Novel repairing structure for prolonging service life of brick steel ladle molten pool wall

By retaining the remaining bricks after the ladle molten pool wall is eroded and using vibration casting technology to form the repair layer, combined with supporting the tire membrane, the problem of material waste and unevenness in the repair of the brick ladle molten pool wall is solved, and efficient The repair effect extends the service life of the ladle molten pool wall.

CN221791015UActive Publication Date: 2024-10-01YANSHI ZHONGYUE REFRACTORY MATERIALS
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323444732.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-18
Publication Date
2024-10-01
Estimated Expiration
2033-12-18

AI Technical Summary

Technical Problem

In the existing technology, the repair of brick ladle molten pool walls has the problems of material waste, unevenness and poor sintering performance, and there is a lack of effective sleeve casting technology to extend the life of the brick ladle molten pool walls.

Method used

The remaining bricks are retained after the ladle molten pool wall is eroded, and the vibration casting technology is used to form a castable repair layer in the eroded area. Combined with the support tire membrane to improve the bonding density and erosion resistance of the repair layer and the remaining bricks, forming an integrated structure .

Benefits of technology

It effectively extends the life of the brick ladle molten pool wall, saves materials, avoids waste caused by re-building, improves the bonding strength and thermal shock resistance after repair, and avoids loose bonding and cracking after casting.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221791015U_ABST
    Figure CN221791015U_ABST
Patent Text Reader

Abstract

The utility model provides a novel repairing structure for prolonging the service life of a brick steel ladle molten pool wall, which comprises a steel ladle molten pool wall brick positioned on one side of a steel facing surface of a steel ladle molten pool area, and the steel ladle molten pool wall brick is of an annular masonry forming structure in a steel ladle; an erosion area which is eroded by molten steel and steel slag after a steel ladle is used for a period of time is arranged on the inner wall of the steel ladle molten pool wall brick, a pouring material repairing layer is formed in the erosion area through vibration pouring, and the pouring material repairing layer after vibration pouring and a residual brick erosion layer are tightly combined in the high-temperature using environment of the steel ladle. After the molten pool wall of the brick steel ladle is eroded, the residual brick erosion layer of the molten pool wall is reserved, the process is simplified, the cost is saved, the reuse of the repaired steel ladle is not influenced, the castable is formed in the erosion area position in a bush casting mode, and the service life of the ladle is prolonged. And the problem of material loss caused by shoveling off the eroded brick bales for re-building is avoided, and meanwhile, the phenomena of loose combination and cracking after pouring are also avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of steel ladles, and in particular relates to a novel repair structure for extending the service life of a molten pool wall of a brick-built steel ladle. Background Art

[0002] In the process of steel smelting, the ladle is one of the important equipment for storing, transporting and heating molten steel. The ladle pool wall is an important equipment for storing and smelting molten steel. However, during long-term use, the pool wall will be affected by various factors, causing its refractory materials to be eroded and damaged. Once the refractory materials are damaged, it will not only affect the life of the ladle, but may also cause safety hazards to steel production. In recent years, the ladle pool wall tends to use brick masonry instead of the previous integral casting. This means that the ladle pool wall needs to be scraped off and rebuilt after being eroded, which greatly increases the consumption of refractory materials.

[0003] Currently, the repair of brick-built ladle molten pool walls is a hot topic of research, and researchers have tried to use gunning for repair. However, the gunning repair method has significant disadvantages, including (1) material rebound and splashing during construction, resulting in material waste; (2) uneven gunning and difficulty in controlling thickness; (3) poor sintering performance due to excessive micropowder content during the gunning process.

