Light-cured additive manufactured lithium disilicate glass ceramic permeable zirconium oxide tooth veneer
Through light-curing additive manufacturing technology, lithium disilicate glass ceramic is used to infiltrate zirconia dental veneers, which solves the problem of reduced strength and increased thickness of dental veneers caused by the sandblasting process, and achieves high-strength, thin-thickness dental veneers. face, protecting the health of teeth and periodontal tissue.
Patent Information
- Application Number
- CN202420123543.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-18
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2034-01-18
AI Technical Summary
The sandblasting process in the existing dental veneer process leads to a reduction in the strength of the tooth veneer, and the increase in thickness requires grinding of the tooth body, which may damage the tooth body and periodontal tissue, posing potential health risks.
Lithium disilicate glass ceramic infiltrated zirconia dental veneers are manufactured using light-curing additives. By setting up surface-increasing through-holes and penetration connections of the adhesive layer in the matrix, a high-strength, thin-thickness dental veneer is formed, avoiding the need for spraying. This eliminates cracking problems in the sand process and reduces the need for grinding of the tooth body.
It improves the strength and service life of dental veneers, reduces damage to the tooth body and periodontal tissue, protects oral health, and achieves a thinner veneer structure.
Smart Images

Figure CN221786710U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to tooth treatment, in particular to a light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconium oxide tooth veneer. Background Art
[0002] Dental veneers are a restorative technology that repairs teeth and restores their whitening. It is mainly used for teeth that have discoloration or partial defects. A layer of material close to the normal tooth color is pasted on the surface of the tooth body, making the veneered teeth look the same as normal teeth, thereby achieving the effect of enhancing the patient's confidence.
[0003] The existing dental veneer is sandblasted on the side close to the tooth body, and then adhesive is applied on the sandblasted side, and then bonded to the tooth body. The advantage of this structure is that the dental veneer has a relatively good fit with the tooth body, but there are also the following problems: 1. Since the essence of the sandblasting process is that the sand particles adhere to the surface of the tooth veneer after hitting the tooth veneer at high speed, cracks will appear on the tooth veneer near the sand particles after the sandblasting process, which leads to a decrease in the strength of the tooth veneer after the sandblasting process; 2. The position of the sand particles is random during the sandblasting process, and the cracks caused by the collision of two adjacent sand particles are likely to be connected, thereby forming a longer crack, further reducing the strength of the dental veneer; 3. The overall thickness of the dental veneer after the sandblasting process is relatively thick. In order to fit on the tooth body, the tooth body needs to be ground. During the grinding process, the tooth body, pulp and periodontal tissue may be damaged, which poses a potential risk to the long-term health of the oral cavity. Summary of the invention
[0004] Purpose of the utility model: The purpose of the utility model is to provide a light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer with high strength and thin overall thickness.
[0005] Technical solution: The utility model discloses a photocuring additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer, comprising a substrate and a bonding layer, wherein the side of the substrate close to the bonding layer is a bonding surface, and the bonding layer and the bonding surface are connected by adhesion; the end surface of the substrate opposite to the bonding layer is a top surface, and a plurality of surface-adding through holes are provided in the substrate, and the two ends of the surface-adding through holes respectively penetrate the bonding surface and the top surface; a plurality of bonding protrusions are arranged on a side of the bonding layer close to the substrate, and the bonding protrusions are embedded in the surface-adding through holes.
[0006] Furthermore, the substrate is composed of a plurality of monomer layers stacked in sequence from bottom to top, and each of the monomer layers is composed of a plurality of component monomers fixedly connected end to end.
[0007] Furthermore, vertex protrusions are respectively arranged on the left and right sides of the component monomers, and the vertex protrusions of two adjacent component monomers in the same monomer layer are connected end to end.
[0008] Furthermore, a plurality of through holes are provided in the component monomer.
