Navigation mark floating body and navigation mark

By using PET foam material and graphene coating combined with the skeleton structure of continuous fiber-reinforced PET composite materials, the problems of easy corrosion, poor dimensional stability and non-environmental protection of navigation mark materials are solved, achieving an efficient, environmentally friendly and recyclable solution for navigation marks. plan.

CN221852136UActive Publication Date: 2024-10-18NANJING CHEM FIBER CO LTD +2
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323420139.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-14
Publication Date
2024-10-18
Estimated Expiration
2033-12-14

AI Technical Summary

Technical Problem

Existing navigation mark materials are easy to rust, have poor dimensional stability, are easy to fade, and are not environmentally friendly, which limits their promotion in the field of navigation marks.

Method used

PET foam material is used as the base material, and the outside is coated with graphene coating. Combined with the skeleton structure profile of continuous fiber reinforced PET composite material, it is fixed by thermal fusion to form an overall structure to ensure the structural strength, anti-corrosion performance and Environmentally friendly recyclability.

Benefits of technology

It improves the dimensional stability, anti-corrosion performance and environmentally friendly recyclability of the navigation mark, reduces production costs and assembly difficulty, avoids material filling and recycling pollution problems, and meets the needs of long-term outdoor use.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221852136U_ABST
    Figure CN221852136U_ABST
Patent Text Reader

Abstract

The utility model relates to a navigation mark floating body and a navigation mark. The navigation mark floating body comprises a floating body, the floating body comprises at least one base material, and the base material is a PET foaming material; the framework structure profile is a continuous fiber reinforced PET composite material, the continuous fiber reinforced PET composite material comprises a plurality of fiber layers and a PET layer, the fiber layers are mutually stacked, the PET layer wraps the outer sides of the fiber layers, and the PET layer of the framework structure profile is fixed to the base material in a hot fusion mode; the protective coating is attached to the outer side of the base material and the outer side of the skeleton structure profile, and the protective coating comprises a graphene coating.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field related to navigation marks, and in particular to a navigation mark buoy and a navigation mark. Background Art

[0002] A navigation mark is an artificial sign that helps guide ships, locate and mark obstacles and issue warnings.

[0003] Most of the current navigation marks are made of steel or produced using MDPE (medium-density polyethylene) rotational molding technology. The former is limited in promotion due to steel prices and rust issues, while the latter has poor dimensional stability due to the large shrinkage rate of MDPE. The product also has defects such as easy fading under sunlight and being environmentally unfriendly, which limits the further promotion of rotational molding MDPE in the field of navigation marks. Summary of the invention

[0004] Based on this, it is necessary to provide a navigation mark buoy, a navigation mark and a method for manufacturing a navigation mark buoy that can comprehensively solve the problems of high cost, easy rust, poor dimensional stability, easy fading and environmental pollution of the current navigation marks.

[0005] The present application first provides a navigation mark buoy, comprising:

[0006] A floating body, wherein the floating body comprises at least one substrate, and the substrate is a PET foam material;

[0007] A skeleton structure profile, wherein the skeleton structure profile is a continuous fiber reinforced PET composite material, wherein the continuous fiber reinforced PET composite material comprises a plurality of fiber layers stacked on each other and a PET layer wrapped around the outside of the fiber layers, wherein the PET layer of the skeleton structure profile is fixed to the substrate by thermal fusion;

[0008] and a protective coating, wherein the protective coating is attached to the substrate and the outer side of the skeleton structure profile, and the protective coating includes a graphene coating.

[0009] In one embodiment, a sheet layer is further fixed between the substrate and the protective coating, and the sheet layer is the continuous fiber reinforced PET composite material.

[0010] In one embodiment, the PET layer of the sheet layer is fixed to the substrate by thermal fusion.

[0011] In one embodiment, the graphene coating is a water-based graphene coating.

[0012] In one embodiment, the graphene content in the graphene coating is greater than or equal to 1.6%.

[0013] In one embodiment, the protective coating further comprises a topcoat layer attached to the outside of the graphene coating, and the topcoat layer is a combination of one or more of an acrylic polyurethane coating, a nano-organic silicon coating or a polyurea coating.

[0014] In one embodiment, the cross-section of each substrate is fan-shaped, and each substrate is fixed in sequence to form a hollow cylinder. The skeleton structure profile is located inside the hollow cylinder formed by each substrate and is fixed to each substrate respectively.

