Semiconductor electroplating probe

By using the rebound mechanism of magnet block and return spring and the detachable plastic outer ring structure in the semiconductor electroplating probe, the problem of rebound failure caused by double sealing is solved, and the service life and maintenance convenience of the probe are improved.

CN221895162UInactive Publication Date: 2024-10-25SICHUAN JUEYUANXIANG SEMICON TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420525391.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-18
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Semiconductor plating probes with a double sealing structure cannot achieve normal rebound, resulting in the inability to guarantee the original performance of the probe.

Method used

A rebound mechanism composed of the first magnet block, the second magnet block and the return spring is used. The magnet block is sealed by a copper sleeve, and the return spring is isolated by an isolation copper sheet to prevent corrosion. At the same time, the detachable plastic outer ring and the card are used. The adapter structure improves the fixation and detachability of the probe.

Benefits of technology

It effectively prevents the corrosion of the rebound mechanism, maintains the elastic strength of the probe, increases the service life, and improves the maintenance and replacement efficiency of the probe through insulation and disassembly convenience.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221895162U_ABST
    Figure CN221895162U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of electroplating probes, and discloses a semiconductor electroplating probe which comprises a probe copper sleeve, a probe body is slidably inserted in the probe copper sleeve, a reset spring is fixed on the top surface in the probe copper sleeve, a first copper sleeve is fixed at one end of the reset spring, and a second copper sleeve is fixed at the other end of the reset spring. A first copper sleeve is fixed in the probe body, a first magnetic block is fixed in the first copper sleeve, an isolation copper sheet is fixed in the probe copper sleeve, a second copper sleeve is fixed at one end of the probe body, and a second magnetic block is fixed in the second copper sleeve. According to the electroplating probe, resilience force is applied to the probe body by using the characteristic that like poles of the first magnetic block and the second magnetic block repel each other, and the reset spring is adopted to assist resilience, so that the elastic strength borne by the probe body is equal to the elastic strength borne by the probe body in a traditional electroplating probe; therefore, under the condition that the original performance of the probe body is not influenced, the internal springback mechanism is effectively prevented from being corroded, and the service life of the electroplating probe is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of electroplating probes, in particular to a semiconductor electroplating probe. Background Art

[0002] When preparing the electrodes of solar cells, the traditional process usually adopts the screen printing process, while electroplating technology, as a new electrode preparation method, is being studied more and more widely. As a more promising electrode preparation method, electroplating can greatly reduce the cost of solar cell production process. At present, when electroplating the grid line electrode on the surface of the cell, the cell is usually clamped by a fixture, and the conductive probe on the fixture is accurately connected with the electroplating contact of the cell to achieve the conduction of the electroplating circuit.

[0003] According to a Chinese patent with publication number CN219653158U, a semiconductor electroplating probe includes a copper sleeve, a probe body arranged at one end of the copper sleeve, a plastic outer ring arranged on the copper sleeve and the probe body, a stop pin arranged between the probe body and the copper sleeve, a first sealing ring group arranged between the copper sleeve and the plastic outer ring, and a second sealing ring group arranged between the probe body and the plastic outer ring; the stop pin and the plastic outer ring are welded and connected, a cylindrical mounting boss is arranged at one end of the probe body close to the copper sleeve, a mounting groove corresponding to the mounting boss is arranged at one end of the copper sleeve close to the probe body, the mounting boss is located in the mounting groove, and the stop pin passes through the mounting groove and the mounting boss.

[0004] In the above scheme, the probe body and the plastic outer ring are sealed by the second sealing ring group, and the double sealing method prevents the electrolyte from seeping into the copper sleeve after sealing, resulting in the following disadvantages: after adopting the double sealing structure, the probe will not be able to achieve normal rebound, and the probe cannot be guaranteed to maintain its original performance. Utility Model Content

[0005] The utility model aims to provide a semiconductor electroplating probe to solve the problem that the probe cannot realize normal rebound and cannot ensure the original performance of the probe after adopting a double sealing structure.

[0006] In order to achieve the above-mentioned purpose of the utility model, the utility model adopts the following technical scheme: a semiconductor electroplating probe, including a probe copper sleeve, a probe body is slidably inserted inside the probe copper sleeve, a reset spring is fixed to the inner top surface of the probe copper sleeve, a first copper sleeve is fixed to one end of the reset spring, a first magnetic block is fixed to the inside of the first copper sleeve, an isolation copper sheet is fixed to the inside of the probe copper sleeve, the first copper sleeve is located above the isolation copper sheet, a second copper sleeve is fixed to one end of the probe body, and a second magnetic block is fixed to the inside of the second copper sleeve.

