Semiconductor assembly
By introducing silicon layers and oxide/metal junction layers into semiconductor components, the heat dissipation problem in PoP components is solved, the risk of overheating is reduced, and the temperature management and functional stability of the components are improved.
Patent Information
- Application Number
- CN202323294700.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2023-01-09
- Filing Date
- 2023-12-04
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-04
AI Technical Summary
In high-density package-on-package (PoP) components, heat dissipation issues have become a bottleneck, leading to overheating risks and functional degradation, which are difficult to effectively solve with existing technologies.
By introducing silicon layers into semiconductor components and forming oxide and metal bonding layers on top of them, the high thermal conductivity of these layers is exploited to dissipate heat while maintaining component miniaturization and high-density packaging.
It effectively improves the heat dissipation capacity of semiconductor components, reduces the risk of overheating, and improves the temperature management and functional stability of the components, while maintaining a smaller appearance and high-density packaging.
Smart Images

Figure CN221861640U_ABST
Abstract
Description
Technical Field
[0001] The embodiment of the utility model relates to an integrated circuit package, and in particular to a semiconductor component including a heat dissipation structure. Background Art
[0002] The semiconductor industry is experiencing rapid growth due to ongoing improvements in the integration density of various electronic components (e.g., transistors, diodes, resistors, capacitors, etc.). The main improvement in integration density comes from the continuous reduction in the minimum feature size, which allows more components to be integrated into a given area. As the demand for shrinking electronic components grows, there has been a demand for packaging technologies for smaller and more creative semiconductor dies. An example of such a packaging system is the Package-on-Package (PoP) technology. In a PoP component, a top semiconductor package is stacked on top of a bottom semiconductor package to provide a high level of integration and component density. PoP technology can generally produce semiconductor components with enhanced functionality and a small footprint on a printed circuit board (PCB). The high level of integration and component density can lead to increased heat generation within the PoP component, which necessitates creative packaging technologies that integrate improved heat dissipation features to maintain the enhanced functionality of these PoP components while maintaining their small footprint. Utility Model Content
[0003] An embodiment of the utility model provides a semiconductor component including a first semiconductor package, a second semiconductor package directly bonded to the first semiconductor package, a silicon layer located on a side of the second semiconductor package opposite to the first semiconductor package, and a heat dissipation structure attached to the silicon layer. The first semiconductor package includes a first internal connection structure located on a first semiconductor substrate and a substrate through hole extending through the first semiconductor substrate and electrically connected to the first internal connection structure. The second semiconductor package includes a second semiconductor substrate and a second internal connection structure located on the second semiconductor substrate.
[0004] In some embodiments, the silicon layer has a thickness in the range of 1 micron to 6 microns. In some embodiments, the semiconductor component further includes a first oxide bonding layer in direct physical contact with the silicon layer and a second oxide bonding layer in direct physical contact with the first oxide bonding layer, and the second oxide bonding layer is in physical contact with the heat dissipation structure. In some embodiments, the semiconductor component further includes a metal bonding layer directly bonded to the silicon layer, and the metal bonding layer is in direct physical contact with the heat dissipation structure. In some embodiments, the second semiconductor package further includes an insulating buffer layer on the second semiconductor substrate, and the insulating buffer layer is in direct physical contact with the silicon layer. In some embodiments, the second semiconductor package further includes a plurality of dummy dies adjacent to the second semiconductor substrate. In some embodiments, the dummy dies are encapsulated by a sealing body. In some embodiments, the sealing body encapsulates the second semiconductor substrate and the second internal wiring structure. In some embodiments, the first semiconductor package is directly bonded to the second semiconductor package by a bonding layer, and the bonding layer includes a bonding pad and a dummy pad. In some embodiments, the first internal wiring structure and the first semiconductor substrate are encapsulated by a sealing body.
[0005] Based on the above, the addition of the silicon layer improves the heat dissipation capabilities of the semiconductor component. The thermal conductivity of the silicon layer can allow for improved heat dissipation from heat generated by components such as the first semiconductor die, the second semiconductor die, and other heat generating structures within the semiconductor component. Thus, the silicon layer can be formed in direct physical contact with the second semiconductor substrate. Utilizing the silicon layer can allow more high-power semiconductor dies to be incorporated into the semiconductor component while maintaining a sufficient temperature within the semiconductor component to avoid overheating within the semiconductor component. In addition, utilizing the silicon layer can improve heat dissipation while occupying a smaller form factor to allow for higher density packaging while improving or maintaining sufficient heat dissipation to reduce the risk of overheating within the semiconductor component. Reducing the risk of overheating semiconductor components is advantageous because it can reduce the risk of thermal degradation within the semiconductor component and reduce the risk of reduced functionality of the semiconductor component that may be caused by overheating.
[0006] In order to make the above features and advantages of the embodiments of the present invention more obvious and easy to understand, embodiments are specifically cited below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1 A cross-sectional view of a first carrier substrate containing alignment mark features utilized during an intermediate step in fabricating a semiconductor package in accordance with some embodiments is shown.
[0008] Figure 2 , Figure 3 , Figure 4 as well as Figure 5 A cross-sectional view illustrates an intermediate step in forming a first semiconductor component over a carrier substrate in accordance with some embodiments.
[0009] Figure 6A cross-sectional view of a second semiconductor component formed over a first semiconductor component to form a package-on-package (PoP) component is shown in accordance with some embodiments.
[0010] Figure 7 A cross-sectional view illustrating formation of a first silicon layer over a second semiconductor component and thinning of the first silicon layer according to some embodiments.
[0011] Figure 8 A cross-sectional view illustrating formation of an oxide layer over a first silicon layer in accordance with some embodiments.
[0012] Fig. 9 A cross-sectional view illustrating formation of a first heat dissipation structure according to some embodiments.
[0013] Fig.10 A cross-sectional view illustrating alignment of a first heat dissipation structure over an oxide layer in accordance with some embodiments.
[0014] Fig.11 A cross-sectional view illustrating attachment of a first thermal dissipation structure to a PoP assembly according to some embodiments.
[0015] Fig.12 A cross-sectional view showing removal of a first carrier substrate in accordance with some embodiments is shown.
[0016] Fig.13 and Fig.14 A cross-sectional view illustrating steps of forming external contacts for a PoP assembly according to some embodiments.
[0017] Fig.15 A cross-sectional view illustrating formation of a first buffer layer over a PoP assembly in accordance with some embodiments.
[0018] Fig.16 A cross-sectional view illustrating formation of a second silicon layer over a first buffer layer and thinning of the second silicon layer according to some embodiments.
[0019] Fig.17 A cross-sectional view illustrating formation of a second heat dissipation structure according to some embodiments.
[0020] Fig.18 and Fig.19 A cross-sectional view illustrating alignment and attachment of a second heat dissipation structure to a PoP assembly in accordance with some embodiments.
[0021] Fig. 20 and Fig.21 A cross-sectional view illustrating removal of a first carrier substrate and formation of external contacts for a PoP assembly in accordance with some embodiments.
[0022] Fig. 22A cross-sectional view illustrating formation of a second buffer layer over a PoP assembly in accordance with some embodiments.
[0023] Fig.23 A cross-sectional view illustrating formation of a metal bonding layer over a second buffer layer in accordance with some embodiments.
[0024] Fig.24 A cross-sectional view illustrating formation of a third heat dissipation structure according to some embodiments.
[0025] Fig.25 and Fig.26 A cross-sectional view illustrating alignment and attachment of a third thermal dissipation structure to a PoP assembly in accordance with some embodiments.
[0026] Fig. 27 and Fig.28 A cross-sectional view illustrating removal of a first carrier substrate and formation of external contacts for a PoP assembly in accordance with some embodiments.