[0015] The present application also provides a navigation mark, including the above-mentioned navigation mark buoy, a lamp rack fixed on the top of the navigation mark buoy, a counterweight fixed on the bottom of the navigation mark buoy, a battery fixed inside the navigation mark buoy, and a solar panel and a navigation mark light respectively fixed on the lamp rack, wherein the solar panel is electrically connected to the battery, and the battery is electrically connected to the navigation mark light.

[0016] In one embodiment, the lamp frame is made of the continuous fiber reinforced PET composite material, and the PET layer of the lamp frame is fixed to the substrate by thermal fusion.

[0017] The above-mentioned navigation beacon buoy, in the first aspect, adopts PET foam material as the base material: (1) The PET foam material block is obtained by extruding PET particles filled with foaming gas at the foaming temperature. The material shrinkage stability of this process is higher than that of the rotational molding process; (2) The base material is obtained by cutting, milling, carving and / or bonding the PET foam material block, so that it can be ensured that the base material has a high dimensional accuracy, effectively reducing the difficulty of assembling the float body; (3) Since PET foam material has excellent thermal stability, it will not bubble at high outdoor temperatures.

[0018] Secondly, by coating the substrate and the outside of the skeleton structure with a graphene coating, the structural strength and anti-corrosion performance of the substrate are increased, which can effectively prevent the substrate from cracking, so that the inside of the substrate does not need to be filled with other materials, and can be made entirely of PET foam material. This not only eliminates the possibility of failure of the substrate due to water seepage inside the substrate caused by damage to the outer layer of the substrate, but also reduces the production cost and difficulty of production. When the outer layer of the substrate has a tendency to deform, the inner substrate can prevent the deformation of the outer layer of the substrate, thereby increasing the stability of the substrate.

[0019] The third aspect is to fix each substrate by a skeleton structure profile made of continuous fiber reinforced PET composite material: (1) Fibers are added to the PET material to form a PET fiber composite structure with a fiber layer inside and a PET layer wrapped outside. The fiber layer inside can act as a skeleton to improve the strength of the skeleton structure profile, while the external PET layer has good corrosion resistance and waterproof properties and will not pollute the environment; (2) The PET layer on the outside of the skeleton structure profile and the PET foam material of the substrate are both PET materials. The two can be directly hot-melt fixed to form an integral structure with high fixing strength and no additional fixing structure is required, which is conducive to the lightweight of the navigation mark; (3) The navigation mark buoy is fixed by the substrate made of PET foam material and the skeleton structure profile made of continuous fiber reinforced PET composite material through hot fusion and other methods. When the navigation mark buoy reaches the end of its service life, the navigation mark buoy can be melted and recycled, that is, the navigation mark buoy as a whole is environmentally friendly and recyclable. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is a schematic diagram of the exploded structure of the float body and the skeleton structure profile in the navigation buoy of this application;

[0021] Figure 2 This is a schematic diagram of the three-dimensional structure of the navigation mark for this application.

[0022] Figure numerals: 10, floating body; 11, substrate; 20, skeleton structure profile; 200, lamp holder; 300, counterweight; 400, battery; 500, solar panel; 600, navigation light. DETAILED DESCRIPTION

[0023] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the specific embodiments of the present invention are described in detail below in conjunction with the accompanying drawings. In the following description, many specific details are set forth to facilitate a full understanding of the present invention. However, the present invention can be implemented in many other ways different from those described herein, and those skilled in the art can make similar improvements without violating the connotation of the present invention, so the present invention is not limited by the specific embodiments disclosed below.

[0024] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0025] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "plurality" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0026] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements, unless otherwise clearly defined. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0028] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and are not intended to be the only implementation method.

[0029] Most of the mainstream navigation buoys on the current market first use MDPE (medium-density polyethylene) through a rotational molding process to manufacture a buoy unit, and then assemble multiple buoy units to obtain a complete navigation buoy; however, for the buoys manufactured by the rotational molding process of medium-density PE:

[0030] On the one hand, the rotomolding process has the characteristics of large material shrinkage and low stability, that is, the shrinkage of the floating unit obtained by rotomolding is difficult to control and the dimensional accuracy is poor, which leads to the problem that the holes of the floating unit obtained by rotomolding cannot be aligned during assembly, and the assembly is difficult;

[0031] On the other hand, since the floating body is used outdoors, the temperature difference between winter and summer is large, and PE has a low glass transition temperature and a low thermal deformation temperature. Therefore, the floating body made of PE is prone to deformation and bulging when the temperature is too high, affecting construction safety and possibly damaging the surface coating. It is easy to become brittle and damaged when the temperature is too low.

