Photosensitive resin compositions, photosensitive resin films, printed wiring boards, methods for manufacturing the same, and semiconductor packages.
By using a combination of photopolymerizable compounds with different molecular weight olefinic unsaturated groups and acidic substituents, the problems of long development time and high viscosity of photosensitive resin compositions have been solved, enabling the application of photosensitive resin compositions with excellent developability and high production efficiency.
Patent Information
- Application Number
- CN202580028313.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-02-19
- Publication Date
- 2026-11-17
AI Technical Summary
In the prior art, the photosensitive resin composition has a long development time during the development process, resulting in low productivity. Furthermore, the photosensitive layer is highly viscous, which easily contaminates the manufacturing equipment and makes it difficult to peel off the protective film.
A photopolymerizable compound with olefinic unsaturated groups and acidic substituents is used to form a photosensitive resin composition by combining component (A) with a molecular weight of less than 6000 and component (B) with a molecular weight of more than 6000. This composition is used to form through-holes by photolithography and exhibits excellent developability and suppressed viscosity.
It exhibits excellent developability and effectively controls viscosity, thereby improving production efficiency and preventing equipment contamination. It is suitable for forming high-density printed wiring boards and semiconductor packages.
Smart Images

Figure FT_1 
Figure SMS_1 
Figure SMS_4
Abstract
Description
Technical Field
[0001] This embodiment relates to a photosensitive resin composition, a photosensitive resin film, a printed wiring board and a method for manufacturing the same, and a semiconductor package. Background Technology
[0002] In recent years, the miniaturization and high performance of electronic devices have continued to develop, and printed circuit boards have become increasingly dense due to the increase in the number of circuit layers and the miniaturization of wiring. In particular, the high density of semiconductor package substrates such as BGA (Ball Grid Array) and CSP (Chip Scale Package) that carry semiconductor chips has become significant. In addition to the miniaturization of wiring, there is also a requirement for thinner insulating layers and further miniaturization of vias used for interlayer connections.
[0003] One commonly used method for manufacturing printed wiring boards is the stacking method (see, for example, Patent Document 1) that utilizes sequentially layered interlayer insulating layers and conductor layers to form a printed wiring board. In printed wiring boards, with the miniaturization of wiring, the semi-additive method of forming conductor layers through plating has become mainstream. In conventional semi-additive methods, for example (1) after laminating a thermosetting resin film on the conductor layer, the thermosetting resin film is cured by heating to form an "interlayer insulating layer". (2) Then, through-holes for interlayer connection are formed by laser processing, followed by desmearing and roughening treatment by alkaline permanganate treatment or the like. (3) After chemically plating copper on the substrate, a pattern is formed using a photoresist, and then copper is electroplated to form a copper circuit as the conductor layer. (4) After stripping the photoresist, the chemically plated layer is flash-etched to form a copper circuit.
[0004] As mentioned above, laser processing has become the mainstream method for forming through-holes in an interlayer insulating layer formed by curing a thermosetting resin film. However, the miniaturization of through-holes using laser irradiation from a laser processing machine is gradually reaching its limit. Furthermore, in forming through-holes using a laser processing machine, each through-hole needs to be formed individually. When multiple through-holes need to be set at a high density, the formation of through-holes requires a lot of time, resulting in poor manufacturing efficiency.
[0005] In this situation, as a method to form multiple through holes at the same time, the following method is proposed: using a photosensitive resin composition containing an acid-modified vinyl epoxy resin, a photopolymerizable compound, a photopolymerization initiator, an inorganic filler and a silane compound, wherein the content of the inorganic filler is 10 to 80% by mass, multiple small-diameter through holes are formed at the same time by photolithography (for example, see Patent Document 2). Existing technical documents Patent documents
[0006] Patent Document 1: Japanese Patent Application Publication No. 7-304931 Patent Document 2: Japanese Patent Application Publication No. 2017-116652 Summary of the Invention The problem that the invention aims to solve
[0007] When forming through-holes using photolithography, a short development time is required to improve productivity (hereinafter, the performance of short development time is referred to as "developability"). Furthermore, if the surface of the photosensitive layer or photosensitive resin film formed from the photosensitive resin composition has high tackiness, the manufacturing apparatus may become contaminated, or the protective film may be difficult to peel off from the photosensitive resin film, resulting in reduced productivity. Therefore, it is necessary to reduce the tackiness of the photosensitive resin composition.
[0008] In view of this situation, the objective of this embodiment is to provide a photosensitive resin composition with excellent developability and suppressed viscosity, a photosensitive resin film using the photosensitive resin composition, a printed wiring board and a method for manufacturing the same, and a semiconductor package. Methods for solving problems
[0009] In order to solve the above-mentioned problems, the inventors conducted research and found that the above-mentioned problems can be solved by the following embodiments. That is, this embodiment relates to the following [1] to
[13] . <1> A photosensitive resin composition comprising: (A) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of less than 6000; and (B) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of 6000 or more. <2> According to the above <1> The photosensitive resin composition wherein component (A) comprises an alicyclic backbone. <3> According to the above <1> or <2> The photosensitive resin composition wherein component (B) is an acrylic resin having olefinic unsaturated groups and acidic substituents. <4> According to the above <1> ~ <3> The photosensitive resin composition according to any one of the above-mentioned components (A) has a weight-average molecular weight (Mw) of 300 to 5000. <5> According to the above <1> ~ <4> The photosensitive resin composition according to any one of the above-mentioned components (B) has a weight-average molecular weight (Mw) of 7,000 to 50,000. <6> According to the above <1> ~ <5> The photosensitive resin composition according to any one of the following, wherein the content of component (B) is 10 to 500 parts by weight relative to 100 parts by weight of component (A). <7> According to the above <1> ~ <6> The photosensitive resin composition described in any one of the following further comprises (C) a thermosetting resin. <8> According to the above <1> ~ <7> The photosensitive resin composition described in any one of the following further comprises (D) an elastomer. <9> According to the above <1> ~ <8> The photosensitive resin composition described in any one of the following is used to form an interlayer insulating layer having light-permeable holes. <10> A photosensitive resin film comprising the above-mentioned... <1> ~ <8> The photosensitive resin composition described in any one of the following statements. <11> A printed wiring board comprising the above <1> ~ <8> The cured product of the photosensitive resin composition described in any one of the above statements. <12> A semiconductor package comprising the above <11> The aforementioned printed wiring board and semiconductor components. <13> A method for manufacturing a printed wiring board, comprising the following (1) to (4). (1): The above <10> The photosensitive resin film is laminated onto one or both sides of the circuit board. (2): By exposing and developing the photosensitive resin film laminated in (1) above, an interlayer insulating layer with through holes is formed. (3): Heat and cure the above-mentioned interlayer insulation layer with through holes. (4): A circuit pattern is formed on the above-mentioned interlayer insulating layer. Invention Effects
[0010] According to this embodiment, it is possible to provide a photosensitive resin composition with excellent developability and suppressed adhesion, a photosensitive resin film using the photosensitive resin composition, a printed wiring board and a method for manufacturing the same, and a semiconductor package. Attached Figure Description
[0011] Figure 1 This is a schematic diagram illustrating one method of manufacturing a printed wiring board using a photosensitive resin film of this embodiment as an interlayer insulating layer. Detailed Implementation
[0012] The lower and upper limits of the numerical ranges described in this specification can be replaced with the values shown in the embodiments. Furthermore, the lower and upper limits of the numerical ranges can be arbitrarily combined with the lower or upper limits of other numerical ranges. In expressions such as "AA~BB", the values AA and BB at both ends are included within the numerical range as the lower and upper limits, respectively.
[0013] In this specification, for example, the description "10 or more" refers to a value of 10 or more, and this is also the basis for cases where the value is different. Similarly, the description "10 or less" refers to a value of 10 or less, and this is also the basis for cases where the value is different.
[0014] In this specification, the content of each component refers to the total content of the multiple substances that belong to each component, unless otherwise specified.
[0015] In this specification, "solid components" refers to non-volatile components other than solvents and other volatile substances, and also includes substances that are liquid at room temperature. Here, room temperature refers to 25°C.
[0016] In this specification, "resin components" refers to resin and compounds that form resin through a curing reaction. In the photosensitive resin composition of this embodiment, for example, components (A), (B), (C), (D) and (E) described below are resin components, while components (F), (G) and (H) are not resin components.
[0017] In this specification, "number of carbon atoms in the ring" refers to the number of carbon atoms required to form a ring, excluding the number of carbon atoms from substituents in the ring. For example, the cyclohexane skeleton and the methylcyclohexane skeleton both have 6 carbon atoms in the ring.
[0018] The expression "(meth)acrylic acid XX" refers to one or both of acrylic acid XX and its corresponding methacrylic acid XX. Additionally, "(meth)acryloyl" refers to one or both of acryloyl and methacryloyl groups.
[0019] In this specification, when a layer is referred to as a "layer" such as an interlayer insulation layer, the concept of "layer" is also included not only when it is a whole layer, but also when it is not a whole layer, but a part of it is island-shaped, has openings, or has an indistinct interface with adjacent layers.
[0020] The weight-average molecular weight (Mw) and number-average molecular weight (Mn) in this specification refer to values converted to polystyrene by gel permeation chromatography (GPC). Specifically, the weight-average molecular weight (Mw) in this specification can be determined by the methods described in the examples.
[0021] The mechanism of action described in this specification is speculative and does not limit the mechanism by which this embodiment achieves its effect.
[0022] This embodiment also includes any combination of the items described in this specification.
