3D printing Alsi10Mg material natural color conductive oxidation device
By using sandblasting, sodium hydroxide cleaning and potassium permanganate oxidizing solution treatment during the oxidation process of 3D printing Alsi10Mg material, the problem of blackening after oxidation caused by silicon residue on the surface in the traditional process was solved, and the surface retention of aluminum alloy materials was achieved. The original color does not become gray or black.
Patent Information
- Application Number
- CN202420418391.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-05
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2034-03-05
AI Technical Summary
The traditional aluminum alloy natural color conductive oxidation process cannot effectively remove the silicon on the surface of Alsi10Mg material during alkali etching and pickling, resulting in the surface turning black after oxidation. Improvements are needed to achieve the surface retaining the original color of the aluminum alloy material without becoming gray or black.
A device for 3D printing natural conductive oxidation of Alsi10Mg material is designed, including sandblasting equipment, alkaline box, pickling box and natural conductive oxidation box. It is cleaned by quartz sand blasting, sodium hydroxide cleaning and hydrofluoric acid cleaning. Treated with potassium permanganate oxidizing solution to form a dense oxide film to remove surface silicon and dirt.
It successfully solved the problem of Alsi10Mg material retaining the original color of the aluminum alloy material after its natural conductive oxidation, avoiding the surface turning gray or black after oxidation, and achieving the effectiveness of surface treatment.
Smart Images

Figure CN221822363U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of alloy surface treatment, and specifically to a device for 3D printing natural color conductive oxidation of Alsi10Mg materials. Background Art
[0002] Alsi10Mg material has the characteristics of high strength, good thermal and electrical conductivity, easy processing, low price, etc., and has been widely used in aerospace, automobile and other fields. Alsi10Mg material itself will be oxidized in the natural environment, but the oxide film is only 5-200nm. It is easy to be damaged by bumps or scratches, so surface treatment must be done before it can become a finished product.
[0003] The patent with announcement number CN102485957A discloses a method of using an electrical contact protective agent to seal the conductive oxidation of aluminum. The method includes: dipping the aluminum parts into the SP-2178C protective agent and soaking for 2-5 minutes; the dipping temperature is controlled at 20-50°C; brushing: using a clean and dry soft brush, apply the protective agent evenly on the surface of the parts, and the gaps of the parts must be brushed thoroughly; drying naturally or drying with hot air or drying at a temperature not exceeding 120°C. In particular, butyl ether humidification salt or propyne humidification salt is added to the SP-2178C protective agent in an amount of 0.06-0.1g / L, and the dipping temperature is controlled at 25-40°C.
[0004] However, in the implementation of relevant technologies, it was found that the above technical solution had the following problems: in the process of 3D printing Alsi10Mg used in the above device, the Si content was 10%, and the traditional natural color conductive oxidation process of aluminum alloy did not remove the silicon on the surface during the alkaline etching and pickling process, resulting in the blackening of the surface after oxidation. Therefore, it is necessary to improve the existing natural color conductive oxidation process to achieve the purpose of natural color conductive oxidation of Alsi10Mg material. Therefore, further improvement is needed. Utility Model Content
[0005] The utility model proposes a device for 3D printing the natural color conductive oxidation of Alsi10Mg material, which solves the problem in the related art that it is inconvenient to realize the natural color conductive oxidation of Alsi10Mg material so that the surface retains the natural color of the aluminum alloy material without changing to gray or black.
[0006] The technical solution of the utility model is as follows:
[0007] A device for 3D printing natural color conductive oxidation of Alsi10Mg material, comprising a part body, a sandblasting device is provided on one side of the part body, an alkali box is connected to one side of the sandblasting device, a first water washing box is connected to one side of the alkali box, a pickling box is connected to one side of the first water washing box, a natural color conductive oxidation box is connected to one side of the pickling box, a second water washing box is connected to one side of the natural color conductive oxidation box, and an air pump is provided on one side of the second water washing box.
[0008] Preferably, heaters are fixedly provided inside the alkaline tank, the first water washing tank, the acid washing tank and the natural color conductive oxidation tank, and the heaters are externally connected to a temperature controller via a wire.
[0009] Preferably, quartz sand is arranged inside the sandblasting equipment.
[0010] Preferably, a sodium hydroxide cleaning solution is provided inside the alkaline box, and the sodium hydroxide cleaning solution is composed of sodium hydroxide with a concentration of 50-60 g / L.
[0011] Preferably, first deionized water is provided inside the first water washing box.