[0027] Description of Reference Numerals
[0028] 101: first carrier substrate; 103: base substrate; 105: first dielectric layer; 107: release layer; 109: first alignment mark; 111: first bonding layer; 201: first semiconductor die; 203: first semiconductor substrate; 205: first internal connection structure; 207: second bonding layer; 209: substrate through hole; 211: first passivation film; 213: first contact pad; 215: first internal connection dielectric layer; 217: first metallization pattern; 301: first seal; 303: first planarization process; 401: isolation layer; 403: first semiconductor component; 501: third bonding layer; 503: first Second dielectric layer; 505: first bonding pad; 505A: active bonding pad; 505B: dummy bonding pad; 601: second semiconductor component; 603: dummy die; 603A: dummy die substrate; 603B: dummy die bonding layer; 605: second semiconductor die; 607: second seal; 609: fourth bonding layer; 611: third dielectric layer; 613: second contact pad; 615: second interconnect structure; 617: second interconnect dielectric layer; 619: second metallization pattern; 621: second semiconductor substrate; 701: first silicon layer; 703: second planarization process; 801: first oxide layer; 901: first carrier structure; 903: second oxide layer; 905: second carrier substrate; 1001: first alignment process; 1201: stripping process; 1301: first opening; 1401: first UBM; 1403: conductive connector; 1405: first PoP component; 1501: first insulating buffer layer; 1601: second silicon layer; 1603: third planarization process; 1701: second carrier structure; 1703: first metal layer; 1705: third carrier substrate; 1707: first groove; 1709: third alignment mark; 1801: second alignment process; 1901: metal silicide; 2101: second PoP component; 2201: second insulating buffer layer; 2301: second metal layer; 2401: third carrier structure; 2403: third metal layer; 2405: fourth carrier substrate; 2407: second groove; 2409: fourth alignment mark; 2501: third alignment process; 2801: third PoP component; T1: first thickness; T2: second thickness; T3: third thickness; T4: fourth thickness; T5: fifth thickness; T6: sixth thickness; T7: seventh thickness; T8: eighth thickness; TH1: first combined thickness; TH2: second combined thickness; TH3: third combined thickness. DETAILED DESCRIPTION
[0029] The following disclosure provides many different embodiments or examples for implementing different features of the present disclosure. Specific examples of components and arrangements are described below to simplify the present disclosure. Of course, these are only examples and are not intended to limit the scope of the present disclosure. For example, in the following description, a first feature is formed "above" or "on" a second feature, which may include an embodiment in which the first feature and the second feature are formed to be in direct contact, and may also include an embodiment in which an additional feature is formed between the first feature and the second feature so that the first feature and the second feature are not in direct contact. In addition, the present disclosure may reuse component numbers and / or letters in each example. Such repetition is for the purpose of simplifying and clearly describing the present disclosure, rather than for limiting the relationship between various embodiments and / or configurations.
[0030] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "upper," etc. may be used herein to describe the relationship of one component or feature to another (other) component or feature as shown in the figures. The spatially relative terms are intended to encompass different orientations of the device in use or operation in addition to the orientation depicted in the figures. The device may be in other orientations (rotated 90 degrees or at other orientations) and the spatially relative descriptors used therein may be interpreted in a similar manner.
[0031] According to some embodiments, a stacked die (e.g., a first die bonded to a second die) and a heat dissipation structure (e.g., a substrate) are bonded to the back side of the second die. In some embodiments, the heat dissipation structure is bonded using an oxide-to-oxide bonding configuration. In some other embodiments, the heat dissipation structure is bonded using a metal-to-metal bonding configuration. In other embodiments, the heat dissipation structure is bonded using another bonding configuration (e.g., a dielectric-to-dielectric bonding, a semiconductor-to-semiconductor bonding, or the like). These bonding configurations improve heat dissipation in the package and improve adhesion between the heat dissipation structure and the second die.
[0032] exist Figure 1 , a first carrier substrate 101 is shown. In some embodiments, the first carrier substrate 101 includes a base substrate 103, a first dielectric layer 105 over a top surface of the base substrate 103, a release layer 107 over the first dielectric layer 105, and a first alignment mark 109 embedded in the release layer 107. In addition, a first bonding layer 111 may be deposited over the top surface of the release layer 107, covering the first alignment mark 109. The first carrier substrate 101 may subsequently facilitate the formation of a plurality of semiconductor components (e.g., package-on-package (PoP) components) on the first carrier substrate 101.
[0033] According to some embodiments, the base substrate 103 may include silicon (e.g., a glass carrier substrate, a ceramic carrier substrate, or the like). In some embodiments, the first dielectric layer 105 may include silicon oxide, silicon nitride, silicon oxynitride, a polymer, or the like, and may be deposited by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD), or the like. In some embodiments, the release layer 107 may include: an epoxy-based thermal release material that loses its adhesive properties when heated, such as a light-to-heat-conversion (LTHC) release coating; an ultra-violet (UV) glue that loses its adhesive properties when exposed to UV light; or the like. Additionally, the first alignment mark 109 may include a first conductive material. The first alignment mark 109 is disposed within the first dielectric layer 105 and may facilitate subsequent structures (e.g., the first semiconductor die 201, see Figure 2 ) on the first carrier substrate 101. According to some embodiments, the first bonding layer 111 may include a silicon-containing dielectric material, such as silicon oxide, silicon nitride, silicon oxynitride, or the like, and the first bonding layer 111 may be deposited using a suitable deposition process, such as CVD, PVD, ALD, high-density plasma chemical vapor deposition (HDPCVD), oxidation of underlying materials, combinations of these processes, or the like. Optionally, a planarization step may then be performed to level the top surface of the first bonding layer 111 so that the first bonding layer 111 has a high degree of planarization. Other materials and formation methods may also be used.
[0034] exist Figure 2 , a first semiconductor die 201 is attached to a first carrier substrate 101. In some embodiments, the first semiconductor die 201 includes a first interconnect structure 205 on a first semiconductor substrate 203. The first semiconductor die 201 may be attached to the first carrier substrate 101 by a second bonding layer 207 such that the first interconnect structure 205 faces the first carrier substrate 101.
[0035] The first semiconductor die 201 may be a bare chip semiconductor die (eg, an unpackaged semiconductor die). For example, the first semiconductor die 201 may be a logic die (e.g., an application processor (AP), a central processing unit, a microcontroller, etc.), a memory die (e.g., a dynamic random access memory (DRAM) die, a hybrid memory cube (HBC), a static random access memory (SRAM) die, a wide input / output (wideIO) memory die, a magnetoresistive random access memory (mRAM) die, a resistive random access memory (rRAM) die, etc.), a power management die (e.g., a power management integrated circuit (PMIC) die), a radio frequency (RF) die, a sensor die, a micro-electro-mechanical-system (MEMS) die, a signal processing die (e.g., a digital signal processing (DSP) die), a front-end die (e.g., an analog front-end (AFE) die), a micro-electro-mechanical-system (MEMS) die, ... front-end, AFE) die), biomedical die or the like.
[0036] The first semiconductor die 201 may be processed according to an applicable manufacturing process to form an integrated circuit in the first semiconductor die 201. For example, the first semiconductor die 201 may include a first semiconductor substrate 203, such as doped or undoped silicon or an active layer of a semiconductor-on-insulator (SOI) substrate. The first semiconductor substrate 203 may include other semiconductor materials, such as germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or combinations thereof. Other substrates, such as multi-layer substrates or gradient substrates, may also be used.
[0037] Components such as transistors, diodes, capacitors, resistors, or the like may be formed in and / or on the first semiconductor substrate 203 and may be interconnected to form one or more integrated circuits via a first interconnect structure 205 including a first metallization pattern 217 (e.g., conductive lines and vias) in one or more first interconnect dielectric layers 215. The first interconnect dielectric layer 215 may include silicon oxide, silicon nitride, silicon oxynitride, a polymer, or the like, and may be deposited by PVD, CVD, ALD, or the like. For example, the first metallization pattern 217 may be a conductive feature formed in the first interconnect dielectric layer 215 by a damascene process.
[0038] The first semiconductor die 201 further includes a through substrate via (TSV) 209 that can be electrically connected to a metallization pattern in the first interconnect structure 205. The TSV 209 can include a conductive material (e.g., copper or the like) and can extend from the first interconnect structure 205 into the first semiconductor substrate 203. An insulating barrier layer (not separately shown) can be formed around at least a portion of the TSV 209 in the first semiconductor substrate 203. The insulating barrier layer can include, for example, silicon oxide, silicon nitride, silicon oxynitride, or the like, and can be used to physically and electrically isolate the TSV 209 from the first semiconductor substrate 203. In subsequent processing steps, the first semiconductor substrate 203 can be thinned to expose the TSV 209 (see FIG. 2 ). Figure 3 After thinning, the TSVs 209 provide electrical connections from the back side of the first semiconductor substrate 203 to the front side of the first semiconductor substrate 203 .
[0039] The first semiconductor die 201 further includes a first contact pad 213 that allows external connections to be made to the first interconnect structure 205 and components on the first semiconductor substrate 203. The first contact pad 213 may include copper, aluminum (e.g., 28K aluminum), or another conductive material that is electrically connected to the metallization pattern of the first interconnect structure 205. The first contact pad 213 is disposed on what may be referred to as an active side or front side of the first semiconductor die 201. The active side / front side of the first semiconductor die 201 may refer to a side on which active components are formed on the first semiconductor substrate 203. The back side of the first semiconductor die 201 may refer to a side opposite to the active side / front side of the first semiconductor substrate 203.
[0040] The first passivation film 211 is disposed on the first interconnect structure 205 and the first contact pad 213. The first passivation film 211 may include silicon oxide, silicon oxynitride, silicon nitride, or the like, which may be deposited by CVD, ALD, PVD, or the like.