[0023] [Photosensitive Resin Composition] The photosensitive resin composition of this embodiment contains: (A) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of less than 6000; and (B) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of 6000 or more.
[0024] In addition, in this specification, each ingredient is sometimes appropriately abbreviated as "(A) ingredient", "(B) ingredient", etc.
[0025] The reason why the photosensitive resin composition of this embodiment has excellent developability and suppressed viscosity is uncertain, but it is speculated that components (A) and (B) contained in the photosensitive resin composition of this embodiment both have acidic substituents, thus resulting in excellent developability, and component (B) is a compound with a relatively large molecular weight, thus suppressing viscosity.
[0026] The photosensitive resin composition of this embodiment can form patterns such as through-holes through exposure and development. Therefore, the photosensitive resin composition of this embodiment is suitable for forming interlayer insulating layers with photosensitive through-holes. Furthermore, in this specification, "photosensitive through-hole" refers to a through-hole formed by photolithography, i.e., exposure and development. Furthermore, the photosensitive resin composition of this embodiment is suitable for negative photosensitive resin compositions. Furthermore, the photosensitive resin composition of this embodiment is also useful as a surface protective film such as a solder resist.
[0027] <(A) Photopolymeric compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of less than 6000> The photosensitive resin composition of this embodiment contains (A) a photopolymerizable compound having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of less than 6000. (A) One ingredient may be used alone or two or more ingredients may be used together. Furthermore, in the photosensitive resin composition of this embodiment, compounds that satisfy the requirements of both component (A) and component (B), and compounds that satisfy the requirements of both component (A) and component (C) are classified as component (A).
[0028] (A) Because it has olefinic unsaturated groups, it is a compound that exhibits photopolymerization, especially free radical polymerization. Examples of olefinic unsaturated groups present in component (A) include vinyl, allyl, propargyl, butenyl, ethynyl, phenylethynyl, maleimide, nadicimide, and (meth)acryloyl. Among these, (meth)acryloyl is preferred from the viewpoint of reactivity and pore resolution.
[0029] From the perspective of being able to undergo alkaline development, component (A) has acidic substituents. Examples of acidic substituents in component (A) include carboxyl groups, sulfonic acid groups, and phenolic hydroxyl groups. Among these, from the viewpoint of pore resolution, carboxyl groups are preferred.
[0030] (A) The acid value of the component is preferably 20~200mgKOH / g, more preferably 40~180mgKOH / g, even more preferably 60~150mgKOH / g, and particularly preferably 80~120mgKOH / g. When the acid value of component (A) is above the lower limit mentioned above, it tends to have better developability. In addition, when the acid value of component (A) is below the upper limit mentioned above, it tends to have better dielectric properties. (A) The acid value of the component can be determined by the method described in the examples.
[0031] From a radiometric point of view, the weight-average molecular weight (Mw) of component (A) is less than 6000. (A) The weight-average molecular weight (Mw) of the component is preferably 300 to 5000, more preferably 600 to 4000, even more preferably 1000 to 3500, even more preferably 1200 to 3000, and particularly preferably 1500 to 2500. When the weight-average molecular weight (Mw) of component (A) is above the lower limit mentioned above, it tends to suppress viscosity more easily. In addition, when the weight-average molecular weight (Mw) of component (A) is below the upper limit mentioned above, it tends to have better developability.
[0032] From the viewpoint of dielectric properties, component (A) preferably contains an alicyclic backbone. From the viewpoints of through-hole resolution, conductor adhesion and dielectric properties, the alicyclic framework of component (A) is preferably an alicyclic framework with 5 to 20 cyclic carbon atoms, more preferably an alicyclic framework with 5 to 18 cyclic carbon atoms, even more preferably an alicyclic framework with 6 to 18 cyclic carbon atoms, even more preferably an alicyclic framework with 8 to 14 cyclic carbon atoms, and particularly preferably an alicyclic framework with 8 to 12 cyclic carbon atoms. Furthermore, from the viewpoints of aperture resolution, conductor adhesion, and dielectric properties, the aforementioned alicyclic framework is preferably composed of two or more rings, more preferably two to four rings, and even more preferably three rings. Examples of alicyclic frameworks with two or more rings include norbornene, decahydronaphthalene, bicycloundecane, and saturated bicyclopentadiene. These alicyclic frameworks may or may not have substituents. Furthermore, in this specification, the saturated dicyclopentadiene skeleton refers to a skeleton containing a ring structure in which the unsaturated bonds in the dicyclopentadiene ring are saturated; it can also be called a tricyclic [5.2.1.0]. 2,6 [Decane structure. Among them, from the viewpoints of through-hole resolution, conductor adhesion and dielectric properties, saturated dicyclopentadiene framework is preferred.] From the same point of view, component (A) preferably contains the alicyclic skeleton shown in the following general formula (A-1).
[0033] [Chemical Formula 1] (where R) A1 Alkyl groups representing 1 to 12 carbon atoms can be substituted at any position in the alicyclic skeleton described above. 1 Integers between 0 and 6. (This refers to the bonding site with other structures.)
[0034] In the above general formula (A-1), R is... A1 Examples of alkyl groups having 1 to 12 carbon atoms include methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, and n-pentyl. Preferably, the alkyl group has 1 to 6 carbon atoms, more preferably 1 to 3 carbon atoms, and even more preferably methyl. m 1 It is an integer from 0 to 6, preferably an integer from 0 to 2, and more preferably 0. m 1 When the integer is between 2 and 6, multiple R A1 They can be the same or different. Furthermore, multiple Rs... A1 It can substitute on the same carbon atom or on different carbon atoms within the possible range. For bonding sites with other structures, bonding can be performed on any carbon atom on the alicyclic framework, preferably on carbon atoms at sites 1 or 2 of the following general formula (A-1') and carbon atoms at sites 3 or 4.
[0035] [Chemical Formula 2] (where R) A1m 1 and R in general formula (A-1) A1 m 1 and same.)
[0036] From the viewpoints of through-hole resolution, conductor adhesion, and dielectric properties, component (A) is preferably an acid-modified vinyl-containing epoxy resin prepared by reacting a polybasic acid anhydride containing saturated or unsaturated groups (a3) with a compound obtained by modifying epoxy resin (a1) with an organic acid containing olefinic unsaturated groups (a2) [hereinafter sometimes referred to as component (A')]. Here, "acid modification" in acid-modified vinyl-containing epoxy resin refers to the presence of acidic substituents, "vinyl" refers to olefinic unsaturated groups, and "epoxy resin" refers to the use of epoxy resin as a raw material. Acid-modified vinyl-containing epoxy resin does not necessarily need to have epoxy groups, and may or may not have epoxy groups. The preferred method for component (A) obtained from (a1) epoxy resin, (a2) organic acid containing olefinic unsaturated groups and (a3) polybasic acid anhydride containing saturated or unsaturated groups will be described below.
[0037] (a1) Epoxy resin) As (a1) epoxy resin, epoxy resin having two or more epoxy groups is preferred. (a1) One type of epoxy resin can be used alone or two or more types can be used together. (a1) Epoxy resins can be classified into glycidyl ether type epoxy resins, glycidyl amine type epoxy resins, glycidyl ester type epoxy resins, etc. Among them, glycidyl ether type epoxy resins are preferred.
[0038] (a1) Epoxy resins can also be classified into various types according to their main skeleton, such as epoxy resins with an alicyclic skeleton, phenolic varnish-type epoxy resins, bisphenol-type epoxy resins, aralkyl-type epoxy resins, and other epoxy resins. Among these, epoxy resins with an alicyclic skeleton and bisphenol-type epoxy resins are preferred.
[0039] -Epoxy resins with an alicyclic backbone- Regarding the alicyclic skeleton of the epoxy resin, it can be described in the same way as the alicyclic skeleton of component (A) above, and the preferred method is also the same. As an epoxy resin having an alicyclic backbone, the epoxy resin shown in the following general formula (A-2) is preferred.
[0040] [Chemical Formula 3] (where R) A1Alkyl groups representing 1 to 12 carbon atoms can be substituted at any position in the alicyclic skeleton described above. R A2 Indicates alkyl groups with 1 to 12 carbon atoms. m 1 m is an integer between 0 and 6. 2 (where n is an integer from 0 to 3.)
[0041] In general formula (A-2), R A1 R in general formula (A-1) A1 The methods for optimization are the same. R in general formula (A-2) A2 Examples of alkyl groups having 1 to 12 carbon atoms include methyl, ethyl, n-propyl, isopropyl, n-butyl, isobutyl, tert-butyl, and n-pentyl. Preferably, the alkyl group has 1 to 6 carbon atoms, more preferably 1 to 3 carbon atoms, and even more preferably methyl. m in general formula (A-2) 1 With m in general formula (A-1) 1 The methods for optimization are the same. m in general formula (A-2) 2 It is an integer from 0 to 3, preferably 0 or 1, and more preferably 0. In general formula (A-2), n represents the number of repetitions of the structural unit within the parentheses, which is a number from 0 to 50. Typically, epoxy resin is a mixture of substances with different numbers of repetitions of the structural units within the parentheses; therefore, in this case, n is represented by the average value of the mixture. Preferably, n is a number from 0 to 30.
[0042] -Bisphenolic epoxy resin- Examples of bisphenol-type epoxy resins include bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol S type epoxy resin, and 3,3',5,5'-tetramethyl-4,4'-diglycidyloxydiphenylmethane. Among these, bisphenol A type epoxy resin is preferred. As a bisphenol type epoxy resin, an epoxy resin having the structural unit shown in the following general formula (A-3) is preferred.
