated in the presence of a hydrogenation catalyst to obtain a mixture of straight-chain alkanes of natural origin (III).
[0125] Complex decomposition step i) The non-isomerizing olefin metathesis catalyst in step i) can consist of a single catalyst or a mixture of non-isomerizing olefin metathesis catalysts. It can be particularly selected from transition metal complexes, especially alkylene complexes of transition metals, particularly alkylene complexes of ruthenium, or mixtures thereof.
[0126] According to a specific embodiment, the non-isomerization metathesis catalyst in step i) above is a selective non-isomerization catalyst because it prevents the isomerization of terminal olefins.
[0127] Therefore, the method according to the present invention still differs from certain methods in the prior art, such as the method described in patent application WO2021 / 183330 A1, which, by contrast, is based on the use of metathesis catalysts that are isomerized rather than selective. Isomerization catalysts such as those described in patent application WO 2021 / 183330 A1 are well known in the prior art.
[0128] Preferably, the ruthenium catalyst is selected from [Ru-1a], [Ru-1b], or mixtures thereof. The catalyst can be used in particular as a mixture of Ru-1a and Ru-1b, especially with a Ru-1a / Ru-1b weight ratio between 1 and 2, particularly 3 / 7.
[0129] [Chemical Formula 1] Ru-1a has the chemical formula: C 51 H 59 Cl2N4Ru and molecular weight: 900.03 g·mol⁻¹ -1 .
[0130] [Chemical Formula 2] Ru-1b has the chemical formula: C 51 H 67 Cl2N2PRu and molecular weight: 911.05 g.mol -1 .
[0131] The amount of catalyst can be from 0.01 to 1.0 mol%, particularly from 0.1 to 0.5 mol relative to the straight-chain terminal olefin mixture used in step i).
[0132] Step i) is carried out, particularly at a temperature of 70°C to 90°C, under an inert atmosphere. It is especially carried out in a polar aprotic solvent, such as THF.
[0133] The mixture can be stirred until the at least one terminal olefin is completely converted, which can be monitored by proton NMR. Therefore, the mixture can be stirred until the protons of the terminal olefin are completely eliminated, for example, 1 to 3 days, especially two days.
[0134] At the end of step i), the catalyst can be neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture.
[0135] Preferably, the metathesis catalyst is removed, for example by silica gel chromatography and / or filtration.
[0136] The selective non-isomerization catalyst makes it particularly possible to control the mixture of inner olefins obtained at the end of step i), and especially to obtain inner olefins with longer chains at the end of step i), thereby avoiding additional distillation steps to remove inner olefins with shorter chains.
[0137] ii) Olefin isomerization metathesis step Step ii) is carried out using the selective and controlled internal olefin mixture obtained in step i) above.
[0138] The isomerization metathesis step can be carried out in the presence of a single catalyst or a mixture of at least two catalysts.
[0139] When a single catalyst is used, it is selected from those capable of simultaneously performing olefin isomerization and olefin metathesis reactions. These include alkylene complexes of transition metals, particularly alkylene complexes of ruthenium, tungsten, or molybdenum. For example, the Ru-2 catalyst described below may be mentioned.
[0140] When using a catalyst mixture, the mixture may contain a first catalyst for olefin metathesis and a second catalyst solely for olefin isomerization. The catalyst for olefin isomerization may be selected from transition metal-based catalysts, particularly palladium, ruthenium, copper, or iron. For example, the isomerization catalyst may be selected from palladium catalysts (CAS: 185812-86-6) and ruthenium catalysts [RuH(Cl)(CO)(PCy3)3] or [CpRu(PN)(MeCN)]BArF4. Alternatively, the mixture may contain two catalysts, both capable of simultaneously carrying out olefin isomerization and olefin metathesis reactions. Such catalysts may be selected from alkylene complexes of transition metals, particularly alkylene complexes of ruthenium, tungsten, or molybdenum. For example, the Ru-2 and Ru-3 catalysts described below may be mentioned.
[0141] Such catalysts or catalyst mixtures are specifically described in the article: LJGooβen et al. Chem. Eur.J [European Journal of Chemistry]. 2019, 25, 7416 - 7425.
[0142] Preferably, the catalyst or catalyst mixture used in step ii) is or contains a transition metal complex, particularly ruthenium.
[0143] Preferably, the isomerization metathesis catalyst is a mixture of Ru-2 and Ru-3 catalysts. Preferably, the Ru-2 / Ru-3 molar ratio is 0.1 to 1, particularly 0.5.
[0144] [Chemical Formula 3] Ru-2 has the chemical formula: C 52 H 77 Cl₂N₂PRu, molar mass: 933.15 g·mol⁻¹ -1 CAS reference: 373640-75-6.
[0145] [Chemical Formula 4] Ru-3 has the chemical formula: C 39 H 50Cl2F3N3O2Ru, molar mass: 821.81 g·mol⁻¹ -1 CAS reference: 1212008-99-5.
[0146] The amount of catalyst can be from 0.01 to 2 mol%, particularly from 0.1 to 1 mol relative to the internal olefin mixture used in step ii).
[0147] Step ii) is carried out, particularly at a temperature of 70°C to 90°C, under an inert atmosphere. It is especially carried out in a polar aprotic solvent, such as THF.
[0148] The reaction mixture in step ii) can be stirred until the olefin mixture from step i) is completely converted, which can be monitored by proton NMR. Therefore, the mixture can be stirred for 1 to 3 hours, especially 2 hours.
[0149] At the end of step i), the catalyst can be neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture of step ii).
[0150] Preferably, the metathesis catalyst is removed, for example by silica gel chromatography and / or filtration.
[0151] Hydrogenation step iii) The hydrogenation step can be carried out in the presence of a palladium-on-carbon catalyst, particularly at temperatures between 40°C and 60°C, in a nonpolar, aprotic solvent such as cyclohexane.
[0152] It is carried out in the presence of hydrogen, for example at a pressure of 1 bar.
[0153] The reaction mixture in step iii) can be stirred until the olefin mixture from step ii) is completely converted, which can be monitored by proton NMR. Therefore, the reaction mixture in step iii) can be stirred for several hours, particularly 10 to 20 hours. This may include a step of filtering to remove the catalyst at the end of the reaction.
[0154] Naturally derived linear terminal olefins The source of the terminal olefin used in step i) can vary. Specifically, the terminal olefin can be synthesized from unsaturated fatty acid esters derived from vegetable oils or fatty esters derived from jojoba oil by methods known to those skilled in the art. In this regard, particular reference may be made to the following publication: JEMoore et al. Journal of Colloid and Interface Science, 547 (2019), 275-290; J. Terao et al.Angew. Chem. Int. Ed. [Applied Chemistry International Edition]. 2007, 46, 2086-2089; Y. Fujimoto et al. ,Org.Biomol.Chem [Organic and Biomolecular Chemistry]. 2016, 14, 6672; Angelici et al. , J.Org.Chem [Organic Chemistry Journal]. 1996, 61, 7784-7792.
[0155] For example, these terminal olefins can be obtained by ethyleneolysis of unsaturated fatty acid esters from vegetable oils, preferably unsaturated fatty acid esters from jojoba oil. Figure 9 The use of ethylene hydrolysis catalysts. These are particularly alkylene complexes of transition metals, especially alkylene complexes of ruthenium. For example, the Ru-4 catalyst described below may be mentioned.
[0156] [Chemical Formula 7] Ru-4 has the chemical formula C 33 H 42 Cl2NORu has a molar mass of 639.67 g / mol.
[0157] Ru-4 is specifically described in the article: Sytniczuk et al. , Chem Catalysis 3, 100713.
[0158] The amount of catalyst can be from 0.001 to 1 mol%, particularly from 0.01 to 0.5 mol relative to jojoba oil.
[0159] The ethylene hydrolysis reaction is carried out at temperatures between 35°C and 45°C, especially at 40°C.
[0160] The ethylene decomposition reaction is carried out in an autoclave in the presence of ethylene (99.95% purity) at a pressure of, for example, 10 bar.
[0161] Therefore, the mixture can be stirred for 4 to 8 hours, especially 6 hours.
[0162] At the end of the ethylene hydrolysis reaction, the catalyst is neutralized, particularly by adding alkyl vinyl ethers to the reaction mixture.
[0163] The conversion rate of the ethylene hydrolysis reaction can be quantified by GC using the internal standard trimethoxybenzene.
[0164] Advantageously, the terminal olefin used in step i) is obtained according to a method comprising at least the following two steps: a) Isomerizing carboxylic acids and / or mixtures of carboxylic acids and / or carboxylic esters and / or mixtures of carboxylic esters in the presence of an acid catalyst or a metal complex, preferably an iron carbonyl complex, preferably iron pentacarbonyl; b) The reaction product of step a) is ethylene-degraded in the presence of a ruthenium catalyst to obtain a mixture of terminal olefins.
[0165] This method enables the use of methods that are known in the art and, as [[ Figure 2 The method described uses fewer steps to synthesize the terminal olefin used in step i), and the known method is based on the following steps: a) Reduction of carboxylic acids to obtain primary alcohols. b) Bromination step a) yields a primary alcohol to obtain a bromoalkane. c) React the bromoalkane from step b) with magnesium to obtain an organomagdium halide. d) Cross-couple the organo-magnesium halide from step c) with terminal brominated olefins to obtain a mixture of terminal olefins.
[0166] In some embodiments, the at least one linear terminal olefin used in step i) is a mixture of at least two different linear terminal olefins, particularly three different terminal olefins, each containing 5 to 24 carbon atoms, particularly 16 to 24 carbon atoms, preferably 16 to 20 carbon atoms.
[0167] Different linear terminal olefins must differ by at least one carbon number. Therefore, step i) is a cross-metathesis step.
[0168] In some embodiments, the at least two linear terminal olefins differ from each other by at least one, particularly at least two, carbon numbers.
[0169] According to a preferred embodiment, the at least one linear terminal olefin used in step i) is a mixture of three linear terminal olefins, preferably C16 / C18 / C20.
[0170] In particular, a mixture of straight-chain terminal olefins comprising or consisting of the following is used: - 0.5% to 10%, preferably 1% to 10%, or even more preferably 1% to 5% of C16 terminal olefins; - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C18-terminated olefins; and - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C20 terminal olefins; These percentages are expressed in moles relative to the total molar weight of the terminal olefin mixture.
[0171] Mixture of straight-chain alkanes from natural sources According to another aspect, the present invention relates to mixtures of straight-chain alkanes of natural origin, particularly of plant origin, which can be obtained by the method according to the invention.
[0172] According to some embodiments, the mixture contains at least two different straight-chain alkanes, each of which contains 8 to 90 carbon atoms, particularly 10 to 85 carbon atoms, preferably 10 to 75 carbon atoms, even more preferably 17 to 70 carbon atoms, and even more preferably 24 to 60 carbon atoms.
[0173] According to another aspect, the present invention relates to a mixture of straight-chain alkanes of natural, particularly plant, origin, in the form of a solid fatty substance, wherein: - Each straight-chain alkane constituting the mixture contains 8 to 90 carbon atoms, particularly 10 to 85 carbon atoms, preferably 10 to 75 carbon atoms, even more preferably 10 to 70 carbon atoms, even more preferably 17 to 70 carbon atoms, and even more preferably C24 to C60, and the number distribution of each straight-chain alkane in ascending order of carbon atom number is as follows: o Increasing from the minimum number of carbon atoms in straight-chain alkanes to the mode of distribution; and o Decreases between the mode of distribution and straight-chain alkanes with the largest number of carbon atoms. These quantities are calculated as a weight percentage relative to the total weight of the mixture of straight-chain alkanes from this natural source.
[0174] According to certain embodiments, each straight-chain alkane in the distribution differs from the next straight-chain alkane in the distribution by one carbon number. For example, in the case of a distribution with a minimum number of carbon atoms of C16 and a maximum number of carbon atoms of C20, the distribution includes the following alkanes: C16, C17, C18, C19, and C20.
[0175] According to some embodiments, the number of different straight-chain alkanes constituting the mixture is at least 10, particularly at least 20, particularly at least 30, particularly at least 40.
[0176] According to some embodiments, the melting point of the mixture is between 32°C and 90°C. The melting point is determined specifically by DSC thermogravimetric analysis.
[0177] Alkanes having a minimum or maximum number of atoms, particularly those whose weight percentage accounts for at least 1% by weight of the total straight-chain alkane mixture. Below this threshold, any optional straight-chain alkane present will be considered as present in trace amounts and will not be considered part of the distribution. For example, a mixture of alkane in a C16-C20 distribution, i.e., a minimum number of carbon atoms of C16 and a maximum number of atoms of C20, according to this patent application, may contain C14, C15, C21, or C22 alkanes, but their respective weight concentrations will be less than 1% by weight of the total mixture.
[0178] This 1% by weight threshold is specifically set relative to samples with a concentration of at least 100 µg / mL, analyzed by gas chromatography (GC) using a Shimadzu GC-2014 instrument and an Agilent VF-5ht column with the following characteristics: 30 m × 0.25 mm × 0.10 µm, maximum temperature: 430 °C, or specifically using a Shimadzu GC-2030 instrument and a Restek MXT-1HT SimDist column with the following characteristics: 5 m × 0.53 mm × 0.10 µm, maximum temperature: 450 °C.
[0179] According to some embodiments, each straight-chain alkane constituting the mixture contains 20 to 65 carbon atoms. In the context of this specification, this also means that the straight-chain alkane with the smallest number of carbon atoms in the distribution is a C20 alkane and / or the alkane with the largest number of atoms is a C65 alkane.
[0180] According to some embodiments, each straight-chain alkane constituting the mixture contains 24 to 60 carbon atoms.
[0181] According to some embodiments, the distribution mode is between 40 and 45 carbon atoms, and particularly 41 carbon atoms.
[0182] According to some embodiments, the median of the distribution is between 40 and 45 carbon atoms, and particularly between 41 and 43 carbon atoms.
[0183] According to some embodiments, the average distribution is between 40 and 45 carbon atoms, and particularly 41 or 42 carbon atoms.
[0184] In some embodiments, the straight-chain alkane distribution is asymmetrical.
[0185] According to some embodiments, the melting point of the mixture is between 75 and 85°C, approximately 80°C.
[0186] Preferably, the straight-chain alkane mixture is characterized by containing 3 to 6% by weight of C30 to C54 straight-chain alkane relative to the total weight of the mixture.
[0187] According to some embodiments, the straight-chain alkane mixture is a mixture of the following, wherein: - The straight-chain alkanes with the smallest number of carbon atoms have 15 to 19 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 42 to 46 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 20 to 24 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 52 to 56 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 10 to 14 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 45 to 49 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 9 to 13 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 48 to 52 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 9 to 13 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 52 to 56 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 16 to 20 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 63 to 67 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 13 to 17 carbon atoms, and the straight-chain alkanes with the largest number of carbon atoms have 66 to 70 carbon atoms; or - The straight-chain alkanes with the smallest number of carbon atoms have 19 to 23 carbon atoms, while the straight-chain alkanes with the largest number of carbon atoms have 49 to 53 carbon atoms.
