Forging and pressing die for building component

The blanks of building components are quickly manufactured through forging molds, which solves the problems of poor strength of light steel columns and complicated on-site assembly in light steel house structures, and achieves efficient installation and production.

CN221909635UActive Publication Date: 2024-10-29CHANGZHOU JINGLING CASTING & FORGING
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322919519.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-31
Publication Date
2024-10-29
Estimated Expiration
2033-10-31

AI Technical Summary

Technical Problem

In the existing light steel house structure, the strength of the light steel columns is poor, and the on-site assembly is complicated, resulting in low installation efficiency.

Method used

The forging mold is used to quickly manufacture the blank of the building component. The bar is heated and forged in the mold to form a shape that matches the mold cavity, and then heat treated and machined to obtain the finished product.

Benefits of technology

It improves the manufacturing efficiency of building components and the yield of finished products, simplifies the installation process, and reduces the construction period and production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221909635U_ABST
    Figure CN221909635U_ABST
Patent Text Reader

Abstract

The utility model relates to a forging and pressing die for building components, which comprises an upper die and a lower die, the upper die comprises an upper die seat, a first cavity is arranged on the upper die seat, two opposite side wall surfaces in the first cavity are first inclined surfaces, two convex parts are arranged in the first cavity, and the upper die seat is provided with a second inclined surface; one side faces of the two protruding parts are combined with the other side wall faces in the first cavities into a whole, and a groove is formed between the two first cavities. The lower die comprises a lower die base, a second cavity is formed in the lower die base, and two opposite side wall faces in the second cavity are third inclined faces. According to the utility model, the workblank form of the building component can be quickly forged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of forging, in particular to a forging die for building components. Background Art

[0002] Steel structure buildings are buildings that use construction steel to form a load-bearing structure. They are usually made of beams, columns, trusses and other components made of steel and steel plates. Steel structure buildings use steel plates or steel to replace reinforced concrete in traditional buildings. They are stronger and more earthquake-resistant, and the components can be factory-made and installed on site, thus greatly reducing the construction period.

[0003] For example, CN102359182A discloses a light steel house structure, which includes a light steel floor and a light steel wall. The light steel wall includes an inner wall plate, a light steel wall frame and an outer wall plate. The light steel wall frame includes vertically arranged light steel columns and transversely arranged cross beams. The light steel columns are laterally spaced and connected into one by the cross beams. One side of the light steel wall frame is connected to the outer wall plate and the other side is connected to the inner wall plate. The light steel floor includes floor beams and floor panels. The floor beams intersect with the light steel wall and are fixedly connected to the cross beams. The floor panels are laid on the floor beams. The light steel columns of the upper and lower floors of the light steel wall are connected by a tenon tube. The two ends of the tenon tube are respectively inserted into the ends of the chord rods where the light steel columns of the upper and lower floors are connected, and the tenon tubes and the chord rods are fixedly connected by screws.

[0004] In the light steel house structure of the above structure, the light steel column is a sheet truss structure composed of two chords or a square truss structure composed of four chords. The strength of the light steel column of this structure is poor, and the light steel columns of the upper and lower floors of the light steel wall are connected by tenon tubes. Each connection of the tenon tube needs to be fixed with screws and needs to be assembled on site. During assembly, due to the large number of parts, the assembly is very complicated, thereby reducing the convenience and efficiency of installation. Utility Model Content

[0005] The utility model provides a forging die for a building component. The utility model can quickly forge a rough shape of the building component.

[0006] Forging dies for building components, including:

[0007] An upper die, the upper die comprising an upper die seat, a first cavity is provided on the upper die seat, two opposite sidewall surfaces in the first cavity are first inclined surfaces, two protrusions are provided in the first cavity, one side surface of the two protrusions is respectively integrated with the remaining sidewall surfaces in the first cavity, and a groove is formed between the two first cavities;

[0008] The lower mold comprises a lower mold base, a second cavity is arranged on the lower mold base, and two opposite side wall surfaces in the second cavity are third inclined surfaces.

[0009] Although the building component involved in the utility model looks relatively simple in shape, there are multiple curved surfaces on its surface. Therefore, it is difficult to obtain the required finished product by directly cutting. Therefore, the utility model adopts forging to manufacture the blank of the building component. When forging is required, the bar heated to a specified temperature is placed in the second cavity on the lower die seat, and the upper die applies a force to deform the bar, thereby forging a blank state of the building component matching the forging die cavity. After the building component in the blank state is heat treated and machined, the finished building component can be obtained. The utility model manufactures the blank by forging die, which is not only efficient, but also has a very high acquisition rate of blanks. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] Figure 1 It is a three-dimensional view of the first component in the first direction.