[0043] [Chemical Formula 4] (where R) A3 Y represents a hydrogen atom or a methyl group. A1 Each can independently represent a hydrogen atom or a glycidyl group. Multiple Rs A3 They can be the same or different. n² represents numbers greater than or equal to 0.
[0044] From the perspective of improving the resolution of vias, R A3 Preferably, all are methyl groups. Furthermore, from the same perspective, Y...A1 Glycidyl group is preferred.
[0045] n2 represents a number greater than or equal to 0, and can be appropriately selected from integers between 10 and 100, between 10 and 80, or between 15 and 60.
[0046] The Y represented by the above general formula (A-3) A1 Bisphenol A type epoxy resin or bisphenol F type epoxy resin, which is glycidyl-based, can be produced by, for example, by making the Y-type epoxy resin of the above general formula (A-3)... A1 The hydroxyl group (-OY) of bisphenol A type epoxy resin or bisphenol F type epoxy resin containing hydrogen atoms A1 It is obtained by reacting with epichlorohydrin.
[0047] Examples of phenolic varnish-type epoxy resins include bisphenol A phenolic varnish-type epoxy resin, bisphenol F phenolic varnish-type epoxy resin, bisphenol S phenolic varnish-type epoxy resin, phenolic varnish-type epoxy resin, cresol phenolic varnish-type epoxy resin, biphenyl phenolic varnish-type epoxy resin, naphthol phenolic varnish-type epoxy resin, etc. Examples of aralkyl-type epoxy resins include phenolic aralkyl-type epoxy resins, biphenyl aralkyl-type epoxy resins, and naphthol aralkyl-type epoxy resins. Other epoxy resins include stilbene-type epoxy resins, naphthalene-containing skeleton-type epoxy resins, biphenyl-type epoxy resins, dihydroanthracene-type epoxy resins, cyclohexanediethanol-type epoxy resins, trimethylolpropionic epoxy resins, alicyclic epoxy resins, aliphatic chain epoxy resins, heterocyclic epoxy resins, spirocyclic epoxy resins, and rubber-modified epoxy resins.
[0048] (a2) Organic acids containing olefinic unsaturated groups) As an organic acid containing an olefinic unsaturated group (a2), a monocarboxylic acid containing an olefinic unsaturated group is preferred. As an olefinic unsaturated group present in component (a2), one can be an example of a group that is the same as an olefinic unsaturated group present in component (A). Examples of components (a2) include acrylic acid, acrylic acid dimers, methacrylic acid, β-furfurylic acid, β-styrylic acid, cinnamic acid, crotonic acid, α-cyanocinonic acid, and other acrylic acid derivatives; half-ester compounds that are the reaction products of hydroxyl-containing acrylates and diacid anhydrides; and half-ester compounds that are the reaction products of vinyl monoglycidyl ethers or vinyl monoglycidyl esters and diacid anhydrides. (a2) One ingredient may be used alone or two or more ingredients may be used together.
[0049] The above-mentioned half-ester compound is obtained by reacting one or more compounds containing an olefinic unsaturated group selected from hydroxyl-containing acrylates, vinyl-containing monoglycidyl ethers, and vinyl-containing monoglycidyl esters with a diacid anhydride. Preferably, the reaction involves reacting the compound containing the olefinic unsaturated group with the diacid anhydride in equimolar amounts.
[0050] Examples of hydroxyl-containing acrylates used in the synthesis of the above-mentioned half-ester compounds include hydroxyethyl (meth)acrylate, hydroxypropyl (meth)acrylate, hydroxybutyl (meth)acrylate, polyethylene glycol mono(meth)acrylate, trimethylolpropane di(meth)acrylate, pentaerythritol tri(meth)acrylate, and dipentaerythritol penta(meth)acrylate. Examples of vinyl-containing monoglycidyl ethers include glycidyl (meth)acrylate.
[0051] The diacid anhydrides used in the synthesis of the aforementioned half-ester compounds may contain saturated or unsaturated groups. Examples of diacid anhydrides include succinic anhydride, maleic anhydride, tetrahydrophthalic anhydride, phthalic anhydride, methyltetrahydrophthalic anhydride, ethyltetrahydrophthalic anhydride, hexahydrophthalic anhydride, methylhexahydrophthalic anhydride, ethylhexahydrophthalic anhydride, and itaconic anhydride.
[0052] When component (A') is formed by reacting component (a1) with component (a2), and using a monocarboxylic acid containing an olefinic unsaturated group as component (a2), it has hydroxyl groups formed by the ring-opening addition reaction of the epoxy group of component (a1) with the carboxyl group of component (a2). Next, by further reacting component (A') with component (a3), an acid-modified vinyl-containing epoxy resin can be obtained by half-esterifying the hydroxyl groups of component (A') (including the hydroxyl groups originally present in component (a1)) with the anhydride group of component (a3).
[0053] (a3) Polybasic acid anhydrides containing saturated or unsaturated groups) As component (a3), it may contain either saturated or unsaturated groups. Examples of components (a3) include succinic anhydride, maleic anhydride, tetrahydrophthalic anhydride, phthalic anhydride, methyltetrahydrophthalic anhydride, ethyltetrahydrophthalic anhydride, hexahydrophthalic anhydride, methylhexahydrophthalic anhydride, ethylhexahydrophthalic anhydride, itaconic anhydride, etc. Among these, tetrahydrophthalic anhydride is preferred from the viewpoint of pore resolution. Component (a3) may be used alone or in combination with two or more.
[0054] In the reaction of component (A') and component (a3), for example, component (a3) is reacted by 0.1 to 1.0 equivalents relative to 1 equivalent of hydroxyl groups in component (A'), thereby adjusting the acid value of the acid-modified vinyl-containing epoxy resin.
[0055] (Content of component (A)) The content of component (A) in the photosensitive resin composition of this embodiment is preferably 5 to 60% by mass, more preferably 10 to 50% by mass, further preferably 15 to 40% by mass, and particularly preferably 20 to 30% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment. When the content of component (A) is above the lower limit mentioned above, the developability tends to be better. In addition, when the content of component (A) is below the upper limit mentioned above, the viscosity tends to be more easily suppressed.
[0056] <(B) Photopolymerizable compounds with olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of 6000 or higher> The photosensitive resin composition of this embodiment contains (B) a photopolymerizable compound having an olefinic unsaturated group and an acidic substituent and a weight-average molecular weight (Mw) of 6000 or more. (B) Components may be used alone or in combination with two or more.
[0057] (B) Components exhibit photopolymerization properties, especially free radical polymerization properties, due to the presence of olefinic unsaturated groups. Examples of olefinic unsaturated groups present in component (B) include vinyl, allyl, propargyl, butenyl, ethynyl, phenylethynyl, maleimide, nadicimide, and (meth)acryloyl groups, which exhibit photopolymerization properties. Among these, (meth)acryloyl is preferred from the viewpoint of reactivity and pore resolution.
[0058] The double bond equivalent of component (B) is preferably 100-1500 g / mol, more preferably 200-1000 g / mol, even more preferably 300-800 g / mol, and particularly preferably 400-600 g / mol. (B) When the double bond equivalent of the component is within the above range, it tends to easily obtain a cured product with better heat resistance and dielectric properties. The double bond equivalent of component (B) can be obtained by calculating the amount of raw materials used in the preparation of component (B).
[0059] Examples of acidic substituents in component (B) include carboxyl groups, sulfonic acid groups, and phenolic hydroxyl groups. Among these, from the viewpoint of pore resolution, carboxyl groups are preferred.
[0060] (B) The acid value of the component is preferably 10~150mgKOH / g, more preferably 20~100mgKOH / g, even more preferably 30~70mgKOH / g, and particularly preferably 35~50mgKOH / g. When the acid value of component (B) is above the lower limit mentioned above, it tends to have excellent developability. In addition, when the acid value of component (B) is below the upper limit mentioned above, it tends to have better dielectric properties. (B) The acid value of the component can be determined by the method described in the examples.
[0061] From the perspective of inhibiting viscosity, the weight-average molecular weight (Mw) of component (B) is above 6000. (B) The weight-average molecular weight (Mw) of the component is preferably 7,000 to 50,000, more preferably 8,000 to 30,000, even more preferably 10,000 to 20,000, and particularly preferably 11,000 to 15,000. When the weight-average molecular weight (Mw) of component (B) is above the lower limit mentioned above, it tends to suppress viscosity more easily. In addition, when the weight-average molecular weight (Mw) of component (B) is below the upper limit mentioned above, it tends to have better developability.
[0062] The difference between the weight-average molecular weight (Mw) of component (B) and that of component (A) [weight-average molecular weight (Mw) of component (B) - weight-average molecular weight (Mw) of component (A)] is preferably 2,000 to 40,000, more preferably 4,000 to 30,000, even more preferably 6,000 to 20,000, and particularly preferably 8,000 to 15,000. When the difference in weight-average molecular weight (Mw) is within the above range, there is a tendency for better developability and easier suppression of viscosity.
[0063] (B) The preferred component is a polymer (B1) having olefinic unsaturated groups and acidic substituents (hereinafter also referred to as "polymer (B1)"). Examples of polymers (B1) include (meth)acrylic resins, styrene resins, vinyl ester polymers, vinyl ether polymers, halogen-containing resins, polyolefins, polycarbonates, polyesters, polyamides, polyurethanes, polysulfone resins, polyphenylene ether resins, cellulose derivatives, and silicone resins, each having an olefinic unsaturated group and an acidic substituent. Among these, (meth)acrylic resins are preferred. (Meth)acrylic resins preferably contain structural units derived from acrylates. Examples of acrylates include methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, butyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, stearyl (meth)acrylate, hydroxyethyl (meth)acrylate, and hydroxypropyl (meth)acrylate.