[0012] Preferably, a hydrofluoric acid cleaning solution is provided inside the pickling box, and the hydrofluoric acid cleaning solution is composed of hydrofluoric acid with a concentration of 3-5%.
[0013] Preferably, a potassium permanganate oxidizing solution is arranged inside the true color conductive oxidizing box, one side of the true color conductive oxidizing box is externally connected to a stable constant voltage power supply through a wire, and the potassium permanganate oxidizing solution consists of potassium permanganate with a concentration of 5%.
[0014] Preferably, the second water washing box is provided with second deionized water, and the second deionized water is deionized water at room temperature.
[0015] The working principle and beneficial effects of the utility model are:
[0016] The utility model sandblasts a part body through quartz sand, then corrodes the part body in a sodium hydroxide cleaning solution for 30-60 seconds, then cleans the part body twice in a first deionized water, then soaks the part body in a hydrofluoric acid cleaning solution for 3-5 minutes, then oxidizes the part body in a potassium permanganate oxidizing solution for 3-5 minutes, then cleans the part body in a second deionized water for 1-3 minutes, and finally blows the part body dry with an air pump, thereby solving the problem that it is inconvenient to realize that after the Alsi10Mg material is oxidized in its original color, the original color of the aluminum alloy material is retained on the surface without changing to gray or black. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The utility model is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0018] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0019] Figure 2 This is a process flow chart of the natural color conductive oxidation of Alsi10Mg material of the utility model.
[0020] In the figure: 1. part body; 2. sandblasting equipment; 21. quartz sand; 3. alkaline box; 31. sodium hydroxide cleaning solution; 4. first water washing box; 41. first deionized water; 5. pickling box; 51. hydrofluoric acid cleaning solution; 6. natural color conductive oxidation box; 61. potassium permanganate oxidation solution; 62. stable constant voltage power supply; 7. second water washing box; 71. second deionized water; 8. heater; 81. temperature controller; 9. air pump. DETAILED DESCRIPTION
[0021] The following will be combined with the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0022] like Figure 1 and Figure 2 As shown, this embodiment proposes a device for 3D printing natural color conductive oxidation of Alsi10Mg material, including a part body 1, a sandblasting device 2 is provided on one side of the part body 1, an alkali box 3 is connected to one side of the alkali box 3, a first water washing box 4 is connected to one side of the first water washing box 4, a pickling box 5 is connected to one side of the pickling box 5, a natural color conductive oxidation box 6 is connected to one side of the natural color conductive oxidation box 6, a second water washing box 7 is connected to one side of the second water washing box 7, an air pump 9 is provided on one side of the second water washing box 7, and the air pump 9 is used to remove deionized water on the surface of the part body 1.
[0023] Furthermore, heaters 8 are fixedly installed inside the alkaline tank 3, the first water washing tank 4, the acid washing tank 5 and the natural color conductive oxidation tank 6, and the heaters 8 are externally connected to a temperature controller 81 through a wire.
[0024] Furthermore, quartz sand 21 is arranged inside the sandblasting equipment 2 , and the quartz sand 21 of the sandblasting equipment 2 is used to remove surface scratches, processing marks, stains, etc. for the part body 1 .
[0025] Furthermore, a sodium hydroxide cleaning solution 31 is provided inside the alkaline box 3. The sodium hydroxide cleaning solution 31 is composed of sodium hydroxide with a concentration of 50-60 g / L. The sodium hydroxide cleaning solution 31 is used to prevent oxidation and contamination of the surface of the part body 1. The purpose of the alkaline type is to remove oil and oxide scale on the surface of the part body 1.
[0026] Furthermore, the first water washing box 4 is provided with first deionized water 41 , and the purpose of the first deionized water 41 is to remove the sodium hydroxide remaining on the surface of the component body 1 .
[0027] Furthermore, a hydrofluoric acid cleaning solution 51 is provided inside the pickling box 5. The hydrofluoric acid cleaning solution 51 is composed of hydrofluoric acid with a concentration of 3-5%. The purpose of pickling with the hydrofluoric acid cleaning solution 51 is to remove silicon on the surface of the part body 1 and prevent the surface of the part body 1 from blackening during the oxidation stage.
[0028] Furthermore, a potassium permanganate oxidizing liquid 61 is arranged inside the natural color conductive oxidizing box 6, and one side of the natural color conductive oxidizing box 6 is externally connected to a stable constant voltage power supply 62 through a wire. The potassium permanganate oxidizing liquid 61 is composed of potassium permanganate with a concentration of 5%. The purpose of oxidation of the potassium permanganate oxidizing liquid 61 is to form a 5-20 micron dense oxide film on the surface of the aluminum alloy using chemical principles.
