Punching die for photovoltaic imbricate welding strip

By designing a photovoltaic welding strip punching mold with guide columns, punching slots and a feeding system, the problem of inconvenient waste removal is solved, rapid cleaning and recycling of waste is achieved, and processing efficiency is improved.

CN221869938UActive Publication Date: 2024-10-22JIZHI (JIANGSU) NEW ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420259407.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-02
Publication Date
2024-10-22
Estimated Expiration
2034-02-02

AI Technical Summary

Technical Problem

The waste generated during the drilling process of the existing photovoltaic welding ribbon drilling mold is inconvenient to clean, affecting the processing efficiency.

Method used

A punching mold including an upper mold and a lower mold is designed. The lower mold is provided with guide pillars and punching slots. After punching, the waste chips enter the conveying trough by gravity and fall on the conveying belt. The driving rod drives the conveyor. The material roller rotates and the conveyor belt is driven to discharge waste chips. It is combined with a power-assisted rack and linkage gear system to automatically disperse and clean waste chips.

Benefits of technology

It achieves fast and convenient cleaning and recycling of waste chips, improves processing efficiency, and reduces manual operations and costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221869938U_ABST
    Figure CN221869938U_ABST
Patent Text Reader

Abstract

The utility model relates to a punching die of a photovoltaic imbricate welding strip, which belongs to the technical field of photovoltaic welding strip production, and adopts the technical scheme that the punching die comprises an upper die and a lower die, a group of guide columns are symmetrically and fixedly arranged on the lower die, the upper die is arranged on the guide columns in a sliding manner, a plurality of punching heads are arranged on the bottom wall of the upper die, and the punching heads are arranged on the bottom wall of the upper die. A punching groove allowing the punching head to be inserted is formed in the surface of the lower die; a conveying groove is formed in the end wall of the lower die in a penetrating mode, the conveying groove communicates with the multiple punching grooves, a set of conveying rollers are symmetrically arranged in the conveying groove and located at the two ends, the conveying rollers are rotationally connected with the inner wall of the conveying groove, and the conveying rollers are jointly sleeved with a conveying belt in a tensioning mode; one conveying roller penetrates through the lower die and is connected with a driving rod; a cam is rotationally arranged in the material conveying groove and can abut against the material conveying belt. The punching device has the beneficial effects that waste chips generated during punching can be conveniently cleaned and recycled, and the machining efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of photovoltaic welding tape production and relates to a punching die for photovoltaic shingled welding tape. Background Art

[0002] Photovoltaic welding ribbon, also known as tinned copper ribbon or tin-coated copper ribbon, is divided into busbars and interconnection strips. It is used to connect the solar cells of photovoltaic modules and plays an important role in conductivity and electricity collection. In the production process of photovoltaic welding ribbon, it is necessary to punch holes on the photovoltaic welding ribbon.

[0003] The punching molds designed in the related art mostly include an upper mold and a lower mold, on which matching punching knives are installed respectively, and the upper mold and the lower mold are closed to achieve the punching of the welding strip. However, in the actual punching process, the waste chips generated after the punching will remain on the mold, which is inconvenient to clean and affects the processing efficiency, so it needs to be improved. Utility Model Content

[0004] The purpose of the utility model is to solve the above problems in the existing technology and to propose a punching die for photovoltaic shingled welding strips.

[0005] The purpose of the utility model can be achieved through the following technical solutions: a punching mold for a photovoltaic shingled welding strip, comprising an upper mold and a lower mold, a group of guide columns are symmetrically fixedly arranged on the lower mold, the upper mold is slidably arranged on the guide columns, a plurality of punching heads are arranged on the bottom wall of the upper mold, and a punching groove for inserting the punching head is opened on the surface of the lower mold; a feed trough is penetrated on the end wall of the lower mold, the feed trough is connected with the plurality of punching grooves, a group of feed rollers are symmetrically arranged in the feed trough and at both ends, the feed rollers are rotatably connected to the inner wall of the feed trough, a feed belt is commonly tensioned on the feed rollers, one of the feed rollers penetrates the lower mold and is connected to a driving rod; a cam is rotatably arranged in the feed trough, and the cam can be against the feed belt.

