Device for increasing growth speed of diamond
By using the bottom ultra-thin-walled tubular carbon source in the diamond growth device to provide the carbon atoms required for catalyst alloy melting and single crystal growth, the problem of slow initial single crystal growth caused by insufficient carbon content is solved, and three-dimensional single crystals are realized. grow and significantly increase growth rate.
Patent Information
- Application Number
- CN202420421242.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-05
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2034-03-05
Smart Images

Figure CN221822395U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of diamond synthesis, in particular to a device for improving the growth speed of diamond. Background Art
[0002] At present, when preparing catalyst alloy rods under normal pressure, in order to reduce the technical difficulties of smelting and subsequent processing, not enough C is added to the catalyst alloy, resulting in that even if the pressure and temperature have reached the eutectic point in the initial stage of synthesis, the carbon content in the alloy rod is still far lower than the carbon content at the eutectic point. Therefore, the low-temperature end of the alloy rod has not melted at this time, so the single crystal growth process has not started, which in turn affects the initial single crystal growth rate. Especially when growing large-sized single crystals, the catalyst alloy column is very high at this time, so the diffusion path becomes longer; or when growing colorless II a large-sized single crystals, the temperature gradient is smaller at this time, so the diffusion rate of carbon atoms slows down. This leads to a slow growth rate of the initial single crystal, so a device that can increase the initial growth rate of diamond single crystals is needed. Utility Model Content
[0003] The purpose of the utility model is to provide a device for increasing the growth rate of diamonds to improve the above problems. In order to achieve the above purpose, the technical solution adopted by the utility model is as follows:
[0004] The present application provides a device for increasing the growth rate of diamond, comprising:
[0005] A growth container, a crystal bed, a catalyst alloy sheet, a single crystal seed, a first film, a second film, a first carbon source, a second carbon source and a catalyst alloy column, wherein the growth container is arranged in a cylindrical shape, and a cavity is arranged in the growth container; the crystal bed is arranged at the bottom of the cavity of the growth container; the catalyst alloy sheet is arranged directly above the crystal bed; the single crystal seed is arranged in the catalyst alloy sheet, and the top of the single crystal seed is flush with the top of the catalyst alloy sheet; the first film is wrapped on the outer side wall of the single crystal seed; the second film is fixedly arranged on the top of the single crystal seed; the first carbon source is arranged at both ends of the catalyst alloy sheet; the second carbon source is arranged directly above the catalyst alloy sheet; the catalyst alloy column is arranged between the catalyst alloy sheet and the second carbon source.
[0006] Optionally, the growth container includes a growth container upper cover, a growth container lower cover, a first growth container side wall and a second growth container side wall, the growth container lower cover is provided with a groove, the depth of the groove is the same as the height of the crystal bed, the second growth container side wall is provided directly above the two ends of the growth container lower cover, the first growth container side wall is provided directly above the second growth container side wall, and the growth container upper cover is provided on the first growth container side wall.
[0007] Optionally, the thickness of the side wall of the second growth container is less than the thickness of the side wall of the first growth container.
[0008] Optionally, the catalyst alloy sheet is fixedly disposed in the side wall 11 of the second growth container.
[0009] Optionally, the material of the catalyst alloy sheet is the same as the material of the catalyst alloy column.
[0010] Optionally, the crystal bed is provided with MgO with a mass ratio of 30% to 70% or SiC with a mass ratio of 30% to 70%.
[0011] Optionally, the first film is a copper foil of 0.05 to 0.25 m, a gold foil of 0.05 to 0.25 m, or a platinum foil of 0.05 to 0.25 m.
[0012] Optionally, the second film is a copper foil with a thickness of 0.3 to 0.45 mm, a gold foil with a thickness of 0.3 to 0.45 mm, or a platinum foil with a thickness of 0.3 to 0.45 mm.
[0013] Optionally, the height of the second carbon source is 0.8 to 1.5 mm, and the height of the second carbon source is the same as the height of the catalyst alloy sheet.