[0064] The polymer (B1) may have acidic substituents at the end or on the side chain, preferably on the side chain. The acidic substituents in the polymer (B1) are preferably contained in structural units derived from monomers having acidic substituents. Examples of monomers having acidic substituents include acids having olefinic unsaturated groups such as (meth)acrylic acid, 2-carboxyethyl (meth)acrylic acid, 2-carboxypropyl (meth)acrylic acid, and maleic acid (anhydride), with (meth)acrylic acid being preferred. That is, polymer (B1) is preferably a polymer having a carboxyl group derived from (meth)acrylic acid, and more preferably a (meth)acrylic acid resin having a carboxyl group derived from (meth)acrylic acid.
[0065] The polymer (B1) may have an olefin unsaturated group at the end or an olefin unsaturated group on the side chain, preferably an olefin unsaturated group on the side chain. As a polymer (B1) having olefinic unsaturated groups in its side chain, an example of a polymer (b1) having a carboxyl group derived from (meth)acrylic acid (hereinafter also referred to as "polymer (b1)") and a compound (b2) having a functional group and an olefinic unsaturated group that are reactive with carboxyl groups (hereinafter also referred to as "compound (b2)") can be considered as reactants. In the case where polymer (B1) is a reactant of polymer (b1) and compound (b2), by reacting a portion of the carboxyl groups of polymer (b1) with compound (b2), polymer (B1) becomes a polymer having carboxyl groups derived from polymer (b1).
[0066] Examples of functional groups in compound (b2) that are reactive with carboxyl groups include epoxy, hydroxyl, amino, and isocyanate groups. Among these, epoxy groups are preferred. As an example of a compound (b) containing an epoxy group, an unsaturated compound containing an alicyclic epoxy group can be cited. Preferably, the unsaturated compound containing an alicyclic epoxy group is a compound having one olefinic unsaturated group and one alicyclic epoxy group per molecule; more preferably, it is a compound having one (meth)acryloyl group and one alicyclic epoxy group per molecule. That is, more preferably, the alicyclic epoxy group of this compound is reacted with the carboxyl group present in the polymer (b1). Examples of alicyclic epoxy groups in unsaturated compounds containing alicyclic epoxy groups include 3,4-epoxycyclohexyl, 2,3-epoxycyclopentyl, and 3,4-epoxytricyclic [5.2.1.0]. 2,6 [K-based, etc.] The preferred manner in which the olefinic unsaturated group of the unsaturated compound containing alicyclic epoxy group is the same as that in which the olefinic unsaturated group of component (B) is present is the same.
[0067] (Content of component (B)) The content of component (B) in the photosensitive resin composition of this embodiment is preferably 5 to 80% by mass, more preferably 10 to 70% by mass, further preferably 15 to 60% by mass, even more preferably 20 to 55% by mass, and particularly preferably 30 to 50% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment. When the content of component (B) is above the lower limit mentioned above, it tends to more easily suppress viscosity. In addition, when the content of component (B) is below the upper limit mentioned above, it tends to have better developability.
[0068] The content of component (B) in the photosensitive resin composition of this embodiment is preferably 10 to 500 parts by weight relative to 100 parts by weight of component (A), more preferably 30 to 400 parts by weight, further preferably 50 to 300 parts by weight, even more preferably 100 to 250 parts by weight, and particularly preferably 150 to 200 parts by weight. When the content of component (B) is above the lower limit mentioned above, it tends to more easily suppress viscosity. In addition, when the content of component (B) is below the upper limit mentioned above, it tends to have better developability.
[0069] <(C) Thermosetting Resins> The photosensitive resin composition of this embodiment preferably further contains (C) a thermosetting resin. The photosensitive resin composition of this embodiment contains (C) a thermosetting resin, and the heat resistance of the cured product of the photosensitive resin composition of this embodiment tends to be further improved. (C) A thermosetting resin may be used alone or in combination with two or more types.
[0070] Examples of thermosetting resins (C) include epoxy resins, maleimide resins, allyl resins, isocyanate resins, phenolic resins, cyanate resins, benzoxazine resins, oxetane resins, amino resins, unsaturated polyester resins, vinyl resins, dicyclopentadiene resins, silicone resins, triazine resins, melamine resins, and other known thermosetting resins. From the viewpoint of heat resistance and conductor adhesion, the photosensitive resin composition of this embodiment preferably contains one or more selected from maleimide resin, allyl resin and isocyanate resin.
[0071] (Maleimide resin) Examples of maleimide resins include aromatic maleimide compounds having N-substituted maleimide groups directly bonded to the aromatic ring, and aliphatic maleimide compounds having N-substituted maleimide groups directly bonded to aliphatic hydrocarbons. From the viewpoint of heat resistance and processability, aromatic maleimide compounds are preferred, and aromatic bismaleimide compounds are more preferred. Examples of aromatic maleimide compounds include bis(4-maleimidephenyl)methane, 2,2-bis[4-(4-maleimidephenoxy)phenyl]propane, 3,3'-dimethyl-5,5'-diethyl-4,4'-diphenylmethane bismaleimide, polyphenylmethane maleimide, biphenyl aralkyl maleimide resin, and aromatic bismaleimide resins having an indmium skeleton. Among these, aromatic bismaleimide resins having an indmium skeleton are preferred. As an aromatic bismaleimide resin having an indane skeleton, the compound shown in the following general formula (C-1) is preferred.
[0072] [Chemical Formula 5] (where R) C1 Each of the following is independently an alkyl group having 1 to 10 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an alkylthio group having 1 to 10 carbon atoms, an aryl group having 6 to 10 carbon atoms, an aryloxy group having 6 to 10 carbon atoms, an arylthio group having 6 to 10 carbon atoms, a cycloalkyl group having 3 to 10 carbon atoms, a halogen atom, a hydroxyl group, or a mercapto group. C1 Each is an independent integer between 0 and 3. R C2 ~R C4 Each is an alkyl group having 1 to 10 carbon atoms. R C5 Each of the following is independently an alkyl group having 1 to 10 carbon atoms, an alkoxy group having 1 to 10 carbon atoms, an alkylthio group having 1 to 10 carbon atoms, an aryl group having 6 to 10 carbon atoms, an aryloxy group having 6 to 10 carbon atoms, an arylthio group having 6 to 10 carbon atoms, a cycloalkyl group having 3 to 10 carbon atoms, a halogen atom, a nitro group, a hydroxyl group, or a mercapto group. C2 Each is an independent integer between 0 and 4. C3 (A number between 0.95 and 10.0.)
[0073] R in the above general formula (C-1) C1 ~R C5Alkyl groups with 1 to 10 carbon atoms are shown, for example, methyl, ethyl, propyl, butyl, pentyl, hexyl, heptyl, octyl, nonyl, decyl, etc. These alkyl groups can be either straight-chain or branched. As R C1 Or R C5 The alkyl groups contained in the alkoxy groups with 1 to 10 carbon atoms and the alkylthio groups with 1 to 10 carbon atoms shown can be alkyl groups that are the same as the alkyl groups with 1 to 10 carbon atoms mentioned above. As a result of R C1 Or R C5 Aryl groups with 6 to 10 carbon atoms are shown, for example, phenyl and naphthyl. As R C1 Or R C5 The aryl groups contained in the aryloxy groups with 6 to 10 carbon atoms and the arylthio groups with 6 to 10 carbon atoms shown can be groups that are the same as the aryl groups with 6 to 10 carbon atoms mentioned above. As a result of R C1 Or R C5 Examples of cycloalkyl groups with 3 to 10 carbon atoms include cyclopropyl, cyclobutyl, cyclopentyl, cyclohexyl, cycloheptyl, cyclooctyl, cyclononyl, and cyclodecyl. From the perspectives of dielectric properties, conductor adhesion, solvent solubility, operability, and heat resistance, n in the above general formula (C-1) C3 The number is preferably 0.98 to 8.0, more preferably 1.0 to 7.0, and even more preferably 1.1 to 6.0.
[0074] (Allyl resin) Examples of allyl resins include compounds having two or more allyl groups. Examples of compounds having two or more allyl groups include isocyanurate compounds containing allyl groups, cyanurate compounds containing allyl groups, and glycourea compounds containing allyl groups. Examples of isocyanurate compounds containing allyl groups include diallyl isocyanurate and other isocyanurate compounds with two allyl groups, and triallyl isocyanurate and other isocyanurate compounds with three allyl groups. Examples of cyanurate compounds containing allyl groups include diallyl cyanurate and other cyanurate compounds with two allyl groups, and triallyl cyanurate and other cyanurate compounds with three allyl groups. Examples of allyl-containing glycourea compounds include 1,3,4,6-tetraallyl glycourea. Among these, isocyanurate compounds containing allyl groups are preferred, and isocyanurate compounds having two allyl groups are more preferred. As isocyanurate compounds having two allyl groups, compounds represented by the following general formula (C-2) are preferred.
[0075] [Chemical Formula 6] (where R) C6 (A substituted or unsubstituted alkyl group having 1 to 20 carbon atoms.)
[0076] R in the above general formula (C-2) C6 The substituted or unsubstituted alkyl group having 1 to 20 carbon atoms is shown, preferably an unsubstituted alkyl group having 1 to 20 carbon atoms, more preferably an unsubstituted alkyl group having 3 to 15 carbon atoms, and even more preferably an unsubstituted alkyl group having 5 to 12 carbon atoms.