[0009] Furthermore, the component monomers in the upper and lower monomer layers are arranged in a staggered manner, and the pores enclosed by the top corner protrusions of two adjacent component monomers in the upper monomer layer correspond to the positions of the through holes of the component monomers in the lower monomer layer.
[0010] Furthermore, the component monomer is a regular octahedron. The regular octahedron includes six vertices, and the vertices of two adjacent regular octahedrons are connected so that the two adjacent regular octahedrons are connected end to end, and a gap is formed after the two adjacent regular octahedrons are connected, and several layers of gaps are stacked to form a surface-increasing through hole.
[0011] Furthermore, the material of the bonding layer is lithium disilicate glass ceramic.
[0012] Furthermore, the lithium disilicate glass ceramic includes silicon dioxide, lithium oxide, phosphorus pentoxide and potassium oxide, wherein the mass proportion of silicon dioxide is 59-70%, the mass proportion of lithium oxide is 14-18%, the mass proportion of phosphorus pentoxide is 3-5%, and the mass proportion of potassium oxide is 3-5%. At 1500°C, the lithium disilicate glass ceramic can better penetrate into the surface-increasing through-holes of zirconium dioxide, thereby having better bonding strength.
[0013] Furthermore, the end surface of the bonding protrusion extending into the surface-increasing through hole is flush with the top surface of the base.
[0014] Furthermore, the thickness of the substrate is 300-800 microns.
[0015] Furthermore, the material of the substrate is zirconium oxide.
[0016] Furthermore, the material of the matrix is 3Y-TZP (ie, 3 mol% yttrium-stabilized tetragonal zirconia).
[0017] Beneficial effects: Compared with the prior art, the utility model has the following advantages: 1. The utility model has only two parts, a substrate and an adhesive layer, and the adhesive layer extends into the surface-increasing through hole of the substrate through an infiltration process and is adhesively connected to the substrate. Compared with the traditional substrate-surface-increasing structure (such as sandblasting or surface-increasing protrusions)-adhesive layer structure, the thickness of the utility model is thinner, so there is no need to grind too much tooth body before bonding, which protects the tooth body, pulp and periodontal tissue, and is more friendly to the long-term health of the oral cavity; 2. In the utility model, the substrate is prepared by a light-curing additive manufacturing process to ensure the integrity of the substrate and avoid creating cracks on the end face of the substrate, thereby improving the strength of the tooth veneer. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 This is an explosion diagram of the utility model.
[0019] Figure 2 FIG. 4 is a cross-sectional view of the base body in the first embodiment.
[0020] Figure 3 It is an enlarged view of a monomer layer of the substrate in the second embodiment.
[0021] Figure 4 It is an enlarged view of the component monomer in the second embodiment.
[0022] Figure 5 It is an enlarged view of a monomer layer of the substrate in the third embodiment.
[0023] Figure 6 It is an enlarged view of the component monomer in the third embodiment.
[0024] Wherein: 1. substrate; 101. first surface-increasing through hole; 102. second component monomer; 1021. top corner protrusion; 1022. through hole; 103. third component monomer; 2. adhesive layer. DETAILED DESCRIPTION
[0025] The technical solution of the utility model is further described below in conjunction with the accompanying drawings.
[0026] Example 1
[0027] See attached Figure 1 and Figure 2 The utility model shows a light-curing additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer, comprising a substrate 1 and a bonding layer 2, wherein the side of the substrate 1 close to the bonding layer 2 is a bonding surface, and the bonding layer 2 is connected to the bonding surface by adhesion; the end surface of the substrate 1 opposite to the bonding layer 2 is a top surface, and a plurality of first surface-increasing through holes 101 are provided in the substrate 1, and the direction of the first surface-increasing through holes 101 is perpendicular to the bonding surface or the top surface, and the two ends of the first surface-increasing through holes 101 directly penetrate the bonding surface and the top surface respectively; a plurality of bonding protrusions are arranged on a side of the bonding layer 2 close to the substrate 1, and the bonding protrusions extend into the first surface-increasing through holes 101 and are embedded with the first surface-increasing through holes 101, and the end surface of the bonding protrusion extending into the first surface-increasing through holes 101 is flush with the top surface of the substrate 1.