[0006] In the above-mentioned punching mold for a photovoltaic shingled welding strip, a power-assisting groove is passed through the lower mold, a power-assisting rack is slidably arranged in the power-assisting groove, a linkage groove is opened on the inner side wall of the power-assisting groove, a linkage gear is rotatably arranged in the linkage groove, and the linkage gear and the power-assisting rack are meshed with each other; a linkage rod is fixedly connected to the end wall of the linkage gear, the linkage rod and the linkage gear are coaxially arranged, and the end of the linkage rod away from the linkage gear is fixedly connected to the cam.

[0007] In the above-mentioned punching mold for a photovoltaic shingled welding strip, a reset groove is provided on the side wall of the assisting groove, a reset block is fixedly provided on the side wall of the assisting rack, the reset block is slidably provided in the reset groove, and a reset spring is provided in the reset groove to resist the reset block.

[0008] In the above-mentioned punching die for photovoltaic shingled welding strip, a scraper is provided on the lower die, and one end of the scraper is against the surface of the conveyor belt.

[0009] In the above-mentioned punching die for photovoltaic shingled welding strip, the punching head is threadedly connected to the upper die.

[0010] Compared with the prior art, the utility model provides an upper mold, a punching head, a lower mold, a guide column, a punching groove, a feed trough, a feed roller, a feed belt, a driving rod and a cam. The waste chips generated when the punching head punches holes on the surface of the photovoltaic shingled welding strip will enter the feed trough through the punching groove under the action of gravity and fall on the surface of the feed belt. When the waste chips need to be cleaned, the driving rod is rotated to drive one of the feed rollers to rotate, and then the feed belt is driven to transmit in the feed trough, which can drive the waste chips to be discharged from the feed trough. The operation is convenient and quick, and the waste chips generated by punching can be cleaned and recycled conveniently, thereby improving the processing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a partial cross-sectional view of a punching die for a photovoltaic shingled welding ribbon provided in an embodiment of the present application;

[0012] Figure 2 It is an overall cross-sectional view of the lower mold used to reflect the embodiment of the present application;

[0013] Figure 3 It is a partial cross-sectional view of the lower mold in the embodiment of the present application.

[0014] In the figure, 1. upper die; 11. punching head; 2. lower die; 21. guide column; 22. punching slot; 3. feed trough; 31. feed roller; 32. feed belt; 33. drive rod; 4. cam; 5. power-assisting slot; 51. power-assisting rack; 52. linkage slot; 521. linkage gear; 53. linkage rod; 6. reset slot; 61. reset block; 62. reset spring; 7. scraper. DETAILED DESCRIPTION

[0015] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.

[0016] Example

[0017] The present application embodiment provides a punching die for a photovoltaic shingled welding strip, referring to Figure 1, including an upper die 1 and a lower die 2, a group of guide pillars 21 are symmetrically fixedly arranged on the lower die 2, the guide pillars 21 are arranged in the vertical direction, and the upper die 1 is slidably arranged on the guide pillars 21. A plurality of punching heads 11 are equidistantly arranged on the bottom wall of the upper die 1, and the punching heads 11 are threadedly connected to the upper die 1. The punching heads 11 can be disassembled from the upper die 1 by rotating the punching heads 11 to replace punching heads 11 of different models.

[0018] Reference Figure 1 and Figure 2 , a punching groove 22 for the punching head 11 to be inserted is provided on the surface of the lower mold 2, and the length direction of the punching groove 22 is arranged along the thickness direction of the lower mold 2, and the caliber of the punching groove 22 and the punching head 11 are adapted to each other. A feed trough 3 is provided through the end wall of the lower mold 2, and the length direction of the feed trough 3 is arranged along the length direction of the lower mold 2, and the feed trough 3 is connected with a plurality of punching grooves 22. The photovoltaic shingled welding strip is pulled through between the upper mold 1 and the lower mold 2, and the photovoltaic shingled welding strip is fitted with the surface of the upper mold 1, and then the upper mold 1 is driven to slide on the guide column 21 under the action of the hydraulic system, so that the upper mold 1 is close to the lower mold 2, and the punching head 11 enters the punching groove 22 at the moment, and the punching head 11 punches holes on the surface of the photovoltaic shingled welding strip, and the waste generated by the punching will enter the feed trough 3 through the punching groove 22 under the action of gravity.

