Bridgman-stockbarger growth device for preparing tellurium dioxide acousto-optic crystals
By using a combination design of T-type heat insulating block and U-type heating rod in the crucible descent growth equipment, the problem of insufficient temperature field symmetry is solved, and the temperature gradient suitable for the growth of tellurium dioxide crystals and the solid-liquid interface shape are achieved. Improves crystal quality and utilization and reduces maintenance costs.
Patent Information
- Application Number
- CN202420558687.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-21
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2034-03-21
AI Technical Summary
The temperature field symmetry in the existing crucible descent growth equipment is not high, resulting in large differences in isothermal shapes and insufficient temperature gradient, which affects the quality and utilization rate of tellurium dioxide crystals and is also high maintenance costs.
A crucible drop growth device including a T-type heat insulating block and a U-type heating rod was designed. Through the directional thinning structure of the T-type heat insulating block and the series connection of the U-type heating rod, a suitable tellurium dioxide crystal growth was constructed. The temperature gradient region achieves uniformity and stability of the temperature gradient, and optimizes the crucible position through the lifting mechanism and the down-tube to maintain the stability of the solid-liquid interface.
The temperature gradient range of 20-50℃/cm is achieved, which reduces the problems of polycrystalline, envelope and component supercooling in crystal growth, improves the quality and utilization rate of tellurium dioxide crystals, and reduces the maintenance cost of equipment.
Smart Images

Figure CN221971728U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of artificial crystal growth equipment, in particular to a crucible descent method growth device for preparing tellurium dioxide acousto-optic crystals. Background Art
[0002] Tellurium dioxide (TeO2) crystal is an acousto-optic material with excellent acousto-optic properties and is widely used in pulse fiber laser modulation and laser radar. The general industrial growth methods of tellurium dioxide crystals mainly include the pulling method and the crucible descent method. In the crucible descent method growth equipment, the temperature gradient in the gradient zone in the middle section of the equipment is used as the driving force for crystal growth. Since two long straight silicon molybdenum rods are used for heating, the high temperature zone and gradient zone required for crystal growth are formed. The temperature field symmetry is not high, and the isotherms and solid-liquid interface shapes at different positions of the furnace body are quite different. At the same time, the heating element is prone to aging and deformation, and the repeatability and consistency of the temperature field will be affected. In particular, for a crystal growth furnace with multiple crucibles, the temperature field difference between the central heating area and the edge area is large. The patent application with publication number CN117344371A discloses a device for growing crystals by a multi-crucible descent method, which reduces the temperature difference between multiple crucibles by setting multiple furnace bodies, each furnace body is equipped with a crucible, and a special structure of induction coil. This improvement method increases manufacturing costs and is not conducive to later maintenance.
[0003] In the process of growing crystals by the crucible descent method, the shape of the solid-liquid interface has a great influence on the quality of crystal growth. Generally, the ideal state pursued by people should be a convex solid-liquid interface, or at least a flat interface, while a concave interface is often considered to be the source of crystal defects such as bubbles, dislocations, and cloud inclusions. In addition, the temperature gradient of the existing crucible descent method growth equipment is small, and it is not easy to form the large temperature gradient and slightly convex solid-liquid interface required for the growth of tellurium dioxide crystals. The grown crystals are prone to defects such as scattering, envelopment, and component supercooling, and the utilization rate is not high. Patent CN101220502B uses segmented heating to solve the problem of component supercooling caused by the small axial temperature gradient. This method of adjusting the temperature field by only adjusting the external heater is difficult to achieve a large adjustment and precise control of the temperature gradient in the center of the thermal field during the crystal growth process, resulting in the inability to effectively adjust the crystal growth interface and the continuous deepening of the concave interface in the later stage of crystal growth. Utility Model Content
[0004] In view of the above-mentioned deficiencies in the prior art, the purpose of the utility model is to provide a crucible descent method growth device suitable for preparing tellurium dioxide crystals. On the one hand, it reduces the shape differences of multi-station crucible isotherms, and on the other hand, it solves the problem of defects caused by too narrow temperature gradient during the growth of tellurium dioxide crystals, so that the crystal can stably maintain a flat or slightly convex solid-liquid interface, effectively reducing problems such as polycrystalline, envelope and component overcooling during crystal growth, achieving the growth of high-quality tellurium dioxide crystals, and greatly improving the quality and effective utilization rate of the crystals.