[0011] Figure 2 It is a three-dimensional view of the first component in the second direction.

[0012] Figure 3 It is a top view of a plurality of first components, columns and connecting parts after being spliced ​​together.

[0013] Figure 4 This is the assembly drawing of the upper and lower first components and the I-beam.

[0014] Figure 5 Schematic diagram of bar heating and temperature screening.

[0015] Figure 6 Schematic diagram of a building component blank formed by forging.

[0016] Figure 7 Schematic diagram of forging die.

[0017] Figure 8 Schematic diagram of the upper mold.

[0018] Fig. 9 Schematic diagram of the lower mold.

[0019] Fig.10 This is a schematic diagram of a high-temperature bar buffer receiving device.

[0020] Fig.11 For Fig.10 The schematic diagram shows a part of the components hidden on the basis of the image.

[0021] Fig.12 To buffer the receiving container from Fig.11 Schematic diagram of switching from the unloading state to the receiving state.

[0022] Fig.13 It is a cross-sectional view of the buffer material receiving container and the connecting rod when the material is not received.

[0023] Fig.14 It is a cross-sectional view of the buffer receiving container and the connecting rod in the material receiving state.

[0024] Fig.15 It is a cross-sectional view of the middle buffer component.

[0025] Fig.16 A three-dimensional diagram of the fixture.

[0026] Fig.17 A cross-sectional view of the fixture.

[0027] Markings in the accompanying drawings: first component A, main body 1, first connecting part 2, recess 2a, splicing part 3, splicing surface 3a, mounting hole 3b, supporting part 4, first notch 4a, second notch 4b, second component B, column 5, connecting piece 6, I-beam 7, crossbeam mounting component 8.

[0028] Upper mold 10, upper mold base 10a, first cavity 10b, first inclined surface 10c, protrusion 10d, groove 10e; second inclined surface 10f, groove bottom 10g, inclined surface 10h, lower mold 11, lower mold base 11a, second cavity 11b, third inclined surface 11c, second pre-pressing groove 11d.

[0029] Rod material C, heating device D, building component blank E, automatic screening device F, chute G.

[0030] High-temperature bar material buffering receiving device H, bracket 20, bar material chute 21, buffering receiving container 22, receiving cylinder 22a, swing arm 22b, swing arm body 22b1, combining seat 22b2, support 22c, shaft 22d, cylinder 22e, bearing 22f, opening 22g, hinged seat 22h, flip driver 23, lower support 24, buffer seat 25, spring 26, connecting rod 27, first contact 27a, second contact 27b, support plate 28, intermediate buffer component 29, first spring 29a, tubular component 29b, transmission rod 29c, annular baffle 29d, slot 29e, clamping part 29f, trigger switch 30.

[0031] The seat body 40 , the clamping support 41 , the supporting boss 42 , the pressing block 43 , the bolt 44 , the second spring 45 , the positioning pin 46 , and the third spring 47 . DETAILED DESCRIPTION

[0032] Combine the following Figures 1 to 17 The utility model is described in detail.

[0033] like Figures 1 to 4As shown, the building component of the utility model includes a first component A, the first component A includes a main body 1, a splicing part 3, and a supporting part 4. A first connecting part 2 is provided on the first side of the main body 1, and the first connecting part 2 is used to form an abutment with a column 5. The first connecting part 2 protrudes from the first side of the main body 1. A recess 2a is provided on the end surface of the first connecting part 2, and there are multiple recesses 2a, which are used to position the first component A during machining.

[0034] The splicing parts 3 are arranged at both ends of the main body 1, and the splicing parts 3 are provided with splicing surfaces 3a for splicing, and the splicing surfaces 3a have an inclination angle of 45°. Each splicing part 3 is also provided with a mounting hole 3b, and the mounting hole 3b is for bolts to pass through. The two adjacent splicing surfaces 3a are spliced ​​together to form an angle of 90°, and the locking bolt (not shown in the figure) is passed through the mounting hole 3b, so that the two splicing parts 3 are locked as a whole; or after a connecting component 6 is provided between the two adjacent splicing surfaces 3a, the locking bolt is passed through the mounting hole 3b and the connecting member 6, and the two splicing parts 3 and the connecting component 6 are locked as a whole.

[0035] The support part 4 is arranged on the second side surface of the main body 1, and is used to connect the I-beam 7. The end of the support part 4 is connected to the splicing part 3, which is conducive to increasing the overall strength of the building component. The support part 4 is provided with a first notch 4a and a second notch 4b.

[0036] In this embodiment, the main body 1, the splicing portion 3 and the supporting portion 4 are integrally formed by forging. After the integral forging, they are machined, that is, the main body 1 and the splicing portion 3 are cut so that the first coupling portion 2 is protruding relative to the main body 1, the splicing portion 3 is drilled to form a mounting hole 3b, and the supporting portion 4 is cut to machine a first notch 4a and a second notch 4b on the supporting portion 4.

