High-temperature roasting stainless steel single-layer barrel and double-layer bottom burning-resistant crucible

By using stainless steel materials with good high-temperature stability and heat conduction materials in high-temperature roasting stainless steel crucibles, and welding the ribs and the cylinder at the double-layer bottom, the problem of uneven heat conduction is solved, and the roasting effect and the stability of the crucible are improved. sex.

CN221903210UActive Publication Date: 2024-10-29HUBEI JUNENG GRAPHITE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322828441.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-20
Publication Date
2024-10-29
Estimated Expiration
2033-10-20

AI Technical Summary

Technical Problem

High-temperature roasting stainless steel single-layer cylinder double-bottom burn-resistant crucible. Due to the single-layer cylinder design, heat conduction is uneven, which affects the accuracy and consistency of the roasting results.

Method used

By selecting stainless steel materials with good high-temperature stability and adding heat conductive materials to the outside of the cylinder, the stability and deformation resistance of the cylinder are enhanced. At the same time, the reinforcement ribs at the double bottom are continuously welded to the cylinder to ensure the stability of the double bottom. and sealing, and set a thermometer and through holes on the cover to improve temperature distribution.

Benefits of technology

It achieves uniform heat conduction, improves the temperature distribution and roasting effect of the sample, ensures the stability and sealing of the crucible, and avoids crucible breakage during the heating process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221903210U_ABST
    Figure CN221903210U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of crucibles, and discloses a high-temperature roasting stainless steel single-layer barrel double-layer bottom burning-resistant crucible which comprises a burning-resistant crucible body, the burning-resistant crucible body comprises a barrel body, a double-layer bottom, reinforcing ribs, a cover plate, a thermometer, a lifting handle, a through hole, an air hole, a sealing ring, internal threads and external threads, the double-layer bottom and the reinforcing ribs are installed at the bottom of the barrel body, and the double-layer bottom is installed at the bottom of the barrel body. The top of the cover plate is provided with a through hole, the bottom of the double-layer bottom is provided with an air hole, the bottom of the cover plate is provided with a sealing ring, the inner side face of the cover plate is provided with internal threads, and the top of the outer side face of the cylinder body is provided with external threads. According to the high-temperature roasting stainless steel single-layer barrel double-layer bottom burning-resistant crucible, a stainless steel material with good high-temperature stability is selected, a heat conduction material can be added outside the barrel to enhance uniform conduction of heat, the double-layer bottom is continuously welded to the barrel through the reinforcing ribs, the stability and the sealing performance of the double-layer bottom are guaranteed, and the service life of the crucible is prolonged. Therefore, the temperature distribution and roasting effect of the sample are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of crucibles, in particular to a high-temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible. Background Art

[0002] High temperature roasting stainless steel single layer cylinder double bottom sintered crucible is a vessel used for high temperature furnace smelting metal or roasting food. It is made of stainless steel, with a single layer cylinder and a double layer bottom, and can withstand high temperature roasting in a high temperature furnace. The single layer cylinder design of this crucible can maintain the high temperature in the furnace and prevent heat loss. The double layer bottom can withstand higher temperatures and prevent the bottom from overheating, thereby protecting the structure and service life of the crucible.

[0003] However, due to the design of the single-layer cylinder, the heat conduction inside the cylinder of the high-temperature roasting stainless steel single-layer cylinder double-layer bottom sintered crucible may be uneven, resulting in uneven temperature distribution of the sample during the roasting process. This may affect the accuracy and consistency of the roasting results, so it is necessary to improve the existing technology to meet actual needs. Utility Model Content

[0004] 1. Technical issues to be resolved

[0005] In view of the deficiencies in the prior art, the utility model provides a high-temperature roasting stainless steel single-layer cylinder double-bottom burn-resistant crucible, which has the advantages of improving the stability and deformation resistance of the cylinder by selecting stainless steel material with good high-temperature stability and conducting reasonable structural design, and heat conduction material can be added to the outside of the cylinder to enhance the uniform conduction of heat, and the double-layer bottom is continuously welded to the cylinder through reinforcing ribs to enhance the connection stability of the double-layer bottom, ensure the stability and sealing of the double-layer bottom, thereby improving the temperature distribution of the sample and the roasting effect, and solving the above-mentioned technical problems.

