Composite board frame and electronic equipment

By using the explosive welding process in bimetallic materials and improving the solid solubility of the third component, the problem of low bonding strength of bimetallic materials is solved, high bonding strength and durability are achieved, and the process flow is simplified.

CN221829186UActive Publication Date: 2024-10-11HUAWEI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322866966.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-24
Publication Date
2024-10-11
Estimated Expiration
2033-10-24

AI Technical Summary

Technical Problem

The existing bimetallic materials have low bonding strength during the rolling process and are prone to delamination during the bending and stamping process, resulting in process failure.

Method used

The explosive welding process is used to achieve reliable combination under the preset structural shape of the bimetallic material. The solid solubility of the material is improved through the third component, thereby improving the bonding strength. The structural reliability and wear resistance are improved through laser welding and PVD appearance treatment. .

Benefits of technology

It achieves high bonding strength of bimetallic materials, avoids the phenomenon of open welding and delamination during the bending and stamping process, improves the drop, bending and wear resistance of electronic equipment, and simplifies the process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221829186U_ABST
    Figure CN221829186U_ABST
Patent Text Reader

Abstract

The utility model provides a composite board frame and electronic device.The composite board frame comprises a first component and a second component, and the second component covers at least part of the outer side face of the first component through an explosive welding process; and the shape of a bonding interface of the first component and the second component has a corrugated composite characteristic. In the application, by adopting the explosive welding process, the first component and the second component can be reliably combined under the condition that the first component and the second component have the preset structural shape, and the drawing force after combination is greater than 100 MPa. Therefore, the bending and stamping process does not need to be carried out after the materials of the first component and the second component are combined, and therefore the phenomenon that the first component and the second component are subjected to open welding and layering in the bending and stamping process after welding can be avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of electronic products, and in particular to a composite board frame and an electronic device. Background Art

[0002] In order to improve the drop resistance, bending resistance and wear resistance of electronic equipment, while ensuring the lightweight of structural parts, bimetallic composite sheets are considered to be used to prepare the middle frame. Existing bimetallic materials are generally combined through rolling process, but this combination method has low strength and is prone to delamination during the process of bending and stamping to form the product, causing process failure. Utility Model Content

[0003] In view of this, the present application provides a composite plate frame and an electronic device to solve the problems of low bimetallic bonding strength and easy delamination during the product manufacturing process in the above-mentioned prior art.

[0004] In a first aspect, an embodiment of the present application provides a composite board frame for preparing an electronic device, wherein the composite board frame comprises a first component and a second component, wherein the second component is covered on at least a portion of the outer surface of the first component by an explosion welding process, and the shape of the bonding interface between the first component and the second component is corrugated.

[0005] In the present application, by adopting the explosive welding process, the first component and the second component can be reliably combined when they have a preset structural shape, and the pull-out force after the combination is greater than 100 MPa. Therefore, it is not necessary to first combine the materials of the first component and the second component into a plate and then perform the bending and stamping process, thereby avoiding the phenomenon of open welding and delamination of the first component and the second component after welding in the bending and stamping process.

[0006] In a possible implementation, the second component is a tubular structure, and the first component is embedded in the second component. The second component has a through hole, and the first component can be embedded in the hole of the second component, so that the second component can cover the outer side of the first component, and the first component and the second component can be reliably combined by an explosion welding process.

[0007] In one possible implementation, the first component includes a plurality of side surfaces, and a plurality of the side surfaces are planes. The second component includes a flat plate portion, and the flat plate portion is connected to at least a portion of the side surfaces by an explosion welding process. When the first component and the second component are combined and fixed, each flat plate portion can be fitted with a corresponding side surface on the first component, and then the flat plate portion can be combined and fixed with each corresponding side surface by an explosion welding process. Since the location of the explosion welding is on the side surface of the first component, rather than at the corner of the first component, the reliability of the combination of the flat plate portion and the side surface of the first component can be improved, and the problem of cold welding at the corner of the first component can be avoided. In addition, since the flat plate portion is a flat plate, there is no need to roll-form the second component, thereby simplifying the process.