[0188] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 15 to 19 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 42 to 46 carbon atoms, and has a melting point of about 49°C.
[0189] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 20 to 24 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 52 to 56 carbon atoms, and has a melting point of about 75°C.
[0190] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 19 to 23 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 49 to 53 carbon atoms, and has a melting point of about 68.5°C.
[0191] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 10 to 14 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 45 to 49 carbon atoms, and has a melting point of about 32°C.
[0192] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 9 to 13 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 48 to 52 carbon atoms, and has a melting point of about 37°C.
[0193] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 9 to 13 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 52 to 56 carbon atoms, and has a melting point of about 58°C.
[0194] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 16 to 20 carbon atoms and the straight-chain alkane having a larger number of carbon atoms has 63 to 67 carbon atoms, and has a melting point of about 74°C.
[0195] According to some embodiments, the straight-chain alkane mixture constituting the mixture is a mixture in which the straight-chain alkane having a smaller number of carbon atoms has 13 to 17 carbon atoms, and the straight-chain alkane having a larger number of carbon atoms has 66 to 70 carbon atoms, and has a melting point of about 74°C.
[0196] The term "about x" refers to a value in the range of x - 0.1x to x + 0.1x.
[0197] Composition According to another aspect, the present invention relates to a composition comprising a mixture of straight-chain alkanes according to the invention, particularly a cosmetic and / or pharmaceutical composition.
[0198] According to certain embodiments, the compositions according to the invention contain less than 3% mineral and / or synthetically derived additional solid fatty substances, particularly less than 1%. Preferably, the cosmetic compositions are free of mineral and / or synthetically derived additional solid fatty substances, the percentages being expressed by weight relative to the total weight of the composition.
[0199] cosmetic compositions According to another aspect, the present invention relates to a cosmetic composition comprising a mixture of straight-chain alkanes according to the present invention.
[0200] According to certain embodiments, the cosmetic composition comprises 0.1 to 25% by weight of a mixture of straight-chain alkanes according to the invention relative to the total weight of the composition.
[0201] In particular, when the cosmetic composition is in the form of a cream, especially a relatively dense cream, it may contain 0.1 to 5% by weight of a mixture of straight-chain alkanes according to the invention relative to the total weight of the composition.
[0202] When the cosmetic composition is in the form of a product poured into a vessel, it may contain 0.1 to 12% by weight of a mixture of straight-chain alkanes according to the invention relative to the total weight of the composition.
[0203] When the cosmetic composition is in rod form, it may contain 0.1 to 25% by weight of a mixture of straight-chain alkanes according to the invention relative to the total weight of the composition.
[0204] When the cosmetic composition is in the form of mascara, it may contain 0.1 to 15% by weight of a mixture of straight-chain alkanes according to the invention relative to the total weight of the composition.
[0205] Cosmetic compositions are particularly characterized as skin care, cosmetic, or fragrance products. These products can be applied to the skin (face or eyelids), mucous membranes (especially lips), or body surfaces (eyelashes, eyebrows, hair, or nails). Among these products, anhydrous products or products in emulsion form are particularly noteworthy, such as water-in-wax emulsions, oil-in-water emulsions, water-in-oil emulsions, or multiple emulsions. Specifically, they can be cosmetic compositions, preferably anhydrous and in solid form, for the care and / or cosmetic application of keratin materials, particularly to the skin, eyelids, eyebrows, or lips, containing a mixture of straight-chain alkanes according to the invention in a physiologically acceptable medium.
[0206] The term "anhydrous composition" specifically refers to a composition in which water is preferably not intentionally added, but may be present in trace amounts in the various compounds used in the composition. In particular, the composition according to the invention contains less than 4% by weight of water relative to the total weight of the composition, preferably less than 3% by weight, more preferably less than 2% by weight, more preferably less than 1% by weight, and even more preferably less than 0.5% by weight, or even completely anhydrous. According to certain embodiments, the composition is anhydrous. According to the invention, the term "solid form composition" refers to a composition with a hardness greater than 30 Nm at 20°C and atmospheric pressure (760 mm Hg). -1 Preferably greater than 40 Nm -1The composition. Hardness can be measured at 20°C using the "butter cut" method, which involves evaluating the lipstick's firmness specifically by measuring the cutting resistance of the product in rod form. This measurement is performed 24 hours after formulation using a texture analyzer (TAXTPlus, MicroStable Systems, UK) equipped with a 5 kg force sensor and its Butter Cutter A / BC probe (Swantech, MicroStable Systems, UK). This allows measurement of the maximum resistance of the rod during the cutting of butter shreds at a speed of 1.6 mm / s to a depth of 9 mm. To ensure reproducibility of the measurements, the analysis is repeated on six rods, and the relative difference between measurements must not exceed 10%, ideally 5%. For each product type, a reference (target) range is established to ensure the mechanical properties of the rod. The solid composition according to the invention generally has a hardness greater than or equal to 70 g, particularly greater than or equal to 90 g, for example 100 g to 400 g, preferably 140 g to 300 g, and even more preferably 175 g to 250 g. These compositions (particularly corresponding to casting sticks in the standard format of approximately 12.7 mm) possess sufficient stability and rigidity: the stick is rigid and strong enough not to break during application, thus being compatible with stick-shaped or other solid forms of packaging and with surfaces to be treated and / or cosmetically applied by friction; they are also characterized by ease of application, such as good slip properties, good deposition upon first application, and a comfortable texture. The compositions can be in stick form or packaged in containers. They can also be fluid products, such as lip gloss or mascara (water-in-wax emulsion). They can also be products in loose powder or pressed powder form.
[0207] The cosmetic compositions according to the invention may also contain other ingredients, particularly additional solid fatty substances, especially polar and / or non-polar waxes, or paste-like fatty substances.
[0208] The term "additional solid fatty substances" herein refers to fatty substances that are different from the straight-chain alkane mixtures according to the present invention. These additional solid fatty substances may in particular be of mineral and / or synthetic origin.
[0209] According to certain embodiments, the cosmetic composition according to the invention contains less than 3% by weight of mineral and / or synthetically derived additional solid fatty substances, particularly less than 1% by weight. Preferably, the cosmetic composition is free of mineral and / or synthetically derived additional solid fatty substances, the percentages being expressed by weight relative to the total weight of the composition.
[0210] The term "polar wax" refers to a wax that contains at least one heteroatom, such as oxygen, nitrogen, silicon, or phosphorus.
[0211] Specifically, polar waxes may be selected from the group consisting of: beeswax, carnauba wax, candelilla wax, cotton wax, rice bran wax, berry wax, Chinese insect wax, lanolin and its alcohols, acetylated, esterified or polyethoxylated derivatives, kapok wax, sugarcane wax, hexyl laurate, jojoba wax, shellac wax, polyethoxylated cholesterol ether, synthetic beeswax sold by Koster Keunen under the trade name Kester Wax K82H, or mixtures thereof.
[0212] Also mentioned are plant ester waxes selected from the following groups: jojoba esters, polyglycerol-3, and acacia purpurea (…). Acacia decurrens A mixture of flower wax and sunflower seed wax, the mixture being sold by Gattefosse under the trade name Actire®; jojoba esters sold by Floratech under the trade names Floraesters 60 or Floraesters 70; and alkyl or hydrogenated alkyl esters sold by Sophim under the trade name Phytowax, such as hydrogenated lauroyl oleate sold under the trade name Phytowax Olive 12L44.
[0213] The term "nonpolar wax" refers to hydrocarbon waxes and / or silicone waxes.
[0214] The term "hydrocarbon-based nonpolar wax" refers to a wax that contains only carbon and hydrogen atoms and no heteroatoms such as oxygen, nitrogen, silicon, or phosphorus.
[0215] Examples of hydrocarbon-based nonpolar waxes suitable for the compositions of this invention include polyethylene waxes, such as those sold by New Phase Technologies under the trade name Performalene 400 (P400) or by Jeen International Corporation under the trade name Jeenate 3H; blends of high molecular weight linear polyethylene and ethylene / propylene copolymers sold by Safi-Alcan under the trade name Lipwax® PZ80-20; synthetic waxes, such as those sold by Sasol under the name Sasol Wax C80; and mixtures of synthetic and plant waxes, such as synthetic waxes and carnauba waxes sold by Strahl & Pitsch under the name Smart Wax 202. Copernica cerifera A mixture of synthetic waxes, candelilla wax, and carnauba wax, marketed by Stonebees Corporation under the name Smart Wax 7743S. Copernica ceriferaMixtures of Fischer-Tropsch waxes, such as those sold by Cirebelle under the name Cirebelle 303, or mixtures thereof; lignite waxes, ceresin waxes, natural ceresin waxes, microcrystalline waxes and mineral paraffin waxes.
[0216] The term "nonpolar silicone wax" refers to a wax containing silicon heteroatoms.
[0217] An example of a nonpolar silicone wax suitable for use in the compositions of the present invention is C24-28 alkyl polydimethylsiloxane, marketed by Evonik Industries AG under the name Abil Wax.
[0218] Cosmetic compositions according to the invention may contain additional creamy fatty substances. Such compounds are in particular mixtures of sterol esters, such as a mixture of cholesterol and lanosterol esters available from the manufacturer Croda under the trade name Super Sterol Ester®.
[0219] The compositions according to the invention may further comprise a paste-like fatty substance, which may advantageously be selected from: - Liquid petroleum jelly, also known as Vaseline, - Lanolin and its derivatives, - Polymerized or non-polymerized silicone compounds, - Polymerized or non-polymerized fluorinated compounds, - Vinyl polymers, particularly homopolymers and copolymers of olefins, homopolymers and copolymers of hydrogenated dienes, linear or branched oligomers, preferably homopolymers or copolymers of (meth)acrylates containing C8-C30 alkyl groups, homopolymers and copolymer oligomers of vinyl esters containing C8-C30 alkyl groups, and homopolymers and copolymer oligomers of vinyl ethers containing C8-C30 alkyl groups. - A lipid-soluble polyether produced by polyetherification between one or more C2-C100, and preferably C2-C50, diols. - A mixture of beeswax and octyldodecanol, such as the product sold by Zenitech under the name ZenibeeCream. - Ester, - Vegetable butters, such as mango butter, shea butter, cocoa butter, cottonseed butter, avocado butter, etc. Or a mixture thereof.
[0220] In esters, the following can be used in particular: - Oligoglycerides, especially diglycerides, particularly adipic acid / glycerol condensates, some of which have reacted with fatty acids such as stearic acid, decanoic acid, stearic acid, isostearic acid, and mixtures of 12-hydroxystearic acid, especially products like those marketed by Sasol under the brand name Softisan 649. - Arachidyl propionate, marketed by Alzo under the brand name Waxenol 801. - Phytosterol esters, such as products with the INCI name "bis-behenol / isostearyl / phytosterol di-linoleyl di-linoleate," marketed by Nippon Fine Chemicals under the name Pladool-G, or "phytosterol / behenol / octyldodecyl / isostearyl lauroyl glutamate," marketed by Ajinomoto under the name Eldew-PS308. - Fatty acid triglycerides and their derivatives, such as a mixture of stearyl heptanoate and stearyl octanoate sold by Stéarinerie Dubois under the name DUB Solide in France. - Pentaerythritol ester, - Non-crosslinked polyesters produced by polycondensation between linear or branched C4-C50 dicarboxylic acids or polycarboxylic acids and C2-C50 diols or polyols. - Aliphatic esters formed by the esterification of aliphatic hydroxycarboxylic acids with aliphatic carboxylic acids, such as hexadecyl lactate sold by ISP (International Speciality Products) under the name Ceraphyl 28. - Polyesters derived from polycarboxylic acid esterification of aliphatic hydroxycarboxylic acid esters, wherein the esters contain at least two hydroxyl groups, such as products Risocast DA-H® and Risocast DA-L®. Or a mixture thereof.
[0221] Among the added creamy fatty substances, phytosterol esters are preferred, such as products corresponding to the INCI name bis-behenol / isostearyl / phytosterol di-linoleyl di-linoleate, which are sold by Nippon Seika Co., Ltd. under the name Pladool-G; phytosterol / behenol / octyldecyl lauroyl glutamate, which are sold by Ajinomoto Co., Ltd. under the name Eldew-PS308, or mixtures thereof.
[0222] The composition may include additional fatty substances with melting points between 25°C and 55°C. The fatty substances with melting points between 25°C and 55°C are selected from hydrogenated oils that are solid at 25°C or fatty esters that are solid at 25°C and mixtures thereof.
[0223] Among hydrogenated oils that are solid at 25°C, hydrogenated castor oil, hydrogenated palm oil, hydrogenated tallow, and hydrogenated coconut oil can be mentioned, for example, they are available from Prod'Hyg under the trade name Hydrobase 32-34.
[0224] Among fatty esters that are solid at 25°C, propylene glycol myristate, myristate myristate, and cetyl alcohol can be mentioned.
[0225] Hydrogenated coconut oil is preferred for fat components with a melting point between 25°C and 55°C.
[0226] The cosmetic compositions according to the present invention may also contain lipophilic gelling agents or film-forming polymers.
[0227] Lipophilic gelling agents In the context of this patent application, the term "lipophilic gelling agent" refers to a substance capable of curing or gelling oils present in the compositions of the present invention.
[0228] Among the lipophilic gelling agents used, polymeric or molecular organic or mineral lipophilic gelling agents are particularly noteworthy.
[0229] Examples of polymeric organic lipophilic gelling agents include sucrose fatty acid esters, preferably esters of sucrose, stearic acid, and acetic acid, such as sucrose tetrastearate triacetate (INCI name sucrose tetrastearate triacetate), which is available from Sisterna under the trade name Sisterna® A10E-C.
[0230] Another type of polymeric organic lipophilic gelling agent besides sucrose polyesters is composed of dextrin esters. Fatty acid esters of dextrin, such as dextrin palmitate, can be mentioned.
[0231] Another type of polymeric organic lipophilic gelling agent is composed of glycerol esters. One example is the diester of eicosapentaic acid and glycerol esterified with behenate. It is specifically available from Nisshin Oillio Co., Ltd. under the trade name Nomcort® HK-G.
[0232] As a lipophilic mineral gelling agent, fumed silica with a particle size of less than 1 µm, optionally with a hydrophobic surface treatment, can be mentioned. The silica surface can indeed be chemically modified through a chemical reaction, thereby reducing the number of silanol groups present on the silica surface. In particular, silanol groups can be replaced by hydrophobic groups to produce hydrophobic silica. The hydrophobic groups can be: - Trimethylsiloxy, specifically obtained by treating fumed silica in the presence of hexamethyldisilazane. Silica treated in this way is referred to as "Silica silylate" according to the CTFA (8th edition, 2000). For example, they are sold by Degussa under index number Aerosil R812® and by Cabot under Cab-O-Sil TS-530®. - Dimethylsiloxy or polydimethylsiloxane, particularly obtained by treating fumed silica in the presence of polydimethylsiloxane or dimethyldichlorosilane. Such treated silica is referred to as "Silica dimethyl silylate" according to the CTFA (8th edition, 2000). They are marketed, for example, by Degussa under index numbers Aerosil R972® and Aerosil R974®, and by Cabot Corporation under CAB-O-SILTS-610® and CAB-O-SILTS-720®.