[0005] In order to achieve the above-mentioned purpose, the technical solution provided by the utility model is: a crucible descent method growth device for preparing tellurium dioxide acousto-optic crystals, including a furnace body and a lifting mechanism, the furnace body includes an outer wall and an inner cavity, the outer wall is made of thermal insulation material, the inner cavity is provided with an insulation block to divide the inner cavity into a high temperature zone, a temperature gradient zone and a low temperature zone, the high temperature zone is the cavity above the insulation block, and the low temperature zone is the cavity part between the bottom of the insulation block and the furnace mouth; there is a temperature gradient zone between the high temperature zone and the low temperature zone; the insulation block is a T-shaped insulation block, and the T-shaped insulation block includes a first horizontal block and a second vertical block; the high temperature zone is provided with a plurality of U-shaped heating rods. The lifting mechanism is arranged at the bottom of the furnace body to realize the longitudinal movement of the crucible in the furnace body. The inner wall of the furnace body and the T-shaped insulation block are both made of Morgan refractory bricks.
[0006] Furthermore, the T-shaped heat insulation block is a directionally thinned structure, that is, the width of the first horizontal block is greater than the width of the second vertical block.
[0007] Preferably, the width ratio of the first horizontal block to the second vertical block is in the range of 2:1 to 3:1; the height ratio of the first horizontal block to the second vertical block is in the range of 1:1 to 1:2.
[0008] Preferably, the total height of the T-shaped insulation block is 30-40 mm.
[0009] In one embodiment, the furnace body is provided with a down-conductor, which is connected to the lifting mechanism, and the crucible is placed in the down-conductor. The number of down-conductors is the same as the number of crucibles. The down-conductor can be fixed on the lifting mechanism or can be detachable. Preferably, the furnace body can accommodate 2 to 20 down-conductors arranged side by side.
[0010] Preferably, the first cross block has a notch matching the outer diameter of the crucible or the downconductor.
[0011] Preferably, the U-shaped heating rods are arranged vertically at equal intervals in the furnace body and vertically above the T-shaped insulation blocks.
[0012] Preferably, the U-shaped heating rods are heated in series.
[0013] In one embodiment, a temperature measuring thermocouple is provided in the furnace body. It is a more preferred method to arrange the temperature measuring thermocouple in the downconductor.
[0014] Beneficial effects of the utility model:
[0015] 1. The utility model constructs a temperature gradient and solid-liquid interface shape suitable for the growth of tellurium dioxide crystals through the differentiated gradient zone design in the furnace body, the structure of the T-type insulation block and the improvement of the heating method, and realizes a temperature gradient range of 20 to 50°C / cm, which is more suitable for the larger temperature gradient range required for the growth of tellurium dioxide crystals, which is 10 to 20% higher than before, adapts to the driving force required for the growth of tellurium dioxide crystals, and is conducive to the purification and removal of raw materials during crystal growth. At the same time, it can effectively reduce the problems of polycrystalline, envelope and component supercooling during crystal growth, adapt to the growth of high-quality tellurium dioxide crystals, and greatly improve the quality and effective utilization rate of crystals.
[0016] 2. The utility model adopts a U-shaped heating rod to replace the original long straight heating rod, which improves the uniformity and stability of the overall temperature field of the equipment and greatly reduces the shape difference of the isotherms of each workstation.
[0017] 3. By adopting the gradient zone design of the utility model and the serial connection of multiple groups of U-shaped heating rods, multiple parallel crucible stations can be set in the furnace body, not limited to concentric circle distribution, the temperature field on the outside and the center is uniform and stable, and multiple tellurium dioxide crystals can be grown at the same time. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a structural schematic diagram of the utility model.
[0019] Figure 2 yes Figure 1 Cross-section view at AA in the middle.