[0028] The thickness of the substrate 1 is 350, the material of the substrate 1 is 3Y-TZP (i.e. 3 mol% yttrium stabilized tetragonal zirconia), and the material of the bonding layer 2 is glass ceramic.
[0029] The advantage of this embodiment is that it is easy to prepare, but the disadvantages are also obvious: first, the vertical first surface-increasing through hole 101 will reduce the strength of the tooth veneer; second, the bonding area between the adhesive layer 2 and the substrate 1 is actually not large, and it is very likely that the tooth veneer will fall off after a period of use.
[0030] Example 2
[0031] See attached Figure 1 , Figure 3 and Figure 4 A photocuring additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer includes a substrate 1 and a bonding layer 2, wherein the side of the substrate 1 close to the bonding layer 2 is a bonding surface, and the bonding layer 2 is connected to the bonding surface by adhesion; the end surface of the substrate 1 opposite to the bonding layer 2 is a top surface.
[0032] The substrate 1 is composed of several monomer layers stacked in sequence from bottom to top, each monomer layer is composed of several second component monomers 102 fixedly connected end to end, the left and right sides of the second component monomer 102 are respectively provided with top corner protrusions 1021, the top corner protrusions 1021 of two adjacent second component monomers 102 in the same monomer layer are connected end to end, and a plurality of through holes 1022 are provided in the second component monomer 102, the second component monomers 102 in the upper and lower monomer layers are arranged in a staggered manner, and the adjacent two second component monomers in the upper monomer layer are arranged in a staggered manner. The pores enclosed by the top corner protrusions 1021 of the monomer 102 correspond to the positions of the through holes 1022 of the second component monomer 102 in the lower monomer layer. After stacking, the top corner protrusions 1021 and the through holes 1022 in the same longitudinal direction form an increased surface through hole, and the two ends of the increased surface through hole respectively penetrate the bonding surface and the top surface; a plurality of bonding protrusions are arranged on one side of the bonding layer 2 close to the substrate 1, and the bonding protrusions extend into the increased surface through hole and are embedded with the increased surface through hole, and the end face of the bonding protrusion extending into the increased surface through hole is flush with the top surface of the substrate 1.
[0033] The thickness of the substrate 1 is 500 microns. The material of the substrate 1 is 3Y-TZP (i.e., 3 mol% yttrium-stabilized tetragonal zirconia), and the material of the bonding layer 2 is glass ceramic.
[0034] The advantages of this embodiment are: 1. The base 1 is integrated and has relatively high strength; 2. The bonding area between the surface-enhanced through hole formed by the top angle protrusion 1021 and the through hole 1022 in the same longitudinal direction and the bonding layer 2 is relatively large, which makes the service life of the dental veneer relatively long; 3. The overall thickness of the dental veneer is relatively thin, and there is no need to grind too much tooth body before bonding, which protects the tooth body, pulp and periodontal tissue, and is more friendly to the long-term health of the oral cavity. Although the structure is more complicated than the traditional structure, it is technically feasible to prepare the base 1 of this structure with the help of light-curing additive manufacturing process.
[0035] Example 3
[0036] See attached Figure 1 , Figure 5 and Figure 6 A photocuring additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer includes a substrate 1 and a bonding layer 2, wherein the side of the substrate 1 close to the bonding layer 2 is a bonding surface, and the bonding layer 2 is connected to the bonding surface by adhesion; the end surface of the substrate 1 opposite to the bonding layer 2 is a top surface.