[0233] In particular, the particle size of hydrophobic fumed silica can be in the nanometer to micrometer range, for example, about 5 to 200 nm.
[0234] Polymerized organic lipophilic gelling agents include, for example, partially or fully crosslinked elastomeric organopolysiloxanes with a three-dimensional structure, such as those marketed by Shin-Etsu Chemical Co., Ltd. under the names KSG6®, KSG16®, and KSG18®; those marketed by Dow Corning under Trefil E-505C® and Trefil E-506C®; those marketed by Grant Industries under Gransil SR-CYC®, SR DMF10®, SR-DC556®, SR 5CYC gel®, SR DMF 10 gel®, and SR DC 556 gel®; and those marketed by General Electric under SF 1204® and JK 113®; ethyl cellulose, such as that marketed by Dow Chemical Company (Dow... Products sold under the name Ethocel® (Chemical); galactomannans, each sugar containing one to six, and particularly two to four, hydroxyl groups substituted with saturated or unsaturated alkyl chains, such as guar gum alkylated with C1 to C6, and particularly C1 to C3 alkyl chains, or mixtures thereof. "Diblock", "triblock", or "star" block copolymers, of the type polystyrene / polyisoprene or polystyrene / polybutadiene, such as those marketed by BASF under the name Luvitol HSB®; of the type polystyrene / copolymer (ethylene-propylene), such as those marketed by Shell Chemical under the name Kraton®; or of the type polystyrene / copolymer (ethylene-butene); mixtures of triblock and star copolymers in isododecane, such as those marketed by Penreco under the name Versagel®, such as mixtures of butene / ethylene / styrene triblock copolymers and ethylene / propylene / styrene star copolymers in isododecane or hydrogenated polyisobutylene (Versagel ME 2000) (Versagel M 5960).
[0235] Another type of polymeric organic lipophilic gelling agent is composed of polyamide resin or poly(ester-amide) resin, such as ester-terminated polyamide (ETPA), ester-terminated poly(ester-amide) (ETPEA), tertiary amide-terminated polyamide (ATPA), polyalkoxy-terminated polyamide (PAOPA), or polyether polyamide (PEPA).
[0236] Examples of ester-terminated polyamides (ETPA) are those with the INCI name “ethylenediamine / stearyl dimer linoleate copolymer”, and are available, for example, from Arizona Chemical under the trade name Uniclear® 100VG.
[0237] Examples of ester-terminated poly(ester-amide) (ETPEA) are those with the INCI name polyamide-8, which is “ethylenediamine bis-stearyl ethylenediamine / neopentyl glycol / stearyl dimer dibenzoate copolymer”, and are available, for example, from Croda under the trade name Oloecraft® LP-20-PA-MV.
[0238] Examples of tertiary amide-terminated polyamides (ATPA) are those with the INCI name "ethylenediamine / hydrogenated di-linoleate copolymer bis-di-C14-18 alkylamide", and are available, for example, from Arizona Chemical Company under the trade names Sylvaclear® A200V or Sylvaclear® A2614V, or those with the INCI name "diisostearyl malate and bis-distearate di-linoleic acid / ethylenediamine copolymer", and are available, for example, from Kokyu Alcohol Kogyo under the trade name Haimalate PAM.
[0239] Examples of polyalkoxy-terminated polyamides (PAOPA) are those with the INCI name polyamide-3, such as those available from Arizona Chemical Company under the names Sylvaclear® AF1900V, Sylvaclear® PE1800V, and Sylvaclear® PA1200V.
[0240] Examples of polyether polyamide (PEPA) are those with the INCI name polyamide-6, such as those available from Arizona Chemical Company under the name Sylvaclear® PE400V.
[0241] Another type of polymeric organic lipophilic gelling agent is formed from N-acylglutamic acid diamides. Particularly noteworthy are N-acylglutamic acid diamides containing straight-chain alkyl groups, such as dibutyllauroyl glutamine, and N-acylglutamic acid diamides containing branched-chain alkyl groups, such as dibutylethylhexanoyl glutamine. Dibutyllauroyl glutamine is marketed under the name GP-1, and dibutylethylhexanoyl glutamine is marketed under the name EB-21; both are marketed by Ajinomoto Co., Ltd.
[0242] Among lipophilic gelling agents, sucrose fatty acid esters, dextrin esters, and glycerides are preferred.
[0243] Film-forming polymers The compositions according to the present invention may further contain at least one film-forming polymer.
[0244] Among the film-forming polymers that can be used in the compositions of the present invention, reference may be made to synthetic polymers, free radical or condensation polymers, polymers of natural origin, and mixtures thereof.
[0245] The term "free radical film-forming polymer" refers to polymers obtained by polymerization, in particular, of olefinically unsaturated monomers, each of which can homopolymerize (unlike condensation polymers).
[0246] Free radical film-forming polymers can be, in particular, vinyl polymers or copolymers, especially acrylic polymers.
[0247] Vinyl film-forming polymers can be obtained by polymerization of olefinic unsaturated monomers containing at least one acid group and / or esters of these acid monomers and / or amides of these acid monomers.
[0248] As monomers with acid groups, unsaturated α,β-olefinic carboxylic acids, such as acrylic acid, methacrylic acid, crotonic acid, maleic acid, and itaconic acid, can be used. (Meth)acrylic acid, itaconic acid, and crotonic acid are preferred, and itaconic acid (e.g., metal salts of poly(itaconic acid), such as those sold by Itaconix Ltd. under the product index number RevcareNE 100S) is more preferred.
[0249] The ester of the acid monomer is advantageously selected from esters of (meth)acrylic acid (also known as (meth)acrylates), especially alkyl (meth)acrylates, particularly C1-C30 alkyl, preferably C1-C20 alkyl, aryl (meth)acrylates, particularly C6-C10 aryl, and hydroxyalkyl (meth)acrylates, particularly C2-C6 hydroxyalkyl.
[0250] Among (meth)acrylate alkyl esters, methyl methacrylate, ethyl methacrylate, butyl methacrylate, isobutyl methacrylate, 2-ethylhexyl methacrylate, lauryl methacrylate, and cyclohexyl methacrylate may be mentioned.
[0251] In the context of (meth)acrylates, hydroxyethyl acrylate, 2-hydroxypropyl acrylate, hydroxyethyl methacrylate, and 2-hydroxypropyl methacrylate may be mentioned.
[0252] Among (meth)acrylates, benzyl acrylate and phenyl acrylate may be mentioned.
[0253] The particularly preferred (meth)acrylate is the (meth)acrylate alkyl ester.
[0254] According to the present invention, the alkyl group of the ester may be fluorinated or perfluorinated, that is, some or all of the hydrogen atoms of the alkyl group are replaced by fluorine atoms.
[0255] Examples of amides as acid monomers include (meth)acrylamides, particularly N-alkyl (meth)acrylamides, especially C2-C12 alkyl. Among N-alkyl (meth)acrylamides, N-ethylacrylamide, N-tert-butylacrylamide, N-tert-octylacrylamide, and N-undecylacrylamide may be mentioned.
[0256] Vinyl film-forming polymers can also be obtained by homopolymerization or copolymerization of monomers selected from vinyl esters and styrene monomers. In particular, these monomers can be polymerized with acid monomers and / or their esters and / or their amides (such as those mentioned above).
[0257] Examples of vinyl esters that may be mentioned include vinyl acetate, vinyl neodecanoate, vinyl neopentanoate, vinyl benzoate, and tert-butylbenzoate.
[0258] As styrene monomers, styrene and α-methylstyrene can be mentioned.
[0259] Styrene / butadiene block copolymers can also be mentioned, such as products from Kraton or Oleoflex EG 200 from Applechem.
[0260] Among film-forming condensates, polyurethane, polyester, polyesteramide, polyamide, epoxy ester resin and polyurea can be mentioned.
[0261] Polyurethane can be selected from anionic, cationic, nonionic or amphoteric polyurethanes, polyurethane-acrylic, polyurethane-polyvinylpyrrolidone, polyester-polyurethane, polyether-polyurethane, polyurea, polyurea-polyurethane and mixtures thereof.
[0262] Polyesters can be obtained in a known manner through the polycondensation of dicarboxylic acids with polyols, particularly diols.
[0263] Dicarboxylic acids can be aliphatic, alicyclic, or aromatic. Examples of such acids include: oxalic acid, malonic acid, dimethylmalonic acid, succinic acid, glutaric acid, adipic acid, pimelic acid, 2,2-dimethylglutaric acid, azelaic acid, octanoic acid, sebacic acid, fumaric acid, maleic acid, itaconic acid, phthalic acid, dodecanoic acid, 1,3-cyclohexanedicarboxylic acid, 1,4-cyclohexanedicarboxylic acid, isophthalic acid, terephthalic acid, 2,5-norbornanedicarboxylic acid, diethylene glycol, thiodipropionic acid, 2,5-naphthalenedicarboxylic acid, and 2,6-naphthalenedicarboxylic acid. These dicarboxylic acid monomers can be used alone or in combination of at least two. Among these monomers, phthalic acid, isophthalic acid, and terephthalic acid are preferred.
[0264] The diol can be selected from aliphatic, alicyclic, or aromatic diols. Preferred diols are those selected from: ethylene glycol, diethylene glycol, triethylene glycol, 1,3-propanediol, cyclohexanediol, and 4-butanediol. Other polyols that can be used include glycerol, pentaerythritol, sorbitol, and trimethylolpropane.
[0265] Polyesteramides can be obtained by polycondensation of diacids with diamines or amino alcohols in a manner similar to that of polyesters. As diamines, ethylenediamine, hexamethylenediamine, meta- or para-phenylenediamine can be used. As amino alcohols, monoethanolamine can be used. As polyamide resins, products corresponding to the INCI name diisostearyl malate & Bis bis-bisoctadecylamine dimerlinoleic acid / ethylenediamine copolymer can also be mentioned, sold by Kokyu Alcohol Kogyo under the trade name Haimalate PAM.
[0266] Polyesters may also contain at least one monomer with at least one -SO3M group, where M represents a hydrogen atom or an ammonium ion (NH4). + Or metal ions, such as Na + Li + K + Mg 2+ Ca 2+ Cu 2+ Fe 2+ Fe 3+ In particular, bifunctional aromatic monomers containing this -SO3M group can be used.
[0267] As described above, the aromatic ring of the bifunctional aromatic monomer also bearing the -SO3M group can be selected, for example, from benzene, naphthalene, anthracene, biphenyl, oxybiphenyl, sulfonylbiphenyl, and methylenebiphenyl. Examples of bifunctional aromatic monomers also bearing the -SO3M group include: sulfoisophthalic acid, sulfoterephthalic acid, sulfophthalic acid, and 4-sulfonnaphthal-2,7-dicarboxylic acid.
[0268] Copolymers based on isophthalic acid esters / sulfonated isophthalic acid esters can be used, and more particularly copolymers obtained by condensation of diethylene glycol, cyclohexanediol, isophthalic acid, and sulfonated isophthalic acid.
[0269] Naturally derived polymers, which may be modified, may be selected from shellac resin, senna resin, gum arabic (Acacia senegal Gum), dammar resin, elemi resin, copal resin, cellulose polymers, polymers extracted from *Lysimachia christinae* fruit and / or *Kappa longifolia* algae (e.g., Filmexel® products sold by Silab), and mixtures thereof. Natural polymers such as Filmexel® particularly provide improved durability of films obtained from compositions according to the invention. Film-forming polymers with INCI names of *Salvia spicatum* resin + beeswax, *Salvia spicatum* resin + sunflower, *Araucaria heterophylla* resin + sunflower seed oil, *Araucaria heterophylla* resin + castor seed oil, and *Salvia spicatum* resin + octyl-dodecyl alcohol may also be mentioned. Rosin esters, such as glyceryl rosinate, may also be mentioned, available from Gattefossé under the trade name NatPure GR.
[0270] According to one embodiment, the film-forming polymer may be a polymer that is solubilized in a liquid fat phase containing organic oil or solvent (in this case, the film-forming polymer is referred to as a fat-soluble polymer).
[0271] Examples of lipid-soluble polymers include copolymers of vinyl esters (where the vinyl group is directly bonded to the oxygen atom of the ester group and the vinyl ester contains a linear or branched saturated hydrocarbon radical of 1 to 19 carbon atoms bonded to the carbonyl group of the ester group) with at least one other monomer, which may be a vinyl ester (different from existing vinyl esters), an α-olefin (containing 8 to 28 carbon atoms), an alkyl vinyl ether (wherein the alkyl group contains 2 to 18 carbon atoms), or an allyl or methyl allyl ester (having a saturated, linear or branched hydrocarbon radical of 1 to 19 carbon atoms bonded to the carbonyl group of the ester group).
[0272] These copolymers can be crosslinked using a crosslinking agent, which can be vinyl, allyl, or methyl allyl, such as tetraallyloxyethane, divinylbenzene, divinyl octanoate, divinyl dodecanoate, and divinyl octadecanoate.
[0273] For example, the following copolymers may be mentioned: vinyl acetate / allyl stearate, vinyl acetate / vinyl laurate, vinyl acetate / vinyl stearate, vinyl acetate / octadecene, vinyl acetate / octadecyl vinyl ether, vinyl propionate / allyl laurate, vinyl propionate / vinyl laurate, vinyl stearate / octadecene-1, vinyl acetate / dodecene-1, vinyl stearate / ethyl vinyl ether, vinyl propionate / cetyl vinyl ether, vinyl stearate / allyl acetate, 2,2-dimethyl octanoate / vinyl laurate, 2,2-dimethyl valerate allyl Ester / vinyl laurate, vinyl dimethylpropionate / vinyl stearate, allyl dimethylpropionate / vinyl stearate, vinyl propionate / vinyl stearate (crosslinked with 0.2% divinylbenzene), vinyl dimethylpropionate / vinyl laurate, crosslinked with 0.2% divinylbenzene, vinyl acetate / octadecyl vinyl ether, crosslinked with 0.2% tetraallyloxyethane, vinyl acetate / allyl stearate, crosslinked with 0.2% divinylbenzene, vinyl acetate / 1-octadecene, crosslinked with 0.2% divinylbenzene, and allyl propionate / allyl stearate, crosslinked with 0.2% divinylbenzene.
[0274] As a lipophilic film-forming polymer, lipophilic copolymers may also be mentioned, especially those obtained by copolymerization of vinyl esters or alkyl esters of acrylic acid or methacrylate containing 9 to 22 carbon atoms, wherein the alkyl group contains 10 to 20 carbon atoms.