[0041] The first semiconductor die 201 may be formed as part of a larger wafer (e.g., connected to other first semiconductor dies 201). In some embodiments, the first semiconductor dies 201 may be singulated from one another prior to packaging. The singulation process may include mechanical sawing, laser cutting, plasma cutting, combinations thereof, or the like. In other embodiments, the first semiconductor die 201 are singulated after being integrated into a semiconductor package. For example, the first semiconductor die 201 may be packaged while still connected as part of a wafer.
[0042] In some embodiments, the second bonding layer 207 is deposited on the first semiconductor die 201, such as on the first passivation layer 211. The second bonding layer 207 may be formed in a similar manner and from similar materials as the first bonding layer 111.
[0043] In an embodiment, the second bonding layer 207 is bonded to the first bonding layer 111 by a first dielectric-to-dielectric bonding process (e.g., oxide-to-oxide bonding). Melt bonding can be performed by first activating the first bonding layer 111 and / or the second bonding layer 207, and then applying pressure, heat, and / or other bonding process steps to bond the first bonding layer 111 to the surface of the second bonding layer 207. Activating the first bonding layer 111 and the second bonding layer 207 can be performed using, for example, dry processing, wet processing, plasma processing, exposure to H2, exposure to N2, exposure to O2, combinations of these, or the like. In an embodiment using wet processing, an RCA cleaning process, for example, can be used. Activation assists the melt bonding of the first bonding layer 111 and the second bonding layer 207 by, for example, allowing lower pressure and temperature to be used in a subsequent melt bonding process. After treatment, the number of OH groups at the surface of the first bonding layer 111 and / or the second bonding layer 207 increases. After activating the surface of the first bonding layer 111 and / or the second bonding layer 207, the first bonding layer 111 and the second bonding layer 207 may be contacted together at a relatively low temperature (e.g., room temperature) to form a weak bond. Subsequently, annealing is performed to strengthen the weak bond and form a molten bond. During annealing, H in the OH bond is discharged, thereby forming a Si-O-Si bond between the first bonding layers, thereby strengthening the bond.
[0044] exist Figure 3In the embodiment of the present invention, the first semiconductor die 201 is encapsulated in the first encapsulant 301, and a first planarization process 303 is performed on the first semiconductor die 201 and the first encapsulant 301. In some embodiments, the first encapsulant 301 may be applied by compression molding, transfer molding, or the like, and may be formed over and around the first semiconductor die 201. The first encapsulant 301 may be applied in a liquid or semi-liquid form and then cured. The first encapsulant 301 may be a molding compound. After the first encapsulant 301 is formed, a first planarization process 303 may be performed. In some embodiments, the first planarization process 303 may remove a portion of the first encapsulant 301 over the first semiconductor die 201, and may thin the first semiconductor substrate 203 to expose the TSV 209. The first planarization process 303 may be a mechanical grinding or chemical-mechanical polish (CMP) process, in which a chemical etchant and an abrasive are used to react and grind away a portion of the first encapsulant 301 and the semiconductor material of the first semiconductor substrate 203. However, any suitable planarization process may be utilized.
[0045] exist Figure 4In the embodiment of the present invention, a portion of the first semiconductor substrate 203 may be further removed to form a groove. The groove may be formed so that the back surface of the first semiconductor substrate 203 is arranged lower than the top surface of the first seal 301. The groove may then be filled with an isolation layer 401. According to some embodiments, the groove is formed in the first semiconductor substrate 203 using an etching process that selectively etches the first semiconductor substrate 203 without significantly etching the TSV 209 or the first seal 301. Therefore, the TSV 209 may extend above the groove in the first semiconductor substrate 203. In some embodiments, an isolation material may be formed in the groove to form an isolation layer 401. The isolation layer 401 is formed of a dielectric material. The dielectric material may be an oxide, such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), tetraethylorthosilicate (TEOS)-based oxides, or the like, which may be formed by a suitable deposition process, such as CVD, ALD, or the like. Other suitable dielectric materials may also be used, such as low temperature polyimide materials, polybenzoxazole (PBO), sealants, combinations thereof, or the like. The isolation layer 401 may isolate the TSV 209 from the semiconductor material of the first semiconductor substrate 203. The first sealant 301 with the isolation layer 401 and the first semiconductor die 201 form a first semiconductor device 403 over the first carrier substrate 101.
[0046] exist Figure 5 In the embodiment, the third bonding layer 501 is formed over the back surface of the first semiconductor component 403 and on the first sealing body 301, and the third bonding layer 501 may include a second dielectric layer 503 and a first bonding pad 505 embedded in the second dielectric layer 503. In some embodiments, the first bonding pad 505 may include a conductive material, such as copper or the like. Some of the first bonding pads 505 may be physically and electrically coupled to the TSV 209. In an embodiment, the second dielectric layer 503 may include a silicon-containing dielectric material, such as silicon oxide, silicon nitride, silicon oxynitride, or the like, and the third dielectric layer 611 may be deposited using a suitable deposition process, such as CVD, PVD, ALD, HDPCVD, a combination of these, or the like. Depending on the situation, a planarization step may then be performed to level the top surface of the third bonding layer 501 so that the third bonding layer 501 has a high flatness. Other materials and formation methods may also be used.
[0047] According to some embodiments, the first bonding pad 505 may be formed above the isolation layer 401 and the TSV 209. As an example, to form the first bonding pad 505, a seed layer is formed on the top surface of the isolation layer 401 and above the TSV 209. In some embodiments, the seed layer is a metal layer, which may be a single layer or a composite layer including multiple sublayers formed of different materials. In some embodiments, the seed layer includes a titanium layer and a copper layer above the titanium layer. The seed layer may be formed using, for example, PVD or the like. A photoresist is then formed and patterned on the seed layer. The photoresist may be formed by spin coating or the like and may be exposed to light for patterning. The pattern of the photoresist corresponds to the first bonding pad 505. Patterning forms an opening through the photoresist to expose the seed layer. A conductive material is formed in the opening of the photoresist and on the exposed portion of the seed layer. The conductive material may be formed by plating such as electroplating or chemical plating or the like. The conductive material may include a metal such as copper, titanium, tungsten, aluminum, or the like. Subsequently, the photoresist and the portion of the seed layer on which the conductive material is not formed are removed. The photoresist may be removed by an acceptable ashing or stripping process (such as using oxygen plasma or the like). Once the photoresist is removed, the exposed portion of the seed layer is removed, such as by using an acceptable etching process (such as by wet etching or dry etching). The remaining portion of the seed layer and the conductive material forms the first bonding pad 505. Additionally, the second dielectric layer 503 may be formed by spin coating, lamination, CVD, the like, or a combination thereof after forming the first bonding pad 505.
[0048] In some embodiments, the second dielectric layer 503 is formed before the first bonding pad 505. The second dielectric layer 503 may be formed over the isolation layer 401 by spin coating, lamination, CVD, the like, or a combination thereof. The first bonding pad 505 may be formed in the second dielectric layer 503 by forming a recess (not shown separately) in the second dielectric layer 503, such as etching, grinding, laser technology, a combination thereof, or the like. A thin barrier layer (not shown separately) may be conformally deposited in the recess, such as by CVD, ALD, PVD, thermal oxidation, a combination thereof, or the like. The barrier layer may be formed of an oxide, a nitride, a carbide, a combination thereof, or the like. A third conductive material may be deposited over the barrier layer and in the recess. The third conductive material may be formed by an electrochemical plating process, CVD, ALD, PVD, a combination thereof, or the like. Examples of the third conductive material include copper, tungsten, aluminum, silver, gold, a combination thereof, or the like. For example, excess conductive material and the barrier layer are removed from the surface of the second dielectric layer 503 by CMP. The remaining portion of the barrier layer and the third conductive material in the groove form the first bonding pad 505.
[0049] According to some embodiments, first bonding pad 505 may include both active bonding pad 505A and dummy bonding pad 505B. Dummy bonding pad 505B is electrically isolated from other conductive features (including circuits within first semiconductor die 201 and second semiconductor die 605), and active bonding pad 505A is actively used to bond other conductive features to first bonding pad 505. Dummy bonding pad 505B may be used to provide uniform pattern density within the bonding layer.
[0050] exist Figure 6 In FIG. 4 , the second semiconductor die 605 and one or more dummy dies 603 are attached to the first semiconductor element 403 via the third bonding layer 501 .
