Powder forming die
Through the design of the upper mold and lower mold of the powder forming mold, multi-point feeding and vibration are used to uniformize the distribution of raw materials, which solves the problem of insufficient uniformity of powder metallurgy molds in the existing technology, improves work efficiency, and through the heating and cooling system Accelerate molding and extend mold life.
Patent Information
- Application Number
- CN202323636079.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-29
AI Technical Summary
Existing powder metallurgy molds have a problem of insufficient local uniformity when filling material powders, which requires manual fine-tuning to find uniformity, resulting in low efficiency.
A powder molding mold is designed, which uses a closable upper mold and a lower mold. The upper mold is equipped with multiple feeding holes and vibration plates, and the lower mold is equipped with a vibrator and a push rod. The raw materials are homogenized through multi-point feeding and vibration. Distributed and equipped with heating rods and cooling tubes to accelerate molding.
It achieves uniform distribution and efficient feeding of raw materials, reduces the need for manual adjustments, improves work efficiency, and extends the service life and production efficiency of the mold through the protective layer and heating and cooling system.
Smart Images

Figure CN221848649U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of molds, in particular to a powder forming mold. Background Art
[0002] Powder metallurgy is a process technology that produces metal powder or uses metal powder (or a mixture of metal powder and non-metallic powder) as raw material, and then forms and sinters it to manufacture metal materials, composite materials and various types of products. Therefore, during manufacturing, the material powder is first filled between the molds, then compacted and heated through the mold, and finally the product is obtained.
[0003] The powder of mold filling material is usually fed into the cavity manually or by a feeding mechanism. At this time, there may be problems with local uniformity, so it is necessary to manually use a spoon to fine-tune it to find uniformity, and then close the mold and compact it, which is inefficient.
[0004] For example, patent number: CN202021849901.5, a powder metallurgy gear forming mold, specifically discloses: "A feeding slot is provided between the gear mold cavity and the feeding device in the workbench, and a feeding pipe is installed in the feeding slot. One end of the feeding pipe is connected to the feeding device, and the other end extends into the gear mold cavity and passes through the silicone pad, so that the material can enter the gear mold cavity with the silicone pad through the feeding pipe." If the feed pipe is used for feeding, the raw materials are usually placed in piles, and manual uniformity is required at this time, which is less efficient. Utility Model Content
[0005] In view of this, the utility model aims at the deficiencies of the prior art, and its main purpose is to provide a powder forming mold, which not only has uniform feeding but also high leveling efficiency, thereby overcoming the deficiencies of the prior art.
[0006] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0007] The present application provides a powder forming mold, comprising an upper mold and a lower mold that can be closed together; the upper mold is provided with a mold core, and the lower mold is provided with a mold cavity; the surfaces of the mold core and the mold cavity are both provided with a protective layer; the sides of the upper mold and the lower mold are provided with a vibration plate, and the vibration plate is connected to the output end of the vibrator;
[0008] The top of the upper mold is provided with a plurality of feeding holes, and the side of the mold core is provided with a plurality of exhaust ports; the feeding holes and the exhaust ports are communicated with the exhaust ports;
[0009] Ejectors and forming blocks are arranged transversely in the cavity, and the forming blocks and ejectors can extend from the cavity;
[0010] The upper mold and the lower mold are penetrated by a plurality of heating rods and cooling tubes, and the corresponding heating rods can heat the mold core and the mold cavity; and the cooling tubes can cool the mold core and the mold cavity.
[0011] Preferably, the lower die is penetrated by a push rod; part of the push rod is obliquely penetrated by the lower die; the molding block is molded on the upper end of the push rod; and a connecting port is provided at the lower end of the push rod.
[0012] Preferably, the depth of the exhaust port is between 5-10 μm.
[0013] Preferably, the protective layer is one of a ceramic wear-resistant layer and a metal nitride layer.
[0014] Preferably, the thickness of the protective layer is between 1 and 3 mm.
[0015] Preferably, the heating rod is made of one of nickel-chromium alloy, iron-chromium-aluminum alloy and silicon carbide.
[0016] Preferably, the cooling tube is one of a stainless steel tube, a molybdenum tube, a titanium alloy tube, and a nano-ceramic tube.