[0275] Such fat-soluble copolymers may be selected from polyvinyl stearate copolymers, polyvinyl stearate, poly(meth)acrylate stearate, polyvinyl laurate, and poly(meth)acrylate copolymers crosslinked with divinylbenzene, diallyl ether, or diallyl phthalate, which may be crosslinked with methylene glycol dimethacrylate or tetraethylene glycol.
[0276] The fat-soluble copolymers defined above are known and specifically described in patent application FR-A-2 232 303; they may have a weight-average molecular weight of 2,000 to 500,000, and preferably 4,000 to 200,000.
[0277] Also mentioned are fat-soluble homopolymers, especially those obtained by homopolymerization of vinyl esters or alkyl esters of acrylic acid or methacrylate containing 9 to 22 carbon atoms, with alkyl radicals containing 2 to 24 carbon atoms.
[0278] Examples of fat-soluble homopolymers include polyvinyl laurate and poly(meth)acrylate, which can be crosslinked using ethylene glycol or tetraethylene glycol dimethacrylate.
[0279] As film-forming lipid-soluble polymers that can be used in this invention, references may also be made to polyalkylene copolymers, and particularly copolymers of C2-C20 olefins, such as polybutene, and alkyl celluloses having linear or branched, saturated or unsaturated C1 to C8 alkyl radicals, such as ethyl cellulose and propyl cellulose, vinylpyrrolidone (VP) copolymers, and particularly vinylpyrrolidone / C2-C40 and even better C3-C20 olefin copolymers. Examples of VP copolymers that can be used in this invention include the following copolymers: VP / vinyl acetate, VP / ethyl methacrylate, butylated polyvinylpyrrolidone (PVP), VP / ethyl methacrylate / methacrylic acid, VP / eicosene (Antaron V220 sold by Ashland), VP / hexadecene (Antaron V216 sold by Ashland), VP / triacene, VP / styrene, and VP / acrylic acid / laurate methacrylate.
[0280] Dextrin esters can also be mentioned, and in particular: - Dextrin isostearate & isostearic acid, sold by Chiba Flour Milling Co., Ltd. under the name Unifilma HVY; - Dextrin palmitate / ethylhexanoate sold by Chiba Milling Co., Ltd. under the name Rheopearl TT; - Dextrin myristate ester sold by Chiba Flour Milling Co., Ltd. under the name Rheopearl MKL2.
[0281] Sugar esters can also be mentioned, especially sucrose isobutyrate sold by Eastman Chemical Company under the name EastmanSustane SAIB.
[0282] Silicone resins may also be mentioned; they are typically soluble in or swellable in silicone oil and are cross-linked polyorganosiloxane polymers. Silicone resins are known by the name "MDTQ," which describes the resin based on the different siloxane monomer units it contains, with each letter "MDTQ" representing a unit type.
[0283] Examples of commercially available polymethylsilsesquioxane resins include those sold by Wacker under the index number Resin MK, such as Belsil PMS MK, and those sold by Shin-Etsu Chemical Co., Ltd. under the index numbers KR-220L or SilForm Flexible Resin.
[0284] As for siloxysilicate resins, trimethylsiloxysilicate (TMS) resins may be mentioned, such as those sold by General Electric under index number SR1000 or by Wacker under index number TMS 803. Also mentioned are trimethylsiloxysilicate resins sold in solvents such as cyclomethicone oils, such as those sold by Shin-Etsu Chemical Co., Ltd. under the name KF-7312J, and by Dow Corning under Dowsil™ RSN-0749 or Dowsil™ 593 Fluid.
[0285] Also mentioned are copolymers of silicone resins (such as those mentioned above) with polydimethylsiloxanes, such as the pressure-sensitive adhesive copolymers sold by Dow Corning under index number BIO-PSA and described in US 5,162,410, or silicone copolymers produced by reacting silicone resins (such as those mentioned above) with diorganosiloxanes, as described in WO 2004 / 073,626.
[0286] Copolymers of non-silicone organic backbones grafted with monomers containing polysiloxane units can also be used, such as butyl acrylate / hydroxypropyl polydimethylsiloxane acrylate copolymers sold by Grant Chemical Company under the name Granacrysil BAS.
[0287] Finally, one may mention acrylate / polytrimethylsiloxymethacrylate copolymers, which contain carbosiloxane dendritic structures grafted onto a vinyl backbone, commercially available under index numbers Dowsil FA 4002 ID or Dowsil FA 4001 CM.
[0288] Alternatively, organosilicon polyamides of the polyorganosiloxane type, such as those described in US-A-5 874 069, US-A-5 919441, US-A-6 051 216 and US-A-5 981 680, can be used.
[0289] Natural resins, dextrin esters, and rosin esters are preferred as film-forming agents.
[0290] In a preferred embodiment, the composition according to the invention comprises 1 to 15% by weight of a film-forming polymer, preferably 5 to 12% by weight of at least one film-forming polymer.
[0291] Oil For the purposes of this invention, the term "oil" refers to a compound that is liquid at room temperature (25°C) and is completely insoluble in water when introduced into water at 25°C in a proportion of at least 1% by weight, or has a solubility of less than 10% by weight relative to the weight of oil introduced into the water.
[0292] Non-volatile oils The term "non-volatile oil" refers to an oil with a boiling point typically above 300°C and a very low or no vapor pressure at 760 mmHg (101,325 Pa).
[0293] Non-volatile oils may be selected in particular from non-volatile silicone oils, non-volatile hydrocarbon oils and mixtures thereof.
[0294] The term "silicone oil" refers to an oil that contains at least one silicon atom, and in particular at least one Si-O group.
[0295] As non-volatile silicone oils, specific examples include polydimethylsiloxane containing at least 8 silicon atoms, polyalkylmethylsiloxane with alkyl chains containing 8 to 20 carbon atoms, and oils with the INCI name phenyl polytrimethylsiloxane.
[0296] The term "hydrocarbon-based oil" refers to oil containing hydrogen and carbon atoms.
[0297] For example, references may be made to hydrocarbons such as squalane, plant squalane, polybutene, hydrogenated polyisobutylene, hydrogenated polydecene, synthetic (poly)esters also known as "ester oils" and (poly)ethers, particularly (poly)esters of C6-C20 acids and C6-C20 alcohols, advantageously branched, such as isononyl isononanoate; vegetable oils; branched and / or unsaturated fatty acids; branched and / or unsaturated fatty alcohols, such as octyldodecyl alcohol; or mixtures thereof.
[0298] The term "ester oil" refers to mono-, di-, tri-, or tetra-ester oils. Ester oils are obtained by reacting mono-, di-, tri-, and more generally, polyols with mono-, di-, tri-, and more generally, polycarboxylic acids. The reagents can be linear or branched, saturated or unsaturated, aliphatic or aromatic, and may contain alkoxyl groups. Ester oils can be particularly hydroxylated.
[0299] In particular, non-volatile ester oils can contain 18 to 70 carbon atoms.
[0300] Non-volatile ester oils can be selected from: - Monoesters containing 18 to 40 carbon atoms, particularly monoesters of the formula R1COOR2, where R1 represents a linear or branched fatty acid residue containing 6 to 20 carbon atoms, and R2 represents a hydrocarbon chain containing 6 to 20 carbon atoms, particularly a branched chain, such as Purcellin oil (cetearyl caprylate), isononyl isononanoate, isodecanyl neopentanoate, C12-C15 alkyl benzoates, 2-ethylhexyl palmitate, and neopentanoic acid. Octyl dodecyl ester, 2-octyl dodecyl stearate, 2-octyl dodecyl erucic acid, isostearate, 2-octyl dodecyl benzoate, octanoic acid, capric acid or alkyl ricinoleate, isopropyl myristate, isopropyl palmitate, butyl stearate, hexyl laurate, 2-ethylhexyl palmitate, 2-hexyl decyl palmitate, 2-octyl decyl palmitate, 2-octyl dodecyl myristate, 2-diethylhexyl succinate; - Diesters containing 18 to 60 carbon atoms, especially 18 to 50 carbon atoms, such as diesters of dicarboxylic acids and monools, such as diisostearate malate; diesters of diols and monocarboxylic acids, such as neopentyl glycol diheptanoate or polyglycerol-2 diisostearate. - Triesters containing 35 to 70 carbon atoms, such as tricarboxylic acid triesters, like triisostearate citrate or tridecyl trimellitate; or triesters of diols and monocarboxylic acids, such as polyglycerol-2-triisostearate, for example, products available from Croda under the trade name Cithrol-PG-32-IS. - Tetraesters containing 35 to 70 carbon atoms, such as pentaerythritol tetraesters of monocarboxylic acids or tetraesters of polyglycerol, such as pentaerythritol tetranonanoate, pentaerythritol tetraisostearate, pentaerythritol tetraisononanoate, glycerol 2-tetrazoleate, polyglycerol-2-tetraisostearate or pentaerythritol 2-tetradecyl ... - Polyesters obtained by condensation of dimers and / or trimers of unsaturated fatty acids with diols, such as those described in patent application FR 0 853 634, such as polyesters of dilinoleic acid and 1,4-butanediol. - Diol dimers and mono- or dicarboxylic acid esters and polyesters, such as diol dimers and fatty acid esters, such as polyglycerol-2 isostearate / dimeric linoleate copolymers available from Kogyo Alcohol under the trade name Hailuscent ISDA-MB, and diol dimers and dicarboxylic acid dimer esters, particularly those obtained from dimers of unsaturated C8 to C34, especially C12 to C22, especially C16 to C20, and more particularly C18 fatty acids, such as esters of dilinoleic acid diacid and dilinoleic acid diol dimers, such as those sold by Honseki Ka Co., Ltd. under the trade names Lusplan DD-DA5® and DD-DA7®; - Fatty acid triglycerides (liquid at room temperature), especially fatty acids containing 7 to 40 carbon atoms, such as heptanoic acid or caprylic acid triglycerides or jojoba oil; saturated triglycerides, such as caprylic / capric acid triglycerides, triheptanoic acid triglycerides, tricaprylic acid triglycerides; C18-36 acid triglycerides (e.g., products sold by Stéarineries Dubois under index number DUB TGI 24); and unsaturated triglycerides (e.g., castor oil, olive oil, sea buckthorn seed oil, Pentacera macroloba seed oil); - or a mixture thereof.
[0301] The non-volatile oil used in this invention can be a gloss oil.
[0302] "Glossy oil" refers to an oil with a refractive index greater than 1.43, preferably greater than 1.45, and even more preferably greater than 1.50.
[0303] The refractive index was measured using an ABBE paralux ref 60-6400-9 refractometer.
[0304] Additional non-volatile oils can also be used to impart additional properties to the compositions of the present invention.
[0305] For example, the following can be added: diisostearate malate, or polyglycerol-3 diisostearate available from Croda under the trade name CithrolPG32IS, or pentaerythritol adipate / decanoate / caprylate / heptanoate available from Inolex under the trade name Lexfeel 700EX-LO MB, because they provide good pigment dispersion.
[0306] Other additional oils can be added to improve the sensory properties of the formula.
[0307] According to one embodiment, the non-volatile oil is selected from squalane, octyldodecyl alcohol, polyglycerol-2 triisostearate, polyglycerol-10 decaisostearate, pentaerythritol adipate / caprylate / heptanoate, dioctyl carbonate, octyldodecyl myristate, di-linoleic di-linoleate, polyglycerol-2 isostearate / di-linoleate, sorbitan sesquiisostearate, polyglycerol-3 diisostearate, isononyl isononanoate, meadowfoam seed oil, caprylic / capric triglyceride, sunflower oil, dipentaerythritol tetrahydroxystearate / isostearate, diisostearate malate, and jojoba oil.
[0308] Volatile oils According to an advantageous embodiment of the invention, the composition contains no (0%) or very little (up to 5% by weight relative to the total weight of the composition) volatile oils.
[0309] The term "volatile oil" refers to oils that can evaporate in less than an hour when in contact with skin at room temperature and atmospheric pressure.
[0310] Volatile oils are volatile cosmetic oils that are liquid at room temperature, especially those with a non-zero vapor pressure at room temperature and atmospheric pressure, particularly between 0.13 Pa and 40,000 Pa (0.001 to 300 mmHg), preferably between 1.3 Pa and 13,000 Pa (0.01 to 100 mmHg), and even more preferably between 1.3 Pa and 1300 Pa (0.01 to 1000 mmHg).
[0311] Volatile oils include volatile silicone oils and / or volatile hydrocarbon oils.
[0312] The volatile silicone oil optionally used in the compositions of the present invention is linear or cyclic, contains 2 to 7 silicon atoms, optionally contains 1 to 10 carbon atoms of alkyl or alkoxy groups, and has a viscosity of less than 5 cSt at room temperature.
[0313] Examples of volatile silicone oils include, in particular, hexamethylcyclotrisiloxane, octamethylcyclotetrasiloxane, decamethylcyclopentasiloxane, dodecylcyclohexasiloxane, cyclotetradimethylsiloxane, cyclopentadimethylsiloxane, cyclohexadimethylsiloxane, hexamethyldisiloxane, octamethyltrisiloxane, hexylheptamethyltrisiloxane, octylheptamethyltrisiloxane, decamethyltetrasiloxane, dodecylpentasiloxane, heptamethylhexyltrisiloxane, heptamethyloctyltrisiloxane, or mixtures thereof.
[0314] Regarding volatile hydrocarbon-based oils, more particular mention may be made of short-chain hydrocarbon-based oils and volatile straight-chain alkanes, such as those described in FR2933865, which are incorporated herein by reference.
[0315] Examples of short-chain hydrocarbon oils may be specifically mentioned as those selected from the group consisting of isododecane, isodecane, isohexadecane, dodecane, or mixtures thereof.
[0316] Examples of volatile straight-chain alkanes include those containing the following hydrocarbon chains: - C9-C17, C10-C14, such as mixtures of undecane and tridecane, are marketed by BASF Care Creations under the name Cetiol® Ultimate. - C15-19, for example, products sold by SEPPIC under the name Emogreen L15. - C12-14, for example, products sold by Biosynthis under the name Vegelight 1214LC. - C9-12 alkanes, such as products sold by Daito Chemical Industry Co., Ltd. under the name Makigreen D10.
[0317] Colorant Colorants may be selected in particular from water-soluble or fat-soluble dyes, pigments, pearlescent agents, lakes or mixtures thereof.
[0318] These colorants can optionally be surface-treated with hydrophobic agents, such as silanes, silicones, fatty acid soaps, and C. 9-15 Fluoroyl phosphates, acrylate / polydimethylsiloxane copolymers, C 9-15 Fluorophosphate / silicone blends, lecithin, carnauba wax, polyethylene, chitosan, and optionally acylated amino acids, such as lauroyl lysine, disodium stearoyl glutamate, and aluminoyl glutamate. Pigments can be mineral or organic, and natural or synthetic.
[0319] Examples of mineral pigments include, in particular, titanium dioxide, zinc oxide, iron, zinc or chromium oxides, manganese violet, ultramarine, ferrocyanide known as Prussian blue, as well as composite pigments and angle-dependent, pearlescent, interference, photochromic, or thermochromic pigments, but this list is not limited to these.