[0051] According to some embodiments, the dummy die 603 may be placed to provide structural support for the second semiconductor component 601 and reduce warping or cracking, especially when multiple integrated circuit dies are attached to the third bonding layer 501. The dummy die 603 may be formed of a material having suitable mechanical hardness or rigidity. In some embodiments, the dummy die 603 may be formed of a semiconductor material such as silicon, silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, the like, or a combination thereof. In some embodiments, the dummy die 603 may be formed of a dielectric material such as a ceramic material, quartz, another electrically inert material, the like, or a combination thereof. In some embodiments, the dummy die 603 may be a metal or a metal alloy, such as a tin-nickel alloy (e.g., "Alloy 42") or the like. In some embodiments, the dummy die 603 is formed of two or more different materials, such as multiple layers of different materials. In some embodiments, the material of the dummy die 603 is selected based on the mechanical hardness or rigidity of the material.
[0052] In some embodiments, a dummy die 603 is included for improving uniformity in the second semiconductor component 601, which may result in improved flatness. A dummy die 603 may also be included to reduce CTE mismatches among various features in the second semiconductor component 601. The dummy die 603 may also serve as a heat dissipation feature. In such embodiments, the material of the dummy die 603 may be selected to have a relatively high thermal conductivity (e.g., higher than the thermal conductivity of the subsequently deposited second seal 607). According to some embodiments, the dummy die 603 may be substantially free of any active components, functional circuits, or the like. For example, the dummy die 603 may include a dummy die substrate 603A (e.g., a bulk silicon substrate) and a dummy die bonding layer 603B. For example, the dummy die bonding layer 603B may be used to bond the dummy die 603 to the third bonding layer 501 using a fusion bonding process (such as a process for bonding the first bonding layer 111 and the second bonding layer 207).
[0053] The second semiconductor die 605 may be a bare chip semiconductor die (e.g., an unpackaged semiconductor die). For example, the second semiconductor die 605 may be a logic die (e.g., an AP, a central processing unit, a microcontroller, etc.), a memory die (e.g., a DRAM die, an HBC, an SRAM die, a wide IO memory die, an mRAM die, an rRAM die, etc.), a power management die (e.g., a PMIC die), an RF die, a sensor die, a MEMS die, a signal processing die (e.g., a DSP die), a front-end die (e.g., an AFE die), a biomedical die, or the like.
[0054] The second semiconductor die 605 may be processed according to an applicable manufacturing process to form an integrated circuit in the second semiconductor die 605. For example, the second semiconductor die 605 may include a second semiconductor substrate 621, such as doped or undoped silicon, or an active layer of a semiconductor-on-insulator (SOI) substrate. The second semiconductor substrate 621 may include other semiconductor materials, such as germanium; compound semiconductors, including silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, and / or indium antimonide; alloy semiconductors, including SiGe, GaAsP, AlInAs, AlGaAs, GaInAs, GaInP, and / or GaInAsP; or combinations thereof. Other substrates, such as multilayer substrates or gradient substrates, may also be used.
[0055] Components such as transistors, diodes, capacitors, resistors, or the like may be formed in and / or on the second semiconductor substrate 621 and may be interconnected by a second interconnect structure 615 including a second metallization pattern 619 (e.g., conductive lines and vias) in one or more second interconnect dielectric layers 617 to form one or more integrated circuits. The second interconnect dielectric layer 617 may include silicon oxide, silicon nitride, silicon oxynitride, a polymer, or the like, and may be deposited by PVD, CVD, ALD, or the like. For example, the second metallization pattern 619 may be a conductive feature formed in the second interconnect dielectric layer 617 by a damascene process.
[0056] The second semiconductor die 605 further includes a second contact pad 613 that allows external connections to be made to the second interconnect structure 615 and components on the second semiconductor substrate 621. The second contact pad 613 may include copper, aluminum (e.g., 28K aluminum), or another conductive material that is electrically connected to a second metallization pattern 619 of the second interconnect structure 615. The second contact pad 613 is disposed on what may be referred to as an active side or front side of the second semiconductor die 605. The active side / front side of the second semiconductor die 605 may refer to a side on which active components are formed on the second semiconductor substrate 621. The back side of the second semiconductor die 605 may refer to a side opposite to the active side / front side of the second semiconductor substrate 621.
[0057] The second semiconductor die 605 can be formed as part of a larger wafer (e.g., connected to other second semiconductor dies 605). In some embodiments, the second semiconductor dies 605 can be singulated from each other before packaging. The singulation process can include mechanical sawing, laser cutting, plasma cutting, combinations thereof, or the like. In other embodiments, the second semiconductor die 605 are singulated after being integrated into a semiconductor package. For example, the second semiconductor die 605 can be packaged while still connected as part of a wafer.
[0058] According to some embodiments, the second semiconductor die 605 is attached to the third bonding layer 501 by the fourth bonding layer 609. The second semiconductor die 605 may be attached to the third bonding layer 501 at the same time, before, or after the dummy die 603 is attached to the third bonding layer 501. The fourth bonding layer 609 may include a third dielectric layer 611 and a second contact pad 613. The third dielectric layer 611 may include a silicon-containing dielectric material such as silicon oxide, silicon nitride, silicon oxynitride, or the like, and the third dielectric layer 611 may be deposited using a suitable deposition process such as CVD, PVD, ALD, HDPCVD, oxidation of the underlying material, a combination of these, or the like. The second contact pad 613 may be formed in a similar manner to the first bonding pad 505. Optionally, a planarization step may then be performed to level the top surface of the fourth bonding layer 609 so that the fourth bonding layer 609 has a high degree of planarity. Other materials and formation methods may also be used.
[0059] In some embodiments, the second semiconductor die 605 is bonded to the third bonding layer 501 by dielectric-to-dielectric and metal-to-metal bonding processes performed between the third bonding layer 501 and the fourth bonding layer 609. In some embodiments, the dielectric-to-dielectric bonding process forms a direct bond (e.g., a fusion bond such as an oxide-to-oxide bond) between the second dielectric layer 503 and the third dielectric layer 611. Additionally, the metal-to-metal bonding process may directly bond the first bonding pad 505 of the third bonding layer 501 to the second contact pad 613 of the second semiconductor die 605 via direct metal-to-metal bonding. Thus, the electrical connection between the first semiconductor die 201 and the second semiconductor die 605 may be provided by the physical connection of the first bonding pad 505 to the second contact pad 613. The dielectric-to-dielectric bonding process may begin by performing a surface treatment on either or both of the second dielectric layer 503 and the third dielectric layer 611 to promote dielectric-to-dielectric bonding (e.g., such as oxide-to-oxide bonding) between the second dielectric layer 503 and the third dielectric layer 611. The surface treatment may include a plasma treatment. The plasma treatment may be performed in a vacuum environment. After the plasma treatment, the surface treatment may further include performing a cleaning process (e.g., rinsing with deionized water or the like) on either or both of the second dielectric layer 503 and the third dielectric layer 611. Next, a dielectric-to-dielectric and metal-to-metal bonding process may be continued to align the second contact pad 613 of the second semiconductor die 605 to the first bonding pad 505 of the third bonding layer 501. Next, the dielectric-to-dielectric and metal-to-metal bonding process includes a pre-bonding step during which the second semiconductor die 605 is contacted with the third bonding layer 501. The pre-bonding may be performed at room temperature (e.g., between about 21° C. and about 25° C.). The dielectric-to-dielectric and metal-to-metal bonding processes continue, for example, by performing an annealing at a temperature between about 150° C. and about 400° C. for a duration between about 0.5 hour and about 3 hours, so that the first bonding pad 505 (e.g., copper) and the second contact pad 613 (e.g., copper) diffuse into each other, thereby forming a direct metal-to-metal bond.
[0060] In addition, according to some embodiments, the one or more dummy dies 603 and the second semiconductor die 605 are encapsulated by a second encapsulant 607. The second encapsulant 607 can be deposited over the one or more dummy dies 603 and the second semiconductor die 605, and in the gap between the one or more dummy dies 603 and the second semiconductor die 605. The second encapsulant 607 can be formed in a similar manner to the first encapsulant 301, and can be a molding compound. In some embodiments, the second encapsulant 607 can be thinned in a similar manner to the first encapsulant 301, so that the one or more dummy dies 603, the second semiconductor die 605, and the second encapsulant 607 share a flat top surface of the second semiconductor component 601.
[0061] exist Figure 7 , a first silicon layer 701 is formed over a second semiconductor component 601. According to some embodiments, the first silicon layer 701 is formed by depositing silicon over the second semiconductor component 601 using CVD, HDPCVD, flowable CVD, spin coating, or the like. The first silicon layer 701 is planarized by a second planarization process 703. According to some embodiments, the second planarization process 703 may be mechanical grinding, a CMP process, or the like. The second planarization process 703 may reduce the thickness of the first silicon layer 701 to a first thickness T1 in the range of 0.05 microns to 5 microns. By forming the first silicon layer 701 to have the first thickness T1 discussed above, the first silicon layer 701 may achieve advantages such as sufficient heat dissipation in the resulting structure.