[0077] (Isocyanate resin) Compounds having two or more isocyanate groups can be cited as examples of isocyanate resins. Examples of compounds having two or more isocyanate groups include aliphatic isocyanates such as trimethylene diisocyanate, tetramethylene diisocyanate, pentamethylene diisocyanate, hexamethylene diisocyanate, and trimethylhexamethylene diisocyanate; alicyclic isocyanates such as 1,3-cyclopentane diisocyanate, 1,4-cyclohexane diisocyanate, 1,2-cyclohexane diisocyanate, isophorone diisocyanate, and norbornene diisocyanate; aromatic isocyanates such as phenyl diisocyanate, 2,4-toluene diisocyanate, and 2,6-toluene diisocyanate; their biuret forms; and their isocyanurate forms. Among these, aliphatic isocyanates having two or more isocyanate groups are preferred, and hexamethylene diisocyanate is more preferred.
[0078] When the photosensitive resin composition of this embodiment contains maleimide resin as (C) thermosetting resin, from the viewpoint of heat resistance, dielectric properties and conductor adhesion, the content of maleimide resin in the photosensitive resin composition of this embodiment is preferably 1 to 30% by mass, more preferably 5 to 20% by mass, and even more preferably 8 to 15% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment.
[0079] When the photosensitive resin composition of this embodiment contains allyl resin as (C) thermosetting resin, from the viewpoint of heat resistance, dielectric properties and conductor adhesion, the content of allyl resin in the photosensitive resin composition of this embodiment is preferably 1 to 30% by mass, more preferably 5 to 20% by mass, and even more preferably 8 to 15% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment.
[0080] When the photosensitive resin composition of this embodiment contains isocyanate resin as (C) thermosetting resin, from the viewpoint of heat resistance, dielectric properties and conductor adhesion, the content of isocyanate resin in the photosensitive resin composition of this embodiment is preferably 1 to 30% by mass, more preferably 5 to 20% by mass, and even more preferably 8 to 15% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment.
[0081] (C) Content of thermosetting resin When the photosensitive resin composition of this embodiment contains (C) thermosetting resin, from the viewpoint of heat resistance, dielectric properties and conductor adhesion, the total content of (C) thermosetting resin in the photosensitive resin composition of this embodiment, based on the total amount of resin components in the photosensitive resin composition of this embodiment, is preferably 5 to 70% by mass, more preferably 10 to 60% by mass, further preferably 20 to 50% by mass, and particularly preferably 30 to 40% by mass.
[0082] <(D) Elastomers> The photosensitive resin composition of this embodiment preferably further contains (D) elastomer. The photosensitive resin composition of this embodiment contains an elastomer (D), and the conductor adhesion of the cured product of the photosensitive resin composition of this embodiment tends to be further improved. Furthermore, the term "elastomer" here refers to a polymer whose glass transition temperature is below 25°C as determined by differential scanning calorimetry according to JIS K 6240:2011. (D) One type of elastomer can be used alone, or two or more types can be used together.
[0083] Examples of (D) elastomers include polybutadiene-based elastomers, butadiene-styrene copolymers, polyester-based elastomers, styrene-based elastomers, olefin-based elastomers, urethane-based elastomers, polyamide-based elastomers, acrylic elastomers, silicone-based elastomers, and derivatives of these elastomers. Among these, polybutadiene-based elastomers are preferred from the viewpoint of compatibility with resin components and from the viewpoint of forming cured products with superior conductive adhesion.
[0084] Polybutadiene-based elastomers are elastomers containing structural units derived from butadiene. They can be polybutadiene homopolymers or copolymers of butadiene with monomers other than butadiene. As copolymers of butadiene with monomers other than butadiene, butadiene-styrene copolymers are preferred. From the viewpoint of resolution, polybutadiene-based elastomers are preferably polybutadiene-based elastomers having anhydride groups, and more preferably polybutadiene-based elastomers having anhydride groups derived from maleic anhydride. When the polybutadiene-based elastomer has an anhydride group, from the viewpoint of resolution and forming a cured product with a superior relative permittivity, the number of anhydride groups in one molecule is preferably 1 to 12, more preferably 3 to 11, and even more preferably 6 to 10.
[0085] (D) The number-average molecular weight (Mn) of the elastomer is preferably 1,000 to 100,000, more preferably 2,000 to 50,000, even more preferably 3,000 to 10,000, and particularly preferably 4,000 to 7,000.
[0086] (D) Content of elastomers When the photosensitive resin composition of this embodiment contains (D) elastomer, from the viewpoint of forming a cured product with better heat resistance and conductor adhesion, the content of (D) elastomer in the photosensitive resin composition of this embodiment is preferably 1 to 30% by mass, more preferably 3 to 20% by mass, and even more preferably 5 to 15% by mass, based on the total amount of resin components in the photosensitive resin composition.
[0087] <(E) Compounds having two or more olefinic unsaturated groups and no acidic substituents> The photosensitive resin composition of this embodiment may further contain (E) a compound having two or more olefinic unsaturated groups and no acidic substituents, or it may not contain such a compound. (E) Components may be used alone or in combination with two or more.
[0088] Examples of olefinic unsaturated groups present in component (E) include vinyl, allyl, propargyl, butenyl, ethynyl, phenylethynyl, maleimide, nadicimide, and (meth)acryloyl. Among these, (meth)acryloyl is preferred from the viewpoint of reactivity and pore resolution.
[0089] As component (E), examples include difunctional monomers having two (meth)acryloyl groups and polyfunctional monomers having three or more (meth)acryloyl groups. Component (E) preferably includes the above-mentioned polyfunctional monomers.
[0090] Examples of the aforementioned difunctional monomers include aliphatic dimethacrylates such as trimethylolpropane dimethacrylate, polypropylene glycol dimethacrylate, and polyethylene glycol dimethacrylate; dimethacrylates with an alicyclic skeleton such as dicyclopentadiene dimethacrylate and tricyclodecanediethanol dimethacrylate; and aromatic dimethacrylates such as 2,2-bis(4-(meth)acryloyloxypolyethoxypolypropoxyphenyl)propane and bisphenol A diglycidyl ether dimethacrylate.
[0091] Examples of the aforementioned multifunctional monomers include trimethylolpropane tri(meth)acrylate and other (meth)acrylate compounds having a skeleton derived from trimethylolpropane; tetramethylolmethane tri(meth)acrylate, tetramethylolmethane tetra(meth)acrylate and other (meth)acrylate compounds having a skeleton derived from tetramethylolmethane; pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate and other (meth)acrylate compounds having a skeleton derived from pentaerythritol; dipentaerythritol penta(meth)acrylate, dipentaerythritol hexa(meth)acrylate and other (meth)acrylate compounds having a skeleton derived from dipentaerythritol; bis(trimethylolpropane tetra(meth)acrylate and other (meth)acrylate compounds having a skeleton derived from bis(trimethylolpropane); and (meth)acrylate compounds having a skeleton derived from diglycerol. From the viewpoints of through-hole resolution and conductor adhesion, (meth)acrylate compounds having a backbone derived from trimethylolpropane, such as trimethylolpropane tri(meth)acrylate, are preferred, and trimethylolpropane tri(meth)acrylate is more preferred. Here, the aforementioned “(meth)acrylate compounds having a skeleton derived from XXX” (where XXX is the name of the compound) refers to the esterification of XXX with (meth)acrylate, which also includes compounds modified with alkoxides.
[0092] (Content of component (E)) When the photosensitive resin composition of this embodiment contains component (E), from the viewpoint of heat resistance and dielectric properties, the content of component (E) in the photosensitive resin composition of this embodiment is preferably 5 to 70% by mass, more preferably 10 to 60% by mass, further preferably 20 to 50% by mass, and particularly preferably 30 to 40% by mass, based on the total amount of resin components in the photosensitive resin composition of this embodiment. From the viewpoint of developability, the content of component (E) in the photosensitive resin composition of this embodiment, based on the total amount of resin components in the photosensitive resin composition of this embodiment, can be 30% by mass or less, 20% by mass or less, 10% by mass or less, 5% by mass or less, or 0% by mass.
[0093] <(F) Inorganic filler materials> The photosensitive resin composition of this embodiment preferably further contains (F) inorganic filler material. The photosensitive resin composition of this embodiment contains (F) inorganic filler material, and tends to further improve the low thermal expansion, heat resistance and flame retardancy of the cured photosensitive resin composition of this embodiment. (F) Inorganic filler materials can be used alone or in combination with two or more.
[0094] Examples of inorganic filler materials (F) include silica, alumina, titanium dioxide, mica, beryllium oxide, barium titanate, potassium titanate, strontium titanate, calcium titanate, aluminum carbonate, magnesium hydroxide, aluminum hydroxide, aluminum silicate, calcium carbonate, calcium silicate, magnesium silicate, silicon nitride, boron nitride, clay, molybdate compounds, talc, aluminum borate, and silicon carbide. Among these, silica and alumina are preferred as inorganic filler materials (F) from the viewpoints of coefficient of thermal expansion, heat resistance, and flame retardancy, with silica being more preferred. Examples of silica include crushed silica, fumed silica, and fused silica. The shape of the inorganic filler material (F) can be, for example, spherical or fragmented, but preferably spherical.
[0095] (F) Volume average particle size of inorganic filler materials (D) 50 The preferred size is 0.01~10μm, more preferably 0.05~5μm, even more preferably 0.1~2μm, even more preferably 0.2~1.5μm, and particularly preferably 0.3~1μm. In addition, in this specification, the volume average particle size (D) 50 The particle size can be determined using a submicron particle analyzer (Beckman Coulter Corporation, trade name: N5) according to the international standard ISO 13321, by measuring the particles dispersed in the solvent with a refractive index of 1.38, and the particle size is calculated as the cumulative value (volume basis) in the particle size distribution.