[0008] In a possible implementation, there is an arc-shaped transition surface between two adjacent side surfaces. The second component also includes a curved portion, which covers the curved transition surface, and the curved portion is welded to the flat portion. The curved portion and the curved transition surface have similar curvatures, so that the matching state of the curved portion and the curved transition surface at various positions can be ensured to be close to the same. In addition, the curved portion and the flat portion can be connected and fixed by a laser welding process to eliminate the gap between the curved portion and the flat portion, thereby completely covering the circumferential side of the first component through the cooperation between the flat portion and the curved portion, so that the second component can be used as the external frame of the electronic device and can avoid the first component from leaking out. In one embodiment, the curved portion and the transition surface can be connected without the explosive welding process, and the curved portion and the curved transition surface can maintain a contact state, or a certain gap can be maintained, which can completely avoid the problem of explosive composite cold welding at the curved transition surface of the first component.

[0009] In one possible implementation, the composite sheet frame further includes a third component, and the third component is connected between the first component and the second component by an explosion welding process. The solid solubility between the third component and the first component and the solid solubility between the third component and the second component are both greater than the solid solubility between the first component and the second component. Among them, the greater the mutual solid solubility of the two materials, the higher the bonding strength of the two materials. Exemplarily, when the solid solubility between the first component and the second component is small, it is difficult to ensure sufficient bonding strength between the first component and the second component. Therefore, by adding a third component between the first component and the second component, and the third component has a relatively large solid solubility with the first component and with the second component, the bonding strength between the first component and the second component can be improved by the third component.

[0010] In one possible implementation, the third component is a tubular structure, the second component covers the outer side surface of the third component, and the first component is embedded in the interior of the third component. In the process of connecting the first component, the second component and the third component, the connection and fixation of the three components can be achieved through a single explosion welding process. In one embodiment, the second component and the third component can both be tubular structures, and the third component can be fixedly embedded in the second component, so as to ensure the consistency and reliability of the connection at various positions between the second component and the third component. In one embodiment, as described above, the second component can include a flat plate portion, and the flat plate portion can be fixedly covered on the plane of the outer wall of the third component. That is to say, when the third component is set between the first component and the second component, the first component can also be made into a tubular shape without roller forming, thereby simplifying the process.

[0011] In a possible implementation, the third component is a flat plate structure, wherein one side of the third component can be attached to the first component, and the other side can be attached to the second component, and the three components can be connected and fixed by an explosion process, thereby ensuring the reliability of the combination of the three components, and further ensuring the structural reliability of the obtained composite plate frame.

[0012] In a possible implementation, the material of the third component is an aluminum alloy. The material of the first component is a magnesium alloy, and the material of the second component is a titanium alloy. The solid solubility between the magnesium alloy and the titanium alloy is relatively small, while the solid solubility between the magnesium alloy and the aluminum alloy and the solid solubility between the titanium alloy and the aluminum alloy is relatively large. Therefore, the magnesium alloy and the aluminum alloy, and the titanium alloy and the aluminum alloy have a greater bonding strength than that between the magnesium alloy and the titanium alloy, so that the reliability of the bonding between the titanium alloy and the magnesium alloy can be improved through the transition of the aluminum alloy.

[0013] In a possible implementation manner, the material of the first component is a magnesium alloy, and the material of the second component is a titanium alloy.

[0014] In a possible implementation, the outer surface of the second component is provided with a treatment layer, wherein the treatment layer can make the appearance of the titanium alloy have metallic luster, high wear resistance and other properties, thereby improving the texture and user experience of the electronic device.

[0015] In a possible implementation, the material of the treatment layer is one of titanium nitride, chromium nitride, chromium aluminum nitride or titanium carbide nitride, all of which can make the outer surface of the second component have properties such as metallic luster and high wear resistance.

[0016] In the second aspect, the embodiment of the present application further provides an electronic device, which includes the composite plate frame provided in the first aspect of the present application. The electronic device including the composite plate frame has similar technical effects as the aforementioned composite plate frame, which will not be described in detail here.