[0017] Preferably, a protrusion is provided at the position of the cavity corresponding to the feeding hole, and the protrusion can block the feeding hole.
[0018] Preferably, there is at least one row of the heating rods and cooling tubes, and the heating rods and cooling tubes are arranged alternately.
[0019] Preferably, the lower mold is provided with at least one pressure sensor, and the upper mold can trigger the pressure sensor.
[0020] Compared with the prior art, the utility model has obvious advantages and beneficial effects. Specifically, it can be seen from the above technical scheme that the powder forming mold comprises an upper mold and a lower mold that can be closed together. The upper mold is provided with a mold core, and the lower mold is provided with a mold cavity; the protective layer provided on the surface of the mold core and the mold cavity can improve the wear resistance of the mold, which is beneficial to prolonging the service life of the mold. Because; the sides of the upper mold and the lower mold are provided with a vibration plate, and the vibration plate is connected to the output end of the vibrator; the top of the upper mold is provided with a plurality of feeding holes. Therefore, the raw material can be fed in from multiple feeding holes, and the vibration of the upper mold allows the raw material to enter multiple positions in the mold cavity more smoothly from the feeding hole. The vibration of the lower mold can make the raw material evenly distributed in the mold cavity. It can be seen that this method of feeding the raw material into the mold cavity is more efficient and does not require manual uniformity.
[0021] The upper mold and the lower mold are penetrated with a plurality of heating rods and cooling tubes. The heating rods can heat the mold core and the mold cavity so that the product can be heated and formed; the cooling tubes can cool the mold core and the mold cavity to accelerate the molding of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of mold opening of an embodiment of the utility model.
[0023] Figure 2 It is an embodiment of the utility model Figure 1 Another state diagram.
[0024] Figure 3 It is a schematic diagram of the lower mold of an embodiment of the utility model.
[0025] Figure 4 It is a top view schematic diagram of an embodiment of the utility model.
[0026] Figure 5 It is an embodiment of the utility model Figure 4 AA section diagram.
[0027] Figure 6 It is a product schematic diagram of an embodiment of the utility model.
[0028] Figure 7 It is an embodiment of the utility model Figure 6 Schematic diagram from another angle.
[0029] Description of the accompanying drawings:
[0030] 10, upper mold 11, mold core 12, vibration plate 13, connecting seat 14, exhaust port 15, heating rod 16, cooling pipe 17, feeding hole 20, lower mold 21, cavity 22, protrusion 23, ejector 24, push rod 25, molding block 27, product 28, ejector 29, connecting port. DETAILED DESCRIPTION
[0031] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose of the utility model, the specific implementation method, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0032] Please refer to Figures 1 to 7 As shown, it shows the specific structure of the preferred embodiment of the utility model, which is a powder molding mold.
[0033] The upper mold 10 and the lower mold 20 are provided with a vibration plate 12 on their sides, and the upper mold 10 is provided with a plurality of feeding holes 17 on its top. The raw materials are fed in from the plurality of feeding holes 17, and the vibration of the upper mold 10 allows the raw materials to enter the plurality of positions in the cavity 21 more smoothly from the feeding holes 17. The vibration of the lower mold 20 allows the raw materials to be evenly distributed in the cavity 21, and this material distribution method is efficient and even.