[0007] Preferably, the outer wall of the probe copper sleeve is provided with two plastic outer rings, and the two plastic outer rings are detachably arranged.

[0008] Preferably, two mounting plates are fixed on the left and right sides of the outer walls of the two plastic outer rings, and a mounting hole is opened on one side of the mounting plate. Among the several mounting holes, two mounting holes corresponding to the front and rear positions are a group, and bolts are inserted inside the mounting holes of each group, and nuts are threadedly connected to the outer walls of the bolts.

[0009] Preferably, two clamping grooves are formed inside the two plastic outer rings, and two clamping rings are fixed on the outer wall of the probe copper sleeve, and the clamping rings are slidably clamped with the inside of the clamping grooves.

[0010] Preferably, a limiting ring is fixed inside the probe copper sleeve, and the limiting ring is located below the second copper sleeve.

[0011] Preferably, two limiting openings are formed on the top surface of the limiting ring, and limiting strips are fixed on both left and right sides of the outer wall of the probe body, and the limiting strips are slidably inserted into the inside of the limiting openings.

[0012] Compared with the prior art, a semiconductor electroplating probe using the above technical solution has the following beneficial effects:

[0013] 1. In use, the spring rebound mechanism of the traditional electroplating probe is replaced with a rebound mechanism composed of the first magnetic block, the second magnetic block and the reset spring, the first copper sleeve and the second copper sleeve are used to effectively seal the first magnetic block and the second magnetic block, and the reset spring is isolated by an isolation copper sheet, so as to effectively prevent the electrolyte from corroding the first magnetic block, the second magnetic block and the reset spring, and utilize the property of the first magnetic block and the second magnetic block that the same charges repel each other to apply a rebound force to the probe body, and the reset spring is used to assist the rebound, so as to ensure that the elastic force strength of the probe body is equal to that of the probe body in the traditional electroplating probe, so as to effectively prevent the internal rebound mechanism from being corroded without affecting the original performance of the probe body, thereby increasing the service life of the electroplating probe;

[0014] 2. During use, the plastic outer ring can insulate the copper sleeve of the probe, making it convenient for the fixture to clamp the electroplated probe. The two plastic outer rings are detachably mounted together by bolts and nuts, making it easy to remove and replace the electroplated probe from the plastic outer ring. The plastic outer ring and the copper sleeve of the probe can be better fixed by providing a slidable clamping connection between the clamping ring and the inside of the clamping groove. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a perspective view of an embodiment.

[0016] Figure 2 It is an exploded stereogram of an embodiment.

[0017] Figure 3 It is a three-dimensional view of the second copper sleeve of the embodiment.

[0018] Figure 4 This is a disassembled stereoscopic view of the copper sleeve of the probe of the embodiment.

[0019] Figure 5 It is a three-dimensional view of the first copper sleeve of the embodiment.

[0020] In the figure: 1. Probe copper sleeve; 2. Probe body; 3. Reset spring; 4. First copper sleeve; 5. First magnetic block; 6. Isolation copper sheet; 7. Second copper sleeve; 8. Second magnetic block; 9. Plastic outer ring; 10. Mounting plate; 11. Mounting hole; 12. Bolt; 13. Nut; 14. Snap-in groove; 15. Snap-in ring; 16. Limiting ring; 17. Limiting opening; 18. Limiting strip. DETAILED DESCRIPTION

[0021] The preferred embodiments of the present invention are described in detail below in conjunction with the accompanying drawings.

[0022] like Figure 1-Figure 5 As shown, a semiconductor electroplating probe comprises a probe copper sleeve 1, a probe body 2 is slidably inserted inside the probe copper sleeve 1, a reset spring 3 is fixed to the inner top surface of the probe copper sleeve 1, a first copper sleeve 4 is fixed to one end of the reset spring 3, a first magnetic block 5 is fixed to the inside of the first copper sleeve 4, an isolation copper sheet 6 is fixed to the inside of the probe copper sleeve 1, the first copper sleeve 4 is located above the isolation copper sheet 6, a second copper sleeve 7 is fixed to one end of the probe body 2, and a second magnetic block 8 is fixed to the inside of the second copper sleeve 7.