[0004] After the original non-brick ladle structure melt pool wall is eroded, the original refractory can be retained by using the cast-in-place technology, which saves the use of refractory materials and directly reduces the use of refractory materials. However, there is no report on the cast-in-place technology for the melt pool wall of the brick-built ladle. This is because the residual brick structure of the melt pool wall is easy to loosen, fall off and have uneven composition during the cleaning process, and the cast-in-place is easy to be loosely combined or even cracked. Therefore, a new repair structure that can extend the life of the brick-built ladle melt pool wall is urgently needed to solve the above problems. Utility Model Content

[0005] In order to solve the above technical problems, the utility model provides a novel repair structure for extending the service life of the brick-built ladle molten pool wall. After the brick-built molten pool wall is eroded, the castable is formed in the eroded area by means of sheath casting while retaining the eroded layer of residual bricks on the molten pool wall, thereby avoiding the problem of material loss caused by shoveling away the eroded bricks for re-building, and also avoiding the phenomenon of loose bonding and cracking after sheath casting.

[0006] The technical solution adopted by the utility model is: a new type of repair structure for extending the life of a brick-built ladle molten pool wall, comprising ladle molten pool wall bricks located in the ladle molten pool area, the ladle molten pool wall bricks are an annular masonry molding structure in the ladle, the inner wall position of the ladle molten pool wall bricks has an erosion zone that is eroded by molten steel and slag after the ladle has been used for a period of time, a castable repair layer is vibrated and casted at the erosion zone position, the castable repair layer after vibration casting is tightly combined with the residual brick erosion layer in the high-temperature use environment of the ladle, so that the castable repair layer and the ladle molten pool wall form an integrated structure.

[0007] The utility model innovatively adopts a supported membrane, and castable is poured between the membrane and the ladle molten pool wall bricks and vibrated to form; the castable and the residual bricks after vibration forming are tightly combined in the high-temperature use environment of the ladle, forming a pinning effect and a wrapping effect, especially improving the steel surface's resistance to molten steel corrosion and thermal shock resistance, while improving the bonding density, bonding strength, thermal shock resistance and erosion resistance of the bonding surface between the residual bricks and the castable, forming an integrated structure of the repair layer and the ladle molten pool wall.

[0008] The residual brick erosion layer is located between the castable repair layer and the ladle molten pool wall bricks.

[0009] The beneficial effects of the utility model are:

[0010] The utility model retains the eroded layer of the residual bricks of the molten pool wall after the molten pool wall of the brick-built ladle is eroded, thereby simplifying the process, saving costs, and not affecting the reuse of the repaired ladle. The castable is formed in the eroded area by the sheathing method, avoiding the problem of material loss caused by shoveling away the eroded bricks for re-building, and also avoiding the phenomenon of loose bonding and cracking after sheathing. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a schematic diagram of the structure of the utility model;

[0012] Figure 2 It is a schematic diagram of the casting process of the utility model.

[0013] Markings in the figure: 1. Ladle molten pool wall bricks; 2. Residual brick erosion layer; 3. Erosion area; 4. Castable material repair layer; 5. Fetal membrane; 6. Slag line bricks; 7. Ladle bottom bricks; a. Slag line area; b. Molten pool area; c. Ladle bottom area. Implementation

[0014] The specific implementation of the utility model is further described in detail below with reference to the accompanying drawings.

[0015] As shown in the figure, a new type of repair structure for extending the life of a brick-built ladle melt pool wall comprises a ladle melt pool wall brick 1 located in the ladle melt pool area b, the ladle melt pool wall brick 1 is a ring-shaped masonry structure in the ladle, the inner wall position of the ladle melt pool wall brick 1 has an erosion zone 3 which is eroded by molten steel and slag after the ladle has been used for a period of time, a castable repair layer 4 is formed by vibration casting at the erosion zone 3, the castable repair layer 4 after vibration casting is tightly combined with the residual brick erosion layer 2 in the high-temperature use environment of the ladle, so that the castable repair layer 4 and the ladle melt pool wall 1 form an integrated structure.