[0019] Reference Figure 1 and Figure 2 A set of feed rollers 31 are symmetrically arranged at both ends in the feed trough 3. The length direction of the feed rollers 31 is arranged along the width direction of the lower die 2. The feed rollers 31 are rotatably connected to the inner wall of the feed trough 3. A feed belt 32 is provided on the feed rollers 31 through a common tensioning sleeve. One of the feed rollers 31 passes through the lower die 2 and is connected to a driving rod 33. The waste generated by punching will enter the feed trough 3 through the punching groove 22 under the action of gravity and fall on the surface of the feed belt 32. When the waste needs to be cleaned, the driving rod 33 is rotated to drive one of the feed rollers 31 to rotate, thereby driving the feed belt 32 to transmit in the feed trough 3, and the waste can be discharged from the feed trough 3.

[0020] Reference Figure 1 A scraper 7 is provided on the lower mold 2. The scraper 7 is inclined, and one end of the scraper 7 is against the surface of the conveyor belt 32. When the conveyor belt 32 is driven to rotate, the scraper 7 is against the surface of the conveyor belt 32, which is beneficial to improve the cleaning effect of the waste chips on the surface of the conveyor belt 32.

[0021] Reference Figure 2 and Figure 3, a plurality of power-assisting grooves 5 are passed through the lower die 2. In this embodiment, two power-assisting grooves 5 are symmetrically arranged. The length direction of the power-assisting groove 5 is arranged along the thickness direction of the lower die 2. A power-assisting rack 51 is slidably arranged in the power-assisting groove 5, and the power-assisting rack 51 and the power-assisting groove 5 are adapted to each other. A linkage groove 52 is provided on the inner side wall of the power-assisting groove 5. A linkage gear 521 is rotatably arranged in the linkage groove 52, and the linkage gear 521 and the power-assisting rack 51 are meshed with each other. A linkage rod 53 is fixedly connected to the end wall of the linkage gear 521. The linkage rod 53 and the linkage gear 521 are coaxially arranged. One end of the linkage rod 53 away from the linkage gear 521 extends into the feed trough 3 and is connected to the cam 4. The cam 4 is located below the feed belt 32. By driving the power-assisting rack 51 to slide in the power-assisting groove 5 along the length direction of the power-assisting groove 5, the power-assisting rack 51 is abutted against the linkage gear 521, thereby driving the linkage gear 521 to rotate. The linkage gear 521 then drives the cam 4 to rotate through the linkage rod 53. The cam 4 can abut against the feed belt 32, driving the feed belt 32 to vibrate, so that waste chips are dispersed on the feed belt 32, reducing the accumulation of waste chips on the surface of the feed belt 32, effectively utilizing the space in the feed trough 3, and reducing the phenomenon of waste chips clogging the punching groove 22.

[0022] Reference Figure 2 and Figure 3 A reset groove 6 is provided on the side wall of the assisting groove 5, and the length direction of the reset groove 6 is arranged along the length direction of the assisting groove 5. A reset block 61 is fixedly provided on the side wall of the assisting rack 51, and the reset block 61 is slidably provided in the reset groove 6. A reset spring 62 is provided in the reset groove 6 to resist the reset block 61. The reset block 61 drives the power-assisting rack 51 to slide away from the bottom wall of the power-assisting groove 5, so that the top end of the power-assisting rack 51 is exposed from the power-assisting groove 5. When the hydraulic system drives the upper mold 1 and the lower mold 2 to approach each other, the upper mold 1 will abut against the top end of the power-assisting rack 51, driving the power-assisting rack 51 to slide toward the bottom wall of the power-assisting groove 5, automatically driving the power-assisting rack 51 to slide so that the linkage gear 521 drives the cam 4 to rotate. When the upper mold 1 and the lower mold 2 move away from each other, under the action of the reset spring 62, the top end of the power-assisting rack 51 is automatically reset out of the power-assisting groove 5, thereby eliminating the need for manual operation of the power-assisting rack 51 to slide to disperse the waste chips on the surface of the conveyor belt 32, thereby improving operational convenience and saving costs.