[0320] Examples of organic pigments that can be used in this invention include, in particular, carbon black, D&C type pigments, cochineal, barium, strontium, calcium or aluminum-based lakes, or diketopyrrolopyrrole (DPP) as described in EP-A-542 669, EP-A-787 730, EP-A-787 731 and WO-A-96 / 08537.
[0321] Pearlescent agents can be selected from those commonly found in cosmetic products, such as mica / titanium dioxide. As variations, they can be based on mica / silica / titanium dioxide, synthetic fluorophlogopite / titanium dioxide (Sunshine® from Maprecos), sodium calcium borosilicate / titanium dioxide (Reflecks® from Engelhard), or calcium aluminum borosilicate / silica / titanium dioxide (Ronastar® from Merck). Bismuth oxychloride may also be mentioned.
[0322] Advantageously, when the composition contains one or more pigments, the composition according to the invention also contains at least one dispersant, such as diisostearic acid malate.
[0323] The colorant content in the composition is from 0.1% to 15%, where the percentage is a weight percentage relative to the total weight of the composition.
[0324] filler These fillers are preferably colorless or white.
[0325] The particles that make them up can be porous or non-porous and have various shapes, especially plate-like, spherical or oblong, regardless of their crystallization form (e.g., plate-like, cubic, hexagonal, orthorhombic, etc.).
[0326] Specifically, the filler may be selected from cellulose, lauroyl lysine, boron nitride, silicone microbeads (e.g., those sold by Toshiba under the name Tospearl), precipitated calcium carbonate, hydroxyapatite, elastomeric polysiloxane particles, glass or ceramic microcapsules, zinc myristate, magnesium myristate, magnesium stearate, magnesium aluminum silicate (e.g., products sold by Fuji Chemical Industry under the trade name Neusilin ULF2), starch, clay, or mixtures thereof.
[0327] Starch, clay, or mixtures thereof may be mentioned in the fillers.
[0328] Starch can be selected from, for example, rice, cassava, potato, or corn starch. Rice starch is preferred, especially the INCI name: distarch phosphate, a product marketed by Agrina Starch under the name Rice PO4 Natural.
[0329] The clay can be natural or synthetic. It becomes lipophilic by treatment with alkylammonium salts such as C10 to C22 ammonium chloride, for example, distearyldimethylammonium chloride. It can be selected from bentonite, especially lithium montmorillonite and montmorillonite, bedesite, soapstone, chlorite, sepiolite, biotite, attapulgite, and vermiculite. Preferably, the clay is selected from lithium montmorillonite. As examples of lithium montmorillonite, references can be made to the product sold by Elementis Specialties under the name Bentone 38VCG (INCI name: distearyldimethylammonium montmorillonite) or the product sold by Elementis Specialties under the name Bentone Gel EUG V.
[0330] Additional additives In addition to the above-mentioned ingredients, the compositions according to the present invention may contain various ingredients, such as UV sunscreens, vegetable or synthetic butter, sweeteners, antioxidants, chelating agents, pH adjusters, preservatives, flavorings, vitamins, humectants, or mixtures thereof.
[0331] UV sunscreens may be selected from organic and inorganic sunscreens or mixtures thereof. As organic sunscreens, particularly noteworthy are dibenzoylmethane derivatives (including butyl methoxydibenzoylmethane), cinnamic acid derivatives (including ethylhexyl methoxycinnamate), and salicylates, p-aminobenzoic acid, β,β'-diphenylacrylate, benzophenone, benzyl camphor derivatives, phenylbenzimidazole, triazine, phenylbenzotriazole, and anthranilic acid derivatives. As inorganic sunscreens, particularly noteworthy are mineral oxide-based sunscreens, in the form of pigments or nano-pigments, whether or not coated, and especially those based on titanium dioxide or zinc oxide.
[0332] The compositions according to the invention may also contain one or more sweeteners, such as sorbitol, sucrose, xylitol, acesulfame K and sodium saccharin; antioxidants, such as alkylated or phosphorylated ascorbic acid esters, or even tocopherols and their esters; chelating agents, such as EDTA salts; pH adjusters; preservatives; flavorings; vitamins; humectants; or mixtures thereof.
[0333] Examples of such adjuvants are specifically mentioned in the CTFA dictionary (International Cosmetic Ingredient Dictionary and Handbook, 11th edition, 2006, published by the Cosmetic, Toiletries and Fragrance Association).
[0334] Preferably, the cosmetic composition according to the invention contains less than 3% by weight of mineral and / or synthetically derived additional solid fatty substances, particularly less than 1% by weight, and even more preferably, the composition does not contain the following: - Solid fatty substances selected from synthetic beeswax or mixtures thereof sold by Koster Keunen under the trade name Kester Wax K82H; polyethylene waxes, such as those sold by New Stage Technologies under the trade name Performalène 400 (P400) or by Jenny International under the trade name Jeenate 3H; mixtures of linear high molecular weight polyethylene and ethylene / propylene copolymers sold by Sasol under the trade name Lipwax® PZ80-20; synthetic waxes, such as those sold by Sasol under the trade name Sasol Wax C80; mixtures of synthetic waxes and plant waxes, such as synthetic waxes and carnauba waxes sold by Stonebis under the name Smart Wax 202. Copernica cerifera A mixture of synthetic waxes, candelilla wax, and carnauba wax, sold by Stonebees Corporation under the name Smart Wax 7743S. Copernica ceriferaMixtures of Fischer-Tropsch waxes, such as those sold by Cirebelle under the name Cirebelle 303, or mixtures thereof, lignite wax, ceresin, natural ceresin, microcrystalline wax, mineral paraffin; and - A paste-like fatty substance selected from liquid petrolatum (also known as Vaseline).
[0335] Pharmaceutical Composition According to another aspect, the present invention relates to a pharmaceutical composition comprising a mixture of straight-chain alkanes according to the present invention.
[0336] Uses of straight-chain alkane mixtures According to another aspect, the present invention relates to the use of straight-chain alkane mixtures according to the invention in the fields of cosmetics, pharmaceuticals, coatings, inks, varnishes, paper, adhesives, candles, plastics, rubber and / or food.
[0337] Specific terminal olefin mixture According to another aspect, the present invention relates to a terminal olefin mixture comprising the following: - 0.5% to 10%, preferably 1% to 10%, or even more preferably 1% to 5% of C16 terminal olefins; - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C18-terminated olefins; and - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C20 terminal olefins; The percentage is expressed in moles relative to the total molar weight of the terminal olefin mixture.
[0338] This mixture is particularly useful for preparing naturally derived waxes with physicochemical properties comparable to those of mineral paraffin, using the method according to the invention, especially for use in the lipstick industry.
[0339] The internal olefin mixture obtained from step ii) According to another aspect, the present invention relates to mixtures of olefins of natural origin, particularly of plant origin, which can be obtained by steps i) and ii) of the method according to the invention.
[0340] In some embodiments, the at least one linear terminal olefin used in step i) of the method is a mixture of C16, C18 and C20 linear terminal olefins.
[0341] In some embodiments, the mixture of C16, C18, and C20 straight-chain terminal olefins comprises the following: - 0.5% to 10%, preferably 1% to 10%, or even more preferably 1% to 5% of C16 terminal olefins; - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C18-terminated olefins; and - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C20 terminal olefins; The percentage is expressed in moles relative to the total molar weight of the terminal olefin mixture.
[0342] This mixture is particularly useful as a synthetic intermediate for preparing straight-chain alkane mixtures according to the method of the present invention.
[0343] Example Materials and methods Material The straight-chain alkane mixture was prepared from commercial products, such as: Ru-2 CAS: 373640-75-6 (M206) Ru-3 CAS: 1212008-99-5 (M711) The Ru1a / Ru1b catalyst was prepared according to Dalton Trans., 2014, 43, 7044.
[0344] method Gas chromatography (GC) analysis : Gas chromatography enables the identification of different components in a mixture that diffuse at varying rates based on their affinity for the mobile and stationary phases. Consequently, the products are separated into chromatograms. Quantification is possible using pre-prepared calibration curves for each separated compound. Samples are prepared in flasks at known concentrations and analyzed by gas chromatography (GC) according to the following methods: - Method 1 A Shimadzu GC-2014 instrument and an Agilent VF-5ht column with the following characteristics were used: 30 m × 0.25 mm × 0.10 µm, maximum temperature: 430 °C. A temperature gradient was used during the analysis. [Table 1] Analysis time: 68 min - Or according to "Method 2" (for the widest distribution). A Restek MXT-1HT SimDist column with the following characteristics was used: 5 m × 0.53 mm × 0.10 µm, maximum temperature: 450 °C. Samples were prepared at a known concentration (0.1 mg / mL). A temperature gradient was used during the analysis. [Table 2] Analysis time: 23 min Gas chromatography-mass spectrometry (GC / MS) analysis : This technique combines gas chromatography (explained above) and mass spectrometry, allowing the determination of the molecular weight of the analyzed compound based on its mass-to-charge ratio. Samples were prepared in vials and analyzed on a Shimadzu SH-Rxi-5ms column on a Shimadzu GC-2010 Plus instrument, characterized by 30 m × 0.25 mm × 0.25 µm and a maximum temperature of 330 °C. A temperature gradient was used during the analysis. [Table 3] Analysis time: 32 min Nuclear magnetic resonance (NMR) analysis : The synthesized molecules were characterized by nuclear magnetic resonance (NMR) spectroscopy. The NMR spectra were recorded on a Bruker ARX400 instrument. 1 H: 400 MHz 13 C: 101 MHz, 31 P: 162 MHz). Solvent: CDCl3.
[0345] DSC (Differential Scanning Calorimetry) Analysis : Synthetic waxes and formulated solid compositions (including lipsticks) were analyzed using a DSC 25 instrument from TA Instruments to accurately determine their melt profiles.
[0346] 100℃ Polymorphism Scheme (Temperature Gradient) : DSC is a thermal analysis technique that measures the difference in heat exchange between a reference material and the sample to be analyzed. It can determine: - The melting point of the sample, - The melting onset temperature should be as high as possible to limit the risk of oil separation and thermal instability. - 100% melt temperature, used to set the industrial process temperature and ensure complete melting of the crystals. - Enthalpy, which corresponds to the energy required to melt wax crystals. The goal is to achieve the highest possible enthalpy to maximize crystal yield and provide harder rods.
[0347] Solid aliphatic substances and more generally crystalline materials can sometimes exhibit what is known as polymorphism. Polymorphism refers to the possibility of forming different types of crystals depending on external conditions such as cooling rate or storage time. Therefore, these coexisting different types of crystals are characterized by different melting points, densities, plasticities, etc. For some waxes, the cooling rate affects the crystals formed. To ensure the stability and repeatability of industrial batches, waxes exhibiting this polymorphism must be avoided. Polymorphism can be predicted from DSC curves by subjecting samples to continuous cooling cycles at different rates.
[0348] All these parameters were evaluated using a differential scanning calorimeter (DSC 25, Discovery DSC Series, TA Instruments, France), connected to a computer using Trios software (TA Instruments, France), which was used to initiate measurements and analyze the obtained spectra. For each candidate, 11 ± 0.5 mg of wax was collected and placed in a standard crucible, sealed using a presser (Tzero Sample Press, TA Instruments, France). The procedure was based on the following scheme: a first heating to eliminate the thermal history of the starting material (5 °C / min from 15 °C to 120 °C), followed by slow cooling (2 °C / min from 120 °C to -5 °C), a second heating (5 °C / min from -5 °C to 120 °C), rapid cooling (25 °C / min from 120 °C to -5 °C), and then a final heating (5 °C / min from -5 °C to 120 °C). Comparison of the curves from the second and third heatings allowed for conclusions regarding the presence of polymorphism in each starting material. For all syntheses, two samples were prepared to ensure the reproducibility of the measurements.
[0349] Texture analyzer: Lipstick Hardness Study : The butter cut test allows for rapid evaluation of lipstick firmness, specifically by measuring the cutting resistance of the stick. This measurement is performed 24 hours after formulation using a texture analyzer (TAXTPlus, MicroStable Systems, UK) equipped with a 5 kg force sensor and its Butter Cutter A / BC probe (Swantech, MicroStable Systems, UK). It allows for the measurement of the maximum resistance of the stick when cutting butter filaments at a speed of 1.6 mm / s to a depth of 9 mm. To ensure reproducibility, the analysis was repeated on six sticks, and the relative difference between measurements must not exceed 10%, ideally 5%.
[0350] Example 1: Synthesis of a mixture of naturally derived straight-chain alkanes (melting point = 80°C) from a mixture of straight-chain terminal olefins.
[0351] The method according to the present invention comprises three steps: olefin metathesis - isomerization olefin metathesis - hydrogenation ([ Figure 1 It allows the preparation of alkane mixtures from terminal olefin mixtures.
[0352] Terminal olefins can be prepared according to known synthetic methods (see [...]). Figure 2 ]、[ Figure 3 ]).
[0353] Step 1: Olefin metathesis using a mixture of terminal olefins Cross-metathesis reactions of three plant-derived terminal olefins with 16, 18, and 20 carbon atoms, respectively, in the presence of a ruthenium catalyst, allowed the production of a mixture of internal olefins ranging from C30 to C38. Figure 4 ].
[0354] plan C 16 (0.01 equivalent, 786 mg), C 18 (0.495 equivalents, 43.74 g) and C 20 A mixture of (0.495 equivalents, 48.6 g) terminal olefins was placed in a double-necked flask equipped with a magnetic rod and a condenser and heated to 80 °C under vacuum. After 1 hour, the catalyst (Ru-1a / Ru-1b 3 / 7, 0.3 mol%, 953 mg) and distilled solvent (THF, 40 mL) were added under argon. The mixture was then stirred at 75 °C for two days. The reaction mixture was hydrolyzed with ethyl vinyl ether and then purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. Cold filtration with acetone was performed to remove the last trace amounts of catalyst, yielding the desired product as a white powder.
[0355] NMR 1 1H NMR analysis (solvent CDCl3) showed the presence of olefin protons from the terminal olefins, as well as the complete disappearance of terminal olefin protons. Gas chromatography analysis of the final product showed a mixture of olefins consisting of 30 to 38 carbons.
[0356] Step 2: Metathesis of isomerized olefins Metathesis of isomerized olefins in the presence of a pair of ruthenium catalysts [ Figure 5 This produces an internal olefin mixture. Gas chromatography analysis can determine the composition of this mixture, producing an internal olefin distribution containing 24 to 60 carbons (according to "Method 1"). Figure 6 ]).
[0357] plan A mixture of internal olefins (50 g) was introduced into a double-necked flask equipped with a magnetic stirrer and a condenser, and heated under vacuum at 80 °C for 1 hour. Then, under argon atmosphere, the catalyst (Ru-2, 0.5 mol%, 464 mg and Ru-3, 1 mol%, 817 mg), along with distilled solvent (THF, 41 mL) and methanol (4.1 mL), were added. The mixture was stirred at 75 °C for 15 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. Cold filtration with acetone was performed to remove any remaining trace catalyst, yielding the desired product as a white powder.