[0037] The building component of the utility model also includes a second component B, which includes a column 5, a connecting component 6, and a locking bolt (not shown in the figure). The cross section of the column 5 is a hollow steel pipe in a rectangular or square shape. The perimeter and wall thickness of the column 5 are manufactured as required. The column 5 is fixed to the connecting component 6. For example, a connecting component 6 is fixed to each of the four corners of the column 5. The connecting component 6 is preferably fixed to the column 5 by welding. The two opposite side walls of the connecting component 6 are respectively matched with one of the splicing surfaces 3a. The locking bolt passes through the mounting hole 3b and the connecting component 6, and the splicing parts 3 on both sides of the connecting component 6 are locked into one. In this way, after the four first components A are matched with the connecting component 6 respectively, the four first components A form a frame, and after the column 5 is matched with the frame, the first combination part 2 protruding from the first side surface of the main body 1 forms abutment with the outer peripheral surface of the column 5, which is conducive to increasing the bonding force between the first component A and the column 5.

[0038] The second component B also includes an I-beam 7 and a beam mounting component 8 for mounting a beam. The I-beam 7 cooperates with the first notch 4 a and the second notch 4 b respectively. The I-beam 7 is fixed to the support portion 4 , and the beam mounting component 8 is fixed to the I-beam 7 .

[0039] In this embodiment, at least two groups of the frame bodies are formed on the column 5, and the two groups of frame bodies are arranged one above the other. After the two ends of the I-beam 7 are respectively matched with the first notch 4a and the second notch 4b on the upper and lower support parts 4, the I-beam 7 is fixed to the support part 4 by welding. The crossbeam mounting component 8 is a steel plate, and an assembly hole is provided on the crossbeam mounting component 8. The crossbeam mounting component 8 and the I-beam 7 are fixed to be integrated by welding. When it is necessary to install a crossbeam between multiple columns 5, the end of the crossbeam is fastened to the crossbeam mounting component 8 by bolts.

[0040] As can be seen from the above, the structure of the building component of the utility model is simple. When it is necessary to use the building component of the utility model to construct a house, after connecting the connecting parts 6 of multiple building components arranged on the column 5 by locking bolts, these building components are tightly held on the column 5, and then the I-beam 7 is matched with the first notch 4a and the second notch 4b on the support part 4, and the I-beam 7 is welded and fixed to the support part 4, and then the crossbeam mounting part 8 and the I-beam 7 are fixed into one by welding. Then, after the column 5 is erected, the column 5 is fixed on the foundation (such as the foundation). When installing the crossbeam between the multiple columns 5, the end of the crossbeam is bolted and locked into one with the crossbeam mounting part 8. When the above structure is adopted, since the column 5 is a hollow steel pipe, a single column 5 does not need to be spliced ​​with multiple steel pipes along the transverse direction, and only needs to be customized according to the stress conditions. Therefore, not only the design and manufacture of the column 5 are simplified, but also the installation of the first component A and the second component B is also very simple. Therefore, the first component A and the second component B can be quickly assembled to form the frame structure of the house.

[0041] like Figures 1 to 15 As shown, the forging die of the building component is described below. The forging die of the building component in the utility model mainly refers to the manufacturing method of the first component A, which includes the following steps:

[0042] S1, sending the rod C into the heating device D for heating. The heating device D can be a medium frequency furnace or a high frequency furnace. In this embodiment, the heating device D preferably uses a medium frequency furnace. For example, the cylindrical rod C is heated to 1175°C in the medium frequency furnace.

[0043] S2, after the heated bar material C passes the temperature screening, the screened qualified bar material C is sent to the forging die in the forging equipment for forging to obtain the building component blank E. In the utility model, an automatic screening device is used to screen whether the temperature of the bar material C is qualified, and the automatic screening device F disclosed in CN112809317A is preferably used. The structure and working principle of the automatic screening device F are not described in detail here.

[0044] Regarding whether the heating of the bar C is qualified, in the present invention, the temperature of the bar C is considered qualified within the range of 1150-1250°C, and the temperature below 1150°C or above 1250°C is considered unqualified. Only the bar C with qualified temperature can be used for forging. In this embodiment, the bar C is preferably heated to 1200°C, and the qualified bar C is transported to the side of the forging equipment through the chute G, and then the bar C is transferred to the mold for forging by a handheld fixture or a manipulator, so as to obtain the building component blank E.