[0017] It should be understood that the foregoing general description and the following detailed description are exemplary only and are not restrictive of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0019] Figure 1 A schematic diagram of the structure of an electronic device provided in an embodiment of the present application;

[0020] Figure 2 A schematic diagram of the structure of a composite plate frame provided in an embodiment of the present application;

[0021] Figure 3 An enlarged view of a bonding interface between a first component and a second component is provided for an embodiment of the present application;

[0022] Figure 4 A schematic diagram of a first component and a second component provided in an embodiment of the present application after being combined;

[0023] Figure 5 This is a process flow chart of obtaining a composite plate frame by combining a first component and a second component in one embodiment of the present application;

[0024] Figure 6 This is a process flow chart of obtaining a composite plate frame by combining a first component and a second component in another embodiment of the present application;

[0025] Figure 7 This is a process flow chart of obtaining a composite board frame by combining a first component, a second component and a third component in another embodiment of the present application.

[0026] Reference numerals:

[0027] 1- first component;

[0028] 11- side;

[0029] 12-arc transition surface;

[0030] 2- second component;

[0031] 21- flat plate;

[0032] 22-bend portion;

[0033] 3- the third component;

[0034] 4-Binding interface;

[0035] 5-Titanium alloy plate;

[0036] 6-Titanium alloy tube;

[0037] 7-Magnesium alloy rod;

[0038] 8-Titanium-magnesium composite profile;

[0039] 9- Composite sheet;

[0040] 10-Titanium-magnesium-aluminum composite profile. DETAILED DESCRIPTION

[0041] In order to better understand the technical solution of the present application, the embodiments of the present application are described in detail below with reference to the accompanying drawings.

[0042] It should be clear that the described embodiments are only part of the embodiments of the present application, rather than all the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.

[0043] The terms used in the embodiments of the present application are only for the purpose of describing specific embodiments, and are not intended to limit the present application. The singular forms "a", "said" and "the" used in the embodiments of the present application and the appended claims are also intended to include plural forms, unless the context clearly indicates other meanings.

[0044] It should be understood that the term "and / or" used in this article is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.

[0045] In the description of this application, unless otherwise clearly specified and limited, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; unless otherwise specified or explained, the term "plurality" refers to two or more; the terms "connected" and "fixed" should be understood in a broad sense, for example, "connected" can be a fixed connection, a detachable connection, an integral connection, or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0046] In order to improve the drop resistance, bending resistance and wear resistance of electronic devices and enhance the user experience, more and more bimetallic composite materials are used in the middle frame, battery cover and other structural parts of electronic devices. When bimetallic composite materials are combined, they are generally prepared into bimetallic composite profiles by die casting, rolling, co-extrusion and other processes. Such profiles are usually straight in shape, and then the profiles need to be formed into products with specific shapes through processes such as bending and stamping.

[0047] However, since the elastic modulus and strength of the two metal materials are generally quite different, it is difficult to ensure that the two metals have a large bonding strength after composite molding through the above-mentioned die-casting, rolling, co-extrusion and other processes. In addition, in the subsequent bending and stamping process, it is also easy to cause the two metals to delaminate and the process to fail.

[0048] The embodiment of the present application provides a composite plate frame, which can be used in electronic devices and can be used as a middle frame, battery cover and other components of the electronic device. The electronic device can be a mobile phone, a tablet computer, a laptop computer, a smart home, a smart bracelet, a smart watch, a smart helmet, smart glasses, etc. The embodiment of the present application does not limit the type of electronic device. Figure 1 An electronic device provided in an embodiment of the present application is exemplarily shown, and the electronic device is described as a mobile phone. Figure 2 It is exemplified that the composite board frame provided in the embodiment of the present application is a back cover of a mobile phone. In some other embodiments, the composite board frame may also be a middle frame, a battery cover, etc.

[0049] Reference Figure 2 , a composite plate frame provided by an embodiment of the present application includes a first component 1 and a second component 2, wherein the first component 1 and the second component 2 may be made of different metal materials, and the two materials have different elastic moduli and strengths. Exemplarily, the material of the first component 1 may be a magnesium alloy, and the material of the second component 2 may be a titanium alloy. Exemplarily, the material of the first component 1 may be an aluminum alloy, and the material of the second component 2 may be a titanium alloy. Exemplarily, the material of the first component 1 may be a steel material, and the material of the second component 2 may be an aluminum alloy.