[0037] The substrate 1 is composed of several layers of monomers stacked in sequence from bottom to top, and each layer of monomers is fixedly connected end to end by several third component monomers 103. The third component monomer 103 is a regular octahedron, and the regular octahedron includes six vertices. The vertices of two adjacent third component monomers 103 are connected so that the two adjacent regular octahedra are connected end to end. After the two adjacent regular octahedra are connected, a gap will be formed. Several layers of gaps are stacked to form a surface-increasing through hole, and the two ends of the surface-increasing through hole respectively penetrate the bonding surface and the top surface; a plurality of bonding protrusions are arranged on a side of the bonding layer 2 close to the substrate 1. After penetration, the bonding protrusions extend into the surface-increasing through hole and are embedded with the surface-increasing through hole, and the end face of the bonding protrusion extending into the surface-increasing through hole is flush with the top surface of the substrate 1.
[0038] The thickness of the substrate 1 is 750 micrometers. The material of the substrate 1 is 3Y-TZP (i.e., 3 mol% yttrium-stabilized tetragonal zirconia), and the material of the bonding layer 2 is glass ceramic.
[0039] The advantages of this embodiment are: 1. The base 1 is integrated and has relatively high strength; 2. The bonding area between the surface-increasing through hole formed by connecting the tops of the regular octahedrons in the same longitudinal direction and the bonding layer 2 is relatively large, which makes the service life of the dental veneer relatively long; 3. The overall thickness of the dental veneer is relatively thin, and there is no need to grind too much of the tooth body before bonding, which protects the tooth body, pulp and periodontal tissue, and is more friendly to the long-term health of the oral cavity. Although the structure is more complex than the traditional structure, it is technically possible to prepare the base 1 of this structure with the help of light-curing additive manufacturing process.
Claims
1. A light-curing additive manufacturing method for lithium disilicate glass ceramic infiltrated zirconia dental veneer, characterized in that: The invention comprises a substrate (1) and an adhesive layer (2), wherein a side of the substrate (1) close to the adhesive layer (2) is an adhesive surface, and the adhesive layer (2) is connected to the adhesive surface by adhesion; an end surface of the substrate (1) opposite to the adhesive layer (2) is a top surface, a plurality of surface-increasing through holes are provided in the substrate (1), and two ends of the surface-increasing through holes respectively penetrate the adhesive surface and the top surface; and a plurality of adhesive protrusions are provided on a side of the adhesive layer (2) close to the substrate (1), and the adhesive protrusions are engaged with the surface-increasing through holes.
2. A light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 1, characterized in that: The substrate (1) is composed of a plurality of monomer layers stacked in sequence from bottom to top, and each monomer layer is composed of a plurality of component monomers fixedly connected end to end.
3. A light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 2, characterized in that: The left and right sides of the component monomers are respectively provided with vertex protrusions, and the vertex protrusions of two adjacent component monomers in the same monomer layer are connected end to end.
4. A light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 3, characterized in that: A plurality of through holes are provided in the component monomer.
5. A light-cured additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 4, characterized in that: The component monomers in the upper and lower monomer layers are arranged in a staggered manner, and the pores enclosed by the top corner protrusions of two adjacent component monomers in the upper monomer layer correspond to the positions of the through holes of the component monomers in the lower monomer layer.
6. The light-curing additive manufacturing method of lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 2, characterized in that: The component monomers are in the form of regular octahedrons, and the top points of two adjacent regular octahedrons are connected so that the two adjacent regular octahedrons are connected end to end.
7. The light-curing additive manufacturing method of lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 1, characterized in that: The material of the bonding layer (2) is lithium disilicate glass ceramic, and the material of the substrate (1) is zirconium oxide.
8. The light-curing additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 1, characterized in that: The end surface of the bonding protrusion extending into the surface-increasing through hole is flush with the top surface of the base body (1).
9. The light-curing additively manufactured lithium disilicate glass ceramic infiltrated zirconia dental veneer according to claim 1, characterized in that: The thickness of the substrate (1) is 300-800 microns.