[0045] There are multiple forging equipment working in the production workshop at the same time. The impact force of the forging equipment during operation causes the foundation to vibrate, and other forging equipment will be affected by this vibration force. Therefore, after placing bar C into the cavity of the forging die, due to the cylindrical shape of bar C itself, it is easy for bar C to roll in the cavity due to the influence of vibration force or other factors, and the front and back position is not accurate, thus affecting the forging forming. Because bar C weighs 60-70 kg, it is difficult for the forger to adjust the position. Two people are required to move the die front and back face to face, which is inefficient. In addition, due to the high temperature of bar C, if the position of bar C is adjusted during the forging process, there is obviously a safety hazard.

[0046] In the present invention, in step S2, the qualified bar material C is pre-pressed by a forging die, so that both ends of the bar material C are bent to form a bending portion, which is the prototype of the splicing portion 3.

[0047] S3, normalizing and quenching and tempering the cooled building component blank E, that is, taking the building component blank E out of the forging die, allowing the building component blank E to cool naturally, and then normalizing and quenching and tempering the building component blank E.

[0048] In this embodiment, the normalizing process of the building component blank E is as follows: after the building component blank E of S2 is naturally cooled, the building component blank E is heated to 890±10°C, kept warm for 100±10 minutes, then air-cooled, and then subjected to a quenching and tempering heat treatment. The quenching and tempering heat treatment process is as follows: the building component blank E is quenched at a quenching temperature of 850±20°C for 130±20 minutes, then the building component blank E is placed in a quenching liquid for water cooling for 5-8 minutes, and then tempered in an environment of 450±20°C for 180±20 minutes.

[0049] For example, the building component blank E is heated to 900°C, kept at this temperature for 100 minutes, and then air-cooled. The building component blank E is then quenched at 860°C for 130 minutes. The building component blank E is then placed in a quenching liquid for water cooling for 7 minutes, and then tempered in an environment at 450°C for 190 minutes.

[0050] S4, the building component blank E after normalizing and quenching and tempering is shot blasted to remove oxide scale.

[0051] S5, checking whether there are cracks on the surface of the building component blank E after the oxide scale is removed, for example, by detecting whether there are cracks on the surface of the building component blank E by means of magnetic particle inspection.

[0052] S6, machining the building component blank E with no cracks on the surface to obtain a finished building component, that is: cutting the main body 1 and the splicing part 3 to form the first connecting part 2, drilling the splicing part 3 to form the mounting hole 3b, and cutting the supporting part 4 to machine a first notch 4a and a second notch 4b on the supporting part 4 to obtain a first component A.

[0053] like Figures 7 to 9 As shown, the forging die used in the above step S2 includes an upper die 10 and a lower die 11, wherein the upper die 10 includes an upper die base 10a, and a first cavity 10b is provided on the upper die base 10a, wherein two opposite side wall surfaces in the first cavity 10b are first inclined surfaces 10c, and two protrusions 10d are provided in the first cavity 10b, and one side surface of the two protrusions 10d is respectively combined with the remaining side wall surfaces in the first cavity 10b to form a whole, and a groove 10e is formed between the two first cavities 10b, and the end surfaces at both ends of the protrusion 10d are second inclined surfaces 10f, and the second inclined surfaces 10f are opposite to the first inclined surfaces 10c.

[0054] The lower mold 11 comprises a lower mold base 11 a , on which a second cavity 11 b is disposed. Two opposite sidewall surfaces in the second cavity 11 b are third inclined surfaces 11 c .

[0055] During the forging process, the groove 10e is used to form the support portion 4, the first inclined surface 10c and the end surfaces of the protruding portion 10d and the third inclined surface 11c are used to form the splicing portion 3 during the forging process, and the second cavity 11b is used to form the main body 1.

[0056] During the initial trial production of the first component A, the upper die 10 and the lower die 11 are made of high-strength alloy steel (such as 5GrNiMo). After the die of this material is used to forge 150-200 pieces of building component blanks E, the die will produce cracks greater than 50mm. In order to overcome the impact force of the hammer head in the forging equipment on the die during the forging process, which is easy to damage the surface of the die, and the joint of the protrusion 10d and the first inclined surface 10c, and the joint of the protrusion 10d and the first cavity 10b (both sides of the groove 10e) are very easy to crack, a first surfacing layer is provided on the surface of the first inclined surface 10c and the groove 10e, and a second surfacing layer is provided on the surface of the protrusion 10d. The surface of the second cavity 11b is provided with a third surfacing layer, which is surfacing with a flux-cored wire with a number of 545, and the surface hardness of the surfacing layer formed after surfacing is 40-45HRC.

[0057] By surfacing the first inclined surface 10c and the groove 10e, and surfacing the surface of the protrusion 10d, the cavity surface of the upper mold 10 is protected. By surfacing the surface of the second cavity 11b, the cavity surface of the lower mold 11 is protected.