[0020] Figure 3 yes Figure 1 Cross-section view at the middle BB.
[0021] Figure 4 It is a structural schematic diagram of a T-shaped heat insulation block of the utility model.
[0022] Figure 5 It is a schematic diagram of the use of the utility model.
[0023] Figure 6 It is the actual furnace temperature distribution curve of the utility model and the existing equipment.
[0024] Figure numerals: 1. furnace body; 2. T-shaped insulation block; 3. first horizontal block; 4. second vertical block; 5. U-shaped heating rod; 6. downconductor; 7. temperature measuring thermocouple; 8. crucible; 9. lifting mechanism; 10. high temperature zone; 11. temperature gradient zone; 12. low temperature zone; 13. raw material; 14. seed crystal; 15. magnesium oxide powder. DETAILED DESCRIPTION
[0025] In order to better understand the technical solution of the utility model, the embodiments of the utility model are described in detail below in conjunction with specific embodiments. It should be clear that the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0026] The terms used in the embodiments of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The singular forms "a", "the" and "the" used in the embodiments of the present invention and the appended claims are also intended to include the plural forms unless the context clearly indicates other meanings. The test materials used in the present invention are all common commercial products and can be purchased on the market.
[0027] Reference Figure 1 and Figure 6 As shown, Figure 1 The schematic cross-sectional view of the structure of the utility model shows a crucible descent method growth device for preparing tellurium dioxide acousto-optic crystals, which includes a furnace body 1 and a lifting mechanism 9. The furnace body 1 includes an outer wall and an inner cavity. The outer wall is made of heat-insulating material. The inner cavity is provided with an insulation block to divide the inner cavity into a high-temperature zone 10, a temperature gradient zone 11 and a low-temperature zone 12. The high-temperature zone 10 is the cavity above the insulation block, and the low-temperature zone 12 is the cavity between the bottom of the insulation block and the furnace mouth. There is a temperature gradient zone 11 between the high-temperature zone 10 and the low-temperature zone 12. The insulation block is a T-shaped insulation block 2, which includes a first horizontal block 3 and a second vertical block 4. The high-temperature zone 10 is provided with a plurality of U-shaped heating rods 5. The lifting mechanism 9 is arranged at the bottom of the furnace body 1 to realize the longitudinal movement of the crucible 8 in the furnace body 1. The inner wall of the furnace body 1 and the T-shaped insulation block 2 are both made of Morgan refractory bricks.
[0028] The T-shaped heat insulation block 2 is a structure that is wide at the top and narrow at the bottom and is directionally thinned; in one embodiment of the utility model, the width ratio of the first horizontal block 3 to the second vertical block 4 is in the range of 2:1 to 3:1, and the height ratio of the first horizontal block 3 to the second vertical block 4 is in the range of 1:1 to 1:2. Figure 4As shown, the widths are represented by d1 and d2, respectively, and the heights are represented by h1 and h2, respectively. Preferably, the overall height of the T-shaped insulation block 2 is 30 to 40 mm. Through the structural design of the directionally thinned T-shaped insulation block 2, the growth of tellurium dioxide crystals in a larger temperature gradient range is achieved, which is beneficial to the purification and removal of raw materials during crystal growth and reduces component overcooling. However, if the T-shaped insulation block is changed to a uniformly directional thinning method such as an isosceles triangle or an isosceles trapezoid, the temperature field in the furnace body 1 will be disturbed, which is not conducive to the formation and growth of tellurium dioxide crystals.
[0029] As one of the preferred embodiments, a down-conductor 6 is provided in the furnace body 1, and a crucible 8 is placed in the down-conductor 6, and the down-conductor 6 is connected to a lifting mechanism 9. The down-conductor 6 can keep the crucible 8 vertical and not tilted on the one hand, and further insulate the crucible 8 on the other hand to prevent the crucible 8 from rising or falling too quickly in temperature. The number of down-conductors 6 is consistent with the number of crucibles 8. The utility model adds the structure of the down-conductor 6, and places the crucible 8 in the down-conductor 6. The crucible 8 contains raw materials 13 and seed crystals 14. The position of the crucible 8 in the furnace body 1 is adjusted by the lifting mechanism 9 to achieve controlled melting of the raw materials 13 and seed crystals 14, and to achieve directional solidification growth of tellurium dioxide crystals. Preferably, the furnace body 1 of the utility model can accommodate 2 to 20 down-conductors in a side-by-side combination.