[0062] The addition of the first silicon layer 701 improves the heat dissipation capabilities of a subsequently formed PoP component. The thermal conductivity of the first silicon layer 701 may allow for improved heat dissipation from heat generated by components such as the first semiconductor die 201, the second semiconductor die 605, and other heat generating structures within a subsequently formed PoP component. Thus, in some embodiments, the first silicon layer 701 may be formed in direct physical contact with the second semiconductor substrate 621 of the second semiconductor die 605. Utilizing the first silicon layer 701 may allow for more high power semiconductor dies to be incorporated into the PoP component while maintaining sufficient temperatures within the PoP component to avoid overheating within the PoP component. Additionally, utilizing the first silicon layer 701 may improve heat dissipation while occupying a smaller form factor to allow for higher density packaging while improving or maintaining sufficient heat dissipation to reduce the risk of overheating within the PoP component. Reducing the risk of overheating the PoP component is advantageous because it may reduce the risk of thermal degradation within the PoP component and reduce the risk of reduced functionality of the PoP component that may be caused by overheating.
[0063] exist Figure 8 In the embodiment of the present invention, a first oxide layer 801 is formed over the top surface of the first silicon layer 701. The first oxide layer 801 can be formed by CVD, ALD, PVD, thermal oxidation, or the like. The first oxide layer 801 may include an oxide material such as silicon oxide or the like. In some embodiments, the first oxide layer 801 has a second thickness T2 in the range of 0.05 microns to 3 microns. Advantages can be achieved by forming the first oxide layer 801 in the range of the second thickness T2. For example, the second thickness T2 can be thin enough so as not to significantly insulate the second semiconductor component 601 while still providing sufficient bonding capability.
[0064] exist Fig. 9, a first carrier structure 901 is shown, wherein a second oxide layer 903 is formed over a second carrier substrate 905. According to some embodiments, the second carrier substrate 905 includes silicon or the like. The second oxide layer 903 may be formed over the second carrier substrate 905 by CVD, ALD, PVD, thermal oxidation, or the like. The second oxide layer 903 may include an oxide material such as silicon oxide or the like. The second oxide layer 903 may have a third thickness T3 in the range of 0.05 micrometers to 3 micrometers. According to some embodiments, the first carrier structure 901 may serve as a heat dissipation structure for the second semiconductor component 601 and the first semiconductor component 403. In addition, the first carrier structure 901 may have a higher thermal conductivity than the second seal 603. Advantages may be achieved by forming the second oxide layer 903 within the range of the third thickness T3. For example, the third thickness T3 may be thin enough so as not to significantly insulate the second semiconductor component 601 while still providing sufficient bonding capabilities.
[0065] exist Fig.10 In the embodiment, a first alignment process 1001 is performed to facilitate attachment of the first carrier structure 901 to the first oxide layer 801. In an embodiment, the bottom surface of the first carrier structure 901 is aligned above the top surface of the first oxide layer 801 before bonding the first oxide layer 801 to the second oxide layer 903. In some embodiments, a second alignment mark (not separately shown) may be used to facilitate placement of the first carrier structure 901 onto the first oxide layer 801 so that the first carrier structure 901 is aligned with the second semiconductor component 601. Fig.18 and Fig.25 An alignment process utilizing alignment marks in a manner similar to the first alignment process 1001 is described in more detail in FIG.
[0066] exist Fig.11In the embodiment, the first carrier structure 901 is attached to the second semiconductor component 601 by bonding the first oxide layer 801 to the second oxide layer 903. According to some embodiments, the first oxide layer 801 is bonded to the second oxide layer 903 by a second fusion bonding process (e.g., oxide-to-oxide bonding). The fusion bonding may be performed by first activating the first oxide layer 801 and / or the second oxide layer 903, and then applying pressure, heat, and / or other bonding process steps to bond the first oxide layer 801 to the second oxide layer 903. Activating the first oxide layer 801 and the second oxide layer 903 may be performed by an activation step, which may be, for example, a dry treatment, a wet treatment, a plasma treatment, exposure to H2, exposure to N2, exposure to O2, a combination of these, or the like. In embodiments using a wet treatment, for example, RCA cleaning may be used. In some embodiments, after the activation step, a pre-bonding step may be performed by first pressing the first oxide layer 801 to the second oxide layer 903. The pre-bonding step may be performed at room temperature (e.g., between about 21° C. and about 25° C.). In some embodiments, after the activation step, an annealing process may be performed by, for example, heating the first oxide layer 801 and the second oxide layer 903 at a temperature between about 150° C. and about 400° C. for a duration between about 0.5 hours and about 8 hours. After the second fusion bonding process, the first oxide layer 801 and the second oxide layer 903 have a first combined thickness TH1 in the range of 0.1 micrometers to 6 micrometers. Advantages may be achieved by bonding the first oxide layer 801 to the second oxide layer 903 so that the first oxide layer 801 and the second oxide layer 903 have the first combined thickness TH1 described above, such as the fusion-bonded first oxide layer 801 to the second oxide layer 903 may be thin enough so as not to significantly reduce heat dissipation in the resulting package. It has been observed that when the combined thickness of the bonded first oxide layer 801 and the second oxide layer 903 is greater than the above range, the heat dissipation of the resulting structure may be unacceptably low.
[0067] exist Fig.12 In the embodiment, a lift-off process 1201 is performed to remove the first carrier substrate 101 from the first semiconductor device 403. In an embodiment, lift-off includes projecting light such as laser or ultraviolet (UV) light onto the release layer 107 so that the release layer 107 decomposes and the first carrier substrate 101 can be removed.
[0068] exist Fig.13 In the embodiment, a first opening 1301 is formed through the first bonding layer 111, the second bonding layer 207 and the first passivation layer 211 to expose the first contact pad 213. In some embodiments, the first opening 1301 is formed by, for example, etching, grinding, laser technology, a combination thereof or the like, so that the bottom surface of the first contact pad 213 is exposed by the first bonding layer 111, the second bonding layer 207 and the first passivation layer 211.
[0069] exist Fig.14 In the embodiment, a first under-bump metallization (UBM) 1401 is formed in the first opening 1301 and along the main surface of the first bonding layer 111, and a conductive connector 1403 is formed above the first UBM 1401. In some embodiments, the first UBM 1401 has a bump portion on and extending along the main surface of the first bonding layer 111, and has a through hole portion extending through the first bonding layer 111, the second bonding layer 207, and the first passivation layer 211 to be physically and electrically coupled to the first contact pad 213. The first UBM 1401 may be formed of the same material as the first contact pad 213. In an embodiment, the conductive connector 1403 may be a ball grid array (BGA) connector, a solder ball, a metal pillar, a controlled collapse chip connection (C4) bump, a microbump, a bump formed by an electroless nickel-electroless palladium-immersion gold technique (ENEPIG) technique, or the like. The conductive connector 1403 may include a conductive material such as solder, copper, aluminum, gold, nickel, silver, palladium, tin, the like, or a combination thereof. In some embodiments, the conductive connector 1403 is formed by first forming a solder layer by evaporation, electroplating, printing, solder transfer, ball planting, or the like. Once the solder layer has been formed on the structure, reflow may be performed to shape the material into the desired bump shape. In another embodiment, the conductive connector 1403 includes a metal pillar (such as a copper pillar) formed by sputtering, printing, electroplating, chemical plating, CVD, or the like. The metal pillars may be solder-free and have substantially vertical sidewalls. In some embodiments, a metal cap layer is formed on top of the metal pillars. The metal cap layer may include nickel, tin, tin-lead, gold, silver, palladium, indium, nickel-palladium-gold, nickel-gold, the like, or a combination thereof, and may be formed by a plating process.
[0070] According to some embodiments of the present disclosure, after forming the conductive connector 1403 over the first UBM 1401, a first PoP component 1405 is formed. In an embodiment, the first PoP component 1405 includes a first carrier structure 901 supporting a second semiconductor component 601 stacked over the first semiconductor component 403, wherein the first carrier structure 901 is attached to the second semiconductor component 601 by oxide-to-oxide bonding between the first oxide layer 801 and the second oxide layer 903.
[0071] Other features and processes may also be included. For example, test structures may be included to assist in verification testing of 3D packages or 3DIC components. Test structures may include, for example, test pads formed in a redistribution layer or formed on a substrate that allow testing of the 3D package or 3DIC, use of probes and / or probe cards, and the like. Verification testing may be performed on intermediate structures as well as final structures. In addition, the structures and methods disclosed herein may be used in conjunction with test methods that incorporate intermediate verification of known good dies to improve yield and reduce costs.