[0029] Furthermore, the second water washing box 7 is provided with second deionized water 71 inside. The second deionized water 71 is deionized water at room temperature. The second deionized water 71 is used to clean the oxidizing liquid on the surface of the part body 1 .
[0030] The working principle and instructions for use of the utility model are as follows: when it is necessary to perform sandblasting and surface treatment on the part body 1, first the staff needs to take out the part body 1, and then the staff needs to place the part body 1 in the sandblasting equipment 2. The sandblasting equipment 2 uses quartz sand 21 to sandblast the part body 1. At this time, the oxide scale, oil stains, etc. on the surface of the part body 1 can be removed. The sandblasting parameters are: 20-60 mesh brown corundum, the sandblasting pressure is 0.3-0.5Mpa, and the number of sandblasting times is less than 3 times. Then the staff places the sandblasted part body 1 in the alkaline box 3 for corrosion for 30-60 seconds to remove the passivation layer, oil stains, impurities, etc., and the temperature controller 81 is used to maintain the temperature of the sodium hydroxide cleaning solution 31 inside the alkaline box 3 at 50-60 degrees. Then the alkaline part body 1 is placed inside the first water washing box 4, and the part body 1 is washed twice in the first deionized water 41. The first time, the temperature controller 81 is used to wash the first deionized water 41 with a temperature of 30-50 degrees for 15-3 0 seconds, the second time the temperature is adjusted to the room temperature in the first deionized water 41 by the temperature controller 81 for washing for 15-30 seconds, then the washed part body 1 is placed in the inside of the pickling box 5, the part body 1 is immersed in the hydrofluoric acid cleaning solution 51 for 3-5 minutes, and the temperature is maintained at 40-50 degrees by the temperature controller 81 to remove the surface oxide scale and dirt, and most importantly, to remove the silicon on the surface of the aluminum alloy to prevent the surface from turning black after oxidation. Then the pickled part body 1 is placed in the inside of the natural color conductive oxidation box 6, and the part body 1 is placed in the potassium permanganate oxidation solution 61 as the anode, and the temperature of the potassium permanganate oxidation solution 61 is controlled at 50-60 degrees by the stable constant voltage power supply 62, the voltage is 30V, and the oxidation time is 3-5 minutes. Then the oxidized part body 1 can be placed in the second washing box 7, and the part body 1 is washed in the second deionized water 71 for 1-3 minutes. Then the washed part body 1 is taken out and blown dry by the air pump 9, and the sandblasting and surface treatment of the part body 1 can be completed.
[0031] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A device for 3D printing Alsi10Mg material natural color conductive oxidation, comprising a part body (1), a sandblasting device (2) is provided on one side of the part body (1), characterized in that: One side of the sandblasting equipment (2) is connected to an alkali box (3), one side of the alkali box (3) is connected to a first water washing box (4), one side of the first water washing box (4) is connected to a pickling box (5), one side of the pickling box (5) is connected to a natural color conductive oxidation box (6), one side of the natural color conductive oxidation box (6) is connected to a second water washing box (7), and one side of the second water washing box (7) is provided with an air pump (9).
2. A device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: Heaters (8) are fixedly arranged inside the alkali tank (3), the first water washing tank (4), the acid washing tank (5) and the natural color conductive oxidation tank (6), and the heaters (8) are externally connected to a temperature controller (81) via a wire.
3. A device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: Quartz sand (21) is arranged inside the sandblasting equipment (2).
4. The device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: A sodium hydroxide cleaning solution (31) is arranged inside the alkaline box (3), and the sodium hydroxide cleaning solution (31) is composed of sodium hydroxide with a concentration of 50-60 g / L.
5. The device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: The first water washing box (4) is provided with first deionized water (41) inside.
6. The device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: The interior of the pickling box (5) is provided with a hydrofluoric acid cleaning liquid (51), and the hydrofluoric acid cleaning liquid (51) is composed of hydrofluoric acid with a concentration of 3-5%.
7. The device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: A potassium permanganate oxidizing solution (61) is arranged inside the natural color conductive oxidizing box (6), and one side of the natural color conductive oxidizing box (6) is externally connected to a stable constant voltage power supply (62) through a wire, and the potassium permanganate oxidizing solution (61) is composed of potassium permanganate with a concentration of 5%.
8. The device for 3D printing Alsi10Mg material natural color conductive oxidation according to claim 1, characterized in that: The second water washing box (7) is provided with second deionized water (71) inside, and the second deionized water (71) is deionized water at room temperature.