[0358] Phase 3: Hydrogenation Then, the hydrogenation of the previously obtained internal olefin mixture in the presence of palladium on carbon was studied according to "Method 1". Figure 7 []), and allows the production of alkane mixtures containing 24 to 60 carbons.
[0359] plan A mixture of internal olefins (48.1 g), catalyst (Pd / C, 1.9 g; 0.4 wt% Pd / substrate), and solvent (cyclohexane, 240 mL) were introduced into a round-bottom flask equipped with a magnetic stirrer. The reaction mixture was heated to 50 °C and purged three times under H2. The mixture was stirred at 50 °C under 1 bar of hydrogen for 16 hours. The reaction medium was filtered through a sintered funnel with hot cyclohexane and then concentrated on a rotary evaporator. Cold filtration with acetone was used to remove trace amounts of catalyst to give the desired product (45 g) as a white powder in 93% mass yield.
[0360] NMR The final mixture 1 1H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0361] GC The reaction mixture was analyzed by GC (using "Method 1"). Figure 8 The presence of a mixture of alkanes was confirmed, and the precise composition of the mixture was determined, showing a distribution of 24 to 60 carbon atoms. This mixture was named "Wax A".
[0362] DSC DSC thermogravimetric analysis showed that the melting point and enthalpy were very close to those of Lipwax® PZ80-20, at 79.6 °C vs. 80.6 °C and 226 J / g vs. 212 J / g, respectively. Furthermore, the “starting point” for determining the initial melting point of wax A was lower than that of Lipwax® PZ80-20 (55.2 °C vs. 63.5 °C), and the melting temperature (“ending point”) of the last alkane constituting the mixture was higher for wax A (90.7 °C vs. 89.9 °C), meaning that wax A has a wider alkane range than Lipwax® PZ80-20.
[0363] Example 2: Synthesis of a mixture of naturally occurring straight-chain alkanes from terminal straight-chain olefins (T° melt = 49°).
[0364] Starting with jojoba oil (Flora Esters®, sold by Floratech), ethylene hydrolysis can be performed without isomerization. Figure 9 The synthesized product, 1-decene, can then participate in sequential metathesis / isomerization metathesis / hydrogenation methods. Figure 10 This process yields a mixture of alkanes ranging from C17 to C44.
[0365] plan Decolorized jojoba oil (1 g) was placed in a vial equipped with a magnetic stir bar and a diaphragm. The oil was heated under vacuum at 180 °C for 2 h. Vacuum-argon purging was then performed. The catalyst (Ru-4, 1 mg / mL in dichloromethane, 120 µL, 0.01 mol%) was added in solution under argon. The diaphragm was quickly removed and the vial was placed in an autoclave. Ethylene purging (purity = 99.95%) was performed, and the mixture was stirred at 40 °C under 10 bar ethylene for 6 h. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the product was analyzed by GC using trimethoxybenzene as an internal standard. The conversion was 98%, and the product was predominantly 1-decene.
[0366] Decene (1 g; 7.13 mmol) was placed in a Schlenk tube equipped with a magnetic stir bar. Rapid vacuum-argon purging was performed, and the catalyst (Ru-1a / Ru-1b 3 / 7, 0.3 mol%, 19.4 mg) and distilled solvent (THF, 7 mL) were added under argon atmosphere. The mixture was then stirred at 75 °C for four days. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the solvent was removed under reduced pressure. The product was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The resulting product (554 mg) was a pale yellow liquid in 62% mass yield and was analyzed by GC and GC-MS.
[0367] A mixture of internal olefins (500 mg) was introduced into a double-necked flask equipped with a magnetic stirrer and a condenser, and heated under vacuum at 80 °C for 1 hour. Then, catalysts Ru-2 (9.2 mg; 0.5 mol%) and Ru-3 (16.3 mg; 1 mol%), along with distilled solvent (THF, 2.8 mL) and methanol (82 µL), were added under argon atmosphere. The mixture was stirred at 75 °C for 2 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst, yielding the desired product (476 mg) as a pale yellow paste, in 95% mass yield.
[0368] A mixture of internal olefins (350 mg) and catalyst (Pd / C, 14 mg; 0.4 wt% Pd / substrate) was placed in a microwave tube equipped with a magnetic stirrer and heated to 50 °C under vacuum. Solvent (cyclohexane, 1.75 mL) was added under argon. Hydrogen-vacuum purging (three times) was performed. The mixture was bubbled at 1 atm hydrogen for 30 seconds and then stirred at 50 °C under 1 atm hydrogen for 6 h. The crude mixture was purified by silica gel chromatography with hot cyclohexane. After removing the solvent under vacuum, cold filtration with acetone was performed to remove trace amounts of catalyst, yielding the desired product as a white powder in 59% mass yield. The product was analyzed by GC and... 1 HNMR analysis.
[0369] NMR The final mixture 1 1H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0370] GC The reaction mixture was analyzed by GC (using "Method 1"). Figure 11 The presence of a mixture exhibiting a Gaussian distribution, consisting of alkanes containing 17 to 44 carbons, was confirmed.
[0371] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 48.9 °C and 134.2 J / g, respectively. The starting point was obtained at 36.3 °C, and the ending point at 56.8 °C.
[0372] Example 3: Synthesis of a mixture of naturally derived straight-chain alkanes from a mixture of straight-chain terminal olefins (T° melt = 75°C).
[0373] From the terminal olefin mixture, an alkane mixture ranging from C22 to C54 can be obtained by sequential metathesis / isomerization metathesis / hydrogenation methods. The final product is uniquely characterized by a melting point of 75°C.
[0374] plan C 16 (0.01 equivalent, 11 mg), C 18 (0.495 equivalents, 625 mg), C 20 A mixture of (0.495 equivalents, 694 mg) terminal olefins and catalyst (Ru-1a, 32 mg) was placed in a Schlenk tube equipped with a magnetic stirrer. The mixture was heated to 80 °C under argon. Hydrochloric acid (3 mL) in ethyl acetate was added. The mixture was then stirred at 80 °C for 2 hours. A few milligrams of catalyst (30 mg) and hydrochloric acid (5 mL) in ethyl acetate were added, and the mixture was stirred at 80 °C for 2 hours. A few milligrams of catalyst (30 mg) and hydrochloric acid (2 mL) in ethyl acetate were added again, and the mixture was stirred at 80 °C for 2 hours. The catalyst was neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture. The product was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The resulting product (811 mg) was a white solid in 61% mass yield and was purified by GC and... 1 HNMR analysis.
[0375] A mixture of internal olefins (300 mg) and catalyst (Ru-2, 0.5 mol%, 3 mg) was introduced into a two-necked flask equipped with a magnetic stirrer and a condenser, and heated at 80 °C for 20 min under vacuum. Then, under argon atmosphere, distilled solvent (THF, 0.6 mL) and methanol (100 µL) were added. The mixture was stirred overnight at 80 °C. The catalyst was neutralized with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (300 mg) was obtained as a white solid in 99% mass yield and analyzed by GC.
[0376] A mixture of internal olefins (260 mg) and a catalyst (1.2 mL; 50 wt% Raney nickel) were placed in an autoclave equipped with a magnetic stirrer and heated to 110 °C. The autoclave was purged with hydrogen (three times). The autoclave was then purged with 25 bar of hydrogen. The mixture was stirred overnight at 110 °C under 25 bar of hydrogen. The crude mixture was purified by silica gel chromatography with hot cyclohexane. After solvent removal under vacuum, the desired product (260 mg) was obtained as a white powder in 99% mass yield. The product was obtained by… 1 HNMR, GC and DSC analysis.
[0377] NMR The final mixture 11H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0378] GC GC analysis of the reaction mixture [ Figure 12 The presence of a mixture of alkanes containing 22 to 54 carbon atoms has been confirmed.
[0379] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 75.2 °C and 214 J / g, respectively. The starting point was obtained at 66.9 °C, and the ending point at 79.2 °C.
[0380] Example 4: Synthesis of a mixture of naturally derived straight-chain alkanes from a mixture of C6, C7 and C8 straight-chain terminal olefins (T° melt = 32°C).
[0381] From the terminal olefin mixture, a mixture of alkanes ranging from C12 to C47 can be obtained via sequential metathesis / isomerization metathesis / hydrogenation. The final product has a melting point of 32°C. Figure 13 ].
[0382] plan The catalyst (Ru-1a, 27 mg) was placed in a double-necked flask equipped with a magnetic stirrer and a condenser. C6 (0.33 equivalents, 737 µL), C7 (0.33 equivalents, 836 µL), and C8 (0.33 equivalents, 933 µL) terminal olefins were added under argon atmosphere. The mixture was heated to 75 °C. Hydrochloric acid (2 mL) in ethyl acetate was added. The mixture was then stirred at 75 °C for 24 hours. A few milligrams of catalyst (14 mg) and hydrochloric acid (1 mL) in ethyl acetate were added, and the mixture was stirred at 75 °C for 20 hours. A few milligrams of catalyst (14 mg) and hydrochloric acid (1 mL) in ethyl acetate were added again, and the mixture was stirred at 75 °C for 6 hours. The catalyst was neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture. The product was purified by silica gel chromatography with pentane to remove residual catalyst. The resulting product (1.1 g) was a pale yellow liquid in 63% mass yield and was purified by GC and... 1 H NMR analysis.
[0383] A mixture of internal olefins (550 mg) was introduced into a two-necked flask equipped with a magnetic stirrer and a condenser, and heated at 75 °C for 10 min under vacuum. Then, catalysts Ru-2 (42 mg; 0.5 mol%) and Ru-3 (73 mg; 1 mol%), along with distilled solvent (THF, 9 mL) and methanol (200 µL), were added under argon atmosphere. The mixture was stirred at 75 °C for 2 h. The catalyst was neutralized with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (404 mg) was obtained as a pale yellow paste in 74% mass yield and analyzed by GC.
[0384] A mixture of internal olefins (300 mg) and catalyst (Pd / C, 12 mg; 0.4 wt% Pd / substrate) were placed in a microwave tube equipped with a magnetic stirrer and heated to 50 °C under vacuum. Solvent (cyclohexane, 1.5 mL) was added under argon. Hydrogen-vacuum purging (three times) was performed. The mixture was bubbled at 1 atm hydrogen for 30 seconds and then stirred at 50 °C under 1 atm hydrogen for 16 h. The crude mixture was purified by silica gel chromatography with hot cyclohexane. The product (278 mg) was obtained as a white paste in 93% mass yield. The product was obtained by… 1 HNMR, GC and DSC analysis.
[0385] NMR The final mixture 1 1H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0386] GC The reaction mixture was analyzed by GC (using "Method 1"). Figure 13 The presence of a mixture of alkanes containing 12 to 47 carbon atoms has been confirmed.
[0387] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 32 °C and 195.9 J / g, respectively. The termination point was obtained at 56.3 °C.
[0388] Example 5 - Synthesis of a naturally sourced straight-chain alkane mixture from a mixture of C8, C9 and C10 straight-chain terminal olefins (T° melt = 37.2°C) From the terminal olefin mixture, a mixture of alkanes ranging from C11 to C50 can be obtained via sequential metathesis / isomerization metathesis / hydrogenation. The final product has a melting point of 37.2 °C. Figure 14 ] plan The catalyst (Ru-1a, 20 mg) was placed in a double-necked flask equipped with a magnetic stirrer and a condenser. C8 (0.33 equivalents, 700 µL), C9 (0.33 equivalents, 771 µL), and C were added under argon atmosphere. 10 (0.33 equivalents, 844 µL) terminal olefin. The mixture was heated to 75 °C. Hydrochloric acid (1 mL) in ethyl acetate was added. The mixture was then stirred at 75 °C for 15 hours. A few milligrams of catalyst (10 mg) and hydrochloric acid (1 mL) in ethyl acetate were added, and the mixture was stirred at 75 °C for 10 hours. A few milligrams of catalyst (10 mg) and hydrochloric acid (1 mL) in ethyl acetate were added again, and the mixture was stirred at 75 °C for 15 hours. The catalyst was neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture. The product was purified by silica gel chromatography with pentane to remove residual catalyst. The resulting product (1.36 g) was a pale yellow liquid in 81% mass yield, and was purified by GC and... 1 HNMR analysis.
[0389] A mixture of internal olefins (679 mg) was introduced into a two-necked flask equipped with a magnetic stirrer and a condenser, and heated at 75 °C for 10 min under vacuum. Then, catalysts Ru-2 (31 mg; 0.5 mol%) and Ru-3 (55 mg; 1 mol%), along with distilled solvent (THF, 7 mL) and methanol (200 µL), were added under argon atmosphere. The mixture was stirred at 75 °C for 2 h. The catalyst was neutralized with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (600 mg) was obtained as a pale yellow paste in 88% mass yield and analyzed by GC.
[0390] A mixture of internal olefins (450 mg) and catalyst (Pd / C, 18 mg; 0.4 wt% Pd / substrate) were placed in a microwave tube equipped with a magnetic stirrer and heated to 50 °C under vacuum. Solvent (cyclohexane, 2.25 mL) was added under argon. Hydrogen-vacuum purging (three times) was performed. The mixture was bubbled at 1 atm hydrogen for 30 seconds and then stirred at 50 °C under 1 atm hydrogen for 16 h. The crude mixture was purified by silica gel chromatography with hot cyclohexane. The product (438 mg) was obtained as a white paste in 97% mass yield. The product was obtained by… 1 HNMR, GC and DSC analysis.
[0391] NMR The final mixture 1 1H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0392] GC The reaction mixture was analyzed by GC (according to "Method 1"). Figure 14 The presence of a mixture of alkanes containing 11 to 50 carbon atoms has been confirmed.
[0393] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 37.2 °C and 217 J / g, respectively. The termination point was obtained at 63.6 °C.
[0394] Example 6: Synthesis of a mixture of naturally derived straight-chain alkanes from a mixture of C10, C12 and C14 straight-chain terminal olefins (T° melt = 58.3°C).
[0395] From the terminal olefin mixture, a mixture of alkanes ranging from C11 to C54 can be obtained via sequential metathesis / isomerization metathesis / hydrogenation. The final product has a melting point of 57°C. Figure 15 ] plan The catalyst (Ru-1a, 19 mg) was placed in a double-necked flask equipped with a magnetic stirrer and a condenser. C was added under argon atmosphere. 10 (0.33 equivalent, 810 µL), C 12 (0.33 equivalent, 950 µL) and C 14 (0.33 equivalents, 1085 µL) terminal olefin. The mixture was heated to 75 °C. Hydrochloric acid (1 mL) in ethyl acetate was added. The mixture was then stirred at 75 °C for 15 hours. A few milligrams of catalyst (10 mg) and hydrochloric acid (1 mL) in ethyl acetate were added, and the mixture was stirred at 75 °C for 10 hours. A few milligrams of catalyst (10 mg) and hydrochloric acid (1 mL) in ethyl acetate were added again, and the mixture was stirred at 75 °C for 15 hours. The catalyst was neutralized, particularly by adding an alkyl vinyl ether to the reaction mixture. The product was purified by silica gel chromatography with pentane to remove residual catalyst. The resulting product (2.03 g) was a pale yellow liquid with a mass yield of 94%, and was purified by GC and... 1 HNMR analysis.