[0050] In one embodiment, the material of the first component 1 is a magnesium alloy, and the material of the second component 2 is a titanium alloy. The profile of the first component 1 can be a rod-shaped profile formed from a magnesium alloy and having an overall solid structure. The profile of the second component 2 can be a profile having a preset shape formed from a titanium alloy profile by a bending process. For example, the second component 2 can be tubular, flat, etc. When the first component 1 and the second component 2 are combined, the profile of the second component 2 can cover at least part of the outer side surface 11 of the profile of the first component 1, and the profile of the first component 1 and the profile of the second component 2 can be combined and fixed by an explosion welding process.

[0051] Among them, the explosion welding process refers to a processing technology that uses the energy of the explosion of explosives to melt two dissimilar metal plates together. During the explosion welding process, multiple and multiple energy transfers, absorptions, conversions and distributions will occur between the metals, and finally a bonding interface between the metal materials of the first component 1 profile and the second component 2 profile will be formed. This process is very short, measured in microseconds, which can improve the efficiency of welding the first component 1 and the second component 2 and facilitate operation. In addition, the explosion welding process can achieve a reliable combination of the first component 1 profile and the second component 2 profile when they have a preset structural shape, and the pull-out force after the combination is greater than 100MPa. As a result, there is no need to weld the materials of the first component 1 profile and the second component 2 profile first, and then perform the bending and stamping process, thereby avoiding the phenomenon of open welding and delamination of the first component 1 profile and the second component 2 profile after welding in the bending and stamping process.

[0052] Figure 3 An enlarged view of the interface 4 between the first component 1 and the second component 2 is provided for the embodiment of the present application, referring to Figure 3 After the first component 1 profile and the second component 2 profile are connected and fixed by the explosion welding process, the bonding interface 4 between the first component 1 profile and the second component 2 profile will present a corrugated feature. This corrugated feature is not a regular shape, but presents an uneven structural feature. This corrugated feature can be formed through multiple and multiple energy transfer, absorption, conversion and distribution during the explosion welding process.

[0053] After the first component 1 profile and the second component 2 profile are welded and composited into a sheet, the composite integral profile can be cut to cut out a parison for preparing an electronic device frame, which has a size that meets the requirements of the electronic device frame and has good flatness. Then, the parison can be injection molded and machined to form various necessary design features on the frame, such as structures for installing various components, structures for improving performance such as strength, etc. Then, physical vapor deposition (PVD) appearance treatment can be performed to obtain the final composite sheet frame product. In one embodiment, in the obtained composite sheet frame product, various structural features can be processed on the first component 1, which are used to install and arrange components, modules, etc., and play a major supporting role. In one embodiment, the second component 2 can be used as a frame of electronic devices such as mobile phones and computers, and can be used to realize electrical connection functions. For example, a part of the first component 1 can be used to make an antenna, and the first component 1 can be used as a radiator in the antenna to radiate energy.

[0054] In one embodiment, Figure 4 A schematic diagram of a first component and a second component combined in accordance with an embodiment of the present application, referring to Figure 4 , the second component 2 is a tubular structure, and the first component 1 is embedded in the second component 2. Among them, the second component 2 has a through hole, and the first component 1 can be embedded in the hole of the second component 2, so that the second component 2 can cover the outer side 11 of the first component 1, and the first component 1 and the second component 2 can be reliably combined by an explosion welding process. In one embodiment, the tubular second component 2 can be roller-formed, and the metal plate used to prepare the second component 2 is bent into a tubular shape by a roller, and then the tubular interface is closed by laser welding or the like. Among them, the second component 2 can be a square tube, and the hole in the second component 2 is a square hole. The first component 1 can have the same shape as the square hole, so that the first component 1 can be embedded in the square hole. Of course, in some other embodiments, the second component 2 can also be processed into a tube structure of other shapes, and the corresponding first component 1 can have a shape that matches the hole in the second component 2, which is not limited in this embodiment.

[0055] In one embodiment, Figure 5 This is a process flow chart of obtaining a composite plate frame by combining a first component 1 and a second component 2 in one embodiment of the present application, wherein the material of the first component 1 is a magnesium alloy, and the material of the second component 2 is a titanium alloy. Figure 5 , the composite sheet frame can be prepared according to the following steps:

[0056] Step 1: Roll-form the titanium alloy plate 5 to form it into a tubular structure, that is, obtain the titanium alloy tube 6. In one embodiment, a bending machine can be used to bend the flat titanium alloy plate 5 in the roll-forming process to bend the titanium alloy plate 5 into a tubular shape. After bending, the two ends of the titanium alloy plate 5 in the bending direction are close to each other, and then the two ends can be welded and connected by a welding process, so as to form a tubular structure closed in the bending direction, that is, obtain the titanium alloy tube 6.