[0072] Advantages can be achieved with this embodiment. For example, by forming the first silicon layer 701 to a first thickness T1, and forming the first oxide layer 801 and the second oxide layer 903 to a first combined thickness TH1, the first PoP component 1405 can achieve improved heat dissipation while maintaining a smaller form factor to achieve high-density packaging. The advantages of this embodiment can be attributed in part to the thermal conductivity of the materials used, for example, at a temperature of 300K, the thermal conductivity of the first Si / SiO2 layer and the second Si / SiO2 layer is about 8W / (m·K). The first thickness T1 and the first combined thickness TH1 allow heat to be dissipated from the first PoP component 1405 at a rate in the range of about 2W / (m·K) to about 8W / (m·K).
[0073] Figures 1 to 14 A cross-sectional view of manufacturing a first PoP assembly 1405 according to some embodiments is shown. Other configurations are also possible. For example, Figures 15 to 21 A cross-sectional view of a second PoP component 2101 formed according to some other embodiments is shown. The second PoP component 2101 can be substantially similar to the first PoP component 1405, where like reference numerals refer to like components formed by like processes. However, in the second PoP component 2101, a second carrier structure 1701 similar to the first carrier structure 901 is bonded to the second semiconductor component 601 by metal-to-silicon bonding.
[0074] exist Fig.15 In FIG. 5 , the second semiconductor component 601 is shown attached to the first semiconductor component 403 by the third bonding layer 501 , and the first semiconductor component 403 is supported by the first carrier substrate 101 . Fig.156. It is further shown that the first insulating buffer layer 1501 is formed over the top surface of the second semiconductor component 601 opposite to the first semiconductor component 403, over the dummy die 603, and over the second seal 607. The first carrier substrate 101, the first semiconductor component 403, the third bonding layer 501, and the second semiconductor component 601 can be formed in a similar manner and from materials similar to those discussed above. The first insulating buffer layer 1501 may include silicon oxide or the like, and the first insulating buffer layer 1501 is deposited by CVD, ALD, PVD, or the like. In addition, the first insulating buffer layer 1501 may be formed to have a fourth thickness T4 in the range of 0.05 microns to 3 microns. It has been observed that a thickness greater than the fourth thickness T4 may result in reduced heat dissipation potential.
[0075] exist Fig.16 In the embodiment, the second silicon layer 1601 is formed over the first insulating buffer layer 1501. According to some embodiments, the second silicon layer 1601 is formed by depositing silicon over the first insulating buffer layer 1501 using CVD, HDPCVD, flowable CVD, spin coating, or the like. Next, the second silicon layer 1601 may be planarized by a third planarization process 1603. According to some embodiments, the third planarization process 1603 may be mechanical grinding, a CMP process, or the like. The third planarization process 1603 may reduce the thickness of the second silicon layer 1601 to a fifth thickness T5 in the range of 0.05 microns to 3 microns. By forming the second silicon layer 1601 to have the fifth thickness T5 discussed above, the second silicon layer 1601 may achieve advantages such as sufficient heat dissipation of the resulting structure and help enhance bonding quality by improved surface roughness. The first insulating buffer layer 1501 may provide electrical insulation between the second silicon layer 1601 and the underlying component die.
[0076] The addition of the second silicon layer 1601 improves the heat dissipation capabilities of a subsequently formed PoP component. For example, the relatively high thermal conductivity of the second silicon layer 1601 (e.g., greater than the first insulating buffer layer 1501) can allow for improved heat dissipation from heat generated by components such as the first semiconductor die 201, the second semiconductor die 605, and other heat generating structures within a subsequently formed PoP component. Utilizing the first silicon layer 701 can allow for more high power semiconductor dies to be incorporated into the PoP component while maintaining sufficient temperatures within the PoP component to avoid overheating within the PoP component. Additionally, utilizing the first silicon layer 701 can improve heat dissipation while occupying a smaller form factor to allow for higher density packaging while improving or maintaining sufficient heat dissipation to reduce the risk of overheating within the PoP component. Reducing the risk of overheating a PoP component is advantageous because it can reduce the risk of thermal degradation within the PoP component and reduce the risk of reduced functionality of the PoP component that can be caused by overheating.
[0077] exist Fig.17, a second carrier structure 1701 is shown, wherein a first metal layer 1703 is formed over a third carrier substrate 1705. According to some embodiments, the third carrier substrate 1705 includes silicon or the like. According to some embodiments, before forming the first metal layer 1703 over the third carrier substrate 1705, a first recess 1707 may be formed in the third carrier substrate 1705. The first recess 1707 may be formed in the third carrier substrate 1705 such that when the first metal layer 1703 is formed over the third carrier substrate 1705, a height difference between a top surface of the third carrier substrate 1705 and a top surface of the first recess 1707 in the third carrier substrate 1705 forms a third alignment mark 1709. The third alignment mark 1709 may be used to facilitate aligning the second carrier structure 1701 to the second semiconductor component 601. The first recess 1707 may be formed in the third carrier substrate 1705 by etching, milling, laser technology, a combination thereof, or the like. According to some embodiments, the first metal layer 1703 may be formed over the third carrier substrate 1705 by sputtering, printing, electroplating, chemical plating, CVD or the like. In embodiments where the first grooves 1707 are formed in the third carrier substrate 1705, grooves in the first metal layer 1703 are formed corresponding to the first grooves 1707, and these grooves form third alignment marks 1709. The third alignment marks 1709 may be formed during the deposition of the first metal layer 1703 due to the height difference between the first grooves 1707 and the remaining portion of the third carrier substrate 1705. In embodiments, the first metal layer 1703 may include a metal such as nickel, copper or the like. After forming the first metal layer 1703, the first metal layer 1703 may have a sixth thickness T6 in the range of 0.05 micrometers to 3 micrometers. According to some embodiments, the second carrier structure 1701 may serve as a heat dissipation structure for the second semiconductor component 601 and the first semiconductor component 403. In addition, the second carrier structure 1701 may have a higher thermal conductivity than the second encapsulation body 603. Advantages may be realized by forming the first metal layer 1703 within the range of the sixth thickness T6. For example, the sixth thickness T6 may provide improved heat dissipation to the second semiconductor device 601 due in part to the thermal conductivity of the first metal layer 1703 while still providing sufficient bonding capabilities.
[0078] exist Fig.18 1, a second alignment process 1801 is performed to facilitate attachment of the second carrier structure 1701 to the second silicon layer 1601. In an embodiment, the bottom surface of the second carrier structure 1701 is aligned above the top surface of the second silicon layer 1601 before bonding the first metal layer 1703 to the second silicon layer 1601. In some embodiments, a third alignment mark 1709 may be used to facilitate placement of the second carrier structure 1701 onto the second silicon layer 1601 such that the second carrier structure 1701 is aligned with the second semiconductor component 601.
[0079] exist Fig.19 In the embodiment, the second carrier structure 1701 is attached to the second semiconductor element 601 by directly bonding the first metal layer 1703 to the second silicon layer 1601. Thus, Figures 15 to 21 In some embodiments, the second silicon layer 1601 may also be referred to as a bonding layer. According to some embodiments, the first metal layer 1703 is bonded to the second silicon layer 1601 by performing a first thermal annealing process. The first thermal annealing process may be performed at a temperature of room temperature (e.g., about 20° C.) to 400° C. for a duration of 0.5 hours to 12 hours, so that the first metal layer 1703 reacts with the second silicon layer 1601 to form a metal-to-silicon bond. According to some embodiments, the metal-to-silicon bond forms a metal silicide 1901 at an interface between the first metal layer 1703 and the second silicon layer 1601. After bonding the first metal layer 1703 to the second silicon layer 1601, the first metal layer 1703 and the second silicon layer 1601 have a second combined thickness TH2 in the range of 1 micron to 6 microns. By bonding the first metal layer 1703 to the second silicon layer 1601 such that the first metal layer 1703 and the second silicon layer 1601 have a second combined thickness TH2, the first metal layer 1703 and the second silicon layer 1601 may provide improved heat dissipation and sufficient bonding strength between the second semiconductor component 601 and the second carrier structure 1701. A thickness below the second combined thickness TH2 may not provide sufficient bonding between the second semiconductor component 601 and the second carrier structure 1701, and a thickness above the second combined thickness TH2 may unnecessarily increase the size of the PoP component.
[0080] According to some embodiments, after the second carrier structure 1701 is bonded to the second semiconductor component 601, a first gap may exist between the second silicon layer 1601 and the first metal layer 1703. The first gap is formed due to a height difference between the first groove 1707 and the remaining portion of the third carrier substrate 1705 during deposition of the first metal layer 1703 when forming the third alignment mark 1709 of the second carrier structure 1701 and the second carrier structure 1701, and when bonded to the flat surface of the second silicon layer 1601, the first gap is formed between the second silicon layer 1601 and the second carrier structure 1701 at a position corresponding to the third alignment mark 1709.