[0034] The present application provides a powder forming mold, comprising an upper mold 10 and a lower mold 20 that can be closed together; the upper mold 10 is provided with a mold core 11, and the lower mold 20 is provided with a mold cavity 21; the surfaces of the mold core 11 and the mold cavity 21 are both provided with a protective layer; the sides of the upper mold 10 and the lower mold 20 are provided with a vibration plate 12, and the vibration plate 12 is connected to the output end of the vibrator; the top of the upper mold 10 is provided with a plurality of feeding holes 17, and the side of the mold core 11 is provided with There are several exhaust ports 14; the feed hole 17 and the exhaust port 14 are connected to the exhaust port 14; the ejector pin 2823 and the molding block 25 are arranged horizontally in the cavity 21, and the molding block 25 and the ejector pin 2823 can extend from the cavity 21; the upper mold 10 and the lower mold 20 are penetrated by multiple heating rods 15 and cooling tubes 16, and the corresponding heating rods 15 can heat the mold core 11 and the cavity 21; the cooling tube 16 can cool the mold core 11 and the cavity 21. The upper mold 10 and the lower mold 20 are preferably made of metal that is resistant to high temperature and has high hardness and strength. The upper mold 10 and the lower mold 20 can be closed together. The preferred working steps of the process: 1. The upper mold 10 and the lower mold 20 are partially closed (not completely closed at this time), and the vibrator (preferably an ultrasonic vibrator or a vibration motor) vibrates the vibration plate 12, so that the upper mold 10 and the lower mold 20 are vibrating. 2. Multiple feeding pipes simultaneously feed the raw materials from different feeding holes 17, and then enter the cavity 21 of the lower mold 20. Since it is multi-point feeding and vibrating, the raw materials are very uniform while feeding, which is more efficient. This step can be done once or multiple times. (For example, partially close the mold to add raw materials, partially open the mold, add raw materials, and repeat continuously to ensure that the added raw materials meet the design standards) 3. After the raw materials are filled in place, the upper mold 10 and the lower mold 20 are completely closed. 4. The heating rod 15 heats the upper mold 10 and the lower mold 20 to melt the raw materials in the cavity 21. The exhaust port 14 discharges excess gas to ensure that the internal pressure is within the design range. Subsequently, the cooling pipe 16 cools the upper mold 10 and the lower mold 20 to accelerate the molding of the product 27. 5. Open the mold, and the ejector 2823 ejects the product 27 from the cavity 21. The vibration plate 12 is provided with at least one vibration connection seat 13. In this embodiment, there are a plurality of vibration connection seats 13. The vibration connection seats 13 are responsible for receiving energy from the vibrator.
[0035] Preferably, the lower die 20 is penetrated by a push rod 24; part of the push rod 24 is obliquely penetrated by the lower die 20; the molding block 25 is formed on the upper end of the push rod 24; and a connection port 29 is provided at the lower end of the push rod 24. The connection port 29 is used to connect an external driving component, so that the molding block 25 can be driven to move up and down by the push rod 24. Part of the push rod 24 is obliquely penetrated by the lower die 20, and this design allows the molding block 25 to move relatively smoothly, avoiding disturbing the raw material in the cavity 21.
[0036] Preferably, the depth of the exhaust port 14 is between 5 μm and 10 μm, for example, 5 μm, 6 μm, 7 μm, 8 μm, 9 μm, and 10 μm, which is specifically set according to design requirements.
[0037] Preferably, the protective layer is one of a ceramic wear-resistant layer and a metal nitride layer. The main component of the ceramic wear-resistant layer is aluminum oxide or silicon oxide, and its hardness can reach Rockwell hardness above 90, and it has extremely high wear resistance. This type of coating is suitable for high-temperature, high-pressure, and high-speed working environments, such as boiler heating surfaces, lubricating oil pumps, turbine impellers and other mechanical equipment, and can effectively prevent surface wear, corrosion and oxidation of components. Metal nitriding refers to the process of exposing the surface of a metal material to high temperature and high pressure of gases such as nitrogen, so that nitrogen atoms react with the metal surface to form a nitride layer. Metal nitriding can significantly improve the hardness, wear resistance, corrosion and fatigue life of metal materials. The protective layer can effectively increase the service life of the mold. The protective layer can be set on the mold by sintering or coating.
[0038] Preferably, the thickness of the protective layer is between 1 and 3 mm, for example, 1 mm, 2 mm, 3 mm, and of course other values are also possible.
[0039] Preferably, the heating rod 15 is made of one of nickel-chromium alloy, iron-chromium-aluminum alloy and silicon carbide. The heating rod 15 can withstand very high temperatures and can effectively melt the raw materials in the cavity 21 .
[0040] Preferably, the cooling tube 16 is one of a stainless steel tube, a molybdenum tube, a titanium alloy tube, and a nano-ceramic tube. The cooling tube 16 can withstand very high temperatures. A coolant (such as cooling water) is passed into the cooling tube 16, which can effectively accelerate the molding of the product 27 and improve production efficiency.