[0014] The beneficial effects of the utility model are:
[0015] The utility model is provided with a device for improving the growth rate of diamond. In the early stage of single crystal growth, the ultra-thin-walled tubular carbon source at the bottom provides the carbon atoms required for melting the catalyst alloy and growing the single crystal, and further expands the surface area of the single crystal, so that there is no need to wait for the carbon atoms of the top carbon source to diffuse to the bottom of the crystal growth container after a long time. As long as the single crystal growth pressure and temperature reach the requirements, the upper plane and the lateral crystal plane of the seed crystal are completely immersed in the catalyst melt, so from this point on, the three-dimensional growth of the single crystal can be achieved. Furthermore, the utility model can significantly improve the initial single crystal growth rate through the above-mentioned synthetic block structure.
[0016] Other features and advantages of the utility model will be described in the following description, and partly become apparent from the description, or understood by implementing the embodiments of the utility model. The purpose and other advantages of the utility model can be realized and obtained by the structures specifically pointed out in the written description, claims, and drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.
[0018] Figure 1 It is a schematic cross-sectional view of the structure of the device for increasing the growth rate of diamond described in the embodiment of the utility model.
[0019] Markings in the figure: 1. crystal bed; 2. powdered catalyst alloy sheet; 3. single crystal seed; 4. first film; 5. second film; 6. second carbon source; 7. first carbon source; 8. catalyst alloy column; 9. upper cover of growth container; 10. lower cover of growth container; 11. side wall of first growth container; 12. side wall of second growth container. DETAILED DESCRIPTION
[0020] In order to make the purpose, technical scheme and advantages of the embodiment of the utility model clearer, the technical scheme in the embodiment of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiment of the utility model. Obviously, the described embodiment is a part of the embodiment of the utility model, rather than all the embodiments. The components of the embodiment of the utility model generally described and shown in the drawings here can be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiment of the utility model provided in the drawings is not intended to limit the scope of the utility model for protection, but merely represents the selected embodiment of the utility model. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work belong to the scope of protection of the utility model.
[0021] It should be noted that similar reference numerals and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in subsequent drawings. At the same time, in the description of the present utility model, the terms "first", "second", etc. are only used to distinguish the description and cannot be understood as indicating or implying relative importance.
[0022] Example 1
[0023] like Figure 1As shown, this embodiment provides a device for improving the growth rate of diamond, including: a growth container structure, a crystal bed 1, a powder catalyst alloy sheet 2, a single crystal seed 3, a first film 4, a second film 5, a first carbon source 7, a second carbon source 6, and a catalyst alloy column 8, wherein the growth container structure is arranged in a cylindrical shape, and a cavity is arranged in the growth container structure; the crystal bed 1 is arranged at the bottom of the cavity of the growth container structure; the catalyst alloy sheet 2 is arranged directly above the crystal bed 1; the single crystal seed 3 is arranged in the catalyst alloy sheet 2, and the top of the single crystal seed 3 is flush with the top of the catalyst alloy sheet 2; the first film 4 is wrapped on the outer wall of the single crystal seed 3; the second film 5 is fixedly arranged on the top of the single crystal seed 3; the second carbon source 6 is arranged around the powder catalyst alloy sheet 2; the first carbon source 7 is arranged directly above the catalyst alloy sheet 2; the catalyst alloy column 8 is arranged between the catalyst alloy sheet 2 and the first carbon source 7.
[0024] The utility model is provided with a device for improving the growth rate of diamond, and the ultra-thin tubular carbon source at the bottom provides the nutrients required for the lateral growth of the single crystal, and further expands the surface area of the single crystal. When the carbon atoms of the top carbon source diffuse to the bottom of the crystal growth container after a long time, the upper plane and the lateral crystal plane of the seed crystal are completely immersed in the catalyst melt, so the three-dimensional growth of the single crystal can be achieved from this point on. Furthermore, the utility model can significantly improve the initial single crystal growth rate through the above-mentioned synthetic block structure.