[0057] Step 2: Cut the titanium alloy tube 6 by a cutting process to cut out a size that can be combined with the magnesium alloy rod.

[0058] Step 3: Process the magnesium alloy into a rod so that the size of the magnesium alloy rod 7 matches the size of the hole in the titanium alloy tube 6 .

[0059] Step 4: embed the magnesium alloy rod 7 into the titanium alloy tube 6, and combine and fix the titanium alloy and the magnesium alloy through an explosion welding process to obtain a titanium-magnesium composite profile 8.

[0060] Step 5: Cut the titanium-magnesium composite profile into composite plates 9 of required thickness through a cutting process.

[0061] Step 6: Injection molding and machining are performed on the composite plate 9 to produce the product form required in the electronic device, such as a middle frame, a back cover, etc.

[0062] Step 7: Perform PVD appearance treatment on the composite board with a certain shape to obtain a composite board frame.

[0063] In one embodiment, Figure 6 This is a process flow chart of obtaining a composite plate frame by combining the first component 1 and the second component 2 in another embodiment of the present application, referring to Figure 6, the first component 1 includes a plurality of side surfaces 11, and the plurality of side surfaces 11 are planes, and the second component 2 includes a flat plate portion 21, and the flat plate portion 21 is connected to at least part of the side surfaces 11 by an explosion welding process. Exemplarily, the first component 1 is a cuboid having four side surfaces 11, and the four side surfaces 11 are planes. The flat plate portion 21 of the second component 2 is a flat plate, and the surface on the flat plate portion 21 for matching with the side surfaces 11 of the first component 1 is a plane. The number of the flat plate portions 21 can be the same as the number of the side surfaces 11 on the first component 1, so that each flat plate portion 21 can correspond to each side surface 11 one by one. When the first component 1 and the second component 2 are combined and fixed, each flat plate portion 21 can be fitted with the corresponding side surface 11 on the first component 1, and then the flat plate portion 21 can be combined and fixed with each corresponding side surface 11 by an explosion welding process. Since the explosive welding is performed on the side 11 of the first component 1 instead of at the corner of the first component 1, the reliability of the combination of the flat plate portion 21 and the side 11 of the first component 1 can be improved, and the problem of explosive composite cold welding at the corner of the first component 1 can be avoided. In addition, since the flat plate portion 21 is a flat plate, the second component 2 does not need to be roll-formed, thereby simplifying the process.

[0064] In one embodiment, referring to Figure 6 , there is an arcuate transition surface 12 between two adjacent side surfaces 11, and the second component 2 also includes a curved portion 22, which covers the curved transition surface 12, and the curved portion 22 is welded to the flat portion 21. Among them, the curved portion 22 and the curved transition surface 12 have similar curvatures, so that the matching state of each position of the curved portion 22 and the curved transition surface 12 can be nearly consistent. In addition, the curved portion 22 and the flat portion 21 can be connected and fixed by a laser welding process to eliminate the gap between the curved portion 22 and the flat portion 21, so that the circumferential side surface 11 of the first component 1 can be completely covered by the cooperation of the flat portion 21 and the curved portion 22, so that the second component 2 can be used as the external frame of the electronic device, and the first component 1 can be prevented from leaking out. In one embodiment, the curved portion 22 and the transition surface can be connected without using an explosive welding process, and the curved portion 22 and the curved transition surface 12 can maintain a contact state, or a certain gap can be maintained, which can completely avoid the problem of explosive composite cold welding at the curved transition surface 12 of the first component 1.

[0065] In one embodiment, Figure 6 This is a process flow chart of obtaining a composite plate frame by combining a first component 1 and a second component 2 in another embodiment of the present application, wherein the material of the first component 1 is a magnesium alloy, and the material of the second component 2 is a titanium alloy. Figure 6 , the composite sheet frame can be prepared according to the following steps:

[0066] Step 1: Processing to obtain the titanium alloy flat plate portion 21 and the magnesium alloy rod 7.