[0006] (II) Technical solution

[0007] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a high-temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible, comprising a crucible, the crucible comprising a cylinder, a double-layer bottom, a reinforcing rib, a cover plate, a thermometer, a handle, a through hole, an air hole, a sealing ring, an internal thread and an external thread;

[0008] A double bottom and reinforcing ribs are installed at the bottom of the cylinder, a thermometer and a handle are installed at the top of the cover plate, a through hole is provided at the top of the cover plate, an air hole is provided at the bottom of the double bottom, a sealing ring is installed at the bottom of the cover plate, an internal thread is provided on the inner side of the cover plate, and an external thread is provided on the top of the outer side of the cylinder.

[0009] Preferably, the double-layer bottom is continuously welded to the cylinder through reinforcing ribs, and air holes are opened at the bottom of the double-layer bottom. The air holes have a diameter of 30 mm and are evenly distributed.

[0010] Through the above technical solution, the double bottom is continuously welded to the cylinder through reinforcing ribs to enhance the connection stability of the double bottom and ensure the stability and sealing of the double bottom. The air holes are provided to exhaust the gas inside the crucible, maintain the air pressure balance and prevent the crucible from breaking during heating.

[0011] Preferably, an internal thread is formed on the inner side of the cover plate, an external thread is welded on the top of the outer side of the cylinder, the external thread is threadably mounted on the internal thread, and a sealing ring is fixedly mounted on the bottom surface of the cover plate.

[0012] Through the above technical solution, the cover plate is placed on the top of the cylinder, the cover plate is rotated to rotate the cylinder, the external thread and the internal thread are threadedly installed, and the setting of the sealing ring facilitates further sealing of the cylinder.

[0013] Preferably, a handle is fixedly installed at the middle end of the top of the cover plate, and a thermometer is connected through one side of the top of the cover plate. The thermometer is of contact type, and the probe is located directly below the cover plate.

[0014] Through the above technical solution, the contact thermometer usually has a probe directly inserted into the crucible, which can accurately measure the temperature in the crucible and facilitate the control of the temperature in the crucible. The setting of the handle facilitates the rotation of the cover.

[0015] Preferably, the top of the cover plate is penetrated by through holes, the through holes have a diameter of 30 mm and are evenly distributed, and the cover plate is made of 0Cr18Ni9 and has a thickness of 3 mm.

[0016] Through the above technical solution, the setting of the cover plate can prevent the sample from sublimation, and the cover plate can also prevent the sample from being contaminated by other samples. The crucible is generally heated in a high-temperature muffle furnace, the heating temperature is high, and the heating time is generally long, so water vapor is generated and discharged through the through hole.

[0017] Preferably, the cylinder body is made of stainless steel with good high-temperature stability, and the outer wall of the cylinder is coated with a heat-conducting material, and the heat-conducting material is aluminum borate.

[0018] Through the above technical scheme, the cylinder is made of stainless steel with good high-temperature stability, and a reasonable structural design is carried out to improve the stability and deformation resistance of the cylinder. Heat conduction material can be added to the outside of the cylinder to enhance the uniform conduction of heat, thereby improving the temperature distribution and roasting effect of the sample.

[0019] Compared with the prior art, the utility model provides a high-temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible, which has the following beneficial effects:

[0020] 1. The utility model selects stainless steel material with good high-temperature stability for the cylinder and performs reasonable structural design to improve the stability and deformation resistance of the cylinder. Heat conduction material can be added to the outside of the cylinder to enhance the uniform conduction of heat. The double bottom is continuously welded to the cylinder through reinforcing ribs to enhance the connection stability of the double bottom, ensure the stability and sealing of the double bottom, thereby improving the temperature distribution and roasting effect of the sample.