[0058] In this embodiment, the first surfacing layer is surfacing welded with flux-cored wire No. 126, and the surface hardness of the surfacing layer formed after surfacing welding is 25-30HRC, and the second surfacing layer is surfacing welded with flux-cored wire No. 248, and the surface hardness of the surfacing layer formed after surfacing welding is 45-50HRC. The surfacing thickness of the first surfacing layer and the second surfacing layer is 70-90mm, and the preferred surfacing thickness is 80mm.

[0059] The above-mentioned first cladding layer and second cladding layer are used. It has been verified that when a 5-ton hammer is used to forge a building component blank E, the mold life is 640-660 pieces. After carbon arc gouging, the bottom cracking degree of the first cladding layer and the second cladding layer is detected. Although the first cladding layer and the second cladding layer have cracks at their bottoms, the depth of the cracks is within 20 mm. The first cladding layer and the second cladding layer of the above-mentioned structure increase the number of times the mold is used to cast products, and reduce production costs. After the cladding layer is partially or completely repaired, the mold can still be used.

[0060] The upper die base 10a is provided with a first pre-pressing forming groove located at one side of the first cavity 10b, the groove bottom 10g of the first pre-pressing forming groove is a plane, and the side wall surface of the first pre-pressing forming groove has at least two opposite inclined surfaces 10h. The lower die base 11a is provided with a second pre-pressing forming groove 11d for cooperating with the first pre-pressing forming groove, the first pre-pressing forming groove is located at one side of the second cavity 11b, and the second pre-pressing forming groove 11d is arc-shaped.

[0061] A plurality of positioning protrusions 11e are provided in the second pre-molding groove 11d. The surface of the positioning protrusions 11e is spherical. During the forging process, these positioning protrusions 11e are used to form a depression 2a on the end face of the first coupling portion 2. The positioning protrusions 11e can also play a positioning role on the first component A during the forging process.

[0062] In order to prevent the temperature-qualified bar C from rolling when placed in the mold cavity, the temperature-qualified bar C is first placed in the second pre-pressing forming groove 11d, and the arc-shaped second pre-pressing forming groove 11d cooperates with a part of the bar C to form a positioning effect on the bar C. Then the upper mold 10 is pressed toward the bar C, and the bar C is deformed by the action of the first pre-pressing forming groove. In this process, the pressure of the pressing bar is much smaller than the subsequent forging pressure in the mold cavity. This process only needs to bend the two ends of the bar C to form a bending portion, and slightly flatten the portion between the bending portions. The bending portion can cooperate with the third inclined surface 11c. When the deformed bar C is placed in the mold cavity, on the one hand, the rolling of the bar C in the cavity is avoided. On the other hand, it also has the effect of preliminary positioning, which avoids the staff from adjusting the position of the bar C during the subsequent forging process, thereby solving the problem of safety hazards.

[0063] In addition, during pre-pressing, since the pre-pressing position is set on the die, after the pre-pressing is completed, the bar C is directly transferred to the die cavity of the die. It is very convenient whether it is at the pre-pressing position or transferring the pre-pressed bar C to the die cavity of the die. Moreover, since oxide scale will form on the surface of the bar C after heating, the oxide scale will be cracked after pre-pressing, making it easy to remove the oxide scale, reducing the impact of the oxide scale on the forging during subsequent forging in the die cavity.

[0064] With the help of Figure 5 For the bar C with qualified temperature, since it is transported to the side of the forging equipment through the chute, the bar C with qualified temperature will not be damaged. For the bar C with unqualified temperature, it is usually received by a basket, that is, a frame is placed under the automatic screening device. After the bar C with unqualified temperature slides out of the automatic screening device, it falls freely into the basket. Since the temperature of the bar C output from the medium frequency furnace is high, the hardness of the surface of the bar C is reduced. After the bar C with unqualified temperature falls freely into the basket, it is easy to deform due to the impact force. If the deformed bar C is cooled to the qualified temperature, or recycled and heated to the qualified temperature and put into the mold for forging, it will inevitably affect the quality of the forging. If the deformation is serious, it will also cause the bar C to be scrapped directly because it cannot be forged.

[0065] like Figure 5 , Figures 10 to 15 As shown, a high-temperature bar material buffer receiving device H is additionally provided at the unqualified material discharging position of the automatic screening device F. Thus, for the bar material C that fails the temperature screening, after being buffered by the high-temperature bar material buffer receiving device H, a portion of the bar material C falls into the high-temperature bar material buffer receiving device H, and another portion of the bar material C is exposed to the outside of the high-temperature bar material buffer receiving device.