[0067] Step 2: The titanium alloy flat plate portion 21 and the magnesium alloy rod 7 are fixed together by explosion welding.

[0068] Step three: align the bent portion 22 of the titanium alloy with the arc-shaped transition surface 12 of the magnesium alloy rod 7 , and weld and fix the bent portion 22 of the titanium alloy with the flat plate portion 21 to obtain a titanium-magnesium composite profile 8 .

[0069] Step 4: Cut the titanium-magnesium composite profile into composite plates 9 of required thickness through a cutting process.

[0070] Step 5: Injection molding and machining are performed on the composite plate 9 to produce the product form required in the electronic device, such as a middle frame, a back cover, etc.

[0071] Step 6: Perform PVD appearance treatment on the composite board with a certain shape to obtain a composite board frame.

[0072] In one embodiment, Figure 7 This is a process flow chart of obtaining a composite plate frame by combining the first component 1, the second component 2 and the third component 3 in another embodiment of the present application, referring to Figure 7 , the composite plate frame also includes a third component 3, which is connected between the first component 1 and the second component 2 by an explosion welding process. The solid solubility between the third component 3 and the first component 1 and the solid solubility between the third component 3 and the second component 2 are both greater than the solid solubility between the first component 1 and the second component 2. Among them, the greater the solid solubility, the higher the bonding strength of the two materials. Exemplarily, when the solid solubility between the first component 1 and the second component 2 is small, it is difficult to ensure that the first component 1 and the second component 2 have sufficient bonding strength. Therefore, by adding the third component 3 between the first component 1 and the second component 2, and the third component 3 has a relatively large solid solubility with the first component 1 and the second component 2, the bonding strength between the first component 1 and the second component 2 can be improved by the third component 3. In one embodiment, the material of the first component 1 is a magnesium alloy, the material of the second component 2 is a titanium alloy, and the material of the third component 3 is an aluminum alloy. Among them, the solid solubility between magnesium alloy and titanium alloy is relatively small, while the solid solubility between magnesium alloy and aluminum alloy, as well as the solid solubility between titanium alloy and aluminum alloy is relatively large. Therefore, the bonding strength between magnesium alloy and aluminum alloy, as well as between titanium alloy and aluminum alloy, is greater than that between magnesium alloy and titanium alloy. Therefore, the reliability of the bonding between titanium alloy and magnesium alloy can be improved through the transition of aluminum alloy.

[0073] In one embodiment, referring to Figure 7, the third component 3 is a tubular structure, the second component 2 covers the outer side surface 11 of the third component 3, and the first component 1 is embedded in the interior of the third component 3. For example, when the third component 3 is made of aluminum, a tubular aluminum alloy profile can be processed through an extrusion process, or an aluminum plate with a smaller thickness can be used to form a tubular structure through a bending process. The first component 1 can be explosion welded to the inner wall of the third component 3, and the second component 2 can be explosion welded to the outer wall of the third component 3. In the process of connecting the first component 1, the second component 2 and the third component 3, the connection and fixation of the three components can be achieved through a single explosion welding process. In one embodiment, the second component 2 and the third component 3 can both be tubular structures, and the third component 3 can be fixedly embedded in the second component 2, so as to ensure the consistency and reliability of the connection at various positions between the second component 2 and the third component 3. In one embodiment, as described above, the second component 2 may include a flat plate portion 21, which may be fixedly covered on the plane of the outer wall of the third component 3. That is, when the third component 3 is arranged between the first component 1 and the second component 2, the second component 2 may also be made into a tubular shape without the need for roller forming, thereby simplifying the process.

[0074] In one embodiment, Figure 7 This is a process flow chart of obtaining a composite plate frame by combining the first component 1, the second component 2 and the third component 3 in another embodiment of the present application. The material of the first component 1 is a magnesium alloy, the material of the second component 2 is a titanium alloy, and the material of the third component 3 is an aluminum alloy. Figure 7 , the composite sheet frame can be prepared according to the following steps:

[0075] Step 1: Roll-form the titanium alloy plate 5 to form a tubular structure.

[0076] Step 2: Cut the titanium alloy tube 6 to a size that can be nested with the aluminum alloy tube.