[0096] From the viewpoints of dielectric properties, chemical resistance, and conductor adhesion, (F) inorganic filler materials can be surface-treated, for example, by surface treatment agents such as coupling agents. When using coupling agents, the treatment method can be either a so-called overall mixing treatment method in which the inorganic filler material is added to the photosensitive resin composition and then the coupling agent is added, or a method of pre-treating the surface with a coupling agent in a dry or wet manner.
[0097] (F) Content of inorganic filler material) When the photosensitive resin composition of this embodiment contains inorganic filler material (F), from the viewpoints of low thermal expansion, heat resistance, flame retardancy, dielectric properties, chemical resistance, and conductor adhesion, the content of inorganic filler material (F) in the photosensitive resin composition of this embodiment, based on the total solid content of the photosensitive resin composition of this embodiment, is preferably 5 to 80% by mass, more preferably 10 to 75% by mass, further preferably 20 to 70% by mass, even more preferably 40 to 65% by mass, and particularly preferably 50 to 60% by mass.
[0098] <(G) Organic Peroxides> The photosensitive resin composition of this embodiment preferably further contains (G) organic peroxide. (G) organic peroxide is a polymerization initiator for the thermal free radical polymerization of olefinic unsaturated groups. The photosensitive resin composition of this embodiment contains (G) organic peroxide, and tends to further improve the dielectric properties and other properties of the cured photosensitive resin composition of this embodiment. (G) Organic peroxides may be used alone or in combination with two or more.
[0099] Examples of (G) organic peroxides include peroxide ketals such as 1,1-di(tert-butylperoxy)cyclohexane, 2,2-di(tert-butylperoxy)butane, 2,2-di(4,4-di-tert-butylperoxycyclohexyl)propane, and 1,1-di(tert-pentylperoxy)cyclohexane; hydroperoxides such as cumene hydroperoxide and tert-butyl hydroperoxide; and alkyl peroxides such as tert-butyl peroxyacetate and tert-pentyl peroxyisononanoate. Dialkyl peroxides such as tert-butyl cumene oxide, di-tert-butyl peroxide, di-isopropylbenzene peroxide, di-tert-hexyl peroxide, and 1,3-di(tert-butylperoxyisopropyl)benzene; peroxide esters such as tert-butyl peroxyacetate, tert-butyl peroxybenzoate, and tert-butyl peroxyisopropyl carbonate; peroxide carbonates such as tert-butyl peroxyisopropyl carbonate and polyether tetra(tert-butyl peroxycarbonate); and diacyl peroxides such as dibenzoyl peroxide. Among these, dialkyl peroxides are preferred, and 1,3-di(tert-butylperoxyisopropyl)benzene is more preferred.
[0100] (Content of organic peroxides (G)) When the photosensitive resin composition of this embodiment contains (G) organic peroxide, from the viewpoints of heat resistance, dielectric properties, chemical resistance, and conductor adhesion, the content of (G) organic peroxide in the photosensitive resin composition of this embodiment is preferably 0.05 to 15 parts by mass relative to 100 parts by mass of the total resin component in the photosensitive resin composition of this embodiment, more preferably 0.1 to 12 parts by mass, further preferably 0.5 to 10 parts by mass, even more preferably 1 to 7 parts by mass, and particularly preferably 2 to 5 parts by mass.
[0101] <(H) Photopolymerization initiator> The photosensitive resin composition of this embodiment preferably further contains a (H) photopolymerization initiator. The photosensitive resin composition of this embodiment tends to have further improved resolution of through-pores by containing a (H) photopolymerization initiator. (H) Photopolymerization initiators can be used alone or in combination with two or more.
[0102] As a (H) photopolymerization initiator, any initiator that can cause the olefin unsaturated group to undergo photopolymerization is acceptable; there are no particular limitations, and it can be appropriately selected from commonly used photopolymerization initiators. Examples of benzoin-based compounds that can serve as (H) photopolymerization initiators include benzoin, benzoin methyl ether, benzoin isopropyl ether, etc.; acetophenone-based compounds such as 2,2-dimethoxy-2-phenylacetophenone, 2,2-diethoxy-2-phenylacetophenone, 1,1-dichloroacetophenone, 1-hydroxycyclohexylphenyl ketone, 2-benzyl-2-dimethylamino-1-(4-morpholinophenyl)-1-butanone, 2-[4-(methylthio)benzoyl]-2-(4-morpholino)propane, N,N-dimethylaminoacetophenone, etc.; and 2-methylanthraquinone, 2-ethylanthraquinone, 2-tert-butylanthraquinone, 1-chloroanthraquinone, 2-pentylanthraquinone, 2 Anthraquinone compounds such as aminoanthraquinone; ketal compounds such as acetophenone dimethyl ketal and benzyl dimethyl ketal; acridine compounds such as 9-phenyl acridine and 1,7-bis(9,9'-acridyl)heptane; acylphosphine oxide compounds such as bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide; oxime ester compounds such as 1,2-octanedione-1-[4-(phenylthio)phenyl]-2-(O-benzoyl oxime), 1-[9-ethyl-6-(2-methylbenzoyl)-9H-carbazole-3-yl] acetophenone 1-(O-acetyl oxime), and 1-phenyl-1,2-propanedione-2-[O-(ethoxycarbonyl)oxime]. From the viewpoint of bottom curing, acylphosphine oxide compounds are preferred, and bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide is more preferred.
[0103] (H) Content of photopolymerization initiator When the photosensitive resin composition of this embodiment contains a (H) photopolymerization initiator, from the viewpoint of easily obtaining a moderate promoting effect on the polymerization reaction, the content of the (H) photopolymerization initiator in the photosensitive resin composition of this embodiment is preferably 0.01 to 10 parts by mass relative to 100 parts by mass of the total resin component in the photosensitive resin composition of this embodiment, more preferably 0.05 to 5 parts by mass, further preferably 0.1 to 1 part by mass, and particularly preferably 0.15 to 0.5 parts by mass.
[0104] <(I) Other ingredients> The photosensitive resin composition of this embodiment may contain (I) other components as needed. Other components, such as resins other than those mentioned above, include curing agents, organic fillers, sensitizers, polymerization inhibitors, pigments, adhesives such as melamine, foam stabilizers such as silicone compounds, thickeners, flame retardants, and organic solvents. Each of them can be used individually or in combination with two or more. The content of other components (I) in the photosensitive resin composition of this embodiment can be adjusted appropriately according to their respective purposes. Each component can be 0.01 to 10% by mass, 0.05 to 5% by mass, or 0.1 to 1% by mass, based on the total amount of solid components in the photosensitive resin composition.
[0105] <Method for manufacturing photosensitive resin composition> The photosensitive resin composition of this embodiment can be obtained by mixing and blending the various components using a roller mill, bead mill, or the like.
[0106] [Photosensitive resin film] The photosensitive resin film of this embodiment comprises the photosensitive resin composition of this embodiment. This photosensitive resin film is useful as a photosensitive layer for forming an interlayer insulating layer. The components and their contents in the photosensitive resin film of this embodiment are as described in the description of the components and their contents in the photosensitive resin composition of this embodiment.
[0107] In this embodiment, the photosensitive resin film can be disposed on a carrier film. Examples of carrier films include polyesters such as polyethylene terephthalate and polybutylene terephthalate; and polyolefins such as polypropylene and polyethylene. The thickness of the carrier film is preferably 5-100 μm, more preferably 10-60 μm, and even more preferably 15-45 μm. In addition, the photosensitive resin film of this embodiment may have a protective film on the side opposite to the side that contacts the carrier film.
[0108] The photosensitive resin film of this embodiment can be formed, for example, by coating a carrier film with the photosensitive resin composition of this embodiment using a known coating apparatus such as a comma-type coating machine, a rod coating machine, a coincidence coating machine, a roller coating machine, a gravure coating machine, or a die coating machine, and then drying it. The coating film formed by applying the photosensitive resin composition can be dried using hot air drying, a dryer utilizing far-infrared or near-infrared light, etc. The drying temperature is preferably 60-150°C, more preferably 70-120°C, and even more preferably 80-110°C. The drying time is preferably 1-60 minutes, more preferably 2-30 minutes, and even more preferably 5-20 minutes. From the viewpoint of preventing the diffusion of diluent during the manufacturing process of the printed wiring board, the residual diluent content in the dried photosensitive resin film is preferably 3% by mass or less, more preferably 2% by mass or less, and even more preferably 1% by mass or less.
[0109] From the viewpoint of making the printed wiring board thinner, the thickness of the photosensitive resin film in this embodiment is preferably 1 to 100 μm, more preferably 3 to 60 μm, and even more preferably 5 to 40 μm.
[0110] Printed wiring board The printed wiring board of this embodiment is a printed wiring board containing a cured product of the photosensitive resin composition of this embodiment. The printed wiring board of this embodiment is preferably a printed wiring board having an interlayer insulating layer that is a cured product of the photosensitive resin film of this embodiment. In addition, the "interlayer insulation layer" of the printed wiring board in this embodiment also includes, for example, layers that have undergone various processing or treatments such as the formation of through holes and wiring, roughening treatment, etc.