[0066] From the above, it can be seen that the bar C that fails the temperature screening is received by the high-temperature bar buffer receiving device H. During the receiving process, due to the cooperation between the bar C and the buffer structure, the bar C is prevented from being greatly impacted, and the bar C and the buffer structure are in surface contact, thereby preventing the bar C from being deformed, so that the bar C that fails the temperature screening can still maintain its original shape (for example, a cylindrical state).

[0067] The high-temperature bar material buffer receiving device H in this embodiment includes a bracket 20, a bar material chute 21, a buffer material receiving container 22, and a flip drive 23. The bar material chute 21 is arranged on the bracket 20 in an inclined state. The bar material chute 21 provides a sliding channel for the bar material C with unqualified temperature. Compared with the free-falling bar, the downward movement speed of the bar material C can be reduced through the guidance of the bar material chute 21, thereby reducing the buffer force generated between the bar material C and the buffer material receiving container 22.

[0068] The buffer receiving container 22 is used to cooperate with or separate from the bar material chute 21, and the buffer receiving container 22 is connected to the bracket 20. When the buffer receiving container 22 cooperates with the bar material chute 21 and is in the receiving position, the buffer receiving container 22 is used to receive the bar material C with unqualified temperature. When the buffer receiving container 22 separates from the bar material chute 21 and reaches the unloading position, the worker uses a clamping tool or a manipulator to take away the bar material C in the buffer receiving container 22.

[0069] The buffer material receiving container 22 includes a material receiving barrel 22a, a buffer assembly, a swing arm 22b, and a support shaft assembly. The material receiving barrel 22a is used to cooperate with or separate from the rod material chute 21. The buffer assembly is installed in the material receiving barrel 22a. When the material receiving barrel 22a is in a position to receive the rod material C, after the rod material C slides into the material receiving barrel 22a through the rod material chute 21, the end face of the rod material C contacts the buffer assembly, so that the buffer assembly buffers the rod material C.

[0070] One end of the swing arm 22b is fixed to the material receiving barrel 22a, the other end of the swing arm 22b is connected to the flip driver 23, the support shaft assembly is fixed to the bracket 20, and the middle part of the swing arm 22b is movably connected to the support shaft assembly. The flip driver 23 applies a force to the swing arm 22b, which can drive the material receiving barrel 22a to rotate, so that the material receiving barrel 22a can be switched between the material receiving and unloading positions.

[0071] The support shaft assembly includes a support 22c, a shaft 22d, and a bearing 22f. The support 22c is fixed to the bracket 20. The end of the shaft 22d is fixed to the support 22c. The bearing 22f is installed on the shaft 22d. The swing arm 22b includes a swing arm body 22b1 and a coupling seat 22b2. The swing arm body 22b1 is sleeved on the shaft 22d. The coupling seat 22b2 is fixed to the swing arm body 22b1. The coupling seat 22b2 is sleeved on the bearing 22f. The support shaft assembly also includes an articulated seat 22h. The articulated seat 22h is fixed to the swing arm 22b. The articulated seat 22h is used to be articulated with the linkage trigger mechanism.

[0072] The buffer assembly includes a lower support 24, a buffer seat 25, and a spring 26. The lower support 24 is provided with a step hole 24a. The buffer seat 25 is I-shaped. One end of the buffer seat 25 cooperates with the step hole 24a. The spring 26 is sleeved on the buffer seat 25. One end of the spring 26 cooperates with the axial end face of the lower support 24, and the other end of the spring 26 cooperates with the other end of the buffer seat 25.

[0073] A barrel 22e is fixed on the inner wall of the barrel 22a. The height of the barrel 22e is smaller than that of the barrel 22a. One end of the barrel 22e cooperates with the axial end surface of the buffer seat 25, and the buffer seat 25 is axially limited by the barrel 22e.

[0074] The buffer assembly further includes a limiting component 26 a , one end of which is fixed to the bottom of the material receiving barrel 22 a , and a distance is provided between the other end of the limiting component 26 a and one end of the buffer seat 25 .

[0075] The flip driver 23 is connected to the buffer receiving container 22, and the flip driver 23 drives the buffer receiving container 22 to switch between the position for receiving the bar material and the position for unloading the bar material. The flip driver 23 is a pneumatic cylinder or an oil cylinder. The flip driver 23 can also be an electric lead screw.

[0076] The high-temperature bar material buffer receiving device H also includes a linkage trigger mechanism for sending a working signal to start the flip drive 23. The bottom of the buffer receiving container 22 is provided with an opening 22g. The linkage trigger mechanism includes a linkage trigger component and a signal generating component that generates an electrical signal when triggered by the linkage trigger component. One end of the linkage trigger component cooperates with the opening 22g, the middle part of the linkage trigger component is hinged to the buffer receiving container 22, the middle part of the linkage trigger component is hinged to the hinge seat 22h, and the signal generating component is fixed to the buffer receiving container 22.