[0077] Step 3: Process the magnesium alloy into rods so that the size of the magnesium alloy rods 7 matches the size of the holes in the aluminum alloy tube.

[0078] Step 4: embed the magnesium alloy rod 7 into the aluminum alloy tube, and combine and fix the titanium alloy, magnesium alloy and aluminum alloy through an explosion welding process to obtain a titanium-magnesium-aluminum composite profile 10.

[0079] Step 5: Cut the titanium-magnesium-aluminum composite profile 10 into composite plates 9 of required thickness through a cutting process.

[0080] Step 6: Injection molding and machining are performed on the composite plate 9 to produce the product form required in the electronic device, such as a middle frame, a back cover, etc.

[0081] Step 7: Perform PVD appearance treatment on the composite board with a certain shape to obtain a composite board frame.

[0082] In one embodiment, the third component 3 can be a flat plate structure, one side of the third component 3 can be attached to the first component 1, and the other side can be attached to the second component 2, and the three components can be connected and fixed by an explosion process. Therefore, the reliability of the combination of the three components can be guaranteed, and then the structural reliability of the obtained composite board frame can be guaranteed.

[0083] In one embodiment, as described above, after the composite sheet of the first component 1 and the second component 2 is cut into a composite sheet of the required thickness, the necessary design features on the frame can be formed by injection molding and machining, and then the outermost second component 2 is surface treated by PVD process to form a treatment layer on the outer surface of the second component 2. For example, when the material of the second component 2 is titanium alloy, a treatment layer can be formed on the surface of the titanium alloy, and the treatment layer can make the appearance of the titanium alloy have metallic luster, high wear resistance and other properties, thereby improving the texture and user experience of the electronic device. In one embodiment, the material of the treatment layer can be one of titanium nitride, chromium nitride, chromium aluminum nitride or titanium nitride carbide, all of which can make the outer surface of the second component have metallic luster and high wear resistance and other properties.

[0084] Of course, in some other embodiments, the treatment layer may also be other materials that can make the outer surface of the second component have metallic luster and high wear resistance, which is not limited in this embodiment.

[0085] The above are only preferred embodiments of the present application and are not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. A composite plate frame, characterized in that: Used for preparing electronic equipment, the composite plate frame comprises: first component; The second component is covered on at least a portion of the outer side of the first component by an explosion welding process, and the shape of the bonding interface between the first component and the second component has a corrugated feature.

2. The composite plate frame according to claim 1, characterized in that: The second component is a tubular structure, and the first component is embedded in the second component.

3. The composite sheet frame according to claim 1, characterized in that: The first component includes a plurality of side surfaces, and a plurality of the side surfaces are planes; The second component includes a flat plate portion, and the flat plate portion is connected to at least a portion of the side surface by an explosion welding process.

4. The composite sheet frame according to claim 3, characterized in that: There is an arc-shaped transition surface between two adjacent side surfaces; The second component further includes a bent portion, the bent portion covers the arc-shaped transition surface, and the bent portion is connected to the flat plate portion by welding.

5. The composite plate frame according to any one of claims 1 to 4, characterized in that: Also included is a third component, the third component being connected between the first component and the second component by an explosion welding process; The solid solubility between the third component and the first component and the solid solubility between the third component and the second component are both greater than the solid solubility between the first component and the second component.

6. The composite plate frame according to claim 5, characterized in that: The third component is a tubular structure, the second component covers the outer side of the third component, and the first component is embedded in the interior of the third component.

7. The composite plate frame according to claim 5, characterized in that: The third component is a flat plate structure.

8. The composite plate frame according to claim 5, characterized in that: The material of the third component is aluminum alloy.

9. The composite plate frame according to any one of claims 1 to 4, characterized in that: The material of the first component is magnesium alloy, and the material of the second component is titanium alloy.

10. The composite plate frame according to any one of claims 1 to 4, characterized in that: The outer surface of the second component is provided with a treatment layer.

11. The composite plate frame according to claim 10, characterized in that: The material of the treatment layer is one of titanium nitride, chromium nitride, chromium aluminum nitride or titanium nitride carbide.

12. An electronic device, characterized in that: It comprises the composite board frame as described in any one of claims 1-11.