[0025] Among them, the powdered catalyst alloy with the same composition as the catalyst alloy column 8 is uniformly mixed with the graphite powder to reach the carbon atom concentration at the high temperature-high pressure eutectic point, and is pressed into a disc of the same size as the crystal bed, and the seed crystal is evenly buried therein. The plane on the seed crystal is flush with the plane on the powder alloy sheet, so that uniform growth of the side of the single crystal can be achieved. In addition, the present invention wraps the single crystal seed 3 with a first film 4 to prevent it from contacting the catalyst alloy too early and causing graphitization.
[0026] like Figure 1 As shown, the growth container includes a growth container upper cover 9, a growth container lower cover 10, a first growth container side wall 11 and a second growth container side wall 12. The growth container lower cover 10 is provided with a groove, and the depth of the groove is the same as the height of the crystal bed 1. The second growth container side wall 12 is arranged directly above the two ends of the growth container lower cover 10, and the first growth container side wall 11 is arranged directly above the second growth container side wall 12. The growth container upper cover 9 is arranged on the first growth container side wall 11.
[0027] The utility model provides a groove at the bottom of the growth container structure, and then places the crystal bed 1 in the groove, and then heats the crystal bed 1 to increase the temperature.
[0028] like Figure 1 As shown, the thickness of the second growth container side wall 12 is smaller than the thickness of the first growth container side wall 11 .
[0029] The second growth container sidewall 12 is relatively thin, so the second growth container has a higher temperature during the heating process, thereby forming a radial temperature gradient inside the second growth container sidewall 12, and the temperature at the outer diameter of the catalyst alloy sheet 2 is high and the temperature at the center is the lowest.
[0030] like Figure 1 As shown, the catalyst alloy sheet 2 is fixedly disposed in the side wall 12 of the second growth container.
[0031] Among them, since a high thermal conductivity uniform temperature crystal bed 1 is placed under the catalyst alloy sheet 2, the radial temperature gradient outside the high thermal conductivity uniform temperature crystal bed 1 is large, and the radial temperature gradient near the plane of the high thermal conductivity uniform temperature crystal bed 1 is small, which can achieve uniform lateral growth of single crystals.
[0032] like Figure 1 As shown, the material of the catalyst alloy sheet 2 is the same as the material of the catalyst alloy column 8 .
[0033] The utility model provides a powder catalyst alloy sheet 2 and a second carbon source 6 so that when the seed crystal in the side wall 12 of the second growth container reaches the eutectic point temperature, the powder catalyst alloy sheet 2 and the second carbon source 6 react, the catalyst melts, and then the single crystal starts to grow, which advances the start growth time of the seed crystal and ensures that the seed crystal can grow laterally uniformly.
[0034] like Figure 1 As shown, the crystal bed 1 is provided with MgO with a mass ratio of 30% to 70% or SiC with a mass ratio of 30% to 70%.
[0035] Among them, the utility model sets MgO with a mass ratio of 30% to 70% or SiC with a mass ratio of 30% to 70% in the crystal bed 1, so that the crystal bed 1 can achieve high thermal conductivity and constant temperature effects, and the radial temperature of the single crystal growth zone on its upper part becomes more uniform.
[0036] like Figure 1 As shown, the first film 4 is a copper foil of 0.05 to 0.25 m, a gold foil of 0.05 to 0.25 m, or a platinum foil of 0.05 to 0.25 m.
[0037] The utility model provides the first film 4 to prevent the single crystal seed 3 from contacting the catalyst alloy sheet 2 too early and causing graphitization.
[0038] like Figure 1As shown, the second film 5 is a copper foil with a thickness of 0.3 to 0.45 mm, a gold foil with a thickness of 0.3 to 0.45 mm, or a platinum foil with a thickness of 0.3 to 0.45 mm.