[0077] The linkage trigger mechanism includes a connecting rod 27, one end of which is provided with a first contact 27a, the first contact 27a is bent into a hook shape, the first contact 27a passes through the opening 22g and extends into the interior of the buffer receiving container 22, and one end of the connecting rod 27 is provided with a second contact 27b for triggering the signal generating component.

[0078] The signal generating assembly includes a support plate 28, an intermediate buffer component 29, and a trigger switch 30. One end of the support plate 28 is fixed to the buffer receiving container 22. In this embodiment, one end of the support plate 28 is fixed to the swing arm 22b, and the support plate 28 is in an "F" shape. The intermediate buffer component 29 is installed in the middle of the support plate 28, and the trigger switch 30 is installed at the other end of the support plate 28. One end of the intermediate buffer component 29 cooperates with the other end of the linkage trigger mechanism, and the other end of the intermediate buffer component 29 cooperates with the trigger switch 30. The trigger switch 30 can be a travel switch or a key switch. The trigger switch sends a signal to the controller (not shown in the figure), and the controller can output a control instruction to the flip driver 23 connected thereto, thereby controlling the flip driver 23 to switch between the material receiving and unloading positions.

[0079] The intermediate buffer component 29 is composed of a first spring 29a, a cylindrical component 29b, and a transmission rod 29c. One end of the cylindrical component 29b is provided with an opening, and the other end is provided with an annular baffle 29d. A clamping groove 29e is provided on the circumferential surface of the cylindrical component 29b. The first spring 29a is located in the cylindrical component 29b, and the transmission rod 29c is composed of two parts with different outer diameters. The first spring 29a is sleeved on the part with a smaller outer diameter of the transmission rod 29c. One end of the transmission rod 29c used to cooperate with the trigger switch 30 passes through the annular baffle 29d. A clamping portion 29f is provided on the circumferential surface of the other end of the transmission rod 29c, and the clamping portion 29f is clearance-matched with the clamping groove 29e on the circumferential surface of the cylindrical component 29b.

[0080] When the other end of the transmission rod 29c is subjected to pressure from the second contact 27b, the transmission rod 29c moves along the axial direction of the tubular component 29b, so that one end of the transmission rod 29c presses against the trigger switch 30. The transmission rod 29c compresses the first spring 29a during the axial displacement, and the transmission rod 29c is buffered by the first spring 29a, thereby reducing the impact force of the transmission rod 29c on the trigger switch 30, and avoiding damage to the trigger switch 30 due to sudden excessive impact force. When the second contact 27b is separated from the transmission rod 29c, the transmission rod 29c is reset under the restoring force of the first spring 29a, so that the transmission rod 29c is separated from the trigger switch 30.

[0081] The working process of the high-temperature bar buffer receiving device H is as follows:

[0082] If it slides to the receiving barrel 22a and is in the receiving position cooperating with the rod chute 21, when the temperature-unqualified rod C slides into the receiving barrel 22a through the rod chute 21, the end face of the rod C contacts the end face of the buffer seat 25, and the kinetic energy of the rod C is loaded onto the buffer seat 25, causing the buffer seat 25 to move axially along the step hole 24a, thereby compressing the spring 26. As the buffer seat 25 continues to move, the power of the buffer seat 25 is loaded onto the first contact 27a, driving the connecting rod 27 to rotate counterclockwise, so that the second contact 27b set at the other end of the connecting rod 27 applies pressure to the intermediate buffer component 29, and the intermediate buffer component 29 moves axially under force. The other end of the intermediate buffer component 29 applies power to the trigger switch 30, and the trigger switch 30 sends a signal to the controller. The controller controls the flip driver 23 to work, and the piston rod of the flip driver 23 retracts, driving the swing arm 22b to swing counterclockwise, thereby switching the receiving barrel 22a from the receiving position to the unloading position.

[0083] When the bar material C in the material receiving barrel 22a is extracted, at this time, under the restoring force of the spring 26, the buffer seat 25 is reset. Since the hinged part of the connecting rod 27 and the hinged seat 22h is not in the middle position of the connecting rod 27, the weight of the part from the hinged part on the connecting rod 27 to the second contact 27b is greater than the weight of the part from the hinged part on the connecting rod 27 to the first contact 27a. Therefore, when the buffer seat 25 is separated from the first contact 27a, the connecting rod 27 automatically rotates clockwise under the action of gravity, so that the first contact 27a is moved to the bottom of the buffer seat 25. At the same time, the second contact 27b is separated from the middle buffer component 29, and the middle buffer component 29 is separated from the trigger switch 30. The controller loses the on signal of the trigger switch 30, and the controller controls the flip driver 23 to work. The piston rod of the flip driver 23 extends, and the flip driver 23 drives the swing arm 22b to swing clockwise, so that the material receiving barrel 22a switches from the unloading position to the receiving position.