[0032] In addition, medium-density PE will fade after long-term use in outdoor environments and after being exposed to wind and sun, and the surface of the beacon is prone to cracking. If water from the external environment penetrates into the floating body through the cracks caused by the cracks, it may cause the floating body to sink. In this regard, most of the current methods will fill PU (polyurethane) or other foaming materials inside the PE material to fill the floating body to prevent water seepage; however, the above treatment method has the following problems:

[0033] 1. Increase production steps and increase production costs;

[0034] 2. It is difficult to control the amount of PU required to completely fill the PE material, the production process is complicated, and the production difficulty is high;

[0035] 3. The internal and external materials are different, and their thermal expansion coefficients are also different, resulting in no corresponding bonding between the two in high and low temperature environments, and unable to assist in suppressing the thermal deformation of the other. For example, at high temperatures, there is no force between the internal PU and the external PE, and the internal PU cannot prevent the external PE from bubbling;

[0036] 4. PE and PU materials cannot be recycled, and discarding them after the navigation mark reaches the end of its service life will cause environmental pollution.

[0037] For the above questions, please refer to Figure 1 As shown, the present application first provides a navigation mark buoy, including: a buoy body 10, the buoy body 10 includes at least one substrate 11, the substrate 11 is a PET foam material; a skeleton structure profile 20, the skeleton structure profile 20 is a continuous fiber reinforced PET composite material, the continuous fiber reinforced PET composite material includes multiple fiber layers stacked on each other and a PET layer wrapped on the outside of the fiber layer, the PET layer of the skeleton structure profile 20 is thermally fused and fixed to the substrate 11; and a protective coating, the protective coating is attached to the outside of the substrate 11 and the skeleton structure profile 20, and the protective coating includes a graphene coating. The advantages of the navigation mark buoy in the above embodiment of the present application compared with the traditional PE rotational molding navigation mark buoy are analyzed from three aspects:

[0038] First aspect:

[0039] This application uses PET foam material as the substrate 11;

[0040] (1) PET foam material blocks are obtained by extruding PET particles filled with foaming gas at the foaming temperature. The material shrinkage stability of this process is higher than that of the rotational molding process;

[0041] (2) The substrate 11 is made of a PET foam material block by cutting, milling, carving and / or bonding, so that the substrate 11 can have a high dimensional accuracy, effectively reducing the difficulty of assembling the floating body 10;

[0042] (3) Since PET foam material has excellent thermal stability, it will not bubble at high temperatures outdoors.

[0043] The above-mentioned PET foam material refers to a closed-cell thermoplastic renewable polymer foam material made by foaming polyethylene terephthalate using supercritical carbon dioxide; specifically, the PET foam material can be made by filling the base material with carbon dioxide or other gases in a supercritical fluid state or after high-temperature melting, and finally relying on an extruder to extrude and shape it, with relatively high production efficiency and an environmentally friendly process.

[0044] Specifically, PET foam material has the characteristics of good thermal stability (no softening at 150 degrees), adjustable density (60kg / m3 to 300kg / m3), high rigidity, adjustable toughness, good thermal insulation performance, low water absorption, excellent fatigue resistance, environmental protection, no pollution, and recyclability. Therefore, in this application, using PET foam material as the substrate 11 also has the advantages of weight reduction, high rigidity / weight ratio, high processing freedom, and recyclability.

[0045] Specifically, the PET foam material is formed by extruding the raw materials after the foaming gas is filled into the raw materials at the foaming temperature; wherein, in parts by mass, the raw materials include 89 to 96 parts of PET particles, 2 to 6 parts of chain extenders, and 1 to 5 parts of nucleating agents; the foaming gases are carbon dioxide and cyclopentane; and the foaming temperature is 250°C-280°C.