[0030] Furthermore, the first cross block 3 can be matched with different notches according to the shape and size of the actual crucible 8 or downconductor 6, such as an arc notch, a square notch or a U-shaped notch, etc., to match the outer diameter of the crucible or downconductor 6, such as Figure 3 The square notches shown are used to grow tellurium dioxide crystals of different orientations, specifications, and shapes. Figure 3 yes Figure 1 The cross-sectional view at point B is a top view schematic diagram of the temperature gradient zone 11.
[0031] On the other hand, see Figure 2 , Figure 2 yes Figure 1 The cross-sectional view is taken at point A in the figure. The U-shaped heating rods 5 in the furnace body 1 are arranged vertically and evenly spaced (not fully marked in the figure). More specifically, the U-shaped heating rods 5 are vertically above the T-shaped insulation block 2. The U-shaped heating rods 5 are externally connected to a corresponding temperature control system (not shown in the figure). Preferably, the U-shaped heating rods 5 are heated in series. Through the improvement of the insulation block and the coordinated effect with the U-shaped heating rods 5, the utility model can achieve a temperature gradient range of 20 to 50°C / cm. In addition, the utility model replaces the two long straight rods used in the prior art for heating by using the U-shaped heating rod 5, that is, by changing the layout and structure of the heating rods in the equipment, the uniformity and stability of the overall temperature field are ensured, and at the same time, the isothermal differences of each station in the furnace body 1 can be effectively adjusted to optimize the solid-liquid interface during crystal growth, so that it can always approximately maintain a plane or slightly convex to the melt.
[0032] As one of the preferred embodiments, a temperature measuring thermocouple 7 is provided in the furnace body 1. More preferably, the temperature measuring thermocouple 7 is placed in the downconductor 6.
[0033] The working mode of the utility model is as follows Figure 5 As shown: the crucible 8 contains raw materials 13 and seed crystals 14, and the crucible 8 is placed in the downconductor 6, and the other space between the crucible 8 and the downconductor 6 is filled with magnesium oxide powder 15. When the tellurium dioxide crystal is grown by the crucible descending method, the downconductor 6 is gradually raised by the lifting mechanism 9 to place the crucible 8 in the high temperature zone 10 to melt the raw materials 13 and the seed crystal 14 in a controlled manner. At this time, the melting condition of the seed crystal 14 can be judged by the value of the temperature measuring thermocouple 7 and the height of the downconductor 6 in the furnace body 1. The position of the crucible 8 or the downconductor 6 in the furnace body 1 is adjusted by the lifting mechanism 9 to make the crucible 8 move from the high temperature zone 10 through the temperature gradient zone 11 to the low temperature zone 12. After the crucible 8 enters the temperature gradient zone 11, the melt is directional cooled, and the part that first reaches a temperature below the melting point crystallizes and cools with the continuous movement of the crucible 8. The crystallization interface or solid-liquid interface grows directional in the opposite direction to its movement, realizing the continuous directional solidification growth of the tellurium dioxide crystal.
[0034] In the existing device, two long straight silicon-molybdenum rods are used for heating. The shapes of the isotherms of various stations in the furnace body 1 are quite different. The height position of the solid-liquid interface in the crucible of different stations can differ by 20 to 40 mm. If the temperature field of the furnace body 1 is not systematically adjusted and the layout and structure of the heating rods are not changed, it is easy to cause the solid-liquid interface of the stations on both sides to be seriously convex, and the solid-liquid interface of the middle station to have a concave interface, which is easy to cause defects such as polycrystalline and envelope in the crystal.