[0039] The utility model provides a second film 5 above the single crystal seed 3 to prevent the seed from contacting with the catalyst alloy column too early, which would lead to graphitization of the seed.
[0040] like Figure 1 As shown, the height of the second carbon source 6 is 0.8 to 1.5 mm, and the height of the second carbon source 6 is the same as the height of the powder catalyst alloy sheet 2 .
[0041] The present invention provides a second carbon source 6 to provide a carbon source for the early growth of the diamond single crystal seed 3. Since the carbon source is relatively small in mass, it is completely consumed and dissolved in the catalyst alloy melt in the late growth of the single crystal seed 3.
[0042] The above description is only the preferred embodiment of the utility model, and is not intended to limit the utility model. For those skilled in the art, the utility model can have various modifications and changes. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model shall be included in the protection scope of the utility model.
[0043] The above is only a specific implementation of the utility model, but the protection scope of the utility model is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed by the utility model, which should be included in the protection scope of the utility model. Therefore, the protection scope of the utility model should be based on the protection scope of the claims.
Claims
1. A device for increasing the growth rate of diamond, It is characterized in that include: Growth container structure: the growth container structure is configured as a circular tube with lids at both ends, and a cavity is provided inside the growth container structure; A crystal bed (1), the crystal bed (1) being arranged at the bottom of the cavity of the growth container structure; A powdered catalyst alloy sheet (2), wherein the catalyst alloy sheet (2) is arranged directly above the crystal bed (1); A single crystal seed (3), wherein the single crystal seed (3) is disposed in the catalyst alloy sheet (2), and the top of the single crystal seed (3) is flush with the top of the catalyst alloy sheet (2); A first film (4), the first film (4) being wrapped around the outer wall of the single crystal seed (3); A second film (5), the second film (5) being fixedly arranged on top of the single crystal seed (3); A second carbon source (6), the second carbon source (6) is in the shape of a thin-walled circular tube and is mounted around the powdered catalyst alloy sheet (2); A first carbon source (7), wherein the first carbon source (7) is disposed directly above the catalyst alloy sheet (2); as well as A catalyst alloy column (8), wherein the catalyst alloy column (8) is arranged between the powder catalyst alloy sheet (2) and the second carbon source (6).
2. The device for increasing the growth rate of diamond according to claim 1, Features: The growth container comprises a growth container upper cover (9), a growth container lower cover (10), a first growth container side wall (11) and a second growth container side wall (12); the growth container lower cover (10) is provided with a groove, the depth of the groove is the same as the height of the crystal bed (1); the second growth container side wall (12) is arranged directly above the two ends of the growth container lower cover (10); the first growth container side wall (11) is arranged directly above the second growth container side wall (12); and the growth container upper cover (9) is arranged on the first growth container side wall (11).
3. The device for increasing the growth rate of diamond according to claim 2, Features: The thickness of the second growth container side wall (12) is smaller than the thickness of the first growth container side wall (11).
4. The device for increasing the growth rate of diamond according to claim 2, Features: The powdered catalyst alloy sheet (2) is fixedly arranged in the side wall (12) of the second growth container.
5. The device for increasing the growth rate of diamond according to claim 1, Features: The material of the powdered catalyst alloy sheet (2) is the same as the material of the catalyst alloy column (8).
6. The device for increasing the growth rate of diamond according to claim 1, Features: The crystal bed (1) is provided with MgO with a mass ratio of 30% to 70% or SiC with a mass ratio of 30% to 70%.
7. The device for increasing the growth rate of diamond according to claim 1, Features: The first film (4) is a copper foil of 0.05 to 0.25 m, a gold foil of 0.05 to 0.25 m, or a platinum foil of 0.05 to 0.25 m.
8. The device for increasing the growth rate of diamond according to claim 1, Features: The second film (5) is a copper foil with a thickness of 0.3 to 0.45 mm, a gold foil with a thickness of 0.3 to 0.45 mm, or a platinum foil with a thickness of 0.3 to 0.45 mm.