[0046] Second aspect:

[0047] The present application also increases the structural strength and corrosion resistance of the substrate 11 by coating a graphene coating on the outside of the substrate 11 and the skeleton structural profile 20, which can effectively prevent the substrate 11 from cracking, so that the inside of the substrate 11 does not need to be filled with other materials, and can be completely made of PET foam material. This not only eliminates the possibility of failure of the substrate 11 due to water seepage inside the substrate 11 caused by damage to the outer layer of the substrate 11, but also reduces the production cost and production difficulty. When the outer layer substrate 11 has a tendency to deform, the inner substrate 11 can prevent the outer layer substrate 11 from deforming, thereby increasing the stability of the substrate 11.

[0048] It should be noted that the currently commonly used anti-corrosion coatings, such as epoxy resin anti-corrosion coatings, have general anti-corrosion performance, poor acid resistance and limited service life, and most of them cannot meet the long-term service life requirements; more importantly, most anti-corrosion coatings can only resist corrosion, but have poor resistance to ultraviolet rays. They can only provide surface corrosion protection and cannot provide resistance to ultraviolet rays, which makes the substrate 11 vulnerable to damage by ultraviolet rays.

[0049] In the present application, a graphene coating is attached to the substrate 11 of the PET foam material, which can optimize the water absorption and corrosion resistance of the PET foam material, reduce the damage of ultraviolet rays to the substrate, reduce the adhesion of attached objects, and improve the physical and mechanical properties of the substrate 11, thereby meeting the needs of long-term use in outdoor corrosive environments.

[0050] The specific effects and principles of graphene coating in the above four aspects are as follows:

[0051] (1) In terms of optimizing water absorption and corrosion resistance, the graphene component in the graphene coating can greatly reduce the penetration rate of the corrosive medium into the substrate, thereby increasing the corrosion resistance of the coating and extending the protection time of the coating on the substrate; specifically, due to the special composition of graphene, the flaky structure of the graphene anti-corrosion coating at the microscopic level can play a maze effect to enhance the shielding effect against water, oxygen and chemical components.

[0052] (2) In terms of reducing the damage of ultraviolet rays to the substrate, the graphene component in the graphene coating also has a blocking effect on ultraviolet rays, thereby reducing the damage of ultraviolet rays to the substrate, so that the substrate of the PET foam material can maintain its original properties, thereby enabling the substrate to maintain excellent performance for a long time.

[0053] (3) In terms of reducing the attachment of marine attachments, the graphene coating can be completely integrated with the PET foam material, reducing the attachment of external corrosive media, including aquatic organisms such as algae and various shellfish; when used in outdoor environments, it can reduce the workload of cleaning and maintenance of the beacon buoy, which is conducive to maintaining the optimal performance of the original structure of the beacon buoy.

[0054] (4) In terms of improving the physical and mechanical properties of the substrate 11, graphene can penetrate into the PET foam material through the penetration effect with the PET foam material, thereby enhancing the strength and rigidity of the material itself; experimental verification shows that the graphene coating improves the tensile modulus, compressive strength / modulus, and shear strength / modulus of the PET foam material, and according to the different component ratios of the graphene coating (graphene coating is obtained by uniformly distributing graphene in the coating), different formulations of graphene coatings have different effects on improving the physical and mechanical properties of the PET foam material. Therefore, the formulation of the graphene coating can be adjusted according to the actual needs under a specific environment to increase the versatility of the navigation beacon buoy of the present application.

[0055] Specifically, the graphene coating used in the graphene coating is prepared from 30 to 40 parts by mass of an aqueous polyurethane resin, 30 to 35 parts of an acrylic emulsion, 10 to 25 parts of modified graphene, 1 to 3 parts of polydopamine, 0.01 to 1.2 parts of a penetrant, 0.01 to 1 part of an emulsifier, 0 to 0.05 parts of a defoaming agent, and 0 to 10 parts of a film-forming aid.

[0056] By combining the substrate 11, improving the graphene coating and optimizing the selection of additives, the dispersibility and compatibility of the graphene coating with the substrate 11 are improved, and the anti-corrosion performance of the graphene coating added to the substrate is improved, so that the coating can provide better anti-corrosion protection for the substrate 11.

[0057] The third aspect:

[0058] In the present application, each substrate 11 is fixed by a skeleton structure profile 12 made of continuous fiber reinforced PET composite material:

[0059] (1) Adding fibers into the PET material to form a PET fiber composite structure with an inner fiber layer and an outer PET layer wrapped therein. The inner fiber layer can act as a skeleton to improve the strength of the skeleton structure profile 12, while the outer PET layer has good corrosion resistance and waterproof performance and will not pollute the environment.