[0081] exist Fig. 20 In the embodiment, a lift-off process 1201 is performed to remove the first carrier substrate 101 from the first semiconductor device 403. In one embodiment, lift-off includes projecting light such as laser or ultraviolet (UV) light onto the release layer 107, causing the release layer 107 to decompose and remove the first carrier substrate 101.
[0082] exist Fig.21, a second PoP assembly 2101 is shown after the formation of the first UBM 1401 and the conductive connector 1403. The first UBM 1401 can be similarly formed and composed of the same as described above with respect to Fig.14 The conductive connector 1403 may be formed in a similar manner and from the same materials as discussed above. Fig.14 In an embodiment, the second PoP component 2101 includes a second carrier structure 1701 supporting a second semiconductor component 601 stacked above the first semiconductor component 403 , wherein the second carrier structure 1701 is attached to the second semiconductor component 601 by bonding the first metal layer 1703 to the second silicon layer 1601 .
[0083] This embodiment can achieve advantages. For example, by forming the second silicon layer 1601 and the first metal layer 1703 to the second combined thickness TH2, the second PoP component 2101 can achieve improved heat dissipation while maintaining a smaller form factor to achieve high-density packaging. The advantages of this embodiment can be attributed in part to the relatively high thermal conductivity of the materials used. For example, at a temperature of 300K, the thermal conductivity of nickel is about 91 W / (m·K). The second combined thickness TH2 allows heat to be dissipated from the second PoP component 2101 at a rate greater than 91 W / (m·K).
[0084] in addition, Figure 22 to Figure 28 A cross-sectional view of a third PoP component 2801 formed according to some other embodiments is shown. The third PoP component 2801 can be substantially similar to the first PoP component 1405, where like reference numerals refer to like components formed by like processes. In the third PoP component 2801, a third carrier structure 2401 similar to the first carrier structure 901 is bonded to the second semiconductor component 601 by metal-to-metal bonding.
[0085] exist Fig. 22 , the second semiconductor component 601 is illustrated as being attached to the first semiconductor component 403 via the third bonding layer 501 and the second insulating buffer layer 2201 formed over the top surface of the second semiconductor component 601 opposite the first semiconductor component 403, and the first semiconductor component 403 is supported by the first carrier substrate 101. The first carrier substrate 101, the first semiconductor component 403, the third bonding layer 501, and the second semiconductor component 601 can be formed in a similar manner and from similar materials as discussed above.
[0086] According to some embodiments, the second insulating buffer layer 2201 may be formed by CVD, ALD, PVD, thermal oxidation, or the like over the top surface of the second semiconductor element 601. The second insulating buffer layer 2201 may include an oxide material such as silicon oxide or the like.
[0087] exist Fig.23 In the embodiment, the second metal layer 2301 is formed above the top surface of the second insulating buffer layer 2201. In an embodiment, the second metal layer 2301 may be formed by forming a seed layer above the second insulating buffer layer 2201, and the seed layer may be a metal layer, which may be a single layer or a composite layer including multiple sublayers formed of different materials. In some embodiments, the seed layer includes a titanium layer and a copper layer above the titanium layer. The seed layer may be formed using, for example, PVD or the like. The second metal layer 2301 may then be formed by plating a metal onto the seed layer, and the plating may be electroplating or electroless plating or the like. The metal may be copper or the like. After plating the metal onto the seed layer, the second metal layer 2301 may have a seventh thickness T7 in the range of 0.05 microns to 10 microns. Advantages may be achieved by forming the second metal layer 2301 within the range of the seventh thickness T7. For example, the seventh thickness T7 may be partially due to the thermal conductivity of the second metal layer 2301 providing improved heat dissipation to the second semiconductor element 601 while still providing sufficient bonding capability.
[0088] exist Fig.24, a third carrier structure 2401 is shown, wherein a third metal layer 2403 is formed over a fourth carrier substrate 2405. According to some embodiments, the fourth carrier substrate 2405 includes silicon or the like. According to some embodiments, before forming the third metal layer 2403 over the fourth carrier substrate 2405, a second recess 2407 may be formed in the fourth carrier substrate 2405. The second recess 2407 may be formed in the fourth carrier substrate 2405 such that when the third metal layer 2403 is formed over the fourth carrier substrate 2405, a height difference between a top surface of the fourth carrier substrate 2405 and a top surface of the second recess 2407 in the fourth carrier substrate 2405 forms a fourth alignment mark 2409. The fourth alignment mark 2409 may be used to facilitate aligning the third carrier structure 2401 to the second semiconductor component 601. The second recess 2407 may be formed in the fourth carrier substrate 2405 by etching, milling, laser technology, a combination thereof, or the like. According to some embodiments, the third metal layer 2403 may be formed over the fourth carrier substrate 2405 by sputtering, printing, electroplating, chemical plating, CVD or the like. In embodiments where the second grooves 2407 are formed in the fourth carrier substrate 2405, the grooves in the third metal layer 2403 are formed corresponding to the second grooves 2407, and these grooves form the fourth alignment mark 2409. In embodiments, the third metal layer 2403 may include a metal such as copper or the like. After forming the third metal layer 2403, the third metal layer 2403 may have an eighth thickness T8 in the range of 0.05 micrometers to 10 micrometers. According to some embodiments, the third carrier structure 2401 may serve as a heat dissipation structure for the second semiconductor component 601 and the first semiconductor component 403. In addition, the third carrier structure 2401 may have a higher thermal conductivity than the second seal 603. Advantages may be achieved by forming the third metal layer 2403 within the range of the eighth thickness T8. For example, the eighth thickness T8 may be partially due to the thermal conductivity of the third metal layer 2403 providing improved heat dissipation to the second semiconductor element 601 while still providing sufficient bonding capability.
[0089] exist Fig.25 , a third alignment process 2501 is performed to facilitate attachment of the third carrier structure 2401 to the second metal layer 2301. In an embodiment, the bottom surface of the third carrier structure 2401 is aligned above the top surface of the second metal layer 2301 before bonding the third metal layer 2403 to the second metal layer 2301. In some embodiments, a fourth alignment mark 2409 may be used to facilitate placement of the third carrier structure 2401 onto the second metal layer 2301 such that the third carrier structure 2401 is aligned with the second semiconductor component 601.
[0090] exist Fig.26, the third carrier structure 2401 is attached to the second semiconductor component 601 by bonding the third metal layer 2403 to the second metal layer 2301. According to some embodiments, the third metal layer 2403 is bonded to the second metal layer 2301 by performing a second thermal annealing process. The second thermal annealing process may be performed at a temperature of room temperature (e.g., about 20° C.) to 400° C. for a duration of 0.5 hours to 12 hours, so that the third metal layer 2403 reacts with the second metal layer 2301 to form a metal-to-metal bond between the third metal layer 2403 and the second metal layer 2301. After forming the metal-to-metal bond between the second metal layer 2301 and the third metal layer 2403, the second metal layer 2301 and the third metal layer 2403 may have a third combined thickness TH3 in the range of 0.05 micrometers to 20 micrometers. The second metal layer 2301 and the third metal layer 2403 having the third combined thickness TH3 may provide improved heat dissipation and sufficient bonding strength between the second semiconductor component 601 and the third carrier structure 2401. A thickness below the third combined thickness TH3 may not provide sufficient bonding between the second semiconductor component 601 and the third carrier structure 2401, and a thickness above the third combined thickness TH3 may unnecessarily increase the size of the PoP component.
[0091] According to some embodiments, after the third carrier structure 2401 is bonded to the second semiconductor component 601, a second gap may exist between the second metal layer 2301 and the third metal layer 2403. The second gap is formed during the deposition of the third metal layer 2403 when forming the fourth alignment mark 2409 of the third carrier structure 2401 and the third carrier structure 2401 due to the height difference between the second groove 2407 and the remaining portion of the fourth carrier substrate 2405, and when bonded to the flat surface of the second metal layer 2301, the second gap is formed between the second metal layer 2301 and the third carrier structure 2401 at a position corresponding to the fourth alignment mark 2409.
[0092] exist Fig. 27 In the embodiment, a lift-off process 1201 is performed to remove the first carrier substrate 101 from the first semiconductor device 403. In one embodiment, lift-off includes projecting light such as laser or ultraviolet (UV) light onto the release layer 107 so that the release layer 107 decomposes and the first carrier substrate 101 can be removed.