[0023] The implementation principle of a punching mold for a photovoltaic shingled welding strip in an embodiment of the present application is as follows: the photovoltaic shingled welding strip is pulled through between an upper mold 1 and a lower mold 2, and at the same time, the photovoltaic shingled welding strip is fitted with the surface of the upper mold 1, and then the upper mold 1 is driven to slide on a guide column 21 under the action of a hydraulic system, so that the upper mold 1 is close to the lower mold 2, and at the moment when the punching head 11 enters the punching groove 22, the punching head 11 punches holes on the surface of the photovoltaic shingled welding strip, and the waste chips generated by the punching will enter the feed trough 3 through the punching groove 22 under the action of gravity and fall on the surface of the feed belt 32. When the waste chips need to be cleaned, the driving rod 33 is rotated to drive one of the feed rollers 31 to rotate, and then the feed belt 32 is driven to transmit in the feed trough 3, which can drive the waste chips to be discharged from the feed trough 3. The operation is convenient and quick, and the waste chips generated by the punching can be cleaned and recycled conveniently, thereby improving the processing efficiency.

[0024] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways, but they will not deviate from the spirit of the present invention or exceed the scope defined by the appended claims.

Claims

1. A punching die for photovoltaic shingled welding strips, comprising an upper die (1) and a lower die (2), wherein a group of guide pillars (21) are symmetrically fixedly arranged on the lower die (2), and the upper die (1) is slidably arranged on the guide pillars (21), characterized in that: A plurality of punching heads (11) are arranged on the bottom wall of the upper die (1), and a punching groove (22) for inserting the punching head (11) is opened on the surface of the lower die (2); a feed trough (3) is arranged through the end wall of the lower die (2), the feed trough (3) and the plurality of punching grooves (22) are connected to each other, a group of feed rollers (31) are symmetrically arranged in the feed trough (3) and located at both ends, the feed rollers (31) are rotatably connected to the inner wall of the feed trough (3), a feed belt (32) is commonly tensioned on the feed rollers (31), one of the feed rollers (31) passes through the lower die (2) and is connected to a driving rod (33); a cam (4) is rotatably arranged in the feed trough (3), and the cam (4) can abut against the feed belt (32).

2. The punching die for photovoltaic shingled ribbon according to claim 1, characterized in that: The lower mold (2) is provided with a power-assisting groove (5), in which a power-assisting rack (51) is slidably arranged, and an interlocking groove (52) is provided on the inner side wall of the power-assisting groove (5), in which a interlocking gear (521) is rotatably arranged, and the interlocking gear (521) and the power-assisting rack (51) are meshed with each other; a interlocking rod (53) is fixedly connected to the end wall of the interlocking gear (521), and the interlocking rod (53) and the interlocking gear (521) are coaxially arranged, and the end of the interlocking rod (53) away from the interlocking gear (521) is fixedly connected to the cam (4).

3. The punching die for photovoltaic shingled welding strip according to claim 2, characterized in that: A reset groove (6) is provided on the side wall of the power-assisting groove (5), a reset block (61) is fixedly provided on the side wall of the power-assisting rack (51), the reset block (61) is slidably provided in the reset groove (6), and a reset spring (62) is provided in the reset groove (6) to abut against the reset block (61).

4. The punching die for photovoltaic shingled ribbon according to claim 1, characterized in that: The lower mold (2) is provided with a scraper (7), and one end of the scraper (7) abuts against the surface of the conveyor belt (32).

5. The punching die for photovoltaic shingled ribbon according to claim 1, characterized in that: The punching head (11) is threadedly connected to the upper die (1).