[0060] (2) The PET layer on the outside of the skeleton structural profile 12 and the PET foam material of the substrate 11 are both made of PET material, and the two can be directly hot-melted and fixed to form an integral structure, with high fixing strength and no need for additional fixing structure, which is conducive to lightweighting of the navigation mark;

[0061] (3) The navigation mark buoy is fixed by means of a base material 11 made of PET foam material and a skeleton structural profile 12 made of continuous fiber reinforced PET composite material through heat fusion or the like. When the navigation mark buoy reaches the end of its service life, the navigation mark buoy can be melted and recycled, that is, the navigation mark buoy as a whole is environmentally friendly and recyclable.

[0062] In addition, the skeleton structure profile 12 of continuous fiber reinforced PET composite material has the following advantages compared with the traditional alloy or steel structure profile: (1) light weight and high strength: low density of 1.65-1.8g / cm3, tensile strength of 200-300MPa, bending strength of 200-300MPa, strength comparable to ordinary steel, weight only 1 / 6 of steel; (2) strong dimensional stability and low deformation rate: the fiber surface in the new PET composite profile is activated and can form a chemical connection with the PET foam material under the action of the coupling agent, with low deformation rate and strong stability; (3) low water absorption: the water absorption rate is only 0.257%, which is suitable for use in harsh open-air and humid environments; (4) strong corrosion resistance: the new PET composite profile can resist acid, alkali, salt, some organic solvents and other corrosive erosion, and has good water resistance and aging resistance; (5) environmentally friendly and recyclable: due to the use of PET materials, it can be recycled and will not cause pollution to the environment.

[0063] The continuous fiber reinforced PET composite material in this application can be glass fiber, carbon fiber, basalt fiber, aramid fiber and other commonly used fibers. This fiber material can be a strip, a sheet (hot-melt bonded to the surface of the PET foam material for reinforcement) or a profile (replacing steel and used as a structural part). In some embodiments, the material of the bracket body is a continuous fiber reinforced PET composite material. In parts by mass, the raw materials of the continuous fiber reinforced PET composite material include 30 to 40 parts of PET particles, 50 to 70 parts of glass fiber, 1 to 5 parts of a compatibilizer, and 0 to 1 part of an antioxidant; wherein the glass fiber is a special glass fiber for PET thermoplastic.

[0064] Specifically, there is an angle between the orientations of each fiber layer and two adjacent fiber layers; it is understandable that the mechanical properties of the bracket body are different depending on the orientation of the fiber layer, and by changing the orientation of the fiber layer by changing the fiber addition method, such as 90 degrees or 45 degrees, the strength performance of the continuous fiber reinforced PET composite material can be changed to meet different needs; the strength performance of the continuous fiber reinforced PET composite material can also be changed by changing the number of fiber layers, thereby achieving the effect of meeting different needs.

[0065] In addition, the substrate 11 and the skeleton structure profile 12 can also be fixed by a special hot-compression synthesis process to solve the problem of fixing the PET foam material and the continuous fiber reinforced PET composite material. Specifically:

[0066] First, the prepreg is made, and the fiber composite material is completely impregnated by a solution impregnation method. The made prepreg is in a continuous strip shape; then it is processed into a molded part by heating and compression molding with PET foam; it is compatible with the same grade resin of the body and the structure is stable; finally, it is cooled to a temperature and crystallization time to improve the thermoplastic properties, energy saving, environmental protection, and recyclability.

[0067] In some embodiments, a sheet layer is further fixed between the substrate 11 and the protective coating. The sheet layer is a continuous fiber reinforced PET composite material. The PET layer of the sheet layer is fixed to the substrate 11 by thermal fusion.

[0068] By wrapping the substrate 11 with a sheet layer, the structural strength of the substrate 11 can be effectively increased and the amount of graphene coating used can be reduced. When the final structural strength is the same, the amount of graphene coating required for wrapping the substrate 11 with a sheet layer is far less than that for a solution without a sheet layer, which can reduce production costs.

[0069] The principles and advantages of thermally fixing and fusing the sheet layer with the substrate 11 are the same as those of thermally fixing and fusing the substrate 11 with the skeleton structural profile 12 described above, and the present application will not repeat them here. Such a setting can further improve the lightweight degree of the navigation mark buoy on the basis of ensuring the structural strength of the navigation mark buoy.