[0041] Preferably, a protrusion 22 is provided at the position of the cavity 21 corresponding to the feed hole 17, and the protrusion 22 can block the feed hole 17. The cross section of the feed hole 17 is preferably an isosceles trapezoid, which is more conducive to allowing the raw material to fall into the cavity 21 more evenly under the action of the vibration force. When the mold is completely closed, the protrusion 22 can block the feed hole 17. This design can effectively prevent the molten raw material from overflowing and ensure the sealing of the mold.
[0042] Preferably, there is at least one row of the heating rods 15 and the cooling tubes 16, and the heating rods 15 and the cooling tubes 16 are arranged alternately. This design can make the heating and cooling very uniform and more efficient during operation.
[0043] Preferably, the lower mold 20 is provided with at least one pressure sensor, and the upper mold 10 can trigger the pressure sensor. The pressure sensor can monitor the degree of mold closing between the upper mold 10 and the lower mold 20 in real time through pressure, thereby ensuring the processing quality and monitoring the working state of the mold.
[0044] In summary, the design focus of the utility model is that the sides of the upper mold 10 and the lower mold 20 are provided with a vibration plate 12, and the vibration plate 12 is connected to the output end of the vibrator; the top of the upper mold 10 is provided with a plurality of feeding holes 17. The raw materials are fed in from the multiple feeding holes 17, and the vibration allows the raw materials to enter the multiple positions in the cavity 21 more smoothly from the feeding holes 17. The vibration of the lower mold 20 can make the raw materials evenly distributed in the cavity 21. This multi-point vibration feeding and material distribution method is more efficient, does not require manual uniformity, and the quality of the material distribution is also better.
[0045] The above description is only a preferred embodiment of the present invention and does not constitute any form of limitation to the present invention. Although the present invention has been disclosed as a preferred embodiment as above, it is not intended to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A powder forming die, characterized in that: It comprises an upper mold and a lower mold that can be closed together; the upper mold is provided with a mold core, and the lower mold is provided with a mold cavity; the surfaces of the mold core and the mold cavity are both provided with a protective layer; the sides of the upper mold and the lower mold are provided with a vibration plate, and the vibration plate is connected to the output end of the vibrator; The top of the upper mold is provided with a plurality of feeding holes, and the side of the mold core is provided with a plurality of exhaust ports; the feeding holes and the exhaust ports are communicated with the exhaust ports; Ejectors and forming blocks are arranged transversely in the cavity, and the forming blocks and ejectors can extend from the cavity; The upper mold and the lower mold are penetrated by a plurality of heating rods and cooling tubes, and the corresponding heating rods can heat the mold core and the mold cavity; and the cooling tubes can cool the mold core and the mold cavity.
2. A powder forming die according to claim 1, characterized in that: The lower die is penetrated by a push rod; part of the push rod is obliquely penetrated by the lower die; the molding block is molded on the upper end of the push rod; and a connecting port is arranged at the lower end of the push rod.
3. A powder forming die according to claim 1, characterized in that: The depth of the exhaust port is between 5 μm and 10 μm.
4. A powder forming die according to claim 1, characterized in that: The protective layer is one of a ceramic wear-resistant layer and a metal nitride layer.
5. A powder forming die according to claim 1 or 4, characterized in that: The thickness of the protective layer is between 1 and 3 mm.
6. A powder forming die according to claim 1, characterized in that: The heating rod is made of one of nickel-chromium alloy, iron-chromium-aluminum alloy and silicon carbide.
7. A powder forming die according to claim 1 or 6, characterized in that: The cooling tube is one of a stainless steel tube, a molybdenum tube, a titanium alloy tube, and a nano ceramic tube.
8. The powder forming die according to claim 1, characterized in that: A protrusion is arranged at the position of the cavity corresponding to the feeding hole, and the protrusion can block the feeding hole.
9. The powder forming die according to claim 1, characterized in that: There is at least one row of heating rods and cooling tubes, and the heating rods and cooling tubes are arranged alternately.
10. The powder forming die according to claim 1, characterized in that: The lower die is provided with at least one pressure sensor, and the upper die can trigger the pressure sensor.