[0093] exist Fig.28 , a third PoP assembly 2801 is shown after the formation of the first UBM 1401 and the conductive connector 1403. The first UBM 1401 can be formed in a similar manner and by the same method as described above with respect to Fig.14 The conductive connector 1403 may be formed in a similar manner and from the same materials as discussed above. Fig.14In an embodiment, the third PoP component 2801 includes a third carrier structure 2401 supporting a second semiconductor component 601 stacked above the first semiconductor component 403 , wherein the third carrier structure 2401 is attached to the second semiconductor component 601 by bonding the third metal layer 2403 to the second metal layer 2301 .
[0094] This embodiment can achieve advantages. For example, by forming the second metal layer 2301 and the third metal layer 2403 to a third combined thickness TH3, the third PoP component 2801 can achieve improved heat dissipation while maintaining a smaller profile to achieve high-density packaging. The advantages of this embodiment can be partially attributed to the thermal conductivity of the materials used, for example, the thermal conductivity of copper is about 400W / (m·K) at a temperature of 300K. The third combined thickness TH3 allows heat to be dissipated from the third PoP component 2801 at a rate greater than 400W / (m·K).
[0095] Embodiments can achieve advantages. Embodiments of the present disclosure utilize various materials at various thicknesses and bonding processes to adhere the second semiconductor component 601 to various carrier structures to improve the heat dissipation capabilities of the formed PoP component. By selecting the materials and thicknesses and bonding methods, the various carrier structures can provide sufficient heat dissipation depending on the thermal requirements of the formed PoP component, thereby improving the performance and reliability of the formed PoP component.
[0096] According to some embodiments of the present disclosure, a semiconductor component includes: a first semiconductor package, including: a first interconnect structure, located on a first semiconductor substrate; a substrate through-hole, extending through the first semiconductor substrate and electrically connected to the first interconnect structure; and a second semiconductor package, directly bonded to the first semiconductor package, the second semiconductor package including a second semiconductor substrate and a second interconnect structure on the second semiconductor substrate; a silicon layer, located on a side of the second semiconductor package opposite to the first semiconductor package; and a heat dissipation structure, attached to the silicon layer. In an embodiment, the silicon layer has a thickness in a range of 1 micron to 6 microns. In an embodiment, it further includes a first oxide bonding layer in direct physical contact with the silicon layer; and a second oxide bonding layer in direct physical contact with the first oxide bonding layer, the second oxide bonding layer in physical contact with the heat dissipation structure. In an embodiment, it further includes a metal bonding layer directly bonded to the silicon layer, the metal bonding layer in direct physical contact with the heat dissipation structure. In an embodiment, the second semiconductor package further includes an insulating buffer layer on the second semiconductor substrate, the insulating buffer layer in direct physical contact with the silicon layer. In an embodiment, the second semiconductor package further includes a plurality of dummy dies, the dummy dies being adjacent to the second semiconductor die. In an embodiment, a first semiconductor package is directly bonded to a second semiconductor package by a bonding layer including bonding pads and dummy pads that electrically couple the first semiconductor die to the second semiconductor die.
[0097] According to some embodiments of the present disclosure, a method for manufacturing a semiconductor device includes: forming a first bonding layer over a first semiconductor die, the first semiconductor die including a first interconnect structure on a first semiconductor substrate; bonding a second semiconductor die to the first bonding layer, the second semiconductor die including a second interconnect structure on a second semiconductor substrate; encapsulating the second semiconductor die in a seal; depositing an insulating buffer layer over the second semiconductor die and the seal; forming a second bonding layer over the top surface of the second semiconductor die and the seal, wherein the second bonding layer has a higher thermal conductivity than the insulating buffer layer; and directly bonding a third bonding layer of a heat dissipation structure to the second bonding layer, wherein the heat dissipation structure includes a third bonding layer on a silicon substrate. In an embodiment, forming the second bonding layer includes depositing a silicon layer over the insulating buffer layer and bonding the third bonding layer to the silicon layer. In an embodiment, bonding the third bonding layer of the heat dissipation structure to the silicon layer includes forming a metal-to-silicon bond between the silicon layer and the third bonding layer. In an embodiment, after forming the metal-to-silicon bond between the silicon layer and the third bonding layer, the silicon layer and the third bonding layer have a combined thickness between 1 micrometer and 6 micrometers. In an embodiment, the silicon layer has a thickness in a range of 1 micron to 6 microns. In an embodiment, the second bonding layer comprises a first metal layer, and the third bonding layer comprises a second metal layer, and wherein the third bonding layer is bonded to the second bonding layer to form a metal-to-metal bond. In an embodiment, the first bonding layer comprises an active bonding pad and a dummy bonding pad, wherein the active bonding pad is used to bond the second semiconductor die to the first bonding layer, and the active bonding pad electrically couples the first semiconductor die to the second semiconductor die.
[0098] According to some embodiments of the present disclosure, a method of manufacturing a semiconductor device includes: bonding a first semiconductor die to a first carrier substrate, the first semiconductor die including: a first interconnect structure; a first semiconductor substrate located above the first interconnect structure; and a substrate through-hole extending from the first interconnect structure through the first semiconductor substrate; bonding a second semiconductor die to the first semiconductor die, the second semiconductor die including: a second interconnect structure; and a second semiconductor substrate located above the second interconnect structure; encapsulating the second semiconductor die in a molding compound; depositing a silicon layer over the molding compound and the second semiconductor die; bonding the second carrier substrate to the silicon layer; and performing a stripping process to release the first carrier substrate from the first semiconductor die. In an embodiment, further includes: exposing a conductive contact pad of the first interconnect structure after the stripping process; and forming an under bump metal in contact with the conductive contact pad. In an embodiment, bonding the second carrier substrate to the silicon layer includes: depositing a first oxide layer on the silicon layer; depositing a second oxide layer on the second carrier substrate; and bonding the first oxide layer directly to the second oxide layer. In an embodiment, bonding the second carrier substrate to the silicon layer further comprises activating a first surface of the first oxide layer or activating a second surface of the second oxide layer before directly bonding the first oxide layer to the second oxide layer. In an embodiment, bonding the second semiconductor die to the first semiconductor die further comprises bonding a contact pad of the second interconnect structure to a metal bonding pad, the metal bonding pad being in direct physical contact with the substrate through-hole and electrically coupling the first semiconductor die to the second semiconductor die. In an embodiment, bonding the second carrier substrate comprises directly bonding a metal layer to the silicon layer, wherein the metal layer contacts the second carrier substrate.
[0099] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the embodiments of the utility model, rather than to limit them. Although the embodiments of the utility model are described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the embodiments of the embodiments of the utility model.
Claims
1. A semiconductor component, It is characterized in that include: A first semiconductor package comprising: A first interconnect structure is located on the first semiconductor substrate; and a through-substrate via extending through the first semiconductor substrate and electrically connected to the first interconnect structure; and A second semiconductor package directly bonded to the first semiconductor package, the second semiconductor package comprising a second semiconductor substrate and a second interconnect structure located on the second semiconductor substrate; a silicon layer on a side of the second semiconductor package opposite to the first semiconductor package; and A heat dissipation structure is attached to the silicon layer.
2. The semiconductor component according to claim 1, It is characterized in that The silicon layer has a thickness in the range of 1 micrometer to 6 micrometers.
3. The semiconductor component according to claim 1, It is characterized in that Also includes: a first oxide bonding layer in direct physical contact with the silicon layer; and The second oxide bonding layer is in direct physical contact with the first oxide bonding layer, and the second oxide bonding layer is in physical contact with the heat dissipation structure.
4. The semiconductor component according to claim 1, It is characterized in that Also includes: The metal bonding layer is directly bonded to the silicon layer, and the metal bonding layer is in direct physical contact with the heat dissipation structure.
5. The semiconductor component according to claim 1, It is characterized in that The second semiconductor package further comprises: An insulating buffer layer is on the second semiconductor substrate, and the insulating buffer layer is in direct physical contact with the silicon layer.
6. The semiconductor component according to claim 1, It is characterized in that The second semiconductor package further comprises: A plurality of dummy dies are provided, the dummy dies being adjacent to the second semiconductor substrate.
7. The semiconductor component according to claim 6, It is characterized in that The second semiconductor package further comprises: A sealing body, wherein the dummy die is encapsulated by the sealing body.
8. The semiconductor component according to claim 7, It is characterized in that The sealing body encapsulates the second semiconductor substrate and the second interconnect structure.
9. The semiconductor component according to claim 1, It is characterized in that The first semiconductor package is directly bonded to the second semiconductor package via a bonding layer, and the bonding layer includes a bonding pad and a dummy pad.
10. The semiconductor component according to claim 1, It is characterized in that The first semiconductor package further comprises: A sealing body, wherein the first interconnect structure and the first semiconductor substrate are encapsulated by the sealing body.
Citation Information
Cited By
Chip packaging structure capable of improving heat dissipation capability and improving warpage and preparation method
CN120300003A