[0035] In addition, the original rectangular insulation block design will cause the overall temperature gradient range of the temperature gradient zone 11 to be relatively consistent, but the temperature gradient is relatively small, about 10-40°C / cm, which is easy to cause problems such as component overcooling and low effective length utilization during crystal growth. Through the differentiated T-shaped insulation block 2 shape design, the temperature gradient at the solid-liquid interface in the crucible 8 is increased to ensure the larger temperature gradient required for the growth of tellurium dioxide crystals. This can effectively reduce the problems of polycrystalline, envelope and component overcooling during crystal growth, adapt to the growth of high-quality tellurium dioxide crystals, and greatly improve the quality and effective utilization of crystals. Figure 6It is the actual furnace temperature distribution curve of the utility model and the existing equipment. From the figure, it can be seen that the difference in temperature field before and after the improvement, especially near the melting point of tellurium dioxide in the temperature gradient zone (represented by Tm in the figure), has a larger temperature gradient range after the improvement. The temperature field is composed of a system dimension. After the adjustment of the temperature gradient zone 11, the temperature gradient of the growth can be increased by 10-20% compared with before, that is, 5-10℃ / cm, which can effectively eliminate the defects of component supercooling, scattering and encapsulation in the growth of tellurium dioxide crystals.
[0036] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A crucible descent method growth device for preparing tellurium dioxide acousto-optic crystals, comprising a furnace body and a lifting mechanism, wherein the lifting mechanism is arranged at the bottom of the furnace body; the furnace body comprises an outer wall and an inner cavity, wherein the outer wall is made of a heat-insulating material, and the inner cavity is provided with a heat-insulating block to divide the inner cavity into a high-temperature zone, a temperature gradient zone and a low-temperature zone, wherein the high-temperature zone is the cavity above the heat-insulating block, and the low-temperature zone is the cavity part between the bottom of the heat-insulating block and the furnace mouth, wherein the furnace body comprises an outer wall and an inner cavity, wherein the outer wall is made of a heat-insulating material, and the inner cavity is provided with a heat-insulating block to divide the inner cavity into a high-temperature zone, a temperature gradient zone and a low-temperature zone, wherein the high-temperature zone is the cavity above the heat-insulating block, and the low-temperature zone is the cavity part between the bottom of the heat-insulating block and the furnace mouth, wherein the furnace body comprises an outer wall and an inner cavity, wherein the outer wall is made of a heat-insulating material, and the inner cavity is provided with a heat-insulating block to divide the inner cavity into a high-temperature zone, a temperature gradient zone and a low-temperature zone, wherein the high-temperature zone is the cavity above the heat-insulating block, and the low-temperature zone is the cavity part between the bottom of the heat-insulating block and the furnace mouth, and ... The insulation block is a T-shaped insulation block, which includes a first horizontal block and a second vertical block; a plurality of U-shaped heating rods are arranged in the high temperature zone; a down-conductor is arranged in the furnace body, and the down-conductor is connected to the lifting mechanism.
2. The device according to claim 1, characterized in that The width ratio of the first horizontal block to the second vertical block is 2:1 to 3:
1.
3. The device according to claim 1, characterized in that The height ratio of the first horizontal block to the second vertical block is 1:1 to 1:
2.
4. The device according to claim 1, characterized in that The total height of the T-shaped heat insulation block is 30-40 mm.
5. The device according to claim 1, characterized in that The first cross piece has a notch matching the outer diameter of the crucible or the downconductor.
6. The device according to claim 1, characterized in that The U-shaped heating rods are arranged vertically and evenly in the furnace body and vertically above the T-shaped insulation blocks.
7. The device according to claim 1, characterized in that The U-shaped heating rods are connected in series.
8. The device according to claim 1, characterized in that The furnace body can accommodate 2 to 20 downconductors arranged side by side.
9. The device according to claim 1, characterized in that A temperature measuring thermocouple is arranged in the furnace body.
10. The device according to claim 9, characterized in that The temperature measuring thermocouple is placed in the down-conductor.
Citation Information
Cited By
Equipment and method for growing various crystals in single furnace
CN120625156A
Equipment and method for growing multiple crystals in a single furnace
CN120625156B