[0111] The manufacturing method of the printed wiring board in this embodiment is not particularly limited as long as the method of using the photosensitive resin film of this embodiment is used, but preferably includes the manufacturing method of the printed wiring board including (1) to (4) below. (1): The photosensitive resin film of this embodiment is laminated onto one or both sides of the circuit board (hereinafter also referred to as "lamination process (1)"). (2): By exposing and developing the photosensitive resin film laminated in (1) above, an interlayer insulating layer with through holes is formed (hereinafter also referred to as "through hole forming process (2)"). (3): Heat-cur the above-mentioned interlayer insulation layer with through holes (hereinafter also referred to as "heat curing process (3)"). (4): A circuit pattern is formed on the above interlayer insulating layer (hereinafter also referred to as "circuit pattern forming process (4)").
[0112] The following is for reference only. Figure 1 The manufacturing method of the printed wiring board according to this embodiment will be described. Furthermore, for convenience, the specified operations are sometimes referred to as "XX process" in this specification, but the "XX process" is not limited to the specific methods described in this specification.
[0113] (Lamination process (1)) In the lamination process (1), the photosensitive resin film of this embodiment is laminated onto one or both sides of the circuit board. Figure 1 (a) illustrates the process of forming a photosensitive layer 103 on both sides of a substrate 101 having a circuit pattern 102. The photosensitive layer 103 can be formed by laminating the photosensitive resin film of this embodiment onto both sides of the substrate 101. Lamination can be achieved by using a vacuum laminator or similar machine that applies pressure and heat while simultaneously pressing the laminators together. After lamination, if a carrier film is attached to the photosensitive layer 103, the carrier film can be peeled off before exposure as described later, or it can be peeled off after exposure.
[0114] (Through hole forming process (2)) In the through-hole forming process (2), an interlayer insulating layer with through holes is formed by exposing and developing the photosensitive layer formed in the lamination process (1). Figure 1 (b) illustrates the process of forming an interlayer insulating layer 104 with through-holes 105 by exposing and developing the photosensitive layer 103. By exposing the photosensitive layer 103, a photoradical polymerization reaction is initiated, thereby curing the photosensitive resin film.
[0115] The exposure method of the photosensitive layer 103 can be, for example, a mask exposure method in which active light is irradiated in an image-like manner through a negative or positive mask pattern called a film, or a direct depiction exposure method in which active light is irradiated in an image-like manner through LDI (Laser Direct Imaging) exposure method, DLP (Digital Light Processing) exposure method, or other methods. Examples of known light sources that emit active light include gas lasers such as carbon arc lamps, mercury vapor arc lamps, high-pressure mercury lamps, xenon lamps, and argon lasers; solid-state lasers such as YAG lasers; and semiconductor lasers, which effectively emit ultraviolet or visible light. The exposure amount can be adjusted appropriately according to the light source used and the thickness of the photosensitive layer. For example, when exposing a photosensitive layer with a thickness of 1 to 100 μm to ultraviolet light from a high-pressure mercury lamp, the preferred exposure amount is 10 to 1,000 mJ / cm. 2 More preferably 50~700mJ / cm 2 Further preferred values are 150~400 mJ / cm 2 .
[0116] Next, if a carrier film is present on the photosensitive layer 103, the carrier film is removed and development is performed. During development, the uncured portion of the photosensitive layer 103 is removed, and the photocured portion is formed on the substrate as an interlayer insulating layer 104. The development method can be either wet development or dry development, with wet development being preferred. From the viewpoint of improving resolution, spray development is preferred when using wet development. Examples of developing solutions include alkaline aqueous solutions, aqueous developing solutions, and organic solvent-based developing solutions, with alkaline aqueous solutions being preferred. After exposure and development, post-exposure can be performed to improve the curing degree of the interlayer insulating layer. The preferred exposure dose in post-exposure is 0.2~10 J / cm. 2 More preferably 0.5~5 J / cm 2 .
[0117] There are no particular restrictions on the shape of the through hole. If we describe it in terms of cross-sectional shape, examples include quadrilaterals and inverted trapezoids. Additionally, an inverted trapezoid is a shape where the top side is longer than the bottom side. Furthermore, if we describe it in terms of top view, examples include circles and quadrilaterals. In the formation of through-holes using photolithography in this embodiment, through-holes with an inverted trapezoidal cross-sectional shape can be formed. Through-holes with this shape are preferred because of the high uniformity of copper plating onto the through-hole walls. In the via formation using photolithography in this embodiment, the diameter of the via can be smaller than the diameter of a via formed by laser processing. The diameter of the via formed by the manufacturing method of this embodiment can be, for example, 40 μm or less, 35 μm or less, or 30 μm or less. There is no particular limitation on the lower limit of the via diameter; for example, it can be 15 μm or more, or 20 μm or more.
[0118] (Heat curing process (3)) In the heat curing process (3), the interlayer insulation layer with through holes is heat-cured. That is, in the heat curing process (3), the thermosetting components contained in the photosensitive resin film of this embodiment are cured by heating. The heating temperature is preferably 100~300℃, more preferably 120~200℃, and even more preferably 150~180℃. The heating time is preferably 0.3~3 hours, more preferably 0.5~2 hours, and even more preferably 0.75~1.5 hours.
[0119] (Circuit pattern formation process (4)) Next, a circuit pattern is formed on the interlayer insulating layer formed above. From the viewpoint of forming fine wiring, the circuit pattern is preferably formed by a semi-additive method that sequentially performs roughening treatment, seed layer formation, resist pattern formation, copper circuit layer formation, and resist pattern removal.
[0120] Roughening treatment is a process that roughens the surface of the interlayer insulation layer to form an uneven anchor. In the case of adhesive residue generated in the through-hole forming process (2), a roughening liquid can be used to simultaneously perform roughening treatment and remove the adhesive residue. Examples of roughening liquids include alkaline permanganate roughening liquids such as sodium permanganate roughening liquid; chromium / sulfuric acid roughening liquids; sodium fluoride / chromium / sulfuric acid roughening liquids; etc.
[0121] Figure 1 (c) illustrates the process of forming the seed layer 106. The seed layer 106 is used to form a power supply layer for performing electrolytic copper plating. The seed layer 106 can be formed by chemically plating copper onto the bottom of the via, the wall of the via, and the entire surface of the interlayer insulating layer using a palladium catalyst or the like.
[0122] Figure 1 (d) illustrates the process of forming a resist pattern 107 on the seed layer 106. The resist pattern 107 can be formed, for example, by hot-pressing a dry film resist onto the seed layer 106 using a roller laminator or similar method, followed by exposure and development. Commercially available dry film resists can be used.
[0123] Exposure of the dry film resist can be performed simply by using a mask to draw the desired wiring pattern. After exposure, the dry film resist is developed using an alkaline aqueous solution to remove unexposed areas, forming the resist pattern 107. Then, plasma treatment can be performed as needed to remove developing residues from the dry film resist.
[0124] Figure 1 (e) illustrates the process of forming the copper circuit layer 108. The copper circuit layer 108 is preferably formed by electrolytic copper plating. As for the electrolytic copper plating solution used for electrolytic copper plating, commercially available electrolytic copper plating solutions such as those containing copper sulfate can be used. After electrolytic copper plating, the resist pattern 107 is removed using an alkaline aqueous solution or an amine-based stripper. Then, flash etching to remove the seed layer 106 between the wirings and removal of the palladium catalyst are performed appropriately using known methods. Furthermore, if necessary, a post-baking treatment can be performed to fully heat-cure unreacted thermosetting components.
[0125] Figure 1 (f) shows a multilayer printed wiring board 100A with a solder resist layer 109 on the outermost surface, which is multilayered by repeating the above-described processes. The solder resist layer 109 can be formed using a known photosensitive resin film for solder resists.
[0126] The manufacturing method of a printed wiring board forming through-holes using the photosensitive resin film of this embodiment has been described above. However, since the photosensitive resin film of this embodiment has excellent pattern resolution, it is also suitable for forming cavities for embedded chips or passive components. For example, as described above in the printed wiring board description, the cavity can be appropriately formed by forming the pattern drawn when the photosensitive resin film is exposed to form a pattern into the desired cavity.
[0127] [Semiconductor Package] The semiconductor package of this embodiment is a semiconductor package having the printed wiring board and semiconductor element of this embodiment. The semiconductor package of this embodiment can be manufactured, for example, by mounting semiconductor components such as semiconductor chips and memory at predetermined positions on the printed wiring board of this embodiment, and sealing the semiconductor components with sealing resin or the like. [Example]
[0128] The following embodiments will be described in more detail, but the embodiments are not limited to these embodiments.
[0129] [Methods for determining acid value] The acid value is calculated from the amount of potassium hydroxide aqueous solution required to neutralize the test object.
[0130] [Methods for determining weight-average molecular weight (Mw) and number-average molecular weight (Mn)] The weight-average molecular weight (Mw) and number-average molecular weight (Mn) were determined using the GPC measuring apparatus and conditions described below, and converted using a standard curve of standard polystyrene. The standard curve was prepared using five sample groups (“PStQuick MP-H” and “PStQuick B”, manufactured by Tosoh Corporation) as standard polystyrene. (GPC measuring device) GPC device: High-speed GPC device "HCL-8320GPC", detector is differential refractometer or UV, manufactured by Tosoh Corporation. Chromatographic column: TSKgel SuperMultipore HZ-H column (column length: 15cm, column inner diameter: 4.6mm), manufactured by Tosoh Corporation. (Measurement conditions) Solvent: Tetrahydrofuran (THF) Measurement temperature: 40℃ Flow rate: 0.35 ml / min Sample concentration: 10 mg / THF 5 ml Injection volume: 20 μl
[0131] [Manufacturing of photosensitive resin compositions and photosensitive resin films] Examples 1-7, Comparative Examples 1-2 (1) Preparation of photosensitive resin composition The components were prepared according to the formulation shown in Table 1 (the values in the table are in parts by mass, and the conversion amount is the solid content in the case of solution). The mixture was then kneaded using a three-roll mill and a rotary mixer. Methyl ethyl ketone was then added to achieve a solid content concentration of 65% by mass to obtain the photosensitive resin composition.