[0070] Preferably, the fiber layer in the sheet layer is in sheet shape, and the thickness of the sheet layer is between 0.5 mm and 1 mm.

[0071] In some embodiments, the graphene coating is a water-based graphene coating.

[0072] (1) Water-based graphene coatings release less VOC (volatile organic compounds) during the spraying process, and do not require a specific filtering structure. They can be directly applied by brush or spray, making the construction simple and environmentally friendly.

[0073] (2) When the navigation mark buoy is damaged due to external reasons, there is no need to transport the navigation mark buoy to the shore for repair and maintenance. It can be repaired directly in situ. Specifically, after the PET patch for repair is directly fixed on the substrate 11 by hot melt adhesive or thermal fusion, the water-based graphene coating can be sprayed directly in situ in the water. The water-based graphene coating will not float on the water surface and will not cause pollution to the environment, which further reduces the difficulty of maintaining the navigation mark buoy.

[0074] (3) Topcoat is also used to color navigation buoys to serve as color identification and warning lights.

[0075] In some embodiments, the graphene content in the graphene coating is greater than or equal to 1.6%. The graphene content in the currently commercially available graphene coating is around 0.5%, and its structural reinforcement effect on the PET foam material is not obvious. However, the present application uses a specially made graphene coating, and its internal graphene content is approximately equal to 1.6%. Only the graphene coating with a graphene content greater than or equal to 1.6% can play a significant reinforcement role on the PET foam material.

[0076] In some embodiments, the protective coating further comprises a topcoat layer attached to the outside of the graphene coating, and the topcoat layer is one or more combinations of an acrylic polyurethane coating, a nano-organic silicon coating or a polyurea coating.

[0077] Using the graphene coating as a primer layer and cooperating with the topcoat layer to form a composite coating can play a dual protective role. The topcoat layer can play an anti-aging role and increase the service life or durability of the protective coating under specific environmental conditions, while the primer layer can play an anti-corrosion role. The combination of the two can further increase the protective effect of the coating on the substrate 11.

[0078] Of course, other materials may also be selected for the topcoat layer as long as they can play an anti-aging role, and this application does not make any further limitations here.

[0079] In some embodiments, the thickness of the graphene coating is greater than or equal to 100 microns, and the thickness of the topcoat layer is greater than or equal to 80 microns.

[0080] It has been verified by experiments that when the thickness of the primer layer is 100 microns, the salt spray resistance index of the navigation mark buoy is 6200 hours, which can meet the needs of long-term use in marine environments; when the topcoat layer is an acrylic polyurethane coating and the thickness is 60 microns, the anti-aging test index is 1200 hours, and when the topcoat layer is a nano-silicone coating and the thickness is 80 microns, the anti-aging test index is 3000 hours. Both solutions can meet the needs of long-term use in marine environments.

[0081] The above-mentioned salt spray resistance test simulates the salt spray and other factors in the marine atmosphere or seaside atmosphere to evaluate the performance of the primer in the composite coating. It is mainly aimed at materials used in the seaside or marine environment, such as ships, marine engineering, marine equipment, etc.; the purpose of the anti-aging test is to evaluate the service life or durability of the topcoat in the composite coating under specific environmental conditions.

[0082] Please refer to Figure 1 As shown, in some embodiments, the cross-section of each substrate 11 is fan-shaped, and the substrates 11 are fixed in sequence to form a hollow cylindrical floating body 10. The skeleton structure profile 20 is located inside the hollow cylinder formed by each substrate 11 and is fixed to each substrate 11 respectively.

[0083] The present application does not further limit the specific number of substrates 11 , and the number of substrates 11 may be 2, 3, 4 or more, as long as they can surround the floating body 10 to form a hollow cylindrical shape.

[0084] Furthermore, in some embodiments, the outer circumferential surfaces of two adjacent substrates 11 are fixed by bolts along the circumferential direction; a groove with a triangular cross-section is formed between the two adjacent substrates 11, and the skeleton structure profile 20 extends along the vertical direction and can be fixed in the triangular groove.

[0085] In some embodiments, the floating body 10 includes a substrate 11, and the substrate 11 is in a hollow cylindrical shape.