[0396] A mixture of internal olefins (1.01 g) was introduced into a double-necked flask equipped with a magnetic stirrer and a condenser, and heated at 75 °C for 10 min under vacuum. Then, catalysts Ru-2 (30 mg; 0.5 mol%) and Ru-3 (53 mg; 1 mol%), along with distilled solvent (THF, 6.5 mL) and methanol (200 µL), were added under argon atmosphere. The mixture was stirred at 75 °C for 2 h. The catalyst was neutralized with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (963 mg) was obtained as a pale yellow paste in 95% mass yield and analyzed by GC.
[0397] A mixture of internal olefins (430 mg) and catalyst (Pd / C, 17 mg; 0.4 wt% Pd / substrate) were placed in a microwave tube equipped with a magnetic stirrer and heated to 50 °C under vacuum. Solvent (cyclohexane, 2.15 mL) was added under argon. Vacuum-hydrogen purging (three times) was performed. The mixture was bubbled at 1 atm hydrogen for 30 seconds and then stirred at 50 °C under 1 atm hydrogen for 16 h. The crude mixture was purified by silica gel chromatography with hot cyclohexane. The product (410 mg) was obtained as a white paste in 95% mass yield. The product was obtained by... 1 HNMR, GC and DSC analysis.
[0398] NMR The final mixture 1 1H NMR analysis (CDCl3) showed no olefin protons at approximately δ = 5.4 ppm, confirming the presence of a mixture of alkanes.
[0399] GC The reaction mixture was analyzed by GC (using "Method 1"). Figure 15 The presence of a mixture of alkanes containing 11 to 54 carbon atoms has been confirmed.
[0400] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 58.3 °C and 201.7 J / g, respectively. The termination point was obtained at 72 °C.
[0401] Example 7: Lipstick ingredients plan The lipstick formulation in Table 4 was prepared as follows: All raw materials constituting the white substance, including the wax with a melting point of 80°C obtained according to Example 1, were melted at 90°C with stirring at approximately 250 rpm. When the mixture was homogeneous and clear, the pre-ground pigment was incorporated into Lexfeel 700. The stirring was increased to 350 rpm for 10 minutes, then reduced to 250 rpm for 5 minutes. The pearlescent agent was incorporated into the mixture. Stirring was continued for another 5 minutes. The antioxidant and fragrance (if present) were added, and stirring was continued for 5 minutes. The resulting mixture was poured into molds at 85°C.
[0402] Keep the mold at -20°C for 10 minutes, and then demold the product.
[0403] Stability tests were conducted on the lipsticks. Different lipstick sticks were incubated at different temperatures (4°C, 20°C, 40°C, and 45°C). The lipsticks were then observed at D+1, D+15, D+30, and D+60. The lipsticks formulated with the wax obtained according to the method described in Example 1 maintained their good durability, smoothness, and shine throughout the incubation period.
[0404] Hardness tests (butter-cutting tests) were performed on lipstick formulations made with Lipwax® PZ80-20 and waxes obtained according to the method described in Example 1. The results of these rheological tests were excellent because the measured hardness of the lipsticks made with the waxes obtained according to the method described in Example 1 was similar to that of the lipsticks made with Lipwax® PZ80-20 (160 g and 150 g, respectively).
[0405] Oil separation was also tested. Oil separation is a type of sweating phenomenon that results in the accumulation of oily deposits, droplets, or oil spots on the surface of anhydrous products. For this test, four lipsticks were placed at different temperatures (27°C, 30°C, 35°C, and 45°C) and examined after 1 h, 4 h, and 24 h to determine if any sweating was visible. No oil separation was observed in the lipstick formulated with the wax obtained according to the method described in Example 1, nor was any oil separation observed in the lipstick formulated with Lipwax® PZ80-20.
[0406] Finally, DSC analysis allowed for comparison of lipsticks containing Lipwax® PZ80-20 with waxes obtained according to the method described in Example 1. According to the thermal analysis graphs, the melting points of these lipsticks were very close (73°C for wax A and 73.7°C for Lipwax® PZ80-20). The onset points (33.5°C vs. 33°C), end points (92.5°C vs. 91.2°C), and enthalpy (25.25 J / g vs. 25.19 J / g) were also comparable.
[0407] [Table 4] Achieving lipstick with sufficient stability and hardness: The stick is rigid and strong enough not to break during application, thus being compatible with stick or other solid forms of packaging and with application to the surface to be made up by friction; the stick is also characterized by ease of application, such as good slip properties, good deposition upon first application, and a comfortable texture.
[0408] Example 8: Aromatic Preparations The formulations shown in Table 5 were prepared as follows: Weigh all raw materials except for cellulose powder, sorbitan sesquiisostearate, and flavoring. Heat the raw materials to 70°C with stirring. When the mixture is completely melted and clear, add cellulose, followed by sorbitan sesquiisostearate, while continuing to stir. Reduce the temperature to 65°C with continued stirring. At 65°C, add the flavoring. Homogenize the resulting mixture and pour it into a container at 65°C.
[0409] [Table 5] A solid aromatic formulation with sufficient stability and hardness is obtained: the composition is sufficiently rigid and robust, does not leak over time and has no surface inhomogeneity, and is therefore compatible with packaging in solid form by pouring into a vessel and with application to the surface to be aromatic by friction; the composition is also characterized by ease of application, such as good slip properties, good deposition upon first application and a comfortable texture.
[0410] Example 9: Lip Gloss Formula The formulation in Table 6 was prepared as follows: Weigh a white substance consisting of wax with a melting point of 80°C obtained according to Example 1, Cithrol PG 32IS, isononyl isononanoate, dextrin palmitate, and sucrose isobutyrate acetate, and heat to 98°C with stirring at 150 rpm. After complete melting, reduce the temperature to 95°C. Weigh the pearlescent agent and add it with stirring at 250 rpm. Reduce the stirring to 150 rpm to degas. Weigh and add the antioxidant. Reduce the temperature to 90°C (±2°C). Discharge the material at 90°C and pour it into a container. After standing at room temperature for 10 minutes, place the container at -19°C for 10 minutes.
[0411] [Table 6] The resulting solid lip gloss, poured into a container, possesses sufficient stability and hardness: the composition is sufficiently rigid and robust to prevent seepage and surface unevenness over time, and is therefore compatible with packaging in solid container form and with application to the surface to be coated by friction; the composition is also characterized by ease of application, such as good slip properties, good deposition upon first application, and a comfortable texture.
[0412] Example 10: Lip Balm Ingredients The formulation in Table 7 was prepared as follows: Weigh all ingredients of the formulation: S-Face, Eutanol G, Super SterolEsters, Bentone gel, wax with a melting point of 80°C obtained according to Example 1, paste with a melting point of 37°C obtained according to Example 5, squalane, Salacos 43V, and shea butter. Do not incorporate pearlescent agents, pigments and their dispersion oils, surfactants, fragrances, or antioxidants. Heat the mixture to 90°C with stirring at 250 rpm. Once completely melted, weigh and add the pigments that have been pre-ground in their dispersion oils. Mix the resulting mixture with stirring at 250 rpm for 10 minutes. Incorporate the pearlescent agents with stirring at 250 rpm. Reduce stirring to 150 rpm to degas. Weigh and add the antioxidants, surfactants, and fragrances. Mix at 150 rpm for 5 minutes. Pour into molds at 90°C. After standing at room temperature for 10 minutes, smooth the molds and then place them at -19°C for 10 minutes. After leaving the product at room temperature for 2 minutes, demold it.
[0413] [Table 7] The resulting lip balm stick possesses sufficient stability and rigidity: the stick is rigid and strong enough not to break upon application, not to bleed over time, not to exhibit any surface unevenness, and therefore compatible with stick-shaped packaging and application to the surface to be made up or protected by friction; the stability tests conducted are the same as those described in Example 7. The stick also features ease of application, such as good slipperiness, good deposition upon first application, and a comfortable texture.
[0414] Example 11: Lipstick ingredients The formulation shown in Table 8 was prepared as follows: All raw materials constituting the white substance, including the wax with a melting point of 80°C obtained according to Example 1 and the paste with a melting point of 32°C obtained according to Example 4, were melted by stirring at approximately 250 rpm at 90°C. When the mixture was homogeneous and clear, the pigment, pre-ground in Cithrol PG32IS, was added. The stirring was increased to 350 rpm for 10 minutes, then reduced to 250 rpm for 5 minutes. The pearlescent agent and surfactant were added to the mixture. Mixing was continued for 5 minutes. The antioxidant and fragrance were added, and stirring was continued for 5 minutes. The product was poured into molds at 85°C.
[0415] [Table 8] The resulting lipstick possesses sufficient stability and rigidity: the stick is rigid and strong enough not to break upon application, not to bleed over time, not to exhibit surface unevenness, and therefore compatible with the stick-shaped packaging and with application to the surface to be coated via friction; the stability tests conducted are the same as those described in Example 7. The stick also features ease of application, such as good slipperiness, good deposition upon first application, and a comfortable texture.
[0416] Example 12: Skin care product formulation: nourishing cream The formulation in Table 9 was prepared as follows: Weigh the fatty phase: Salacos 168EV, Salacos 222, Indopol H-100, meadowfoam seed oil, jojoba oil, Floraester, shea butter, Nomcort HK-G, wax with a melting point of 49°C according to the present invention (wax of Example 2), camellia oil, rice wax, Span 120, and starch, and heat at 90°C for about 30 minutes with stirring at 250 rpm. Once the fatty phase is homogeneous, add cellulose powder and Lipex omega, and increase the stirring to 350 rpm for 5 minutes, then adjust to 250 rpm for 5 minutes. Add glycerin and camellia extract, then reduce the stirring to 150 rpm for 10 minutes to avoid bubbling. Add antioxidants and fragrance, and continue stirring for 5 minutes. Discharge the product at 90°C or pour it into a container at 80°C, place at room temperature (RT) for 7 minutes, and then at -19°C for 10 minutes.
[0417] [Table 9] The resulting skin care cream, poured into a jar, possesses sufficient stability and hardness: the poured skin care cream is rigid and firm enough not to seep out over time, not to show surface unevenness, and is therefore compatible with packaging in solid jar form and with application to the surface to be nourished by friction; the cream is also characterized by ease of application, such as good slipperiness, good deposition upon first application, and a comfortable texture.
[0418] Example 13: Mascara formulation The formulation shown in Table 10 was prepared as follows: All fatty phase raw materials were stirred and melted at 90°C: palm stearic acid, wax with a melting point of 58°C according to the present invention (wax of Example 6), beeswax, carnauba wax, and PVP hexadecene copolymer. When completely melted and homogeneous, iron oxide was added, and the mixture was milled for 30 minutes using a deflocculator. Water, polyol, preservative, triethanolamine, and AMPD were heated to 85°C. The gel was dispersed. An emulsion was prepared by pouring the colored fatty phase into the aqueous phase. Homogenization was carried out for 20 minutes. Cellulose beads were added. The resulting mixture was cooled to 50°C and an antioxidant was added. The mixture was discharged at 30°C.
[0419] [Table 10] A mascara with sufficient stability and rheological properties is obtained: the mascara composition is compatible with the packaging in the bottle and with application to eyelashes or eyebrows with a brush; the composition is also characterized by its ease of application, such as good adhesion, good deposition and a texture that gives eyelashes volume, which is similar to the volume obtained by using a mascara whose formulation is identical to that of the composition in all respects except that the wax in Example 6 is replaced with paraffin.
[0420] Example 14: Synthesis of a naturally sourced straight-chain alkane mixture from a mixture of straight-chain terminal olefins derived from jojoba oil (T° melt = 68.5°C).
[0421] From jojoba oil, a mixture of alkanes ranging from C21 to C51 can be obtained through a sequential isomerization / ethyleneolysis / metathesis / isomeric metathesis / hydrogenation process. The final product is uniquely characterized by a melting point of 68.5°C.
[0422] plan Decolorized jojoba oil (4.7 g), pre-treated under vacuum at 150 °C for 2 hours, Fe(CO)₅ (600 µL, 50 mol%), and solvent (hexane, 89 mL) were placed in a round-bottom flask equipped with a magnetic stirrer. The mixture was stirred at 50 °C under UV radiation (2 lamps, λ = 365 nm) for 24 hours under an argon flow. After returning to room temperature, pyridine (7.2 mL, 20 equivalents / Fe(CO)₅) was added, and the mixture was stirred for 10 minutes. The solvent was removed by rotary evaporation, and the reaction mixture was purified by silica gel chromatography with hot ethyl acetate. The desired product (4.2 g) was obtained as an orange paste.
[0423] Isomerized jojoba oil (4.2 g) was dried in a vial equipped with a magnetic stirrer under vacuum at 40 °C for 1 hour. Then, catalyst (Ru-4, 0.5 mol%, 25.3 mg) dissolved in a minimal solvent (dichloromethane, 1.5 mL) was added under argon. The vial was placed in an autoclave and purged with ethylene. The mixture was stirred at 40 °C under 20 bar ethylene for 16 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (1.4 g) was obtained as a pale yellow liquid after vacuum distillation at 120 °C.
[0424] A mixture of terminal olefins (1.4 g) was placed in a double-necked flask equipped with a magnetic stirrer and a condenser and heated to 80 °C under vacuum. After 1 hour, the catalyst (Ru-1a / Ru-1b 3 / 7, 5.1 mg) and distilled solvent (THF, 500 µL) were added under argon atmosphere. The mixture was then stirred at 75 °C for 3 hours. A few milligrams of catalyst (5.1 mg) diluted in the solvent (500 µL) were added, and the mixture was stirred at 75 °C for 3 hours. A few milligrams of catalyst (15.4 mg) diluted in the solvent (1 mL) were added, and the mixture was stirred at 75 °C for 16 hours. A few milligrams of catalyst (25 mg) diluted in the solvent (1.3 mL) were added again, and the mixture was stirred at 75 °C for 8 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether and then purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The product was then recrystallized from acetone and dried under vacuum at 200 °C. The desired product (425 mg) was obtained as a colorless paste.
[0425] A mixture of internal olefins (425 mg) was introduced into a double-necked flask equipped with a magnetic stirrer and a condenser, and heated under vacuum at 75 °C for 1 hour. Then, under argon atmosphere, the catalyst (Ru-2, 0.5 mol%, 4.3 mg and Ru-3, 1 mol%, 7.6 mg), along with distilled solvent (THF, 926 µL) and methanol (38 µL), were added. The mixture was stirred at 75 °C for 2 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (400 mg) was obtained as a colorless paste.