[0132] (2) Manufacturing of photosensitive resin film A polyethylene terephthalate film (manufactured by Toyobo Co., Ltd., trade name "TOYOBOESTER HPE") with a thickness of 25 μm was prepared as a carrier film. The photosensitive resin composition prepared in each example was coated on the carrier film to achieve a film thickness of 25 μm after drying, and dried at 100°C for 10 minutes using a hot air convection dryer, thereby forming a photosensitive resin film. Next, a polyethylene film (manufactured by UNITIKA Co., Ltd., trade name "TRFA") is laminated onto the surface of the photosensitive resin film opposite to the side that contacts the carrier film as a protective film, thus producing a photosensitive resin film with a carrier film and a protective film laminated together.
[0133] [Methods for determining relative permittivity (Dk)] Two photosensitive resin films, with their protective films removed, were laminated together and exposed using a flatbed exposure machine at 400 mJ / cm² while still having the carrier films on both sides. 2 Irradiation, using a UV conveyor-type exposure machine at 2J / cm 2 Irradiation. Next, the product was heated at 170°C for 1 hour using a hot air circulating dryer, and then cut into 7cm × 10cm pieces as evaluation samples. The obtained evaluation samples were sealed with a desiccant and dried for at least 10 hours. The relative permittivity (Dk) at 10 GHz was determined using the separated column dielectric resonator method (SPDR method), and the evaluation was based on the following benchmarks. (Evaluation criteria for relative permittivity (Dk)) A: Less than 3.30 B: More than 3.30
[0134] [Determination of minimum development time] The surface of the copper foil on a printed wiring board substrate (manufactured by Risennoko Co., Ltd., trade name "MCL-E-679"), which is made by laminating copper foil (12 μm thick) onto a glass epoxy material, was roughened using a roughening pretreatment solution (manufactured by MEC Co., Ltd., trade name "CZ-8101"). The substrate was then washed and dried. Next, a photosensitive resin film with the protective film removed was laminated onto the copper foil of the roughened printed wiring board substrate, with the photosensitive resin film serving as the adhesive surface. The lamination was performed using a vacuum laminator (manufactured by Meiki Seisakusho Co., Ltd., trade name "MVLP-500"), under the following conditions: vacuum time 20 seconds, pressure 4 kPa or less, lamination pressing time 30 seconds, hot plate temperature 75°C, and pressing pressure 0.4 MPa. After lamination, the substrate is left at room temperature for more than 1 hour to obtain an evaluation laminate in which a photosensitive resin film and a carrier film are sequentially laminated on the copper foil surface of a printed wiring board substrate. The above-obtained evaluation was removed using the carrier film of the laminate, and the photosensitive resin film was spray-developed using a 1% sodium carbonate aqueous solution at 30°C. At this point, the minimum developable time was taken as the minimum development time, and the evaluation was performed based on the following criteria. (Evaluation Criteria) A: The minimum development time is less than 30 seconds. B: The minimum development time is 30 seconds or more but less than 60 seconds. C: Minimum development time exceeds 60 seconds.
[0135] [Evaluation of stickiness] The protective film was peeled off from the photosensitive resin film with carrier film and protective film manufactured in the various embodiments and comparative examples. The exposed surface of the photosensitive resin film was used as the object of adhesion measurement. Adhesion tester (manufactured by RHESCA Co., Ltd., trade name "Tacking Tester TAC-II") was used to measure the adhesion under the following conditions. • Probe: has a tip with a diameter of 0.196 cm 2 flat circular surface 5.1mm stainless steel probe • Pressing load: 100gf • Pressing speed: 120mm / s • Pressing time: 1 second • Lifting speed: 120mm / s • Workbench temperature: 25℃ • Probe temperature: 25℃ The viscosity value obtained by the above method is evaluated based on the following criteria. (Evaluation Criteria) A: Viscosity value is less than 100gf. B: Viscosity value is above 100gf and below 150gf. C: Viscosity value exceeds 150gf.
[0136]
[0137] The ingredients used in Table 1 are described below. [(A) Ingredient] • Compounds containing carboxyl and acryloyl groups: A compound manufactured by Nippon Kayaku Co., Ltd., trade name "ZXR-1807H", acid value: 100 mg KOH / g, weight-average molecular weight (Mw): 2,000, containing carboxyl and acryloyl groups, and comprising the alicyclic skeleton shown in the above general formula (A-1).
[0138] [(B) Component] • Acrylic resin with carboxyl and methacryl groups 1: Manufactured by DAICEL-ALLNEX Co., Ltd., trade name "CYCLOMER P(ACA)Z230AA", weight average molecular weight (Mw): 13000, double bond equivalent (calculated): 450 g / mol, acid value: 40 mg KOH / g • Acrylic resin with carboxyl and methacryl groups 2: Manufactured by DAICEL-ALLNEX Co., Ltd., trade name "CYCLOMER P(ACA)Z251", weight average molecular weight (Mw): 14000, double bond equivalent (calculated): 380 g / mol, acid value: 66 mg KOH / g • Acrylic resins containing carboxyl and methacryl groups 3: Manufactured by DAICEL-ALLNEX Co., Ltd., trade name "CYCLOMER P(ACA)Z200M", weight-average molecular weight (Mw): 12000, double bond equivalent (calculated): 450 g / mol, acid value: 114 mg KOH / g
[0139] [(C) Component] • Maleimide resin: Aromatic bismaleimide resin having an indane skeleton, or a compound represented by the above general formula (C-1). • Allyl resin: diallyl isocyanurate compound, manufactured by Shikoku Chemical Industry Co., Ltd., trade name "L-DAIC", the compound represented by the above general formula (C-2). • Isocyanate resin: Hexamethylene diisocyanate
[0140] [(D) component] • Elastomer 1: Anhydride-modified polybutadiene: manufactured by Cray Valley, trade name "Ricon131MA17", number average molecular weight (Mn): 5,400, number of anhydride groups per molecule: 9 • Elastomer 2: Butadiene-styrene-random copolymer, manufactured by Cray Valley, trade name "Ricon100", number average molecular weight (Mn): 4,500
[0141] [(E) component] Trimethylolpropane triacrylate
[0142] [(F)Component] • Silica: Molten spherical silica, volume average particle size (D) 50 ): 0.5μm
[0143] [(G) component] • Organic peroxide: 1,3-Di(tert-butylperoxyisopropyl)benzene
[0144] [(H) component] Photopolymerization initiator: bis(2,4,6-trimethylbenzoyl)phenylphosphine oxide
[0145] [(I)INGREDIENTS] Sensitizer: 4,4'-bis-(diethylamino)benzophenone Polymerization inhibitor: tert-butylcatechol
[0146] As shown in Table 1, the photosensitive resin compositions of Examples 1 to 7 of this embodiment all exhibit excellent developability and their viscosity is suppressed. Explanation of reference numerals in the attached figures
[0147] 100A Multilayer Printed Wiring Board 101 substrate 102 Circuit Pattern 103 Photosensitive layer 104 interlayer insulation layer 105 Through Hole 106 seed layers 107 Resist Pattern 108 copper circuit layers 109 Solder resist layer
Claims
1. A photosensitive resin composition comprising: (A) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of less than 6000; and (B) Photopolymerizable compounds having olefinic unsaturated groups and acidic substituents and a weight-average molecular weight (Mw) of 6000 or more.
2. The photosensitive resin composition according to claim 1, wherein, The (A) component comprises an alicyclic skeleton.
3. The photosensitive resin composition according to claim 1 or 2, wherein, The component (B) is an acrylic resin having olefinic unsaturated groups and acidic substituents.
4. The photosensitive resin composition according to claim 1 or 2, wherein, The weight-average molecular weight (Mw) of component (A) is 300-5000.
5. The photosensitive resin composition according to claim 1 or 2, wherein, The weight-average molecular weight (Mw) of component (B) is 7,000 to 50,000.
6. The photosensitive resin composition according to claim 1 or 2, wherein, The content of component (B) is 10 to 500 parts by mass relative to 100 parts by mass of component (A).
7. The photosensitive resin composition according to claim 1 or 2, further comprising (C) a thermosetting resin.
8. The photosensitive resin composition according to claim 1 or 2, further comprising (D) an elastomer.
9. The photosensitive resin composition according to claim 1 or 2, used to form an interlayer insulating layer having light-permeable holes.
10. A photosensitive resin film comprising the photosensitive resin composition of claim 1 or 2.
11. A printed wiring board comprising a cured product of the photosensitive resin composition of claim 1 or 2.
12. A semiconductor package comprising the printed wiring board and semiconductor element as described in claim 11.
13. A method for manufacturing a printed wiring board, comprising the following steps (1) to (4): (1): The photosensitive resin film of claim 10 is laminated onto one or both sides of the circuit board; (2): By exposing and developing the photosensitive resin film laminated in (1), an interlayer insulating layer with through holes is formed; (3): Heating and curing the interlayer insulation layer with through holes; (4): A circuit pattern is formed on the interlayer insulating layer.
Citation Information
Patent Citations
Thermosetting resin composition, multilayered printed wiring board, and preparation thereof
JP1995304931A
Photosensitive resin composition, and dry film, printed wiring board and method for manufacturing printed wiring board using the composition