[0021] 2. The contact thermometer of the utility model usually has a probe directly inserted into the crucible, which can accurately measure the temperature in the crucible, making it convenient to control the temperature in the crucible, and the setting of the handle makes it convenient to rotate the cover. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a three-dimensional schematic diagram of the structural crucible of the utility model;

[0023] Figure 2 This is a front view schematic diagram of the crucible structure of the utility model;

[0024] Figure 3 It is a side cross-sectional schematic diagram of the structural crucible of the utility model.

[0025] Among them: 1. crucible; 2. cylinder; 3. double bottom; 4. reinforcing ribs; 5. cover plate; 6. thermometer; 7. handle; 8. through hole; 9. air hole; 10. sealing ring; 11. internal thread; 12. external thread. DETAILED DESCRIPTION

[0026] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0027] See also Figure 1-3 A high-temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible, comprising a crucible 1, the crucible 1 comprising a cylinder 2, a double-layer bottom 3, a reinforcing rib 4, a cover plate 5, a thermometer 6, a handle 7, a through hole 8, an air hole 9, a sealing ring 10, an internal thread 11 and an external thread 12;

[0028] A double bottom 3 and a reinforcing rib 4 are installed at the bottom of the cylinder 2, a thermometer 6 and a handle 7 are installed on the top of the cover plate 5, a through hole 8 is provided on the top of the cover plate 5, an air hole 9 is provided at the bottom of the double bottom 3, a sealing ring 10 is installed at the bottom of the cover plate 5, an internal thread 11 is provided on the inner side of the cover plate 5, and an external thread 12 is provided on the top of the outer side of the cylinder 2.

[0029] Specifically, the double bottom 3 is continuously welded to the cylinder 2 through the reinforcing ribs 4, and air holes 9 are opened at the bottom of the double bottom 3. The air holes 9 have a diameter of 30 mm and are evenly distributed. The advantage is that the double bottom 3 is continuously welded to the cylinder 2 through the reinforcing ribs 4, which strengthens the connection stability of the double bottom 3 and ensures the stability and sealing of the double bottom 3. The air holes 9 are provided to exhaust the gas inside the crucible 1, maintain the air pressure balance, and prevent the crucible 1 from breaking during heating.

[0030] Specifically, an internal thread 11 is provided on the inner side surface of the cover plate 5, an external thread 12 is welded on the top of the outer side surface of the cylinder 2, the external thread 12 is threadedly installed with the internal thread 11, and a sealing ring 10 is fixedly installed on the bottom surface of the cover plate 5. The advantage is that the cover plate 5 is placed on the top of the cylinder 2, and the cover plate 5 is rotated to rotate the cylinder 2, the external thread 12 is threadedly installed with the internal thread 11, and the setting of the sealing ring 10 facilitates further sealing of the cylinder 2.

[0031] Specifically, a handle 7 is fixedly installed at the middle end of the top of the cover plate 5, and a thermometer 6 is connected through one side of the top of the cover plate 5. The thermometer 6 is of contact type, and the probe is located directly below the cover plate 5. The advantage is that the contact thermometer 6 usually has a probe directly inserted into the crucible 1, which can accurately measure the temperature in the crucible 1, and is convenient for controlling the temperature in the crucible 1. The setting of the handle 7 facilitates the rotation of the cover plate 5.

[0032] Specifically, the top of the cover plate 5 is penetrated by through holes 8, the through holes 8 have a diameter of 30 mm and are evenly distributed, the cover plate 5 is made of 0Cr18Ni9 and has a thickness of 3 mm, and the advantage is that the setting of the cover plate 5 can prevent the sample from sublimating, and the cover plate 5 can also prevent the sample from being contaminated by other samples. The crucible 1 is generally heated in a high-temperature muffle furnace, the heating temperature is high, and the time is generally long, so water vapor is generated and discharged through the through holes 8.