[0426] A mixture of internal olefins (390 mg), catalyst (Pd / C, 15.6 mg; 0.4 wt% Pd / substrate), and solvent (cyclohexane, 2 mL) were introduced into a round-bottom flask equipped with a magnetic stirrer. The reaction mixture was heated to 60 °C and purged four times under H2. The mixture was stirred at 65 °C under 1 bar of hydrogen for 16 h. The catalyst (Pd / C, 7.8 mg; 0.4 wt% Pd / substrate) and solvent (cyclohexane, 2 mL) were added, and the mixture was stirred at 75 °C for 16 h to achieve complete conversion. The crude mixture was purified by silica gel chromatography with hot cyclohexane. Filtration with acetone at room temperature was used to remove trace amounts of catalyst to give the desired product (313 mg) as a white powder in 80% mass yield.
[0427] GC Analysis of the reaction mixture by GC (“Method 2”) Figure 18 The presence of a mixture exhibiting a Gaussian distribution, consisting of alkanes containing 21 to 51 carbons, was confirmed.
[0428] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 68.5 °C and 232 J / g, respectively. The starting point was obtained at 56.8 °C, and the ending point at 75.1 °C.
[0429] Example 15: Synthesis of a naturally sourced straight-chain alkane mixture from a mixture of straight-chain terminal olefins derived from methyl erucic acid (T° melt = 74°C).
[0430] From methyl erucic acid, a mixture of alkanes ranging from C15 to C68 can be obtained through a sequential isomerization / ethyleneolysis / metathesis / isomeric metathesis / hydrogenation process. The final product is uniquely characterized by a melting point of 74°C.
[0431] plan Methyl erucic acid (5.2 g), iron pentacarbonyl Fe(CO)5 (200 µL, 10 mol%), and solvent (hexane, 400 mL) were placed in a round-bottom flask equipped with a magnetic stirrer. The mixture was stirred at 50 °C under UV radiation (2 lamps, λ = 365 nm) for 1 h under an argon atmosphere. After returning to room temperature, pyridine (2.38 mL, 20 equivalents / Fe(CO)5) was added, and the mixture was stirred for 10 min. The solvent was removed by rotary evaporation, and the reaction mixture was purified by silica gel chromatography with hot ethyl acetate. The product (5.17 g) was again placed in a round-bottom flask equipped with a magnetic stirrer with iron pentacarbonyl Fe(CO)5 (198 µL, 10 mol%) and solvent (hexane, 396 mL). The mixture was stirred at 50 °C under UV radiation (2 lamps, λ = 365 nm) for 6 h under an argon atmosphere. After returning to room temperature, pyridine (2.37 mL, 20 equivalents / Fe(CO)5) was added and the mixture was stirred for 10 minutes. The solvent was removed by rotary evaporation, and the reaction mixture was purified by silica gel chromatography with hot ethyl acetate. The desired product (5.17 g) was obtained as an orange paste.
[0432] Isomerized methyl erucic acid (5.17 g) was treated in a vial equipped with a magnetic stirrer under vacuum at 40 °C for 1 hour. Then, the catalyst (Ru-4, 0.3 mol%, 28.2 mg) dissolved in a minimal solvent (dichloromethane, 1.5 mL) was added under argon. The vial was placed in an autoclave and purged with ethylene. The mixture was stirred at 40 °C under 20 bar ethylene for 16 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. The desired product (1.1 g) was obtained as a pale yellow liquid.
[0433] A mixture of terminal olefins (1 g) was placed in a double-necked flask equipped with a magnetic stirrer and a condenser and heated to 75 °C under vacuum. After 1 hour, the catalyst (Ru-1a / Ru-1b 3 / 7, 12.6 mg) and distilled solvent (THF, 1.2 mL) were added under argon atmosphere. The mixture was then stirred at 75 °C for 40 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether and then purified by silica gel chromatography with hot cyclohexane to remove residual catalyst. A few milligrams of catalyst (8.4 mg) diluted in the solvent (1.2 mL) were added, and the mixture was stirred at 75 °C for 16 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether and then purified by silica gel chromatography with hot cyclohexane. The desired product (800 mg) was obtained as a pale yellow paste.
[0434] A mixture of internal olefins (800 mg) was introduced into a double-necked flask equipped with a magnetic stirrer and a condenser, and heated under vacuum at 75 °C for 1 hour. Then, under argon, a catalyst (Ru-2, 0.5 mol%, 10 mg and Ru-3, 1 mol%, 17.5 mg), a distillation solvent (THF, 2.1 mL), and methanol (86 µL) were added. The mixture was stirred at 75 °C for 2 hours. The reaction mixture was hydrolyzed with ethyl vinyl ether, and the crude mixture was purified by silica gel chromatography with hot cyclohexane. The desired product (700 mg) was obtained as a colorless paste.
[0435] A mixture of internal olefins (670 mg), catalyst (Pd / C, 27 mg; 0.4 wt% Pd / substrate), and solvent (cyclohexane, 3.4 mL) were introduced into a round-bottom flask equipped with a magnetic stirrer. The reaction mixture was heated to 60 °C and purged four times under H2. The mixture was stirred at 60 °C under 1 bar of hydrogen for 16 hours. The crude mixture was purified by silica gel chromatography with hot cyclohexane. Cold filtration with acetone was used to remove trace amounts of catalyst to give the desired product (543 mg) as a white powder in 81% mass yield.
[0436] GC Analysis of the reaction mixture by GC (“Method 2”) Figure 19 The presence of a mixture exhibiting a Gaussian distribution, consisting of alkanes containing 15 to 68 carbons, was confirmed.
[0437] DSC Thermogravimetric analysis (DSC) showed that the melting point and enthalpy were 74 °C and 228.6 J / g, respectively. The starting point was obtained at 32 °C, and the ending point at 86.4 °C.
[0438] Table 11 summarizes the DSC curve results for Examples 1 to 3, 14 and 15 above: [Table 11] Example 16: Comparative Example It reproduces the description in Example 4 of patent application WO 2021 / 183 330 A1 and [ Figure 20 [Illustrative display method]
[0439] GC GC analysis of the reaction mixture ([ Figure 21 The results show that the straight-chain alkane distribution obtained in this way is not characterized by a Gaussian distribution.
[0440] Furthermore, the smallest alkanes have 28 carbon atoms, while the largest have 34. Therefore, this distribution has a very narrow span of 6 carbon atoms.
[0441] Binary formulations To determine whether the straight-chain alkane mixture described in patent application WO 2021 / 183 330 A1 provides a wax that reproduces all the properties of synthetic waxes, the following tests were performed.
[0442] A mixture of straight-chain alkanes with a very narrow span (as described in patent application WO 2021 / 183 330 A1) is formulated into a cosmetic composition.
[0443] The mixture contains straight-chain alkane C. 36 H 74 C 38 H 78 and C 40 H 82 The ratio is 1:1:1.
[0444] The C36 / C38 / C40 mixture prepared in this way is used to prepare binary formulations containing 30% wax and 70% oil.
[0445] The visual analysis results of the binary formulation prepared in this way are summarized in Table 12 below: [Table 12] Binary formulations using a C36 / C38 / C40 mixture exhibit poor gelation and / or uneven surface crystallization, unlike binary formulations using the commercially available synthetic wax Lipwax® PZ80-20 sold by Safic Alcan.
[0446] The same C36 / C38 / C40 alkane mixture prepared in this way was used to prepare a lipstick containing 12% wax. Unlike lipsticks using Lipwax® PZ80-20, the lipstick stick prepared in this way could not be demolded, demonstrating that prior art alkane mixtures cannot provide lipsticks with the desired properties.
Claims
1. A method for preparing a mixture of straight-chain alkanes of natural origin, preferably plant origin, comprising the following steps: i. Metathesis of at least one straight-chain terminal olefin comprising 5 to 24 carbon atoms in the presence of a non-isomerizing olefin metathesis catalyst, wherein the straight-chain terminal olefin is derived from at least one natural, preferably plant-derived, fatty acid or fatty acid ester, thereby obtaining a first internal olefin mixture (I). ii. The internal olefin mixture (I) obtained in step i) is subjected to isomerization metathesis in the presence of a catalyst or a mixture of catalysts to obtain a second internal olefin mixture (II), and iii. The mixture of inner olefins (II) is hydrogenated in the presence of a catalyst to obtain a mixture of straight-chain alkanes of natural origin (III).
2. The method according to claim 1, wherein the non-isomeric olefin metathesis catalyst in step i) is selected from transition metal complexes, particularly alkylene complexes of transition metals, especially alkylene complexes of ruthenium.
3. The method according to claim 2, wherein the non-isomeric olefin metathesis catalyst is selected from Ru-1a, Ru-1b, or a mixture thereof. [Chemical Formula 1] [Chemical Formula 2] 4. The method according to any one of the preceding claims, wherein the catalyst or mixture of catalysts used in step ii) is a transition metal complex, particularly a ruthenium complex.
5. The method according to claim 4, wherein the isomerization olefin metathesis catalyst is a mixture of Ru-2 and Ru-3. [Chemical Formula 3] [Chemical Formula 4] 6. The method according to any one of the preceding claims, wherein the terminal olefins used in step i) are prepared from fatty acid esters of jojoba oil.
7. The method according to any one of the preceding claims, wherein the terminal olefins used in step i) are prepared according to the following method: a) Reduction of carboxylic acids to obtain primary alcohols. b) Bromination step a) yields the primary alcohol to obtain a bromoalkane. c) Reaction of the bromoalkane from step b) with magnesium to obtain an organomagdium halide. d) Cross-couple the organo-magnesium halide from step c) with terminal brominated olefins to obtain a mixture of terminal olefins.
8. The method according to any one of the preceding claims, wherein the terminal olefins used in step i) are prepared according to the following method: a) Isomerizing carboxylic acids and / or mixtures of carboxylic acids and / or carboxylic esters and / or mixtures of carboxylic esters in the presence of an acid catalyst or a metal complex, preferably an iron carbonyl complex, preferably iron pentacarbonyl; b) The reaction product of step a) is ethylene-degraded in the presence of a ruthenium catalyst to obtain a mixture of terminal olefins.
9. The method according to any one of the preceding claims, wherein the at least one linear terminal olefin used in step i) is a mixture of at least two different linear terminal olefins, each containing 5 to 24 carbon atoms, particularly 16 to 24 carbon atoms, preferably 16 to 20 carbon atoms.
10. The method of claim 9, wherein the at least two linear terminal olefins differ from each other by at least two carbon atoms.
11. The method according to any one of the preceding claims, wherein the at least one linear terminal olefin used in step i) is a mixture of three linear terminal olefins, preferably C6 / C7 / C8, C8 / C9 / C10, C10 / C12 / C14 or C16 / C18 / C20.
12. The method of claim 11, wherein the mixture comprises: - 0.5% to 10%, preferably 1% to 10%, or even more preferably 1% to 5% of C16 terminal olefins; - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C18-terminated olefins; and - 45% to 55%, preferably 45% to 52.5%, and even more preferably 45% to 49.5% of C20 terminal olefins; These percentages are expressed in moles relative to the total molar weight of the terminal olefin mixture.
13. The method according to any one of the preceding claims, wherein the terminal olefin used in step i) is bio-based.
14. A mixture of straight-chain alkanes of natural origin, particularly of plant origin, said mixture being obtainable by the methods defined in claims 1 to 13.
15. A mixture of straight-chain alkanes of natural, particularly plant, origin, especially in the form of a solid aliphatic substance, wherein: - Each straight-chain alkane constituting the mixture contains 8 to 90 carbon atoms, particularly 10 to 85 carbon atoms, more preferably 10 to 75, even more preferably 24 to 60 carbon atoms, and - The quantity distribution of each straight-chain alkane arranged in ascending order of carbon atom number is as follows: o Increasing from the minimum number of carbon atoms in straight-chain alkanes to the mode of distribution; and o Decreases between the mode of this distribution and the straight-chain alkane with the largest number of carbon atoms. These quantities are calculated as a weight percentage relative to the total weight of the mixture of straight-chain alkanes from this natural source.
16. The straight-chain alkane mixture according to claim 15, characterized in that... The span is greater than 15, preferably greater than 20, and less than 60, preferably less than 55. The span is defined as the difference between the number of carbon atoms in a straight-chain alkane with a larger number of carbon atoms and the number of carbon atoms in a straight-chain alkane with a smaller number of carbon atoms.
17. The straight-chain alkane mixture according to claim 15 or 16, wherein each straight-chain alkane in the distribution differs from the preceding and / or consecutive straight-chain alkane in the distribution by one carbon atom.
18. The straight-chain alkane mixture according to claims 15 to 17, wherein the straight-chain alkane having the minimum number of carbon atoms has 8 to 26 carbon atoms, and the straight-chain alkane having the maximum number of carbon atoms has 55 to 90 carbon atoms.
19. The straight-chain alkane mixture according to claims 15 to 18, wherein the mode of the distribution is between 40 and 45 carbon atoms.
20. A mixture of straight-chain alkanes according to any one of claims 15 to 19, wherein the median distribution is between 40 and 45 carbon atoms.
21. The straight-chain alkane mixture according to any one of claims 15 to 20, wherein the melting point of the mixture is between 75°C and 85°C.
22. The straight-chain alkane mixture according to any one of claims 15 to 17, wherein: - The straight-chain alkane with the smallest number of carbon atoms has 15 to 19 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 42 to 46 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 20 to 24 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 52 to 56 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 10 to 14 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 45 to 49 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 9 to 13 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 48 to 52 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 9 to 13 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 52 to 56 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 16 to 20 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 63 to 67 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 13 to 17 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 66 to 70 carbon atoms; or - The straight-chain alkane with the smallest number of carbon atoms has 19 to 23 carbon atoms, and the straight-chain alkane with the largest number of carbon atoms has 49 to 53 carbon atoms.
23. A composition comprising a mixture of straight-chain alkanes according to any one of claims 14 to 22.
24. The composition of claim 23, comprising less than 3% by weight, particularly less than 1% by weight, and preferably free of solid fatty substances of mineral and / or synthetic origin, these weight percentages being expressed relative to the total weight of the composition.
25. The composition according to claim 23 or 24, characterized in that... The composition is a cosmetic or pharmaceutical composition, preferably a cosmetic composition in the form of a fragrance, care or makeup product for use on the skin, mucous membranes or body surface.
26. The composition according to any one of claims 23 to 25, characterized in that... The composition is a solid composition, preferably in rod form.
27. Use of the straight-chain alkane mixture according to any one of claims 14 to 22 as a substitute for petroleum-derived synthetic waxes.
Citation Information
Patent Citations
Process for the manufacture of pigments, especially fluorescent pigments
EP0542669A1
Polymerisable diketopyrrolopyrroles and polymers prepared with same
EP0787730A1
Polymerizable diketopyrrolopyrroles and polymers thereof
EP0787731A2
FR2232303A1
Long-lasting coloured cosmetic composition
FR2933865A1