[0023] During use, the spring rebound mechanism of the traditional electroplating probe is replaced with a rebound mechanism composed of the first magnetic block 5, the second magnetic block 8 and the reset spring 3, the first copper sleeve 4 and the second copper sleeve 7 are used to effectively seal the first magnetic block 5 and the second magnetic block 8, and the reset spring 3 is isolated with the isolation copper sheet 6, so as to effectively prevent the electrolyte from corroding the first magnetic block 5, the second magnetic block 8 and the reset spring 3, and utilize the property of the first magnetic block 5 and the second magnetic block 8 that like charges repel each other to apply a rebound force to the probe body 2, and the reset spring 3 is used to assist the rebound, so as to ensure that the elastic force strength applied to the probe body 2 is equal to the elastic force strength applied to the probe body 2 in the traditional electroplating probe, thereby effectively preventing the internal rebound mechanism from being corroded without affecting the original performance of the probe body 2, thereby increasing the service life of the electroplating probe.

[0024] like Figure 2-Figure 5As shown, the outer wall of the probe copper sleeve 1 is provided with two plastic outer rings 9, and the two plastic outer rings 9 are detachably arranged. Two mounting plates 10 are fixed on the left and right sides of the outer walls of the two plastic outer rings 9. A mounting hole 11 is provided on one side of the mounting plate 10. Among the plurality of mounting holes 11, two mounting holes 11 corresponding to the front and rear positions are a group, and bolts 12 are inserted into the interior of the mounting holes 11 of each group. Nuts 13 are threadedly connected to the outer walls of the bolts 12. Two clamping grooves 14 are provided in the interior of the two plastic outer rings 9. Two clamping rings 15 are fixed on the outer wall of the probe copper sleeve 1, and the clamping rings 15 are slidably clamped with the interior of the clamping groove 14. A limiting ring 16 is fixed inside the probe copper sleeve 1, and the limiting ring 16 is located below the second copper sleeve 7. Two limiting openings 17 are provided on the top surface of the limiting ring 16. Limiting strips 18 are fixed on the left and right sides of the outer wall of the probe body 2, and the limiting strips 18 are slidably inserted into the interior of the limiting opening 17.

[0025] During use, the plastic outer ring 9 can insulate the probe copper sleeve 1, making it convenient for the fixture to clamp the electroplated probe. The two plastic outer rings 9 are detachably mounted together by bolts 12 and nuts 13, making it easy to disassemble and replace the electroplated probe from the plastic outer ring 9. By setting a snap ring 15 and a slidable snap connection inside the snap groove 14, the plastic outer ring 9 and the probe copper sleeve 1 are better fixed. The limiting ring 16 can limit the probe body 2 to prevent the probe body 2 from falling off from the inside of the probe copper sleeve 1. By setting a limiting strip 18 and a slidable insertion inside the limiting opening 17, the probe body 2 is limited to prevent the probe body 2 from rotating when it rebounds.

[0026] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A semiconductor electroplating probe, comprising a probe copper sleeve (1), characterized in that: A probe body (2) is slidably inserted into the probe copper sleeve (1); a reset spring (3) is fixed to the internal top surface of the probe copper sleeve (1); a first copper sleeve (4) is fixed to one end of the reset spring (3); a first magnetic block (5) is fixed to the inside of the first copper sleeve (4); an isolation copper sheet (6) is fixed to the inside of the probe copper sleeve (1); the first copper sleeve (4) is located above the isolation copper sheet (6); a second copper sleeve (7) is fixed to one end of the probe body (2); a second magnetic block (8) is fixed to the inside of the second copper sleeve (7).

2. A semiconductor electroplating probe according to claim 1, characterized in that: The outer wall of the probe copper sleeve (1) is provided with two plastic outer rings (9), and the two plastic outer rings (9) are detachably arranged.

3. A semiconductor electroplating probe according to claim 2, characterized in that: Two mounting plates (10) are fixed on the left and right sides of the outer walls of the two plastic outer rings (9), and a mounting hole (11) is opened on one side of the mounting plate (10). Among the plurality of mounting holes (11), two mounting holes (11) corresponding to the front and rear positions form a group, and bolts (12) are inserted into the interior of each group of mounting holes (11), and nuts (13) are threadedly connected to the outer walls of the bolts (12).

4. A semiconductor electroplating probe according to claim 3, characterized in that: Two clamping grooves (14) are provided inside the two plastic outer rings (9), and two clamping rings (15) are fixed on the outer wall of the probe copper sleeve (1), and the clamping rings (15) are slidably clamped with the inside of the clamping grooves (14).

5. A semiconductor electroplating probe according to claim 4, characterized in that: A limiting ring (16) is fixed inside the probe copper sleeve (1), and the limiting ring (16) is located below the second copper sleeve (7).

6. A semiconductor electroplating probe according to claim 5, characterized in that: The top surface of the limiting ring (16) is provided with two limiting openings (17), and limiting strips (18) are fixed on both left and right sides of the outer wall of the probe body (2), and the limiting strips (18) are slidably inserted into the inside of the limiting openings (17).