[0033] Specifically, the barrel 2 is made of stainless steel with good high-temperature stability, and the outer wall of the barrel 2 is coated with a heat-conducting material, and the heat-conducting material is aluminum borate. The advantage is that the barrel 2 is made of stainless steel with good high-temperature stability and a reasonable structural design is performed to improve the stability and deformation resistance of the barrel 2. Heat-conducting material can be added to the outside of the barrel 2 to enhance the uniform conduction of heat, thereby improving the temperature distribution and roasting effect of the sample.

[0034] When in use, the sample is placed inside the cylinder 2, the cover plate 5 is placed on the top of the cylinder 2, the cover plate 5 is rotated to rotate the cylinder 2, the external thread 12 and the internal thread 11 are threadedly installed, and the cylinder 2 is placed in a high-temperature muffle furnace for heating. The air hole 9 is provided to exhaust the gas inside the crucible 1, maintain the air pressure balance, and prevent the crucible 1 from breaking during the heating process. The water vapor generated inside the cylinder 2 is discharged through the through hole 8. The contact thermometer 6 usually has a probe directly inserted into the crucible 1, which can accurately measure the temperature inside the crucible 1 and facilitate the control of the temperature inside the crucible 1. The handle 7 is provided to facilitate the rotation of the cover plate 5 to complete the use process of the crucible 1.

[0035] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A high-temperature roasted stainless steel single-layer cylindrical double-layer bottom sintered crucible, comprising a crucible (1), characterized in that: The crucible (1) comprises a cylinder (2), a double bottom (3), a reinforcing rib (4), a cover plate (5), a thermometer (6), a handle (7), a through hole (8), an air hole (9), a sealing ring (10), an internal thread (11) and an external thread (12); A double-layer bottom (3) and reinforcing ribs (4) are installed at the bottom of the cylinder (2); a thermometer (6) and a handle (7) are installed at the top of the cover plate (5); a through hole (8) is provided at the top of the cover plate (5); an air hole (9) is provided at the bottom of the double-layer bottom (3); a sealing ring (10) is installed at the bottom of the cover plate (5); an internal thread (11) is provided on the inner side surface of the cover plate (5); and an external thread (12) is provided on the top of the outer side surface of the cylinder (2).

2. The high temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible according to claim 1, characterized in that: The double-layer bottom (3) is continuously welded to the cylinder (2) via reinforcing ribs (4), and air holes (9) are provided at the bottom of the double-layer bottom (3). The air holes (9) have a diameter of 30 mm and are evenly distributed.

3. The high temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible according to claim 1, characterized in that: The inner side surface of the cover plate (5) is provided with an internal thread (11), the top of the outer side surface of the cylinder (2) is welded with an external thread (12), the external thread (12) is threadedly mounted with the internal thread (11), and a sealing ring (10) is fixedly mounted on the bottom surface of the cover plate (5).

4. The high temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible according to claim 1, characterized in that: A handle (7) is fixedly mounted at the middle of the top of the cover plate (5), and a thermometer (6) is connected through one side of the top of the cover plate (5). The thermometer (6) is of contact type, and the probe is located directly below the cover plate (5).

5. The high temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible according to claim 1, characterized in that: The top of the cover plate (5) is penetrated by through holes (8), the through holes (8) have a diameter of 30 mm and are evenly distributed, and the cover plate (5) is made of 0Cr18Ni9 and has a thickness of 3 mm.

6. The high temperature roasted stainless steel single-layer cylinder double-layer bottom sintered crucible according to claim 1, characterized in that: The cylinder (2) is made of stainless steel with good high-temperature stability, and the outer wall of the cylinder (2) is coated with a heat-conducting material, wherein the heat-conducting material is aluminum borate.