[0084] In the above S6, the building component blank E without surface cracks is machined, usually the splicing part 3 and the supporting part 4 are machined first, and the method is as follows: Fig.16 The fixture is used to clamp the building component blank E, and the fixture includes a base body 40, a clamping support 41, a supporting boss 42, and multiple clamping components. The base body 40 is used to be fixed on a machine tool, the clamping support 41 is fixed on the side wall of the base body 40, and the supporting boss 42 is fixed on the clamping support 41. When the building component blank E is clamped, the building component blank E is first carried to the supporting boss 42 by personnel, and a supporting force is pre-formed on the building component blank E by the supporting boss 42, and then the building component blank E is clamped by the clamping component.

[0085] like Fig.16 and Fig.17The clamping assembly includes a clamping block 43, a bolt 44 (composed of a screw and a nut), and a second spring 45. A threaded hole is provided on the clamping support 41. The bolt 44 passes through the clamping block 43 and is threadedly connected to the threaded hole on the clamping support 41. The clamping block 43 is L-shaped. The second spring 45 is sleeved on the bolt 44. One end of the second spring 45 cooperates with the clamping block 43, and the other end of the second spring 45 cooperates with the end face of the clamping support 41. Through the action of the second spring 45, a gap is avoided between the clamping block 43 and the nut of the bolt 44, so that it is easier for the building component blank E to be clamped between the clamping assembly and the clamping support 41.

[0086] The clamp further includes a positioning assembly, and the clamping support 41 is provided with an assembly hole, a part of the positioning assembly is installed in the assembly hole, and the other part of the positioning assembly is exposed outside the assembly hole. In this embodiment, the positioning assembly includes a positioning pin 46 and a third spring 47, and the third spring 47 is located in the assembly hole on the clamping support 41, and the third spring 47 is connected to one end of the positioning pin 46, and the other end of the positioning pin 46 is exposed outside the assembly hole.

[0087] Since the end surface of the first connecting portion 2 is provided with a recess 2a, when each positioning pin 46 is matched with each recess 2a one by one, the building component blank E is accurately positioned with the clamping support 41, and the building component blank E can be clamped between the clamping support 41 and the clamping assembly through the action of the clamping assembly.

[0088] The lower part of the seat body 40 in this embodiment is connected to a dividing mechanism (not shown in the figure), through which the seat body 40 can be rotated 180 degrees. Therefore, a set of clamping supports 41, supporting bosses 42, and clamping components are respectively installed at both ends of the seat body 40, which is beneficial to improve processing efficiency.

Claims

1. Forging dies for building components, It is characterized in that include: An upper mold (10), the upper mold (10) comprising an upper mold base (10a), a first cavity (10b) being provided on the upper mold base (10a), two opposite side wall surfaces in the first cavity (10b) being first inclined surfaces (10c), two protrusions (10d) being provided in the first cavity (10b), one side surface of the two protrusions (10d) being respectively integrated with the remaining side wall surfaces in the first cavity (10b), and a groove (10e) being formed between the two first cavities (10b); The lower mold (11) comprises a lower mold base (11a), a second cavity (11b) is provided on the lower mold base (11a), and two opposite side wall surfaces in the second cavity (11b) are third inclined surfaces (11c).

2. The forging die for a building component according to claim 1, It is characterized in that The end surfaces at both ends of the raised portion (10d) are second inclined surfaces (10f), and the second inclined surfaces (10f) are opposite to the first inclined surfaces (10c).

3. The forging die for a building component according to claim 1, It is characterized in that The surfaces of the first inclined surface (10c) and the groove (10e) are provided with a first surfacing layer, and the surface of the protruding portion (10d) is provided with a second surfacing layer.

4. The forging die for a building component according to claim 1, It is characterized in that A third surfacing layer is provided on the surface of the second cavity (11b).

5. The forging die for a building component according to any one of claims 1 to 4, It is characterized in that The upper die seat (10a) is provided with a first pre-pressing forming groove located on one side of the first cavity (10b), the groove bottom (10g) of the first pre-pressing forming groove is a plane, and the side wall surface of the first pre-pressing forming groove has at least two opposite inclined surfaces (10h); The lower die seat (11a) is provided with a second pre-pressing forming groove (11d) for cooperating with the first pre-pressing forming groove, the first pre-pressing forming groove is located on one side of the second cavity (11b), and the second pre-pressing forming groove (11d) is arc-shaped.