[0086] Please refer to Figure 2 As shown, the second aspect of the present application provides a navigation mark, including the above-mentioned navigation mark buoy, a lamp rack 200 fixed on the top of the navigation mark buoy, a counterweight 300 fixed on the bottom of the navigation mark buoy, a battery 400 fixed inside the navigation mark buoy, and a solar panel 500 and a navigation mark light 600 respectively fixed on the lamp rack 200, wherein the solar panel 500 is electrically connected to the battery 400, and the battery 400 is electrically connected to the navigation mark light 600.

[0087] In some embodiments, there is a gap between the upper surface of the counterweight 300 and the lower surface of the floating body 10, and the counterweight 300 is provided with a through hole in the vertical direction; in the process of pulling the navigation mark to the set position, the navigation mark is tilted as a whole, and the through hole on the counterweight 300 is used to drain water to reduce resistance during the pulling process of the navigation mark; in addition, the through hole can also play a role in buffering and stabilizing the navigation mark after the navigation mark comes to rest.

[0088] In some embodiments, the lamp holder 200 is a continuous fiber reinforced PET composite material, and the PET layer of the lamp holder 200 is fixed to the substrate 11 by thermal fusion; the characteristics and effects of the continuous fiber reinforced PET composite material itself, as well as the effect of thermal fusion and fixation with the substrate 11 of the PET foam material are the same as described above, and the present application will not repeat them here. Such a setting can further improve the lightweight degree of the beacon while ensuring the overall structural strength of the beacon.

[0089] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0090] The above-mentioned embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A navigation mark buoy, characterized in that: include: A floating body (10), wherein the floating body (10) comprises at least one substrate (11), and the substrate (11) is a PET foam material; A skeleton structure profile (20), wherein the skeleton structure profile (20) is a continuous fiber reinforced PET composite material, wherein the continuous fiber reinforced PET composite material comprises a plurality of fiber layers stacked on each other and a PET layer wrapped around the outside of the fiber layers, and the PET layer of the skeleton structure profile (20) is fixed to the substrate (11) by thermal fusion; and a protective coating, wherein the protective coating is attached to the substrate (11) and the outer side of the skeleton structure profile (20), and the protective coating comprises a graphene coating.

2. The navigation mark buoy according to claim 1, characterized in that: A sheet material layer is also fixedly arranged between the substrate (11) and the protective coating, and the sheet material layer is the continuous fiber reinforced PET composite material.

3. The navigation mark buoy according to claim 2, characterized in that: The PET layer of the sheet layer is fixed to the substrate (11) by thermal fusion.

4. The navigation mark buoy according to claim 2, characterized in that: The fiber layer in the sheet material layer is in sheet shape, and the thickness of the sheet material layer ranges from 0.5 mm to 1 mm.

5. The navigation mark buoy according to claim 1, characterized in that: The graphene coating is a water-based graphene coating.

6. The navigation mark buoy according to claim 1, characterized in that: The graphene content in the graphene coating is greater than or equal to 1.6%.

7. The navigation mark buoy according to claim 1, characterized in that: The protective coating also includes a topcoat layer attached to the outside of the graphene coating, and the topcoat layer is one or more combinations of acrylic polyurethane coating, nano-organic silicon coating or polyurea coating.

8. The navigation mark buoy according to claim 1, characterized in that: The floating body (10) includes at least two substrates (11), each of which has a fan-shaped cross-section. The substrates (11) are fixed in sequence to form a hollow cylinder. The skeleton structure profile (20) is located inside the hollow cylinder formed by the substrates (11) and is fixed to each substrate (11) respectively.

9. A navigation mark, characterized in that: It comprises a navigation mark buoy as claimed in any one of claims 1 to 8, a lamp rack (200) fixedly mounted on the top of the navigation mark buoy, a counterweight (300) fixedly mounted on the bottom of the navigation mark buoy, a battery (400) fixedly mounted inside the navigation mark buoy, and a solar panel (500) and a navigation mark light (600) respectively fixedly mounted on the lamp rack (200), wherein the solar panel (500) is electrically connected to the battery (400), and the battery (400) is electrically connected to the navigation mark light (600).

10. The navigation mark according to claim 9, characterized in that: The lamp holder (200) is the continuous fiber reinforced PET composite material, and the PET layer of the lamp holder (200) is fixed to the substrate (11) by thermal fusion.

Citation Information

Cited By

  • Navigation mark floating body, navigation mark and navigation mark floating body manufacturing method

    CN117842284A