[0016] The residual brick erosion layer 2 is located between the castable repair layer 4 and the ladle molten pool wall bricks 1. When the castable erosion layer 4 is not cast, the residual brick erosion layer 2 is integrally connected to the ladle molten pool wall bricks 1. It is the part that is corroded when the ladle molten pool wall bricks 1 come into contact with molten steel and slag.

[0017] like Figure 2 As shown in FIG. 1 , the interior of the overall ladle includes the bottom area c at the bottom, the slag line area a above the inner wall of the ladle facing the steel surface, and the molten pool area b below the inner wall of the ladle facing the steel surface. Figure 1 As shown, the bottom bricks 7 are built at the bottom area c, the ladle molten pool wall bricks 1 are built at the molten pool area b, and the slag line bricks 6 are built at the slag line area a (specifically built above the ladle molten pool wall bricks 1). During use, due to the erosion and scouring of molten steel and steel slag, the surface of each area will be eroded to a certain extent. Among them, the slag line bricks 6 and the bottom bricks 7 can be knocked off and rebuilt after being eroded. If the ladle molten pool wall bricks 1 in the molten pool area b are knocked off and rebuilt, it will cause huge material waste and high economic cost. Therefore, this embodiment adopts the method of casting in the eroded area 3 to repair the ladle molten pool wall bricks 1.

[0018] More specifically, after the traditional ladle melt pool wall bricks 1 are corroded, on the one hand, an erosion zone 3 will be formed at the inner wall position of the ladle melt pool wall bricks 1, and on the other hand, a residual brick erosion layer 2 will be formed at the position where the molten steel contacts the ladle melt pool wall bricks 1. In this embodiment, the residual brick erosion layer 2 is retained (the traditional method is to grind off the residual brick erosion layer 2, but after grinding, the connection stability between the remaining residual bricks becomes poor, which will affect the service life of the ladle after the casing is cast), and only a simple cleaning is required before casing casting. During casing casting, the fetal membrane 5 is placed inside the ladle, and then the mixed casting material is introduced into the erosion zone 3. The casting material is expelled from the internal gas by the vibration molding technology. After the casting material is solidified, the fetal membrane 5 is taken out, thereby forming a casting material repair layer 4 inside the ladle melt pool wall bricks 1, completing the entire casing casting process. This casing casting method can solve the problems of the traditional brick-built ladle being unable to be casing cast, the casing casting being loose, and the cracking after casing casting.

[0019] More specifically, the novel repair structure for extending the life of the brick-built ladle molten pool wall mainly includes the following steps:

[0020] Step 1: Clean the ladle molten pool wall bricks 1, and remove the easily peeling residues on the surface of the residual bricks by manual and mechanical methods;

[0021] Step 2: Support the mold 5, the distance between the supported mold 5 and the molten pool wall (i.e. the inner wall position of the ladle molten pool wall brick 1 in the complete state) is 2-15 cm;

[0022] Step 3: prepare the casting material and perform vibration casting between the fetal membrane 5 and the ladle molten pool wall brick 1;

[0023] Step 4: After curing, demoulding and baking, the cast-in repair is completed to complete the entire repair process.

Claims

1. A new type of repair structure for extending the life of the brick-built ladle molten pool wall, characterized by: It includes ladle melt pool wall bricks located in the ladle melt pool area. The ladle melt pool wall bricks are annular masonry molding structure in the ladle. The inner wall position of the ladle melt pool wall bricks has an erosion zone that is eroded by molten steel and slag after the ladle has been used for a period of time. The erosion zone position is vibrated and castable repair layer is formed. The vibrated castable repair layer and the residual brick erosion layer are tightly combined in the high-temperature use environment of the ladle, so that the castable repair layer and the ladle melt pool wall form an integrated structure.

2. A novel repair structure for extending the life of a brick-built ladle molten pool wall according to claim 1, characterized in that: The residual brick erosion layer is located between the castable repair layer and the ladle molten pool wall bricks.

Citation Information

Cited By

  • Brick steel ladle molten pool wall bush casting repairing method

    CN117655312A